Method for manufacturing thin film coil

The manufacturing method for thin film coils with reinforcement patterns and insulating films addresses defects in thin film coils, ensuring durability and electromagnetic force for smaller electronic devices.

WO2026235285A1PCT designated stage Publication Date: 2026-11-12STEMCO CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2026/004329
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-09
Filing Date
2026-03-17
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Thin film coils used in camera modules for image stabilization or autofocus control face defects such as bending or breaking due to reduced thickness, which is necessary for smaller electronic devices.

Method used

A method for manufacturing thin film coils involves forming a base with a reinforcement pattern and insulating film, using materials like polyimide and conductive materials, to enhance structural integrity and prevent defects during manufacturing.

Benefits of technology

The method enables the formation of thin film coils with improved durability, preventing bending and tearing, allowing for increased number of stacked coils and enhanced electromagnetic force.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2026004329_12112026_PF_FP_ABST
    Figure KR2026004329_12112026_PF_FP_ABST
Patent Text Reader

Abstract

The present technique is a method for manufacturing a thin film coil, comprising the steps of: forming a base in which an active region is defined; forming, on one surface of the base, a reinforcement pattern exposing the active region; forming a first circuit pattern on the exposed active region; removing the reinforcement pattern; and forming a first insulating film to cover the first circuit pattern.
Need to check novelty before this filing date? Find Prior Art

Description

Method for manufacturing thin film coils

[0001] The present invention relates to a method for manufacturing a thin film coil.

[0002] As the size of electronic devices such as smartphones and tablet PCs becomes smaller, the size of camera modules mounted on these devices is also gradually shrinking. Consequently, the coils used for image stabilization or autofocus control in camera modules are also transitioning from wire types to thin-film types. For example, while coils formed by winding metal wires were conventionally used, thin-film coils with patterns formed by plating metal materials are being used recently.

[0003] These thin-film coils can be used in camera modules for lens image stabilization or autofocus control. More specifically, image stabilization or autofocus control of the camera lens can be implemented by the electromagnetic force of the coil. Although the electromagnetic force increases as the thickness of the thin-film coil increases and the number of turns increases, the thickness of the thin-film coil is also required to be thin as there is a demand for electronic devices with smaller sizes.

[0004] However, as the thickness of the thin film coil decreases, problems may arise where parts of the thin film coil bend or break due to increased weight in some areas during the manufacturing stage.

[0005] An embodiment of the present invention provides a method for manufacturing a thin film coil that can prevent the occurrence of defects caused by a reduction in the thickness of the thin film coil during the step of manufacturing the thin film coil.

[0006] A method for manufacturing a thin film coil according to the present embodiment comprises the steps of: forming a base having an active region defined therein; forming a reinforcement pattern on one surface of the base to expose the active region; forming a first circuit pattern on the exposed active region; removing the reinforcement pattern; and forming a first insulating film to cover the first circuit pattern.

[0007] In one embodiment of the present invention, the step of forming the base includes the step of forming a seed layer on the lower surface and the upper surface of the base layer.

[0008] In one embodiment of the present invention, the base layer or the reinforcing pattern is formed by including at least one material selected from polyimide, polyethylene, polyethylene terephthalate, polyethylene naphthalate, polycarbonate, epoxy, and glass fiber, which are insulating resins.

[0009] The above base layer or the above reinforcing pattern is formed as a film type or a sheet type.

[0010] The above reinforcing pattern is formed from a material selected from nickel (Ni), chromium (Cr), copper (Cu), gold (Au), aluminum (Al), stainless steel, and palladium (Pd), or is formed from an alloy composed of two or more of the above materials.

[0011] In one embodiment of the present invention, the seed layer is formed to have a thinner thickness than the base layer.

[0012] In one embodiment of the present invention, the step of forming the reinforcing pattern comprises forming an opening corresponding to the active area defined on one surface of the base and the reinforcing pattern surrounding the opening in a reinforcing layer for the reinforcing pattern, and then forming the reinforcing pattern on one surface of the base.

[0013] In one embodiment of the present invention, the step of forming the reinforcing pattern comprises: forming a reinforcing layer on one surface of the base; and removing an area corresponding to the active area of ​​the base from the reinforcing layer to expose the active area.

[0014] In one embodiment of the present invention, the reinforcing pattern is formed to have a thickness greater than the thickness of the base layer.

[0015] In one embodiment of the present invention, the reinforcing pattern includes first bridges extended in a first direction and second bridges extended in a second direction orthogonal to the first direction.

[0016] In one embodiment of the present invention, the first bridges overlap with the ends of the second bridges.

[0017] In one embodiment of the present invention, the active region is surrounded by the first and second bridges.

[0018] In one embodiment of the present invention, the step of forming the first circuit pattern comprises: forming a photosensitive pattern on the base; forming the first circuit pattern by filling a conductive material between the photosensitive patterns; and removing the photosensitive pattern.

[0019] In one embodiment of the present invention, the photosensitive pattern is formed thicker than the reinforcing pattern.

[0020] In one embodiment of the present invention, prior to the step of forming the first circuit pattern, the method further includes the step of removing a portion of the base located in the active region to form a first via hole; and the step of forming a barrier layer along the surface of the base exposed through the first via hole.

