Phase and diffraction contrast imaging-based electron beam lithography
Phase and diffraction contrast imaging in electron beam lithography addresses throughput limitations and efficiency challenges of EBL and EUV lithography by using a patterned crystalline mask for high-resolution, large-area patterning with improved throughput and power efficiency.
Patent Information
- Application Number
- PCT/US2026/027064
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-08
- Filing Date
- 2026-05-07
- Publication Date
- 2026-11-12
AI Technical Summary
Current electron beam lithography (EBL) systems are limited by low throughput and are impractical for mass production of integrated circuits due to their rastered process, while EUV lithography faces challenges with complex light sources and inefficient power conversion, leading to high operational costs and pattern fidelity issues.
Phase and diffraction contrast imaging-based electron beam lithography utilizes a patterned crystalline mask to achieve high electron beam power and resolution, allowing for nanometer-scale features over large areas with improved throughput by using diffraction and elastic scattering to modulate electron beam dose without degrading coherence.
This approach enables high-resolution patterning at nanometer scales with throughput comparable to EUV lithography, achieving 100X faster exposure rates than conventional rastered EBL and significantly reducing operational costs by enhancing power conversion efficiency.
Smart Images

Figure US2026027064_12112026_PF_FP_ABST
Abstract
Description
Attorney Docket No. 146-097WO1PHASE AND DIFFRACTION CONTRAST IMAGING-BASED ELECTRON BEAM LITHOGRAPHYCross Reference to Related Application
[0001] This application claims the benefit of US Provisional Application Serial No. 63 / 802146, filed May 8, 2025 entitled “PHASE AND DIFFRACTION CONTRAST IMAGING BASED ELECTRON BEAM LITHOGRAPHY”, the contents of which are incorporated herein by reference.Field Of The Invention
[0002] The present disclosure relates generally to lithographic patterning technologies used in semiconductor fabrication and nanofabrication. More particularly, the disclosure relates to electron beam lithography systems and methods that utilize phase contrast imaging and diffraction contrast imaging of electron beams interacting with patterned crystalline masks to produce nanoscale lithographic features over large exposure areas.Background Of The Invention
[0003] Photolithography is a crucial process in semiconductor fabrication, enabling the precise patterning of integrated circuits (IC) onto silicon and other wafers. This technique uses light to transfer geometric patterns from a photomask onto a light-sensitive chemical fdm known as a photoresist, which coats the wafer. The goal is to create microscopic features that form the components of ICs, such as transistors, capacitors, and interconnects. Photolithography allows for the production of complex patterns with high accuracy, essential for manufacturing modem electronic devices.
[0004] In semiconductor fabrication, photolithography works through a multi-step process. First, the wafer is coated with a photoresist and then exposed to ultraviolet (UV) light through a photomask, which contains the desired circuit patterns. Depending on whether a positive or negative resist is used, the exposed or unexposed areas of the resist are chemically altered. A developer is then applied to remove either the exposed orunexposed areas, revealing the wafer underneath. This patterned wafer is then subjected to etching, ion implantation, or other processes to build the circuit layers. Multiple cycles of photolithography and subsequent processes are repeated to fabricate the entire IC.
[0005] The application of photolithography in semiconductor fabrication is vital to achieving the ever-smaller feature sizes needed for advanced electronics. As the demand for faster and more energy-efficient devices grows, semiconductor manufacturers are pushing the limits of photolithography. Techniques like deep ultraviolet (DUV) and extreme ultraviolet (EUV) lithography are employed to pattern features at the nanometer scale, enabling the production of cutting-edge microchips used in computers, smartphones, and other technologies.
[0006] EUV lithography introduces significant complexity due to the nature of the light source and optical systems required. EUV light, with a wavelength of 13.5 nm, is absorbed by most materials, making it impossible to use traditional lenses or mirrors. Instead, EUV systems rely on sophisticated multi-layer mirrors with precise coatings to reflect the light at shallow angles, requiring extreme precision in both alignment and manufacturing. The EUV light source itself is challenging to generate and maintain at high power levels, involving complex systems that use high-energy lasers to vaporize tin droplets, which in turn emit the desired EUV radiation. Maintaining consistent power output, stability, and uptime of these tools is difficult and can lead to increased downtime and higher operational costs for semiconductor fabs.
