Battery cell, battery and electric device
By optimizing the groove section structure of the pressure relief components of the battery cell, the fatigue resistance and pressure relief timeliness are improved, and the problem of insufficient fatigue resistance of the existing battery cell is solved when the thermal runaway is performed, and the service life of the battery is extended .
Patent Information
- Application Number
- PCT/CN2023/111809
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-31
- Filing Date
- 2023-08-08
- Publication Date
- 2024-12-05
AI Technical Summary
The existing battery cell has insufficient fatigue resistance when thermally out of control, resulting in poor pressure relief and affecting the service life of the battery cell.
A battery cell is designed, and its pressure relief component consists of a multi-stage groove, including a first groove section, a second groove section and a third groove section. By adjusting the residual thickness ratio and connection method of the groove section, the detonation position and crack are optimized. The diffusion path improves the fatigue resistance and timeliness of pressure relief components.
It effectively improves the timeliness and service life of the battery cell during normal use, reduces the probability of cracking of the pressure relief components in the groove area, and enhances the safety of the battery.
Smart Images

Figure CN2023111809_05122024_PF_FP_ABST
Abstract
Description
Battery cells, batteries and electrical equipment
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to Chinese patent application (2023106406395) entitled “Battery Cell, Battery and Electrical Equipment” filed on May 31, 2023, the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present application relates to the field of battery technology, and in particular to a battery cell, a battery, and an electrical device. Background Art
[0004] With the development of new energy technology, batteries are used more and more widely, for example, in mobile phones, laptops, electric vehicles, electric airplanes, electric ships, electric toy cars, electric toy ships, electric toy airplanes and power tools.
[0005] Typical battery cells are equipped with pressure relief components. In the event of thermal runaway, these components release internal pressure to improve reliability. In addition to improving battery reliability, the lifespan of battery cells is also a key consideration. Therefore, increasing the lifespan of battery cells is a pressing issue in battery technology.
[0006] Summary of the Invention
[0007] The embodiments of the present application provide a battery cell, a battery, and an electrical device, which can effectively increase the service life of the battery cell.
[0008] In a first aspect, an embodiment of the present application provides a battery cell, comprising a shell, the shell comprising a pressure relief component, the pressure relief component being provided with a groove portion, the pressure relief component being configured to be able to split along the groove portion to release the pressure inside the battery cell, and the pressure relief component having a detonation position; wherein the groove portion comprises a first groove section, a second groove section and a third groove section, the first groove section is arranged opposite to the third groove section, the second groove section connects the first groove section and the third groove section, and the detonation position is formed in the first groove section and / or the third groove section.
[0009] In the above technical solution, the detonation position of the pressure relief component is formed in the first slot segment and / or the third slot segment, and the detonation position is not formed in the second slot segment, so that the pressure relief component has higher fatigue strength in the area of the second slot segment, reducing the possibility of the pressure relief component cracking in the second slot segment during normal use of the battery cell, improving the long-term reliability of the pressure relief component, and increasing the service life of the battery cell.
[0010] In some embodiments, the first slot segment forms a detonation location, and the residual thickness of the first slot segment is smaller than that of the second slot segment. This allows the detonation location to be formed near the point where the second slot segment connects to the first slot segment. During pressure relief, after the pressure relief component cracks at the detonation location, the crack can propagate along both the first slot segment and the second slot segment. Furthermore, because the residual thickness of the first slot segment is smaller than that of the second slot segment, the residual thickness of the second slot segment is increased, thereby improving the fatigue strength of the pressure relief component in the area where the second slot segment is located and further reducing the possibility of the pressure relief component cracking in the area of the second slot segment during normal use of the battery cell.
[0011] In some embodiments, the residual thickness of the first slot segment is D1, and the residual thickness of the second slot segment is D2, satisfying the following relationship: 0.15 ≤ D1 / D2 ≤ 0.95. If D1 / D2 < 0.15, the residual thickness of the second slot segment is too large, and during pressure relief, there is a risk that the pressure relief component may not break along the second slot segment, resulting in poor timeliness of pressure relief. If D1 / D2 > 0.95, the residual thickness of the second slot segment is too small, and the pressure relief component may break along the second slot segment during normal use of the battery cell, shortening the battery cell's service life. A value of 0.15 ≤ D1 / D2 ≤ 0.95 can improve both the timeliness of pressure relief and the service life of the battery cell.
[0012] In some embodiments, 0.3≤D1 / D2≤0.9, which improves the performance of the battery cell and increases the timeliness of pressure release and the service life of the battery cell.
[0013] In some embodiments, 0.5≤D1 / D2≤0.85. This further improves the overall performance of the battery cell, by lowering the probability of the pressure relief component cracking along the second groove segment during normal use of the battery cell and lowering the probability of the battery cell exploding during thermal runaway.
[0014] In some embodiments, 0.03 mm ≤ D1 ≤ 0.5 mm.
[0015] In some embodiments, 0.15 mm ≤ D1 ≤ 0.4 mm.
[0016] In some embodiments, 0.05 mm ≤ D2 ≤ 0.65 mm.
[0017] In some embodiments, 0.25 mm ≤ D2 ≤ 0.5 mm.
[0018] In some embodiments, the depth of the first groove segment is greater than the depth of the second groove segment, such that the residual thickness of the first groove segment is smaller than that of the second groove segment. During molding, the first groove segment can be machined deeper than the second groove segment on the pressure relief component to achieve a smaller residual thickness of the first groove segment than that of the second groove segment. This is simple to implement.
[0019] In some embodiments, the first groove segment includes first-stage grooves and second-stage grooves, the first-stage grooves and second-stage grooves being arranged along the thickness direction of the pressure relief component, and the second-stage grooves being provided on the bottom surfaces of the first-stage grooves. During molding, the first-stage grooves can be first molded on the pressure relief component, and then the second-stage grooves can be molded on the bottom surfaces of the first-stage grooves to form the first groove segment. This can reduce the molding depth of each stage groove in the first groove segment, reduce the molding force applied to the pressure relief component during molding of the first groove segment, and reduce the possibility of cracks in the pressure relief component during molding of the first groove segment.
[0020] In some embodiments, the bottom surface of the first-stage groove is flush with the bottom surface of the second groove segment. This allows the first-stage groove and the second groove segment of the first groove segment to be coplanar. During molding, the first-stage groove of the first groove segment and the second groove segment can be molded together before the second-stage groove of the first groove segment is molded, thereby improving the molding efficiency of the groove portion.
[0021] In some embodiments, the pressure relief component has a first surface and a second surface facing each other along its thickness, with the first and second grooves being arranged sequentially along a direction from the first surface to the second surface, and the bottom surface of the second groove being closer to the second surface than the bottom surface of the second groove segment; wherein the bottom surface of the second groove is connected to the bottom surface of the second groove segment via a first inclined plane or a first arc surface. During pressure relief, after the pressure relief component cracks at the detonation position, the crack on the bottom surface of the second groove can quickly spread along the first inclined plane or the first arc surface to the bottom surface of the second groove segment, thereby reducing the time for the crack to spread from the first groove segment to the second groove segment, and further shortening the time it takes for the pressure relief component to crack along the groove portion.
[0022] In some embodiments, the third slot segment is formed with a detonation location, and the residual thickness of the third slot segment is smaller than that of the second slot segment. This allows the detonation location to be formed near the junction of the second and third slot segments. During pressure relief, after the pressure relief component cracks at the detonation location, the crack can propagate along both the third slot segment and the second slot segment. Since the residual thickness of the third slot segment is smaller than that of the second slot segment, this effectively increases the residual thickness of the second slot segment, improving the fatigue strength of the pressure relief component in the area where the second slot segment is located and further reducing the likelihood of the pressure relief component cracking in the second slot segment during normal use of the battery cell. Furthermore, since both the first and third slot segments are formed with detonation locations, when the internal pressure of the battery cell reaches the detonation pressure, the detonation locations of both the first and third slot segments can crack. This allows the crack to propagate along both the first and third slot segments while also spreading from both ends of the second slot segment toward the center, shortening the time it takes for the pressure relief component to crack along the slot.
[0023] In some embodiments, the residual thickness of the third groove section is equal to the residual thickness of the first groove section. When the battery cell is depressurized, the pressure relief component has better synchronization when it splits along the first and third groove sections, further shortening the time it takes for the pressure relief component to split along the groove portion and improving the timeliness of pressure relief.
[0024] In some embodiments, the residual thickness of the second slot segment is D2, and the residual thickness of the third slot segment is D3, satisfying the following: 0.15 ≤ D3 / D2 ≤ 0.95. If D3 / D2 < 0.15, the residual thickness of the second slot segment is too large, and there is a risk that the pressure relief component will not crack along the second slot segment during pressure relief, resulting in poor pressure relief timeliness. If D3 / D2 > 0.95, the residual thickness of the second slot segment is too small, and there is a risk that the pressure relief component will crack along the second slot segment during normal use of the battery cell, shortening the battery cell's service life. A value of 0.15 ≤ D3 / D2 ≤ 0.95 can improve both the timeliness of pressure relief and the service life of the battery cell.
[0025] In some embodiments, 0.3≤D3 / D2≤0.9, which improves the performance of the battery cell, increases the timeliness of pressure release of the battery cell, and improves the service life of the battery cell.
[0026] In some embodiments, 0.5≤D3D2≤0.85. This further improves the overall performance of the battery cell, by lowering the probability of the pressure relief component cracking along the second groove segment during normal use of the battery cell and lowering the probability of the battery cell exploding during thermal runaway.
[0027] In some embodiments, 0.03 mm ≤ D3 ≤ 0.5 mm.
[0028] In some embodiments, 0.15 mm ≤ D3 ≤ 0.4 mm.
[0029] In some embodiments, the depth of the third groove segment is greater than that of the second groove segment, such that the residual thickness of the third groove segment is smaller than that of the second groove segment. During molding, the third groove segment can be machined deeper than the second groove segment on the pressure relief component to achieve a smaller residual thickness of the third groove segment than that of the second groove segment, which is simple to implement.
[0030] In some embodiments, the third groove segment includes a third-stage groove and a fourth-stage groove, the third-stage groove and the fourth-stage groove being arranged along the thickness direction of the pressure relief component, and the fourth-stage groove being disposed on the bottom surface of the third-stage groove. During molding, the third-stage groove can be first molded on the pressure relief component, and then the fourth-stage groove can be molded on the bottom surface of the third-stage groove to form the third groove segment. In this way, the molding depth of each stage groove in the third groove segment can be reduced, reducing the molding force applied to the pressure relief component during molding of the third groove segment, and reducing the possibility of cracks in the pressure relief component during molding of the third groove segment.
[0031] In some embodiments, the bottom surface of the third-stage groove is flush with the bottom surface of the second groove segment. This allows the third-stage groove of the third groove segment and the second groove segment to be coplanar. During molding, the third-stage groove of the third groove segment and the second groove segment can be molded together before molding the fourth-stage groove of the third groove segment, thereby improving the molding efficiency of the groove portion.
[0032] In some embodiments, the pressure relief component has a first surface and a second surface facing each other along its thickness direction, and the third and fourth grooves are arranged sequentially along a direction from the first surface to the second surface, with the bottom surface of the fourth groove being closer to the second surface than the bottom surface of the second groove segment; wherein the bottom surface of the fourth groove is connected to the bottom surface of the second groove segment via a second inclined plane or a second arc surface. During pressure relief, after the pressure relief component cracks at the detonation position, the crack on the bottom surface of the fourth groove can quickly spread along the second inclined plane or the second arc surface to the bottom surface of the second groove segment, thereby reducing the time for the crack to spread from the third groove segment to the second groove segment, and further shortening the time it takes for the pressure relief component to crack along the groove portion.
[0033] In some embodiments, along the extension direction of the second slot segment, both ends of the second slot segment are connected to the first slot segment and the third slot segment, respectively. Thus, both ends of the second slot segment do not extend beyond the first slot segment and the third slot segment, respectively. During pressure relief, pressure can be accurately relieved through the area defined by the first, second, and third slot segments, without causing cracks in other areas of the pressure relief component, and thus more easily achieving directional pressure relief.
[0034] In some embodiments, the first slot segment and the second slot segment are connected at a first position, and along the extension direction of the first slot segment, the first position is offset from both ends of the first slot segment. During the pressure relief process, after the pressure relief component cracks at the first position, the crack can spread along the first slot segment from the first position to both ends, thereby shortening the time it takes for the pressure relief component to crack along the first slot segment.
[0035] In some embodiments, the first position is located at the midpoint of the first slot segment along its extension direction. During the pressure relief process, the crack propagates from the first position to both ends of the first slot segment over an equal distance, further shortening the time it takes for the pressure relief component to crack along the first slot segment.
[0036] In some embodiments, the third slot segment is connected to the second slot segment at a second position, and along the extension direction of the third slot segment, the second position is offset from both ends of the third slot segment. During the pressure relief process, after the pressure relief component cracks at the second position, the crack can spread along the third slot segment from the second position to both ends, thereby shortening the time it takes for the pressure relief component to crack along the third slot segment.
[0037] In some embodiments, the second position is located at the midpoint of the third slot segment along its extension direction. During the pressure relief process, the crack propagates from the second position to both ends of the third slot segment over an equal distance, further shortening the time it takes for the pressure relief component to crack along the third slot segment.
[0038] In some embodiments, the first slot segment, the second slot segment, and the third slot segment are all slots extending along a straight line. The first slot segment, the second slot segment, and the third slot segment are all straight slots, which can reduce the difficulty of forming the first slot segment, the second slot segment, and the third slot segment.
[0039] In some embodiments, the first slot segment is perpendicular to the second slot segment; and / or the third slot segment is perpendicular to the second slot segment. If the first slot segment is perpendicular to the second slot segment, stress is more concentrated near the location where the first and second slot segments meet. If the detonation position is located near the location where the first and second slot segments meet, the processing depth of the first slot segment can be reduced, thereby reducing the difficulty of processing the first slot segment, provided the detonation pressure of the battery cell remains constant. If the third slot segment is perpendicular to the second slot segment, stress is more concentrated near the location where the third and second slot segments meet. If the detonation position is located near the location where the third and second slot segments meet, the processing depth of the third slot segment can be reduced, thereby reducing the difficulty of processing the third slot segment, provided the detonation pressure of the battery cell remains constant.
[0040] In some embodiments, the first, second, and third groove segments define a pressure relief zone; the pressure relief component is provided with a guide groove, which is spaced apart from the second groove segment and configured to guide the pressure relief zone in flipping and opening. The provision of the guide groove facilitates flipping and opening the pressure relief zone, reduces the difficulty of flipping the pressure relief zone, and effectively improves the timeliness of pressure relief.
[0041] In some embodiments, the first, second, and third slot sections define two pressure relief zones, one located on either side of the second slot section. The pressure relief component is provided with two guide grooves, with the second slot section located between the two guide grooves. The two guide grooves are configured to guide the two pressure relief zones to flip open. During the pressure relief process, the two guide grooves can guide the two pressure relief zones, thereby increasing the opening speed of the two pressure relief zones and providing more timely pressure relief.
[0042] In some embodiments, neither the first nor the third slot segments contact the guide slot. The guide slot is less likely to affect the first and third slot segments, improving the fatigue strength of the pressure relief component at the first and third slot segments. This reduces the likelihood of stress concentration caused by the connection between the guide slot and the first and third slot segments, which could cause the pressure relief component to crack at the connection during normal use of the battery cell. Furthermore, during the pressure relief process, after the pressure relief component cracks along the first and third slot segments, the cracks are less likely to spread to the guide slot, reducing the likelihood of splashing from the pressure relief component after the pressure relief area is opened.
[0043] In some embodiments, the guide groove and the groove portion are provided on either side of the pressure relief component along the thickness direction of the pressure relief component. This reduces the impact of the guide groove on the groove portion during molding, and provides a better guiding effect on the pressure relief area, making it easier to flip open.
[0044] In some embodiments, the guide groove extends along an extension direction of the second groove segment.