[0021] In one embodiment of the present invention, the first circuit pattern is formed with a thinner thickness than the photosensitive pattern.

[0022] In one embodiment of the present invention, after removing the photosensitive pattern, an isotropic plating or anisotropic plating step is further performed on the first circuit pattern.

[0023] In one embodiment of the present invention, after the step of forming the first insulating film, the method further comprises the steps of: forming a first via hole that exposes a portion of the first circuit pattern in the first insulating film; forming a second circuit pattern connected to the first circuit pattern through the first via hole; and forming a second insulating film that covers the second circuit pattern.

[0024] In one embodiment of the present invention, the second circuit pattern has the same spiral shape as the first circuit pattern.

[0025] In one embodiment of the present invention, in the step of forming the reinforcement pattern, the step of forming an alignment key on the reinforcement pattern is performed.

[0026] In one embodiment of the present invention, the method includes the step of aligning the base and the reinforcement pattern based on the alignment key formed on the reinforcement pattern and the alignment key formed on the base.

[0027] A method for manufacturing a thin film coil according to the present embodiment comprises the steps of: forming a base having an active region defined therein; forming a reinforcement pattern on the lower and upper surfaces of the base to expose the active region; forming a first circuit pattern on each of the lower and upper surfaces of the base exposed through the active region; removing the reinforcement pattern; and forming a first insulating film to cover the first circuit pattern.

[0028] In one embodiment of the present invention, after the step of forming the first insulating film, the method further comprises the steps of: forming a first via hole that exposes a portion of the first circuit pattern in the first insulating film; forming a second circuit pattern connected to the first circuit pattern through the first via hole; and forming a second insulating film that covers the second circuit pattern.

[0029] According to the present technology, thin film coils can be easily formed.

[0030] According to the present technology, defects such as bending or tearing of the base or the thin film can be prevented when manufacturing a thin film coil.

[0031] According to this technology, the number of stacked thin film coils can be increased.

[0032] FIG. 1 is a plan view for illustrating a reinforcement pattern according to an embodiment of the present invention.

[0033] Figure 2 is a perspective view illustrating the reinforcement pattern of Figure 1.

[0034] FIG. 3 is a plan view for explaining a first circuit pattern according to an embodiment of the present invention.

[0035] FIGS. 4 to 14 are drawings for explaining a method for manufacturing a thin film coil according to an embodiment of the present invention.

[0036] FIG. 15 is a drawing for explaining a thin film coil according to another embodiment of the present invention.

[0037] Hereinafter, embodiments of the present invention are described in detail with reference to the attached drawings so that those skilled in the art can easily implement the invention. The present invention may be embodied in various different forms and is not limited to the embodiments described herein. To clearly explain the present invention, parts unrelated to the description in the drawings have been omitted, and the same reference numerals have been used throughout the specification for identical or similar components.

[0038] The words and terms used in this specification and claims are not limited to their ordinary or dictionary meanings, but should be interpreted in a meaning and concept consistent with the technical spirit of the invention in accordance with the principles by which the inventor defines terms and concepts to best describe his invention.

[0039] FIG. 1 is a plan view for illustrating a reinforcement pattern according to an embodiment of the present invention.

[0040] Referring to FIG. 1, a thin film coil (100) can be used in a camera module mounted on an electronic device such as a smartphone or tablet PC. For example, the thin film coil can be used for anti-shake or autofocus control of the camera module. FIG. 1 shows the XY plane of the step in which a reinforcement pattern (RPT) is formed during the manufacturing process of the thin film coil (100). The thin film coil (100) may include a base (BST) corresponding to a substrate, first holes (1H) formed at both ends of the base layer, active regions (AR) defined between the first holes (1H), and a reinforcement pattern (RPT) surrounding the active regions (AR). An align key (AK) may be further formed in the reinforcement pattern (RPT). The align key (AK) may be formed in a polygonal shape such as a circle, ellipse, triangle, or square.

[0041] The base (BST) is a film-type substrate and can be formed from an insulating resin, which is a flexible polymeric material. For example, the base layer can be formed from at least one material selected from polyimide, polyethylene, polyethylene terephthalate, polyethylene naphthalate, polycarbonate, epoxy, and glass fiber. Not limited thereto, the base (BST) may also be provided as a sheet-type substrate including the above materials.

[0042] The first holes (1H) may be sprocket holes. A sprocket hole is a hole that engages with a sprocket wheel or a sprocket roll and can be used to position or move the base (BST) to the correct position. The first hole (1H) may be formed in a circular, square, or polygonal shape, and in this embodiment, a first hole (1H) made of a circular shape is described as an example.

[0043] Each active region (AR) is an area where a circuit pattern is formed, and can be defined as a single number or a plurality of numbers between the first holes (1H) formed at both ends of the thin film coil (100). In this embodiment, a plurality of active regions (AR) is described as an example. At least one circuit unit (CU) may be formed in each active region (AR). The following embodiment describes a thin film coil (100) comprising a plurality of circuit units (CU).

