Conductive material, preparation method therefor, pressure sensor, battery cell and electric device
By using conductive materials and flexible substrates in pressure sensors, combined with the ratio design of temperature rise and temperature drop materials, the problem of temperature change interference in the lithium battery is solved, and higher detection sensitivity and accuracy are achieved.
Patent Information
- Application Number
- PCT/CN2024/076633
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-19
- Filing Date
- 2024-02-07
- Publication Date
- 2024-11-28
AI Technical Summary
The existing pressure sensors have a great interference to the detection under the complex temperature variable environment inside the lithium battery, resulting in an increase in detection error and making it difficult to obtain accurate battery internal information.
Using conductive materials, by mixing temperature rise and temperature drop materials, the change rate of its resistivity is controlled so that it is basically unaffected by temperature. Combined with flexible substrates and conductive particles, pressure sensors suitable for different temperature ranges are designed, including The electrode layer and the sensitive layer, and the raised structures of different heights are provided on the sensitive layer to enhance the sensitivity.
It improves the detection sensitivity of the sensor at different temperatures, reduces the error caused by temperature changes, enhances the accuracy of obtaining internal information of the battery, and is suitable for a wide range of pressure detection environments.
Smart Images

Figure CN2024076633_28112024_PF_FP_ABST
Abstract
Description
Conductive material and preparation method, pressure sensor, battery cell and electrical equipment Technical Field
[0001] The present application relates to the field of measurement technology, and in particular to a conductive material and a preparation method thereof, a pressure sensor, a battery cell and an electrical device. Background Art
[0002] Pressure sensors are components that output applied pressure as an electrical signal. They are characterized by their simple structure, low power consumption, and fast dynamic response. They are widely used in various fields. For example, they can be embedded in batteries to detect internal electrode expansion and other behaviors, reflecting the evolution of the battery's internal structure and providing real-time insights into the battery's operating status. Temperature significantly interferes with pressure sensor measurements. Achieving temperature suppression is crucial to the practical application of sensors, especially in the complex temperature fluctuations found in lithium batteries.
[0003] Summary of the Invention
[0004] The main technical problem addressed by this application is to provide a conductive material and preparation method, a pressure sensor, a battery cell, and an electrical device. These materials can prevent the resistivity of the conductive material from significantly changing with temperature, i.e., the resistivity of the conductive material is essentially unaffected by temperature, thereby improving the sensor's detection sensitivity at different temperatures and reducing detection errors caused by temperature changes.
[0005] In a first aspect, the present application provides a conductive material comprising a flexible substrate and conductive particles dispersed within the flexible substrate. The conductive particles comprise a temperature-rising material and a temperature-reducing material. The temperature-rising material is a material whose resistivity increases as temperature increases, and the temperature-reducing material is a material whose resistivity decreases as temperature increases. The ratio of the temperature-reducing material to the temperature-rising material is set such that, within a temperature range of -40°C to +200°C, the absolute value of the rate of change of the resistivity of the conductive material is less than or equal to 0.01. By mixing the temperature-rising and temperature-reducing materials, the resistance of the mixed material does not change significantly when the temperature changes, that is, the resistivity of the mixed material is substantially unaffected by temperature, thereby improving the detection sensitivity of the sensor at different temperatures and reducing the error caused by temperature changes in detection.
[0006] In some embodiments of the present application, the ratio of the temperature-reducing material to the temperature-raising material is set so that the absolute value of the rate of change of the resistivity of the conductive material is less than or equal to 0.008 within a temperature range of +25°C to +80°C. The closer the rate of change of the resistivity of the conductive material is to zero, the better. This makes the resistivity of the conductive material insensitive to temperature and reduces errors in the collected resistance caused by temperature changes.
[0007] In some embodiments of the present application, the ratio of the temperature-lowering material to the temperature-raising material is set so that the absolute value of the rate of change of the conductive material's resistance is less than or equal to 0.01 within the temperature range of -40°C to +200°C. This arrangement substantially unaffects the material's resistance, thereby improving the sensor's detection sensitivity at different temperatures and reducing detection errors caused by temperature fluctuations.
[0008] In some embodiments of the present application, the ratio of the temperature-lowering material to the temperature-raising material is set so that the absolute value of the rate of change of the conductive material's resistance is less than or equal to 0.008 within a temperature range of +25°C to +80°C. This arrangement effectively reduces the effect of temperature on the material's resistance within a conventional temperature range.
[0009] In some embodiments of the present application, within the temperature range of -40°C to +200°C, the absolute value ratio of the temperature coefficient of resistance of the temperature-rising material to the temperature-reducing material is 30:1-1:30, and optionally 15:1-1:10. The temperature coefficient of resistance is the relative change in the resistance of a material when the temperature changes by 1°C. This configuration allows the ratio of the temperature-rising material content to the temperature-reducing material content to be controlled within an optimal range, ensuring that the difference in the content between the two materials is not too large, thereby preventing uneven mixing.
[0010] In some embodiments of the present application, within a temperature range of -40°C to +200°C, the absolute value of the ratio of the rate of change of the resistivity of the temperature-raising material to the rate of change of the resistivity of the temperature-lowering material is 25:1-1:25, and can optionally be 10:1-1:5. This configuration allows the ratio of the content of the temperature-raising material to the content of the temperature-lowering material to be controlled within an optimal range, ensuring that the difference in content between the two materials is not too large, thereby preventing uneven mixing.
[0011] In some embodiments of the present application, the mass ratio of the temperature-raising material to the temperature-lowering material is 15:1-1:20, and can optionally be 12:1-1:8. This arrangement allows the ratio of the temperature-raising material content to the temperature-lowering material content to be controlled within an optimal range, ensuring that the difference in the content of the temperature-raising material and the temperature-lowering material content is not too large, thereby preventing uneven mixing.
[0012] In some embodiments of the present application, the electrical conductivity of the temperature-rising material is greater than 1S·m -1 ; and / or the conductivity of the temperature drop material is greater than 1S·m -1 ; and / or the conductivity of the conductive material is greater than 1S·m -1 By controlling the conductivity and improving the conductivity of the conductive material, the sensor can be made more sensitive.
[0013] In some embodiments of the present application, the temperature-rising material includes one or more of graphite, gold powder, silver powder, nickel powder, zinc-chromium alloy, nickel-copper alloy, etc. By selecting these materials, the sensor detection can be made more sensitive.
[0014] In some embodiments of the present application, the temperature-reducing material includes one or more of carbon nanotubes, Keqin black, graphene, carbon black, and ceramic materials primarily composed of metal oxides of manganese, cobalt, nickel, and copper. The selection of these materials can make the sensor more sensitive.
[0015] In some embodiments of the present application, the conductive particles include graphite particles and carbon nanotube particles, with the mass ratio of graphite particles to carbon nanotube particles being 1:1-1:20, and optionally 1:9-1:15. The combination of graphite particles and carbon nanotube particles provides enhanced conductivity, and the nanoscale size of the conductive particles facilitates dispersion and more uniform mixing, resulting in more sensitive signal feedback and improved sensitivity.
[0016] In some embodiments of the present application, the carbon nanotube particles include multi-walled carbon nanotube particles, with an outer diameter of 6-13 nm and a length of 2.5-20 μm. By selecting carbon nanotubes of this size, the material has better conductivity and more sensitive detection.
[0017] In some embodiments of the present application, the particle size Dv50 of the graphite particles is 7-10 μm. By selecting graphite of this size, the conductive performance of the material is improved and the detection is more sensitive.
[0018] In some embodiments of the present application, the mass ratio of the flexible substrate to the conductive particles is 15:1-5:1, and can be optionally 12:1-8:1. This configuration can improve the elasticity and conductivity of the sensitive layer.
[0019] In some embodiments of the present application, the flexible substrate includes one or more of thermoplastic polyurethane, polyvinyl alcohol, chloroprene rubber, nitrile rubber, styrene-butadiene block copolymer, and polyacrylic acid, and may be aliphatic thermoplastic polyurethane. This configuration can provide the sensitive layer with higher durability and wear resistance.
[0020] In a second aspect, the present application provides a pressure sensor, which includes an electrode layer and a sensitive layer. The sensitive layer uses any of the above-mentioned conductive materials, which can improve the detection sensitivity and broaden the applicable temperature.
[0021] In some embodiments of the present application, the sensitive layer includes a base layer and at least two protrusion structures protruding from the base layer at different heights. Each protrusion structure includes at least one protrusion. Each protrusion is located on the side of the base layer facing the electrode layer, and the contact area between each protrusion and the electrode layer is configured to vary with the pressure applied to the electrode layer. By providing two protrusion structures of different heights, the pressure sensitivity range of each protrusion structure is differentiated, enabling the pressure sensor to be adapted for detection in a variety of pressure environments, thereby effectively achieving the desired range and sensitivity of the pressure sensor.