[0045] In some embodiments, along the extension direction of the second slot segment, the first and third slot segments are located on either side of the guide groove, respectively. The length of the portion of the second slot segment between the first and third slot segments is L1, and the length of the guide groove is L2, satisfying the following: 1 mm ≤ L1 - L2 ≤ 10 mm. If L1 - L2 < 1 mm, the distance between at least one of the first and third slot segments and the guide groove is small, and the guide groove has a significant impact on the first and third slot segments, potentially leading to premature rupture of the pressure relief component near the guide groove in the first or third slot segment, increasing the likelihood of premature pressure relief. If L1 - L2 > 10 mm, the length of the guide groove is short, and the guide groove's ability to facilitate the opening of the pressure relief zone is poor. A value of 1 mm ≤ L1 - L2 ≤ 10 mm can both reduce the likelihood of premature pressure relief from the pressure relief component and improve the guide groove's ability to facilitate the opening of the pressure relief zone.
[0046] In some embodiments, 2 mm ≤ L1 - L2 ≤ 6 mm, thereby further reducing the possibility of the pressure relief component releasing pressure prematurely and further improving the guiding capability of the guide groove in helping the pressure relief area to flip open.
[0047] In some embodiments, along the extension direction of the first slot segment, the distance between the guide groove and the second slot segment is L3. The length L4 of the portion of the first slot segment extending from the second slot segment toward the guide groove is 0.5 mm ≤ |L3-L4| ≤ 15 mm. If |L3-L4| is less than 0.5 mm, the distance between the end of the first slot segment and the guide groove is small. When a crack in the pressure relief component propagates along the first slot segment to the end of the first slot segment, the crack is likely to spread to the guide groove, causing the pressure relief area to detach. If |L3-L4| is greater than 15 mm, the distance between the guide groove and the second slot segment is large, and the guide groove's ability to assist in the pressure relief area's flipping is poor. If L3 is less than L4, the distance between the guide groove and the second slot segment is small, resulting in a smaller area for the pressure relief area to be flipped open, reducing the pressure relief area. If 0.5 mm ≤ |L3-L4| ≤ 15 mm, this reduces the possibility of the pressure relief area detaching and splashing, while also increasing the difficulty of flipping open and the opening area of the pressure relief area.
[0048] In some embodiments, 1 mm ≤ |L3-L4| ≤ 10 mm.
[0049] In some embodiments, the housing includes a first wall; the pressure relief component is the first wall; or the pressure relief component is separately provided from the first wall, with the pressure relief component mounted on the first wall. If the first wall serves as the pressure relief component, the groove can be formed directly on the first wall, forming an integrated pressure relief structure, which improves reliability, eliminates the installation process of the pressure relief component, and can reduce the production cost of the battery cell. If the pressure relief component is mounted on the first wall, the pressure relief component is independent of the housing, and the pressure relief component and the housing can be manufactured and assembled separately, which reduces production difficulty and improves efficiency.
[0050] In some embodiments, the housing includes a shell and an end cover, wherein the shell has an opening and the end cover closes the opening, and the end cover is the first wall portion, so that the end cover has a pressure relief function and the difficulty of forming the groove portion on the end cover is lower.
[0051] In some embodiments, the housing includes a shell and an end cap, wherein the shell has an opening, the end cap closes the opening, and at least one wall portion of the shell is a first wall portion. This allows the shell to have a pressure relief function. During pressure relief, emissions discharged from the interior of the battery cell are less likely to affect external components outside the end cap, thereby reducing the possibility of damage to the external components by the emissions.
[0052] In some embodiments, the housing includes a bottom wall and multiple side walls, the multiple side walls being arranged around the bottom wall. The housing has an opening at one end opposite the bottom wall, and the bottom wall serves as the first wall portion. The bottom wall has a pressure relief function, and in the event of thermal runaway of a battery cell, pressure can be relieved through the bottom wall. In the battery, the pressure relief component is not easily obstructed by other battery cells.
[0053] In some embodiments, the first wall portion is a rectangular wall portion, the second slot segment extends along the length of the first wall portion, and the first slot segment and the third slot segment both extend along the width of the first wall portion. In this way, the second wall portion can provide more space for the second slot segment, allowing the second slot segment to be made longer, thereby increasing the pressure relief area of the pressure relief component.
[0054] In some embodiments, along the thickness direction of the pressure relief component, the first wall portion has an outer surface facing away from the interior of the housing; the first slot segment has a first midplane extending along its extension direction, the second slot segment has a second midplane extending along its extension direction, and the third slot segment has a third midplane extending along its extension direction. The minimum distance from the center point of the outer surface to the first midplane is M1, the minimum distance from the center point of the outer surface to the second midplane is M2, and the minimum distance from the center point of the outer surface to the third midplane is M3, satisfying the following conditions: M2 < M1, M2 < M3. When the internal pressure of the battery cell changes, the first wall portion is more likely to deform closer to the center point, and M2 < M1, M2 < M3. This allows the first and third slot segments to be further away from the center point, thereby improving the fatigue strength of the pressure relief component at the first and third slot segments.
[0055] In some embodiments, along the thickness direction of the pressure relief component, the projection of the center point of the outer surface lies within the second groove segment; and / or |M3 - M1| ≤ 5 mm. If the projection of the center point of the outer surface lies within the second groove segment, the second groove segment is closer to the center point of the outer surface, allowing the pressure relief component to rupture more promptly along the second groove segment during pressure relief, thereby improving the timely pressure relief performance of the pressure relief component. If |M3 - M1| ≤ 5 mm, the first and third groove segments are both farther from the center point, reducing the impact of deformation of the pressure relief component near the center point on the first and third groove segments.
[0056] In a second aspect, an embodiment of the present application provides a battery, comprising a battery cell provided by any embodiment of the first aspect.
[0057] In a third aspect, an embodiment of the present application provides an electrical device, comprising a battery cell provided by any one embodiment of the first aspect, wherein the battery cell is used to provide electrical energy to the electrical device. BRIEF DESCRIPTION OF THE DRAWINGS
[0058] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the following is a brief introduction to the drawings required for use in the embodiments. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without creative work.
[0059] FIG1 is a schematic structural diagram of a vehicle provided in some embodiments of the present application;
[0060] FIG2 is an exploded view of a battery provided in some embodiments of the present application;
[0061] FIG3 is an exploded view of a battery cell provided in some embodiments of the present application;
[0062] FIG4 is an axonometric view of a battery cell provided in some embodiments of the present application;
[0063] FIG5 is a partial view of the pressure relief component shown in FIG4;
[0064] FIG6 is a cross-sectional view taken along line AA of the pressure relief component shown in FIG5 ;
[0065] FIG7 is a partial enlarged view of point B in FIG6;
[0066] FIG8 is a partial enlarged view of point C in FIG6;
[0067] FIG9 is a partial enlarged view of a battery cell provided in some other embodiments of the present application;
[0068] FIG10 is a partial view of the pressure relief component shown in FIG9;
[0069] FIG11 is a DD cross-sectional view of the pressure relief component shown in FIG10 ;
[0070] FIG12 is a partial enlarged view of point E in FIG11 ;
[0071] FIG13 is a partial cross-sectional view of a pressure relief component provided in some other embodiments of the present application;
[0072] FIG14 is a partial enlarged view of the pressure relief component F shown in FIG11;
[0073] FIG15 is a partial cross-sectional view of a pressure relief component provided in yet other embodiments of the present application;
[0074] FIG16 is a partial view of a pressure relief component provided in some other embodiments of the present application;
[0075] FIG17 is a cross-sectional view taken along line GG of the pressure relief component shown in FIG16 ;
[0076] FIG18 is an exploded view of a housing provided in some embodiments of the present application;
[0077] FIG19 is an exploded view of a housing provided in some other embodiments of the present application;
[0078] FIG20 is an exploded view of a housing provided in yet other embodiments of the present application;
[0079] FIG21 is an exploded view of a housing provided in some further embodiments of the present application;
[0080] FIG22 is a partial view of the first wall portion provided in some embodiments of the present application.
[0081] Icons: 1-shell; 11-shell; 111-bottom wall; 112-side wall; 12-end cover; 13-pressure relief component; 131-groove; 1311-first groove section; 1311a-first groove bottom surface; 1311b-first groove side surface; 1311c-first level groove; 1311d-second level groove; 1311e-first arc surface; 1311f-first midplane; 1312-second groove section; 1312b-second groove bottom surface; 1312c-second midplane; 1313-third groove section; 1313a-third groove bottom surface; 1313c-third level groove; 1313d-fourth level groove; 1313e-second arc surface; 1313f-third midplane Surface; 1314-detonation position; 1315-first position; 1316-second position; 132-first surface; 133-second surface; 134-pressure relief area; 135-guide groove; 14-first wall; 141-pressure relief hole; 142-outer surface; 1421-center point; 2-electrode assembly; 21-ear; 3-electrode terminal; 4-current collecting member; 5-insulating member; 10-battery cell; 20-housing; 201-first part; 202-second part; 100-battery; 200-controller; 300-motor; 1000-vehicle; X-thickness direction of pressure relief component; Y-length direction of first wall; Z-width direction of first wall. DETAILED DESCRIPTION
[0082] To make the purpose, technical solutions, and advantages of the embodiments of this application more clear, the technical solutions in the embodiments of this application will be clearly described below in conjunction with the drawings in the embodiments of this application. Obviously, the described embodiments are part of the embodiments of this application, not all of the embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.
[0083] Unless otherwise defined, all technical and scientific terms used in this application have the same meanings as commonly understood by those skilled in the art to which this application belongs. The terms used in the specification of this application are for the purpose of describing specific embodiments only and are not intended to limit this application. The terms "including" and "having" and any variations thereof in the specification and claims of this application and the above-mentioned drawings are intended to cover non-exclusive inclusions. The terms "first" and "second" in the specification and claims of this application or the above-mentioned drawings are used to distinguish different objects, rather than to describe a specific order or a primary-secondary relationship.
[0084] References to "embodiments" in this application mean that a particular feature, structure, or characteristic described in connection with the embodiment may be included in at least one embodiment of the application. The appearance of this phrase in various places in the specification does not necessarily refer to the same embodiment, nor does it constitute an independent or alternative embodiment that is mutually exclusive of other embodiments.
[0085] The term "and / or" in this application simply describes an association between related objects, indicating that three possible relationships exist. For example, A and / or B can represent: A exists alone, A and B exist simultaneously, and B exists alone. In addition, the character " / " in this application generally indicates that the related objects are in an "or" relationship.
[0086] In the embodiments of this application, the same reference numerals represent the same components, and for the sake of brevity, detailed descriptions of the same components in different embodiments are omitted. It should be understood that the thickness, length, width, and other dimensions of the various components in the embodiments of this application, as well as the overall thickness, length, width, and other dimensions of the integrated device shown in the drawings are merely illustrative and should not constitute any limitation on this application.
[0087] The term "plurality" used in this application refers to two or more (including two).
[0088] In the embodiment of the present application, the battery cell may be a secondary battery. A secondary battery refers to a battery cell that can be continuously used by activating active materials by charging after the battery cell is discharged.
[0089] Battery cells include but are not limited to lithium-ion batteries, sodium-ion batteries, sodium-lithium-ion batteries, lithium metal batteries, sodium metal batteries, lithium-sulfur batteries, magnesium-ion batteries, nickel-hydrogen batteries, nickel-cadmium batteries, lead-acid batteries, etc.
[0090] A battery cell typically includes an electrode assembly. This assembly includes a positive electrode, a negative electrode, and a separator. During the charge and discharge process, active ions (such as lithium ions) are inserted and removed between the positive and negative electrodes. A separator, placed between the positive and negative electrodes, reduces the risk of short circuits while allowing the active ions to pass through.
[0091] In some embodiments, the positive electrode may be a positive electrode sheet, which may include a positive electrode current collector and a positive electrode active material disposed on at least one surface of the positive electrode current collector.
[0092] As an example, the positive electrode current collector has two surfaces facing each other in its thickness direction, and the positive electrode active material is provided on either or both of the two facing surfaces of the positive electrode current collector.
[0093] As an example, the positive electrode current collector may be a metal foil or a composite current collector. For example, as the metal foil, aluminum with a silver-plated surface, stainless steel with a silver-plated surface, stainless steel, copper, aluminum, nickel, carbon electrode, carbon, nickel or titanium, etc. may be used. The composite current collector may include a polymer material base layer and a metal layer. The composite current collector may be formed by forming a metal material (aluminum, aluminum alloy, nickel, nickel alloy, titanium, titanium alloy, silver and silver alloy, etc.) on a polymer material substrate (such as a substrate of polypropylene, polyethylene terephthalate, polybutylene terephthalate, polystyrene, polyethylene, etc.).
[0094] As an example, the positive electrode active material may include at least one of the following materials: lithium-containing phosphates, lithium transition metal oxides and their respective modified compounds. However, the present application is not limited to these materials, and other traditional materials that can be used as battery positive electrode active materials may also be used. These positive electrode active materials may be used alone or in combination of two or more. Among them, examples of lithium-containing phosphates may include but are not limited to at least one of lithium iron phosphate (such as LiFePO4 (also referred to as LFP)), a composite material of lithium iron phosphate and carbon, lithium manganese phosphate (such as LiMnPO4), a composite material of lithium manganese phosphate and carbon, lithium iron manganese phosphate, and a composite material of lithium iron manganese phosphate and carbon. Examples of lithium transition metal oxides may include but are not limited to lithium cobalt oxide (such as LiCoO2), lithium nickel oxide (such as LiNiO2), lithium manganese oxide (such as LiMnO2, LiMn2O4), lithium nickel cobalt oxide, lithium manganese cobalt oxide, lithium nickel manganese oxide, lithium nickel cobalt manganese oxide (such as LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 O2 (also referred to as NCM 333 ), LiNi 0.5 Co 0.2 Mn 0.3 O2 (also referred to as NCM 523 ), LiNi 0.5 Co 0.25 Mn 0.25 O2 (also referred to as NCM 211 ), LiNi 0.6 Co 0.2 Mn 0.2 O2 (also referred to as NCM 622 ), LiNi 0.8 Co 0.1 Mn 0.1 O2 (also referred to as NCM 811 ), lithium nickel cobalt aluminum oxide (such as LiNi 0.85 Co 0.15 Al 0.05 O2) and at least one of its modified compounds, etc.
[0095] In some embodiments, a positive electrode may be a metal foam. The metal foam may be nickel foam, copper foam, aluminum foam, alloy foam, or carbon foam, among others. When a metal foam is used as the positive electrode, the surface of the metal foam may or may not be provided with a positive electrode active material. For example, a lithium source material, potassium metal, or sodium metal may be filled and / or deposited within the metal foam, where the lithium source material is lithium metal and / or a lithium-rich material.
[0096] In some embodiments, the negative electrode may be a negative electrode sheet, and the negative electrode sheet may include a negative electrode current collector.
[0097] As an example, the negative electrode current collector can be a metal foil, a metal foam, or a composite current collector. For example, as the metal foil, aluminum or stainless steel with a silver surface treatment, stainless steel, copper, aluminum, nickel, carbon electrode, carbon, nickel, or titanium can be used. The metal foam can be nickel foam, copper foam, aluminum foam, alloy foam, or carbon foam. The composite current collector can include a polymer material base layer and a metal layer. The composite current collector can be formed by forming a metal material (copper, copper alloy, nickel, nickel alloy, titanium, titanium alloy, silver, and silver alloy, etc.) on a polymer material substrate (such as a substrate of polypropylene, polyethylene terephthalate, polybutylene terephthalate, polystyrene, polyethylene, etc.).
[0098] As an example, the negative electrode sheet may include a negative electrode current collector and a negative electrode active material disposed on at least one surface of the negative electrode current collector.
[0099] As an example, the negative electrode current collector has two surfaces facing each other in its thickness direction, and the negative electrode active material is provided on either or both of the two facing surfaces of the negative electrode current collector.
[0100] As an example, the negative electrode active material may adopt the negative electrode active material for battery cells that is well known in the art. As an example, the negative electrode active material may include at least one of the following materials: artificial graphite, natural graphite, soft carbon, hard carbon, silicon-based materials, tin-based materials, lithium titanate, etc. The silicon-based material may be selected from at least one of elemental silicon, silicon oxide compounds, silicon-carbon composites, silicon-nitrogen composites, and silicon alloys. The tin-based material may be selected from at least one of elemental tin, tin oxide compounds, and tin alloys. However, the present application is not limited to these materials, and other traditional materials that can be used as negative electrode active materials for batteries may also be used. These negative electrode active materials may be used alone or in combination of two or more.
[0101] In some embodiments, the material of the positive electrode current collector may be aluminum, and the material of the negative electrode current collector may be copper.