[0007] On the resist side, the challenges of EUV lithography stem from the fact that traditional photoresists, designed for longer wavelengths like deep ultraviolet (DUV), struggle to perform well under EUV exposure. EUV photons have much higher energy, which can cause unwanted secondary electron effects, reducing pattern fidelity and creating issues like line edge roughness (LER) or pattern collapse. Additionally, there is a need to balance sensitivity, resolution, and etch resistance in EUV resists. Higher sensitivity resists may lead to faster exposure times but often sacrifice the fine resolution needed for sub- 10 nm features.
[0008] Electron beam lithography (EBL) is a high-precision technique used to pattern extremely small features on a substrate, making it a valuable tool for research and thedevelopment of advanced semiconductor devices. Unlike traditional photolithography, which uses light, EBL employs a focused beam of electrons to directly write patterns onto a resist-coated substrate. This direct-write process allows for the creation of features down to the sub- 10 nanometer scale, well beyond the resolution limits of optical lithography. EBL is commonly used for fabricating prototype devices, research in nanoscale structures, and mask writing, where extreme accuracy and control over feature size are required.
[0009] However, despite its high resolution, electron beam lithography faces significant limitations, particularly in terms of throughput. Because it is a rastered process — where a nanometer-scale beam is moved across the wafer — EBL is much slower than the parallel nature of photolithography, which can expose a significant area of the wafer in a single step. This makes EBL impractical for mass production of ICs, where high-volume manufacturing is required. The technology is more commonly used in specialized applications, such as the production of photomasks for EUV lithography or in research environments where flexibility and extreme resolution are prioritized over speed.
[0010] Electron beam lithography (EBL) tools are presently used as a technique for producing microelectronics and integrated circuits (IC) with resolution comparable or superior to the most advanced (extreme ultraviolet or EUV) lithography systems.However, the relatively low exposure rate has prevented this approach from being adopted as a platform for the mass production of ICs. When comparing the exposure rate delivered by present single-beam EBL compared to photolithography, EBL lags by many orders of magnitude. However, EBL provides two significant advantages. First, the intrinsic resolution achievable with EBL is superior photolithography, as demonstrated routinely with the atomic scale resolution of transmission electron microscopes. This is 100X smaller than the resolution in the best EUV photolithography tools. The second advantage is the overall efficiency at which the EBL dose can be produced and delivered. The acceleration of electron beams to the voltages needed, can be extremely electrically efficient, approaching 100% for DC acceleration and 10s% efficiency for RF acceleration. This compares remarkably to the 0.05-0.1% electrical efficiency of EUV photolithography tools that use laser plasma sources. Furthermore, electron beam devicescan have operational lifetimes of 100,000 hours, providing for a pathway to high throughput operation. Unfortunately, current EBL systems are primarily based on the rastering of extremely fine electron beams (nanometer scale) on resist making them extremely slow.Summary Of The Invention
[0011] Phase and diffraction contrast imaging-based electron beam lithography is a lithographic technique for leveraging the extreme resolution possible with electron beams while matching the large area formats of traditional photolithography. In certain embodiments of the present invention, an electron beam interacts with a mask through diffraction which allows for high electron beam power while utilizing the full resolution of the electron beam and allowing for extreme precision. An additional advantage of utilizing electron beams over photons at short wavelengths (EUV or beyond-EUV lithography) is that the power conversion efficiency of energy into the electron beam is extremely high (near unity for DC beams) and several orders of magnitude more efficient than a conventional EUV photolithography tool. At the same time, electron beam powers can far exceed the EUV power, allowing for systems to match the rate of production for an EUV system. The intrinsic resolution limit of the system for imaging of the electron beam approaches the de Broglie wavelength of the electrons and is much smaller than an individual atom (as seen in systems that use electron beams for imaging such as TEMs). The mask, which diffracts the electron beam and produces the pattern on the electron beam resist, can also handle high power as the mask is extremely thin and primarily interacts with the beam through coherent elastic scattering which does not result in energy deposition in the mask. The mask can be produced from a variety of materials. In some embodiments the active part of the mask that interacts with the beam should generally be single crystal, although other portions of the mask such as those acting as a mechanical support may be polycrystalline or amorphous. In other embodiments the active portion of the mask may be polycrystalline or hybrid. In its simplest form a single crystal silicon wafer patterned with varying thickness can produce the desired image which is then projected, 1 : 1 or with demagnification, onto the resist. Withdemagni fi cation, the ultimate resolution is not set by the mask geometry but rather by the imaging fidelity of the electron optical system and the interactions of the electron beam with the resist, both of which can surpass EUV resolution.Brief Description Of The Figures
[0012] FIG. 1 (left) shows the extinction length as a function of energy for the first 5 lowest order diffraction peaks in Si and (right) the stopping power of inelastic scattering.
