Method and device for the production of polyurethane structural parts
The device addresses mixing challenges by using a nozzle element with a constriction to generate local negative pressure and countercurrent injection, ensuring effective and gentle mixing of additives in polyurethane production, particularly for shear-sensitive fillers, thus enhancing processing efficiency and reducing wear.
Patent Information
- Application Number
- PCT/EP2024/062713
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-06-02
- Filing Date
- 2024-05-08
- Publication Date
- 2024-12-05
AI Technical Summary
Existing methods for producing polyurethane components face challenges in adequately mixing liquid and solid additives, particularly abrasive and shear-sensitive fillers like expanded graphite, due to insufficient pulse energy and mechanical stress, leading to issues like wear, separation, and inadequate mixing.
A device with a nozzle element featuring a first flow path with a constriction and a second flow path ending at the constriction, generating local negative pressure to gently mix additives into the reaction mixture with high pulse energy, using countercurrent injection and gas introduction to maintain flowability and reduce shear stress.
This solution ensures thorough mixing of additives with minimal shear stress and low initial pressures, preventing wear and segregation, and maintaining the integrity of sensitive fillers like expanded graphite, while allowing for precise control and efficient processing.
Smart Images

Figure EP2024062713_05122024_PF_FP_ABST
Abstract
Description
[0001] Method and device for the production of
[0002] Polyurethane components
[0003] The invention relates to a method for producing polyurethane components, in which at least two different chemical components, including at least one polyol component and one isocyanate component, are individually metered and then fed to the mixing chamber of a mixing head, in which they are mixed to form a polyurethane reactive mixture and then discharged from the mixing chamber, in particular into an open or closed mold, wherein a further component, in particular a filler, is added to at least one of the chemical components before entering the mixing chamber of the chemical component, wherein the further component is in liquid or solid form, in particular as a powdery, granular or lumpy mixture, and wherein the chemical component to which the further component is added is passed through a nozzle element,which is arranged in front of or on the mixing chamber and which has a first flow path for the chemical component, wherein the first flow path for the chemical component has a constriction, wherein the further component is fed to the nozzle element and guided along a second flow path through the nozzle element. Furthermore, the invention relates to a device for carrying out such a method.
[0004] Known mixing devices for polyurethane high-pressure mixing – without the additional addition of special components – are designed so that the at least two reactive components meet in a mixing chamber with high flow energy in the form of pulse energy, thus mixing them together. In high-pressure mixing, there are generally no additional mixing elements for further mixing of the reaction mixture, so mixing occurs exclusively through the flow energy contained in the reactive components. In practice, the countercurrent injection process has become established.
[0005] Mixing primarily takes place in a mixing chamber that is mechanically cleaned by a plunger. Groove-controlled mixing heads feature return grooves in the control piston, through which the components circulate separately from the inlet opening through the grooves in the circulation position without mixing. In the metering position, the plunger is moved accordingly, forming a mixing chamber in the area of the inlet openings and mixing the reactive components.
[0006] As an alternative, nozzle-controlled mixing heads are known, which are designed without such circulation grooves. Component control is achieved by controlled nozzles arranged in the inlet openings.
[0007] The task of the nozzles is to generate the required flow energy and convert the pressure energy into flow energy. Narrow flow cross-sections are required in the nozzle to create the required orifice effect.
[0008] Due to the properties required of the produced components, it is sometimes necessary to add various additives to the reaction mixture. These additives can be in liquid, solid, lumpy, or powdered form.
[0009] Liquid additional components include, for example, activators, additives, and colors. The liquid components are usually only added to the reaction mixture in small quantities. They are either mixed into the polyol component in a batch or dosed directly into the mixing chamber. When added directly into the mixing chamber, the problem often arises that the pulse generated by the very small dosage does not generate enough momentum to be adequately mixed during countercurrent injection. Processing as a polyol batch has the disadvantage that the sometimes corrosive properties of the additional component cause problems with the service life of the system and sometimes require special components for conditioning and conveying. If colors are to be processed in batches, multiple rinsing processes are often necessary when changing the color, which makes rapid color changes difficult.
[0010] Solid fillers are usually in lumpy, short-fiber, or powdered form. These are often abrasive and cause significant wear on conveying equipment and piping systems. Furthermore, some fillers, such as expandable graphite, are particularly shear-sensitive, creating further challenges in handling and mixing into the reaction mixture.