[0102] In some embodiments, the separator is a separator membrane, which can be any known porous separator membrane with good chemical and mechanical stability.
[0103] As an example, the separator can be made of at least one of fiberglass, non-woven fabric, polyethylene, polypropylene, and polyvinylidene fluoride. The separator can be a single-layer film or a multi-layer composite film. In the case of a multi-layer composite film, the materials of each layer can be the same or different. The separator can be a separate component positioned between the positive and negative electrodes, or it can be attached to the surfaces of the positive and negative electrodes.
[0104] In some embodiments, the separator is a solid electrolyte, which is disposed between the positive electrode and the negative electrode and serves to transport ions and isolate the positive and negative electrodes.
[0105] In some embodiments, the battery cell further includes an electrolyte, which acts as a conductor of ions between the positive and negative electrodes. The electrolyte can be liquid, gel, or solid. Liquid electrolytes include an electrolyte salt and a solvent.
[0106] In some embodiments, the electrolyte salt may include at least one of lithium hexafluorophosphate, lithium tetrafluoroborate, lithium perchlorate, lithium hexafluoroarsenate, lithium bisfluorosulfonyl imide, lithium bistrifluoromethanesulfonyl imide, lithium trifluoromethanesulfonate, lithium difluorophosphate, lithium difluorooxalatoborate, lithium bisoxalatoborate, lithium difluorodioxalatophosphate, and lithium tetrafluorooxalatophosphate.
[0107] In some embodiments, the solvent may include at least one of ethylene carbonate, propylene carbonate, ethyl methyl carbonate, diethyl carbonate, dimethyl carbonate, dipropyl carbonate, methylpropyl carbonate, ethylpropyl carbonate, butylene carbonate, fluoroethylene carbonate, methyl formate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, ethyl butyrate, 1,4-butyrolactone, cyclopentane, dimethyl sulfone, methyl ethyl sulfone and diethyl sulfone. The solvent may also be an ether solvent. The ether solvent may include one or more of ethylene glycol dimethyl ether, ethylene glycol diethyl ether, diethylene glycol dimethyl ether, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, 1,3-dioxolane, tetrahydrofuran, methyltetrahydrofuran, diphenyl ether and crown ether.
[0108] Among them, the gel electrolyte includes a skeleton network with a polymer as the electrolyte, combined with an ionic liquid-lithium salt.
[0109] Among them, solid electrolytes include polymer solid electrolytes, inorganic solid electrolytes, and composite solid electrolytes.
[0110] As an example, the polymer solid electrolyte may be polyether (polyethylene oxide), polysiloxane, polycarbonate, polyacrylonitrile, polyvinylidene fluoride, polymethyl methacrylate, a single ion polymer, polyionic liquid-lithium salt, cellulose, or the like.
[0111] As an example, the inorganic solid electrolyte may include an oxide solid electrolyte (crystalline perovskite, sodium superconducting ion conductor, garnet, amorphous LiPON film), a sulfide solid electrolyte (crystalline lithium superion conductor (lithium germanium phosphosulfide, silver germanium sulfide), amorphous sulfide) and one or more of a halide solid electrolyte, a nitride solid electrolyte and a hydride solid electrolyte.
[0112] As an example, a composite solid electrolyte is formed by adding an inorganic solid electrolyte filler to a polymer solid electrolyte.
[0113] In some embodiments, the electrode assembly is a wound structure, wherein the positive electrode sheet and the negative electrode sheet are wound into the wound structure.
[0114] In some embodiments, the electrode assembly is a laminate structure.
[0115] As an example, multiple positive electrode sheets and multiple negative electrode sheets can be provided respectively, and the multiple positive electrode sheets and the multiple negative electrode sheets can be alternately stacked.
[0116] As an example, a plurality of positive electrode sheets may be provided, and the negative electrode sheet may be folded to form a plurality of stacked folded segments, with a positive electrode sheet being sandwiched between adjacent folded segments.
[0117] As an example, both the positive electrode sheet and the negative electrode sheet are folded to form a plurality of stacked folded segments.
[0118] As an example, a plurality of separators may be provided, each of which is disposed between any adjacent positive electrode sheets or negative electrode sheets.
[0119] As an example, the separator may be provided continuously, and may be provided between any adjacent positive electrode sheets or negative electrode sheets by folding or winding.
[0120] In some embodiments, the shape of the electrode assembly can be cylindrical, flat, or polygonal.
[0121] In some embodiments, the electrode assembly is provided with tabs that can conduct current from the electrode assembly. The tabs include a positive tab and a negative tab.
[0122] In some embodiments, a battery cell may include a housing. The housing is used to encapsulate components such as the electrode assembly and the electrolyte. The housing may be a steel housing, an aluminum housing, a plastic housing (e.g., polypropylene), a composite metal housing (e.g., a copper-aluminum composite housing), or an aluminum-plastic film.
[0123] As an example, the battery cell can be a cylindrical battery cell, a prismatic battery cell, a soft-pack battery cell or a battery cell of other shapes. The prismatic battery cell includes a square-shell battery cell, a blade-shaped battery cell, and a polygonal battery. The polygonal battery is, for example, a hexagonal battery, etc. There is no special limitation in this application.
[0124] The battery mentioned in the embodiments of the present application refers to a single physical module including one or more battery cells to provide higher voltage and capacity.
[0125] In some embodiments, the battery may be a battery module. When there are multiple battery cells, the multiple battery cells are arranged and fixed to form a battery module.
[0126] In some embodiments, the battery may be a battery pack, which includes a case and battery cells, wherein the battery cells or battery modules are housed in the case.
[0127] In some embodiments, the box body can be used as a part of the chassis structure of the vehicle. For example, part of the box body can become at least a part of the floor of the vehicle, or part of the box body can become at least a part of the cross beam and longitudinal beam of the vehicle.
[0128] In some embodiments, the battery may be an energy storage device, including an energy storage container, an energy storage cabinet, and the like.
[0129] The development of battery technology must take into account multiple design factors at the same time, such as energy density, cycle life, discharge capacity, charge and discharge rate and other performance parameters. In addition, battery safety must also be considered.
[0130] To improve the safety of battery cells, a pressure relief component can be installed in the battery cell. In the event of thermal runaway, the pressure relief component can be used to release the internal pressure of the battery cell. To achieve timely pressure relief, a groove can be provided in the pressure relief component. The pressure relief component is thinner where the groove is provided. When the internal pressure of the battery cell reaches a threshold, the pressure relief component breaks at the groove location to release the internal pressure of the battery cell.
[0131] In order to further improve the timeliness of pressure relief of the pressure relief component, the groove on the pressure relief component can be divided into multiple sections, for example, a first groove section, a second groove section and a third groove section, the first groove section and the third groove section are arranged opposite to each other, and the second groove section connects the first groove section and the third groove section. In this way, after the pressure relief component is cracked along the first groove section, the second groove section and the third groove section, it has a larger pressure relief area, thereby achieving rapid pressure relief. In such a battery cell, the pressure relief component has an ignition position, that is, when the internal pressure of the battery cell reaches the ignition pressure, the pressure relief component first cracks at the ignition position. The ignition position is generally formed in the second groove section. When the internal pressure of the battery cell reaches the ignition pressure, the pressure relief component cracks at the ignition position, and the cracks then spread along the second groove section to the first groove section and the third groove section.
[0132] During normal use of the battery cell, the internal pressure of the battery cell may change. During long-term use, the pressure relief component may deform as the pressure of the battery cell changes, causing the pressure relief component to crack at the position of the second slot segment. In particular, the fatigue strength of the area near the detonation position of the second slot segment is worse, and there is a risk of the pressure relief component cracking in the area of the second slot segment during normal use of the battery cell, affecting the service life of the battery cell.
[0133] In view of this, an embodiment of the present application provides a battery cell, in which a pressure relief component in the battery cell is provided with a groove portion, the groove portion includes a first groove section, a second groove section and a third groove section, the first groove section is arranged opposite to the third groove section, the second groove section connects the first groove section and the third groove section, and the detonation position of the pressure relief component is formed in the first groove section and / or the third groove section.
[0134] The battery cells described in the embodiments of the present application are suitable for batteries and electrical equipment using the battery cells.
[0135] Electrical equipment can be vehicles, mobile phones, portable devices, laptops, ships, spacecraft, electric toys, and electric tools, etc. Vehicles can be fuel vehicles, gas vehicles, or new energy vehicles. New energy vehicles can be pure electric vehicles, hybrid vehicles, or extended-range vehicles, etc. Spacecraft include airplanes, rockets, space shuttles, and spacecraft, etc. Electric toys include fixed or mobile electric toys, such as game consoles, electric car toys, electric ship toys, and electric airplane toys, etc. Electric tools include metal cutting electric tools, grinding electric tools, assembly electric tools, and railway electric tools, such as electric drills, electric grinders, electric wrenches, electric screwdrivers, electric hammers, impact drills, concrete vibrators, and electric planers, etc. The embodiments of the present application do not impose any special restrictions on the above-mentioned electrical equipment.
[0136] For the convenience of description, the following embodiments are described by taking the electric device as a vehicle as an example.
[0137] Please refer to Figure 1, which is a schematic diagram of the structure of a vehicle 1000 provided in some embodiments of the present application. A battery 100 is disposed within vehicle 1000. Battery 100 can be located at the bottom, front, or rear of vehicle 1000. Battery 100 can be used to power vehicle 1000, for example, as an operating power source for vehicle 1000.
[0138] The vehicle 1000 may further include a controller 200 and a motor 300 . The controller 200 is used to control the battery 100 to supply power to the motor 300 , for example, to meet the power requirements of the vehicle 1000 during startup, navigation, and driving.
[0139] In some embodiments of the present application, the battery 100 can not only serve as the operating power source of the vehicle 1000, but also serve as the driving power source of the vehicle 1000, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle 1000.
[0140] Please refer to Figure 2, which is an exploded view of a battery 100 provided in some embodiments of the present application. The battery 100 includes a battery cell 10 and a housing 20, wherein the battery cell 10 is accommodated in the housing 20.
[0141] The housing 20 is a component that houses the battery cells 10 and provides a storage space for the battery cells 10. The housing 20 can have various structures. In some embodiments, the housing 20 can include a first portion 201 and a second portion 202, which overlap to define a storage space for the battery cells 10. The first portion 201 and the second portion 202 can have various shapes, such as a rectangular parallelepiped or a cylinder. The first portion 201 can be a hollow structure with one side open, and the second portion 202 can also be a hollow structure with one side open. The open side of the second portion 202 overlaps the open side of the first portion 201, forming the housing 20 with a storage space. Alternatively, the first portion 201 can be a hollow structure with one side open, and the second portion 202 can be a plate-like structure. The second portion 202 overlaps the open side of the first portion 201, forming the housing 20 with a storage space. The first portion 201 and the second portion 202 can be sealed by a sealing element, which can be a sealing ring, sealant, etc.
[0142] In the battery 100, there can be one or more battery cells 10. If there are multiple battery cells 10, the multiple battery cells 10 can be connected in series, parallel, or in a hybrid connection. A hybrid connection refers to a combination of series and parallel connections among the multiple battery cells 10. Multiple battery cells 10 can be connected in series, parallel, or in a hybrid connection to form a battery module, which can then be connected in series, parallel, or in a hybrid connection to form a single unit and housed within the housing 20. Alternatively, all battery cells 10 can be directly connected in series, parallel, or in a hybrid connection, and then the entire unit formed by all battery cells 10 can be housed within the housing 20.
[0143] Please refer to Figure 3, which is an exploded view of a battery cell 10 provided in some embodiments of the present application. The battery cell 10 may include a housing 1 and an electrode assembly 2, wherein the electrode assembly 2 is accommodated in the housing 1.
[0144] In some embodiments, the housing 1 may include a shell 11 and an end cover 12 , wherein the shell 11 has an opening and the end cover 12 closes the opening of the shell 11 .
[0145] The housing 11 is a component for accommodating the electrode assembly 2. The housing 11 can be a hollow structure with an opening at one end, or a hollow structure with openings at opposite ends. The housing 11 can have various shapes, such as a cylinder or a rectangular parallelepiped. The housing 11 can be made of various materials, such as copper, iron, aluminum, steel, and aluminum alloys.
[0146] The end cap 12 is a component that closes the opening of the shell 11 to isolate the internal environment of the battery cell 10 from the external environment. The end cap 12 and the shell 11 together define a receiving space for accommodating the electrode assembly 2, electrolyte and other components. The end cap 12 can be connected to the shell 11 by welding or rolling to close the opening of the shell 11. The shape of the end cap 12 can be adapted to the shape of the shell 1. For example, the shell 11 is a rectangular parallelepiped structure, and the end cap 12 is a rectangular plate structure adapted to the shell 1. For another example, the shell 11 is a cylindrical structure, and the end cap 12 is a circular plate structure adapted to the shell 11. The material of the end cap 12 can also be a variety of materials, such as copper, iron, aluminum, steel, aluminum alloy, plastic, etc. The material of the end cap 12 and the shell 11 can be the same or different.
[0147] In an embodiment where the housing 11 is open at one end, one end cap 12 may be provided. In an embodiment where the housing 11 is open at two opposite ends, two end caps 12 may be provided, each of which closes the two openings of the housing 11, and the two end caps 12 and the housing 11 together define a receiving space.
[0148] In some embodiments, the battery cell 10 may further include an electrode terminal 3, which is disposed on the outer casing 1. The electrode terminal 3 is used to electrically connect to the tab 21 of the electrode assembly 2 to output electrical energy from the battery cell 10. The electrode terminal 3 may be disposed on the shell 11 of the outer casing 1 or on the end cap 12 of the outer casing 1. The electrode terminal 3 and the tab 21 may be directly connected, for example, by direct welding the electrode terminal 3 and the tab 21. The electrode terminal 3 and the tab 21 may also be indirectly connected, for example, by indirectly connecting the electrode terminal 3 and the tab 21 through a current collecting member 4. The current collecting member 4 may be a metal conductor, such as copper, iron, aluminum, steel, an aluminum alloy, or the like.
[0149] As an example, as shown in FIG3 , an opening is formed at one end of the housing 11. There is only one end cap 12 in the outer shell 1, and each end cap 12 closes the opening of the housing 11. Two electrode terminals 3 are provided on the end cap 12, which are respectively a positive electrode terminal and a negative electrode terminal. A positive electrode tab and a negative electrode tab are formed on the end of the electrode assembly 2 facing the end cap 12. The positive electrode terminal is connected to the positive electrode tab via a current collecting member 4, and the negative electrode terminal is connected to the negative electrode tab via another current collecting member 4.
[0150] 3 , the battery cell 10 may further include an insulating member 5 . The insulating member 5 is a component that separates the housing 11 from the electrode assembly 2 , thereby achieving insulation isolation between the housing 11 and the electrode assembly 2 . The insulating member 5 is made of an insulating material, including but not limited to plastic, rubber, and the like.
[0151] As an example, the insulating member 5 wraps around the outside of the electrode assembly 2 along the circumference of the opening of the housing 11. There can be one or more electrode assemblies 2 within the housing 1. If there is a single electrode assembly 2, the insulating member 5 wraps around it. If there are multiple electrode assemblies 2, one insulating member 5 can be provided for each electrode assembly 2, with each insulating member 5 wrapping around a single electrode assembly 2. Alternatively, multiple electrode assemblies 2 can be formed as a single integral component, with the insulating member 5 wrapping around the integral component.
[0152] Please refer to Figures 4 and 5. Figure 4 is an isometric view of a battery cell 10 provided in some embodiments of the present application; Figure 5 is a partial view of the pressure relief component 13 shown in Figure 4. The present application provides a battery cell 10, comprising a housing 1, which includes a pressure relief component 13. The pressure relief component 13 is provided with a groove 131. The pressure relief component 13 is configured to rupture along the groove 131 to release pressure within the battery cell 10. The pressure relief component 13 has an initiation location 1314. The groove 131 includes a first groove section 1311, a second groove section 1312, and a third groove section 1313. The first groove section 1311 is disposed opposite the third groove section 1313. The second groove section 1312 connects the first groove section 1311 and the third groove section 1313. The initiation location 1314 is formed in the first groove section 1311 and / or the third groove section 1313.