[0013] FIG. 2 shows the Bragg angle as a function of electron energy for the first five lowest order diffraction peaks in Si.
[0014] FIG. 3 shows a simplified schematic diagram of one example of a diffraction based EBL system.
[0015] FIG. 4 is a schematic representation of a mask illuminated by a collimated electron beam.
[0016] FIG. 5 shows a simplified, schematic diagram of one example of a diffraction arrangement for demonstrating the principle of patterning PMMA with a diffraction patterned electron beam.
[0017] FIG. 6 is a simplified schematic diagram depicting one example of a method of thermal stabilization.Detailed Description
[0018] Fundamentally, what is needed to realize the full benefit for EBL is an approach that allows the electron beam dose patterned over a wide area (e.g., greater than mm-scale), with nanometer precision and with high dose. Using diffraction or phase contrast imaging of electron beams propagated through patterned, single-crystal targets and demagnification optics allows for the exposure of resist with nanometer scale features over mm-scale areas.
[0019] The approach described herein begins with the patterning of a crystal, for example silicon, with the desired mask. The thickness of the crystal depends on the electron beam voltage that will be used in the EBL as well as the specific Bragg peak chosen, but typically would range from 10’s to 100’s of nm in thickness. The mask thickness must beequivalent to the extinction length of the particular Bragg peak chosen with etched regions having a thickness of half the extinction length. This allows nearly 100% probability of a single diffraction event in the etched region and nearly 100% probability of two diffraction events (and thus no net diffraction) in the unetched region. This configuration results in the maximum contrast ration between diffracted and forward scattered electrons, for the proper orientation of the crystal. However, when optimizing the mask for a particular exposure the desired dose deposition may not be a 100% contrast (0% or 100% intensity) and may instead be a “gray-scale” image with a contrast ratio anywhere between 0-100%. This can be achieved by varying the thickness of the mask, either less than or more than the extinction length to provide anywhere between 0-100% intensity at the sample. Furthermore, the orientation of the crystal can be chosen to involve elastic scattering of the electrons between the forward-scattered and a single Bragg peak or multiple Bragg peaks to optimize image formation.
[0020] FIG. 1 shows the extinction length of various diffraction peaks as a function of energy for the first 5 lowest order diffraction peaks in Si. As expected, higher energies require thicker masks. However, due to relativistic effects, the required thickness plateaus. Higher order diffractions require a thicker mask, but all of the shown Bragg peaks require mask thicknesses that are well within the thickness range of commercially available Silicon membranes. In contrast, the mask thickness needed to inelastically stop the beam is impractically large.
[0021] Electrons which are diffracted do so by a well-defined Bragg angle, which depends on the electron energy and diffraction peak, as shown in FIG. 2. By separating out these diffracted electrons, a spatially modulated electron beam carrying the same spatial pattern as the mask is created. The variation in dose deposition is achieved through the elastic scattering of electrons, which is determined by the thickness of the crystal where the electron beam passes through. It should be noted that this is not stopping the electron beam, which is an inelastic process that deposits energy in the mask whether it is crystalline or amorphous. Furthermore, inelastic scattering ruins the beam's coherence or resolution as electrons are stopped and the energy spread and momentum spread of the beam will increase. The stopping power of inelastic scattering also requiresa significantly thicker target which results in higher aspect ratios for the mask features and degrades the imaging resolution.
[0022] Elastic scattering does not deposit energy in the mask, does not alter the beam's coherence or resolution and allows for full contrast modulation 0-100% in the imaging plane. The pattern on the mask does not need to have nanometer- scale features as the image of the beam can be demagnified for exposure onto the resist. A demagnification of 100X is possible, allowing standard photolithographic, electron beam lithographic or other microfabrication techniques to produce the needed mask pattern. After fabrication of the mask, it is placed in the EBL system.