[0044] A reinforcement pattern (RPT) can be used to prevent defects such as a portion of the base (BST) bending or tilting in a specific direction, which occur when a base (BST) of 30 μm or less flows during the manufacturing stage of the thin film coil (100) or when a circuit pattern thicker than 20 μm is formed on one or both sides of the base (BST). The reinforcement pattern (RPT) can be formed to surround the periphery of the active regions (AR). For example, the reinforcement pattern (RPT) can be formed in the inactive region surrounding the active regions (AR). The reinforcement pattern (RPT) can be formed to surround the sides of the active regions (AR) and may include openings formed in the Z direction. The reinforcement pattern (RPT) can be formed from a material that can be used as the base (BST) or from a conductive material.

[0045] When the reinforcing pattern (RPT) is formed from a material that can be formed as a base (BST), the reinforcing pattern (RPT) may be formed from an insulating resin which is a polymer material. For example, the reinforcing pattern (RPT) may be formed from at least one material selected from polyimide, polyethylene, polyethylene terephthalate, polyethylene naphthalate, polycarbonate, epoxy, and glass fiber.

[0046] When the reinforcing pattern (RPT) is formed from a conductive material, the reinforcing pattern (RPT) may be formed from a material selected from nickel (Ni), chromium (Cr), copper (Cu), gold (Au), aluminum (Al), stainless steel, and palladium (Pd), or may be formed from an alloy composed of two or more of the conductive materials.

[0047] Meanwhile, the reinforcing pattern (RPT) can be formed as a film, ink, or sheet type containing the materials described above.

[0048] To prevent defects such as bending during the manufacturing process of the thin film coil (100), the reinforcing pattern (RPT) can be formed to have a constant thickness in the Z direction. The reinforcing pattern (RPT) can be removed after forming a circuit pattern within the active regions (AR).

[0049] When forming the reinforcement pattern (RPT), an alignment key (AK) may be further formed on the reinforcement pattern (RPT) to align it with the base (BST). For this purpose, an alignment key (AK) may also be formed on the base (BST). At least one alignment key (AK) may be formed within the inactive area, and may also be formed in the surrounding area of ​​the reinforcement pattern (RPT) (e.g., the surrounding area of ​​the first holes where the reinforcement pattern is not formed). The alignment key (AK) may be formed in a polygonal shape such as a circle, ellipse, triangle, or square.

[0050] The manufacturing method of the thin film coil (100) described below is explained with reference to a cross-section cut in the A1-A2 direction.

[0051] Figure 2 is a perspective view illustrating the reinforcement pattern of Figure 1.

[0052] Referring to FIG. 2, a reinforcing pattern (RPT) may be formed to surround one or more active regions (AR). The reinforcing pattern (RPT) surrounds the sides of the active regions (AR) and may have a certain thickness in the Z direction to enhance reinforcing performance. The reinforcing pattern (RPT) may include openings (OP) that expose the active regions (AR). Since the reinforcing pattern (RPT) is formed in a grid shape that exposes the active regions (AR), stiffness in the X direction, Y direction, and Z direction can be maintained.

[0053] The reinforcement pattern (RPT) is formed along the outer surface of the openings (OP) and may include bridges corresponding in the thickness direction to the non-effective area of ​​the base (BST in FIG. 1). Here, the non-effective area may be the remaining area excluding the surrounding area where the first holes (1H in FIG. 1) are formed and the active area (AR in FIG. 1).

[0054] The reinforcement pattern (RPT) may be composed of first bridges (1Ba, 1Bb, 1Bc) extended in the X direction and second bridges (2Ba, 2Bb, 2Bc) extended in the Y direction. A portion of the first bridges (1Ba, 1Bb, 1Bc) and a portion of the second bridges (2Ba, 2Bb, 2Bc) may overlap each other. The first bridges (1Ba, 1Bb, 1Bc) and the second bridges (2Ba, 2Bb, 2Bc) serve to support the base (BST in FIG. 1) even if a portion of the reinforcement layer is open to form a circuit. The widths of the first bridges (1Ba, 1Bb, 1Bc) and the second bridges (2Ba, 2Bb, 2Bc) may be the same, different, or only partially different.

[0055] The alignment key (AK in FIG. 1) may be further formed on some of the first bridges (1Ba, 1Bb, 1Bc) and the second bridges (2Ba, 2Bb, 2Bc). The alignment key (AK in FIG. 1) may be further formed on the first bridges (1Ba, 1Bb, 1Bc) or the second bridges (2Ba, 2Bb, 2Bc). The alignment key (AK in FIG. 1) may be further formed in some area where the first bridges (1Ba, 1Bb, 1Bc) and the second bridges (2Ba, 2Bb, 2Bc) overlap each other. The alignment key (AK in FIG. 1) may be further formed on the base (BST in FIG. 1) around the first holes (1H in FIG. 1) in the area where the reinforcement pattern (RPT) is not formed.

[0056] The alignment key (AK in FIG. 1) can be formed simultaneously when the openings (OP) of the reinforcing layer are formed. The alignment key (AK in FIG. 1) can be formed in a polygonal shape such as a circle, ellipse, triangle, or square.

[0057] FIG. 3 is a plan view for explaining a first circuit pattern according to an embodiment of the present invention.

