Method and apparatus for laser machining superhard material to form cutting edge
By sequentially processing ultrahard material bodies with three types of laser beams of different energies to form grooves and continuous processing surfaces, the problems of low efficiency and reduced precision in laser processing are solved, enabling the manufacturing of cutting edges with high precision and large-scale production.
Patent Information
- Application Number
- PCT/CN2026/091162
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-08
- Filing Date
- 2026-04-16
- Publication Date
- 2026-11-12
AI Technical Summary
Existing laser processing methods for superhard materials suffer from low efficiency, reduced processing accuracy due to the heat-affected zone, rough cutting edges, and thermal damage, making it difficult to meet the requirements of high precision and large-scale production.
Three laser beams of different energies are used to process the superhard material in sequence to form a groove and a continuous processing surface. The heat diffusion path is changed by changing the inner cavity of the groove to avoid local heat accumulation and form a high-precision cutting edge.
It improves the efficiency of laser processing of superhard materials, ensures the accuracy and stability of the cutting edge, is suitable for existing equipment, and meets the needs of high precision and large-scale production.
Smart Images

Figure CN2026091162_12112026_PF_FP_ABST
Abstract
Description
Method and apparatus for forming cutting edges using laser processing of superhard materials Technical Field
[0001] This invention relates to a method for processing materials, and more particularly to a method for forming a cutting edge for machining by using laser processing of materials. Background Technology
[0002] To increase the lifespan of machining tools, superhard materials are increasingly being used. However, series of superhard materials, such as polycrystalline diamond (PCD) and polydiamond composite (PDC), are difficult to grind using grinding wheels or similar methods. While laser processing (also known as cutting) has solved this problem, it still has several limitations, such as lower efficiency, longer processing time, difficulty in large-scale manufacturing, and high requirements for processing equipment. Furthermore, obtaining cutting edges made of superhard materials suitable for high-precision machining remains a significant challenge.
[0003] When the energy density of a laser beam exceeds the material's damage threshold, the material in contact with the laser vaporizes due to heat, resulting in the apparent removal of some material. For economic reasons, laser beams are typically focused, concentrating energy into a single point—a laser spot—and then controlling the spatial position of this spot to achieve the processing objective. Therefore, the thickness of material removed in each laser processing operation of a superhard material is extremely limited; it is generally believed that only the surface layer of material within the focused laser beam spot can be removed. To cut a superhard material, the laser must reciprocate along the same path, removing material layer by layer from the surface in the depth direction. During this process, visible cutting marks, or "kerfs," are formed on the superhard material. As the laser beam penetrates deeper, material outside the laser spot (i.e., material on both sides of the kerf) also comes into contact with the laser beam. At this point, the high-energy light waves are absorbed by the material and converted into heat energy, creating a heat-affected zone (also known as a "white zone"). The localized material expands in volume and then contracts upon cooling. Although this process is invisible to the naked eye, it obstructs the propagation path of the focused laser, which is detrimental to laser processing. This causes the laser spot to fail to act on the material to be removed as expected, resulting in a rough cutting edge (deterioration), a significant increase in tool lip and runout, and a change in tool processing diameter. These phenomena reduce the overall processing accuracy and make it difficult to meet the high-efficiency processing requirements of high-precision workpieces.
[0004] In addition, in the heat-affected zone, not only does the surface of the diamond particles oxidize, but the metals in the binder phase, such as cobalt (nickel), also precipitate and oxidize due to the high temperature. The surface roughness and bonding force of the superhard material are damaged, causing bumps, chipping, burrs and blunt rounding at the cutting edge, which also leads to a decrease in machining accuracy.
[0005] To avoid or reduce thermal damage to materials caused by the thermal effects of laser processing, several solutions have been proposed. For example, a beam shaping technique can be used to obtain a flat-top beam, which can then be used to cut single-crystal sapphire to obtain high-quality cut edges. Another example is using ultrafast lasers such as picosecond / femtosecond lasers for "cold" ablation processing of PCD. Yet another is using "water lasers" for special processing. While these solutions address problems in specific processing areas, they suffer from low versatility and applicability. Furthermore, they require sophisticated equipment and are costly, making them unsuitable for large-scale manufacturing.
[0006] Step-by-step cutting of superhard materials is a commonly used approach in laser processing. This involves first using a high-energy focused laser beam to cut the superhard material, inevitably creating a heat-affected zone (HAZ). Then, a lower-energy focused laser beam is applied to the HAZ, gradually cutting to remove it (although new HAZs will form during this process, their size is reduced) until the HAZ is minimized. However, this method further reduces laser processing efficiency. Summary of the Invention
[0007] One object of the present invention is to provide a method for forming cutting edges using laser processing of superhard materials, so as to improve the efficiency of laser processing of superhard material bodies.
