Optoelectronic semiconductor component and method for producing an optoelectronic semiconductor component
The semiconductor layer sequence with a three-dimensional buffer layer and recessed areas addresses inefficiencies in charge carrier injection and distribution, resulting in improved optoelectronic semiconductor component efficiency and quality by reducing threading dislocations and enhancing charge carrier homogeneity.
Patent Information
- Application Number
- PCT/EP2024/063422
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-24
- Filing Date
- 2024-05-15
- Publication Date
- 2024-11-28
AI Technical Summary
Current optoelectronic semiconductor components face inefficiencies due to high point defect density, surface roughness, and threading dislocations, which lead to reduced quality and efficiency, particularly in charge carrier injection and distribution.
A semiconductor layer sequence with a three-dimensional buffer layer and strategically arranged recessed areas allows for lateral charge carrier injection, reducing threading dislocations and enhancing the homogeneity of charge carrier distribution, thereby improving efficiency.
The solution results in a more efficient optoelectronic semiconductor component with improved charge carrier distribution and reduced leakage currents, leading to enhanced internal quantum efficiency and component quality.
Smart Images

Figure EP2024063422_28112024_PF_FP_ABST
Abstract
Description
[0001] Description
[0002] OPTOELECTRONIC SEMICONDUCTOR COMPONENT AND METHOD FOR PRODUCING AN OPTOELECTRONIC SEMICONDUCTOR COMPONENT
[0003] An optoelectronic semiconductor component and a method for producing an optoelectronic semiconductor component are specified. For example, the optoelectronic semiconductor component is a nitride-based semiconductor component. The optoelectronic semiconductor component can be designed to generate or emit electromagnetic radiation.
[0004] To improve the current injection into an active zone of an optoelectronic semiconductor component or to increase the efficiency, it is possible, for example, to form V-defects (V-pits) in a semiconductor layer sequence of the optoelectronic semiconductor component by setting suitable growth parameters or creating suitable buffer and opening layers and to inject charge carriers laterally into the active zone via the V-defects. However, the creation of the
[0005] Opening layer, which leads to an opening of the V-defects, causes an increased point defect density associated with increased absorption and a rougher surface associated with a reduction in the quality of semiconductor layers deposited thereon. In addition, threading dislocations, which are one-dimensional crystal defects and promote the opening of the V-defects, can continue through the V-defects to a surface of the semiconductor layer sequence and form leakage paths and / or non-radiative recombination centers. In addition, the creation of threading dislocations requires a buffer layer with an optimized threading dislocation density and a minimum thickness. Finally, the threading dislocations and therefore also the V-defects are locally stochastically distributed, which can lead to the distance between V-defects not adequately matching the drift and diffusion length of the charge carriers.
[0006] One problem to be solved in the present case is, among other things, to provide a more efficient optoelectronic semiconductor component. Another problem to be solved in the present case is, among other things, to provide a method for producing an optoelectronic semiconductor component with higher efficiency.
[0007] These objects are achieved, inter alia, by an optoelectronic semiconductor component and a method for producing an optoelectronic semiconductor component having the features of the independent claims.
[0008] Further advantages and embodiments of an optoelectronic semiconductor component and of a method for producing an optoelectronic semiconductor component are the subject of the dependent claims.
[0009] According to at least one embodiment of an optoelectronic semiconductor component, the component comprises a semiconductor layer sequence. The semiconductor layer sequence can comprise a buffer layer with a three-dimensional structure having coalesced regions, wherein the coalesced regions have depressions with a cross-sectional size that decreases with increasing depth. The cross-sectional size of the depressions can continuously decrease with increasing depth. The buffer layer is provided, for example, to reduce strains that can occur when the semiconductor layer sequence is grown on a growth substrate if the lattice constants of the materials used for the semiconductor layer sequence and the growth substrate differ.
[0010] In this case, a three-dimensional structure is understood to mean, for example, a non-planar structure with inclined surfaces.
[0011] Furthermore, the coalesced regions can be grown together regions which, for example, arise during three-dimensional epitaxial growth of the buffer layer through the growing together of originally separate regions by means of lateral overgrowth, as is described in more detail below in connection with the method. In particular, the coalesced regions are in each case not completely, i.e. only partially, coalesced regions, i.e. regions which arise during three-dimensional growth through partial coalescence. The depressions are advantageously the result of partial coalescence. In particular, the depressions are therefore not V-defects which arose from previously planar semiconductor structures.
[0012] The alternative production of the recesses using partial coalescence offers several advantages over the formation of V-defects. Firstly, the semiconductor layer sequence can be made thinner, since the buffer layer does not need to have an optimized thread dislocation density, and secondly, an opening layer can be omitted. Secondly, the quality of the semiconductor layer sequence and thus the efficiency of the optoelectronic semiconductor component can be improved due to a smaller number of thread dislocations.