[0022] In a third aspect, the present application provides a method for preparing a pressure-sensitive layer, comprising: providing a flexible substrate slurry; adding conductive particles to the flexible substrate slurry, the conductive particles comprising a temperature-rising material and a temperature-reducing material, wherein the temperature-rising material is a material whose resistivity increases with increasing temperature, and the temperature-reducing material is a material whose resistivity decreases with increasing temperature, the ratio of the temperature-reducing material to the temperature-rising material being set such that the absolute value of the rate of change of the resistivity of the conductive material is less than or equal to 0.01 within a temperature range of -40°C to +200°C; and curing the flexible substrate slurry to form the pressure-sensitive layer. The resulting pressure-sensitive layer has a wide applicable temperature range.
[0023] In a fourth aspect, the present application provides a battery cell, comprising a housing and any one of the above-mentioned pressure sensors, wherein the pressure sensor is disposed inside the housing, thereby enabling acquisition of internal information of the battery, and the acquired data is more accurate.
[0024] In a fifth aspect, the present application provides an electrical device including the aforementioned battery cell, which can acquire internal information of the battery, and the acquired data is more accurate.
[0025] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are listed below. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present application. Those skilled in the art can also derive other drawings based on these drawings without inventive work, among which:
[0027] FIG1 is a schematic cross-sectional view of a pressure sensor according to one or more embodiments of the present application;
[0028] FIG2 is a schematic cross-sectional view of a pressure sensor under different pressure states according to one or more embodiments of the present application;
[0029] FIG3 a is a diagram showing the arrangement of the protrusion structure of the sensitive layer of the pressure sensor according to one or more embodiments of the present application;
[0030] FIG3 b is a schematic diagram illustrating the arrangement of the protrusion structures of the sensitive layer on the pressure sensor sample according to one or more embodiments of the present application;
[0031] FIG4 is a schematic plan view of the structure of a pressure sensor according to one or more embodiments of the present application;
[0032] FIG5 is a schematic diagram of an exploded structure of a battery according to one or more embodiments;
[0033] FIG6 is a schematic diagram of the exploded structure of a battery cell according to one or more embodiments;
[0034] FIG7 is a schematic structural diagram of a vehicle according to one or more embodiments;
[0035] FIG8 is a schematic diagram of resistance change rate and temperature curves of the embodiment and the comparative example.
[0036] In the attached figure:
[0037] 1000, vehicle; 300, motor; 200, controller; 100, battery; 10, housing; 11, first portion; 12, second portion; 20, battery cell; 21, end cap; 21a, electrode terminal; 22, housing; 23, electrode assembly;
[0038] 400, pressure sensor; 40, electrode layer; 42, sensitive layer; 420, base layer; 422, protrusion structure; 4221, protrusion; 4222, protrusion; 4223, protrusion; 401, first electrode; 402, second electrode; 403, electrode base; 44, corrosion-resistant protective layer; 46, insulating layer; 48, sensitive layer adhesive; 49, insulating layer adhesive. DETAILED DESCRIPTION
[0039] The following will be combined with the accompanying drawings in the embodiments of this application to clearly and completely describe the technical solutions in the embodiments of this application. Obviously, the embodiments described are only part of the embodiments of this application, not all of the embodiments. Based on the embodiments of this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.
[0040] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this application belongs; the terms used herein are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" and any variations thereof in the specification and claims of this application and the above-mentioned figure descriptions are intended to cover non-exclusive inclusions.
[0041] In the description of the embodiments of the present application, the technical terms "first" and "second" are only used to distinguish different objects, and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features. In the description of the embodiments of the present application, unless otherwise clearly and specifically defined, the term "multiple" refers to more than two (including two). Similarly, "multiple groups" refers to more than two groups (including two groups), and "multiple pieces" refers to more than two pieces (including two pieces).
[0042] References herein to "embodiments" mean that a particular feature, structure, or characteristic described in connection with the embodiments may be included in at least one embodiment of the present application. The appearance of this phrase in various places in the specification does not necessarily refer to the same embodiment, nor does it constitute an independent or alternative embodiment that is mutually exclusive of other embodiments. It is understood, both explicitly and implicitly, by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0043] In the description of the embodiments of this application, the term "and / or" is simply a description of the association relationship between associated objects, indicating that three relationships can exist. For example, A and / or B can represent the following three situations: A exists alone, A and B exist simultaneously, and B exists alone. In addition, the character " / " in this document generally indicates that the associated objects are in an "or" relationship.
[0044] In the description of the embodiments of the present application, the technical terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the embodiments of the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the embodiments of the present application.
[0045] In the description of the embodiments of the present application, unless otherwise expressly specified or limited, technical terms such as "installed," "connected," "connected," and "fixed" should be understood in a broad sense. For example, they can refer to fixed connections, detachable connections, or integration; mechanical connections or electrical connections; direct connections or indirect connections through an intermediate medium; internal connections between two components or interactions between two components. Those skilled in the art can understand the specific meanings of the above terms in the embodiments of the present application based on specific circumstances.
[0046] Amounts, ratios, and other numerical values are presented herein in a range format. It should be understood that such range format is used for convenience and brevity and should be interpreted flexibly to include not only the values explicitly specified as range limits, but also all individual values or sub-ranges encompassed within the range, as if each value and sub-range were explicitly specified.
[0047] With the widespread application of electrochemical devices (e.g., lithium-ion batteries), people have increasingly higher requirements for their performance, especially battery safety, stability, and capacity. They expect batteries to have good comprehensive performance in all aspects. Lithium batteries are complex systems in which chemical energy, thermal energy, and electrical energy are highly coupled in (electro)chemical reactions. Real-time understanding of the internal working state of the battery is key to the development and design of new batteries and their efficient and safe operation. At the microscopic level, lithium de-lithiation and lithium insertion reactions during the charge and discharge process of lithium batteries cause the electrode materials to expand, increasing internal stress in the battery and easily leading to electrode delamination and increased SEI film thickness. Studies have shown that the expansion of graphite electrodes can reach 10%, while that of graphite-silicon composite electrodes can reach 280%. Under long-term cycling, the internal electrode sheets will experience irreversible expansion and associated problems such as electrolyte consumption, capacity reduction, and lithium dendrites due to changes in the battery potential, resulting in decreased battery performance and shortened battery life. At a macroscopic level, the combined expansion of multiple layers of wound electrode sheets causes the cell to expand in volume, which in turn compresses against the battery casing, causing deformation. This synergistic mechanical-thermal coupling significantly alters the internal and external stresses and heat generation behavior of the battery, with uncontrollable factors increasing with age. Electrode expansion behavior reflects the evolution of the internal structure and contains a wealth of information. Obtaining information on battery expansion behavior is crucial for a comprehensive and in-depth understanding of lithium-ion battery operating modes, optimizing battery material selection, monitoring battery energy conversion status, gaining a deeper understanding of the battery's internal operating mechanisms, and establishing more accurate digital twin models of the battery cell. This information can provide crucial information to battery management systems (BMS), further improving the safety, efficiency, and stability of lithium-ion batteries during operation.
[0048] To obtain more accurate and reliable information from the battery's interior, embedded sensors can be used to measure temperature and stress. However, temperature significantly interferes with pressure sensor measurements. Achieving temperature suppression is crucial for the practical application of sensors, especially in the complex, fluctuating temperature environments found within lithium batteries. The development and design of high-performance embedded sensors is severely lacking.
[0049] To solve the above technical problems, the present application provides a pressure sensor. Referring to FIG1 , FIG1 is a schematic cross-sectional view of a pressure sensor according to one or more embodiments of the present application. The pressure sensor 400 includes an electrode layer 40 and a sensitive layer 42 .
[0050] The pressure sensor 400 is a component that outputs the applied pressure in the form of an electrical signal. The pressure sensor 400 may be a resistive sensor that converts the measured pressure into an electrical signal that is related to the pressure by using a change in resistance.
[0051] Pressure sensor 400 can be a thin-film sensor. It can be fabricated using metals, semiconductors, and polymers to form temperature, pressure, and strain sensors. These sensors can be embedded within batteries to measure temperature and stress. This enables in-situ detection of internal electrode expansion pressure signals and temperature under various operating conditions. This provides critical data for the construction of accurate battery numerical models and battery management systems, and serves as a crucial tool for the industrialization of a new generation of safe and efficient lithium-ion batteries.
[0052] Specifically, the electrode layer 40 is used to collect changes in the electrical signal of the sensitive layer 42, forming a conductive network in contact with the sensitive layer 42 to convert the pressure signal into an electrical signal. The sensitive layer 42 is used to form a contact resistance with the electrode layer 40, so that the pressure sensor 400 can detect the pressure based on the contact resistance between the sensitive layer 42 and the electrode layer 40. In other words, it can be a bulk resistive pressure sensor, which mainly relies on the deformation of the sensitive layer under the action of external force, causing the internal conductive network to break or reconstruct, resulting in a change in resistance, thereby reflecting the magnitude of the applied external force.
