Multi-layer metal composite molded product
By designing a metallurgical bonding layer in a multi-layer metal composite structure, the problem of easy damage to traditional single-layer metal equipment in highly corrosive environments is solved. This achieves a balance between mechanical properties and corrosion resistance, reduces manufacturing costs, and improves the bonding strength and corrosion resistance of the product.
Patent Information
- Application Number
- PCT/CN2026/095011
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-07
- Filing Date
- 2026-05-07
- Publication Date
- 2026-11-12
AI Technical Summary
Traditional single-layer metal structure equipment is prone to corrosion and damage in highly corrosive media and harsh environments. Existing protection solutions are costly or cannot achieve both mechanical performance and corrosion resistance. It is also difficult to balance the bonding strength and thickness of multi-layer metal composite materials.
A multi-layer metal composite structure is adopted, in which the base pipe layer and the corrosion-resistant layer are bonded together by a metallurgical bonding layer. The thickness of the bonding layer is 0.01 mm to 0.5 mm, and the thickness of the base pipe layer and the corrosion-resistant layer is at least 2 to 300 times that of the bonding layer. Alloy materials are selected to ensure bonding strength and material saving.
It improves mechanical properties and corrosion resistance, reduces manufacturing costs, ensures that the product is not easily separated during machining, and improves the yield rate and corrosion resistance of the product.
Smart Images

Figure CN2026095011_12112026_PF_FP_ABST
Abstract
Description
Multi-layer metal composite molded products Technical Field
[0001] This invention belongs to the field of metal composite processing, and specifically relates to a multi-layer metal composite molded product. Background Technology
[0002] In industrial production, especially in scenarios involving highly corrosive media or harsh environments such as thermal combustion, chemical engineering, marine engineering, and oil and gas extraction, production equipment (such as pipelines, reaction vessels, reaction tanks, and combustion chambers) is exposed to complex corrosive factors such as acidic and alkaline media, high salt spray environments, or high temperatures and pressures for extended periods. Traditional single-layer metal structure equipment often suffers from surface corrosion, leading to wall thinning, stress cracking, and even media leakage, seriously threatening production safety and significantly increasing equipment replacement frequency.
[0003] For example, in the field of marine engineering, equipment such as offshore platform jackets and seawater desalination evaporators face the coupled effects of multiphase corrosion in the fully immersed seawater zone, splash zone, and atmospheric zone. Marine microbial corrosion causes ulcer-like corrosion with a depth exceeding 4 mm to form on equipment made of carbon steel within 6 months. In the field of oil and gas extraction, equipment in highly acidic oil and gas fields containing H2S / CO2 must withstand the dual threats of hydrogen-induced cracking and sulfide stress corrosion cracking. Specifically, in high-pressure gas wells, L80 grade tubing steel experiences hydrogen embrittlement fracture after 9 months of service, and sand-containing oil and gas flows at velocities above 15 m / s can cause scouring corrosion on X65 pipeline steel. In the field of chemical production, especially in chlor-alkali, fertilizer, and sulfuric acid production systems, equipment is in long-term contact with highly corrosive media such as concentrated sulfuric acid with a concentration exceeding 60% and boiling hydrochloric acid, also facing severe corrosion resistance challenges. For example, chlor-alkali industrial electrolytic cells are prone to interfacial hydrogen embrittlement cracking in a humid chlorine environment at 90℃, and 316L stainless steel reactors are prone to pitting corrosion penetration in media containing Cl- ions.
[0004] While existing technologies offer solutions involving surface coatings or spraying anti-corrosion paints, these single protective layers are prone to localized peeling under dynamic erosion and alternating thermal stress conditions, leading to substrate exposure and the spread of pitting corrosion. Although existing technologies also employ single corrosion-resistant alloy materials to manufacture equipment, this approach presents a technical dilemma: excessive cost and difficulty in achieving a balance between mechanical properties and corrosion resistance.
[0005] Compared to the aforementioned existing technologies, if the production equipment is implemented as a multi-layer metal composite molded product, the manufacturing cost, mechanical performance, and corrosion resistance of the production equipment can be further balanced. Compared with the solution of surface plating or spraying anti-corrosion coating, the solution of using multi-layer metal composite materials has significantly improved mechanical performance and corrosion resistance. Compared with the solution of using a single corrosion-resistant alloy material to manufacture the equipment, the solution of using multi-layer metal composite materials has significantly reduced manufacturing costs.
[0006] In solutions using multilayer metal composite materials, the molded products of multilayer metal composites include at least two layers: a base pipe layer and a corrosion-resistant layer. The base pipe layer is mainly used to provide rigidity, while the corrosion-resistant layer wraps around the outer surface of the base pipe layer or covers the inner surface of the base pipe layer to provide corrosion protection. If both the inner and outer surfaces of the base pipe layer are covered with corrosion-resistant layers, then such pipes with corrosion-resistant treatment on both the inside and outside can cope with harsh working scenarios where both the external environment and internal transmission are subject to corrosion.
