Recycled resin production method, production device, control device, control method, and computer program

The method and apparatus enhance the precision of viscosity adjustment in recycled resin production by measuring resin composition and viscosity, and dynamically controlling additive supply, addressing the inconsistency issues in existing technologies.

WO2026235088A1PCT designated stage Publication Date: 2026-11-12MITSUI CHEMICALS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2026/017067
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-08
Filing Date
2026-04-30
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Existing methods for regenerating recycled resin pellets struggle with accurately adjusting the melt flow rate (MFR) and viscosity due to variations in resin composition, particularly when mixed with reactive additives like peroxides, leading to inconsistencies in resin properties.

Method used

A method and apparatus that involve measuring resin composition and viscosity during the kneading process, calculating the required amount of reactive additives, and adjusting their supply to achieve precise viscosity control through a control device and kneading units, utilizing sensors and a control system to monitor and adjust resin properties in real-time.

Benefits of technology

Improves the accuracy of adjusting resin viscosity in recycled resin production, ensuring consistent quality by dynamically controlling the addition of reactive additives based on real-time measurements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2026017067_12112026_PF_FP_ABST
    Figure JP2026017067_12112026_PF_FP_ABST
Patent Text Reader

Abstract

Provided is a recycled resin production method comprising: kneading a recovered resin by using a first kneader 10; measuring a first measurement value related to the composition of the kneaded recovered resin by using a first measurement unit K1; measuring a second measurement value related to a first viscosity of the kneaded recovered resin by using a second measurement unit K2; calculating, by using a control device 30 and on the basis of the first measurement value and the second measurement value, a control amount which includes a type and an addition amount of a reactive additive for adjusting the first viscosity; adjusting the type and the addition amount on the basis of the control amount to supply, from a supply unit 28B, the reactive additive; and kneading the recovered resin discharged from the first kneader 10 and the reactive additive supplied from the supply unit 28B by using a second kneader 20.
Need to check novelty before this filing date? Find Prior Art

Description

Recycled resin production method, production apparatus, control apparatus, control method, and computer program

[0001] The present invention relates to a recycled resin production method, production apparatus, control apparatus, control method, and computer program for kneading resin.

[0002] Methods for collecting and reusing resin components recovered from discarded products (consumer materials), resin components discharged in manufacturing processes (off-grade materials), and the like have been studied (hereinafter, the recovered resin components are simply referred to as "recovered resin", and the resin component obtained by regenerating the recovered resin is simply referred to as "recycled resin"). Recovered resins differ in their form, physical properties, and other characteristics, leading to variations in the melt flow rate (MFR) that indicates their properties. For this reason, it has been difficult to regenerate recovered resin into pellets having a predetermined MFR.

[0003] Patent Document 1 discloses a granulator comprising: a first extruder that extrudes a first molten resin obtained by melting and kneading recovered resin; a measuring instrument that measures the melt flow rate (MFR) indicating the properties of the first molten resin; a second extruder that adds an additive resin whose supply amount is adjusted based on the MFR to the first molten resin, kneads the mixture, and extrudes a second molten resin having a predetermined MFR; and a pelletizer that forms the second molten resin into granular resin.

[0004] Japanese Unexamined Patent Publication No. 2019-65092

[0005] According to the technique described in Patent Document 1, it is possible to obtain recycled resin pellets having a predetermined MFR and viscosity from recovered resin. However, the recovered resin is a mixture of multiple types of resins, which have different reactivities with reactive additives such as peroxides, and there is room for improvement in order to adjust the viscosity with higher accuracy than the technique described in Patent Document 1.

[0006] In view of the above circumstances, the present invention aims to provide a recycled resin production method, a recycled resin production apparatus, a control apparatus, a control method, and a computer program capable of improving the accuracy of adjusting the resin viscosity of recycled resin.

[0007] (1) One aspect of the present disclosure is a method for producing recycled resin, comprising: kneading a recovered resin with a first kneader; measuring a first measurement value relating to the composition of the kneaded recovered resin with a first measuring unit; measuring a second measurement value relating to the first viscosity of the kneaded recovered resin with a second measuring unit; calculating a control amount, including the type and amount of reactive additive for adjusting the first viscosity, based on the first and second measurement values, with a control device; supplying the reactive additive with the type and amount adjusted based on the control amount with a supply unit; and kneading the recovered resin extruded from the first kneader and the reactive additive supplied by the supply unit with a second kneader.

[0008] (2) The method for producing recycled resin as described in item (1), wherein the first measurement value and the second measurement value are measured during the process in which the recovered resin is extruded by the first kneader.

[0009] (3) A method for producing recycled resin according to item (1) or (2), wherein a third measuring unit measures a third measurement value relating to the second viscosity of the recycled resin extruded by the second kneader, and the control device calculates the control amount based on the third measurement value and performs a feedback process to control the supply unit.

[0010] (4) A method for producing recycled resin according to any one of items (1) to (3), comprising generating a dataset including the first measurement value, the second measurement value, the control amount, and information regarding the product lot of the generated recycled resin.

[0011] (5) A method for producing recycled resin according to item (3), comprising generating a dataset including the first measurement value, the second measurement value, the third measurement value, the control amount, and information regarding the product lot of the generated recycled resin.

[0012] (6) A method for producing recycled resin according to any one of items (1) to (5), wherein the spectrum of the recovered resin is measured as the first measurement value by the first measuring unit.