[0058] Referring to FIGS. 1 and FIGS. 3, a first circuit pattern (1CP) can be formed inside each of the circuit units (CU). Since the first circuit pattern (1CP) formed in each of the circuit units (CU) can have the same structure, FIG. 3 illustrates a first circuit pattern (1CP) formed in one of the circuit units (CU) as an example.

[0059] The first circuit pattern (1CP) may be formed in a spiral shape. For example, the first circuit pattern (1CP) may be formed in a square spiral shape or in a circular spiral shape. In this embodiment, the first circuit pattern (1CP) formed in a square spiral shape is disclosed, but the structure of the first circuit pattern (1CP) is not limited to the structure shown in FIG. 3.

[0060] The outer end (30) of the first circuit pattern (1CP) can be connected to a wire (not shown) that receives current.

[0061] FIGS. 4 to 13 are drawings for explaining a method for manufacturing a thin film coil according to an embodiment of the present invention.

[0062] The cross-sections shown in FIGS. 4 to 13 correspond to the cross-sections cut in the A1-A2 direction shown in FIGS. 1 to 3. The method for manufacturing the thin film coil is described step-by-step as follows.

[0063] Referring to FIG. 4, a seed layer (SD) may be formed on the upper and lower surfaces of a base layer (BS). The base layer (BS) may be formed as a film-type substrate and may be formed from an insulating resin, which is a flexible polymeric material. For example, the base layer (BS) may be formed from at least one material selected from polyimide, polyethylene, polyethylene terephthalate, polyethylene naphthalate, polycarbonate, epoxy, and glass fiber. Not limited thereto, the base (BST) may be provided as a sheet-type substrate including the above materials.

[0064] The base layer (BS) may have a first thickness (1T). The first thickness (1T) may be the height from the lower surface to the upper surface of the base layer (BS).

[0065] The seed layer (SD) may be formed from a conductive material. For example, the seed layer (SD) may be formed from at least one material selected from conductive materials such as nickel (Ni), chromium (Cr), copper (Cu), gold (Au), aluminum (Al), and palladium (Pd), or may be formed from an alloy composed of multiple of these materials. The seed layer (SD) may be formed on the base layer (BS) by physical methods such as deposition, adhesion, or plating, or may be formed on the base layer (BS) by chemical methods. The seed layer (SD) may have a second thickness (2T) that is thinner than the first thickness (1T). For example, “1T+2(2T)”, which is the sum of the total thicknesses of the base layer (BS) and the seed layer (SD), may be determined to be between 3 μm and 30 μm.

[0066] The base layer (BS) and the seed layer (SD) become the base (BST) for manufacturing the thin film coil.

[0067] After the seed layer (SD) is formed, first holes (1H) may be formed at both ends of the base layer (BS) and the seed layer (SD). The first holes (1H) may be formed spaced apart from each other along the Y direction as shown in FIG. 1.

[0068] An alignment key (AK in FIG. 1) may be further formed in the seed layer (SD) or in an inactive region of the seed layer (SD) and the base layer (BS). The alignment key (AK) may be formed in a polygonal shape such as a circle, ellipse, triangle, or square.

[0069] Referring to FIG. 5a, a reinforcing pattern (RPT) including an opening (OP) that exposes an active region (AR) and contacts a seed layer (SD) formed on the lower surface of a base layer (BS) can be formed.

[0070] At this time, the total width (length in the X direction) of the reinforcement pattern (RPT) is formed to be narrower than the total width (length in the X direction) of the base (BST). By doing so, a portion of the base (BST) that does not overlap with the reinforcement pattern (RPT) in the thickness direction may be exposed. Preferably, by forming the reinforcement pattern (RPT) on the base (BST) such that a virtual center axis extending in the width direction (X direction) coincides with each other, a portion of the ends of the base (BST) may be exposed. Accordingly, first holes (1H) and an incoming wiring portion (not shown) are exposed in the exposed portions of the ends of the base (BST) to enable the application of current for process flow and circuit formation of the base (BST). For example, the first holes (1H) may be sprocket holes for moving the base (BST) during the manufacturing process of a thin film coil, and the incoming wiring portion (not shown) may be a current application portion for circuit formation.

[0071] A reinforcement pattern (RPT) can be formed around an opening (OP) after the opening (OP) is defined. For example, a reinforcement pattern (RPT) can be formed around an opening (OP) by forming the opening (OP) by punching or using a laser in an area corresponding to an active region (AR). Alternatively, after a reinforcement layer for the reinforcement pattern (RPT) is formed, the opening (OP) can be formed by patterning the reinforcement layer. For example, after the reinforcement layer is provided, the opening (OP) can be formed by removing a portion of the reinforcement layer using a lithography method. Alternatively, after the reinforcement layer is provided, the opening (OP) can be formed by removing a portion of the reinforcement layer using an etching method.

[0072] The opening (OP) of this reinforcing pattern (RPT) may be formed before the reinforcing layer is provided on one or both sides of the base (BST), or it may be formed after the reinforcing layer is provided on one or both sides of the base (BST).

[0073] Multiple circuit units (CU) may be formed within the active area (AR) through a subsequent process, which is described in the manufacturing step described below.