[0007] To meet the requirements of installation and assembly, multilayer metal composite molded products require further machining processes such as diameter expansion, bending, and flattening. During this process, it is crucial to ensure that the base tube layer and the corrosion-resistant layer do not easily separate or delaminate. Therefore, in manufacturing multilayer metal composite molded products, selecting the appropriate composite process for both the base tube layer and the corrosion-resistant layer to ensure sufficient bonding strength has been a research hotspot in this field. Furthermore, given the selected composite process, achieving both the required bonding strength to ensure production efficiency and material savings to reduce manufacturing costs while maintaining a predetermined yield rate, determining the thickness of each layer and the proportional relationship between their thicknesses are also technical challenges in this field. Summary of the Invention
[0008] To overcome the aforementioned deficiencies in the prior art, the present invention provides a multilayer metal composite molded product, which includes a first layer, a second layer, and a bonding layer, wherein:
[0009] The first layer has a first surface facing the second layer, and the material of the first layer is a first alloy;
[0010] The second layer has a second surface facing the first layer, and the second layer conformally covers the first surface. The material of the second layer is a second alloy. The bonding layer is disposed between the first surface and the second surface and forms a metallurgical bond with the first surface and the second surface respectively. The material of the bonding layer is a third alloy, and the melting point of the third alloy is lower than that of the first alloy and the second alloy.
[0011] The first layer is bonded to the second layer through the bonding layer, and the separation strength between the first layer and the second layer is not less than 137 MPa;
[0012] The thickness of the bonding layer ranges from 0.01 mm to 0.5 mm, and the thickness of the first layer and the thickness of the second layer are at least twice the thickness of the bonding layer.
[0013] According to one aspect of the invention, the molded product has an inner cavity; the inner cavity is formed by the extension of the first layer or the second layer.
[0014] According to another aspect of the present invention, the molded product is a metal composite pipe; the first layer extends and surrounds to form the base pipe of the metal composite pipe; the second layer extends and surrounds to form the inner liner pipe of the metal composite pipe; the inner wall of the inner liner pipe surrounds to form the inner cavity.
[0015] According to another aspect of the invention, in the molded product, the thickness of the first layer is 6 to 2000 times the thickness of the bonding layer; and the thickness of the second layer is 2 to 300 times the thickness of the bonding layer.
[0016] According to another aspect of the invention, in the molded product, the ratio of the melting point of the third alloy to the melting point of the first alloy is 0.55 to 0.715; and the ratio of the melting point of the third alloy to the melting point of the second alloy is 0.586 to 0.853.
[0017] According to another aspect of the present invention, in the molded product, the first alloy includes any or all of carbon steel and iron-based alloys; the second alloy includes any, any combination or all of alloy steel, 316L stainless steel, nickel-based alloys, cobalt-based alloys and titanium alloys; and the third alloy includes any, any combination or all of nickel-based alloys, cobalt-based alloys and iron-based alloys doped with boron and / or silicon.
[0018] According to another aspect of the present invention, the molded product is a metal composite pipe; the first layer extends and surrounds to form an outer sleeve of the metal composite pipe; the second layer extends and surrounds to form a base pipe of the metal composite pipe; and the inner wall of the base pipe surrounds to form the inner cavity.
[0019] According to another aspect of the invention, in the molded product, the thickness of the first layer is 2 to 300 times the thickness of the bonding layer; and the thickness of the second layer is 6 to 2000 times the thickness of the bonding layer.
[0020] According to another aspect of the invention, in the molded product, the ratio of the melting point of the third alloy to the melting point of the second alloy is 0.55 to 0.715; and the ratio of the melting point of the third alloy to the melting point of the first alloy is 0.586 to 0.853.
[0021] According to another aspect of the present invention, in the molded product, the first alloy includes any, any combination of, or all of alloy steel, 316L stainless steel, nickel-based alloy, cobalt-based alloy, and titanium alloy; the second alloy includes any or all of carbon steel and iron-based alloy; and the third alloy includes any, any combination of, or all of nickel-based alloy, cobalt-based alloy, and iron-based alloy doped with boron and / or silicon.
[0022] According to another aspect of the present invention, in the molded product, the radial cross-sectional shape of the metal composite tube is circular, rectangular, regular polygonal or irregular polygonal; the first layer, the second layer and the bonding layer all have substantially uniform thickness.
[0023] According to another aspect of the invention, in the molded product, the porosity of the bonding layer does not exceed 5%; the separation strength between the first layer and the second layer is greater than 300 MPa.
[0024] This invention provides a multilayer metal composite molded product with a multilayer structure. A bonding layer is disposed between a first layer and a second layer, forming a metallurgical bond with both the first and second layers. The first layer forms an interface bond with the second layer through the bonding layer. Due to the high strength of the metallurgical bond, the first and second layers have sufficient bonding strength and are not easily separated even after subsequent machining. The thickness of the bonding layer is set to be between 0.01 mm and 0.5 mm, which can effectively save materials while ensuring the metallurgical bond strength and reduce the manufacturing cost of the multilayer metal composite molded product. Furthermore, the thickness of the first and second layers is set to be at least twice the thickness of the bonding layer, which facilitates the control of the diffusion uniformity of the bonding layer during heat treatment and avoids excessive diffusion of the components of the bonding layer into the first and second layers during the formation of the metallurgical bond. Excessive diffusion would affect the performance of the first and second layers themselves. Attached Figure Description
[0025] Other features, objects, and advantages of the invention will become more apparent from the following detailed description of non-limiting embodiments with reference to the accompanying drawings:
[0026] Figure 1A is a cross-sectional structural schematic diagram of a specific embodiment of the molded product of multilayer metal composite according to the present invention.