[0013] (7) One aspect of the present disclosure is a recycled resin manufacturing apparatus comprising: a first kneader for kneading a recovered resin; a first measuring unit for measuring a first measurement value relating to the composition of the recovered resin kneaded in the first kneader; a second measuring unit for measuring a second measurement value relating to a first viscosity of the recovered resin kneaded in the first kneader; a second kneader for adding a reactive additive for adjusting the viscosity of the resin to the recovered resin extruded from the first kneader and kneading it; a supply unit for adding the reactive additive to the second kneader; and a control device for calculating a control amount including the type and amount of the reactive additive based on the first and second measurement values, and controlling the supply unit based on the control amount to supply the reactive additive to the second kneader.

[0014] (8) The apparatus for manufacturing recycled resin according to item (7), wherein the second kneader has a third measuring unit for measuring the second viscosity of the recycled resin.

[0015] (9) One aspect of the present disclosure is a control device connected to a recycled resin manufacturing apparatus, which comprises: a first kneader for kneading a recovered resin; a first measuring unit for measuring a first measurement value relating to the composition of the recovered resin kneaded in the first kneader; a second measuring unit for measuring a second measurement value relating to a first viscosity of the recovered resin kneaded in the first kneader; a second kneader for adding a reactive additive for adjusting the viscosity of the resin to the recovered resin extruded from the first kneader and kneading it; and a supply unit for adding the reactive additive to the second kneader, the control device comprising: a control unit that calculates a control amount including the type and amount of the reactive additive based on the first measurement value and the second measurement value, and controls the supply unit based on the control amount to supply the reactive additive to the second kneader.

[0016] (10) One aspect of the present disclosure is a control method for a control device connected to a recycled resin manufacturing apparatus, comprising: a first kneader for kneading a recovered resin; a first measuring unit for measuring a first measurement value relating to the composition of the recovered resin kneaded in the first kneader; a second measuring unit for measuring a second measurement value relating to a first viscosity of the recovered resin kneaded in the first kneader; a second kneader for adding a reactive additive for adjusting the viscosity of the resin to the recovered resin extruded from the first kneader and kneading it; and a supply unit for adding the reactive additive to the second kneader, wherein a computer mounted on the control device calculates a control amount including the type and amount of the reactive additive based on the first and second measurement values, and controls the supply unit based on the control amount to supply the reactive additive to the second kneader.

[0017] (11) One aspect of the present disclosure is a computer program for controlling a control device connected to a recycled resin manufacturing apparatus, which comprises: a first kneader for kneading a recovered resin; a first measuring unit for measuring a first measurement value relating to the composition of the recovered resin kneaded in the first kneader; a second measuring unit for measuring a second measurement value relating to a first viscosity of the recovered resin kneaded in the first kneader; a second kneader for adding a reactive additive for adjusting the viscosity of the resin to the recovered resin extruded from the first kneader and kneading it; and a supply unit for adding the reactive additive to the second kneader, wherein the computer program causes a computer mounted on the control device to perform a process of calculating a control amount including the type and amount of the reactive additive based on the first measurement value and the second measurement value, and controlling the supply unit based on the control amount to supply the reactive additive to the second kneader.

[0018] According to the present invention, the accuracy of adjusting the resin viscosity of recycled resin can be improved.

[0019] Figure 1 is a cross-sectional view showing the configuration of the manufacturing apparatus. Figure 2 is a block diagram showing the configuration of the manufacturing apparatus. Figure 3 is a flowchart showing the processing flow of a method for manufacturing recycled resin using the manufacturing apparatus. Figure 4 is a flowchart showing the processing flow executed in the control device.

[0020] As shown in Figure 1, the manufacturing apparatus 1 is configured to be communicatively connected to the control device 30 and to produce recycled resin by adding a reactive additive to the recovered resin and kneading it. The manufacturing apparatus 1 includes, for example, a first kneader 10 that melts and kneads the recovered resin, and a second kneader 20 that adds a reactive additive to the recovered resin extruded from the first kneader 10 and kneads it to produce recycled resin. In the illustrated example, the first kneader 10 and the second kneader 20 are shown to be arranged vertically for convenience, but are not limited to this, and may be arranged based on other arrangement relationships, such as parallel to the ground surface, and the orientation of their arrangement may also be changed as desired.

[0021] The first kneader 10 is equipped with a cylindrical cylinder 12. A cylindrical internal space 12A is formed inside the cylinder 12. The cylinder 12 is heated by a heater (not shown) to melt the resin being introduced. The shape of the internal space 12A of the cylinder 12 is not limited to a cylindrical shape and can be changed according to the shape and / or number of screws 13, which will be described later.

[0022] The cylinder 12 has a first opening 12B that communicates with the outside on the upstream side (-x direction side) of the internal space 12A. The first opening 12B is formed above the cylinder 12 (+z direction). Upstream of the cylinder 12, a hopper 18 is provided to supply resin to the internal space 12A through the first opening 12B. The top of the hopper 18 is open to allow resin material to be fed in. The bottom of the hopper 18 is open to communicate with the first opening 12B. The hopper 18 is formed to guide the fed pelletized or crushed resin material into the inside of the cylinder 12.

[0023] A first supply unit 18A is located above the hopper 18 to supply the recovered resin to the cylinder 12. The recovered resin is resin recovered from waste materials, and is, for example, resin fragments containing a mixture of thermoplastic resins such as polyethylene and polypropylene, which are recovered from waste and separated after crushing by magnetic separation or specific gravity separation. The types and ratios of resin fragments contained in the recovered resin are unknown. Therefore, the viscosity of the recovered resin after it has been melted and kneaded is unknown. Reactive additives, as described later, are added to the recovered resin to adjust its viscosity. Alternatively, the first supply unit 18A may be omitted, and the recovered resin may be supplied to the cylinder 12 manually.