[0153] The pressure relief component 13 is a component within the battery cell 10 that is used to release pressure within the battery cell 10. The pressure relief component 13 may be the end cap 12 of the outer casing 1, or at least a portion of the shell 11 of the outer casing 1. For example, the outer casing 1 includes multiple walls that together define the interior space of the outer casing 1, and at least one wall of the outer casing 1 serves as the pressure relief component 13. The pressure relief component 13 may also be a component independent of the shell 11 and the end cap 12. For example, the pressure relief component 13 may be mounted on the end cap 12. In another example, the pressure relief component 13 may be mounted on the shell 11. It is understood that if the end cap 12 serves as the pressure relief component 13, the groove 131 is provided on the end cap 12; if at least a portion of the shell 11 serves as the pressure relief component 13, the groove 131 is provided on the shell 11.
[0154] The groove portion 131 can be formed in a variety of ways, such as stamping, milling, etching, etc. The first groove segment 1311, the second groove segment 1312, and the third groove segment 1313 can be linear grooves extending along a straight line, or non-linear grooves extending along a non-straight line, such as arcuate grooves extending along an arcuate line. If the first groove segment 1311, the second groove segment 1312, and the third groove segment 1313 are linear grooves, the first groove segment 1311 and the third groove segment 1313 can be arranged in parallel or at a small angle, such as the angle between the first groove segment 1311 and the third groove segment 1313 is less than or equal to 10 degrees. The first groove segment 1311 and the second groove segment 1312 can be arranged perpendicularly, or at an acute angle or an obtuse angle; the third groove segment 1313 and the second groove segment 1312 can be arranged perpendicularly, or at an acute angle or an obtuse angle. In the groove portion 131, the groove portion 131 may only include the first groove section 1311, the second groove section 1312, and the third groove section 1313. The groove portion 131 may also include other groove sections in addition to the first groove section 1311, the second groove section 1312, and the third groove section 1313. For example, the groove portion 131 also includes a fourth groove section, which is located between the first groove section 1311 and the third groove section 1313 and is connected to the second groove section 1312. The first groove section 1311 can be a single-stage groove or a multi-stage groove. If the first groove section 1311 is a multi-stage groove, the first groove section 1311 is a stepped groove. During molding, the first groove section 1311 can be machined step by step along the thickness direction X of the pressure relief component. The second groove section 1312 can be a single-stage groove or a multi-stage groove. If the second groove section 1312 is a multi-step groove, or a stepped groove, during molding, the second groove section 1312 can be machined stepwise along the thickness direction X of the pressure relief component. The third groove section 1313 can be a single-step groove or a multi-step groove. If the third groove section 1313 is a multi-step groove, or a stepped groove, during molding, the third groove section 1313 can be machined stepwise along the thickness direction X of the pressure relief component.
[0155] The second trough section 1312 is connected to the first trough section 1311 and the third trough section 1313. The second trough section 1312 may be connected to the first trough section 1311 and the third trough section 1313 at both ends, or at least one of the first trough section 1311 and the third trough section 1313 may be connected to a position offset from the end of the second trough section 1312, such that at least one of the first trough section 1311 and the third trough section 1313 is located between the two ends of the second trough section 1312. The first trough section 1311 and the second trough section 1312 may be connected at one end of the first trough section 1311, or offset from the two ends of the first trough section 1311. The third trough section 1313 and the second trough section 1312 may be connected at one end of the third trough section 1313, or offset from the two ends of the third trough section 1313. The first trough section 1311, the second trough section 1312, and the third trough section 1313 may be formed in various shapes, such as a U-shape, an N-shape, an H-shape, etc.
[0156] The detonation point 1314 is the location where the pressure relief component 13 first ruptures when the internal pressure of the battery cell 10 reaches the detonation pressure. There can be one or more detonation points 1314 in the groove portion 131. When the pressure relief component 13 releases pressure, the detonation point 1314 can be formed on the bottom surface of the first groove section 1311 and / or the bottom surface of the third groove section 1313. The detonation point 1314 can be formed only in the first groove section 1311, only in the third groove section 1313, or in both the first and third groove sections 1311, 1313. In the embodiment where the first slot segment 1311 is formed with the detonation position 1314, the detonation position 1314 can be located at any position of the first slot segment 1311. For example, the detonation position 1314 can be located near the end of the first slot segment 1311. In another example, the detonation position 1314 can be located near the connection between the first slot segment 1311 and the second slot segment 1312. Taking the example of the second slot segment 1312 where both ends are connected to the first slot segment 1311 and the third slot segment 1313, respectively, as viewed along the thickness direction X of the pressure relief component, as long as the minimum distance between the end of the second slot segment 1312 connected to the first slot segment 1311 and the detonation position 1314 is less than the width of the first slot segment 1311, it can be understood that the detonation position 1314 is located near the connection between the first slot segment 1311 and the second slot segment 1312. In the embodiment where the third slot segment 1313 is formed with the detonation position 1314, the detonation position 1314 can be located at any position of the third slot segment 1313. For example, the detonation position 1314 can be located near the end of the third slot segment 1313. In another example, the detonation position 1314 can be located near the connection between the third slot segment 1313 and the second slot segment 1312. Taking the example of the second slot segment 1312 where both ends are connected to the first slot segment 1311 and the third slot segment 1313, respectively, as viewed along the thickness direction X of the pressure relief component, as long as the minimum distance between the end of the second slot segment 1312 connected to the third slot segment 1313 and the detonation position 1314 is less than the width of the third slot segment 1313, it can be understood that the detonation position 1314 is located near the connection between the third slot segment 1313 and the second slot segment 1312.
[0157] In the embodiment of the present application, the detonation position 1314 of the pressure relief component 13 is only formed in the first slot section 1311 and / or the third slot section 1313, and the detonation position 1314 is not formed in the second slot section 1312, so that the pressure relief component 13 has a higher fatigue strength in the area of the second slot section 1312, thereby reducing the possibility of the pressure relief component 13 cracking in the area of the second slot section 1312 during normal use of the battery cell 10, improving the long-term reliability of the pressure relief component 13, and increasing the service life of the battery cell 10.
[0158] In some embodiments, referring to Figures 6-8, Figure 6 is a cross-sectional view taken along line AA of the pressure relief component 13 shown in Figure 5; Figure 7 is a partial enlarged view of point B in Figure 6; and Figure 8 is a partial enlarged view of point C in Figure 6. A first slot segment 1311 is formed with a detonation location 1314 (shown in Figure 5), and the residual thickness of the first slot segment 1311 is less than the residual thickness of the second slot segment 1312.
[0159] The residual thickness of the first slot segment 1311 is the thickness of the remaining portion after the pressure relief component 13 is provided with the first slot segment 1311. This residual portion may be the slot bottom wall of the first slot segment 1311. The thickness of the slot bottom wall of the first slot segment 1311 may be uniform or uneven. If the thickness of the slot bottom wall of the first slot segment 1311 is uneven, the thickness of the thinnest portion of the slot bottom wall of the first slot segment 1311 is the residual thickness of the first slot segment 1311. The residual thickness of the second slot segment 1312 is the thickness of the remaining portion after the pressure relief component 13 is provided with the second slot segment 1312. This residual portion may be the slot bottom wall of the second slot segment 1312. The thickness of the slot bottom wall of the second slot segment 1312 may be uniform or uneven. If the thickness of the slot bottom wall of the second slot segment 1312 is uneven, the thickness of the thinnest portion of the slot bottom wall of the second slot segment 1312 is the residual thickness of the second slot segment 1312.
[0160] As shown in Figures 7 and 8, the residual thickness of the first slot segment 1311 is D1, the residual thickness of the second slot segment 1312 is D2, and the residual thickness of the third slot segment 1313 is D3. It can be understood that D1<D2. D1 and D3 can be equal or different.
[0161] In this embodiment, the residual thickness of the first slot segment 1311 is smaller than that of the second slot segment 1312, allowing the detonation location 1314 to be formed near the junction of the second slot segment 1312 and the first slot segment 1311. During pressure relief, after the pressure relief component 13 cracks at the detonation location 1314, the crack propagates along both the first slot segment 1311 and the second slot segment 1312. Furthermore, because the residual thickness of the first slot segment 1311 is smaller than that of the second slot segment 1312, the residual thickness of the second slot segment 1312 is increased, thereby improving the fatigue strength of the pressure relief component 13 in the region where the second slot segment 1312 is located, further reducing the possibility of the pressure relief component 13 cracking in the region of the second slot segment 1312 during normal use of the battery cell 10. In addition, since the stress is more concentrated at the position where the first slot segment 1311 and the second slot segment 1312 are connected, the detonation position 1314 of the first slot segment 1311 can be formed near the position where the first slot segment 1311 and the second slot segment 1312 are connected.
[0162] In some embodiments, the residual thickness of the first slot segment 1311 is D1, and the residual thickness of the second slot segment 1312 is D2, satisfying: 0.15≤D1 / D2≤0.95.
[0163] D1 / D2 can be any point value among 0.15, 0.2, 0.25, 0.3, 0.35, 0.4, 0.45, 0.5, 0.55, 0.6, 0.65, 0.7, 0.75, 0.8, 0.85, 0.9, 0.95, etc., or a range value between any two of them.
[0164] The inventors conducted multiple groups of tests, in which the D2 of the battery cells 10 in different groups was different. The explosion rate of the battery cells 10 in each group during thermal runaway and the cracking rate of the pressure relief component 13 along the second groove section 1312 under normal use conditions of the battery cells 10 were measured. The test results are shown in Table 1.
[0165] The method for measuring the residual thickness of the first groove segment 1311 and the residual thickness of the third groove segment 1313 is as follows: the pressure relief component 13 is cut into three sections, and the cutting direction is perpendicular to the extension direction of the first groove segment 1311. The cross section of the middle section is polished to fully remove burrs and then placed on a three-dimensional coordinate measuring machine. The residual thickness of the first groove segment 1311 and the residual thickness of the third groove segment 1313 on the cross section are measured by the three-dimensional coordinate measuring machine.
[0166] Method for measuring the residual thickness of the second groove segment 1312: cut the above-mentioned middle segment into three segments, and the cutting direction is perpendicular to the extension direction of the second groove segment 1312. Polish the cross section of the middle segment among the three segments to fully remove burrs and then place it on a three-dimensional coordinate measuring machine. Measure the residual thickness of the second groove segment 1312 on the cross section using the three-dimensional coordinate measuring machine.
[0167] The explosion rate of battery cells 10 during thermal runaway is measured by installing a small heating membrane within the battery cell 10. This membrane is energized, heating the battery cell 10 until thermal runaway occurs. The cell 10 is then observed for explosion. Each test uses 1,000 battery cells 10, and the explosion rate is calculated: explosion rate Q1 = number of exploded battery cells 10 / total number of battery cells 10 × 100%.
[0168] Method for measuring the cracking rate of the pressure relief component 13 along the second groove section 1312 under normal use conditions of the battery cell 10: place the battery cell 10 at 25±2°C and perform cyclic charge and discharge in the charge and discharge range of 5%-97% SOC, and conduct 1000 groups of tests at the same time to observe whether the pressure relief component 13 cracks along the second groove section 1312 when the battery cell 10 life drops to 80% SOH, and calculate the cracking rate of the pressure relief component 13 along the second groove section 1312, cracking rate Q2 = number of cracked battery cells 10 / total number of battery cells 10 × 100%.
[0169] Table 1
[0170] As can be seen from Table 1 above, when D1 / D2 is less than 0.15, the timely pressure relief is poor, and the probability of explosion of the battery cell 10 during thermal runaway is high. When D1 / D2 is greater than 0.95, the pressure relief component 13 is more likely to crack along the second groove section 1312 during normal use of the battery cell 10, shortening the service life of the battery cell 10. However, when 0.15≤D1 / D2≤0.95, the timely pressure relief of the battery cell 10 is improved, and the service life of the battery cell 10 is also increased.
[0171] In some embodiments, 0.3≤D1 / D2≤0.9.
[0172] In this embodiment, D1 / D2 can be any one of the point values of 0.3, 0.32, 0.35, 0.38, 0.4, 0.42, 0.45, 0.48, 0.5, 0.52, 0.55, 0.58, 0.6, 0.62, 0.65, 0.68, 0.7, 0.72, 0.75, 0.78, 0.8, 0.82, 0.85, 0.88, 0.9, etc., or a range value between any two of them.
[0173] It can be seen from Table 1 above that when 0.3≤D1 / D2≤0.9, the performance of the battery cell 10 is better, and the timeliness of pressure release of the battery cell 10 and the service life of the battery cell 10 can be improved.
[0174] In some embodiments, 0.5≤D1 / D2≤0.85.
[0175] In this embodiment, D1 / D2 can be any one of the point values of 0.5, 0.52, 0.53, 0.55, 0.57, 0.58, 0.59, 0.6, 0.62, 0.63, 0.65, 0.67, 0.68, 0.69, 0.7, 0.72, 0.73, 0.75, 0.77, 0.78, 0.79, 0.8, 0.82, 0.83, 0.85, etc., or a range value between any two of them.
[0176] As can be seen from Table 1 above, when 0.5≤D1 / D2≤0.85, the overall performance of the battery cell 10 is further improved. This can not only control the probability of the pressure relief component 13 cracking along the second groove section 1312 during normal use of the battery cell 10 to a low level, but also control the probability of the battery cell 10 exploding during thermal runaway to a low level.
[0177] In some embodiments, 0.03 mm ≤ D1 ≤ 0.5 mm.
[0178] In this embodiment, D1 can be any point value of 0.03mm, 0.1mm, 0.15mm, 0.2mm, 0.25mm, 0.3mm, 0.35mm, 0.4mm, 0.45mm, 0.5mm, etc., or a range value between any two of them.
[0179] In some embodiments, 0.15 mm ≤ D1 ≤ 0.4 mm.
[0180] In this embodiment, D1 can be any point value of 0.15mm, 0.18mm, 0.2mm, 0.22mm, 0.25mm, 0.28mm, 0.3mm, 0.32mm, 0.35mm, 0.38mm, 0.4mm, etc., or a range value between any two of them.
[0181] In some embodiments, 0.05 mm ≤ D2 ≤ 0.65 mm.
[0182] In this embodiment, D2 can be any point value of 0.05mm, 0.1mm, 0.15mm, 0.2mm, 0.25mm, 0.3mm, 0.35mm, 0.4mm, 0.45mm, 0.5mm, 0.55mm, 0.6mm, 0.65mm, etc., or a range value between any two of them.
[0183] In some embodiments, 0.25 mm ≤ D2 ≤ 0.5 mm.
[0184] D2 can be any point value among 0.25mm, 0.27mm, 0.3mm, 0.32mm, 0.35mm, 0.37mm, 0.4mm, 0.42mm, 0.45mm, 0.47mm, 0.5mm, etc., or a range value between any two of them.
[0185] In some embodiments, referring to FIG. 7 , the depth of the first slot segment 1311 is greater than the depth of the second slot segment 1312 , so that the residual thickness of the first slot segment 1311 is smaller than the residual thickness of the second slot segment 1312 .
[0186] As an example, along the thickness direction X of the pressure relief component, the pressure relief component 13 includes a first surface 132 and a second surface 133 disposed opposite each other. A first groove section 1311 and a second groove section 1312 are disposed on the first surface 132. The first surface 132 and the second surface 133 may be parallel planes. The distance between the first surface 132 and the second surface 133 is H0. The distance between the groove bottom surface of the first groove section 1311 (the first groove bottom surface 1311a) and the second surface 133 is D1. The distance between the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312b) and the second surface 133 is D2. The depth of the first groove section 1311 is H0-D1, and the depth of the second groove section 1312 is H0-D2, where H0-D1>H0-D2. Where H0 may be the thickness of the pressure relief component 13.
[0187] The first groove section 1311 may include a first groove bottom surface 1311a and two first groove side surfaces 1311b. The two first groove side surfaces 1311b are arranged opposite each other along the width direction of the first groove section 1311 and are connected by the first groove bottom surface 1311a. The two first groove side surfaces 1311b may be arranged in parallel or at an acute angle. For example, the distance between the two first groove side surfaces 1311b in the width direction of the first groove section 1311 gradually decreases along the depth direction of the first groove section 1311, so that the two first groove side surfaces 1311b are inclined surfaces. The first groove bottom surface 1311a may be a flat surface or an arcuate surface.