[0027] Figure 1B is a disassembly diagram of the specific embodiment shown in Figure 1A;
[0028] Figure 2 is a cross-sectional structural schematic diagram of another specific embodiment of the molded product of multilayer metal composite according to the present invention;
[0029] Figure 3A is a cross-sectional structural schematic diagram of another specific embodiment of the molded product of multilayer metal composite according to the present invention;
[0030] Figure 3B is a cross-sectional view of the specific embodiment shown in Figure 3A.
[0031] Figure 3C is a metallographic enlargement view of the specific embodiment shown in Figure 3B;
[0032] Figure 3D is a real photograph of the flattening test performed on the specific embodiment shown in Figure 3B.
[0033] Figure 4 is a cross-sectional structural schematic diagram of another specific embodiment of the molded product of multilayer metal composite according to the present invention;
[0034] Figure 5 is a cross-sectional structural schematic diagram of another specific embodiment of the molded product of multilayer metal composite according to the present invention;
[0035] The same or similar reference numerals in the accompanying drawings represent the same or similar parts. Detailed Implementation
[0036] To better understand and explain this invention, a further detailed description will be provided below with reference to the accompanying drawings. This invention is not limited to these specific embodiments. Rather, any modifications or equivalent substitutions made to this invention should be covered within the scope of the claims.
[0037] It should be noted that numerous specific details are provided in the following detailed embodiments. Those skilled in the art should understand that the present invention can be practiced without these specific details. In the various detailed embodiments given below, structures and components well-known in the art are not described in detail in order to highlight the spirit of the invention.
[0038] In the following description of the specific embodiments, the terms "upper" and "lower," etc., refer to the orientation or positional relationship shown in the accompanying drawings, and are used only for ease of description. They do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the present invention. In addition, the terms "first" and "second" are used only for distinction in description and have no special meaning.
[0039] The following description, in conjunction with the accompanying drawings, details various specific embodiments of the present invention. It should be noted that the accompanying drawings are merely illustrative of the technical solutions and core concepts of the present invention. The shapes and dimensions of the components in the specific embodiments shown in the accompanying drawings are not strictly based on the form of an actual product, and the shape and size proportions of the actual product may differ from those of the specific embodiments shown in the accompanying drawings. Therefore, the specific embodiments shown in the drawings should not be construed as the sole limitation on the actual product corresponding to the present invention, nor should they be used as the sole basis for determining shape and size comparisons in patent infringement cases.
[0040] First, please refer to Figures 1A and 1B. Figure 1A is a cross-sectional view of a specific embodiment of the multilayer metal composite molded product according to the present invention. More specifically, the part shown in Figure 1A is a partial cut from a continuous multilayer metal composite molded product, only to illustrate the relative positional relationship of the layers in the multilayer metal composite molded product.
[0041] As shown in Figure 1A, the multilayer metal composite molded product 10 includes a first layer 110, a second layer 120, and a bonding layer 130. The first layer 110 is bonded to the second layer 120 through the bonding layer 130. Figure 1B is a disassembled schematic diagram of the specific embodiment shown in Figure 1A. As shown in Figure 1B, the first layer 110 has a first surface 111 facing the second layer 120. The second layer 120 has a second surface 121 facing the first layer 110, and the second layer 120 conformally covers the first surface 111. The bonding layer 130 is disposed between the first surface 111 and the second surface 121, and forms a metallurgical bond with the first surface 111 and the second surface 121, respectively. In this specific embodiment or other specific embodiments, the first surface 111 can be defined as the metallurgical bonding interface between the first layer 110 and the bonding layer 130, and the second surface 121 can be defined as the metallurgical bonding interface between the second layer 120 and the bonding layer 130. This definition can be applied to the description of other specific embodiments below. The first surface 111 and the second surface 121 are difficult to observe with the naked eye in most cases, but the first surface 111 and the second surface 121 can usually be defined by metallographic microscopic observation.
[0042] Since the multi-layer metal composite molded product 10 requires subsequent machining, the first layer 110 and the second layer 120 need to have sufficient bonding strength, and metallurgical bonding is undoubtedly the bonding method with the highest bonding strength at present. In this specific embodiment, the bonding layer 130 forms a metallurgical bond with the first surface 111 and the second surface 121 respectively, which also makes the first layer 110 and the second layer 120 form a metallurgical interface bond. Accordingly, the materials selected for the first layer 110, the second layer 120 and the bonding layer 130 should be metals. The material of the first layer 110 is a first alloy, the material of the second layer 120 is a second alloy, and the material of the bonding layer 130 is a third alloy. This bonding method gives the first layer 110 and the second layer 120 a high bonding strength, and the separation strength of the first layer 110 and the second layer 120 is not less than 137 MPa.