[0024] The recovered resin is not particularly limited as long as it is resin recovered from waste products; it may be post-consumer recycled material (PCR material) or post-industrial recycled material (PIR material; also called pre-consumer recycled material). Furthermore, in the following explanation, resin obtained by processing recovered resin for reuse will be referred to as "recycled resin."

[0025] The first supply unit 18A has a storage unit 18A1 for temporarily storing the recovered resin before supplying it. The storage unit 18A1 has a stirrer 18A2 for stirring the recovered resin. The stirrer 18A2 is configured to stir the recovered resin when it falls from the storage unit 18A1. The stirrer 18A2 is composed of dry blenders such as a tumble mixer, V-blender, ribbon blender, double-roll mixer, shaker, and buffer tank with internal rotor blades. The stirrer 18A2 is configured to drop the stirred recovered resin fragments downwards from below.

[0026] The hopper 18 receives the recovered resin from the first supply unit 18A and supplies the recovered resin into the cylinder 12. The hopper 18 may be supplied with additives such as stabilizers, antioxidants, and nucleating agents, reinforcing fiber materials such as glass fibers, carbon fibers, and organic fibers, rubber or talc, and fillers such as calcium carbonate.

[0027] The cylinder 12 has a lid portion 12D that closes the upstream side of the internal space 12A. The cylinder 12 has a resin outlet 12C on the downstream (+x direction) side, which has a conical surface formed such that its diameter decreases towards the downstream side of the internal space 12A. The downstream side of the resin outlet 12C is open. A filtration section 16 is located downstream of the resin outlet 12C to remove foreign matter contained in the kneaded recovered resin. The filtration section 16 filters the kneaded resin composition.

[0028] The filtration section 16 is composed of a filter that removes foreign matter such as soil or sand contained in the recovered resin. The filtration section 16 suppresses the incorporation of foreign matter into the recovered resin. Any filter can be used in the filtration section 16 as long as it can filter the resin and remove foreign matter. Downstream of the filtration section 16 is an extrusion section 15 that extrudes the kneaded recovered resin.

[0029] An internal space 15A is formed inside the extrusion section 15. A gear pump 15B capable of pushing the recovered resin downstream is located in the internal space 15A. By using the gear pump 15B, the amount of resin discharged in the extrusion section 15 is accurately measured. Downstream of the extrusion section 15, a die 17 is provided for pushing the recovered resin into the external space. A resin channel 17A is formed in the die 17 through which the extruded recovered resin flows.

[0030] The resin channel 17A is a channel through which the recovered resin extruded from the extrusion section 15 flows in a molten state. The resin channel 17A may be provided with a heater (not shown) for heating the flowing recovered resin. The resin channel 17A is provided with a first measurement unit K1 for measuring a first measurement value regarding the composition of the kneaded recovered resin. In one example, the first measurement unit K1 is an infrared sensor that measures the spectrum of reflected light from the recovered resin by irradiating it with near-infrared light. In another example, the first measurement unit K1 is an optical sensor that measures the spectrum of Raman scattered light from the recovered resin by irradiating it with monochromatic laser light. According to the first measurement value, the type of resin contained in the recovered resin can be estimated by analyzing the spectral components. The Raman scattered light spectrum is preferable because it is less affected by moisture or temperature changes, shows high sensitivity to bonds C=C, C≡C, and S-S, and is suitable for reactive groups that are difficult to observe with infrared reflected light spectra.

[0031] The first measurement unit K1 may use any device capable of measuring the composition of the recovered resin, such as an infrared or optical sensor, an apparatus for analyzing the structure of the recovered resin based on nuclear magnetic resonance (NMR), an apparatus for analyzing the structure of the recovered resin based on pyrolysis gas chromatography-mass spectrometry (Py-GC-MS), an apparatus for analyzing the structure of the recovered resin based on chemical analysis, or an apparatus for analyzing the structure of the recovered resin based on chemical sensors such as an electron nose (e-Nose) or one or more suspended microchannel resonators (SMR). Multiple of the above devices may be provided as the first measurement unit K1, and the analysis data obtained from multiple devices may be combined using models such as partial least squares regression (PLS regression) or artificial neural networks (ANN) to measure the composition of the recovered resin.

[0032] The resin channel 17A is provided with a second measuring unit K2 for detecting a second measurement value related to the viscosity (first viscosity) of the kneaded recovered resin. The second measurement value may be, for example, the first viscosity itself, or a parameter of the kneaded recovered resin from which the first viscosity can be derived using a known relational formula. The second measuring unit K2 is, for example, an inline viscometer that takes out at least a portion of the recovered resin kneaded by the first kneader 10 and measures its viscosity. The second measuring unit K2 may be composed of other sensors as long as they can detect the viscosity of the recovered resin obtained by melt-kneading by the first kneader 10.

[0033] The first measurement value and the second measurement value are measured during the process in which the recovered resin is extruded downstream of the first kneader 10. The first measurement value and the second measurement value are measured simultaneously, for example, by the first measurement unit K1 and the second measurement unit K2. The first measurement value and the second measurement value do not necessarily have to be measured exactly at the same time, and may be measured during a measurement period in which the viscosity of the recovered resin can be measured. The first measurement value and the second measurement value do not necessarily have to be measured in the resin flow path 17A, and may be measured at any other location downstream of the first kneader 10 in which the composition or viscosity of the kneaded recovered resin can be measured. The first measurement unit K1 and the second measurement unit K2 may be located in different positions, and their order of arrangement is not restricted.