[0011] A method of the aforementioned generic type is known from DE 33 35 787 A1. A similar solution is disclosed in DE 10 2010 031 958 A1.
[0012] For conveying powdery fillers, DE 27 50 938 A1 proposes the use of the internal pressure of a gas-filled filler container. This represents a particularly gentle conveying option, as no pumps or other dynamic conveying devices are required. The gas pressure can be used as a targeted conveying pressure via a control system, thus allowing the desired flow rate to be adjusted. Since solid fillers are prone to flow problems, such as pitting and bridging, it is necessary to keep the bulk material flowing.
[0013] Fluidizing bulk materials by means of air aeration is well known in silo technology. The aforementioned DE 27 50 938 A1 applies this approach to polyurethane processing. A porous cone in the filler container creates a fine air distribution, keeping the bulk material flowable. The mixing process in the mixing chamber is not described.
[0014] Various methods are known for adding solid fillers, such as chalk, expandable graphite or similar materials, to the reaction mixture:
[0015] First, the filler can be added to one of the main components. Furthermore, the filler can be added to the reaction mixture within the discharge system after high-pressure mixing.
[0016] Finally, the filler can be added via a separate feed into the mixing chamber.
[0017] When the filler is added to one of the reaction components, the filler is injected into the mixing chamber together with the main component, meaning the fillers must be pumped together with the main component under high pressure via a metering pump. A disadvantage here is that fluids filled with fillers tend to segregate and form deposits in the pipes. Abrasive fillers often lead to increased wear on surfaces subject to high mechanical and fluidic stress, for example, inside nozzles, metering pumps, and valves. Sensitive fillers can be damaged to an unacceptable degree by processing under high pressure.
[0018] The processing of expandable graphite, in particular, presents significant challenges for machine technology. Expandable graphite is used as a flame retardant in polyurethane processing. The mode of action, advantages, and problems associated with the processing of shear-sensitive fillers such as expandable graphite are explained, for example, in EP 3 892 432 A2.
[0019] One problem with processing expanded graphite is that the expanded graphite particles can be destroyed when exposed to mechanical stress, particularly shear forces in pumps or nozzles. This impairs their flame-retardant properties; on the other hand, the acid released negatively impacts the chemistry of the foaming process.
[0020] It is therefore problematic if expandable graphite, as is common with other fillers, is mixed as a filler-polyol mixture in a container, where it must be kept in suspension by means of a stirrer and additionally pumped in a circuit to prevent expandable graphite from settling in the pipes.
[0021] A method for reducing the circulation time of the expandable graphite-polyol mixture under high pressure is described in the aforementioned EP 3 892 432 A2.
[0022] Addition downstream of the mixing chamber is proposed, for example, in EP 0 037 523 A1, DE 27 50 938 A1, and DE 10 2009 011 900 B3, but this disadvantageously leads to insufficient mixing. In these previously known solutions, the additional component is added to the reaction mixture. No additional mixing device is present in these cases; this procedure is not feasible with self-cleaning mixing heads.
[0023] DE 42 16 943 A1 describes a process in which the filler is fed directly into the mixing chamber. However, the arrangement described therein results in insufficient mixing for many applications. Tests have shown that the pulse energy is usually insufficient to mix the additional component sufficiently well into the reaction mixture. In light of the problems described above, the object of the present invention is to provide a generic process and a corresponding device with which both liquid and solid, lumpy or powdery additives can be introduced into a reaction mixture, which is mixed using the countercurrent injection process, in such a way that the additive is mixed as well as possible.Particular attention should be paid to ensuring that filler particles can be mixed in as gently as possible and with low shear stress, and that liquid additives can be mixed in small quantities with low pre-pressures.
[0024] The solution to this problem by the invention is characterized in that the second flow path ends in the region of the constriction so that the further component can be mixed with the chemical component, wherein the flow rate of the chemical component to which the further component is added is increased by the constriction and thus a local negative pressure is generated in the chemical component and wherein the further component is fed to the chemical component in the region of the local negative pressure.
[0025] The constriction in the first flow path of the chemical component can be designed as an annular gap, and the additional component can be fed concentrically in the flow direction of the components behind the annular gap. In particular, it can be provided that the additional component is fed behind the annular gap in the direction of an axis of the nozzle element.