[0043] Those skilled in the art will understand that to form the aforementioned metallurgical bond, the bonding layer 130 needs to undergo a remelting heat treatment. By raising the temperature of the bonding layer 130, atomic diffusion occurs between the bonding layer 130 and the first layer 110 at the first surface 111, and atomic diffusion occurs between the bonding layer 130 and the second layer 120 at the second surface 121, thereby achieving a metallurgical bond between the bonding layer 130 and the first layer 110 and the second layer 120, respectively. In the actual manufacturing process, the first layer 110, the bonding layer 130, and the second layer 120 are first stacked sequentially as shown in Figure 1A, and appropriate pressure is applied from the outside. At this time, the bonding layer 130 is completely covered by the first layer 110 and the second layer 120. Subsequently, an appropriate heating method is used to continuously raise the temperature of the bonding layer 130 until the melting point of the bonding layer 130 is reached. Regardless of whether the heating source is located on the outside of the first layer 110, the second layer 120, or both the first and second layers 110, heat cannot be directly transferred to the bonding layer 130. Instead, it is transferred through either the first or second layer 120. Therefore, the multilayer metal composite molded product 10 is heated as a whole during manufacturing, and the bonding layer 130 cannot be heated separately. Ideally, during the metallurgical bonding process between the bonding layer 130 and the first and second layers 110, the strength and surface properties of the first and second layers 120 should not be damaged. Based on this consideration, it is desirable that when the temperature of the bonding layer 130 is heated to its melting point, the temperatures of the first and second layers 110 should not have reached their corresponding melting points. Therefore, the melting point of the third alloy is selectively set to be lower than that of the first and second alloys. If the melting point of the third alloy is greater than that of the first alloy and the second alloy, the first layer 110 and the second layer 120 will melt before the bonding layer 130 forms a metallurgical bond with the first layer 110 and the second layer 120. During the subsequent recooling process, the first layer 110 and the second layer 120 may become embrittled, resulting in cracks. Porosity, coarse grains, stress accumulation and other adverse effects may also occur inside, causing the first layer 110 and the second layer 120 to lose toughness and strength.
[0044] Obviously, only by selectively setting the melting point of the third alloy to be lower than that of the first alloy and the second alloy can the structure of the multilayer metal composite molded product 10 shown in FIG1A be stably and qualifiedly formed.
[0045] In most cases, considering the manufacturing cost of the multilayer metal composite molded product 10, the first layer 110 and the second layer 120 are usually made of different materials. In this case, the first alloy and the second alloy are different types of metal alloys. For example, the first layer 110 is formed using the lower-cost first alloy, mainly to provide the mechanical properties of the multilayer metal composite molded product 10 to resist tensile forces, pressures, impact forces, etc., applied inside and outside the multilayer metal composite molded product 10. The second layer 120 is formed using the higher-cost second alloy, mainly to enhance the corrosion resistance of the multilayer metal composite molded product 10 to resist chemical corrosion, impact corrosion, etc., inside or outside the multilayer metal composite molded product 10. Of course, the functions of the first layer 110 and the second layer 120 can also be interchanged, depending on the working environment of the multilayer metal composite molded product 10, that is, depending on whether the corrosive factor of the multilayer metal composite molded product 10 comes from the external space of the first layer 110 or the external space of the second layer 120.
[0046] In some special cases, the multilayer metal composite molded product 10 operates in a location or environment where post-maintenance is difficult, or the multilayer metal composite molded product 10 has a highly corrosive environment both inside and outside. To deal with these special cases, cost is often ignored and the corrosion resistance of the multilayer metal composite molded product 10 is enhanced as much as possible. Therefore, the first layer 110 and the second layer 120 can be made of the same material. In this case, the first alloy and the second alloy can be selected as the same high-cost metal alloy, or two high-cost metal alloys can be selected.
[0047] Of course, regardless of the materials chosen for the first and second alloys, the third alloy must have a melting point lower than that of the first and second alloys. The melting point of the third alloy can be adjusted by adding a metal-like dopant, such as boron or silicon.
[0048] Based on this, through repeated experiments, it was verified that when the thickness of the bonding layer 130 is greater than 0.01 mm, it can stably and controllably form a metallurgical bond with the first layer 110 and the second layer 120 respectively. Ultimately, the first layer 110 forms a metallurgical bond with sufficient strength through the bonding layers 130 and 120. From the perspective of material conservation, the maximum thickness of the bonding layer 130 can be set to 0.5 mm. Therefore, the thickness of the bonding layer 130 can be selected within the range of 0.01 mm to 0.5 mm. Furthermore, further experiments verified that when the thickness of the first layer 110 and the second layer 120 is set to be at least twice the thickness of the bonding layer 130, because the first and second layers 110 and 120 have sufficient thickness, even if there are slight deviations in temperature control or heating time during the remelting process of the bonding layer 130, it is not easy for the components of the bonding layer 130 to excessively diffuse into the first and second layers 110 and 120. The excessive diffusion may cause overall or local elemental imbalance and metallographic deterioration in the first layer 110 and the second layer 120. For example, the diffusion of boron or silicon may cause grain boundary brittleness or elemental segregation, thereby reducing the overall performance of the first layer 110 and the second layer 120.