[0053] In some embodiments of the present application, the electrode layer 40 includes a first electrode 401 and a second electrode 402 arranged in a forked manner. The forked electrodes are electrodes with a periodic pattern in a finger-like or comb-like surface. The first electrode 401 and the second electrode 402 are located on the same side of the sensitive layer 42, that is, the first electrode 401 and the second electrode 402 are coplanar electrodes. Due to the narrow internal space of the battery, if the sensor is too thick, when the sensor is placed inside the battery, it may cause damage to the battery electrode material and lithium deposition due to stress concentration at a single point. In this embodiment, the use of coplanar electrodes based on forked electrodes can effectively reduce the thickness of the sensor without affecting the deformation ability of the sensitive layer under pressure, thereby obtaining sensitive resistance change acquisition capabilities.
[0054] In some embodiments of the present application, the material of the sensitive layer 42 includes a flexible substrate and conductive particles dispersed in the flexible substrate.
[0055] The flexible substrate is used to enable the sensitive layer 42 to deform under pressure and recover after pressure is released. The conductive particles form a conductive network in contact with the electrode layer 40. The choice of flexible substrate largely determines the mechanical properties of the pressure sensor, affecting its deformation and recovery under pressure. The choice of conductive particles, in turn, affects the contact resistance, influencing the sensitivity, accuracy, and range of the pressure sensor. Therefore, the material of the sensitive layer is crucial in determining its mechanical and electrical properties. The selection of the sensitive layer material must consider the sensor's application environment within a lithium battery. For example, the sensor's need to operate under high pressure (greater than 1.2 MPa) for extended periods (greater than 3 months) and multiple cycles (greater than 100 times) places high demands on its mechanical properties. Furthermore, temperature can significantly interfere with pressure sensor measurements, especially in the complex, fluctuating temperature environments of lithium batteries. Furthermore, after being embedded in a lithium battery, the sensor undergoes subsequent drying, liquid injection, and aging processes, with temperatures reaching as high as 105°C. Therefore, the sensor must be able to withstand even higher temperatures without breaking while suppressing thermal fluctuations. However, the current common sensitive layer materials are incompressible, and have disadvantages such as response speed being limited by the material rebound speed, severe creep phenomenon, thick thickness, and large temperature fluctuation.
[0056] To solve the above technical problems, the present application provides a conductive material for a pressure-sensitive layer, wherein the conductive material includes a flexible substrate and conductive particles dispersed in the flexible substrate, wherein the conductive particles include a temperature-rising material and a temperature-dropping material, wherein the temperature-rising material is a material whose resistivity increases as the temperature increases, and the temperature-dropping material is a material whose resistivity decreases as the temperature increases, and the ratio of the temperature-dropping material to the temperature-rising material is set such that in a temperature range of -40°C to +200°C, the absolute value of the rate of change of the resistivity of the conductive material is less than or equal to 0.01.
[0057] In this embodiment, the resistivity change rate is based on the resistivity of the conductive particles at 25°C. The difference between the resistivity at different temperatures and the reference resistivity is calculated, and then the ratio is calculated with the reference resistivity. For example, the resistivity change rate from 25°C to 50°C = (resistivity 50℃ -Resistivity 25℃ ) / resistivity 25℃ .
[0058] Among them, resistivity is a physical quantity used to express the resistance characteristics of various materials. A certain material is 1m long and has a cross-sectional area of 1m. 2 The resistance of a conductor is numerically equal to the resistivity of the material. Resistivity reflects a material's ability to resist electric current. It depends not only on the type of material but also on external factors such as temperature. Specifically, when the temperature changes, the resistivity of a material also changes. For some materials, the resistivity increases with increasing temperature, while for others, the resistivity decreases. In other words, when the length and cross-sectional area of a material remain constant, the resistance of a temperature-rising material increases with increasing temperature, while the resistance of a temperature-decreasing material decreases with increasing temperature.
[0059] In this embodiment, by mixing a temperature-rising material and a temperature-lowering material, the resistance increase of the temperature-rising material is balanced by the resistance decrease of the temperature-lowering material, or the resistance decrease of the temperature-lowering material is balanced by the resistance increase of the temperature-rising material, so that the resistance of the mixed material does not change significantly when the temperature changes, that is, the resistivity of the mixed material is basically unaffected by temperature, thereby improving the detection sensitivity of the sensor at different temperatures and reducing the error caused by temperature changes in detection.
[0060] In some embodiments of the present application, the ratio of the temperature-reducing material to the temperature-raising material is set so that within the temperature range of +25°C to +80°C, the absolute value of the rate of change of the resistivity of the conductive material is less than or equal to 0.008. For example, the rate of change of the resistivity of the conductive material can be 0.001, 0.0015, 0.002, 0.0025, 0.003, 0.004, 0.005, 0.0055, 0.006, 0.007, 0.008, etc. The closer the rate of change of the resistivity of the conductive material is to zero, the better, making the resistivity of the conductive material insensitive to temperature and reducing the error in the collected resistance caused by temperature changes. Through this setting, the pressure sensor can also operate at extreme temperatures such as -40°C to +200°C with a small detection error; and at normal temperatures of +25°C to +80°C, the rate of change of the resistivity is even smaller, and the detection sensitivity is higher.
[0061] In some embodiments of the present application, the ratio of the temperature-dropping material to the temperature-raising material is set so that the absolute value of the rate of change of the resistance of the conductive material is less than or equal to 0.01 within the temperature range of -40°C to +200°C. Alternatively, the ratio of the temperature-dropping material to the temperature-raising material is set so that the absolute value of the rate of change of the resistance of the conductive material is less than or equal to 0.008 within the temperature range of +25°C to +80°C. For example, it can be 0.001, 0.0015, 0.002, 0.0025, 0.003, 0.004, 0.0045, 0.005, 0.0055, 0.006, 0.007, 0.008, etc. The rate of change of resistance is based on the resistance of the conductive particles at 25°C, and the difference between the resistance at different temperatures and the reference resistance is calculated, and then the ratio is calculated with the reference resistance. For example, the rate of change of resistance from 25°C to 50°C = (resistance 50℃ -resistance 25℃ ) / resistance 25℃ .
[0062] From the perspective of the conductive material's material properties, this application aims to minimize the rate of change in its resistivity. Furthermore, from the perspective of the sensor's resistance, the goal is to maintain the contact resistance between the sensitive layer 42 and the electrode layer 40 at essentially the same level under the same pressure conditions and at different temperatures. In other words, when the pressure remains constant, the contact area between the sensitive layer 42 and the electrode layer 40 remains constant, and the contact resistance is unaffected by temperature changes.
[0063] In one embodiment, a temperature coefficient can be used to represent the rate at which the physical properties of a material change with temperature. Specifically, the temperature coefficient of resistance (TCR) can be used to represent the relative change in the resistance value of a material when the temperature changes by 1 degree Celsius. Specifically, TCR = (R2-R1) / (R1*(T2-T1)) = (R2-R1) / (R1*ΔT), where R1 is the resistance value (Ω) at temperature T1 and R2 is the resistance value (Ω) at temperature T2. The larger the temperature coefficient, the greater the resistance change (increase or decrease) under the same temperature change.
[0064] The temperature coefficient of resistance can be positive, negative, or zero. A material with a positive temperature coefficient has a property where its resistivity increases with increasing temperature; a material with a negative temperature coefficient has a resistivity that decreases with increasing temperature; and a zero temperature coefficient means its resistivity remains essentially unchanged with temperature. In this application, the goal is to achieve a temperature coefficient of zero for the conductive material by adjusting the ratio of temperature-rising materials to temperature-reducing materials.
[0065] In some embodiments of the present application, within the temperature range of -40°C to +200°C, the absolute value ratio of the temperature coefficient of resistance of the temperature-raising material to the temperature coefficient of resistance of the temperature-dropping material is 30:1-1:30, and can optionally be 15:1-1:10. For example, it can be 30:1, 20:1, 10:1, 5:1, 1:1, 1:5, 1:8, or 1:10. Specifically, materials with smaller temperature coefficients can be selected, that is, materials that are inherently insensitive to temperature. It is best if the temperature coefficient of the selected temperature-raising material is similar to the temperature coefficient of the selected temperature-dropping material; that is, when the materials are of similar size, the resistance increase caused by the same amount of temperature-raising material is similar to the resistance decrease caused by the temperature-dropping material. By setting the absolute value ratio of the temperature coefficient of resistance of the temperature-raising material to the temperature-dropping material to 30:1-1:30, the ratio of the temperature-raising material content to the temperature-dropping material content can be adjusted to a preferred range, ensuring that the difference in content between the two is not too large, thereby avoiding uneven mixing. When the absolute value ratio of the resistance temperature coefficient of the temperature-rising material to that of the temperature-dropping material is 15:1-1:10, the absolute values of the resistance temperature coefficients of the temperature-rising material and the temperature-dropping material can be made closer, making the difference in their content smaller and the mixing more uniform. When the absolute value ratio of the resistance temperature coefficient of the temperature-rising material to that of the temperature-dropping material is greater than 30:1 or less than 1:30, the absolute value difference in the resistance temperature coefficient of the temperature-rising material and the temperature-dropping material is large, resulting in a large difference in the ratio between the two and uneven mixing.