[0023] FIG. 3 shows a simplified schematic diagram of one example of the EBL system 100. The electron source 100 may consist of a photo, field or thermionic electron source. The acceleration mechanism includes either D C. electric fields and / or rf electromagnetic waves in accelerating structures. Magnets are used to collimated and focus the electron beam as need to illuminate the mask with a small divergence. The diffracted beam is projected, with or without demagnification, onto the sample. Solenoids 115 or quadrupole magnets 120 can be used to focus the beam. Higher order magnets, not shown, (e.g. sextupoles and octupoles) can used to correct for aberrations. A high-coherence electron beam, with post acceleration as needed, illuminates the patterned crystalline target 125. The crystalline target 125 is located in the image plane of the electron beam, where the divergence of the beam is smaller than the Bragg angle for this energy and the target material. After the beam passes through the target the electron beam is reimaged onto the resist on the wafer 140 for exposure. This imaging can be performed with static magnetic fields from solenoids 135 or quadrupoles 130 with higher order magnets for aberration correction, similar to a standard TEM column but projecting or demagnifying the beam to the desired feature size.
[0024] The stability of the pattern on the resist is primarily determined by the stability of the static crystalline target position and the static magnetic field quality, as the divergence of the beam must be less than the Bragg angle, which therefore imposes a condition that electron beam have a pointing jitter that does not impact the image resolution. If the image is projected with diffraction contrast either a bright or dark field image can beproduced by placing an aperture in the focal plane. If the image is produced with phase contrast multiple Bragg peaks up to the full beam is reimaged onto the target. The scale of the full EBL tool is on the order of a few meters for the electron column, with additional space needed to load patterning targets or wafers. The achievable dose rate is determined by the electron beam current which can be in the 10s of mA range which is 6-7 orders of magnitude greater than the dose delivered from a conventional rastered EBL system and matches or exceeds the equivalent dose rate by an EUV lithography tool.
[0025] An experimental demonstration of the nanopatterning scheme is shown in FIG. 4. A mask 200 is illuminated by a collimated electron beam 210. In this bright field imaging mode the diffracted electrons are blocked at the back focal plane and the undiffracted electrons are projected onto the image plane 220. In this experiment all of the essential components to produce the electron beam are present. However, the nanopatterned beam is magnified to make it visible on the detector in an electron microscope. In an EBL system, the image could be demagnified. At the image plane 220 a wafer coated with resist would be exposed to the patterned electron beam for selective exposure. To increase the throughput of the system the electron beam current can be increased.
[0026] This nanomodulation scheme was originally proposed for the longitudinal patterning of electron beams for generating fully coherent x-rays in a free electron laser (FELs), and was shown theoretically to produce sub-nm scale patterns. Subsequently, the beam patterning and contrast has been demonstrated experimentally at both the fewhundred keV and MeV scale, and showing full contrast is achievable over mm-scale exposures. In order for the diffraction contrast to be observed the electron beam coherence (or achievable resolution) should be sufficient to coherently interact with the atomic structure of the silicon crystal, verifying that the electron beam holds the potential for sub-nm resolution.
[0027] In EBL, the resist plays an important role in defining the patterns on a substrate. EBL resists, like optical resists, are materials that undergo chemical changes when exposed to an electron beam, allowing selective areas to be developed and removed after exposure. The two primary types of resists used in EBL are positive and negative resists.In positive resists like poly methyl methacrylate (PMMA), absorbed dose severs polymer chains, causing the exposed areas to become soluble and wash away during development, leaving the unexposed regions intact. In contrast, negative resists like Hydrogen silsesquioxane (HSQ) become cross-linked and hardened when exposed to the electron beam, making the exposed areas resistant to the developer. The choice of resist depends on the specific requirements of the application, with positive resists often used for higher resolution patterns and negative resists for applications requiring greater etch resistance.
[0028] The performance of a resist in EBL is determined by key factors such as sensitivity, resolution, and contrast. Sensitivity refers to how much electron dose is required to expose the resist — high sensitivity resists require less exposure time, improving throughput. However, high sensitivity often comes at the expense of resolution because the electron beam can cause scattering and secondary electron effects, blurring the pattern. Resolution is a measure of how small a feature the resist can accurately reproduce, and for advanced EBL, it needs to be on the scale of a few nanometers.Contrast is how sharply the exposed and unexposed regions are differentiated during development, which is critical for maintaining feature accuracy. The challenge is balancing these properties to optimize the performance of the resist, especially at nanometer scales where pattern fidelity and line edge roughness become more difficult to control.