[0049] Furthermore, when the thickness of the bonding layer 130 is selected to fall within the range of 0.01 mm to 0.5 mm, the bonding layer 130 possesses the easy heating and melting characteristics naturally inherent in thin-layer metals. This reduces the probability of porosity arising during cooling due to uneven melting of the bonding layer 130. Additionally, the elastic deformation of the thin-layer metal can offset some of the internal stress, resulting in a tighter metallurgical bond between the bonding layer 130 and the first layer 110 and the second layer 120. Typically, the porosity of the bonding layer 130 does not exceed 5%, and the separation strength between the first layer 110 and the second layer 120 is greater than 300 MPa.
[0050] In the embodiment shown in Figure 1A, the first layer 110, the second layer 120, and the bonding layer 130 of the multilayer metal composite molded product 10 are all flat. In other embodiments, depending on the function corresponding to the multilayer metal composite molded product, the multilayer metal composite molded product can be implemented in other shapes. Please refer to Figure 2, which is a cross-sectional structural schematic diagram of another specific embodiment of the multilayer metal composite molded product according to the present invention. Similar to the embodiment shown in Figure 1A, the multilayer metal composite molded product 20 has a first layer 210, a second layer 220, and a bonding layer 230 with an arc-shaped cross section. The bonding layer 230 forms a metallurgical bond with the first layer 210 and the second layer 220, respectively. The multilayer metal composite molded product 20 shown in Figure 2 can be used in the production of chemical products. The cavity formed by the second layer 220 contains a corrosive liquid for participating in the chemical reaction. Accordingly, the material of the second layer 220, i.e., the second alloy, should be a corrosion-resistant alloy.
[0051] In most application scenarios, the multilayer metal composite molded product of the present invention often has an inner cavity, which is formed by the extension and enclosure of the first layer or the second layer. A typical embodiment is that the multilayer metal composite molded product is a metal composite tube. Please refer to FIG3A, which is a cross-sectional structural schematic diagram of another specific embodiment of the multilayer metal composite molded product according to the present invention. In the specific embodiment shown in FIG3A, the multilayer metal composite molded product is a metal composite tube 30, which has a first layer 310, a second layer 320 and a bonding layer 330. The bonding layer 330 forms a metallurgical bond with the first layer 310 and the second layer 320 respectively, so that the first layer 310 forms an interface bond with the second layer 320 through the bonding layer 330. The first layer 310 extends and encloses to form the base pipe of the metal composite pipe 30, and the second layer 320 extends and encloses to form the inner liner of the metal composite pipe 30. The inner wall of the inner liner forms the inner cavity 340. The typical application scenario of this metal composite pipe 30 is for closed transportation of high-temperature flue gas discharge, oil and gas transportation, and strong oxidizing media transportation. In these application scenarios, the inner cavity 340 is filled with highly corrosive media (such as flue gas or combustible gas containing particulate matter, crude oil, strong oxidizing wet chlorine gas, etc.). Therefore, the corrosion source of the metal composite pipe 30 mainly exists in its inner cavity 340.
[0052] Accordingly, the first alloy constituting the first layer 310 can be a low-cost alloy, typically including any or all of carbon steel and iron-based alloys; the second alloy constituting the second layer 320 needs to have sufficient corrosion resistance, therefore a higher-cost alloy should be selected, typically including any, any combination of, or all of alloy steel, 316L stainless steel, nickel-based alloys, cobalt-based alloys, and titanium alloys. The third alloy constituting the bonding layer 330 should have a melting point lower than the first alloy and the second alloy, typically including any, any combination of, or all of nickel-based alloys, cobalt-based alloys, and iron-based alloys doped with boron and / or silicon. It is known to those skilled in the art that doping nickel-based / cobalt-based / iron-based alloys with boron and / or silicon can effectively reduce the melting point of the nickel-based / cobalt-based / iron-based alloys, and controlling the amount of boron and / or silicon doping can adjust the temperature difference between the melting point of the third alloy and the melting points of the first alloy and the second alloy.
[0053] In manufacturing the metal composite pipe 30, a common method is to spray a layer of the third alloy onto the outer surface of the inner liner formed in the second layer 320 to form a bonding layer 330. Then, the inner liner is inserted into the base pipe formed in the first layer 310 with an interference fit. The multi-layer pipe, which consists of the base pipe, the bonding layer 330, and the inner liner, is further heat-treated to remelt the bonding layer 330 and form a metallurgical bond with the first layer 310 and the second layer 320, respectively. According to the specific composition of the first alloy, the second alloy, and the third alloy listed in this specific embodiment, the melting point of the first alloy is the same as or close to that of elemental iron, i.e., not higher than 1538°C. The melting point of the second alloy typically falls within the range of 1290°C to 1450°C. The melting point of the third alloy is preferably adjusted to fall within the range of 850°C to 1100°C. Therefore, in this specific embodiment, preferably, the ratio of the melting point of the third alloy to that of the first alloy is 0.55 to 0.715, and the ratio of the melting point of the third alloy to that of the second alloy is 0.586 to 0.853. The selection of the melting points of each layer is beneficial to improving the yield rate when manufacturing the metal composite pipe 30.