[0013] According to at least one embodiment, the semiconductor layer sequence comprises a first semiconductor layer of a first conductivity type, which is arranged on an undoped layer of the buffer layer and has depressed regions in the region of the depressions. For example, the first conductivity type can be n-conductivity. Furthermore, the first semiconductor layer can be a doped layer of the buffer layer. In particular, the depressed regions of the first semiconductor layer are identical to the depressions of the buffer layer. However, it is also possible for the first semiconductor layer to be a layer applied to the buffer layer, which has depressed regions in the region of the depressions, each of which has a different vertical position and is produced, for example, by conformal application to the buffer layer, but not by coalescence.In both cases, the first semiconductor layer can follow the three-dimensional structure of the buffer layer. The first semiconductor layer can have a predominantly uniform thickness.
[0014] The undoped layer is, for example, a layer that is not deliberately doped, but may contain a low concentration of dopants, for example, single-source dopants from the first semiconductor layer. In particular, the first semiconductor layer has a higher doping than the undoped layer. The doping, for example Si doping, of the first semiconductor layer may, for example, be at least 10 18 cur 3 amount to .
[0015] According to at least one embodiment, the semiconductor layer sequence comprises an active zone, which is arranged at least in part on the first semiconductor layer. The active zone is arranged, in particular, in regions located outside the recessed regions or depressions. Furthermore, the active zone can extend into the recessed regions or depressions.
[0016] According to at least one embodiment, the semiconductor layer sequence comprises a second semiconductor layer of a second conductivity type, which is arranged on a side of the active zone facing away from the first semiconductor layer and extends into the recesses and / or recessed regions. For example, the second conductivity type can be a p-type conductivity.
[0017] According to at least one embodiment, during operation, a lateral charge carrier injection into the active zone takes place from the second semiconductor layer arranged in the recesses and / or recessed regions. The lateral charge carrier injection can increase the charge carrier density in more distant regions of the active zone, which are further away from a main surface, for example a second main surface of the optoelectronic semiconductor component, whereby the distribution of the charge carriers, for example the holes, in the active zone is particularly homogeneous and the efficiency of the component is improved.
[0018] According to at least one embodiment, the optoelectronic semiconductor component comprises:
[0019] - a semiconductor layer sequence comprising
[0020] - a buffer layer having a three-dimensional structure with coalesced regions, wherein the coalesced regions have depressions with a cross-sectional size decreasing with increasing depth,
[0021] - a first semiconductor layer of a first
[0022] conductivity type, which is arranged on an undoped layer of the buffer layer and has recessed areas in the region of the depressions,
[0023] - an active zone which is arranged at least in part on the first semiconductor layer, and
[0024] - a second semiconductor layer of a second
[0025] Conductivity type, which is arranged on a side of the active zone facing away from the first semiconductor layer and extends into the depressions and / or recessed regions, wherein during operation a lateral charge carrier injection into the active zone takes place from the second semiconductor layer arranged in the depressions and / or recessed regions, and wherein the coalesced regions are each not completely coalesced regions.
[0026] Using the method described in more detail below, it is possible for the depressions or depressed regions to be spatially distributed in a targeted, controlled manner and thus not follow a stochastic distribution. This enables a homogeneous current density and a homogeneous current injection into the active zone. For example, the depressions can be arranged at equal intervals, at least in some regions. At the edge of the semiconductor layer sequence, the number density of the depressions can be reduced, for example, to avoid leakage currents.
[0027] According to at least one embodiment or configuration, the semiconductor layer sequence is based on nitride compound semiconductors. In the present context, "based on nitride compound semiconductors" means that the semiconductor layer sequence or at least one layer thereof comprises a nitride III / V compound semiconductor material, preferably Al n Ga m Ini-n-m N , where 0 < n < 1 , 0 < m < 1 and n+m < 1 . This material does not necessarily have to have a mathematically exact composition according to the above formula . Rather, it can contain one or more dopants as well as additional components that affect the characteristic physical properties of Al n Ga m Ini- n-m N-material does not change substantially. For the sake of simplicity, however, the above formula only includes the essential components of the crystal lattice (Al, Ga, In, N), even if these may be partially replaced by small amounts of other substances. The undoped layer can be a GaN layer. The first semiconductor layer can be an n-doped GaN layer. Furthermore, the second semiconductor layer can be a p-doped GaN layer.
[0028] According to at least one embodiment or configuration, the depressions have the shape of an inverse pyramid, an inverse truncated pyramid, an inverse cone, or an inverse truncated cone. A base area of the inverse pyramid or of the inverse truncated pyramid can be formed by an n-gon, which has, for example, up to twelve corners. For example, the depressions can have a V-shaped cross-section transverse to a main extension plane of the semiconductor layer sequence. Furthermore, the depressions can have a hexagonal or dodecagonal cross-section parallel to the main extension plane of the semiconductor layer sequence. Furthermore, the depressions can form a honeycomb-shaped structure in a plan view of the buffer layer, which is composed of several polygons, each having, for example, six or twelve corners. The same can apply to the recessed regions.
[0029] According to at least one embodiment or configuration, the depressions are each laterally delimited by inner surfaces of the coalesced regions which run along {10-11} crystal surfaces and / or {11-22} crystal surfaces.