[0029] Dosage requirements vary greatly depending on the resist, substrate, pattern geometry, and beam energy. Typical dosages for PMMA with beam energies from 30-150 keV lie between 300-1500 pC / cm2, though dosages as high as 3000 pC / cm2may be required for small, isolated features. HSQ requires even higher dosages around 2000 pC / cm2. Modern chemically amplified resist are engineered to amplify the effects of absorbed dose, allowing dosages below even 10 pC / cm2, at the cost of resolution. High required dosage remains a constraint of EBL.
[0030] Curing (or exposing) photoresist is a critical step in lithography processes, whether using photons or an electron beam. Each method requires different radiation doses due to the distinct interactions between the radiation and the photoresist. EUV lithography requires a significantly lower dose (measured in energy terms) compared toe-beam lithography. The dose for EUV is typically in the millijoules per square centimeter range, while for e-beam lithography, it is in microcoulombs per square centimeter, which corresponds to a much larger energy deposition. EUV is more efficient compared to conventional EBL in large-scale manufacturing due to lower doses and faster processing times, but it requires expensive and complex infrastructure.Conventional EBL is more precise for small-scale, high-resolution applications but is much slower and requires higher doses to achieve the desired exposure.
[0031] Electrons do not have a wavelength in the conventional sense, but their de Broglie wavelength at typical e-beam energies (e.g., 100 keV) is extremely small (on the order of picometers), enabling very fine feature resolution. The dose required for e-beam lithography is significantly higher than for EUV, typically ranging from 300 to 3000 pC / cm2, depending on the resist material (e.g., PMMA, HSQ) and the desired resolution. To convert this to energy, the relationship depends on the resist sensitivity and the acceleration voltage, but it generally corresponds to higher energy deposition than EUV. Electron beams cause exposure primarily by electron scattering, leading to the breaking of chemical bonds in the photoresist or cross-linking depending on the resist type (positive or negative).
[0032] At 300 W, a system can pattern about 170 wafers per hour. To match this with EBL, EUV power is converted to beam current using the dose deposition required to treat the resist of 10-30 mJ / cm2for EUV and 50 to 500 pC / cm2for an electron beam. While the deposited charge would require a current in the range of 2-20 mA, the overall system performance would require significantly elevated currents to match the full production rate of 200 wafers per hour. However, if such a system operates in this current range and we assume a voltage of 300 keV, the beam power required would be in the range of 600 W to 6 kW or -100X less power than required by an EUV system.
[0033] FIG. 5 shows a simplified, schematic diagram of one example of a diffraction arrangement for demonstrating the principle of patterning PMMA with a diffraction patterned electron beam. The arrangement includes a PMMA-coated substrate 300 attached directly to a single-crystal silicon diffraction mask 310. The PMMA-coated substrate 300 has a window 315 to facilitate angular alignment of the package withrespect to the incident electrons by monitoring the diffraction pattern produced by the mask without the effects of the PMMA and sample substrate. The mask membrane should have a thickness equal to the diffraction extinction length. In some cases the mask may consist of a grating 320 etched into the membrane to half the depth of half the extinction length. In his way, maximum diffraction occurs in electrons passing through the etched region, and no diffraction occurs in electrons passing through the un-etched region. By matching the spatial period of the grating (P) to the Bragg angle (0) and drift length between the membrane and PMMA (L) by tan(0) = P / L, contrast is produced at the plane of the resist without the need for optics separating the diffracted electrons. This arrangement does not allow for the demagnification of the mask pattern and does require a specific exposure pattern, but is otherwise fully equivalent and consistent with a diffraction-based approach to EBL.Additional Embodiments and Variations
[0034] In addition to the embodiments described above, numerous variations, modifications, and alternative configurations may be employed without departing from the scope of the present disclosure.
[0035] In various embodiments, the patterned target may comprise materials other than single-crystal silicon. For example, the target may include polycrystalline materials, amorphous materials, compound semiconductors, metals, ceramics, multilayer structures, or composite materials. The target may also include hybrid structures combining crystalline and non-crystalline regions.