[0008] Another objective of this invention is to provide a method for forming cutting edges using laser processing of superhard materials, thereby manufacturing superhard material cutting edges suitable for high-precision machining.
[0009] Another objective of this invention is to provide a method for forming cutting edges using laser processing of superhard materials, so that the cutting edge difference and runout of the resulting tool meet the requirements, and avoid significant increases and enlargement of the processing diameter.
[0010] Another objective of this invention is to provide a method for forming cutting edges using laser processing of superhard materials, which is applicable to existing laser processing equipment and meets the requirements of large-scale production and manufacturing.
[0011] In machining, common machining tools currently include grinding wheels, cutting tools, and lasers.
[0012] In machining, the term "material" or "workpiece" typically refers to materials or semi-finished products used to manufacture parts or components; it is the object of machining during the mechanical process. That is, after machining the workpiece, a product that meets the machining or design requirements is obtained, such as hole-making tools and milling cutters. For workpieces used for tool machining, they typically include an axis, with the axial length greater than the radial length.
[0013] Precision machining refers to machining techniques that achieve extremely high levels of precision and surface quality. For example, in tool machining, dimensions, straightness, contour accuracy, surface roughness, and cutting edge radius are all achieved at a level exceeding micrometers.
[0014] Machining equipment (or machining centers) are processing devices with multiple axes of motion. These are the X, Y, and Z axes, which move along straight lines in a right-handed Cartesian coordinate system, and the A, B, and C axes, which rotate around the X, Y, and Z axes, respectively. For example, CNC machine tools typically have various control software programs loaded, which receive and issue commands in code form to automate the machining of workpieces. For instance, by forming the method for forming the drill tip of a machining tool provided by this invention into control code, it can be automatically implemented on machining equipment to obtain products that meet machining or design requirements.
[0015] To achieve more accurate runout measurement and calculation at the cutting edge position, especially for large-diameter tools, while avoiding the aforementioned problems of non-contact measurement, this invention proposes a method comprising:
[0016] A focused laser beam is used to contact the surface of a superhard material with a laser spot of first energy, and a first groove is formed on the superhard material along the depth direction of laser processing (i.e., the shortest path to cut off the superhard material). The first groove includes a groove bottom and a groove inner wall. The groove bottom and the groove inner wall together form a groove cavity. The groove cavity is connected to the groove opening. The groove opening is formed by the laser spot of first energy contacting the superhard material.
[0017] The slot opening includes an inner edge surface, which defines the shape of the slot opening and the boundary between the slot opening and the inner cavity of the slot along the depth direction of the laser processing.
[0018] The inner edge surface is used as the back face of the formed cutting edge, and the cutting edge line of the cutting edge is formed at the intersection with the surface of the superhard material body located at the outer edge of the slot opening, thus obtaining the cutting edge of the tool. The surface of the superhard material body located at the outer edge of the slot opening is the rake face of the formed cutting edge.
[0019] Next, using a laser with a second energy, the material is gradually removed from the superhard material body by contacting the inner cavity side of the groove along the depth direction of the laser processing, forming a continuous second processing surface to cut off the superhard material body;
[0020] Then, a laser with a third energy is used to continue to act on the second processing surface, and a third processing surface is formed in the superhard material body to obtain the desired cutting edge shape.
[0021] In the method of the present invention, during processing, the outer edge of the laser spot forms an inner edge surface at the point where it is tangent to the superhard material body.
[0022] The method of the present invention ensures that the line connecting the outer edge of the laser spot and the superhard material body at all points tangent to each other along the depth direction of laser processing is a straight line.
[0023] The method of this invention utilizes a laser with a second energy level. Along the depth direction of laser processing, a second processing surface is formed that is offset from the inner wall of the groove by a distance such as 0.005mm to 0.2mm, particularly 0.03mm to 0.1mm. This facilitates the diffusion of laser energy within the ultrahard material, preventing localized heat accumulation and significant localized material expansion.
[0024] In the method of the present invention, the local edge of the third processing surface is close to the inner wall of the groove, or it is formed by processing the inner wall of the groove with a laser having a third energy.
[0025] The method of the present invention uses a first energy that can form a first groove on a superhard material, with a groove opening width of 0.01mm to 0.5mm, which is more suitable for the width of subsequent laser processing, such as 0.03mm, 0.05mm, 0.07mm and 0.1mm.