[0030] According to at least one embodiment or configuration, the maximum distance between the recesses is at most as large as the drift and diffusion length of the charge carriers. This advantageously allows the internal quantum efficiency to be increased.
[0031] According to at least one embodiment or configuration, the second semiconductor layer has a varying thickness with thickness maxima in the region of the recesses. This allows lateral charge carrier injection to be increased compared to vertical charge carrier injection. The term "lateral" or "lateral" can, for example, refer to directions running parallel to the main extension plane of the semiconductor layer sequence. The term "vertical" can, for example, refer to directions running transversely, in particular perpendicularly, to the main extension plane of the semiconductor layer sequence.
[0032] According to at least one embodiment or configuration, the semiconductor layer sequence has a planar main surface on a side facing away from the buffer layer. In particular, existing unevennesses in regions of the recesses are compensated for by the second semiconductor layer.
[0033] According to at least one embodiment or configuration, the active zone has a sequence of individual layers by means of which a quantum well structure, for example a single quantum well structure (SQW, single quantum well) or multiple quantum well structure (MQW, multiple quantum well), is formed. The individual layers comprise at least two barrier layers, between which (in each case) a quantum well layer is arranged. The lateral charge carrier injection can increase the charge carrier density in deeper regions or quantum well layers of the active zone that are further away from a main surface, for example the second main surface, whereby the distribution of the charge carriers, for example the holes, in the active zone is particularly homogeneous and the efficiency of the component is improved.For example, the barrier layers can be GaN layers and the at least one quantum well layer can be an InGaN layer.
[0034] According to at least one embodiment or configuration, the optoelectronic semiconductor component is a micro-LED. For example, the optoelectronic semiconductor component is free of a growth substrate. Furthermore, the optoelectronic semiconductor component in this embodiment or configuration can be characterized by particularly small dimensions. A vertical extent of the optoelectronic semiconductor component, which is determined, for example, along the vertical direction, can be in the single-digit to double-digit micrometer range, for example between 1.5 pm and 10 pm. Furthermore, lateral extents of the optoelectronic semiconductor component, which are determined, for example, along the lateral directions, can be in the single-digit to triple-digit micrometer range.For example, a possible range of values for the lateral directions extends up to and including 100 pm, up to and including 70 pm, or up to and including 50 pm. Due to the non-stochastic distribution of the recesses, it is possible to form the micro-LED, which has a comparatively small cross-sectional area, with a sufficient number of recesses.
[0035] For external electrical contacting, the optoelectronic semiconductor component can have a first electrical contact means electrically connected to the first semiconductor layer and a second electrical contact means electrically connected to the second semiconductor layer.
[0036] The method described below is suitable for producing at least one optoelectronic semiconductor component described above. Features described in connection with the semiconductor component can therefore also be used for the method, and vice versa.
[0037] According to at least one embodiment of a method for producing an optoelectronic semiconductor component of the above-mentioned type, this comprises the following steps, for example in the specified order:
[0038] - Providing a growth substrate comprising a growth structure with openings and edge regions, wherein the openings are laterally delimited by the edge regions,
[0039] - producing a semiconductor layer sequence on the growth substrate, wherein the semiconductor layer sequence comprises a buffer layer, a first semiconductor layer of a first conductivity type, an active zone and a second semiconductor layer of a second conductivity type, and the production of the semiconductor layer sequence comprises the following steps:
[0040] - growing a buffer layer on the growth substrate in such a way that the growth begins in the openings and continues beyond the openings to the edge regions, wherein the buffer layer is formed with a three-dimensional structure having coalesced regions, and wherein the coalesced regions have depressions with a cross-sectional size that decreases with increasing depth,
[0041] - producing a first semiconductor layer of a first conductivity type on an undoped layer of the buffer layer such that the first semiconductor layer has recessed regions in the region of the recesses,
[0042] - producing an active zone at least in regions on the first semiconductor layer and - growing a second semiconductor layer of a second conductivity type such that the second semiconductor layer is arranged on a side of the active zone facing away from the first semiconductor layer and extends into the depressions and / or depressed regions, wherein the coalesced regions are each not completely coalesced regions which are produced by partial coalescence of regions which are grown in the openings of the growth structure.
[0043] According to at least one embodiment or configuration, the buffer layer is produced by means of metal-organic vapor phase epitaxy (MOVPE).
[0044] According to at least one embodiment or configuration, the buffer layer is produced by three-dimensional growth. The growth conditions are selected such that the regions created in the openings have a three-dimensional shape at the beginning of growth. As growth progresses, the separated regions can coalesce by lateral overgrowth of the edge regions.
[0045] The coalesced regions and thus also the recesses can be created on the edge regions of the growth structure. For example, the buffer layer is grown using FACELO (facet-assisted epitaxial lateral overgrowth). This method is particularly suitable for producing a low-defect buffer layer.