[0026] The chemical component is preferably accelerated to a speed of at least 20 m / s after flowing through the constriction. The chemical components are mixed in the mixing chamber, preferably by countercurrent injection. They are preferably injected into the mixing chamber via nozzles.
[0027] The other component is preferably expanded graphite.
[0028] The nozzle element is preferably arranged near the mixing chamber.
[0029] The device for producing polyurethane components comprises at least one metering pump for metering a chemical component in the form of a polyol component, at least one metering pump for metering a chemical component in the form of an isocyanate component, a mixing head with a mixing chamber for mixing the polyol component and the isocyanate component, at least one container for storing a further component, in particular expandable graphite, wherein a nozzle element is arranged in front of or on the mixing chamber, which is designed to mix the further component with at least one of the chemical components, wherein the nozzle element has a first flow path for the chemical component, which has a constriction, and a second flow path for the further component, wherein the invention provides that the second flow path for the further component ends in the region of the constriction,wherein means for generating vibration are arranged on or in the nozzle element, and / or wherein the second flow path for the additional component has a chamber that communicates with means for introducing a gas. The constriction in the first flow path of the chemical component is preferably designed as an annular gap, wherein the second flow path for the additional component ends behind the annular gap in the flow direction of the components. In particular, it is provided that the second flow path for the additional component extends at least partially in the direction of an axis of the nozzle element.
[0030] The second flow path for the further component is preferably formed, at least in sections, by a cylindrical opening at which a piston-like, axially displaceable slide is arranged, which is designed to enter the opening in order to close it.
[0031] The nozzle element preferably comprises a nozzle housing and a nozzle needle that is axially displaceable relative to the nozzle housing, wherein the constriction, in particular the annular gap, is formed between one axial end of the nozzle needle and the nozzle housing. Means are preferably arranged to influence the position of the nozzle needle relative to the nozzle housing, wherein the means can be designed in particular as electrical, hydraulic, or pneumatic control and / or regulating means.
[0032] It is also possible that spring means are arranged to generate a pressing force of one axial end of the nozzle needle against the nozzle housing, wherein the spring means are preferably designed as a mechanical spring or as a pneumatic spring.
[0033] The pulsation element according to the invention, which is arranged, for example, on the housing of the nozzle or within the nozzle, can keep the material to be added flowable inside the nozzle element (in particular in the chamber explained below). Using the chamber provided according to the invention, a gas, in particular carbon dioxide, can be introduced into the additional component before it is conveyed further. A particularly suitable gas is a readily soluble gas such as the aforementioned carbon dioxide, with which the additional component is flooded. The discharge rate from the nozzle element can also be regulated via the gas pressure, if necessary.
[0034] The introduction of a pressurized gas can also be provided to flow through the region of the second flow path and thus keep the other component flowable. For this purpose, corresponding gas inlet and outlet openings can be provided between the axial end regions of the second flow path to conduct gas through the second flow path.
[0035] According to the proposed concept, a liquid, lumpy or powdery additional component is mixed, preferably concentrically, into at least one of the two reaction components by means of the nozzle element in the form of a multi-component nozzle, wherein the nozzle element is arranged in the region of the line of a main component immediately before the entry into the mixing chamber and the additional component is injected into the mixing chamber only during the mixing process with the main component.
[0036] Mixing preferably occurs in such a way that the additional component is guided within one of the two countercurrents and meets at the same point as the high-pressure component. The concentric addition causes acceleration of the additional component, thereby increasing its momentum.
[0037] Separation of polyol and isocyanate as well as the additional component occurs until shortly before the mixing chamber.
[0038] The additional component is therefore preferably introduced concentrically within the main component stream. It is preferably not introduced at high pressure.
[0039] The inlet opening for the additive component into the mixing chamber can be closed by a plunger (see the axially movable slide mentioned above). This allows the production of a reaction mixture with or without the additive component. Furthermore, the plunger prevents the additive component from leaking into the reaction components or from clogging the additive component with the reaction mixture. In recirculation mode (see the recirculation grooves mentioned below), the slide closes the opening. In shot mode, it can either open the opening or keep it closed, depending on whether the additive is to be introduced into the mixing chamber during this shot or not.