[0066] In some embodiments of the present application, within the temperature range of -40°C to +200°C, the absolute value of the ratio of the rate of change of the resistivity of the temperature-raising material to the rate of change of the resistivity of the temperature-reducing material is 25:1-1:25, and can optionally be 10:1-1:5. For example, it can be 25:1, 20:1, 10:1, 5:1, 1:1, 1:2, 1:3, 1:5, etc. Specifically, materials with a small resistivity change can be selected, that is, materials that are inherently insensitive to temperature. It is best if the resistivity change rate of the selected temperature-raising material is similar to that of the selected temperature-reducing material; that is, when the materials are of similar size, the increase in resistance caused by the same amount of temperature-raising material is similar to the decrease in resistance caused by the same amount of temperature-reducing material. By setting the absolute value of the ratio of the rate of change of the resistivity of the temperature-raising material to the rate of change of the resistivity of the temperature-reducing material to 25:1-1:25, the content ratio of the temperature-raising material to the temperature-reducing material can be adjusted to an optimal range, ensuring that the difference in content between the two is not too large, thereby avoiding uneven mixing. When the absolute value of the ratio of the rate of change of the resistivity of the temperature-rising material to the rate of change of the resistivity of the temperature-dropping material is between 10:1 and 1:5, the absolute values of the rates of change of the resistivity of the temperature-rising material and the temperature-dropping material can be made closer, making the difference in their content smaller and the mixing more uniform. When the absolute value ratio of the temperature coefficient of resistance of the temperature-rising material to the temperature-dropping material is greater than 10:1 or less than 1:5, the absolute value of the rate of change of the resistivity of the temperature-rising material and the temperature-dropping material differs significantly, resulting in a significant difference in the ratio between the two and uneven mixing.
[0067] In some embodiments of the present application, the mass ratio of the temperature rising material and the temperature dropping material is 15:1-1:20, and can be optionally 12:1-1:8. For example, it can be 15:1, 13:1, 10:1, 5:1, 1:1, 1:3, 1:5, 1:8, etc. By controlling the mass ratio within this range, the difference in content between the two will not be too large, so as to avoid uneven mixing due to too large a difference in content between the two. When the mass ratio of the temperature rising material and the temperature dropping material is 12:1-1:8, the difference in content between the temperature rising material and the temperature dropping material can be made smaller, and the mixing can be more uniform. When the ratio of the mass content of the temperature rising material to the mass content of the temperature dropping material is greater than 15:1, or less than 1:8, the difference in content between the temperature rising material and the temperature dropping material is large, resulting in uneven mixing.
[0068] In some embodiments of the present application, the electrical conductivity of the temperature-rising material is greater than 1S·m -1 ; and / or the conductivity of the temperature drop material is greater than 1S·m -1 ; and / or the conductivity of the conductive material is greater than 1S·m -1The conductivity of the conductive material can be between the conductivity of the temperature-rising material and the conductivity of the temperature-dropping material; it can also be greater than the conductivity of both the temperature-rising and temperature-dropping materials; or it can be less than the conductivity of both the temperature-rising and temperature-dropping materials. By controlling the conductivity and selecting a material with relatively high conductivity, the conductivity of the conductive material can be improved, making the sensor more sensitive.
[0069] In some embodiments of the present application, the temperature-rising material includes one or more of graphite, gold powder, silver powder, nickel powder, zinc-chromium alloy, nickel-copper alloy, etc. By selecting these materials, the sensor detection can be made more sensitive.
[0070] In some embodiments of the present application, the temperature-reducing material includes one or more of carbon nanotubes, Keqin black, graphene, carbon black, and ceramic materials primarily composed of metal oxides of manganese, cobalt, nickel, and copper. The selection of these materials can make the sensor more sensitive.
[0071] When the temperature-rising material and the temperature-dropping material include multiple materials, the mass ratio of the temperature-rising material to the temperature-dropping material is the ratio of the total mass of all the temperature-rising materials to the total mass of all the temperature-dropping materials.
[0072] In some embodiments of the present application, the conductive particles include graphite particles and carbon nanotube particles, and the mass ratio of the graphite particles to the carbon nanotube particles is 1:1-1:20. It can be 1:9-1:15. For example, it can be 1:1, 1:3, 1:5, 1:7, 1:9, 1:11, 1:12, 1:15, 1:18, 1:20, etc. By selecting a mixture of graphite particles and carbon nanotube particles, the material is relatively stable and has high conductivity, and the conductive particles can be made nanometer-sized, which is easier to disperse and mix more evenly, making the signal feedback more sensitive and improving sensitivity. When the mass ratio of graphite particles to carbon nanotube particles is 1:9-1:15, the difference in content between the graphite particles and the carbon nanotube particles can be smaller, and the mixing is more uniform. When the mass content ratio of the graphite particles to the carbon nanotube particles is greater than 1:1, or less than 1:20, the difference in content between the graphite particles and the carbon nanotube particles is large, resulting in uneven mixing.
[0073] In some embodiments of the present application, the carbon nanotube particles include multi-walled carbon nanotube particles, with an outer diameter of 6-13 nm and a length of 2.5-20 μm. The graphite particles have a particle size (Dv50) of 7-10 μm. By selecting carbon nanotubes and graphite of these sizes, the material exhibits improved electrical conductivity and more sensitive detection.
[0074] In some embodiments of the present application, the flexible substrate comprises one or more of thermoplastic polyurethane, polyvinyl alcohol, chloroprene rubber, nitrile rubber, styrene-butadiene block copolymer, and polyacrylic acid. Aliphatic thermoplastic polyurethane may be used. The use of polyurethane provides greater durability and wear resistance than base materials such as polydimethylsiloxane (PDMS) and aliphatic aromatic random copolyester (Eco-flex).
[0075] In some embodiments of the present application, the mass ratio of the flexible substrate to the conductive particles is 15:1-5:1, and can be optionally 12:1-8:1. For example, it can be 15:1, 12:1, 10:1, 8:1, 6:1, 5:1, etc. Among them, if the content of the flexible substrate is too low, the elasticity of the material will be insufficient, resulting in a smaller range of the sensor; if the content of the flexible substrate is too high, the support of the sensitive layer will be insufficient, resulting in collapse, which will reduce the detection accuracy. By setting the mass ratio of the flexible substrate to the conductive particles to 15:1-5:1, the elasticity and conductivity of the sensitive layer can be improved. By setting the mass ratio of the flexible substrate to the conductive particles to 12:1-8:1, the elasticity and conductivity of the sensitive layer can be further improved.
[0076] In the above embodiments, by regulating the material composition of the sensitive layer, especially regulating the conductive material composition, the conductive material is made insensitive to temperature, which can expand the operating temperature range of the sensor, reduce the error caused by temperature changes in detection, and improve detection sensitivity.
[0077] Please continue to refer to Figure 1. In some embodiments of the present application, the sensitive layer 42 has a microstructure, specifically including a plurality of protruding structures 422 of at least two different heights. The protruding structures 422 are in contact with two electrodes that are not connected to the electrode layer 40, thereby building a conductive network and forming a contact resistance. The height direction is along the direction from the substrate layer 420 to the electrode layer 40 (the X direction shown in the figure), and the height of the protruding structure 422 can be measured under a scanning electron microscope. As the pressure gradually increases, the contact area between the protruding structure 422 and the electrode gradually increases, and the contact resistance gradually decreases. The change in the contact area of the protruding structure 422 is caused by the compression deformation of the protruding structure 422 caused by the pressure and the support of the electrode layer 40.
[0078] Please refer to Figure 2, which is a schematic diagram of the cross-sectional structure of the pressure sensor under different pressure states of one or more embodiments of the present application. Among them, Figure 2 (a) is a schematic diagram of the cross-sectional structure of the pressure sensor under the first pressure state of one or more embodiments of the present application, Figure 2 (b) is a schematic diagram of the cross-sectional structure of the pressure sensor under the second pressure state of one or more embodiments of the present application, and Figure 2 (c) is a schematic diagram of the cross-sectional structure of the pressure sensor under the third pressure state of one or more embodiments of the present application. As the pressure increases further, the protruding structure 422 that was not originally involved in the construction of the conductive network contacts the electrode and is incorporated into the conductive network, which is equivalent to connecting a new resistor in parallel to the original conductive network, thereby further reducing the overall resistance at both ends of the electrode to reflect the change in pressure value.