[0034] A cylindrical screw 13 is inserted into the internal space 12A of the cylinder 12. Two or more screws 13 may be arranged in parallel. The screw 13 is rotatably positioned within the cylinder. Fins 13A extending spirally in the direction of the axis 13S are formed on the outer wall of the screw 13. The screw 13 has a shaft 13D aligned with the direction of the axis 13S. The shaft 13D is rotatably supported by the cover portion 12D. The shaft 13D is connected to a drive unit 14 that generates rotational driving force.

[0035] The drive unit 14 rotates the screw 13 via the shaft 13D. The drive unit 14 includes, for example, a motor (not shown) that serves as a drive source, and a reduction gear (not shown) that reduces the rotational output of the motor and increases the torque to output rotational driving force. The drive unit 14 may be controlled by the control device 30, or it may be configured to operate at a preset operating timing without being controlled by the control device 30. The control device 30 is configured, for example, to control the first kneader 10 to rotate the screw 13 and push out the kneaded recovered resin. The first kneader 10 may be configured to repeatedly perform predetermined operations at a preset operating timing without being controlled by the control device 30.

[0036] With the above configuration, the recovered resin is supplied to the first kneader 10 from the first supply unit 18A. The recovered resin is supplied into the cylinder 12 via the hopper 18. The recovered resin melts inside the heated cylinder 12. The molten recovered resin fills the space between the screw 13 and the inner wall of the cylinder 12. When the screw 13 is rotated by the drive unit 14, the recovered resin is guided by the fins 13A and pumped downstream while being kneaded.

[0037] The kneaded recovered resin is extruded downstream from the resin outlet 12C and passes through the filtration section 16. After passing through the filtration section 16, the recovered resin is decontaminated and flows into the downstream extrusion section 15. The recovered resin is pushed into the downstream resin flow path 17A by the gear pump 15B of the extrusion section 15. The recovered resin flows through the resin flow path 17A and is pushed into the connecting flow path T provided at the downstream outlet. The connecting flow path T is a flow path through which the kneaded recovered resin flows. The connecting flow path T is formed by a pipeline through which the kneaded recovered resin can flow and connects the downstream side of the first kneader 10 and the upstream side of the second kneader 20. The kneaded recovered resin flows through the connecting flow path T and is pumped to the upstream side of the second kneader 20.

[0038] The second kneader 20 has the same configuration as the first kneader 10. The second kneader 20 is equipped with a cylindrical cylinder 22. A cylindrical internal space 22A is formed inside the cylinder 22. The cylinder 22 is heated by a heater (not shown) to melt the resin being introduced. Note that the shape of the internal space 22A of the cylinder 22 is not limited to a cylindrical shape and can be changed according to the shape and / or number of screws 23, which will be described later.

[0039] The cylinder 22 has a second opening 22B that communicates with the outside on the upstream side (-x direction side) of the internal space 22A. The second opening 22B is formed above the cylinder 22 (+z direction). The recovered resin mixed in the first kneader 10 flows through the connecting channel T and is guided into the inside of the cylinder 22 through the second opening 22B.

[0040] Furthermore, the cylinder 22 has an opening on the upstream side (-x direction side) of the internal space 22A that communicates with the outside and supplies a reactive additive to the cylinder 22 for adjusting the viscosity of the recovered resin. The opening for supplying the reactive additive to the cylinder 22 is formed above the cylinder 22 (+z direction). Upstream of the cylinder 22, a hopper 28 is provided to supply the reactive additive to the internal space 22A. Above the hopper 28, a second supply unit 28B (supply unit) is located to supply the reactive additive to the cylinder 22.

[0041] The reactive additives include a first reactive additive for lowering the viscosity of the recovered resin and a second reactive additive for increasing the viscosity of the recovered resin. Examples of the first reactive additives include chain severing agents that reduce viscosity by severing the molecular chains of the recovered resin, or depolymerizing agents that reduce viscosity by decomposing the recovered resin. Examples of chain severing agents include radical chain severing agents such as peroxides or azo compounds, and oxide chain severing agents such as potassium permanganate or ozone. Examples of depolymerizing agents include acid catalysts such as sulfuric acid or hydrochloric acid, alkaline catalysts such as sodium hydroxide or 4-dimethylaminopyridine, amine catalysts such as ethanolamine or ammonia, and glycol catalysts such as ethylene glycol or propylene glycol.

[0042] For example, radical chain scission agents are suitably used for polypropylene or polyethylene, alkali catalysts are suitably used for polyamides, and glycol catalysts or amine catalysts are suitably used for polyethylene terephthalate. Examples of the second reactive additive include chain extenders that react with molecular chain end groups of the recovered resin to increase viscosity, and crosslinking agents that link the molecular chains of the recovered resin to increase viscosity. Examples of the chain extender include organic peroxides and polyfunctional compounds.

[0043] Examples of the crosslinking agent include epoxy-based crosslinking agents, isocyanate-based crosslinking agents, amino resin-based crosslinking agents, and phenol resin-based crosslinking agents. For example, organic peroxides or isocyanate-based crosslinking agents are suitably used for polypropylene or polyethylene, and polyfunctional epoxy-based compounds are suitably used for polyamides or polyethylene terephthalate.

[0044] The first reactive additive and the second reactive additive are additives that are added to and mixed with the recovered resin to react with the recovered resin and adjust the viscosity of the recovered resin to a predetermined range (target value).