[0040] Solid fillers are preferably conveyed into the mixing chamber via the internal pressure of a gas-filled filler container (see the means for introducing gas mentioned above). An overflow opening in the nozzle area ensures that lumpy, granular, or powdery fillers remain free-flowing and prevents any leakage of the solid fillers. Gas can be introduced through the overflow opening, thus keeping the material being added flowable. The overflow opening can be designed as a valve or as a bore or orifice. Although gas can enter the chamber through this opening, no solid component can escape from the chamber.
[0041] In addition, active vibration generators (see the means for generating vibration mentioned above) can lead to an improvement in flow behavior.
[0042] The nozzle element is preferably designed with a drilled nozzle needle through which the additional component is guided into the mixing chamber. The nozzle needle has an annular throttle gap. The throttle gap converts the pressure energy of the reaction components into flow energy and thus into mixing energy. The throttle gap can be adjusted either as a function of the travel distance or as a function of the component pressure upstream of the nozzle. Mechanical and gas springs are preferred as pressure-dependent adjustment elements.
[0043] The position of the nozzle needle allows the amount of component flow to be adjusted depending on the distance and / or pressure, as this allows the size of the annular gap to be specifically changed. This can be done either manually or via a control or closed-loop control system.
[0044] The proposed solution allows for particularly gentle processing of fillers. These do not need to be pre-mixed into one of the two main components. Thus, particularly shear-sensitive solid fillers are not subjected to the otherwise required pumps and nozzles. Abrasive or corrosive additives can be conveyed to the mixing chamber in a separate dosing line, which has no negative impact on the longevity of the production system.
[0045] Problems with deposits and segregation of solid particles in a liquid main component can be prevented with the proposed solution.
[0046] By mixing the additional component into the main component stream with high pulse energy, the additional component is entrained and therefore does not need to be conveyed with high energy itself until it enters the mixing chamber.
[0047] An embodiment of the invention is shown in the drawings.
[0048] Fig. 1 shows schematically an apparatus for producing a molded part from polyurethane, in which a high-pressure mixing head is used, into which polyol and isocyanate as well as a further component in the form of expandable graphite are injected by means of component nozzles,
[0049] Fig. 2 shows the section through a nozzle element which is arranged on or in the mixing head, whereby the working position of the nozzle element is sketched, in which the further component in the form of expandable graphite is added to the polyol, and
[0050] Fig. 3 shows the nozzle element in the representation according to Figure 2, whereby the position of the nozzle element is now sketched in which both the supply of the chemical component and the supply of the further component are blocked.
[0051] Figure 1 shows an apparatus for producing a molded part 27 from polyurethane. In this case, the reactive mixture is dispensed into a mold 5.
[0052] A container for polyol 1 and a container for isocyanate 2 can be seen. Each container is connected via a line to a metering pump 11 and 12, respectively. The metering pumps 11, 12 then convey the respective component to a mixing head 4, which has a mixing chamber 3. Both the polyol 1 and the isocyanate 2 are injected into the mixing chamber 3 at high pressure via a nozzle element 7 and the nozzle 19, where they are mixed, creating the reactive mixture.
[0053] Also indicated in Figure 1 are an axially movable control slide 30 and recirculation grooves 28 and 29 for circulating the components. The related technology is only marginally relevant here and is well known in the state of the art.
[0054] A container 13 is also provided for a further component 6 in the form of expandable graphite. The aim is to mix the further component 6 into the polyol 1 as evenly distributed as possible without subjecting it to strong stresses, particularly in the form of shear.
[0055] This is achieved by the special nozzle element 7, which in the exemplary embodiment is arranged directly next to the mixing chamber 3. The nozzle element 7 is shown in more detail in Figures 2 and 3, with Figure 2 illustrating a position of the nozzle element open for the additional component 6, while Figure 3 shows both the supply for the chemical component 1 and for the additional component 6 blocked. The components of the nozzle element 7 correspond to one another, so that only a few reference numbers mentioned in Figure 2 are also entered in Figure 3.
[0056] The nozzle element 7 has a housing 20 to which a nozzle housing 16 is attached. A nozzle needle 17 is arranged in the nozzle housing 16 so as to be displaceable in the direction of an axis a. The housing 20 has a supply line 22 for the additional component 6. A supply line 21 for the polyol 1 is provided in the nozzle housing 16. Furthermore, an outlet 23 for the mixture consisting of the polyol 1 and the additional component 6 is provided in the nozzle housing 16.