[0046] According to at least one embodiment or configuration, the provision of the growth substrate comprises a step of providing a substrate body. The openings can be formed in the substrate body by structuring the substrate body or in a mask layer on the
[0047] The substrate body can be produced by structuring the mask layer. The edge regions can be formed by the substrate body itself or the mask layer. For example, the substrate body can be made of a nitride-based material such as GaN or sapphire. Materials such as silicon oxide, for example, SiO2, silicon nitride, magnesium nitride, or molybdenum can be used for the mask layer.
[0048] According to at least one embodiment or configuration, the structuring of the substrate body or the mask layer is carried out using a lithographic process. Using a photomask used for the lithographic process, the positions of the openings and thus the recesses, as well as their spacing from one another, can be precisely controlled. To obtain spacings that are always smaller than the drift and diffusion length of the charge carriers, methods such as nanoimprint lithography or deep UV lithography are particularly suitable.
[0049] For example, the openings are arranged at equal intervals within standard manufacturing tolerances. Furthermore, it is possible that the maximum thickness of the buffer layer, within standard manufacturing tolerances, is at most as large as the distances between the openings. The openings can, for example, be formed with a hexagonal cross-section.
[0050] According to at least one embodiment or configuration, the growth of the buffer layer comprises the growth of the undoped layer and the continuation of the growth with the supply of a dopant, whereby the first semiconductor layer is produced.
[0051] According to at least one embodiment or configuration, the active zone is grown onto the first semiconductor layer. For example, a vertical growth rate may be greater than a lateral growth rate on the inner surfaces of the coalesced regions, so that the active zone has a smaller layer thickness on the inner surfaces than in regions outside the recessed regions or depressions.
[0052] MOVPE is a suitable manufacturing process for the active zone and the second semiconductor layer.
[0053] According to at least one embodiment or configuration, the growth substrate is removed from the semiconductor layer sequence. In this case, the finished optoelectronic semiconductor component is free of a growth substrate.
[0054] According to at least one embodiment or refinement, the method is carried out for a plurality of optoelectronic semiconductor components in a wafer assembly. The targeted, non-stochastic distribution of the recesses advantageously reduces intensity fluctuations within the plurality of optoelectronic semiconductor components.
[0055] The optoelectronic semiconductor component is suitable as an LED or micro-LED for display, projection, and lighting applications. For example, multiple micro-LEDs can form pixels or subpixels of a display and emit light of a defined color. Due to their small dimensions or pixel size and high density with close spacing, micro-LEDs are suitable for small monolithic displays, which are used, for example, in AR applications such as data glasses.
[0056] Further advantages, advantageous embodiments and further developments emerge from the exemplary embodiments described below in conjunction with the figures.
[0057] It shows :
[0058] Figure 1 shows a schematic cross-sectional view of an optoelectronic semiconductor component according to an embodiment or a final stage of a method for producing an optoelectronic semiconductor component according to the embodiment and
[0059] Figure 2 shows a schematic cross-sectional view of an optoelectronic semiconductor component according to a further embodiment or a final stage of a method for producing an optoelectronic semiconductor component according to the further embodiment.
[0060] In the embodiments and figures, identical, similar or similarly acting elements can each be provided with the same reference numerals. The elements shown and their relative sizes to one another are not necessarily to scale; rather, individual elements may be exaggerated for clarity and / or clarity. A first embodiment of an optoelectronic semiconductor component 1 is described in more detail below with reference to figure 1. For example, the optoelectronic semiconductor component 1 is a radiation-emitting semiconductor component. The optoelectronic semiconductor component 1 is provided, for example, to emit electromagnetic radiation having at least one wavelength from the ultraviolet to infrared spectral range during operation.The optoelectronic semiconductor component 1 can be a micro-LED, the nature of which is explained in more detail in connection with Figure 2.
[0061] However, it is also conceivable that the optoelectronic semiconductor component 1 is a radiation-detecting semiconductor component.
[0062] The optoelectronic semiconductor component 1 comprises a growth substrate 20 and a semiconductor layer sequence 10 arranged thereon. The semiconductor layer sequence 10 has a first main surface 10A facing the growth substrate 20 and a second, for example planar, main surface 10B facing away from the growth substrate 20. For example, the optoelectronic semiconductor component 1 can emit radiation at the second main surface 10B during operation. For the semiconductor layer sequence 10, for example, nitride-based compound semiconductors with the material composition Al n Ga m Ini- n-mN comes into question, where 0 < n < 1, 0 < m < 1 and n + m < 1. The growth substrate 20 comprises a substrate body 21 which is suitable for growing, for example epitaxially, the semiconductor layer sequence 10. For example, the substrate body 21 can be formed from a nitride-based material such as GaN or from sapphire. Furthermore, the growth substrate 20 has a growth structure 22 with openings 23 and edge regions 24, the openings 23 being laterally delimited by the edge regions 24. The growth structure 22 can be formed by a mask layer 25 arranged on the substrate body 21. However, it is also possible for the growth structure 22 to be part of the substrate body 21, so that the growth substrate 20 is, for example, a so-called RSS (patterned sapphire substrate). Materials such as silicon oxide, for example SiO2, silicon nitride, magnesium nitride, or molybdenum are suitable for the mask layer 25.