[0045] The second supply unit 28B includes a first reactive additive supply unit 28C that supplies the first reactive additive, and a second reactive additive supply unit 28D that supplies the second reactive additive. The first reactive additive supply unit 28C includes a storage unit 28C1 that stores the first reactive additive, and a stirrer 28C2 that stirs the first reactive additive. The second reactive additive supply unit 28D includes a storage unit 28D1 that stores the second reactive additive, and a stirrer 28D2 that stirs the second reactive additive.

[0046] The second supply unit 28B acquires the control amount output by the control device 30, and operates based on the operation content preset according to the control amount. The second supply unit 28B may be directly controlled by the control device 30 based on the control amount.

[0047] Additives such as stabilizers, antioxidants and crystal nucleating agents, reinforcing fiber materials such as glass fibers, carbon fibers and organic fibers, rubber and talc, as well as fillers such as calcium carbonate may be supplied to the hopper 28. The change in viscosity caused by adding a certain amount of these fillers and the like is within a range that can be predicted by known theoretical formulas or empirical formulas, so the supply of these additives and the like will not make the viscosity of the kneaded recovered resin and the finally obtained recycled resin unpredictable.

[0048] The cylinder 22 has a lid portion 22D that closes the upstream side of the internal space 22A. On the downstream (+x direction) side, the cylinder 22 has a resin outlet 22C formed with a conical surface such that the diameter decreases toward the downstream side of the internal space 22A. The downstream side of the resin outlet 22C is open.

[0049] On the downstream side of the resin outlet 22C, a die 27 is provided that extrudes the recycled resin, which is obtained by kneading the recovered resin and the reactive additive to adjust the viscosity, into the external space. The die 27 is formed with a resin flow path 27A through which the extruded recycled resin flows. At the outlet of the resin flow path 27A, an apparatus (not shown) for extruding the recycled resin into a plurality of strands to produce pellets may be provided. The resin flow path 27A is additionally provided with a third measurement unit K3 that measures a third measured value related to the viscosity (second viscosity) of the recycled resin extruded by the second kneader 20. The third measured value may be, for example, the second viscosity itself, or may be a parameter of the recycled resin from which the second viscosity can be derived by a known relational expression. The third measurement unit K3 is, for example, an in-line viscometer that takes out at least a part of the recycled resin kneaded by the second kneader 20 and measures the viscosity.

[0050] The third measurement unit K3 may be configured with other sensors as long as it can detect the viscosity of the recycled resin obtained by melt-kneading with the second kneader 20. The third measurement unit K3 may be arranged at another position as long as it can detect the viscosity of the recycled resin obtained by melt-kneading with the second kneader 20.

[0051] A cylindrical screw 23 is inserted into the internal space 22A of the cylinder 22. Two or more screws 23 may be arranged in parallel. The screw 23 is rotatably positioned within the cylinder. Fins 23A extending spirally in the direction of the axis 23S are formed on the outer wall of the screw 23. The screw 23 has a shaft 23D aligned with the direction of the axis 23S. The shaft 23D is rotatably supported by the cover portion 22D. The shaft 23D is connected to a drive unit 24 that generates rotational driving force.

[0052] The drive unit 24 rotates the screw 23 via the shaft 23D. The drive unit 24 includes, for example, a motor (not shown) that serves as a drive source, and a reduction gear (not shown) that reduces the rotational output of the motor and increases the torque to output rotational driving force. The drive unit 24 may be controlled by the control device 30, or it may be configured to operate at a preset operating timing without being controlled by the control device 30. The control device 30 is configured, for example, to control the second kneader 20 to rotate the screw 23 and extrude the kneaded recycled resin. The second kneader 20 may be configured to repeatedly perform predetermined operations at a preset operating timing without being controlled by the control device 30.

[0053] With the above configuration, the second kneader 20 is supplied with a reactive additive from the second supply unit 28B. The reactive additive is supplied into the cylinder 22 via the hopper 28. The reactive additive, together with the recovered resin supplied from the connecting flow path T, fills the internal space between the screw 23 and the inner wall of the cylinder 22. When the screw 23 is rotated by the drive unit 24, the recovered resin and reactive additive are guided by the fins 23A and pumped downstream while being kneaded. The kneaded recovered resin and reactive additive react and are extruded downstream from the resin outlet 22C as recycled resin.

[0054] As shown in Figure 2, the control device 30 comprises a control unit 31 that controls the first kneader 10 and the second kneader 20, and a storage unit 32 that stores data and computer programs necessary for control. The control unit 31 is composed of at least one hardware processor such as a CPU (Central Processing Unit). The storage unit 32 is composed of a non-temporary storage medium such as a hard disk drive (HDD) or solid state disk (SSD). The storage unit 32 stores computer programs and data necessary for control.

[0055] The control unit 31 is configured to control the drive unit 14 in the first kneader 10 to rotate the screw 13, to control the first supply unit 18A to supply the recovered resin into the cylinder 12, and to control the extrusion unit 15 to extrude the kneaded recovered resin. The control unit 31 is configured to control the drive unit 24 in the second kneader 20 to rotate the screw 23, to control the second supply unit 28B to supply the reactive additive into the cylinder 22, so that the recovered resin and the reactive additive are kneaded together to produce a regenerated resin through a reaction.

[0056] The first kneader 10 and the second kneader 20 do not necessarily have to be controlled by the control unit 31 and may be configured to perform predetermined operations sequentially. In this case, the control unit 31 may be configured to control the second supply unit 28B based on a first measurement, a second measurement, and optionally a third measurement. The control unit 31 may transmit a control signal to the second supply unit 28B to adjust the type and amount of reactive additive based on the first measurement, the second measurement, and optionally a third measurement, and the second supply unit 28B may be configured to adjust the type and amount of reactive additive based on the control signal.