[0188] The second groove section 1312 may include a second groove bottom surface 1312b and two second groove side surfaces (not shown in FIG7 ). The two second groove side surfaces are arranged opposite each other along the width direction of the second groove section 1312 and connected by the second groove bottom surface 1312b. The two second groove side surfaces may be arranged in parallel or at an acute angle. For example, the distance between the two second groove side surfaces in the width direction of the second groove section 1312 gradually decreases along the depth direction of the second groove section 1312, so that the two second groove side surfaces form inclined surfaces. The second groove bottom surface 1312b may be a flat surface or an arcuate surface.
[0189] During molding, the first groove section 1311 can be processed deeper than the second groove section 1312 on the pressure relief component 13, so that the residual thickness of the first groove section 1311 is smaller than the residual thickness of the second groove section 1312, and the implementation method is simple.
[0190] In some embodiments, please refer to Figures 9-12. Figure 9 is a partial enlarged view of a battery cell 10 provided in other embodiments of the present application; Figure 10 is a partial view of the pressure relief component 13 shown in Figure 9; Figure 11 is a cross-sectional view taken along line DD of the pressure relief component 13 shown in Figure 10; and Figure 12 is a partial enlarged view of point E in Figure 11. The first groove section 1311 includes a first-stage groove 1311c and a second-stage groove 1311d. The first-stage groove 1311c and the second-stage groove 1311d are arranged along the thickness direction X of the pressure relief component, and the second-stage groove 1311d is provided on the bottom surface of the first-stage groove 1311c.
[0191] The first groove section 1311 can be a two-stage groove, one of which is a first-stage groove 1311c and the other is a second-stage groove 1311d. The extension direction of the first-stage groove 1311c is the same as the extension direction of the second-stage groove 1311d, and the width direction of the first-stage groove 1311c is the same as the width direction of the second-stage groove 1311d. If the first groove section 1311 is a groove extending along a straight trajectory, the first-stage groove 1311c and the second-stage groove 1311d are both grooves extending along a straight trajectory. If the first groove section 1311 is a groove extending along an arcuate trajectory, the first-stage groove 1311c and the second-stage groove 1311d are both grooves extending along an arcuate trajectory. Along the depth direction of the first groove section 1311, the second-stage groove 1311d is located at the bottom of the first-stage groove 1311c. The bottom wall of the second-stage groove 1311d is the bottom wall of the first groove section 1311, and the bottom surface of the second-stage groove 1311d is the bottom surface of the first groove section 1311 (first groove bottom surface 1311a). As an example, along the thickness direction X of the pressure relief component, the pressure relief component 13 has a first surface 132 and a second surface 133 facing each other. The first-stage groove 1311c and the second-stage groove 1311d are arranged in sequence in a direction from the first surface 132 to the second surface 133. The distance between the bottom surface of the second-stage groove 1311d and the second surface 133 is D1.
[0192] Among them, the groove bottom surface of the first-stage groove 1311c and the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312b) can be flush, or they can be staggered along the thickness direction X of the pressure relief component. For example, along the thickness direction X of the pressure relief component, the groove bottom surface of the first-stage groove 1311c is closer to the second surface 133 than the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312b).
[0193] During molding, the first-level groove 1311c can be formed on the pressure relief component 13 first, and then the second-level groove 1311d can be formed on the bottom surface of the first-level groove 1311c to form the first groove section 1311. In this way, the molding depth of each level groove in the first groove section 1311 can be reduced, the molding force applied to the pressure relief component 13 when molding the first groove section 1311 can be reduced, and the possibility of cracks in the pressure relief component 13 when molding the first groove section 1311 can be reduced.
[0194] In some embodiments, please continue to refer to FIG. 12 , the bottom surface of the first-stage groove 1311 c is flush with the bottom surface of the second groove section 1312 (the second groove bottom surface 1312 b ).
[0195] As an example, the groove bottom surface of the first-stage groove 1311 c and the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312 b ) are both planes, and both are located in the same plane.
[0196] In this embodiment, the bottom surface of the first-level groove 1311c is flush with the bottom surface of the second groove section 1312 (the second groove bottom surface 1312b), so that the bottom surface of the first-level groove 1311c is coplanar with the bottom surface of the second groove section 1312 (the second groove bottom surface 1312b). During molding, the first-level groove 1311c of the first groove section 1311 and the second groove section 1312 can be molded together, and then the second-level groove 1311d of the first groove section 1311 can be molded, thereby improving the molding efficiency of the groove portion 131.
[0197] In some embodiments, please refer to FIG. 13 , which is a partial cross-sectional view of a pressure relief component 13 provided in another embodiment of the present application. Along the thickness direction X of the pressure relief component 13 , the pressure relief component 13 has opposing first and second surfaces 132 and 133 . The first-stage groove 1311 c and the second-stage groove 1311 d are sequentially arranged in a direction from the first surface 132 to the second surface 133 . The bottom surface of the second-stage groove 1311 d (the first bottom surface 1311 a ) is closer to the second surface 133 than the bottom surface of the second groove segment 1312 (the second bottom surface 1312 b ). The bottom surface of the second-stage groove 1311 d (the first bottom surface 1311 a ) and the bottom surface of the second groove segment 1312 (the second bottom surface 1312 b ) are connected by a first inclined plane (not shown in FIG. 13 ) or a first arcuate surface 1311 e .
[0198] The groove bottom surface (first groove bottom surface 1311a) of the second-stage groove 1311d and the groove bottom surface (second groove bottom surface 1312b) of the second groove segment 1312 can be connected by a first inclined plane or by a first arcuate surface 1311e. In the embodiment shown in FIG13 , the groove bottom surface (first groove bottom surface 1311a) of the second-stage groove 1311d and the groove bottom surface (second groove bottom surface 1312b) of the second groove segment 1312 are connected by a first arcuate surface 1311e. As an example, the groove bottom surface (first groove bottom surface 1311a) of the second-stage groove 1311d is parallel to the groove bottom surface (second groove bottom surface 1312b) of the second groove segment 1312, the first arcuate surface 1311e is tangent to the groove bottom surface (second groove bottom surface 1312b) of the second groove segment 1312, and the first arcuate surface 1311e is a groove side surface of the second-stage groove 1311d.
[0199] During pressure relief, after the pressure relief component 13 cracks at the detonation position 1314, the cracks on the bottom surface of the second-stage groove 1311d can quickly spread along the first inclined plane or the first arc surface 1311e to the bottom surface of the second groove section 1312, thereby reducing the time for the cracks to spread from the first groove section 1311 to the second groove section 1312, and further shortening the time for the pressure relief component 13 to crack along the groove portion 131.
[0200] In some embodiments, referring to Figures 8 and 14 , Figure 14 is a partial enlarged view of point F of the pressure relief component 13 shown in Figure 11 . The third slot segment 1313 is formed with an initiation location 1314 (shown in Figures 5 and 10 ), and the residual thickness of the third slot segment 1313 is less than the residual thickness of the second slot segment 1312.
[0201] The residual thickness of the third groove section 1313 is the thickness of the remaining portion of the pressure relief component 13 after the third groove section 1313 is provided. This remaining portion may be the bottom wall of the third groove section 1313. The thickness of the bottom wall of the third groove section 1313 may be uniform or non-uniform. If the thickness of the bottom wall of the third groove section 1313 is non-uniform, the thickness of the thinnest portion of the bottom wall of the third groove section 1313 is considered the residual thickness of the third groove section 1313.
[0202] The residual thickness of the second slot segment 1312 is D2, and the residual thickness of the third slot segment 1313 is D3. It can be understood that D3<D2.
[0203] In this embodiment, the residual thickness of the third slot segment 1313 is smaller than that of the second slot segment 1312, allowing the initiation location 1314 to be formed near the junction of the second and third slot segments 1312, 1313. During pressure relief, after the pressure relief component 13 cracks at the initiation location 1314, the crack propagates along the third slot segment 1313 while also propagating along the second slot segment 1312. Because the residual thickness of the third slot segment 1313 is smaller than that of the second slot segment 1312, the residual thickness of the second slot segment 1312 is increased, thereby improving the fatigue strength of the pressure relief component 13 in the region where the second slot segment 1312 is located, and further reducing the possibility of the pressure relief component 13 cracking in the region of the second slot segment 1312 during normal use of the battery cell 10. In addition, since the first groove section 1311 and the third groove section 1313 are both formed with a detonation position 1314, when the internal pressure of the battery cell 10 reaches the detonation pressure, the detonation positions 1314 of the first groove section 1311 and the third groove section 1313 can both crack, so that the crack spreads from the two ends of the second groove section 1312 to the middle position while spreading along the first groove section 1311 and the third groove section 1313, shortening the time for the pressure relief component 13 to crack along the groove portion 131.
[0204] In some embodiments, the residual thickness of the third slot segment 1313 is equal to the residual thickness of the first slot segment 1311 .
[0205] As can be understood, D1 = D3 . As an example, the depth of the first slot segment 1311 is equal to the depth of the third slot segment 1313 , so that the residual thickness of the first slot segment 1311 is equal to the residual thickness of the third slot segment 1313 .
[0206] When the battery cell 10 releases pressure, the pressure relief component 13 has better synchronization when it breaks along the first groove section 1311 and the third groove section 1313, further shortening the time for the pressure relief component 13 to break along the groove portion 131 and improving the timeliness of pressure relief.
[0207] In some embodiments, the residual thickness of the second slot segment 1312 is D2, and the residual thickness of the third slot segment 1313 is D3, satisfying: 0.15≤D3 / D2≤0.95.
[0208] D3 / D2 can be any point value of 0.15, 0.2, 0.25, 0.3, 0.35, 0.4, 0.45, 0.5, 0.55, 0.6, 0.65, 0.7, 0.75, 0.8, 0.85, 0.9, 0.95, etc., or a range of values between any two of them.
[0209] As can be seen from Table 1 above, when D3 / D2 is less than 0.15, the timely pressure relief is poor, and the battery cell 10 is more likely to explode during thermal runaway. When D3 / D2 is greater than 0.95, the pressure relief component 13 is more likely to crack along the second groove section 1312 during normal use of the battery cell 10, shortening the service life of the battery cell 10. However, when 0.15≤D3 / D2≤0.95, the timely pressure relief of the battery cell 10 is improved, and the service life of the battery cell 10 is also increased.
[0210] In some embodiments, 0.3≤D3 / D2≤0.9.
[0211] In this embodiment, D3 / D2 can be any one of the point values of 0.3, 0.32, 0.35, 0.38, 0.4, 0.42, 0.45, 0.48, 0.5, 0.52, 0.55, 0.58, 0.6, 0.62, 0.65, 0.68, 0.7, 0.72, 0.75, 0.78, 0.8, 0.82, 0.85, 0.88, 0.9, etc., or a range value between any two of them.
[0212] It can be seen from Table 1 above that when 0.3≤D3 / D2≤0.9, the performance of the battery cell 10 is better, and the timeliness of pressure release of the battery cell 10 and the service life of the battery cell 10 can be improved.
[0213] In some embodiments, 0.5≤D3D2≤0.85.
[0214] In this embodiment, D3 / D2 can be any one of the point values of 0.5, 0.52, 0.53, 0.55, 0.57, 0.58, 0.59, 0.6, 0.62, 0.63, 0.65, 0.67, 0.68, 0.69, 0.7, 0.72, 0.73, 0.75, 0.77, 0.78, 0.79, 0.8, 0.82, 0.83, 0.85, etc., or a range value between any two of them.
[0215] As can be seen from Table 1 above, when 0.5≤D3 / D2≤0.85, the overall performance of the battery cell 10 is further improved. This can not only control the probability of the pressure relief component 13 cracking along the second groove section 1312 during normal use of the battery cell 10 to a low level, but also control the probability of the battery cell 10 exploding during thermal runaway to a low level.
[0216] In some embodiments, 0.03 mm ≤ D3 ≤ 0.5 mm.
[0217] In this embodiment, D3 can be any point value of 0.03mm, 0.1mm, 0.15mm, 0.2mm, 0.25mm, 0.3mm, 0.35mm, 0.4mm, 0.45mm, 0.5mm, etc., or a range value between any two of them.
[0218] In some embodiments, 0.15 mm ≤ D3 ≤ 0.4 mm.
[0219] In this embodiment, D3 can be any point value of 0.15mm, 0.18mm, 0.2mm, 0.22mm, 0.25mm, 0.28mm, 0.3mm, 0.32mm, 0.35mm, 0.38mm, 0.4mm, etc., or a range value between any two of them.
[0220] In some embodiments, the depth of the third slot segment 1313 is greater than the depth of the second slot segment 1312 , such that the residual thickness of the third slot segment 1313 is less than the residual thickness of the second slot segment 1312 .
[0221] As an example, along the thickness direction X of the pressure relief component, the pressure relief component 13 includes a first surface 132 and a second surface 133 disposed opposite each other. A first groove section 1311 and a second groove section 1312 are disposed on the first surface 132. The first surface 132 and the second surface 133 may be parallel planes. The distance between the first surface 132 and the second surface 133 is H0. The distance between the groove bottom surface of the third groove section 1313 (the third groove bottom surface 1313a) and the second surface 133 is D3. The distance between the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312b) and the second surface 133 is D2. The depth of the third groove section 1313 is H0-D3, and the depth of the second groove section 1312 is H0-D2, where H0-D3>H0-D2. H0 may be the thickness of the pressure relief component 13. The third groove bottom surface 1313a may be a flat surface or an arcuate surface.
[0222] During molding, the third groove section 1313 can be processed deeper than the second groove section 1312 on the pressure relief component 13, so that the residual thickness of the third groove section 1313 is smaller than the residual thickness of the second groove section 1312, and the implementation method is simple.
[0223] In some embodiments, please continue to refer to Figure 14, the third groove section 1313 includes a third-level groove 1313c and a fourth-level groove 1313d, the third-level groove 1313c and the fourth-level groove 1313d are arranged along the thickness direction X of the pressure relief component, and the fourth-level groove 1313d is set on the groove bottom surface of the third-level groove 1313c.
[0224] The third groove section 1313 can be a two-stage groove, one of which is a third-stage groove 1313c and the other is a fourth-stage groove 1313d. The extension direction of the third-stage groove 1313c is the same as the extension direction of the fourth-stage groove 1313d, and the width direction of the third-stage groove 1313c is the same as the width direction of the fourth-stage groove 1313d. If the third groove section 1313 is a groove extending along a straight trajectory, the third-stage groove 1313c and the fourth-stage groove 1313d are both grooves extending along a straight trajectory. If the third groove section 1313 is a groove extending along an arcuate trajectory, the third-stage groove 1313c and the fourth-stage groove 1313d are both grooves extending along an arcuate trajectory. Along the depth direction of the third groove section 1313, the fourth-stage groove 1313d is located at the bottom of the third-stage groove 1313c. The bottom wall of the fourth-stage groove 1313d is the bottom wall of the third groove section 1313, and the bottom surface of the fourth-stage groove 1313d is the bottom surface of the third groove section 1313 (third groove bottom surface 1313a). As an example, along the thickness direction X of the pressure relief component, the pressure relief component 13 has a first surface 132 and a second surface 133 facing each other. The third-stage groove 1313c and the fourth-stage groove 1313d are arranged in sequence in a direction from the first surface 132 to the second surface 133. The distance between the bottom surface of the fourth-stage groove 1313d and the second surface 133 is D3.
[0225] Among them, the groove bottom surface of the third-level groove 1313c can be flush with the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312b), or can be staggered along the thickness direction X of the pressure relief component. For example, along the thickness direction X of the pressure relief component, the groove bottom surface of the third-level groove 1313c is closer to the second surface 133 than the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312b).
[0226] During molding, the third-level groove 1313c can be formed on the pressure relief component 13 first, and then the fourth-level groove 1313d can be formed on the bottom surface of the third-level groove 1313c to form the third groove section 1313. In this way, the molding depth of each level groove in the third groove section 1313 can be reduced, the molding force applied to the pressure relief component 13 when molding the third groove section 1313 can be reduced, and the possibility of cracks in the pressure relief component 13 when molding the third groove section 1313 can be reduced.
[0227] In some embodiments, the groove bottom surface of the third-level groove 1313 c is flush with the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312 b ).
[0228] As an example, the groove bottom surface of the third-stage groove 1313 c and the groove bottom surface of the second groove section 1312 (the second groove bottom surface 1312 b ) are both planes, and both are located in the same plane.