[0074] The reinforcing pattern (RPT) can be formed into a three-dimensional structure as shown in FIG. 2 to prevent defects such as bending or tilting in a specific direction of the base or part of the thin film coil (100 in FIG. 1) during the manufacturing step of the thin film coil (100). For example, the reinforcing pattern (RPT) can ensure process fluidity of the base layer (BS) having a thickness of 30 μm or less, more preferably 15 μm or less, and prevent the base layer (BS) from bending during the subsequent manufacturing step of forming a photosensitive film or forming a circuit pattern.

[0075] The reinforcement pattern (RPT) may be formed to surround the periphery of the active area (AR). For example, the reinforcement pattern (RPT) may be formed in an inactive area surrounding the active area (AR). The reinforcement pattern (RPT) may be formed to surround the side of the active area (AR) and may include an opening (OP) drilled in the Z direction. The reinforcement pattern (RPT) may have a third thickness (3T) that is thicker than the first thickness (1T) to ensure reinforcement performance. For example, the third thickness (3T) may be determined between 20 μm and 100 μm. Both ends of the reinforcement pattern (RPT) may be adjusted so as not to overlap with the first hole (1H).

[0076] The reinforcing pattern (RPT) can be formed from a material that can be used as a base layer (BS) or from a conductive material. When the reinforcing pattern (RPT) is formed from a material that can be formed as a base layer (not shown), the reinforcing pattern (RPT) can be formed from an insulating resin which is a polymer material. For example, the reinforcing pattern (RPT) can be formed from at least one material selected from polyimide, polyethylene, polyethylene terephthalate, polyethylene naphthalate, polycarbonate, epoxy, and glass fiber. When the reinforcing pattern (RPT) is formed from a conductive material, the reinforcing pattern (RPT) can be formed from a material selected from nickel (Ni), chromium (Cr), copper (Cu), gold (Au), aluminum (Al), stainless steel, and palladium (Pd), or can be formed from an alloy composed of two or more of the conductive materials. In addition, the reinforcing pattern (RPT) may be formed from a film, ink, or sheet-type material including at least one of the materials described above.

[0077] Although a reinforcing pattern (RPT) formed on the lower part of a base layer (BS) is illustrated as an example in FIG. 5a, the reinforcing pattern (RPT) may be formed on both the upper and lower parts of the base layer (BS) as illustrated in FIG. 5b. The reinforcing pattern (RPT) formed on the upper part of the base layer (BS) may have the same structure as the reinforcing pattern (RPT) formed on the lower part of the base layer (BS). Alternatively, the reinforcing patterns (RPT) formed on the upper and lower parts of the base layer (BS), respectively, may have different structures. For example, the reinforcing patterns (RPT) formed on the upper and lower parts of the base layer (BS), respectively, may have different layouts or different thicknesses. Although not illustrated in FIG. 5a and FIG. 5b, the reinforcing pattern (RPT) may be formed only on the upper surface of the base layer (BS). In this embodiment, a manufacturing method for forming a reinforcement pattern (RPT) on the lower part of a base layer (BS) is described as an example, but the location where the reinforcement pattern (RPT) according to the present invention is formed is not limited to the location shown in FIG. 5a or FIG. 5b. After the manufacturing step described with reference to FIG. 5a or FIG. 5b, an alignment key (AK in FIG. 1) may be further formed on the reinforcement pattern (RPT). Alternatively, the alignment key (AK) may be formed simultaneously when forming an opening (OP) corresponding to an active area (AR). The alignment key (AK) may be formed in a polygonal shape such as a circle, ellipse, triangle, or square. If the pattern of the alignment key (AK) of the reinforcement pattern (RPT) matches the pattern of the alignment key (AK) of the seed layer (SD), alignment is preferably achieved, so the process can proceed to the next manufacturing step.

[0078] Referring to FIG. 6, a second hole (2H) may be formed in an active region (AR) surrounded by a reinforcement pattern (RPT). The second hole (2H) may be a via hole that allows circuit patterns formed on the upper and lower parts of the base layer (BS) to be electrically connected to each other. Thus, at least one second hole (2H) may be formed within the active region (AR).

[0079] Referring to FIG. 7, a barrier layer (BR) may be formed along the inner surface of the first and second holes (1H, 2H). The barrier layer (BR) may be formed of a conductive material. For example, the barrier layer (BR) may be formed by an electroless or electroplating method.

[0080] Referring to FIG. 8, a photoresist (PR) can be formed on the seed layer (SD) and the reinforcement pattern (RPT). For example, the photoresist (PR) can be formed simultaneously on the upper and lower parts of the base (BST). The photoresist (PR) can be formed in a liquid or film form, and the present invention describes an embodiment using a film type (Dry film Resist, DFR). Since a film-type photoresist (PR) is formed, the photoresist (PR) is not formed inside the second hole (2H). As the first hole (1H) is formed to be exposed when the photoresist (PR) is formed, the flow of the base (BST) is continuously possible during the manufacturing process. Therefore, the left end of the photoresist (PR) can be located between the first hole (1H) and the reinforcement pattern (RPT). That is, a photosensitive resist (PR) with a narrower width compared to the width of the base (BST) extended along the X direction is formed on the base (BST).