[0057] The control unit 31 acquires a first measurement value regarding the composition of the recovered resin measured by the first measurement unit K1 and a second measurement value regarding the first viscosity of the recovered resin measured by the second measurement unit K2. Based on the first and second measurement values, the control unit 31 calculates a control amount including the type and amount of reactive additive to adjust the first viscosity of the recovered resin.

[0058] The control quantity may be calculated based on a data table showing the correspondence between first and second measured values, which are set in advance so that the second viscosity of the recycled resin reaches a target value, and the first type and first supply amount of the first reactive additive, as well as the second type and second supply amount of the second reactive additive. Alternatively, it may be calculated based on a calculation formula showing the correspondence between first and second measured values ​​and the type and supply amount of the first reactive additive, as well as the type and supply amount of the second reactive additive. The control quantity may be calculated not only on a data table or calculation formula, but also on a learning model obtained by machine learning or the like.

[0059] The control quantity can be calculated using any method, as long as it can be calculated based on the correspondence between the first measured value, the second measured value, the target value, the first type, the first supply amount, the second type, the second supply amount, etc. Based on the calculated control quantity, the control unit 31 controls the second supply unit 28B to adjust the type and supply amount of the reactive additive, that is, the first type and first supply amount of the first reactive additive and the second type and second supply amount of the second reactive additive, so that the first viscosity of the recovered resin becomes the target value.

[0060] For example, when the viscosity of the recycled resin is to be reduced, the control unit 31 controls the first reactive additive supply unit 28C to determine the first type of first reactive additive according to the composition of the recovered resin and adds the first reactive additive in a predetermined first supply amount. For example, when the viscosity of the recycled resin is to be increased, the control unit 31 controls the second reactive additive supply unit 28D to determine the second type of second reactive additive according to the composition of the recovered resin and adds the second reactive additive in a predetermined second supply amount.

[0061] The control unit 31 may determine whether the viscosity of the recycled resin extruded from the second kneader 20 is the desired viscosity based on the third measured value of the second viscosity of the recycled resin detected by the third measuring unit K3 located downstream of the second kneader 20. Alternatively, the control unit 31 may perform feedback control to adjust the supply amount of reactive additive by controlling the second supply unit 28B so that the second viscosity of the recycled resin extruded from the second kneader 20 reaches the target value, based on the third measured value of the second viscosity.

[0062] In addition, if the control unit 31 obtains a measurement value that detects a disturbance that causes a change in the state of the first kneader 10 and / or the second kneader 20, it may further perform feedforward control to reduce the change in the properties of the recycled resin due to the disturbance and calculate the control amount. The control unit 31 may update the parameters included in the calculation formula for calculating the control amount to reduce the error between the third measurement value and the target viscosity value. For example, the least squares method or robust estimation method may be used to adjust the parameters, but any calculation method that can reduce the error may be used. The control unit 31 may adjust the control parameters for controlling the supply amount of the second supply unit 28B to reduce the error between the third measurement value and the target value.

[0063] The control unit 31 adjusts the control parameters of the first reactive additive supply unit 28C to increase the supply amount of the first reactive additive if, for example, the second viscosity based on the third measurement value is higher than the target value. The control unit 31 also adjusts the control parameters of the second reactive additive supply unit 28D to increase the supply amount of the second reactive additive if, for example, the second viscosity based on the third measurement value is lower than the target value. Here, the target value may be not only a single viscosity value, but also a numerical range that includes viscosity values.

[0064] The control unit 31 may, if using a data table, update the data in the data table to reduce the error between the third measured value of the recycled resin and the target value, or, if using a learning model obtained by machine learning, perform machine learning using the third measured value to update the learning model.

[0065] Figure 3 shows the process flow of a method for manufacturing recycled resin using the manufacturing apparatus 1. In the manufacturing apparatus 1, the recovered resin supplied from the first supply unit 18A is melted and kneaded in the first kneader 10 (S100). The first measuring unit K1 measures a first measurement value regarding the composition of the kneaded recovered resin (S102). The first measuring unit K1 measures, for example, the spectrum and chemical properties of the recovered resin as first measurement values. The second measuring unit K2 measures a second measurement value regarding the first viscosity of the kneaded recovered resin (S104). From the viewpoint of further improving the accuracy of adjusting the resin viscosity of the recycled resin, it is preferable that the measurement of the first measurement value (S102) and the measurement of the second measurement value (S104) be performed inline in the manufacturing apparatus 1, but they may also be measured offline. As a specific example of offline measurement, a first measurement unit K1 and a second measurement unit K2 may be located away from the first kneader 10 and the second kneader 20, and a portion of the recovered resin kneaded by the first kneader 10 may be sampled to measure the first and second measurement values.

[0066] The first measurement value and the second measurement value are measured simultaneously by the first measurement unit K1 and the second measurement unit K2 during the process in which the recovered resin is extruded by the first kneader, or during a measurement period in which the viscosity of the recovered resin can be measured. Based on the first measurement value and the second measurement value, the control unit 31 calculates a control amount including the type and amount of reactive additive to adjust the first viscosity of the recovered resin (S106). The second supply unit 28B adjusts the supply amount including the type and amount of reactive additive based on the control amount and supplies the reactive additive to the second kneader 20 (S106).