[0229] In this embodiment, the bottom surface of the third groove 1313c is flush with the bottom surface of the second groove section 1312 (the second groove bottom surface 1312b), so that the bottom surface of the third groove 1313c is coplanar with the bottom surface of the second groove section 1312 (the second groove bottom surface 1312b). During molding, the third groove 1313c of the third groove section 1313 and the second groove section 1312 can be molded together, and then the fourth groove 1313d of the third groove section 1313 can be molded, thereby improving the molding efficiency of the groove portion 131.
[0230] In some embodiments, please refer to FIG15 , which is a partial cross-sectional view of a pressure relief component 13 provided in yet other embodiments of the present application. Along the thickness direction X of the pressure relief component, the pressure relief component 13 has a first surface 132 and a second surface 133 facing each other. The third-stage groove 1313c and the fourth-stage groove 1313d are sequentially arranged in a direction from the first surface 132 to the second surface 133. The bottom surface of the fourth-stage groove 1313d is closer to the second surface 133 than the bottom surface of the second groove segment 1312. The bottom surface of the fourth-stage groove 1313d (the third bottom surface 1313a) is connected to the bottom surface of the second groove segment 1312 (the second bottom surface 1312b) via a second inclined plane or a second arc surface 1313e.
[0231] The groove bottom surface (third groove bottom surface 1313a) of the fourth-stage groove 1313d and the groove bottom surface (second groove bottom surface 1312b) of the second groove segment 1312 can be connected by a second inclined plane or by a second arcuate surface 1313e. In the embodiment shown in FIG14 , the groove bottom surface (third groove bottom surface 1313a) of the fourth-stage groove 1313d and the groove bottom surface (second groove bottom surface 1312b) of the second groove segment 1312 are connected by a second arcuate surface 1313e. As an example, the groove bottom surface (third groove bottom surface 1313a) of the fourth-stage groove 1313d is parallel to the groove bottom surface (second groove bottom surface 1312b) of the second groove segment 1312, the second arcuate surface 1313e is tangent to the groove bottom surface (second groove bottom surface 1312b) of the second groove segment 1312, and the second arcuate surface 1313e is a groove side surface of the fourth-stage groove 1313d.
[0232] During pressure relief, after the pressure relief component 13 cracks at the detonation position 1314, the cracks on the bottom surface of the fourth-level groove 1313d can quickly spread along the second inclined plane or the second arc surface 1313e to the bottom surface of the second groove section 1312, thereby reducing the time for the cracks to spread from the third groove section 1313 to the second groove section 1312, and further shortening the time for the pressure relief component 13 to crack along the groove portion 131.
[0233] In some embodiments, please refer to Figures 5, 10, and 16. Figure 16 is a partial view of the pressure relief component 13 provided in other embodiments of the present application. Along the extension direction of the second slot segment 1312, the two ends of the second slot segment 1312 are respectively connected to the first slot segment 1311 and the third slot segment 1313.
[0234] Along the extension direction of second slot segment 1312, one end of second slot segment 1312 connects to first slot segment 1311 at a first position 1315, and the other end of second slot segment 1312 connects to third slot segment 1313 at a second position 1316. For example, detonation position 1314 on first slot segment 1311 is located near first position 1315, and detonation position 1314 on third slot segment 1313 is located near second position 1316.
[0235] In this embodiment, the two ends of the second slot segment 1312 are respectively connected to the first slot segment 1311 and the third slot segment 1313, and the two ends of the second slot segment 1312 do not extend beyond the first slot segment 1311 and the third slot segment 1313 respectively. During the pressure relief process, the pressure can be accurately relieved through the area defined by the first slot segment 1311, the second slot segment 1312 and the third slot segment 1313, which is not likely to cause cracking and pressure relief in other areas of the pressure relief component 13, and it is easier to achieve directional pressure relief.
[0236] In some embodiments, the first slot segment 1311 and the second slot segment 1312 are connected at a first position 1315 . Along the extension direction of the first slot segment 1311 , the first position 1315 deviates from both ends of the first slot segment 1311 .
[0237] The first position 1315 is offset from both ends of the first slot segment 1311. That is, the first position 1315 is not located at either end of the first slot segment 1311. Along the extension direction of the first slot segment 1311, the first position 1315 is located between the two ends of the first slot segment 1311. The first position 1315 can be located at the midpoint of the first slot segment 1311 or offset from the midpoint of the first slot segment 1311.
[0238] During the pressure relief process, after the pressure relief component 13 cracks at the first position 1315 , the crack can spread from the first position 1315 to both ends along the first slot section 1311 , shortening the time it takes for the pressure relief component 13 to crack along the first slot section 1311 .
[0239] In some embodiments, along the extension direction of the first slot segment 1311 , the first position 1315 is located at the midpoint of the first slot segment 1311 .
[0240] Along the extension direction of the first slot segment 1311 , the first position 1315 can divide the first slot segment 1311 into two parts, and the two parts have the same length.
[0241] As an example, along the extension direction of the first slot segment 1311 , the detonation position 1314 on the first slot segment 1311 is located at the midpoint of the first slot segment 1311 .
[0242] It should be noted that, in the embodiment where the first slot segment 1311 includes the first-level slot 1311c and the second-level slot 1311d, along the extension direction of the first slot segment 1311, the two ends of the first-level slot 1311c are the two ends of the first slot segment 1311, and the midpoint of the first-level slot 1311c is the midpoint of the first slot segment 1311.
[0243] In this embodiment, the first position 1315 is located at the midpoint of the first slot section 1311. During the pressure relief process, the crack spreads from the first position 1315 to both ends along the first slot section 1311 at an equal distance, further shortening the time for the pressure relief component 13 to crack along the first slot section 1311.
[0244] In some embodiments, the third slot segment 1313 is connected to the second slot segment 1312 at a second position 1316 . Along the extension direction of the third slot segment 1313 , the second position 1316 deviates from both ends of the third slot segment 1313 .
[0245] The second position 1316 is offset from both ends of the third slot segment 1313. That is, the second position 1316 is not located at either end of the third slot segment 1313. Along the extension direction of the third slot segment 1313, the second position 1316 is located between the two ends of the third slot segment 1313. The second position 1316 can be located at the midpoint of the third slot segment 1313 or offset from the midpoint of the third slot segment 1313.
[0246] When the first position 1315 deviates from the two ends of the first slot section 1311 and the second position 1316 deviates from the two ends of the third slot section 1313, the first slot section 1311, the second slot section 1312 and the third slot section 1313 will jointly define two pressure relief areas 134. The two pressure relief areas 134 are located on both sides of the second slot section 1312. During the pressure relief process, both pressure relief areas 134 can be opened, which can effectively improve the timeliness of pressure relief.
[0247] During the pressure relief process, after the pressure relief component 13 cracks at the second position 1316 , the crack can spread from the second position 1316 to both ends along the third slot section 1313 , shortening the time it takes for the pressure relief component 13 to crack along the third slot section 1313 .
[0248] In some embodiments, along the extension direction of the third slot segment 1313 , the second position 1316 is located at the midpoint of the third slot segment 1313 .
[0249] Along the extension direction of the third slot segment 1313 , the second position 1316 can divide the third slot segment 1313 into two parts, and the two parts have the same length.
[0250] As an example, along the extension direction of the third slot segment 1313 , the detonation position 1314 on the third slot segment 1313 is located at the midpoint of the third slot segment 1313 .
[0251] It should be noted that, in the embodiment where the third slot segment 1313 includes a third-level slot 1313c and a fourth-level slot 1313d, along the extension direction of the third slot segment 1313, the two ends of the third-level slot 1313c are the two ends of the third slot segment 1313, and the midpoint of the third-level slot 1313c is the midpoint of the third slot segment 1313.
[0252] In this embodiment, the second position 1316 is located at the midpoint of the third slot section 1313. During the pressure relief process, the crack spreads from the second position 1316 to both ends along the third slot section 1313 at an equal distance, further shortening the time for the pressure relief component 13 to crack along the third slot section 1313.
[0253] In some embodiments, the first slot segment 1311 , the second slot segment 1312 , and the third slot segment 1313 are all slots extending along a straight line.
[0254] The first slot segment 1311, the second slot segment 1312, and the third slot segment 1313 are all linear slots. The first slot segment 1311 and the second slot segment 1312 can be perpendicular, or at an acute or obtuse angle. The third slot segment 1313 and the second slot segment 1312 can be perpendicular, or at an acute or obtuse angle. The lengths of the first slot segment 1311 and the third slot segment 1313 can be equal or unequal. In the embodiments shown in Figures 5, 10, and 16, the length of the first slot segment 1311 is equal to the length of the third slot segment 1313. In the embodiments shown in Figures 10 and 15, the length of the first-stage slot 1311c is equal to the length of the first slot segment 1311, and the length of the third-stage slot 1313c is equal to the length of the third slot segment 1313. As an example, the length of the first-stage slot 1311c is equal to the length of the third-stage slot 1313c, and the length of the second-stage slot 1311d is equal to the length of the fourth-stage slot 1313d.
[0255] In this embodiment, the first slot segment 1311 , the second slot segment 1312 and the third slot segment 1313 are all linear slots, which can reduce the difficulty of forming the first slot segment 1311 , the second slot segment 1312 and the third slot segment 1313 .
[0256] In some embodiments, the first slot segment 1311 is perpendicular to the second slot segment 1312 ; and / or the third slot segment 1313 is perpendicular to the second slot segment 1312 .
[0257] It is understood that, when the first slot segment 1311 is perpendicular to the second slot segment 1312, the third slot segment 1313 can be perpendicular to the second slot segment 1312, or the third slot segment 1313 and the second slot segment 1312 can be arranged at an acute or obtuse angle; when the third slot segment 1313 is perpendicular to the second slot segment 1312, the first slot segment 1311 can be perpendicular to the second slot segment 1312, or the first slot segment 1311 and the second slot segment 1312 can be arranged at an acute or obtuse angle. In the embodiments shown in Figures 5, 10, and 16, the first slot segment 1311 and the third slot segment 1313 are both perpendicular to the second slot segment 1312.
[0258] If the first groove section 1311 is perpendicular to the second groove section 1312, stress is more concentrated near the junction of the first and second groove sections 1311, 1312. If the detonation position 1314 is located near the junction of the first and second groove sections 1311, under a constant detonation pressure of the battery cell 10, the processing depth of the first groove section 1311 can be reduced, thereby reducing the difficulty of processing the first groove section 1311. If the third groove section 1313 is perpendicular to the second groove section 1312, stress is more concentrated near the junction of the third and second groove sections 1313, 1312. If the detonation position 1314 is located near the junction of the third and second groove sections 1313, 1312, under a constant detonation pressure of the battery cell 10, the processing depth of the third groove section 1313 can be reduced, thereby reducing the difficulty of processing the third groove section 1313.
[0259] 16 , the first slot section 1311, the second slot section 1312, and the third slot section 1313 define a pressure relief area 134. The pressure relief component 13 is provided with a guide groove 135, which is spaced apart from the second slot section 1312 and configured to guide the pressure relief area 134 to flip open.
[0260] The pressure relief zone 134 is the area defined by the first slot section 1311, the second slot section 1312 and the third slot section 1313 of the pressure relief component 13. The first slot section 1311, the second slot section 1312 and the third slot section 1313 are located at the edge of the pressure relief zone 134. The pressure relief zone 134 can flip outward and open during the process of the pressure relief component 13 splitting along the first slot section 1311, the second slot section 1312 and the third slot section 1313. The first slot section 1311, the second slot section 1312 and the third slot section 1313 can define a pressure relief zone 134. For example, the first slot section 1311, the second slot section 1312 and the third slot section 1313 are connected in sequence to form a U-shaped structure. The first slot section 1311, the second slot section 1312 and the third slot section 1313 can also define two pressure relief zones 134. For example, the first slot section 1311, the second slot section 1312 and the third slot section 1313 form an H-shaped structure.
[0261] In an embodiment in which the first slot section 1311, the second slot section 1312, and the third slot section 1313 are sequentially connected to form a U-shaped structure, a line connecting an end of the first slot section 1311 away from the second slot section 1312 and an end of the third slot section 1313 away from the second slot section 1312 is a first line, and an area enclosed by the first slot section 1311, the second slot section 1312, the third slot section 1313, and the first line is the pressure relief area 134. In an embodiment in which the first slot section 1311, the second slot section 1312, and the third slot section 1313 form an H-shaped structure, a line connecting one end of the first slot section 1311 and one end of the third slot section 1313 is a second line, a line connecting the other end of the first slot section 1311 and the other end of the third slot section 1313 is a third line, an area enclosed by the first slot section 1311, the second slot section 1312, the third slot section 1313, and the second line is one pressure relief area 134, and an area enclosed by the first slot section 1311, the second slot section 1312, the third slot section 1313, and the third line is another pressure relief area 134.
[0262] The guide groove 135 is a groove provided on the pressure relief component 13 to facilitate the pressure relief area 134 to flip open. The guide groove 135 can be a linear groove or a non-linear groove, such as an arc groove. As an example, the guide groove 135 is a linear groove parallel to the second groove section 1312.
[0263] As an example, the residual thickness of the first slot segment 1311 and the residual thickness of the third slot segment 1313 are both smaller than the residual thickness of the guide slot 135 .
[0264] In this embodiment, the provision of the guide groove 135 helps the pressure relief area 134 to flip open, reduces the difficulty of flipping the pressure relief area 134, and can effectively improve the timeliness of pressure relief.
[0265] 16 , the first slot section 1311, the second slot section 1312, and the third slot section 1313 define two pressure relief areas 134, with the two pressure relief areas 134 located on either side of the second slot section 1312. The pressure relief component 13 is provided with two guide grooves 135, with the second slot section 1312 located between the two guide grooves 135. The two guide grooves 135 are configured to guide the two pressure relief areas 134 to flip open.
[0266] The areas of the two pressure relief zones 134 can be equal or different. As an example, the two pressure relief zones 134 are symmetrically distributed on both sides of the second slot segment 1312. In the embodiment shown in Figure 16, the first slot segment 1311, the second slot segment 1312, and the third slot segment 1313 are all linear slots. The first slot segment 1311 is parallel to the third slot segment 1313, the first slot segment 1311 is perpendicular to the second slot segment 1312, the length of the first slot segment 1311 is equal to the length of the third slot segment 1313, and the second slot segment 1312 is connected to the midpoint of the first slot segment 1311 and the midpoint of the third slot segment 1313, so that the two pressure relief zones 134 are symmetrically distributed on both sides of the second slot segment 1312.
[0267] As an example, the two guide grooves 135 are parallel to the second groove section 1312 , the distances between the two guide grooves 135 and the second groove section 1312 are equal, and the two guide grooves 135 are symmetrically distributed on both sides of the second groove section 1312 .
[0268] During the pressure relief process, the two guide grooves 135 can guide the two pressure relief areas 134 respectively, thereby increasing the opening rate of the two pressure relief areas 134 and releasing pressure more timely.
[0269] In some embodiments, the first slot segment 1311 and the third slot segment 1313 are not in contact with the guide slot 135 .
[0270] First slot section 1311 does not contact guide groove 135, that is, first slot section 1311 is not connected to guide groove 135. First slot section 1311 and guide groove 135 may be spaced apart to achieve non-contact. For example, along the extension direction of first slot section 1311, first slot section 1311 and guide groove 135 are spaced apart; and / or along the extension direction of guide groove 135, first slot section 1311 and guide groove 135 are spaced apart; and / or along the thickness direction X of the pressure relief component, first slot section 1311 and guide groove 135 are spaced apart. Third slot section 1313 does not contact guide groove 135, that is, third slot section 1313 is not connected to guide groove 135. The third slot section 1313 and the guide groove 135 may be spaced apart from each other so as to achieve non-contact between the two. For example, along the extension direction of the third slot section 1313, the third slot section 1313 and the guide groove 135 are spaced apart from each other; and / or, along the extension direction of the guide groove 135, the third slot section 1313 and the guide groove 135 are spaced apart from each other; and / or, along the thickness direction X of the pressure relief component, the third slot section 1313 and the guide groove 135 are spaced apart from each other.
[0271] In this embodiment, the first and third groove sections 1311, 1313 do not contact the guide grooves 135. Therefore, the guide grooves 135 are less likely to affect the first and third groove sections 1311, 1313. This improves the fatigue strength of the pressure relief component 13 at the first and third groove sections 1311, 1313, and reduces the likelihood of stress concentration caused by the connection between the guide grooves 135, the first and third groove sections 1311, 1313, and cracking of the pressure relief component 13 at the connection during normal use of the battery cell 10. Furthermore, during the pressure relief process, after the pressure relief component 13 cracks along the first and third groove sections 1311, 1313, the cracks are less likely to spread to the guide grooves 135, reducing the likelihood of the pressure relief component 13 detaching and splashing after the pressure relief area 134 opens.