[0081] In addition, since the width of the photosensitive resist (PR) in the X direction is wider than the width of the reinforcement pattern (RPT), the adhesion between the photosensitive resist (PR) and the reinforcement pattern (RPT) can be improved. Accordingly, the phenomenon of the photosensitive resist (PR) detaching from the base (BST) can be prevented. Although not shown in the drawing, the right end of the photosensitive resist (PR) may also be located between the first hole (1H) located to the right of the thin film coil (100 in FIG. 1) and the reinforcement pattern (RPT). The photosensitive resist (PR) may have a fourth thickness (4T). Here, the fourth thickness (4T) is the thickness from the upper surface to the lower surface of the photosensitive resist (PR), and in FIG. 8, it refers to the thickness from the surface of the seed layer (SD).

[0082] The photosensitive resist (PR) can be formed in a manner that contacts the outer surface of the reinforcing pattern (RPT) and the surface of the seed layer (SD). It is preferable that the photosensitive resist (PR) be formed so that the entire reinforcing pattern (RPT) is covered. For example, the fourth thickness (4T) should be thicker than the third thickness (3T). If the thickness of the photosensitive resist (PR) is insufficient, that is, if the fourth thickness (4T) is thinner than the third thickness (3T), the contact area between the photosensitive resist (PR) and the reinforcing pattern (RPT) may be reduced. As a result, the photosensitive resist (PR) and the seed layer (SD) may not be in complete contact in the active area (AR) inside the reinforcing pattern (RPT), and a void may be formed. That is, a void may occur in the region (81) where the photosensitive resist (PR) and the seed layer (SD) come into contact, and the circuit pattern may not be formed in a desirable way during the manufacturing process described later. The importance of the thickness of the photosensitive resist (PR) is explained in detail as follows.

[0083] The photosensitive resist (PR) can be applied to the reinforcing pattern (RPT) and the seed layer (SD) by lamination. Since the photosensitive resist (PR) comes into contact with the surfaces of the reinforcing pattern (RPT) and the seed layer (SD), the thicker the reinforcing pattern (RPT), the larger the contact area between the photosensitive resist (PR) and the reinforcing pattern (RPT). Additionally, because the reinforcing pattern (RPT) has a shape that protrudes from the base (BST), a sufficient area for the photosensitive resist (PR) to be applied to the seed layer (SD) is not secured, and as described above, a void may occur between the photosensitive resist (PR) and the seed layer (SD) in the area where the reinforcing pattern (RPT) and the seed layer (SD) come into contact. The occurrence of voids means that the bonding surface between the photosensitive resist (PR) and the seed layer (SD) is reduced, which may cause lifting of the photosensitive resist (RPT) in subsequent processes. Therefore, in order to increase the contact surface between the photosensitive resist (RPT) and the seed layer (SD), the photosensitive resist (RPT) must be formed thicker than the reinforcing pattern (RPT).

[0084] During the photosensitive resist (PR) formation process, heat and pressure are applied inside the chamber, and at this time, the reinforcing pattern (RPT) can prevent the base (BST) from bending.

[0085] Referring to FIG. 9, a photosensitive pattern (PRp) can be formed by patterning a photosensitive resist (PR of FIG. 8). For example, after forming the photosensitive resist (PR of FIG. 8), a photosensitive pattern (PRp) can be formed by removing a portion of the photosensitive resist (PR) through an exposure and development process. In a subsequent process, a circuit pattern can be formed inside the third hole (3H) between the photosensitive patterns (PRp). The photosensitive pattern (PRp) can be formed such that the second hole (2H) is exposed through the third hole (3H). The seed layer (SD) can be exposed through the third hole (3H). Since the drawings are illustrated to facilitate understanding of embodiments of the present invention, the width of the third hole (3H) and the photosensitive pattern (PRp) may substantially be narrower than the width shown in the drawings, taking into account the circuit pattern to be formed on each of the plurality of circuit units. In the XY plane, the opening of the photosensitive pattern (PRp) may have a spiral shape (see FIG. 3). For example, the opening of the photosensitive pattern (PRp) may have a square spiral shape or a circular spiral shape.

[0086] Referring to FIG. 10, a first circuit pattern (1CP) may be formed inside a third hole (3H) between photosensitive patterns (PRp). The first circuit pattern (1CP) may be formed from a conductive material. There are various methods for forming the first circuit pattern (1CP). For example, the first circuit pattern (1CP) may be formed through a method selected from etching, an additive process (AP), a semi-additive process (SAP), printing, and coating. As described with reference to FIG. 3, the first circuit pattern (1CP) extends in a spiral shape relative to each other in the XY plane, but must be separated from each other by the photosensitive pattern (PRp) at the A2-A2 cross-section. To this end, it is preferable that the conductive material for the first circuit pattern (1CP) be formed with a fifth thickness (5T) that is thinner than the fourth thickness (4T) of the photosensitive pattern (PRp). If the conductive material for the first circuit pattern (1CP) is formed thicker than the photosensitive pattern (PRp), the conductive material for the first circuit pattern (1CP) is applied up to the upper surface of the photosensitive pattern (RPT), resulting in a mushroom shape with an expanded upper width, and thus the shape of the circuit pattern cannot be formed in a desirable manner. Furthermore, the upper surfaces of the first circuit patterns (1CP), which should be spaced apart from each other in the cross-sectional direction, may come into contact with each other, potentially causing short circuit defects. Therefore, it is preferable that the conductive material for the first circuit pattern (1CP) be formed thinner than the photosensitive pattern (PRp).