[0026] In the method of the present invention, the three energies of the laser beam used are not equal, wherein the first energy is the lowest, the second energy is the highest, and the third energy is between the first energy and the second energy.
[0027] The method of the present invention uses a laser beam with a wavelength of 1064±60nm or 532±60nm, a pulse width ≤200 nanoseconds, and a pulse energy ≤2mJ.
[0028] In the method of the present invention, the first energy has one or more of the following parameters:
[0029] Pulse width ≤150ns, especially ≤60ns, preferably ≤30ns.
[0030] Pulse energy ≤ 0.3 mJ, and
[0031] The repetition frequency is ≤2000kHz, especially ≤60kHz.
[0032] In the method of the present invention, the second energy has one or more of the following parameters:
[0033] 60ns ≤ pulse width ≤ 200ns
[0034] 0.5mJ ≤ pulse energy ≤ 2mJ, and
[0035] The repetition frequency is ≥30kHz, especially ≥60kHz.
[0036] In the method of the present invention, the third energy has one or more of the following parameters:
[0037] 60ns ≤ pulse width ≤ 200ns
[0038] 0.4mJ ≤ pulse energy ≤ 2mJ, and
[0039] The repetition frequency is ≥30kHz, especially ≥50kHz.
[0040] The method of this invention is applicable to various superhard materials such as diamond, CBN, and ceramics, and can be implemented on existing laser processing equipment (such as 4-axis, 5-axis, and 6-axis machine tools). For example, it can generate computer-executable code to meet the requirements of large-scale production. Depending on the material, the first, second, and third energy parameters may vary, resulting in some overlap in the range of energy values. However, they all follow the rule that the first energy is the lowest, the second energy is the highest, and the third energy is between the first and second energies. Attached Figure Description
[0041] Figure 1 is a schematic diagram of an embodiment of the method of the present invention for processing superhard material bodies using a laser with a first energy.
[0042] Figure 2 is a schematic diagram of forming the first groove on the superhard material body by the method shown in Figure 1;
[0043] Figure 3 is a schematic diagram of an embodiment of the method of the present invention for processing superhard material bodies using a laser with a second energy.
[0044] Figure 4 is a schematic diagram of forming a second processing surface on a superhard material body using the method shown in Figure 3;
[0045] Figure 5 is a schematic diagram of an embodiment of the method of the present invention for processing superhard material bodies using a third energy laser.
[0046] Figure 6 is a schematic diagram of forming a third processing surface on a superhard material body using the method shown in Figure 5;
[0047] Figure 7 is a schematic diagram of the heat propagation direction when implementing the method of the present invention. The arrows in the figure indicate the direction of heat diffusion.
[0048] Figure 8 shows a partial photograph of the cutting edge under a 400x bright field microscope. In the figure, A is a partial photograph of the cutting edge of a tool manufactured by the method of the present invention, and B is a partial photograph of the cutting edge of a tool manufactured by the prior art. Detailed Implementation
[0049] The technical solution of the present invention will be described in detail below with reference to the accompanying drawings. The embodiments of the present invention are only used to illustrate the technical solution of the present invention and are not intended to limit it. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solution of the invention without departing from the spirit and scope of the technical solution of the present invention, and all such modifications and substitutions should be covered within the scope of the claims of the present invention.
[0050] Figure 1 is a schematic diagram of an embodiment of the method of the present invention using a laser with first energy to process a superhard material body, and Figure 2 is a schematic diagram of the method shown in Figure 1 forming a first groove on the superhard material body. As shown in Figures 1 and 2, the surface 11 of the superhard material body is the rake face of the forming cutting edge. A focused laser acts on the superhard material body, and a laser spot with first energy 21 (pulse width < 200 nanoseconds, pulse energy < 2 mJ, wavelength of 1064 ± 60 nm or 532 ± 60 nm, repetition rate < 2000 kHz, preferably pulse width < 150 nanoseconds, especially < 60 ns, more preferably < 30 ns, pulse energy < 0.3 mJ, repetition rate < 60 kHz) contacts the surface of the superhard material body 10, and forms a first groove 100 on the superhard material body along the depth direction of laser processing (i.e., the shortest path to cut the superhard material body, see the arrow direction in Figure 1), with a depth ≤ 0.5 mm, especially ≤ 0.2 mm.