[0067] At this time, the control unit 31 may control the second supply unit 28B (supply unit) based on the control amount to adjust the amount of reactive additive supplied, or the second supply unit 28B may adjust the amount of reactive additive supplied based on the control amount. In S106, the control unit 31 can perform dynamic processing. Specifically, the first measuring unit K1 and the second measuring unit K2 can continue to measure the first and second measured values, respectively, and the control unit 31 may dynamically calculate or determine the control amount in accordance with the first and second measured values ​​recorded in the storage unit 32 as needed, the first and second measured values ​​input to the control unit 31 as needed, or the third measured value fed back from the third measuring unit K3 as needed. The control unit 31 uses the second kneader 20 to knead the recovered resin extruded from the first kneader 10 and the reactive additive supplied by the second supply unit 28B and react them (S110). The second kneader 20 generates and extrudes the recycled resin (S112).

[0068] The control unit 31 generates a dataset containing a first measurement value, a second measurement value, a control variable, and information regarding the product lot of the generated recycled resin, and stores it in the storage unit 32. The dataset may be used for quality control of the recycled resin, or it may be used as a database of training data for updating the parameters of a machine learning model.

[0069] The control unit 31 may measure the properties of the recycled resin and perform feedback control. The third measuring unit K3 measures a third measured value relating to the second viscosity of the recycled resin extruded by the second kneader 20 (S114). Based on the third measured value, the control unit 31 calculates a control amount for the second supply unit 28B (S116). The second supply unit 28B performs feedback processing, supplying reactive additives to the second kneader 20 by adjusting the supply amount, including the type and amount of additive, based on the control amount (S118). From the viewpoint of further improving the accuracy of adjusting the viscosity of the recycled resin, it is preferable that the measurement of the third measured value (S114) be performed in-line in the manufacturing apparatus 1, but it may also be measured offline. As a specific example of offline measurement, the third measuring unit K3 may be located away from the second kneader 20, and a portion of the recycled resin kneaded by the second kneader 20 may be sampled to measure the third measured value.

[0070] The control unit 31 may measure the properties of the recycled resin, monitor the progress of the reaction between the recovered resin and the reactive additive (reaction progress of the recycled resin), and perform feedback control. The fourth measuring unit (not shown, but hereinafter referred to as "K4") measures a fourth measurement value related to the reaction progress of the recycled resin extruded by the second kneader 20. The fourth measuring unit K4 can use the same apparatus as the first measuring unit K1. Similarly, the fourth measurement value may be, for example, a spectrum or chemical property value measured during the reaction of the recycled resin. It is preferable that the fourth measurement value be measured in-line in the manufacturing apparatus 1, but it may also be measured offline. As a specific example of offline measurement, the fourth measuring unit K4 may be located away from the second kneader 20, and a portion of the recycled resin kneaded by the second kneader 20 may be sampled to measure the fourth measurement value.

[0071] The second kneader 20 mixes and reacts the recovered resin extruded from the first kneader 10 with the reactive additive supplied by the second supply unit 28B to produce and extrude recycled resin. The control unit 31 generates a dataset including a first measurement value, a second measurement value, optionally a third measurement value and / or a fourth measurement value, a control amount, and information regarding the product lot of the produced recycled resin, and stores it in the storage unit 32. The dataset may be used for quality control of the recycled resin, or it may be used as a database of training data for updating the parameters of a machine learning model. The manufacturing apparatus 1 repeatedly performs the above process to produce recycled resin. The control unit 31 may collect multiple datasets from multiple other factory facilities where the manufacturing apparatus 1 is installed and generate a database of training data for updating the parameters of a machine learning model.

[0072] Figure 4 shows the process flow of a control method for a control device 30 connected to a recycled resin manufacturing apparatus 1, which comprises a first kneader 10, a first measuring unit K1 for measuring a first measurement value in the first kneader 10, a second measuring unit K2 for measuring a second measurement value related to the first viscosity of the recovered resin, a second kneader 20, and a second supply unit 28B for adding a reactive additive to the second kneader 20. The control method is executed based on a computer program installed in the computer mounted on the control device 30.

[0073] The computer program causes the control unit 31 of the control device 30 (for example, a computer or its processor) to perform the following processes. The control method is applied when the control device 30 is communicatively connected to the manufacturing device 1 and performs a process to calculate the control amount required for the manufacturing device 1, but does not directly control all of the operation of the manufacturing device 1.

[0074] The control unit 31 calculates a control amount, including the type and amount of reactive additive, based on the first and second measured values ​​(S200). The control unit 31 outputs the calculated control amount to the second supply unit 28B, which directly or indirectly controls to adjust the supply amount of reactive additive and supply it to the second kneader 20 (S202).

[0075] As described above, the recycled resin manufacturing apparatus 1 can improve the accuracy of adjusting the resin viscosity of the recycled resin by calculating a control amount, including the type and amount of reactive additive supplied in the second kneader 20, based on a second measurement value for the first viscosity of the recovered resin and a first measurement value for the properties of the recovered resin in the first kneader 10. The control device 30 can provide feedback control to the second supply unit 28B based on a third measurement value from the third measurement unit K3 and / or a fourth measurement value from the fourth measurement unit K4, which are located downstream of the second kneader 20.

[0076] According to the control device 30, parameters such as the calculation formula for calculating the viscosity of the recycled resin based on the third measurement value of the third measurement unit K3, and parameters and data necessary for control such as the data table can be updated, thereby reducing the error between the actual viscosity of the recycled resin and the estimated result.

[0077] This application is a priority application claiming based on Japanese Patent Application No. 2025-077955, filed on 8 May 2025, and the claims, specification and drawings of said Japanese Patent Application are incorporated herein by reference.