[0079] In this embodiment, three protrusion structures 422 of different heights are included, wherein protrusion 4221 is a protrusion of a protrusion structure of a first height, protrusion 4222 is a protrusion of a protrusion structure of a second height, and protrusion 4223 is a protrusion of a protrusion structure of a third height. The height of protrusion 4223 is greater than the height of protrusion 4221, and the height of protrusion 4221 is greater than the height of protrusion 4222. As shown in (a) of Figure 2, under the first pressure state, protrusions 4221 and protrusions 4223 contact the first electrode 401 and the second electrode 402 of electrode layer 40, respectively, to form a conductive network. At this time, the contact area between the protrusions and the electrodes is small. As the pressure increases, as shown in (b) of Figure 2, under the second pressure (the second pressure is greater than the first pressure) state, the contact area between protrusions 4221 and protrusions 4223 and the electrodes increases. As the pressure continues to increase, as shown in Figure 2(c), under the third pressure (the third pressure is greater than the second pressure), protrusion 4222, which was originally not in contact with the electrode, begins to contact the electrode. Protrusion 4222 also contacts the first electrode 401 and the second electrode 402, forming a new conductive network. From state (a) to state (c) in Figure 2, the contact area between protrusion 4221 and the first electrode 401 gradually increases. From state (a) to state (b) in Figure 2, the contact area between protrusion 4223 and the second electrode 402 gradually increases. However, from state (b) to state (c) in Figure 2, the contact area between protrusion 4223 and the second electrode 402 does not increase significantly. This is because after being compressed to a certain extent, protrusion 422 reaches its deformation limit and no longer changes significantly. In other words, when the compression of the protrusion structure is within a certain range (i.e., the pressure-sensitive range), the contact area changes relatively significantly, thereby effectively detecting the pressure applied. However, beyond this range, the contact area does not change significantly or does not change, and thus the pressure cannot be effectively detected or the sensitivity deteriorates. In this embodiment, by providing two protrusion structures of different heights, the pressure sensitive range of each protrusion structure is differentiated, which enables the pressure sensor to be applicable to detection environments under various pressures, thereby effectively obtaining the range and sensitivity of the pressure sensor. For example, from state (b) to state (c) in Figure 2, the contact area between the protrusion 4223 and the second electrode 402 does not increase significantly, but at this time, the protrusion 4222 begins to contact the electrode, forming a new conductive network, that is, a new resistor is incorporated, and the resistance change is further realized more sensitively, thereby improving the range and sensitivity.
[0080] In some embodiments of the present application, at least some of the relatively low-height protrusions 422 are spaced apart from the electrode layer 40 along the height direction of the protrusions 422 and contact the electrode layer 40 after the pressure applied exceeds a predetermined threshold. Simultaneously, at least some of the highest-height protrusions 422 are configured to maintain contact with the electrode layer 40. This arrangement effectively slows down the sharp drop in resistance, thereby improving the sensor's range. The highest-height protrusions can be used to provide support for the sensitive layer, effectively reducing the adverse effects of sensitive layer collapse. Specifically, if the sensitive layer collapses, this can cause abnormal contact between the protrusions and the electrode layer, leading to changes in the contact area of the protrusions that are inconsistent with design expectations, affecting measurement accuracy. Furthermore, after the relatively high-height protrusions are compressed to a certain extent, the relatively low-height protrusions can be brought into contact with the electrode layer. This effectively staggers the pressure-sensitive range of the relatively high-height protrusions from that of the relatively low-height protrusions, further increasing the range and sensitivity.
[0081] In some embodiments of the present application, the protrusions of the raised structure 422 are shaped like a large base and a small top. For example, they can be tapered from the bottom to the top in a cone or frustum shape, or they can be spherical segments with arc-shaped variations. This arrangement allows the contact area of the raised structure with the electrode layer to gradually change when compressed by pressure, effectively increasing the sensitivity of the raised structure's contact area to pressure. When the higher-level microstructure reaches its compression limit under pressure, the lower-level microstructure adds a contact electrode. By dividing the pressure through the microstructure, the sensitivity of the sensor over a wide range can be significantly improved, enabling better discrimination of pressure changes.
[0082] Please refer to Figures 3a and 3b. Figure 3a is a design diagram of the arrangement of the protrusion structure of the sensitive layer of the pressure sensor according to one or more embodiments of the present application. Figure 3b is a schematic diagram of the arrangement of the protrusion structure of the sensitive layer on the pressure sensor sample according to one or more embodiments of the present application. In some embodiments of the present application, the protrusions of the protrusion structure 422 of the same height are arranged at intervals on a circular reference line centered on a preset reference point. The arrangement can be equidistant or non-equidistant. As shown in Figure 3a, there are three types of protrusion structures 422 of different heights, wherein protrusion 4221 is a protrusion of the protrusion structure of the first height, protrusion 4222 is a protrusion of the protrusion structure of the second height, and protrusion 4223 is a protrusion of the protrusion structure of the third height. The height of protrusion 4223 is greater than the height of protrusion 4221, and the height of protrusion 4221 is greater than the height of protrusion 4222. Multiple protrusions 4221 are spaced apart on annular reference line 1 centered on a preset reference point A; multiple protrusions 4222 are spaced apart on annular reference line 2 centered on a preset reference point A; and multiple protrusions 4223 are spaced apart on annular reference line 3 centered on a preset reference point A. By arranging the protrusions of the same height on the annular reference line, the design process can use the annular reference line as a unit for design considerations, reducing the complexity of the arrangement of the protrusion structures.
[0083] As shown in Figure 3a, multiple protrusions 4221 are spaced apart on annular reference line 1 centered on a predetermined reference point A; multiple protrusions 4222 are spaced apart on annular reference line 2 centered on a predetermined reference point A; and multiple protrusions 4223 are spaced apart on annular reference line 3 centered on a predetermined reference point A. By arranging protrusions of the same height along the annular reference line, the design process can be based on the annular reference line as a unit, reducing the complexity of the arrangement of the protrusions.
[0084] In some embodiments of the present application, a method for preparing a pressure-sensitive layer is also provided, specifically including: providing a flexible substrate slurry; adding conductive particles to the flexible substrate slurry, the conductive particles including a temperature-rising material and a temperature-lowering material, the ratio of the temperature-lowering material to the temperature-rising material being set such that in a temperature range of -40°C to +200°C, the absolute value of the rate of change of the resistivity of the conductive material is less than or equal to 0.01; and curing the flexible substrate slurry to form a pressure-sensitive layer.
[0085] Among them, a mold can be used for reverse molding to form a sensitive layer. The mold used for reverse molding of the sensitive layer can be composed of an acrylic plate outer layer and a PDMS (polydimethylsiloxane) inner layer. PDMS is the main body of the mold, and the acrylic outer frame is used to support PDMS. The PDMS solution is mixed with a curing agent, and the mass ratio of PDMS solution to curing agent is 10:1. The mixture is placed in a vacuum box for 30 minutes to remove all bubbles and then heated at 80°C for 1 hour to fully cross-link and cure. After molding, an infrared / ultraviolet laser is used to perform microstructure processing and groove processing on the PDMS mold. Specifically, an infrared laser can be used to process corresponding pits on the PDMS surface according to the designed structural pattern. The depth and diameter of the microstructure can be adjusted by changing the processing power, number of dot counts and processing frequency of the laser. The sensitive layer solution is scraped into the processed groove to achieve reverse molding preparation.
[0086] Please refer to Figure 4, which is a schematic diagram of the planar structure of a pressure sensor according to one or more embodiments of the present application. The pressure sensor 400 also includes a corrosion-resistant protective layer 44, which is used to resist corrosion from the main electrolyte inside the lithium battery; a sensitive layer 42 for sensing external forces, and the sensitive layer 42 includes a base layer 420 and at least two protruding structures 422 protruding from the base layer 420 at different heights; the electrode layer 40 and the sensitive layer 42 are encapsulated by a sensitive layer adhesive 48, and the two together constitute a key circuit that responds to pressure; the electrode layer 40 includes an electrode base 403, and a first electrode 401 and a second electrode 402 arranged in an interdigitated manner. The electrode base 403 is used to support the membrane structure such as the sensitive layer 42. An insulating layer 46 is located between the sensitive layer 42 and the corrosion-resistant protective layer 44 to protect the sensitive layer 42 from being affected or damaged during the processing and manufacturing of the corrosion-resistant protective layer 44. The insulating layer 46 is connected to the electrode base 403 via an insulating layer adhesive 49. The pressure sensor 400 is a piezoresistive sensor based on the change of contact resistance between the microstructure of the sensitive layer and the coplanar interdigitated electrodes.