[0051] The first groove 100 includes a groove bottom 110, a groove inner wall, and a groove opening 140. The groove opening 140 is formed by the contact of a laser spot of first energy with the ultrahard material, and the groove opening width is 0.01mm~0.5mm. The groove inner wall 120 includes a first side wall 121 and a second side wall 122, with its upper end near the groove opening 140 and its lower end near the groove bottom 110. Thus, the first side wall 121 and the second side wall 122 are positioned on both sides of the groove bottom 110, and the groove bottom and the groove inner wall together form a groove cavity 130, which communicates with the groove opening 140. "Positioned" should be understood as having an angle with the groove bottom, rather than simply meaning "perpendicular".
[0052] The slot opening 140 includes an inner edge surface 141, which defines the shape of the slot opening and the boundary between the slot opening and the inner cavity along the depth direction of laser processing. During processing, the inner edge surface is formed where the outer edge of the laser spot is tangent to the superhard material. This inner edge surface serves as the flank face of the formed cutting edge, and the cutting edge 30 is formed at the intersection with the surface 12 of the superhard material located at the outer edge of the slot opening, thus obtaining the cutting edge of the tool. During processing, the line connecting the outer edge of the laser spot and the superhard material at all points tangent along the depth direction of laser processing is controlled to be a straight line.
[0053] After obtaining the first groove 100, a laser 22 with second energy is used to gradually remove the material from the superhard material body by contacting the inner cavity side of the groove along the depth direction of laser processing, forming a continuous second processing surface to cut the superhard material body. Figure 3 is a schematic diagram of an embodiment of the method of the present invention using a laser with second energy to process a superhard material body, and Figure 4 is a schematic diagram of the method shown in Figure 3 forming a second processing surface on the superhard material body. Referring to Figure 2, and as shown in Figures 3 and 4, the second processing surface 200 formed by the laser with second energy along the depth direction of laser processing is offset from the inner wall 120 of the groove by a distance of 0.005 mm or more, for example, 0.005 mm to 0.2 mm. This utilizes the space of the formed groove cavity to change the diffusion path of the heat converted by the laser within the superhard material body. Referring to Figure 7, the arrows in the figure indicate the direction of heat diffusion and transfer after the material is acted upon by the laser, avoiding direct heat diffusion to the material forming the cutting edge 30, avoiding local heat accumulation at the cutting edge, and preventing the material from expanding significantly.
[0054] During this process, a laser with a second energy level (pulse width < 200 nanoseconds, pulse energy < 2 mJ, wavelength 1064 ± 60 nm or 532 ± 60 nm, repetition rate > 30 kHz, preferably pulse width > 60 nanoseconds, pulse energy > 0.5 mJ, repetition rate > 60 kHz) is continuously used to cut the superhard material. To reduce the total heat absorbed by the superhard material, a superhard material with a thickness of 0.3 mm to 3.2 mm is selected for machining the cutting edge.
[0055] After the superhard material is cut, the second-energy laser is stopped, and a third-energy laser (pulse width < 200 nanoseconds, pulse energy < 2 mJ, wavelength 1064 ± 60 nm or 532 ± 60 nm, repetition rate > 30 kHz, more preferably, pulse width > 60 nanoseconds, pulse energy > 0.4 mJ, repetition rate > 50 kHz) continues to act on the second processing surface. Figure 5 is a schematic diagram of an embodiment of the method of the present invention using a third-energy laser to process a superhard material, and Figure 6 is a schematic diagram of the method shown in Figure 5 forming a third processing surface on the superhard material. Referring to Figures 2 and 4, and as shown in Figures 5 and 6, the third-energy laser continues to form a third processing surface 300 on the superhard material, obtaining the desired cutting edge morphology. Depending on the cutting edge morphology, the third-energy laser still acts on the material at the inner wall of the groove, causing the local edge of the third processing surface to be close to the inner wall of the groove, or formed by processing the inner wall of the groove.
[0056] The method provided in this embodiment first forms a shallow groove on the superhard material body with a low-energy (i.e., first-energy) laser beam before processing the superhard material body with a laser beam of the highest energy (i.e., the second energy). On the one hand, the heat energy in the high-energy laser beam processing changes the heat conduction path due to the setting of the groove cavity, avoiding the direct diffusion of heat to the material forming the cutting edge, which would cause local overheating. This solves the problem of the heat-affected zone and effectively avoids many adverse effects such as cutting edge breakage, burrs and blunting caused by the thermal leaching of metals such as cobalt (nickel), thus significantly improving the processing quality of the cutting edge.
[0057] The processing system that forms a cutting edge (main technical parameters and shape) on a superhard material with a laser beam is completed before it is subjected to high-energy irradiation. Therefore, thermal deformation of the material at the cutting edge due to processing is avoided, and the edge difference and runout no longer have significant deviations.