[0057] In the present case, the nozzle element 7 is arranged directly upstream of the mixing chamber 3 and, via this, the further component 6 is mixed into the polyol 1 (additively or alternatively also into the isocyanate 2). The nozzle element 7 has a first flow path 8 for the polyol 1, wherein the first flow path 8 has a constriction 9 in the form of an annular gap. Furthermore, the further component 6 is fed to the nozzle element 7, wherein it is guided along a second flow path 10 in the nozzle element 7. The second flow path 10 ends in the region of the constriction 9. The flow paths 8 and 10 are illustrated in Figure 2 by dotted lines.
[0058] The size of the annular gap 9 can be adjusted by appropriately positioning the nozzle needle 17 relative to the nozzle housing 16. An adjustment device 25 is provided for this purpose. By appropriately adjusting the size of the annular gap 9, the polyol 1 is accelerated accordingly, so that the static pressure in the material is reduced. The second flow path 10 opens in the area of reduced pressure, so that when the further component 6 is added, this is optimally mixed into the polyol 1. As can be seen from Figure 2, the annular gap 9 and the end of the second flow path 10 are arranged concentrically to the axis a. In the preferred exemplary embodiment, the further component 6 is guided radially inward and the polyol 1 radially outward, and both components are combined behind the annular gap 9 in the conveying direction and thus optimally mixed with one another.
[0059] Whether and how much material of the further component 6 is added to the polyol 1 can be influenced by an axially displaceable slide 15 with a drive 24, whereby the slide 15 can enter a cylindrical opening 14 in the nozzle needle 17 (this happens in the illustration according to Figure 3).
[0060] In the second flow path 10 for the additional component 6, a chamber 18 is formed, which is provided with an overflow valve 26. Gas can be introduced into the chamber 18 from the outside via the overflow valve 26; however, no material of the additional component 6 can escape through the valve. By introducing a gas, the additional component 6 can be kept in a readily pumpable state, thus allowing for precise dosing of the additional component 6. Reference symbols:
[0061] 1 chemical component (polyol)
[0062] 2 chemical component (isocyanate)
[0063] 3 Mixing chamber
[0064] 4 Mixing head
[0065] 5 Shape
[0066] 6 additional components (filler, expandable graphite)
[0067] 7 Nozzle element
[0068] 8 first flow path
[0069] 9 Constriction (annular gap)
[0070] 10 second flow path
[0071] 11 Dosing pump for polyol
[0072] 12 Dosing pump for isocyanate
[0073] 13 Container for the additional component
[0074] 14 cylindrical opening
[0075] 15 axially movable slide
[0076] 16 nozzle housings
[0077] 17 Nozzle needle
[0078] 18 chamber
[0079] 19 Nozzle for isocyanate
[0080] 20 Nozzle element housing
[0081] 21 Feed chemical component (polyol)
[0082] 22 Feeding additional component (expandable graphite)
[0083] 23 Outlet for mixing chemical component including other component
[0084] 24 Drive for slide 25 Adjustment device for constriction (annular gap)
[0085] 26 Overflow valve
[0086] 27 molded part
[0087] 28 recirculation groove 29 recirculation groove
[0088] 30 Control slide a axis of the nozzle element
Claims
Patent claims:
1. A method for producing polyurethane components, in which at least two different chemical components (1, 2), including at least one polyol component and one isocyanate component, are individually metered and then fed to the mixing chamber (3) of a mixing head (4), in which they are mixed to form a polyurethane reactive mixture and then discharged from the mixing chamber (3), in particular into an open or closed mold (5), wherein a further component (6) is added to at least one of the chemical components (1) before the chemical component (1) enters the mixing chamber (3), wherein the further component (6) is in liquid or solid form, and wherein the chemical component (1), to which the further component (6) is added, is passed through a nozzle element (7) which is arranged upstream of or on the mixing chamber (3) and which has a first flow path (8) for the chemical component (1),wherein the first flow path (8) for the chemical component (1) has a constriction (9), wherein the further component (6) is fed to the nozzle element (7) and is guided along a second flow path (10) through the nozzle element (7), characterized in that that the second flow path (10) ends in the region of the constriction (9) so that the further component (6) can be mixed with the chemical component (1), wherein the flow rate of the chemical component (1) to which the further component (6) is added is increased by the constriction (9) and thus a local negative pressure is generated in the chemical component (1), and wherein the further component (6) is fed in the region of the local negative pressure of the chemical component (1).