[0087] In the above embodiments, the sensing function relies primarily on the change in contact resistance between the conductive sensitive layer and the electrode as pressure changes. Fabricating specific microstructures on the sensitive layer that contact the electrode, such as pyramidal or dome-shaped structures, can alter the contact characteristics between the sensitive layer and the electrode, thereby improving or regulating the sensor's piezoresistive properties. The introduction of specifically shaped microstructures can, to a certain extent, enhance the pressure sensor's performance, including sensitivity and range.
[0088] In some embodiments of the present application, a pressure sensor can be used to detect the internal pressure of a battery. That is, the present application provides a battery cell, which includes a housing and a pressure sensor according to any of the above embodiments, wherein the pressure sensor is disposed inside the housing.
[0089] The embodiments of the present application are applicable to batteries of various systems, including but not limited to lithium batteries, sodium batteries, etc. The shape of the battery includes but is not limited to cylindrical, square or other arbitrary shapes.
[0090] In some embodiments, the battery 100 of the present application includes a housing 10 and a battery cell 20, with the battery cell 20 housed within the housing 10. See FIG5 , which is a schematic diagram of the exploded structure of a battery according to one or more embodiments. The housing 10 is used to accommodate the battery cell 20 and can have various structures. In some embodiments, the housing 10 can include a first portion 11 and a second portion 12, which overlap each other and together define a space for accommodating the battery cell 20. The second portion 12 can be a hollow structure with one end open. The first portion 11 can be a plate-like structure, with the first portion 11 overlapping the open side of the second portion 12, so that the first and second portions 11 and 12 together define a space. Alternatively, the first and second portions 11 and 12 can each be a hollow structure with one end open, with the open side of the first portion 11 overlapping the open side of the second portion 12. Of course, the housing 10 formed by the first and second portions 11 and 12 can have various shapes, such as a cylinder or a rectangular parallelepiped.
[0091] In the battery 100, there may be multiple battery cells 20, and the multiple battery cells 20 may be connected in series, in parallel, or in a hybrid connection. A hybrid connection refers to a combination of series and parallel connections among the multiple battery cells 20. The multiple battery cells 20 may be directly connected in series, in parallel, or in a hybrid connection, and then the entire battery cell 20 may be housed within the housing 10. Alternatively, the battery 100 may be constructed by first connecting multiple battery cells 20 in series, in parallel, or in a hybrid connection to form a battery module, which is then connected in series, in parallel, or in a hybrid connection to form a complete battery module, and then housed within the housing 10. The battery 100 may also include other structures, such as a busbar assembly for electrically connecting the multiple battery cells 20.
[0092] Each battery cell 20 may be a secondary battery, such as a lithium-ion battery, a sodium-ion battery, a magnesium-ion battery, or an aluminum-ion battery, but is not limited thereto. The battery cell 20 may be cylindrical, flat, rectangular, or have other shapes.
[0093] Battery manufacturing methods include laminated and wound types. Laminated batteries offer uniform current collection, low internal resistance, and high specific power, but they require extremely high mold precision, high equipment investment, and a complex process, resulting in low production efficiency. Wound batteries are simple to manufacture, with moderate equipment precision requirements during the production and assembly processes. They offer high production efficiency and low costs. In terms of performance, wound batteries offer excellent high and low temperature performance, extremely fast charging, an extremely long lifespan, stable high output voltage, a sturdy structure, and strong shock resistance.
[0094] Please refer to Figure 6, which is a schematic diagram of the exploded structure of a battery cell 20 in one or more embodiments. A battery cell 20 is the basic unit within a battery that converts chemical energy into electrical energy. The battery cell 20 includes an end cap 21, a housing 22, an electrode assembly 23, and other functional components.
[0095] The end cap 21 refers to a component that covers the opening of the shell 22 to isolate the internal environment of the battery cell 20 from the external environment. Without limitation, the shape of the end cap 21 can be adapted to the shape of the shell 22 to match the shell 22. Optionally, the end cap 21 can be made of a material with a certain hardness and strength (such as aluminum alloy). In this way, the end cap 21 is not easily deformed when squeezed or collided, so that the battery cell 20 can have a higher structural strength and improved safety performance. Functional components such as electrode terminals 21a can be provided on the end cap 21. The electrode terminal 21a can be used to electrically connect to the electrode assembly 23 for outputting or inputting electrical energy of the battery cell 20. In some embodiments, the end cap 21 can also be provided with a pressure relief mechanism for releasing internal pressure when the internal pressure or temperature of the battery cell 20 reaches a threshold. The material of the end cap 21 can also be various, including but not limited to copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc. In some embodiments, an insulating member may be provided inside the end cap 21 to isolate the electrical connection components in the housing 22 from the end cap 21 to reduce the risk of short circuit. For example, the insulating member may be made of plastic, rubber, or the like.
[0096] The housing 22 is a component that cooperates with the end cap 21 to form the internal environment of the battery cell 20, wherein the formed internal environment can be used to accommodate the electrode assembly 23, electrolyte, and other components. The housing 22 and the end cap 21 can be independent components. An opening can be provided in the housing 22, and the end cap 21 is closed at the opening to form the internal environment of the battery cell 20. The end cap 21 and the housing 22 can also be integrated. Specifically, the end cap 21 and the housing 22 can form a common connection surface before other components are inserted into the housing. When the interior of the housing 22 needs to be encapsulated, the end cap 21 is closed to the housing 22. The housing 22 can be of various shapes and sizes, such as a rectangular parallelepiped, a cylindrical shape, a hexagonal prism, etc. Specifically, the shape of the housing 22 can be determined according to the specific shape and size of the electrode assembly 23. The housing 22 can be made of various materials, including but not limited to copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc.
[0097] The electrode assembly 23 is a component in the battery cell 20 where electrochemical reactions occur. One or more electrode assemblies 23 may be contained in the housing 22. The electrode assembly 23 is mainly formed by winding or stacking cathode sheets and anode sheets, and a separator is usually provided between the cathode sheets and the anode sheets. The parts of the cathode sheets and the anode sheets with active materials constitute the main body of the electrode assembly, and the parts of the cathode sheets and the anode sheets without active materials each constitute a tab 23a. The cathode tab and the anode tab may be located together at one end of the main body or respectively at both ends of the main body. During the charge and discharge process of the battery, the cathode active material and the anode active material react with the electrolyte, and the tab 23a connects the electrode terminals to form a current loop.
[0098] The cathode electrode generally includes a cathode current collector and a cathode film layer arranged on the cathode current collector.
[0099] The cathode current collector generally adopts a conventional metal foil or a composite current collector (a metal material can be disposed on a polymer substrate to form a composite current collector). As an example, the cathode current collector can adopt aluminum foil.
[0100] The cathode film layer includes cathode active materials as well as a binder, a conductive agent and other optional additives.
[0101] As an example, the cathode active material may include one or more of lithium transition metal oxides, lithium phosphates with an olivine structure and their respective modified compounds, transition metal oxides, polyanionic compounds, and Prussian blue analogs. Examples of lithium transition metal oxides may include one or more of lithium cobalt oxide, lithium nickel oxide, lithium manganese oxide, lithium nickel cobalt oxide, lithium manganese cobalt oxide, lithium nickel manganese oxide, lithium nickel cobalt manganese oxide, lithium nickel cobalt aluminum oxide, and their modified compounds. Examples of lithium phosphates with an olivine structure may include one or more of lithium iron phosphate, a composite material of lithium iron phosphate and carbon, lithium manganese phosphate, a composite material of lithium manganese phosphate and carbon, lithium manganese iron phosphate, a composite material of lithium manganese iron phosphate and carbon, and their modified compounds. The modified compounds of the above materials may be doping modification and / or surface coating modification of the materials. These materials can all be obtained through commercial channels.
[0102] As an example, the conductive agent may be one or more of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, Super P (SP), graphite, and carbon nanofibers.
[0103] As an example, the binder can be one or more of styrene-butadiene rubber (SBR), water-based acrylic resin, polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), ethylene-vinyl acetate copolymer (EVA), polyacrylic acid (PAA), carboxymethyl cellulose (CMC), polyvinyl alcohol (PVA) and polyvinyl butyral (PVB).
[0104] As an example, other optional auxiliary agents may be thickening and dispersing agents (such as sodium carboxymethyl cellulose CMC-Na), and PTC thermistor materials.
[0105] The anode plate generally includes an anode current collector and an anode film layer disposed on the anode current collector.
[0106] The anode current collector may be a conventional metal foil or a composite current collector (for example, a metal material may be disposed on a polymer substrate to form a composite current collector). As an example, the anode current collector may be a copper foil.
[0107] The anode film layer includes an anode active material, a binder, a conductive agent and other optional additives.