[0087] For example, the fifth thickness (5T) can be determined to be between 30 μm and 200 μm, and the spacing between the first circuit patterns (1CP) can be between 1 μm and 10 μm. However, since the thickness and spacing of the first circuit patterns (1CP) can be changed depending on the thin film coil, they are not limited to the values ​​disclosed in this embodiment. The first circuit pattern (1CP) can be formed to be wound at least three times. Through this structure, the thin film coil can secure sufficient electromagnetic force.

[0088] Since the second hole (2H) is exposed between the photosensitive pattern (PRp), a portion of the first circuit pattern (1CP) can fill the interior of the second hole (2H). Thus, the first circuit pattern (1CP) formed on the upper part of the base layer (BS) and the first circuit pattern (1CP) formed on the lower part of the base layer (BS) can be electrically connected to each other. Thus, a portion of the first circuit pattern (1CP) formed in the second hole (2H) can become the first via (1VA). Referring to FIG. 11, after the first circuit pattern (1CP) is formed, a peeling step can be performed to remove the photosensitive pattern (PRp in FIG. 10). When the photosensitive pattern (PRp) is completely removed, the first circuit pattern (1CP), the seed layer (SD), and the reinforcement pattern (RPT) can be exposed through the fourth hole (4H) from which the photosensitive pattern (PRp) was removed. After removing all photosensitive patterns (PRp), a plating step may be further performed to control the thickness and width of the first circuit pattern (1CP). For example, an isotropic plating or anisotropic plating step may be further performed.

[0089] Referring to FIG. 12, a peeling step for removing the reinforcement pattern (RPT) may be performed. The peeling step for removing the reinforcement pattern (RPT) may be performed in a dry or wet manner, but preferably, a wet peeling step is performed. A portion of the seed layer (SD) may be exposed through the area where the reinforcement pattern (RPT) has been removed.

[0090] Referring to FIG. 13, if a seed layer (SD) remains between first circuit patterns (1CP), migration or short circuit defects may occur between adjacent first circuit patterns (1CP). To prevent such problems, a step of etching a portion of the seed layer (SD) or base exposed between the first circuit patterns (1CP) may be further performed. The step of etching a portion of the seed layer (SD) or base may be performed optionally. That is, to reduce the number of manufacturing processes, the step of etching a portion of the seed layer (SD) or base may be omitted. However, as described above, it is more desirable to perform the step of etching a portion of the seed layer (SD) or base to prevent migration or short circuit defects. The seed layer (SD) remaining after the etching step becomes a seed pattern (SDp).

[0091] Referring to FIG. 14, a first insulating film (1ITL) covering the entire structure may be formed. The first insulating film (1ITL) may be formed of an insulating resin. By forming the first insulating film (1ITL), a thin film coil (100) made of a first laminate (1STK) may be formed.

[0092] FIG. 15 is a drawing for explaining a thin film coil according to another embodiment of the present invention.

[0093] Referring to FIG. 15, in order to increase the electromagnetic force of the thin film coil (200), a second laminate (2STK) may be further formed on the lower part of the first laminate (1STK), and a third laminate (3STK) may be further formed on the upper part of the first laminate (1STK). The second or third laminate (2STK or 3STK) may be formed by the manufacturing method described with reference to FIG. 8 to 13. The second laminate (2STK) may include a second circuit pattern (2CP) and a second insulating film (2ITL). The third laminate (3STK) may include a third circuit pattern (3CP) and a third insulating film (3ITL). The second and third circuit patterns (2CP, 3CP) may be formed with the same structure as the first circuit pattern (1CP). Also, not limited thereto, the circuit patterns of each layer may be formed with different numbers of windings or structures.

[0094] In order to electrically connect the first circuit pattern (1CP) and the second circuit pattern (2CP), a second via (2VA) penetrating the first insulating film (1ITL) may be formed. In order to electrically connect the first circuit pattern (1CP) and the third circuit pattern (3CP), a third via (3VA) penetrating the first insulating film (1ITL) may be formed.

[0095] Additionally, although not shown in the drawing, the second circuit pattern (2CP) or the third circuit pattern (3CP) may be formed to include a seed layer (SD) like the first circuit pattern (1CP).

[0096] In the embodiment described with reference to FIG. 14, a thin film coil (200) including first to third laminates (1STK to 3STK) is shown, but the number of laminates included in the thin film coil (200) may be changed. Meanwhile, the thin film coil (200) of the present invention can be applied to various electronic devices such as camera modules, smartphones, display devices, and wearable devices. In addition, since it is manufactured to include a base (BST) of 30㎛ or less, more preferably 15㎛, the thin film coil (200) of the present invention may be effective for miniaturization of electronic devices to which it is applied.