[0036] The patterned target may be formed as a membrane, wafer, thin film, suspended structure, or supported structure. In some embodiments, the target may include multiple layers configured to produce different diffraction or phase modulation effects. Patterning of the target may include variations in thickness, composition, crystallographic orientation, strain, doping, or other material properties to achieve desired electron beam modulation characteristics.
[0037] The electron source may comprise any suitable source capable of producing an electron beam with sufficient coherence and brightness. Non-limiting examples include:DC field emission sources, RF field emission sources, thermionic emitters, photoemission sources, laser-driven electron sources. In some embodiments, multiple electron sources may be used, either sequentially or simultaneously, to increase throughput or enable parallel processing.
[0038] The electron optical system may include any combination of elements configured to shape, direct, focus, filter, or otherwise manipulate the electron beam. These may include, without limitation solenoids, quadrupole lenses, higher-order multipole elements (e g., sextupoles, octupoles), electrostatic lenses, apertures or beam stops, aberration correction elements. In some embodiments, adaptive or dynamically adjustable optical elements may be used to compensate for drift, aberrations, and process variations.
[0039] The resist material may include any material responsive to electron beam exposure, including: positive resists, negative resists, chemically amplified resists, inorganic and hybrid resists.
[0040] Substrates may include semiconductor wafers, glass, metals, polymers, or other materials. In some embodiments, multilayer substrates or pre-patterned substrates may be used.
[0041] Process conditions such as dose, beam energy, and exposure time may be varied to optimize resist response and pattern fidelity. In some embodiments, throughput may be increased through higher beam current, multiple beams, parallel exposure regions, scanning or stepping of the substrate and / or multiple patterned targets The system may also be configured for continuous processing, batch processing, or hybrid modes. The system may be implemented at various physical scales, including compact laboratory systems or large-scale industrial systems. The electron column may be configured in vertical, horizontal, or angled orientations. Multiple columns may be used in parallel or series. In some embodiments, modular system architectures may be employed, allowing replacement or reconfiguration of components such as targets, sources, or optical elements.
[0042] The system may include alignment and control subsystems configured to maintain proper positioning and stability of components. These may include, without limitation, feedback systems, beam position monitors, vibration isolation systems, and thermalstabilization systems Control systems may be automated and may include real-time adjustment of beam parameters.
[0043] The electron beam employed during exposure delivers substantial energy to the wafer, resulting in localized heating and corresponding thermal expansion. At small feature sizes, such thermal expansion can induce positional drift of features during exposure, thereby degrading patterning accuracy. Because the exposure process is intermittent such that the electron beam is inactive while the wafer is repositioned between exposure fields, the resulting thermal input is non-steady-state in nature, rendering compensation for thermally induced distortions particularly challenging. This effect is more pronounced in electron projection lithography relative to extreme ultraviolet (EUV) lithography due to the higher heat deposition associated with electron beams.
[0044] In some embodiments, a system is provided that supplies auxiliary thermal energy to the exposure region during intervals in which the primary electron beam is inactive, and reduces or terminates such auxiliary heating when the primary beam is active. By supplementing the intermittent thermal input of the electron beam with controlled auxiliary heating, the net thermal profile experienced by the wafer may be maintained in a substantially steady-state condition, thereby facilitating more effective compensation of thermal expansion effects.
[0045] Although such auxiliary heating may increase the total thermal load to be removed from the wafer, it advantageously enables the wafer to maintain a substantially constant temperature, thereby reducing feature displacement attributable to thermal expansion. In further embodiments, one or more additional heat sources may be positioned to direct thermal energy toward peripheral regions of the wafer, thereby promoting a more uniform temperature distribution across the wafer surface.
[0046] FIG. 6 is a simplified schematic diagram illustrating an example of a method for thermal stabilization consistent with the foregoing embodiments. As shown, the method employs a system 300 configured to provide auxiliary heat 310 to an exposure zone during intervals in which the electron beam 320 is inactive, and to reduce or discontinue the auxiliary heat 310 when the electron beam 320 is active. In this manner, the auxiliaryheating supplements the intermittent thermal input from the electron beam 320 to produce a substantially steady heat input.