[0108] The anode active material may include one or more of silicon-based materials, silicon-carbon materials, carbon materials, and selenium-based materials. Specifically, it includes one or more of artificial graphite, natural graphite, hard carbon, soft carbon, silicon-based materials and selenium-based materials. Silicon-based materials can be selected from one or more of elemental silicon, silicon oxide compounds (such as silicon monoxide), silicon-carbon composites, silicon-nitrogen composites, and silicon alloys. Selenium-based materials can be selected from one or more of elemental selenium, selenium oxide compounds, and selenium alloys. These materials can all be obtained through commercial channels. In some embodiments of the present application, the design concept of active density is also applicable to sodium batteries, or in other words, the type of battery is not limited. The present application does not limit the selection and matching of electrode materials. Different combinations of anode and cathode materials may have different active density control standards.
[0109] As an example, the conductive agent may be one or more of superconducting carbon, acetylene black, carbon black, Ketjen black, carbon dots, carbon nanotubes, graphite, and carbon nanofibers.
[0110] As an example, the binder may be one or more of styrene-butadiene rubber (SBR), water-based acrylic resin, polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), ethylene-vinyl acetate copolymer (EVA), polyvinyl alcohol (PVA) and polyvinyl butyral (PVB).
[0111] As an example, other optional auxiliary agents may be thickening and dispersing agents (such as sodium carboxymethyl cellulose CMC-Na), and PTC thermistor materials.
[0112] In one embodiment, the cathode active material, the anode active material, the binder, and the conductive agent are mixed in proportion to obtain cathode slurry and anode slurry, and then the cathode slurry and anode slurry are coated on the corresponding current collectors respectively, and dried after coating to obtain cathode and anode pole pieces.
[0113] Furthermore, the battery cell also includes a separator and an electrolyte.
[0114] The separator is placed between the cathode and anode electrodes. As an insulating layer, it effectively prevents contact between the cathode and anode electrodes, which could cause an internal short circuit, while allowing electrolyte ions to pass smoothly. The performance of the separator determines the battery's interface structure and internal resistance, directly affecting the battery's mechanical strength and safety.
[0115] The specific type of separator material is not limited. Any material known in the art for battery separators can be used, and those skilled in the art can select the material based on their needs. For example, the separator material can include one or more of polyolefins, fluoropolymers, cellulose, and fiberglass. Polyolefins can include, but are not limited to, one or more of polypropylene and polyethylene. All of these materials are commercially available.
[0116] In some embodiments, the isolation membrane includes a base membrane and a coating located on one side / both sides of the base membrane, and the coating includes a filler. The filler may include an inorganic material, a polymer adhesive, and a dispersant. The inorganic material includes one or more of boehmite and silica, and the polymer adhesive material includes one or more of PVDF (polyvinylidene fluoride) and polystyrene-acrylate; the dispersant material includes polyvinyl alcohol, etc. By providing a coating on one side / both sides of the isolation membrane, the performance of the isolation membrane can be improved and regulated. The performance of the isolation membrane can be regulated by regulating the type of filler. For example, a filler with heat insulation and heat resistance can be added to improve the heat resistance of the isolation membrane. The specific type of the base membrane material is not limited, and can include one or more of polyethylene, polypropylene and glass fiber. These materials can be obtained through commercial channels.
[0117] The electrolyte plays the role of conducting ions between the cathode electrode and the anode electrode, and may include electrolyte salts and solvents.
[0118] As an example, the electrolyte salt can be selected from one or more of lithium hexafluorophosphate (LiPF6), lithium tetrafluoroborate (LiBF4), lithium perchlorate (LiClO4), lithium hexafluoroarsenate (LiAsF6), lithium bis(fluorosulfonyl)imide (LiFSI), lithium bis(trifluoromethanesulfonyl)imide (LiTFSI), lithium trifluoromethanesulfonate (LiTFS), lithium difluorooxalatoborate (LiDFOB), lithium dioxalatoborate (LiBOB), lithium difluorophosphate (LiPO2F2), lithium difluorobis(oxalatophosphate) (LiDFOP) and lithium tetrafluorooxalatophosphate (LiTFOP).
[0119] As an example, the solvent may be selected from ethylene carbonate (EC), propylene carbonate (PC), methyl ethyl carbonate (EMC), diethyl carbonate (DEC), dimethyl darbonate (DMC), dipropyl carbonate (DPC), methyl propyl carbonate (MPC), ethyl propyl carbonate (EPC), butylene carbonate (BC), fluoroethylene carbonate (FEC), methyl formate (MF), methyl acetate (MA), ethyl acetate (EA), n-propyl acetate (PA), methyl propionate (MP), ethyl propionate (EP), n-propyl propionate (NP), propylene glycol (PEG), propylene glycol (PP), propylene glycol (C1), propylene glycol (C2), propylene glycol (C3), propylene glycol (C4), propylene glycol (C5), propylene glycol (C6), propylene glycol (C7), propylene glycol (C8), propylene glycol (C9), propylene glycol (D1), propylene glycol (D2), propylene glycol (D3), propylene glycol (D4), propylene glycol (D5), propylene glycol (D6), propylene glycol (D7), propylene glycol (D8), propylene glycol (D9), propylene glycol (D10), propylene glycol (D11), propylene glycol (D12), propylene glycol (D13), propylene glycol (D14), propylene glycol (D15), propylene glycol (D16), propylene glycol (D17), propylene glycol (D18), propylene glycol (D19), propylene glycol (D20), propylene glycol (D21), propylene glycol (D22), propylene glycol (D23), propylene glycol (D24), propylene glycol (D25), propylene glycol (D26), propylene glycol (D27), propylene glycol (D28), propylene glycol (D29), propylene glycol (D31), propylene glycol (D32), propylene glycol (D33), propylene glycol (D34), propylene glycol (D35), propylene glycol (D36), propylene glycol (D37), propylene glycol (D38), propylene glycol (D39), propylene One or more of the group consisting of propionate (PP), methyl butyrate (Methyl Butyrate MB), ethyl butyrate (Ethyl Butyrate, EB), 1,4-butyrolactone (1,4-Butyrolactone, GBL), tetramethylene sulfone (SF), dimethyl sulfone (Methyl Sulfone, MSM), methyl ethyl sulfone (Methyl Ethyl Sulfone, EMS) and diethyl sulfone (Diethyl Sulfone, ESE).
[0120] In some embodiments, the electrolyte further includes additives. For example, the additives may include anode film-forming additives, cathode film-forming additives, or additives capable of improving certain battery properties, such as additives that improve battery overcharge performance, additives that improve battery high-temperature performance, and additives that improve battery low-temperature performance.
[0121] The battery disclosed in the embodiments of the present application can be used in electrical devices that use the battery as a power source or various energy storage systems that use the battery as an energy storage element. The electrical devices may be, but are not limited to, mobile phones, tablets, laptops, electric toys, power tools, battery cars, electric cars, ships, spacecraft, and the like. Among them, electric toys may include fixed or mobile electric toys, such as game consoles, electric car toys, electric ship toys, and electric airplane toys, and the like, and spacecraft may include airplanes, rockets, space shuttles, and spacecraft, and the like.
[0122] The energy storage system can be a hydropower, thermal, wind power, solar power station or other energy storage power supply system.
[0123] For the convenience of description, the following embodiments are described by taking a vehicle 1000 as an example of an electrical device according to an embodiment of the present application.
[0124] Please refer to Figure 7, which is a schematic structural diagram of a vehicle 1000 in some embodiments of the present application. The vehicle 1000 can be a fuel vehicle, a gas vehicle or a new energy vehicle. The new energy vehicle can be a pure electric vehicle, a hybrid vehicle or an extended-range vehicle, etc. A battery 100 is provided inside the vehicle 1000, and the battery 100 can be provided at the bottom, head or tail of the vehicle 1000. The battery 100 can be used to power the vehicle 1000. For example, the battery 100 can serve as an operating power source for the vehicle 1000. The vehicle 1000 may also include a controller 200 and a motor 300. The controller 200 is used to control the battery 100 to power the motor 300, for example, for starting, navigating and driving the vehicle 1000.
[0125] In some embodiments of the present application, the battery 100 can serve not only as an operating power source for the vehicle 1000, but also as a driving power source for the vehicle 1000, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle 1000.
[0126] The above-mentioned electrical equipment and energy storage systems are also within the protection scope of this application.
[0127] The beneficial effects of the present application are further illustrated below with reference to the examples.
[0128] In order to make the technical problems, technical solutions and beneficial effects solved by the embodiments of the present application clearer, the following will be further described in detail with reference to the embodiments and the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present application, rather than all of the embodiments. The following description of at least one exemplary embodiment is actually merely illustrative and does not serve as any limitation to the present application and its applications. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0129] 1. Preparation of Sensitive Layer
[0130] A certain amount of temperature-lowering material (e.g., multi-walled carbon nanotube (MWCNT) powder) and temperature-raising material (e.g., graphite flake (GPs) powder) were weighed in a certain mass ratio and placed in a reagent bottle. A certain amount of acetone solution was added as a dispersion medium. The mixture was ultrasonically cleaned at 30°C for 3 hours to disperse the agglomerated conductive material (e.g., MWCNT). The mixture was then added to a 20wt% flexible substrate solution (e.g., TPU / DMAc (dimethylacetamide) solution) and stirred at 50°C for 12 hours using a magnetic stirrer. The reagent bottle was opened to allow the acetone in the solution to evaporate, thereby increasing the viscosity of the precursor solution and facilitating the subsequent doctor blade coating process. The material composition and ratio of each example are detailed in Table 1.