[0054] The implementer of this specific embodiment can select the material of the second alloy according to the type of corrosive medium in the inner cavity 340. For example, austenitic stainless steel (e.g., 316L stainless steel) can be selected to deal with salt spray corrosion, duplex stainless steel can be selected to deal with scouring corrosion and chloride ion corrosion, Hastelloy, a nickel-based alloy, can be selected to deal with high-temperature flue gas corrosion, acidic gas corrosion, and boiling strong acid corrosion, TA2 titanium alloy can be selected to deal with brine corrosion and chloride ion stress corrosion, and Stellite, a cobalt-based alloy, can be selected to deal with the coexistence of chemical corrosion and wear corrosion. Therefore, the selection of the material of the second alloy is highly related to the working environment of the metal composite pipe 30 and can be flexibly selected according to the actual situation. This invention does not limit this.
[0055] Similar to the specific embodiment shown in Figure 1A, in this specific embodiment of the metal composite pipe 30, the thickness of the bonding layer 330 ranges from 0.01 mm to 0.5 mm, and the thickness of the first layer 310 and the second layer 320 is at least twice the thickness of the bonding layer 330. More typically, since the first layer 310 is used to form the base pipe of the metal composite pipe 30, and the strength of the base pipe is positively correlated with the strength of the metal composite pipe 30, the thickness of the first layer 310 is preferably from 3 mm to 20 mm; the second layer 320 forms the inner liner of the metal composite pipe 30, and the thickness of the inner liner is positively correlated with the corrosion resistance of the metal composite pipe 30, while also taking into account the economic cost of manufacturing, the thickness of the second layer 320 is preferably from 1 mm to 3 mm. Based on the selection of the thickness range of each layer, in this specific embodiment, preferably, the thickness of the first layer 310 is 6 to 2000 times the thickness of the bonding layer 330, and the thickness of the second layer 320 is 2 to 300 times the thickness of the bonding layer 330.
[0056] Similar to the specific embodiment shown in Figure 1A, in this specific embodiment, when the thicknesses of the first layer 330, the second layer 320, and the bonding layer 330 meet the values defined above, the porosity of the bonding layer 330 does not exceed 5%, and the separation strength of the first layer 310 and the second layer 320 is greater than 300 MPa.
[0057] Please refer to Figure 3B, which is a cross-sectional view of the specific embodiment shown in Figure 3A. In the metal composite pipe 30 shown in Figure 3B, the thickness of the first layer 310 is about 10 mm, the thickness of the second layer 320 is about 2 mm, and the thickness of the bonding layer 330 is about 0.1 mm. The first layer 310, the second layer 320, and the bonding layer 330 all have a basically uniform thickness. This consistency in thickness is also beneficial to improving the yield rate when manufacturing the metal composite pipe 30.
[0058] Please refer to Figure 3C, which is an enlarged metallographic view of the specific embodiment shown in Figure 3B. More specifically, the metallographic structure shown in Figure 3C is the metallographic state of the first layer 310 after it is bonded to the second layer 320 through the bonding layer 330 in the metal composite tube 30 shown in Figure 3B. It can be seen that the bonding layer 330 forms a dense metallurgical bond with both the first layer 310 and the second layer 320, resulting in sufficient bonding strength between them. This bonding strength can approach the shear strength of the first layer 310 and the second layer 320, reaching a maximum of approximately 450 MPa.
[0059] A flattening test performed on the metal composite pipe 30 shown in Figure 3B also demonstrates that the first layer 310 and the second layer 320 have sufficiently high bonding strength. Even with significant shear stress generated due to deformation, the first layer 310 and the second layer 320 will not delaminate. Please refer to Figure 3D, which is a photograph of the flattening test performed on the specific embodiment shown in Figure 3B. After applying radial pressure to the metal composite pipe 30 and deforming it to the state shown in Figure 3D, the first layer 310 and the second layer 320 still maintain interfacial bonding.