[0078] 1 Manufacturing equipment, 10 First kneader, 12 Cylinder, 12A Internal space, 12B First opening, 12C Resin outlet, 12D Lid, 13 Screw, 13A Fin, 13D Shaft, 13S Axle, 14 Drive unit, 15 Extrusion unit, 15A Internal space, 15B Gear pump, 16 Filtration unit, 17 Die, 17A Resin flow path, 18 Hopper, 18A First supply unit, 18A1 Storage unit, 18A2 Agitator, 20 Second kneader, 22 Cylinder, 22A Internal space, 22B Second opening, 22C Resin outlet, 22D Lid, 23 Screw, 23A Fin, 23D Shaft, 23S Axle, 24 Drive unit, 27 Die, 27A Resin flow path, 28 Hopper, 28B Second supply unit, 28C First reactive additive supply unit, 28C1 Storage unit, 28C2 Stirrer, 28D Second reactive additive supply unit, 28D1 Storage unit, 28D2 Stirrer, 30 Control device, 31 Control unit, 32 Memory unit, K1 First measuring unit, K2 Second measuring unit, K3 Third measuring unit, T Connecting channel

Claims

1. A method for producing recycled resin, comprising: kneading the recovered resin with a first kneader; measuring a first measurement value regarding the composition of the kneaded recovered resin with a first measuring unit; measuring a second measurement value regarding the first viscosity of the kneaded recovered resin with a second measuring unit; calculating a control amount, including the type and amount of reactive additive for adjusting the first viscosity, based on the first and second measurement values, using a control device; supplying the reactive additive with its type and amount adjusted based on the control amount using a supply unit; and kneading the recovered resin extruded from the first kneader and the reactive additive supplied by the supply unit using a second kneader.

2. The method for producing recycled resin according to claim 1, wherein the first measurement value and the second measurement value are measured during the process in which the recovered resin is extruded by the first kneader.

3. A method for producing recycled resin according to claim 1, wherein a third measuring unit measures a third measurement value relating to the second viscosity of the recycled resin extruded by the second kneader, and the control device calculates the control amount based on the third measurement value and performs a feedback process to control the supply unit.

4. A method for producing recycled resin according to claim 1, comprising generating a dataset including the first measurement value, the second measurement value, the control amount, and information regarding the product lot of the generated recycled resin.

5. A method for producing recycled resin according to claim 3, comprising generating a dataset including the first measurement value, the second measurement value, the third measurement value, the control amount, and information regarding the product lot of the generated recycled resin.

6. The method for producing recycled resin according to claim 1, wherein the spectrum of the recovered resin is measured as the first measurement value using the first measuring unit.

7. A recycled resin manufacturing apparatus comprising: a first kneader for kneading recovered resin; a first measuring unit for measuring a first measurement value relating to the composition of the recovered resin kneaded in the first kneader; a second measuring unit for measuring a second measurement value relating to a first viscosity of the recovered resin kneaded in the first kneader; a second kneader for adding a reactive additive for adjusting the viscosity of the resin to the recovered resin extruded from the first kneader and kneading it; a supply unit for adding the reactive additive to the second kneader; and a control device that calculates a control amount including the type and amount of the reactive additive based on the first and second measurement values, and controls the supply unit based on the control amount to supply the reactive additive to the second kneader.

8. The apparatus for manufacturing recycled resin according to claim 7, further comprising a third measuring unit in the second kneader for measuring the second viscosity of the recycled resin.

9. A control device connected to a recycled resin manufacturing apparatus comprising: a first kneader for kneading recovered resin; a first measuring unit for measuring a first measurement value relating to the composition of the recovered resin kneaded in the first kneader; a second measuring unit for measuring a second measurement value relating to a first viscosity of the recovered resin kneaded in the first kneader; a second kneader for adding a reactive additive for adjusting the viscosity of the resin to the recovered resin extruded from the first kneader and kneading it; and a supply unit for adding the reactive additive to the second kneader, the control device comprising: a control unit that calculates a control amount including the type and amount of the reactive additive based on the first and second measurement values, and controls the supply unit based on the control amount to supply the reactive additive to the second kneader.

10. A control method for a control device connected to a recycled resin manufacturing apparatus, comprising: a first kneader for kneading recovered resin; a first measuring unit for measuring a first measurement value relating to the composition of the recovered resin kneaded in the first kneader; a second measuring unit for measuring a second measurement value relating to a first viscosity of the recovered resin kneaded in the first kneader; a second kneader for adding a reactive additive for adjusting the viscosity of the resin to the recovered resin extruded from the first kneader and kneading it; and a supply unit for adding the reactive additive to the second kneader, wherein a computer mounted on the control device calculates a control amount, including the type and amount of the reactive additive, based on the first and second measurement values, and controls the supply unit based on the control amount to supply the reactive additive to the second kneader.

11. A computer program for controlling a control device connected to a recycled resin manufacturing apparatus, the apparatus comprising: a first kneader for kneading recycled resin; a first measuring unit for measuring a first measurement value relating to the composition of the recycled resin kneaded in the first kneader; a second measuring unit for measuring a second measurement value relating to the first viscosity of the recycled resin kneaded in the first kneader; a second kneader for adding a reactive additive for adjusting the viscosity of the resin to the recycled resin extruded from the first kneader and kneading it; and a supply unit for adding the reactive additive to the second kneader, wherein the computer program calculates a control amount including the type and amount of the reactive additive based on the first and second measurement values, and causes a computer mounted on the control device to execute a process of controlling the supply unit to supply the reactive additive to the second kneader based on the control amount.