[0272] In some embodiments, please refer to Figure 17, which is a GG cross-sectional view of the pressure relief component 13 shown in Figure 16. Along the thickness direction X of the pressure relief component, the guide groove 135 and the groove portion 131 are respectively provided on both sides of the pressure relief component 13.
[0273] During molding, along the thickness direction X of the pressure relief component, a guide groove 135 can be formed on one side of the pressure relief component 13, and a groove portion 131 can be formed on the other side of the pressure relief component 13. In some embodiments, the groove portion 131 faces the exterior of the housing 1, and the guide groove 135 faces the interior of the housing 1. In other embodiments, the groove portion 131 faces the interior of the housing 1, and the guide groove 135 faces the exterior of the housing 1.
[0274] As an example, along the thickness direction X of the pressure relief component, the pressure relief component 13 includes a first surface 132 and a second surface 133 disposed opposite each other. The groove portion 131 may be disposed on the first surface 132, and the guide groove 135 may be disposed on the second surface 133. It is understood that the first groove section 1311, the second groove section 1312, and the third groove section 1313 are all disposed on the first surface 132.
[0275] In this embodiment, the guide groove 135 and the groove portion 131 are respectively arranged on both sides of the pressure relief component 13. On the one hand, the influence of the guide groove 135 on the groove portion 131 during molding is reduced; on the other hand, the guide groove 135 can produce a better guiding effect on the pressure relief area 134, making the pressure relief area 134 easier to flip open.
[0276] In some embodiments, please continue to refer to 16 , the guide groove 135 extends along the extension direction of the second groove section 1312 .
[0277] It is understood that the extension direction of the guide groove 135 is consistent with the extension direction of the second groove segment 1312. In some embodiments, the guide groove 135 and the second groove segment 1312 are grooves extending along an arcuate trajectory. When viewed along the thickness direction X of the pressure relief component, the center of the arcuate trajectory of the guide groove 135 coincides with the center of the arcuate trajectory of the second groove segment 1312. In other embodiments, as shown in FIG16 , the guide groove 135 and the second groove segment 1312 are grooves extending along a straight trajectory, with the guide groove 135 parallel to the second groove segment 1312.
[0278] In some embodiments, along the extension direction of the second slot segment 1312, the first slot segment 1311 and the third slot segment 1313 are respectively located on both sides of the guide groove 135, the length of the portion of the second slot segment 1312 located between the first slot segment 1311 and the third slot segment 1313 is L1, and the length of the guide groove 135 is L2, satisfying: 1mm≤L1-L2≤10mm.
[0279] Along the extension direction of second slot segment 1312, one end of guide slot 135 is spaced apart from first slot segment 1311, with a distance therebetween. The other end of guide slot 135 is spaced apart from third slot segment 1313, with a distance therebetween. For example, along the extension direction of second slot segment 1312, the distance between one end of guide slot 135 and first slot segment 1311 is equal to the distance between the other end of guide slot 135 and third slot segment 1313.
[0280] L1-L2 can be any point value of 1mm, 2mm, 3mm, 4mm, 5mm, 6mm, 7mm, 8mm, 9mm, 10mm, etc., or a range value between any two of them.
[0281] If L1-L2 is less than 1 mm, the distance between at least one of the first groove section 1311 and the third groove and the guide groove 135 is small, and the guide groove 135 has a significant impact on the first and third groove sections 1311, 1313. This can easily lead to premature cracking of the pressure relief component 13 near the guide groove 135 in the first or third groove section 1311, 1313, increasing the likelihood of premature pressure release. If L1-L2 is greater than 10 mm, the length of the guide groove 135 is too short, and the guide groove 135's ability to assist the pressure relief area 134 in its rotation is less effective. A value of 1 mm ≤ L1-L2 ≤ 10 mm can reduce the likelihood of premature pressure release of the pressure relief component 13 while improving the guide groove 135's ability to assist the pressure relief area 134 in its rotation and opening.
[0282] In some embodiments, 2 mm ≤ L1 - L2 ≤ 6 mm.
[0283] In this embodiment, L1-L2 can be any point value of 2mm, 2.3mm, 2.5mm, 2.8mm, 3mm, 3.3mm, 3.5mm, 3.8mm, 4mm, 4.3mm, 4.5mm, 4.8mm, 5mm, 5.3mm, 5.5mm, 5.8mm, 6mm, etc., or a range value between any two of them.
[0284] In this embodiment, 2 mm ≤ L1 - L2 ≤ 6 mm, which further reduces the possibility of premature pressure relief of the pressure relief component 13 and further improves the guiding ability of the guide groove 135 to help the pressure relief area 134 flip open.
[0285] In some embodiments, along the extension direction of the first slot segment 1311, the distance between the guide slot 135 and the second slot segment 1312 is L3, and the length L4 of the part of the first slot segment 1311 extending from the second slot segment 1312 toward the guide slot 135 is 0.5mm≤|L3-L4|≤15mm.
[0286] The distance between the guide groove 135 and the second groove section 1312 is equal to the length of the shortest line connecting the guide groove 135 and the second groove section 1312 , and the shortest line is consistent with the extending direction of the first groove section 1311 .
[0287] It can be L3>L4, or L4>L3. In the embodiment of L3>L4, the guide groove 135 is more helpful for the pressure relief area 134 to flip open.
[0288] |L3-L4| can be any point value of 0.5mm, 1mm, 2mm, 3mm, 4mm, 5mm, 6mm, 7mm, 8mm, 9mm, 10mm, 11mm, 12mm, 13mm, 14mm, 15mm, etc., or a range value between any two of them.
[0289] If |L3-L4| is less than 0.5 mm, the distance between the end of the first groove section 1311 and the guide groove 135 is small. When a crack in the pressure relief component 13 propagates along the first groove section 1311 to the end of the first groove section 1311, the crack easily propagates to the guide groove 135, causing the pressure relief area 134 to detach. If |L3-L4| is greater than 15 mm, when L3 is greater than L4, the distance between the guide groove 135 and the second groove section 1312 is large, and the guide groove 135's ability to assist the pressure relief area 134 in flipping is poor. When L3 is less than L4, the distance between the guide groove 135 and the second groove section 1312 is small, resulting in a smaller area for the pressure relief area 134 to flip open, and the pressure relief area of the pressure relief area 134 is reduced. When 0.5 mm ≤ |L3-L4| ≤ 15 mm, the possibility of the pressure relief area 134 detaching and splashing is reduced, while also increasing the difficulty of flipping and opening the pressure relief area 134 and the opening area of the pressure relief area 134.
[0290] In some embodiments, 1 mm ≤ |L3-L4| ≤ 10 mm.
[0291] In this embodiment, |L3-L4| can be any point value of 1mm, 1.5mm, 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm, 5mm, 5.5mm, 6mm, 6.5mm, 7mm, 7.5mm, 8mm, 8.5mm, 9mm, 9.5mm, 10mm, etc., or a range value between any two of them.
[0292] In some embodiments, please refer to FIG18 , which is an exploded view of the housing 1 provided in some embodiments of the present application. The housing 1 includes a first wall portion 14 , and the pressure relief component 13 (not shown in FIG18 ) is the first wall portion 14 .
[0293] The housing 1 may include multiple walls that collectively define the interior space of the housing 1. For example, if the housing 1 is a rectangular parallelepiped, the housing 1 may have six walls, with the housing 1 having two opposing walls in the length direction, two opposing walls in the width direction, and two opposing walls in the height direction.
[0294] In the housing 1, at least one wall portion is the first wall portion 14, that is, at least one wall portion is provided with a groove portion 131. Taking the housing 1 including the shell 11 and the end cover 12 as an example, the end cover 12 is a wall portion in the housing 1. The end cover 12 can be the first wall portion 14, or at least one wall portion in the shell 11 can be the first wall portion 14.
[0295] It is understood that the groove 131 is provided on the first wall portion 14. The groove 131 may face the inside of the housing 1 or the outside of the housing 1.
[0296] In this embodiment, the first wall portion 14 serves as the pressure relief component 13 , and the groove portion 131 can be directly formed on the first wall portion 14 to form an integrated pressure relief structure, which has higher reliability, eliminates the installation process of the pressure relief component 13 , and can reduce the production cost of the battery cell 10 .
[0297] In some embodiments, please refer to FIG19 , which is an exploded view of the housing 1 provided in some other embodiments of the present application. The housing 1 includes a first wall portion 14 , and a pressure relief component 13 is provided separately from the first wall portion 14 . The pressure relief component 13 is installed on the first wall portion 14 .
[0298] The pressure relief component 13 and the housing 1 are two separate components that are molded separately and then assembled together. The pressure relief component 13 can be mounted to the first wall portion 14 by welding, bonding, or the like. As an example, the first wall portion 14 is provided with a pressure relief hole 141, and the pressure relief component 13 covers the pressure relief hole 141.
[0299] In this embodiment, the pressure relief component 13 is installed on the first wall portion 14. The pressure relief component 13 is a component independent of the housing 1. The pressure relief component 13 and the housing 1 can be produced and assembled separately, with low production difficulty and high efficiency.
[0300] 18 and 19 , the housing 1 includes a shell 11 and an end cap 12 . The shell 11 has an opening, and the end cap 12 closes the opening. At least one wall portion of the shell 11 is a first wall portion 14 .
[0301] The housing 11 may include multiple walls defining an interior space of the housing 11. In the housing 11, one wall may be the first wall 14, or multiple walls may be the first wall 14. As an example, in FIG. 18 and FIG. 19 , only one wall of the housing 11 is the first wall 14.
[0302] In this embodiment, the housing 11 has a pressure relief function. During pressure relief, the exhaust from the interior of the battery cell 10 is less likely to affect the external components outside the end cap 12, thereby reducing the possibility of damage to the external components by the exhaust. The external components referred to here may be components located outside the battery cell 10 and connected to the electrode terminals 3 on the end cap 12.
[0303] 18 and 19 , the housing 11 includes a bottom wall 111 and a plurality of side walls 112 . The side walls 112 surround the bottom wall 111 , and the housing 11 forms an opening at one end opposite the bottom wall 111 . The bottom wall 111 is the first wall portion 14 .
[0304] The bottom wall 111 is the wall portion of the housing 11 opposite the opening, and the side walls 112 are the wall portions of the housing 11 surrounding the bottom wall 111. The bottom wall 111 and the side walls 112 are integrally formed. The housing 11 may have three, four, five, six, or more side walls 112. As an example, in Figures 18 and 19, the housing 11 is rectangular and has four side walls 112.
[0305] In this embodiment, the bottom wall 111 has a pressure relief function. When the battery cell 10 experiences thermal runaway, pressure can be relieved through the bottom wall 111 . In the battery 100 , the pressure relief component 13 is not easily blocked by other battery cells 10 .
[0306] In some embodiments, referring to Figures 20 and 21 , Figure 20 is an exploded view of a housing 1 provided in yet another embodiment of the present application; Figure 21 is an exploded view of a housing 1 provided in yet another embodiment of the present application. The housing 1 includes a shell 11 and an end cap 12 . The shell 11 has an opening, and the end cap 12 closes the opening. The end cap 12 serves as a first wall portion 14 .
[0307] In the embodiment shown in FIG. 20 , the end cover 12 is a pressure relief component 13 .
[0308] In the embodiment shown in FIG. 21 , the pressure relief component 13 and the end cover 12 are two separate components, and the pressure relief component 13 is mounted on the end cover 12 .
[0309] In this embodiment, the end cover 12 has a pressure relief function, and the difficulty of forming the groove portion 131 on the end cover 12 is lower.
[0310] In some embodiments, the first wall portion 14 is a rectangular wall portion, the second slot segment 1312 extends along the length direction Y of the first wall portion, and the first slot segment 1311 and the third slot segment 1313 both extend along the width direction Z of the first wall portion.
[0311] It can be understood that the length of the first wall portion 14 is greater than the width of the first wall portion 14 , and the first slot segment 1311 and the third slot segment 1313 are both perpendicular to the second slot segment 1312 .
[0312] In this embodiment, the second slot section 1312 extends along the length direction Y of the first wall portion. The second wall portion can provide more space for the second slot section 1312, and the second slot section 1312 can be made longer, thereby increasing the pressure relief area of the pressure relief component 13.
[0313] In other embodiments, the second slot segment 1312 may extend along the width direction Z of the first wall portion, and the first slot segment 1311 and the third slot segment 1313 may extend along the length direction Y of the first wall portion.
[0314] In some embodiments, please refer to FIG. 22 , which is a partial view of the first wall portion provided in some embodiments of the present application. Along the thickness direction X of the pressure relief component (not shown in FIG. 22 ), the first wall portion 14 has an outer surface 142 , which faces away from the interior of the housing 1 . The first slot segment 1311 has a first midplane 1311f extending along its extension direction, the second slot segment 1312 has a second midplane 1312c extending along its extension direction, and the third slot segment 1313 has a third midplane 1313f extending along its extension direction. The minimum distance from the center point 1421 of the outer surface 142 to the first midplane 1311f is M1, the minimum distance from the center point 1421 of the outer surface 142 to the second midplane 1312c is M2, and the minimum distance from the center point 1421 of the outer surface 142 to the third midplane 1313f is M3, satisfying the following conditions: M2 < M1, M2 < M3.
[0315] Among them, M1 can be M3, M1<M3, or M1>M3.
[0316] In the embodiment where the first wall 14 serves as the pressure relief component 13, the thickness direction X of the pressure relief component is the thickness direction of the first wall 14. In the embodiment where the pressure relief component 13 is mounted on the first wall 14, the thickness direction X of the pressure relief component is consistent with the thickness direction of the first wall 14.
[0317] The outer surface 142 is the surface of the first wall portion 14 facing away from the interior of the housing 1; that is, the outer surface 142 faces the exterior of the housing 1. Along the thickness direction X of the pressure relief component, the first wall portion 14 also has an inner surface facing the interior of the housing 1. The first groove section 1311, the second groove section 1312, and the third groove section 1313 can all be recessed in a direction from the outer surface 142 of the first wall portion 14 toward the inner surface, or can be recessed in a direction from the inner surface of the first wall portion 14 toward the outer surface 142. In the embodiment where the first wall portion 14 serves as the pressure relief component 13, one of the inner surface and the outer surface 142 of the first wall portion 14 serves as the first surface 132 of the pressure relief component 13, and the other serves as the second surface 133 of the pressure relief component 13.
[0318] The center point 1421 of the outer surface 142 is the geometric center of the outer surface 142. The outer surface 142 can be circular, polygonal, etc. The polygon can be a triangle, a quadrilateral, a pentagon, a hexagon, etc.
[0319] The first midplane 1311f is aligned with the direction in which the first slot segment 1311 extends. In the width direction of the first slot segment 1311, the first midplane 1311f is centrally located within the first slot segment 1311, and is perpendicular to the width direction of the first slot segment 1311. In embodiments where the first slot segment 1311 is a multi-stage slot, the first midplane 1311f is centrally located within the deepest stage of the first slot segment 1311, in the width direction of the first slot segment 1311. The second midplane 1312c is aligned with the direction in which the second slot segment 1312 extends. In the width direction of the second slot segment 1312, the second midplane 1312c is centrally located within the second slot segment 1312, and is perpendicular to the width direction of the second slot segment 1312. In the embodiment where the second slot segment 1312 is a multi-stage slot, the second midplane 1312c is centered in the width direction of the second slot segment 1312 at the deepest primary slot in the second slot segment 1312. The third midplane 1313f extends in the same direction as the third slot segment 1313. In the width direction of the third slot segment 1313, the third midplane 1313f is centered in the third slot segment 1313, and is perpendicular to the width direction of the third slot segment 1313. In the embodiment where the third slot segment 1313 is a multi-stage slot, the third midplane 1313f is centered in the width direction of the third slot segment 1313 at the deepest primary slot in the third slot segment 1313.