[0063] The semiconductor layer sequence 10 comprises a buffer layer 11 adjacent to the growth substrate 20, wherein a first surface 11A of the buffer layer 11 facing the growth substrate 20 forms the first main surface 10A. The buffer layer 11 can be formed in multiple layers, wherein a layer adjacent to the growth substrate 20 is, for example, an undoped layer 12, for example an undoped GaN layer. The fact that the layer 12 is an undoped layer means in particular that the layer 12 is not deliberately doped, but can contain a low concentration of dopants, for example of diffused dopants from other layers.
[0064] In addition, the semiconductor layer sequence 10 comprises a first
[0065] Semiconductor layer 13 of a first conductivity type, an active zone 14, which in the case of a radiation-emitting semiconductor component generates radiation during operation and in the case of a radiation-detecting semiconductor component absorbs radiation during operation, and a second semiconductor layer 15 of a second conductivity type. The first conductivity type can be an n-type conductivity and the second conductivity type a p-type conductivity. However, it is also possible for the first conductivity type to be a p-type conductivity and the second conductivity type an n-type conductivity. For example, the first semiconductor layer 13 is an n-GaN layer. The first semiconductor layer 13 can be doped with Si. The n-doping can be at least 10 18 cur 3The active zone 14 can have a single quantum well structure or a multiple quantum well structure with a plurality of barrier layers, for example, GaN layers, and an intermediate quantum well layer, for example, an InGaN layer (not shown). Furthermore, the second semiconductor layer 15 can be a p-GaN layer.
[0066] The first semiconductor layer 13, the active zone 14, and the second semiconductor layer 15 follow one another, at least in some regions, in a vertical direction V in the specified order. The vertical direction V can denote a direction running perpendicular to a main extension plane of the semiconductor layer sequence 10. Directions running parallel to the main extension plane can be referred to as lateral directions L.
[0067] Furthermore, the first semiconductor layer 13 is arranged on the undoped layer 12 and is part of the buffer layer 11. The first semiconductor layer 13 has, in particular, a higher doping than the undoped layer 12.
[0068] The buffer layer 11 has a three-dimensional structure, i.e., a non-planar structure with inclined surfaces. The three-dimensional structure is created by a three-dimensional growth of the semiconductor layer sequence 10 on the growth substrate 20.
[0069] With increasing thickness dl, the three-dimensional structure can increasingly approximate a planar structure with a {0001}-oriented surface. However, in this case, growth is stopped before the planar structure is reached. The thickness dl can denote a vertical extension determined along the vertical direction V.
[0070] In particular, the buffer layer 11 has a three-dimensional structure with coalesced regions 111. The coalesced regions 111 are coalesced regions which arise through the coalescence of originally separate, isolated regions 112, the growth of which begins in the openings 23. The coalesced regions 111 are only partially coalesced regions which have depressions 113 with a cross-sectional size which decreases with increasing depth t. The depth t can here denote a vertical extent which is determined opposite to the vertical direction V. The depth t of the depressions 113 decreases with increasing thickness dl, so that the undoped layer 12 has, for example, deeper depressions 113 than the first semiconductor layer 13.The depth t of the depressions 113, which are present on a second surface 11B of the buffer layer 11 facing the active zone 14, can be between 100 nm and 500 nm inclusive or between 200 nm and 400 nm inclusive.
[0071] If the first semiconductor layer 13 is part of the buffer layer 11, as in the case of this exemplary embodiment, then in particular a surface 13A of the first semiconductor layer 13 forms the second surface 11B of the buffer layer 11. The first semiconductor layer 13 has depressed regions 133 which are identical to the depressions 113. However, it is also possible for the first semiconductor layer 13 to be a layer applied to the buffer layer which has depressed regions 133 in the region of the depressions 113, which each have a different vertical position and are produced, for example, by conformal application, but not by coalescence. In both cases, the first semiconductor layer 13 can follow the three-dimensional structure of the buffer layer 11. Furthermore, the first semiconductor layer 13 can have a predominantly uniform thickness d2.
[0072] The depressions 113 can have the shape of an inverse pyramid, an inverse truncated pyramid, an inverse cone or an inverse truncated cone. For example, the depressions 113 have a V-shaped cross-section transversely or perpendicular to the main extension plane and a hexagonal or dodecagonal cross-section parallel to the main extension plane. In a plan view of the buffer layer 11, the depressions 113 can, for example, have a honeycomb-shaped structure. The depressions 113 are each laterally delimited by inner surfaces 111A of the coalesced regions 111, wherein the inner surfaces 111A run, for example, along {10-11} crystal faces and / or {11-22} crystal faces. The depressions 113 are arranged in a targeted manner and are not stochastically distributed. For example, the recesses 113 can be arranged at equal distances a1, at least in some areas, within the scope of usual manufacturing tolerances.In this case, a maximum distance a1 between the recesses 113 is preferably at most as large as a drift and diffusion length of the charge carriers, for example, as large as a drift and diffusion length of the holes. This can advantageously increase the internal quantum efficiency.