2. Method according to claim 1, characterized in that the constriction (9) in the first flow path (8) is designed as an annular gap and the further component (6) is fed concentrically in the flow direction of the components behind the annular gap (9).
3. Method according to claim 2, characterized in that the further component (6) is fed in the direction of an axis (a) of the nozzle element (7) behind the annular gap (9).
4. Method according to one of claims 1 to 3, characterized in that the chemical component (1) is accelerated to a speed of at least 20 m / s after flowing through the constriction (9).
5. Method according to one of claims 1 to 4, characterized in that the chemical components (1, 2) are mixed in the mixing chamber (3) by means of countercurrent injection.
6. Method according to one of claims 1 to 5, characterized in that the chemical components (1, 2) are injected into the mixing chamber (3) by means of nozzles.
7. Process according to one of claims 1 to 6, characterized in that the further component (6) is expandable graphite.
8. Device for the production of polyurethane components, in particular for carrying out the method according to one of claims 1 to 7, comprising at least one metering pump (11) for metering a chemical component in the form of a polyol component (1), at least one metering pump (12) for metering a chemical component in the form of an isocyanate component (2), a mixing head (4) with a mixing chamber (3) for mixing the polyol component (1) and the isocyanate component (2), at least one container (13) for storing a further Component (6), wherein a nozzle element (7) is arranged in front of or on the mixing chamber (3), which nozzle element is designed to mix the further component (6) with at least one of the chemical components (1), wherein the nozzle element (7) has a first flow path (8) for the chemical component (1), which has a constriction (9), and a second flow path (10) for the further component (6), characterized in that the second flow path (10) for the further component (6) ends in the region of the constriction (9), wherein means for generating a vibration are arranged on or in the nozzle element (7) and / or wherein the second flow path (10) for the further component (6) has a chamber (18) which is connected to means for introducing a gas.
9. Device according to claim 8, characterized in that the constriction (9) in the first flow path (8) of the chemical component (1) is designed as an annular gap and the second flow path (10) for the further component (6) ends behind the annular gap in the flow direction of the components.
10. Device according to claim 9, characterized in that the second flow path (10) for the further component (6) extends at least in sections in the direction of an axis (a) of the nozzle element (7).
11. Device according to one of claims 8 to 10, characterized in that the second flow path (10) for the further component (6) is formed at least in sections by a cylindrical opening (14) on which a piston-like, axially displaceable slide (15) is arranged, which is designed to enter the opening (14) in order to close it.
12. Device according to one of claims 8 to 11, characterized in that the nozzle element (7) has a nozzle housing (16) and a nozzle needle (17) which is axially displaceable relative to the nozzle housing (16), wherein the constriction (9) can be formed between one axial end of the nozzle needle (17) and the nozzle housing (16).
13. Device according to claim 12, characterized in that means are arranged to influence the position of the nozzle needle (17) relative to the nozzle housing (16), wherein the means are designed in particular as electrical, hydraulic or pneumatic control and / or regulating means, or that spring means are arranged to apply a pressure force of one axial end of the nozzle needle (17) to the Nozzle housing (16), wherein the spring means are preferably designed as a mechanical spring or as a pneumatic spring.
Citation Information
Patent Citations
Device for manufacturing plastic parts reinforced with reinforcing fibers
DE102009011900B3
Device for mixing and dosing of liquids in small quantities under high pressure, comprises small hole, which is formed in pipeline in mixing chamber of flowing liquid
DE102010031958A1
Metering and mixing plant for filled polyurethane foams - maintains mechanical characteristics by preventing component separation and sedimenting
DE2750938A1
Multi-component nozzle for merging at least one flowable additive component with at least two flowable, plastics-forming, especially foam-forming, main components in order to initiate the reaction by mixing
DE3335787A1
Appts. for mixing reagents to produce e.g. polyurethane resins - has mixing chamber with extra inlet for fillers to enter just below bottom end of plunger so that they are fully wetted by reagents added