[0097] Although embodiments of the present invention have been described, the spirit of the present invention is not limited by the embodiments presented in this specification. Those skilled in the art who understand the spirit of the present invention may easily propose other embodiments within the scope of the same spirit by adding, changing, deleting, or adding components, and such are also to be considered to fall within the scope of the spirit of the present invention.

Claims

1. A step of forming a base in which an active region is defined; A step of forming a reinforcing pattern that exposes the active area on one surface of the base; A step of forming a first circuit pattern in the exposed active area; Step of removing the above reinforcement pattern; and A method for manufacturing a thin film coil comprising the step of forming a first insulating film so as to cover the first circuit pattern.

2. In claim 1, the step of forming the base is, A method for manufacturing a thin film coil comprising the step of forming a seed layer on the lower and upper surfaces of a base layer.

3. In Paragraph 2, A method for manufacturing a thin film coil in which the base layer or the reinforcing pattern comprises at least one material selected from insulating resins such as polyimide, polyethylene, polyethylene terephthalate, polyethylene naphthalate, polycarbonate, epoxy, and glass fiber.

4. In Paragraph 3, A method for manufacturing a thin film coil in which the above base layer or the above reinforcing pattern is formed as a film type or a sheet type.

5. In Paragraph 1, A method for manufacturing a thin film coil in which the above reinforcing pattern is formed from a material selected from nickel (Ni), chromium (Cr), copper (Cu), gold (Au), aluminum (Al), stainless steel, and palladium (Pd), or from an alloy composed of two or more of the above materials.

6. In Paragraph 2, A method for manufacturing a thin film coil in which the seed layer is formed to have a thickness thinner than the base layer.

7. In paragraph 1, the step of forming the reinforcing pattern is, After forming an opening corresponding to the active area defined on one surface of the base and the reinforcing pattern surrounding the opening in the reinforcing layer for the reinforcing pattern, A method for manufacturing a thin film coil comprising the step of forming the above-mentioned reinforcing pattern on one surface of the base.

8. In paragraph 1, the step of forming the reinforcing pattern is, A step of forming a reinforcing layer on one surface of the above base; and A method for manufacturing a thin film coil comprising the step of removing a region corresponding to the active region of the base from the reinforcing layer to expose the active region.

9. In Paragraph 2, A method for manufacturing a thin film coil in which the above reinforcing pattern is formed to have a thickness greater than the thickness of the base layer.

10. In paragraph 1, the reinforcement pattern is, First bridges extended in the first direction, and A method for manufacturing a thin film coil comprising second bridges extended in a second direction orthogonal to the first direction.

11. In Paragraph 10, A method for manufacturing a thin film coil in which the first bridges overlap the ends of the second bridges.

12. In Paragraph 10, A method for manufacturing a thin film coil in which the active region is surrounded by the first and second bridges.

13. In claim 1, the step of forming the first circuit pattern comprises: A step of forming a photosensitive pattern on the above base; A step of forming the first circuit pattern by filling a conductive material between the photosensitive patterns; and A method for manufacturing a thin film coil comprising the step of removing the above photosensitive pattern.

14. In Paragraph 13, A method for manufacturing a thin film coil in which the above photosensitive pattern is formed thicker than the above reinforcing pattern.

15. In Clause 13, prior to the step of forming the first circuit pattern, A step of forming a first via hole by removing a portion of the base located in the active region; and A method for manufacturing a thin film coil, further comprising the step of forming a barrier layer along the surface of the base exposed through the first via hole.

16. In Paragraph 15, A method for manufacturing a thin film coil in which the first circuit pattern is formed with a thickness thinner than the photosensitive pattern.

17. In Paragraph 13, A method for manufacturing a thin film coil in which, after removing the above photosensitive pattern, an isotropic plating or anisotropic plating step is further performed on the first circuit pattern.

18. In claim 1, after the step of forming the first insulating film, A step of forming a first via hole in the first insulating film that exposes a portion of the first circuit pattern; A step of forming a second circuit pattern connected to the first circuit pattern through the first via hole; and A method for manufacturing a thin film coil, further comprising the step of forming a second insulating film covering the second circuit pattern.

19. In Paragraph 18, A method for manufacturing a thin film coil in which the second circuit pattern has the same spiral shape as the first circuit pattern.

20. In the step of forming the reinforcing pattern according to claim 1, A method for manufacturing a thin film coil in which the step of forming an alignment key on the above reinforcement pattern is performed.

21. In Paragraph 20, A method for manufacturing a thin film coil comprising the step of aligning the base and the reinforcing pattern based on the alignment key formed on the reinforcing pattern and the alignment key formed on the base.

22. A step of forming a base in which an active region is defined; A step of forming a reinforcing pattern that exposes the active area on the lower and upper surfaces of the base; A step of forming a first circuit pattern on each of the lower and upper surfaces of the base exposed through the active region; Step of removing the above reinforcement pattern; and A method for manufacturing a thin film coil comprising the step of forming a first insulating film so as to cover the first circuit pattern.

23. In paragraph 22, after the step of forming the first insulating film, A step of forming a first via hole in the first insulating film that exposes a portion of the first circuit pattern; A step of forming a second circuit pattern connected to the first circuit pattern through the first via hole; and A method for manufacturing a thin film coil, further comprising the step of forming a second insulating film covering the second circuit pattern.