[0060] As mentioned earlier, a typical embodiment of the multilayer metal composite molded product according to the present invention is implemented as a metal composite pipe. However, it is clear that the metal composite pipe is not limited to the structure provided in the specific embodiment of FIG3B. In the specific embodiment of FIG3B, the function of the second layer 320 is defined as a corrosion-resistant layer, which is for the case where the metal composite pipe 30 is used to transport corrosive media, that is, the corrosion source is mainly located in its inner cavity 340. In other application scenarios, the metal composite pipe needs to deal with the situation where there is a corrosion source in its installation environment, that is, the corrosion source comes from the outside of the metal composite pipe. For these application scenarios, it is obviously necessary to consider corrosion-resistant treatment of the outer layer of the metal composite pipe. Please refer to FIG4, which is a cross-sectional structural schematic diagram of another specific embodiment of the multilayer metal composite molded product according to the present invention. As shown in FIG4, the metal composite pipe 40 has a first layer 410, a second layer 420 and a bonding layer 430. The bonding layer 430 forms a metallurgical bond with the first layer 410 and the second layer 420, so that the first layer 410 forms an interface bond with the second layer 420 through the bonding layer 430. The first layer 410 extends and encloses to form the outer sleeve of the metal composite pipe 40, and the second layer 420 extends and encloses to form the base pipe of the metal composite pipe 40. The inner wall of the base pipe encloses to form an inner cavity. The function of the outer sleeve is to provide a corrosion-resistant layer on the outside of the base pipe. Therefore, a typical application scenario for this metal composite pipe 40 is to transport weakly corrosive media in a closed environment under working conditions where there are many corrosive factors in the external environment. For example, the metal composite pipe 40 is used to construct deep-sea oil and gas pipelines, underwater cooling pipes, fluidized bed walls, and waste incineration combustion chamber walls.
[0061] Accordingly, in this specific embodiment, the first alloy constituting the first layer 410 needs to have sufficient corrosion resistance and can be a higher-cost alloy. Typically, the first alloy includes any, any combination of, or all of alloy steel, 316L stainless steel, nickel-based alloys, cobalt-based alloys, and titanium alloys. The second alloy constituting the second layer 420 can be a lower-cost alloy. Typically, the second alloy includes any or all of carbon steel and iron-based alloys. The third alloy constituting the bonding layer 430 should have a melting point lower than that of the first alloy and the second alloy. Typically, the third alloy includes any, any combination of, or all of nickel-based alloys, cobalt-based alloys, and iron-based alloys doped with boron and / or silicon. According to the specific composition of the first alloy, the second alloy, and the third alloy listed in this specific embodiment, the melting point of the second alloy is the same as or close to that of elemental iron, i.e., not higher than 1538°C. The melting point of the first alloy typically falls within the range of 1290°C to 1450°C. The melting point of the third alloy is preferably adjusted to fall within the range of 850°C to 1100°C. Therefore, in this specific embodiment, preferably, the ratio of the melting point of the third alloy to that of the second alloy is 0.55 to 0.715; and the ratio of the melting point of the third alloy to that of the first alloy is 0.586 to 0.853. The selection of the melting points of each layer is beneficial to improving the yield rate when manufacturing the metal composite pipe 40.
[0062] The implementer of this specific embodiment can select the material of the first alloy according to the working environment of the metal composite pipe 40. The selection of the first alloy is related to the corrosion factors in the working environment of the metal composite pipe 40, and can be flexibly selected according to the actual situation. This invention does not limit this.
[0063] In the metal composite pipe 40 of this specific embodiment, the thickness of the bonding layer 430 ranges from 0.01 mm to 0.5 mm. The first layer 410 serves as a corrosion-resistant layer, with a thickness ranging from 1 mm to 3 mm. Therefore, the thickness of the first layer 410 is 2 to 300 times the thickness of the bonding layer 430. The second layer 420 forms the base pipe of the metal composite pipe 40, with a thickness ranging from 3 mm to 20 mm. Therefore, the thickness of the second layer 420 is 6 to 2000 times the thickness of the bonding layer 430. Based on the selection of the thickness range of each layer, the manufacturing cost, corrosion resistance, and yield of the metal composite pipe 40 can all meet the expected values. The porosity of the bonding layer 430 does not exceed 5%, and the separation strength of the first layer 410 and the second layer 420 is greater than 300 MPa. Preferably, the first layer 410, the second layer 420, and the bonding layer 430 all have a basically uniform thickness. This consistency in thickness also helps to improve the yield of the metal composite pipe 40 during manufacturing.
[0064] Figures 3A and 4 show two specific embodiments of the metal composite pipe, in which the metal composite pipe is implemented as a common cylindrical pipe, and therefore its radial cross-sectional shape is circular. In more specific embodiments, the metal composite pipe can be implemented as other shapes, and correspondingly its radial cross-sectional shape is rectangular, regular polygonal or irregular polygonal. Please refer to Figure 5, which is a cross-sectional structural schematic diagram of another specific embodiment of the multilayer metal composite molded product according to the present invention. Specifically, the multilayer metal composite molded product in this specific embodiment is a square tube 50, which has a first layer 510, a second layer 520 and a bonding layer 530. The bonding layer 530 forms a metallurgical bond with the first layer 510 and the second layer 520 respectively, so that the first layer 510 forms an interface bond with the second layer 520 through the bonding layer 530. The only difference from the specific embodiment shown in Figure 3A is that the cross-sectional shape of the square tube 50 is an approximately rectangular polygon, and the first layer 510, the second layer 520 and the bonding layer 530 can be referred to in the description of the specific embodiment of Figure 3A above, or in the description of the specific embodiment of Figure 4 above. For the sake of simplicity, they will not be described again here.