[0058] Because the cutting edge is directly isolated from the heat of laser processing due to the inner cavity of the groove, it is completely blocked from the direct thermal influence, thus eliminating the need to perform a process to "remove" the heat-affected zone and improving the processing efficiency of using ultrahard material bodies as cutting edges.
[0059] Although lower-energy laser spots achieve only a smaller amount of material removal on the superhard material, this processing method is less prone to generating particulate debris and plasma plumes. Therefore, the interaction between the laser spot and the contacting material is more stable, resulting in a finer and smoother surface. The edges formed (e.g., cutting edges) are sharper and less prone to chipping and protrusions, as shown in Figure 8A. The surface formed using existing laser processing methods, as shown in Figure 8B, is rougher, with a significantly lower smoothness than the superhard material surface obtained by the method in this embodiment.
Claims
1. A method for forming cutting edges using laser processing of superhard materials, characterized in that... include: A focused laser beam is used to contact the surface of a superhard material with a laser spot of first energy, and a first groove is formed on the superhard material along the depth direction of laser processing. The first groove includes a groove bottom and a groove inner wall. The groove bottom and the groove inner wall surround to form a groove cavity. The groove cavity is connected to the groove opening. The groove opening is formed by the laser spot of first energy contacting the superhard material. The slot opening includes an inner edge surface, which defines the shape of the slot opening and the boundary between the slot opening and the inner cavity of the slot along the depth direction of the laser processing. The inner edge surface is used as the back face of the formed cutting edge, and the cutting edge line of the cutting edge is formed at the intersection with the surface of the superhard material body located at the outer edge of the slot opening, thus obtaining the cutting edge of the tool. The surface of the superhard material body located at the outer edge of the slot opening is the rake face of the formed cutting edge. Next, using a laser with a second energy, the material is gradually removed from the superhard material body by contacting the inner cavity side of the groove along the depth direction of the laser processing, forming a continuous second processing surface to cut off the superhard material body; Then, a laser with a third energy is used to continue to act on the second processing surface, and a third processing surface is formed in the superhard material body to obtain the desired cutting edge morphology; The three energies of the laser beam used are not equal.
2. The method according to claim 1, characterized in that... During processing, the outer edge of the laser spot forms an inner edge surface where it is tangent to the superhard material.
3. The method according to claim 1, characterized in that... The first groove has an opening width of 0.01mm to 0.5mm.
4. The method according to claim 1, characterized in that... Using a laser with a second energy, a second processing surface is formed along the depth direction of laser processing, which is offset from the inner wall of the groove by a distance of 0.005mm to 0.2mm.
5. The method according to claim 1, characterized in that... Along the depth direction of laser processing, the lines connecting the outer edge of the laser spot to the tangent points of the superhard material body are straight.
6. The method according to claim 1, characterized in that... The wavelength of the laser beam used is 1064±60nm or 532±60nm, the pulse width is ≤200 nanoseconds, and the pulse energy is ≤2mJ.
7. The method according to claim 1, characterized in that... The first energy is the lowest, the second energy is the highest, and the third energy is between the first and second energies.
8. The method according to claim 1, characterized in that... The first energy has one or more of the following parameters: Pulse width ≤ 150 ns Pulse energy ≤ 0.3 mJ, and Repetition rate ≤ 2000kHz.
9. The method according to claim 8, characterized in that... The pulse width is ≤30ns and the repetition rate is ≤60kHz.
10. The method according to claim 1, characterized in that... The second energy has one or more of the following parameters: 60ns ≤ pulse width ≤ 200ns 0.5mJ ≤ pulse energy ≤ 2mJ, and Repetition rate ≥ 30kHz.
11. The method according to claim 10, characterized in that... The repetition frequency is ≥60kHz.
12. The method according to claim 1, characterized in that... The third energy has one or more of the following parameters: 60ns ≤ pulse width ≤ 200ns 0.4mJ ≤ pulse energy ≤ 2mJ, and Repetition rate ≥ 30kHz.
13. The method according to claim 12, characterized in that... The repetition frequency is ≥50kHz.
14. The method according to claim 1, characterized in that... The various superhard materials mentioned are selected from one or more of diamond, CBN and ceramics.
15. An apparatus, characterized in that... The cutting tool is machined using the method described in claim 1.
16. The apparatus according to claim 15, characterized in that... It is a 5-axis machining center.
17. The apparatus according to claim 15, characterized in that... Includes computer-executable code to implement the method of claim 1.