[0131] An infrared laser was used to create corresponding pits on the surface of the PDMS mold according to the designed microstructure pattern. The resulting microstructure data is detailed in Table 2.
[0132] The processed PDMS mold was ultrasonically cleaned in anhydrous ethanol for 30 minutes. The mold was preheated to 30°C on a heating plate to reduce bubbles during the doctor blade coating process. A certain volume of precursor solution was then measured and applied to the mold surface using a pipette. The solution was then smoothed with a glass rod and placed on a 50°C hotplate for 1 hour. The solution was then fully evaporated at 120°C to allow the DMAc and acetone solvents to evaporate.
[0133] The cured sensitive layer film was then peeled from the PDMS mold, cut, and placed in an 80°C oven for hot pressing to ensure flatness. Figure 3b shows an optical microscopy image of the microstructured sensitive layer film. The microstructures are well-molded, and the first, second, and third-level microstructures are clearly distinguishable.
[0134] 2. Performance Testing
[0135] Resistance test
[0136] The prepared pressure sensor was placed in a high and low temperature box, connected to the matching resistance meter equipment, applied a 1000N weight, recorded the initial resistance R0, changed the external temperature, continued to apply a 1000N weight and recorded the resistance R, the resistance change rate = (R-R0) / R0.
[0137] Table 1: Sensitive layer battery parameters of various examples and comparative examples Note: The mass ratio is the mass ratio of the temperature-rising material to the temperature-dropping material.
[0138] Table 2: Data parameters of the protruding structure of the sensitive layer of each embodiment and comparative example
[0139] Combined with the data in Table 1 and Figure 8, Figure 8 is a schematic diagram of the resistance change rate and temperature curve of the embodiment and the comparative example. The present application scheme mixes the temperature-rising material and the temperature-dropping material, and uses the reduced resistance of the temperature-dropping material to balance the increased resistance of the temperature-rising material, or uses the increased resistance of the temperature-dropping material to balance the reduced resistance of the temperature-dropping material, so that the resistance of the mixed material does not change significantly when the temperature changes, that is, the resistivity of the mixed material is basically unaffected by temperature, so as to improve the detection sensitivity of the sensor at different temperatures, reduce the error caused by temperature changes to the detection, expand the operating temperature space of the sensor, and improve the detection sensitivity. At the same time, manufacturing a specific microstructure in contact with the electrode on the sensitive layer can change the contact characteristics between the sensitive layer and the electrode, thereby achieving the improvement or regulation of the piezoresistive characteristics of the sensor. The introduction of microstructures of specific shapes can improve the sensitivity, range and other performance indicators of the pressure sensor to a certain extent.
[0140] The above description is only an implementation method of the present application and does not limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the description and drawings of this application, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. A conductive material for a pressure sensitive layer, wherein: The conductive material includes a flexible substrate and conductive particles dispersed in the flexible substrate, the conductive particles include a temperature rising material and a temperature dropping material, the temperature rising material is a material whose resistivity increases as the temperature rises, and the temperature dropping material is a material whose resistivity decreases as the temperature rises, and the ratio of the temperature dropping material to the temperature rising material is set so that within the temperature range of -40°C to +200°C, the absolute value of the rate of change of the resistivity of the conductive material is less than or equal to 0.
01.
2. The conductive material according to claim 1, wherein The ratio of the temperature-dropping material to the temperature-raising material is set so that within a temperature range of +25°C to +80°C, the absolute value of the rate of change of the resistivity of the conductive material is less than or equal to 0.
008.
3. The conductive material according to claim 1 or 2, wherein: The ratio of the temperature-dropping material to the temperature-raising material is set so that within a temperature range of -40°C to +200°C, the absolute value of the rate of change of the resistance of the conductive material is less than or equal to 0.
01.
4. The conductive material according to claim 3, wherein The ratio of the temperature-dropping material to the temperature-raising material is set so that within a temperature range of +25°C to +80°C, the absolute value of the rate of change of the resistance of the conductive material is less than or equal to 0.
008.
5. The conductive material according to any one of claims 1 to 4, wherein: In the temperature range of -40°C to +200°C, the ratio of the absolute value of the resistance temperature coefficient of the temperature rise material to the resistance temperature coefficient of the temperature drop material is 30:1-1:30; The temperature coefficient of resistance is the relative change in the resistance value of a material when the temperature changes by 1 degree Celsius.
6. The conductive material according to any one of claims 1 to 5, wherein: In the temperature range of -40°C to +200°C, the absolute value of the ratio of the change rate of the resistivity of the temperature-rising material to the change rate of the resistivity of the temperature-dropping material is 25:1-1:
25.
7. The conductive material according to any one of claims 1 to 6, wherein: The mass ratio of the temperature-raising material to the temperature-lowering material is 15:1-1:
20.
8. The conductive material according to any one of claims 1 to 7, wherein: The electrical conductivity of the temperature-rising material is greater than 1S·m -1 ; and / or The electrical conductivity of the temperature drop material is greater than 1S·m -1 ; and / or The electrical conductivity of the conductive material is greater than 1 S·m -1 .
9. The conductive material according to any one of claims 1 to 8, wherein: The temperature-rising material includes one or more of graphite, gold powder, silver powder, nickel powder, zinc-chromium alloy, nickel-copper alloy and the like.
10. The conductive material according to any one of claims 1 to 9, wherein: The temperature-reducing material includes one or more of carbon nanotubes, chromium black, graphene, carbon black, and ceramic materials with metal oxides of manganese, cobalt, nickel and copper as main materials.
11. The conductive material according to any one of claims 1 to 10, wherein: The conductive particles include graphite particles and carbon nanotube particles, and the mass ratio of the graphite particles to the carbon nanotube particles is 1:1-1:20, and can be 1:9-1:
15.
12. The conductive material according to claim 11, wherein The carbon nanotube particles include multi-walled carbon nanotube particles, wherein the outer diameter of the multi-walled carbon nanotube particles is 6-13 nm and the length is 2.5-20 μm; and / or The particle size Dv50 of the graphite particles is 7-10 μm.
13. The conductive material according to any one of claims 1 to 12, wherein: The mass ratio of the flexible substrate to the conductive particles is 15:1-5:1, and can be optionally 12:1-8:
1.
14. The conductive material according to claim 13, wherein The flexible substrate includes one or more of thermoplastic polyurethane, polyvinyl alcohol, chloroprene rubber, nitrile rubber, styrene-butadiene block copolymer, and polyacrylic acid, and may be aliphatic thermoplastic polyurethane.
15. A pressure sensor, wherein: The pressure sensor comprises: Electrode layer; A sensitive layer, wherein the sensitive layer is made of the conductive material as described in any one of claims 1 to 14.
16. The pressure sensor according to claim 15, wherein: The sensitive layer includes a base layer and at least two protrusion structures protruding from the base layer at different heights, each of the protrusion structures includes at least one protrusion, each of the protrusions is located on a side of the base layer facing the electrode layer, and the contact area between each protrusion and the electrode layer is configured to change with the change of the pressure applied to the electrode layer.
17. A method for preparing a pressure sensitive layer, wherein: The method comprises: Providing a flexible substrate slurry; Adding conductive particles to the flexible substrate slurry, the conductive particles comprising a temperature rising material and a temperature falling material, the temperature rising material being a material whose resistivity increases as the temperature rises, the temperature falling material being a material whose resistivity decreases as the temperature rises, the ratio of the temperature falling material to the temperature rising material being set within a temperature range of -40°C to +200°C, and the absolute value of the rate of change of the resistivity of the conductive material being less than or equal to 0.01; The flexible substrate slurry is cured to form the pressure sensitive layer.
18. A battery cell, wherein: The battery cell comprises a housing and the pressure sensor according to claim 15 or 16, wherein the pressure sensor is disposed inside the housing.
19. An electrical device, wherein: Comprising the battery cell as claimed in claim 18.
Citation Information
Patent Citations
Strain sensor with temperature compensation function and composite material of strain sensor
CN108627080A
Pressure sensor and preparation method thereof
CN110118624A
Resistance-type flexible pressure sensor and preparation method thereof
CN111060238A
Preparation method of flexible conductive composite material insensitive to strain and temperature
CN113205900A
Flexible pressure sensor and preparation method thereof, and wearable device
CN114323369A
Cited By
Flexible pressure sensor with staggered skeleton structure and preparation method thereof
CN119688125A
Test method for pressure instrument temperature influence test
CN119827043A