[0065] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the invention can be implemented in other specific forms without departing from its spirit or essential characteristics. Therefore, the embodiments should be considered illustrative and non-limiting, and the scope of the invention is defined by the appended claims rather than the foregoing description. All variations within the meaning and scope of equivalents of the claims are embraced within the present invention. No reference numerals in the claims should be construed as limiting the scope of the claims. Furthermore, it is clear that the word "comprising" does not exclude other components, elements, or steps, and the singular does not exclude the plural.
[0066] This invention provides a multilayer metal composite molded product with a multilayer structure. A bonding layer is disposed between a first layer and a second layer, forming a metallurgical bond with both the first and second layers. The first layer forms an interface bond with the second layer through the bonding layer. Due to the high strength of the metallurgical bond, the first and second layers have sufficient bonding strength and are not easily separated even after subsequent machining. The thickness of the bonding layer is set to be between 0.01 mm and 0.5 mm, which can effectively save materials while ensuring the metallurgical bond strength and reduce the manufacturing cost of the multilayer metal composite molded product. Furthermore, the thickness of the first and second layers is set to be at least twice the thickness of the bonding layer, which facilitates the control of the diffusion uniformity of the bonding layer during heat treatment and avoids excessive diffusion of the components of the bonding layer into the first and second layers during the formation of the metallurgical bond. Excessive diffusion would affect the performance of the first and second layers themselves.
[0067] The above-disclosed embodiments are merely some preferred embodiments of the present invention and should not be construed as limiting the scope of the present invention. Equivalent variations made in accordance with the claims of the present invention are still within the scope of the present invention.
Claims
1. A multilayer metal composite molded product, the molded product comprising a first layer, a second layer, and a bonding layer, wherein: The first layer has a first surface facing the second layer, and the material of the first layer is a first alloy; The second layer has a second surface facing the first layer, the second layer conformally covers the first surface, and the material of the second layer is a second alloy; The bonding layer is disposed between the first surface and the second surface, and forms a metallurgical bond with the first surface and the second surface respectively. The material of the bonding layer is a third alloy, and the melting point of the third alloy is lower than that of the first alloy and the second alloy. The first layer is bonded to the second layer through the bonding layer, and the separation strength between the first layer and the second layer is not less than 137 MPa; The thickness of the bonding layer ranges from 0.01 mm to 0.5 mm, and the thickness of the first layer and the thickness of the second layer are at least twice the thickness of the bonding layer.
2. The molded product according to claim 1, wherein: The molded product has an internal cavity; The inner cavity is formed by the extension of either the first layer or the second layer.
3. The molded product according to claim 2, wherein: The molded product is a metal composite pipe; The first layer extends and encloses to form the base pipe of the metal composite pipe; The second layer extends and encloses to form the inner lining of the metal composite pipe; The inner wall of the liner tube encloses and forms the inner cavity.
4. The molded product according to claim 3, wherein: The thickness of the first layer is 6 to 2000 times the thickness of the bonding layer; The thickness of the second layer is 2 to 300 times the thickness of the bonding layer.
5. The molded product according to claim 3, wherein: The ratio of the melting point of the third alloy to that of the first alloy is 0.55 to 0.715; The ratio of the melting point of the third alloy to that of the second alloy is 0.586 to 0.
853.
6. The molded product according to claim 5, wherein: The first alloy includes any or all of carbon steel and iron-based alloys; The second alloy includes any, any combination of, or all of the following: alloy steel, 316L stainless steel, nickel-based alloys, cobalt-based alloys, and titanium alloys; The third alloy includes any, any combination of, or all of the following: nickel-based alloys, cobalt-based alloys, and iron-based alloys doped with boron and / or silicon.
7. The molded product according to claim 2, wherein: The molded product is a metal composite pipe; The first layer extends and encloses to form the outer sleeve of the metal composite pipe; The second layer extends and encloses to form the base pipe of the metal composite pipe; The inner wall of the base tube encloses and forms the inner cavity.
8. The molded product according to claim 7, wherein: The thickness of the first layer is 2 to 300 times the thickness of the bonding layer; The thickness of the second layer is 6 to 2000 times the thickness of the bonding layer.
9. The molded product according to claim 7, wherein: The ratio of the melting point of the third alloy to that of the second alloy is 0.55 to 0.715; The ratio of the melting point of the third alloy to that of the first alloy is 0.586 to 0.
853.
10. The molded product according to claim 9, wherein The first alloy includes any, any combination of, or all of the following: alloy steel, 316L stainless steel, nickel-based alloys, cobalt-based alloys, and titanium alloys; The second alloy includes any or all of carbon steel and iron-based alloys; The third alloy includes any, any combination of, or all of the following: nickel-based alloys, cobalt-based alloys, and iron-based alloys doped with boron and / or silicon.
11. The molded product according to claim 3 or 7, wherein: The radial cross-sectional shape of the metal composite pipe is circular, rectangular, regular polygonal, or irregular polygonal; The first layer, the second layer, and the bonding layer all have a substantially uniform thickness.
12. The molded product according to claim 1, 4 or 8, wherein: The porosity of the bonding layer does not exceed 5%; The separation strength between the first layer and the second layer is greater than 300 MPa.