[0073] The active zone 14 is arranged at least in some regions on the first semiconductor layer 13. The active zone 14 can have a greater thickness in regions located outside the recesses 113 than in regions within the recesses 113. In particular, the shape and size of the recesses 113 change only insignificantly due to the active zone 14.
[0074] The second semiconductor layer 15, which is arranged on a side of the active zone 14 facing away from the first semiconductor layer 13, extends into the depressions 113. In this case, cavities existing at locations of the depressions 113 can be completely filled by regions 151 of the second semiconductor layer 15. The regions 151 can at least approximate the depressions 113 in shape and size. The second semiconductor layer 15 has a varying thickness d3 with thickness maxima in the region of the depressions 113. Advantageously, existing unevennesses in regions of the depressions 113 can be compensated for by the second semiconductor layer 15. Furthermore, lateral charge carrier injection (cf. arrows) into the active zone 14 is possible during operation by the second semiconductor layer 15, the regions 151 of which laterally delimit the active zone 14.By means of the lateral charge carrier injection, the charge carrier density can be increased in more distant regions of the active zone 14 which are further away from the second main surface 10B, whereby the distribution of the charge carriers, for example the holes, in the active zone 14 is particularly homogeneous and the efficiency of the component 1 is improved.
[0075] For external electrical contacting, the optoelectronic semiconductor component 1 can have a first electrical contact means electrically connected to the first semiconductor layer 13 and a second electrical contact means electrically connected to the second semiconductor layer 15 (not shown).
[0076] In conjunction with Figure 1, a first embodiment of a method for producing an optoelectronic semiconductor component 1 will now be described in more detail.
[0077] The method comprises a step of providing a growth substrate 20 comprising a growth structure 22 with openings 23 and edge regions 24, wherein the openings 23 are laterally delimited by the edge regions 24. For example, the openings 23 are arranged at equal distances a2 within the scope of usual manufacturing tolerances. Furthermore, the openings 23 can be formed, for example, with a hexagonal cross-section. The openings 23 can be produced in a substrate body 21 by structuring the substrate body 21 or in a mask layer 25 on the substrate body 21 by structuring the mask layer 25. For further design of the substrate body 21 and the mask layer 25, reference is made to the explanations given above.
[0078] The structuring of the substrate body 21 or the mask layer 25 is carried out, for example, by means of a lithographic process. Using a photomask for this purpose, the positions of the openings 23 and thus of the recesses 113, as well as their distances a1 from one another, can be precisely controlled. To obtain distances a1 that are always smaller than the drift and diffusion length of the charge carriers, processes such as nanoimprint lithography or deep UV lithography are particularly suitable.
[0079] The method further comprises a step of producing a semiconductor layer sequence 10 on the growth substrate 20. In this case, a buffer layer 11 is grown on the growth substrate 20 such that the growth begins in the openings 23 and continues beyond the openings 23 to the edge regions 24, which are overgrown thereby. The buffer layer 11 can be produced by three-dimensional growth by means of metal-organic vapor phase epitaxy (MOVPE), wherein the growth conditions are selected such that the regions 112 grown in the openings 23 are formed with a three-dimensional shape, for example with the shape of a pyramid, a truncated pyramid, a cone or a truncated cone, at the beginning of the growth.
[0080] The buffer layer 11 is provided with a three-dimensional
[0081] A structure is formed with coalesced regions 111, wherein growth is stopped before a planar structure with a {0001}-oriented surface is achieved. The coalesced regions 111 are therefore only partially coalesced regions, which are produced by partial coalescence of the regions 112 and have depressions 113 with a cross-sectional size that decreases with increasing depth t, as already explained in more detail above. The coalesced regions 111, like the depressions 113 on the edge regions 24, are formed by lateral overgrowth of the edge regions 24.
[0082] For example, the buffer layer 11 is grown using FACELO (facet assisted epitaxial lateral overgrowth). This method is particularly suitable for producing a buffer layer 11 with few defects.
[0083] For example, the buffer layer 11 is formed within the scope of usual manufacturing tolerances with a maximum thickness dl which is at most as large as the distances a2 between the openings 23.
[0084] The buffer layer 11 is provided, for example, to reduce strains and to adjust the density of thread dislocations that can occur during the growth of the semiconductor layer sequence 10 onto the growth substrate 20 if the lattice constants of the materials used for the semiconductor layer sequence 10 and the growth substrate 20 differ.
[0085] The method further comprises a step of producing a first semiconductor layer 13 of a first
[0086] Conductivity type on an undoped layer 12 of the buffer layer 11. As already mentioned above, the first semiconductor layer 13 can be formed as a part of the buffer layer 11, so that recessed regions 133 of the first semiconductor layer 13 are identical to the recesses 113. For example, the undoped layer 12 can be grown first, and the first semiconductor layer 13 can be formed by continuing the growth while supplying a dopant, in particular an n-dopant such as Si.