[0320] The minimum distance from the center point 1421 of the outer surface 142 to the first mid-plane 1311f can be measured on a perpendicular line to the first mid-plane 1311f, which passes through the center point 1421 of the outer surface 142. The minimum distance from the center point 1421 of the outer surface 142 to the second mid-plane 1312c can be measured on a perpendicular line to the second mid-plane 1312c, which passes through the center point 1421 of the outer surface 142. The minimum distance from the center point 1421 of the outer surface 142 to the third mid-plane 1313f can be measured on a perpendicular line to the third mid-plane 1313f, which passes through the center point 1421 of the outer surface 142.
[0321] When the internal pressure of the battery cell changes, the closer the first wall portion 14 is to the center point 1421, the easier it is to deform, and M2 < M1, M2 < M3, so that the first groove section 1311 and the third groove section 1313 are farther away from the center point 1421, thereby improving the fatigue strength of the pressure relief component 13 at the first groove section 1311 and the third groove section 1313.
[0322] In some embodiments, along the thickness direction X of the pressure relief component, the projection of the center point 1421 of the outer surface 142 is located within the second groove section 1312 ; and / or, |M3−M1|≤5 mm.
[0323] Along the thickness direction of the pressure relief component 13, the projection of the center point 1421 is located in the second groove section 1312, that is, the perpendicular line of the outer surface 142 passing through the center point 1421 passes through the second groove section 1312. As an example, the center point 1421 of the outer surface 142 is located in the second midplane 1312c.
[0324] |M3-M1| can be any point value among 0mm, 1mm, 2mm, 3mm, 4mm, 5mm, etc., or a range value between any two.
[0325] In this embodiment, the projection of the center point 1421 of the outer surface 142 is located within the second groove section 1312. The second groove section 1312 is closer to the center point 1421 of the outer surface 142. This allows the pressure relief component 13 to rupture more promptly along the second groove section 1312 during pressure relief, thereby improving the timeliness of pressure relief. The |M3-M1| value is ≤ 5 mm, which means that the first and third groove sections 1311, 1313 are both farther from the center point 1421, reducing the impact of deformation of the pressure relief component 13 near the center point 1421 on the first and third groove sections 1311, 1313.
[0326] In some embodiments, the outer surface 142 is rectangular, circular, or a regular polygon.
[0327] In the embodiment where the outer surface 142 is rectangular, the intersection of the two diagonals of the rectangle is the center point 1421 of the outer surface 142. The first wall portion 14 is a rectangular wall portion, and the length direction of the outer surface 142 is consistent with the length direction Y of the first wall portion, and the width direction of the outer surface 142 is consistent with the width direction Z of the first wall portion. The outer surface 142 can be a regular rectangle or an irregular rectangle, for example, where two adjacent sides of the rectangle are connected by a chamfer, and the chamfer can be a circular arc chamfer.
[0328] In the embodiment where the outer surface 142 is circular, the center of the circle is the center point 1421 of the outer surface 142. The first wall portion 14 may be a circular wall portion to achieve the outer surface 142 being circular.
[0329] In the embodiment where outer surface 142 is a regular polygon, the center of the inscribed circle of the regular polygon is the center point 1421 of outer surface 142. Regular polygons may be regular triangles, regular quadrilaterals, regular pentagons, regular hexagons, etc. Outer surface 142 may be a regular regular polygon or an irregular regular polygon. For example, two adjacent sides of a regular polygon may be connected by a chamfer, which may be a circular chamfer. First wall portion 14 may be a regular polygonal wall portion to achieve outer surface 142 being a regular polygon.
[0330] An embodiment of the present application provides a battery 100 , comprising the battery cell 10 provided in any one of the above embodiments.
[0331] An embodiment of the present application provides an electrical device, comprising a battery cell 10 provided by any one of the above embodiments, and the battery cell 10 is used to provide electrical energy to the electrical device.
[0332] The present embodiment also provides a battery cell 10, comprising a housing 1 and an electrode assembly 2. The electrode assembly 2 has a positive tab and a negative tab, and the electrode assembly 2 is housed within the housing 1. The housing 1 is rectangular and includes a shell 11 and an end cap 12. The shell 11 has an opening, and the end cap 12 closes the opening. The end cap 12 is provided with a positive electrode terminal and a negative electrode terminal. The positive electrode terminal is electrically connected to the positive tab via a current collecting member 4, and the negative electrode terminal is electrically connected to the negative tab via another current collecting member 4. The wall of the housing 11 opposite the end cap 12 is a pressure relief component 13. The pressure relief component 13 is provided with a groove 131. The pressure relief component 13 is configured to rupture along the groove 131 to release pressure within the battery cell 10. The pressure relief component 13 has an initiation position 1314. The groove portion 131 includes a first groove section 1311, a second groove section 1312 and a third groove section 1313. The first groove section 1311 and the third groove section 1313 are arranged opposite to each other, and the second groove section 1312 connects the first groove section 1311 and the third groove section 1313. The first groove section 1311, the second groove section 1312 and the third groove section 1313 are all grooves extending along a straight line. The first groove section 1311 and the third groove section 1313 are both perpendicular to the second groove section 1312. One end of the second groove section 1312 is connected to the midpoint of the first groove section 1311, and the other end of the second groove section 1312 is connected to the midpoint of the third groove section 1313. The residual thickness of the first groove section 1311 and the residual thickness of the third groove section 1313 are both smaller than the residual thickness of the second groove section 1312, and the residual thickness of the first groove section 1311 is equal to the residual thickness of the third groove section 1313. The first slot section 1311 and the third slot section 1313 are both formed with a detonation position 1314. The residual thickness of the first slot section 1311 is D1, and the residual thickness of the second slot section 1312 is D2, 0.15≤D1 / D2≤0.95, 0.03mm≤D1≤0.5mm; 0.25mm≤D2≤0.5mm.
[0333] The first slot section 1311 includes a first-stage slot 1311c and a second-stage slot 1311d, which are arranged along the thickness direction X of the pressure relief component. The second-stage slot 1311d is provided on the bottom surface of the first-stage slot 1311c, and the bottom surface of the first-stage slot 1311c is flush with the bottom surface of the second slot section 1312. The third slot section 1313 includes a third-stage slot 1313c and a fourth-stage slot 1313d, which are arranged along the thickness direction X of the pressure relief component. The fourth-stage slot 1313d is provided on the bottom surface of the third-stage slot 1313c, and the bottom surface of the third-stage slot 1313c is flush with the bottom surface of the second slot section 1312.
[0334] It should be noted that, unless there is any conflict, the embodiments and features in the embodiments of this application can be combined with each other.
[0335] The above embodiments are intended only to illustrate the technical solutions of this application and are not intended to limit this application. Those skilled in the art will appreciate that various modifications and variations are possible. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of this application are intended to be within the scope of protection of this application.
Claims
1. A battery cell, comprising: The housing includes a pressure relief component, the pressure relief component is provided with a groove portion, the pressure relief component is configured to be able to be split along the groove portion to release the pressure inside the battery cell, and the pressure relief component has an explosion position; Wherein, the slot portion includes a first slot section, a second slot section and a third slot section, the first slot section is arranged opposite to the third slot section, the second slot section connects the first slot section and the third slot section, and the detonation position is formed in the first slot section and / or the third slot section.
2. The battery cell according to claim 1, wherein: The first slot segment is formed with the detonation position, and the residual thickness of the first slot segment is smaller than the residual thickness of the second slot segment.
3. The battery cell according to claim 2, wherein: The residual thickness of the first groove section is D1, and the residual thickness of the second groove section is D2, which satisfies: 0.15≤D1 / D2≤0.
95.
4. The battery cell according to claim 3, wherein: 0.3≤D1 / D2≤0.
9.
5. The battery cell according to claim 4, wherein: 0.5≤D1 / D2≤0.
85.
6. The battery cell according to any one of claims 3 to 5, wherein: 0.03mm≤D1≤0.5mm.
7. The battery cell according to claim 6, wherein: 0.15mm≤D1≤0.4mm.
8. The battery cell according to any one of claims 3 to 7, wherein: 0.05mm≤D2≤0.65mm.
9. The battery cell according to claim 8, wherein: 0.25mm≤D2≤0.5mm.
10. The battery cell according to any one of claims 2 to 9, wherein: The depth of the first slot segment is greater than the depth of the second slot segment, so that the residual thickness of the first slot segment is smaller than the residual thickness of the second slot segment.
11. The battery cell according to any one of claims 2 to 10, wherein: The first groove section includes a first-level groove and a second-level groove, the first-level groove and the second-level groove are arranged along the thickness direction of the pressure relief component, and the second-level groove is arranged on the groove bottom surface of the first-level groove.
12. The battery cell according to claim 11, wherein: The groove bottom surface of the first-stage groove is flush with the groove bottom surface of the second groove section.
13. The battery cell according to claim 11, wherein: Along the thickness direction of the pressure relief component, the pressure relief component has a first surface and a second surface opposite to each other, the first-stage groove and the second-stage groove are sequentially arranged along the direction from the first surface to the second surface, and the groove bottom surface of the second-stage groove is closer to the second surface than the groove bottom surface of the second groove section; Wherein, the groove bottom surface of the second-stage groove and the groove bottom surface of the second groove section are connected through a first inclined plane or a first arc surface.
14. The battery cell according to any one of claims 2 to 13, wherein: The third slot segment forms the detonation position, and the residual thickness of the third slot segment is smaller than the residual thickness of the second slot segment.
15. The battery cell according to claim 14, wherein: The residual thickness of the third slot segment is equal to the residual thickness of the first slot segment.
16. The battery cell according to claim 14 or 15, wherein: The residual thickness of the second groove segment is D2, and the residual thickness of the third groove segment is D3, which satisfies: 0.15≤D3 / D2≤0.
95.
17. The battery cell according to claim 16, wherein: 0.3≤D3 / D2≤0.
9.
18. The battery cell according to claim 17, wherein: 0.5≤D3D2≤0.
85.
19. The battery cell according to any one of claims 16 to 18, wherein: 0.03mm≤D3≤0.5mm.
20. The battery cell according to claim 19, wherein: 0.15mm≤D3≤0.4mm.
21. The battery cell according to any one of claims 14 to 20, wherein: The depth of the third slot segment is greater than the depth of the second slot segment, so that the residual thickness of the third slot segment is smaller than the residual thickness of the second slot segment.
22. The battery cell according to any one of claims 14 to 21, wherein: The third groove section includes a third-level groove and a fourth-level groove, the third-level groove and the fourth-level groove are arranged along the thickness direction of the pressure relief component, and the fourth-level groove is arranged on the groove bottom surface of the third-level groove.
23. The battery cell according to claim 22, wherein: The groove bottom surface of the third-level groove is flush with the groove bottom surface of the second groove section.
24. The battery cell according to claim 22, wherein: Along the thickness direction of the pressure relief component, the pressure relief component has a first surface and a second surface opposite to each other, the third-stage groove and the fourth-stage groove are sequentially arranged in a direction from the first surface to the second surface, and the groove bottom surface of the fourth-stage groove is closer to the second surface than the groove bottom surface of the second groove segment; Wherein, the groove bottom surface of the fourth-level groove is connected to the groove bottom surface of the second groove segment through a second inclined plane or a second arc surface.
25. The battery cell according to any one of claims 1 to 24, wherein: Along the extending direction of the second slot segment, two ends of the second slot segment are connected to the first slot segment and the third slot segment respectively.
26. The battery cell according to any one of claims 1 to 25, wherein: The first slot section is connected to the second slot section at a first position, and along the extension direction of the first slot section, the first position deviates from two ends of the first slot section.
27. The battery cell according to claim 26, wherein: Along the extension direction of the first slot segment, the first position is located at the midpoint of the first slot segment.
28. The battery cell according to any one of claims 1 to 27, wherein: The third slot segment is connected to the second slot segment at a second position, and along the extension direction of the third slot segment, the second position deviates from two ends of the third slot segment.
29. The battery cell according to claim 28, wherein: Along the extension direction of the third slot segment, the second position is located at the midpoint of the third slot segment.
30. The battery cell according to any one of claims 1 to 29, wherein: The first slot segment, the second slot segment and the third slot segment are all slots extending along a straight line trajectory.
31. The battery cell according to claim 30, wherein: The first slot segment is perpendicular to the second slot segment; and / or the third slot segment is perpendicular to the second slot segment.
32. The battery cell according to any one of claims 1 to 31, wherein: The first slot section, the second slot section and the third slot section define a pressure relief area; The pressure relief component is provided with a guide groove, the guide groove is arranged at a distance from the second groove section, and the guide groove is configured to guide the pressure relief area to flip open.
33. The battery cell according to claim 32, wherein: The first slot section, the second slot section and the third slot section define two pressure relief areas, and the two pressure relief areas are respectively located on both sides of the second slot section; The pressure relief component is provided with two guide grooves, the second groove section is located between the two guide grooves, and the two guide grooves are configured to respectively guide the two pressure relief areas to flip open.
34. The battery cell according to claim 32 or 33, wherein: The first slot section and the third slot section are not in contact with the guide slot.
35. The battery cell according to any one of claims 32 to 34, wherein: The guide groove and the groove portion are respectively arranged on both sides of the pressure relief component along a thickness direction of the pressure relief component.
36. The battery cell according to any one of claims 32 to 35, wherein: The guide groove extends along an extending direction of the second groove segment.
37. The battery cell according to any one of claims 32 to 36, wherein: Along the extension direction of the second slot segment, the first slot segment and the third slot segment are respectively located on both sides of the guide groove, the length of the second slot segment between the first slot segment and the third slot segment is L1, and the length of the guide groove is L2, satisfying: 1mm≤L1-L2≤10mm.
38. The battery cell according to claim 37, wherein: 2mm≤L1-L2≤6mm.
39. The battery cell according to any one of claims 32 to 38, wherein: Along the extending direction of the first slot segment, the distance between the guide slot and the second slot segment is L3, the length L4 of the portion of the first slot segment extending from the second slot segment toward the guide slot is 0.5 mm ≤ |L3-L4| ≤ 15 mm.
40. The battery cell according to claim 39, wherein: 1mm≤|L3-L4|≤10mm.
41. The battery cell according to any one of claims 1 to 40, wherein: The housing includes a first wall portion; The pressure relief component is the first wall portion; or, the pressure relief component and the first wall portion are separately provided, and the pressure relief component is installed on the first wall portion.
42. The battery cell according to claim 41, wherein: The housing comprises: a housing having an opening; An end cover closes the opening, and the end cover is the first wall portion.
43. The battery cell according to claim 41, wherein: The housing comprises: a housing having an opening; an end cap for closing the opening; Wherein, at least one wall portion of the shell is the first wall portion.
44. The battery cell according to claim 43, wherein: The shell comprises a bottom wall and a plurality of side walls, the plurality of side walls are arranged around the bottom wall, and the shell forms the opening at one end opposite to the bottom wall; Wherein, the bottom wall is the first wall portion.
45. The battery cell according to any one of claims 41 to 44, wherein: The first wall portion is a rectangular wall portion, the second slot segment extends along the length direction of the first wall portion, and the first slot segment and the third slot segment both extend along the width direction of the first wall portion.
46. The battery cell according to any one of claims 41 to 45, wherein: The first wall portion has an outer surface along the thickness direction of the pressure relief component, and the outer surface faces away from the interior of the housing; The first slot segment has a first midplane extending along its extension direction, the second slot segment has a second midplane extending along its extension direction, the third slot segment has a third midplane extending along its extension direction, the minimum distance from the center point of the outer surface to the first midplane is M1, the minimum distance from the center point of the outer surface to the second midplane is M2, and the minimum distance from the center point of the outer surface to the third midplane is M3, satisfying: M2<M1, M2<M3.
47. The battery cell according to claim 46, wherein: Along the thickness direction of the pressure relief component, the projection of the center point of the outer surface is located in the second groove segment; and / or, |M3-M1|≤5mm.
48. The battery cell according to claim 46 or 47, wherein: The outer surface is a rectangle, a circle or a regular polygon.
49. A battery comprising the battery cell according to any one of claims 1 to 48.
50. An electrical device, comprising the battery cell according to any one of claims 1 to 48, wherein the battery cell is used to provide electrical energy to the electrical device.
Citation Information
Patent Citations
Shell component, battery cell, battery and electric equipment
CN115663389A
Pressure relief device, battery monomer, battery and electric equipment
CN215989101U
Pressure relief device, battery monomer, battery and electric equipment
CN218769952U
Sealed battery
JP2013239274A
Battery module, secondary battery and cap plate assembly thereof