[0047] In combination with a wafer cooling system, such as a helium backside gas cooling chuck 330 configured to cool the wafer 340, the temperature of the wafer 340 may be maintained in a substantially stable condition, thereby minimizing thermal expansion effects. In some embodiments, additional heat sources 350 may be directed toward peripheral regions of the wafer 340 to promote a more uniform temperature distribution. The auxiliary heat 310 and / or the additional heat sources 350 may be provided by infrared laser sources, other infrared emitters, resistive heating elements, or other suitable heating mechanisms.
[0048] Any of the features described herein may be combined in any suitable manner. Elements described in connection with one embodiment may be used in other embodiments. Dimensions, materials, and operating parameters provided herein are examples and may be varied depending on application.
[0049] It is to be understood that the disclosure teaches just some examples of embodiments in accordance with the invention and that many variations of the invention can easily be devised by those skilled in the art after reading this disclosure and that the scope of the present invention is to be determined by the following claims.
Claims
What is claimed is:
1. An electron beam lithography system comprising:an electron source configured to generate an electron beam;a patterned target positioned to interact with the electron beam, the patterned target being configured to modulate the electron beam through diffraction such that the patterned target interacts with the electron beam through elastic scattering;an electron optical system configured to project at least a portion of the modulated electron beam onto a substrate; anda substrate support configured to position a resist-coated substrate at an image plane of the electron optical system,wherein the system is configured to produce a spatially patterned electron dose on the substrate corresponding to a pattern defined by the patterned target.
2. The system of claim 1, wherein the patterned target comprises a crystalline material configured to produce diffraction of the electron beam.
3. The system of claim 2, wherein the crystalline material comprises silicon.
4. The system of claim 2, wherein the patterned target has a thickness selected based on an extinction length associated with a Bragg diffraction condition.
5. The system of claim 4, wherein at least a portion of the patterned target comprises regions having a thickness corresponding to approximately one-half of the extinction length.
6. The system of claim 1, wherein the electron optical system is configured to demagnify the patterned electron beam prior to exposure of the substrate.
7. The system of claim 6, wherein the demagnification is at least 10 times.
8. The system of claim 6, wherein the demagnification is approximately 100 times.
9. The system of claim 1, wherein the electron source comprises at least one of a field emission source, a thermionic source, or a photoinjector.
10. The system of claim 1, wherein the electron optical system comprises one or more magnetic elements selected from solenoids, quadrupoles, sextupoles, and octupoles.
11. The system of claim 1, wherein the system is configured such that a divergence of the electron beam at the patterned target is less than a Bragg angle associated with the patterned target.
12. The system of claim 1, wherein the patterned target is configured to modulate the electron beam without substantial inelastic scattering.
13. The system of claim 1, wherein the system is configured to operate with an electron beam current in a milliampere range.
14. The system of claim 1, wherein the system is configured to produce a dose rate comparable to or exceeding that of an extreme ultraviolet lithography system.
15. The system of claim 1, wherein the patterned target comprises a membrane structure having patterned thickness variations configured to control diffraction behavior.
16. The method of claim 2, wherein the patterned target comprises a grating structure configured such that a spatial period of the grating corresponds to a Bragg angle and a distance to the substrate.
17. The system of claim 1, wherein the system is configured to produce nanoscale features over an area greater than one millimeter.
18. A method of patterning a substrate using an electron beam, the method comprising: generating an electron beam;directing the electron beam toward a patterned target;modulating the electron beam via interaction with the patterned target through diffraction and elastic scattering;projecting the modulated electron beam onto a resist-coated substrate; andexposing the resist-coated substrate to produce a patterned exposure corresponding to the patterned target.
19. The method of claim 18, wherein modulating the electron beam comprises diffracting electrons at a Bragg angle determined by an energy of the electron beam.
20. The method of claim 18, wherein modulating the electron beam comprises producing contrast based on elastic scattering within the patterned target.
21. The method of claim 18, further comprising selecting a thickness of the patterned target based on an extinction length associated with a diffraction condition.
22. The method of claim 18, further comprising demagnifying the modulated electron beam prior to exposure of the substrate.
23. The method of claim 22, wherein the demagnification is greater than 50 times.
24. The method of claim 18, further comprising controlling at least one of beam energy, beam current, or exposure dose to optimize interaction with the resist.
25. The method of claim 18, wherein projecting the modulated electron beam comprises using magnetic focusing elements.