[0087] The method further comprises a step of producing an active zone 14, wherein the active zone 14 is arranged at least in regions on the first semiconductor layer 13. For example, a vertical growth rate may be greater than a lateral growth rate on the inner surfaces 111A of the coalesced regions, so that the active zone 14 has a smaller layer thickness on the inner surfaces 111A than in regions outside the recesses 113.
[0088] Furthermore, the method comprises a step of growing a second semiconductor layer 15 of a second
[0089] Conductivity type such that the second semiconductor layer 15 is arranged on a side of the active zone 14 facing away from the first semiconductor layer 13 and extends into the depressions 113.
[0090] MOVPE is a suitable manufacturing method for producing the active zone 14 and the second semiconductor layer 15.
[0091] The method can be carried out for a large number of optoelectronic semiconductor components 1 in the wafer composite. The optoelectronic semiconductor components 1 are characterized by comparatively small intensity fluctuations among one another. The alternative production of the recesses 113 by means of partial coalescence results in several advantages compared to the formation and use of V-defects. The semiconductor layer sequence 10 can be made thinner because, on the one hand, the buffer layer 11 does not have to have an optimized thread dislocation density and, on the other hand, an opening layer can be dispensed with. Furthermore, due to the smaller number of thread dislocations 16, the quality of the semiconductor layer sequence 10 and thus the efficiency of the optoelectronic semiconductor component 1 can be improved. Omitting an opening layer also leads to a lower point defect density and a smoother second surface 11B.
[0092] In conjunction with Figure 2, a further embodiment of an optoelectronic semiconductor component 1 or a method for producing an optoelectronic semiconductor component 1 is explained in more detail.
[0093] The method further comprises a step of removing the growth substrate 20 from the semiconductor layer sequence 10, so that the optoelectronic semiconductor component 1 is free of a growth substrate.
[0094] The optoelectronic semiconductor component 1 is, for example, a micro-LED, which is characterized by particularly small dimensions. A vertical extent h of the optoelectronic semiconductor component 1, which is determined, for example, along the vertical direction V, can lie in the single-digit to double-digit micrometer range, for example between 1.5 pm and 10 pm. Furthermore, lateral extents b of the optoelectronic semiconductor component 1, which are determined, for example, along the lateral directions L, can be in the single-digit to triple-digit micrometer range. For example, a possible value range of the lateral extents b extends up to and including 100 pm, or up to and including 70 pm, or up to and including 50 pm.
[0095] The invention is not limited by the description based on the exemplary embodiments. Rather, the invention encompasses any novel feature and any combination of features, including in particular any combination of features in the patent claims, even if this feature or combination itself is not explicitly stated in the patent claims or exemplary embodiments.
[0096] This patent application claims priority from German patent application 102023113584 . 8 , the disclosure of which is hereby incorporated by reference .
[0097] Reference symbol list
[0098] I optoelectronic semiconductor component
[0099] 10 Semiconductor layer sequence
[0100] 10A first main area
[0101] 10B second main area
[0102] II Buffer layer
[0103] 11A first surface
[0104] 11B second surface
[0105] 12 undoped layer
[0106] 13 first semiconductor layer
[0107] 13A Surface
[0108] 14 active zones
[0109] 15 second semiconductor layer
[0110] 16 Thread displacement
[0111] 20 Growth substrate
[0112] 21 substrate bodies
[0113] 22 Growth structure
[0114] 23 Opening
[0115] 24 Marginal area
[0116] 25 mask layer
[0117] III coalesced area
[0118] 111A inner surface
[0119] 112 isolated area
[0120] 113 Deepening
[0121] 133 deepened area
[0122] 151 Area of the second semiconductor layer a1 , a2 Distance b Lateral extent dl , d2 , d3 Thickness h Vertical extent t Depth
[0123] L lateral direction
[0124] V vertical direction
Claims
Patent claims 1. Optoelectronic semiconductor component (1) comprising - a semiconductor layer sequence (10) comprising - a buffer layer (11) having a three-dimensional structure with coalesced regions (111), wherein the coalesced regions (111) have depressions (113) with a cross-sectional size that decreases with increasing depth (t), - a first semiconductor layer (13) of a first conductivity type, which is arranged on an undoped layer (12) of the buffer layer (11) and has recessed regions (133) in the region of the recesses (113), - an active zone (14) which is arranged at least in regions on the first semiconductor layer (13), and - a second semiconductor layer (15) of a second conductivity type, which is arranged on a side of the active zone (14) facing away from the first semiconductor layer (13) and extends into the depressions (113) and / or recessed regions (133), wherein during operation a lateral charge carrier injection into the active zone (14) takes place from the second semiconductor layer (15) arranged in the depressions (113) and / or recessed regions (133), and wherein the coalesced regions (111) are each not completely coalesced regions.
2. Optoelectronic semiconductor component (1) according to the preceding claim, wherein the depressions (113) have the shape of an inverse pyramid, an inverse a truncated pyramid, an inverse cone, or an inverse truncated cone.
3. Optoelectronic semiconductor component (1) according to one of the preceding claims, wherein the recesses (113) have a V-shaped cross-section.
4. Optoelectronic semiconductor component (1) according to one of the preceding claims, wherein the depressions (113) are each laterally delimited by inner surfaces (111A) of the coalesced regions (111) which run along {10-11} crystal faces and / or {11-22} crystal faces.
5. Optoelectronic semiconductor component (1) according to one of the preceding claims, wherein the recesses (113) are arranged at least in regions at equal intervals (al).
6. Optoelectronic semiconductor component (1) according to one of the preceding claims, wherein a maximum distance (al) between the recesses (113) is at most as large as a drift and diffusion length of the charge carriers.
7. Optoelectronic semiconductor component (1) according to one of the preceding claims, wherein the first semiconductor layer (13) has a higher doping than the undoped layer (12) of the buffer layer (11).
8. Optoelectronic semiconductor component (1) according to one of the preceding claims, wherein the first semiconductor layer (13) has a predominantly uniform thickness (d2).
9. Optoelectronic semiconductor component (1) according to one of the preceding claims, wherein the second semiconductor layer (15) has a varying thickness (d3) with thickness maxima in the region of the recesses (113).
10. Optoelectronic semiconductor component (1) according to one of the preceding claims, wherein the active zone (14) has a sequence of individual layers by means of which a quantum well structure is formed.
11. Optoelectronic semiconductor component (1) according to one of the preceding claims, which is a micro-LED.
12. A method for producing an optoelectronic semiconductor component (1) according to one of the preceding claims, comprising: - Providing a growth substrate (20) comprising a growth structure (22) with openings (23) and edge regions (24) , wherein the openings (23) are laterally delimited by the edge regions (24), - producing a semiconductor layer sequence (10) on the growth substrate (20), wherein the semiconductor layer sequence (10) a buffer layer (11), a first semiconductor layer (13) of a first conductivity type, an active zone (14) and a second semiconductor layer (15) of a second conductivity type and the generation of the Semiconductor layer sequence (10) comprises the following steps: - growing a buffer layer (11) on the Growth substrate (20) such that the growth begins in the openings (23) and continues beyond the openings (23) to the edge regions (24), wherein the buffer layer (11) is formed with a three-dimensional structure having coalesced regions (111), and wherein the coalesced areas (111) form depressions (113) with a cross-sectional size that decreases with increasing depth (t), - producing a first semiconductor layer (13) of a first conductivity type on an undoped layer (12) of the buffer layer (11) such that the first semiconductor layer (13) has recessed areas (133) in the area of the recesses (113), - producing an active zone (14) at least in regions on the first semiconductor layer (13) and - growing a second semiconductor layer (15) of a second conductivity type such that the second semiconductor layer (15) is located on a side of the active zone facing away from the first semiconductor layer (13) (14) and extends into the depressions (113) and / or depressed regions (133), wherein the coalesced regions (111) are each not completely coalesced regions which are produced by partial coalescence of regions (112) which are grown in the openings (23) of the growth structure (22).
13. The method according to the preceding claim, wherein the growth of the buffer layer (11) is carried out by means of FACELO ("facet assisted epitaxial lateral overgrowth").
14. Method according to one of the two preceding claims, wherein the coalesced regions (111) are produced on the edge regions (24).
15. The method according to any one of claims 12 to 14, wherein providing the growth substrate (20) comprises: - Providing a substrate body (21) and - producing the openings (23) in the substrate body (21) by structuring the substrate body (21) or producing the openings (23) in a mask layer (25) on the substrate body (21) by structuring the mask layer (25).
16. The method according to any one of claims 12 to 15, wherein the structuring is carried out by means of a lithographic process.
17. The method according to any one of claims 12 to 16, wherein a maximum thickness of the buffer layer (11) is, within the scope of usual manufacturing tolerances, at most as large as the distances (a2) between the openings (23).
18. Method according to one of claims 12 to 17, wherein the openings (23) are formed with a hexagonal cross-section.
19. The method according to any one of claims 12 to 18, wherein the growth of the buffer layer (11) comprises: - growing the undoped layer (12) and - continuing the growth with supply of a dopant, whereby the first semiconductor layer (13) is produced.
20. The method according to any one of claims 12 to 19, wherein the growth substrate (20) is removed from the semiconductor layer sequence (10).
Citation Information
Patent Citations
OPTOELECTRONIC SEMICONDUCTOR COMPONENT AND METHOD FOR FABRICING AN OPTOELECTRONIC SEMICONDUCTOR COMPONENT
DE102023113584A1
Method of manufacturing compound semiconductor device
JP2010157603A
Semiconductor light emitting device and fabrication method thereof
KR1020090017945A
Stacked structure including vertically grown semiconductor, p-n junction device including the stacked structure, and method of manufacturing thereof
US20120222732A1
Nanowire device
US20220262978A1