Method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate
Through steps such as dilution, neutralization, reduction and spray drying, high-purity chromium formate is produced from chromium-containing waste liquid, which solves the high cost and safety problems in the existing chromium formate production process and realizes low-cost and efficient formic acid production. Chromium production avoids the direct handling of hexavalent chromium and the use of carcinogens.
Patent Information
- Application Number
- CN202410879327.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-02
- Publication Date
- 2024-10-29
AI Technical Summary
The existing chromium formate production process has high cost, safety and technical difficulties, and involves the carcinogen chromate, resulting in an unsafe production process, high equipment requirements, and construction costs that are not proportional to benefits.
Using chromium-containing waste liquid or basic chromium sulfate as the chromium source, high-purity chromium formate is produced through the steps of dilution, neutralization, reduction, precipitation, filtration, steam heating and spray drying, avoiding the direct treatment of hexavalent chromium. Reduces energy consumption and utilizes sea wave waste water resources for reuse.
It achieves low-cost and efficient conversion of low-value-added chromium-containing waste liquid into high-value-added chromium formate, reducing reaction time and cost, and does not involve carcinogens, improves product purity and production safety, and is suitable for large-scale production .
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of fine chemicals and new materials, and more specifically, the invention relates to a method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate. Background Art
[0002] Chromium formate is a green powder, which decomposes into Cr at 300-400℃. 2 O 3 , mainly used in leather tanning, mordant dyeing and trivalent chromium electroplating; as well as the film and photography industries. It can also be used as a chemical reagent, olefin polymerization catalyst, oxidation catalyst, latex hardening, and drilling slurry for mining. It is an important product to improve the chromium material sector.
[0003] Chromium-containing waste liquid is a low-value-added product generated in the process of producing chromium-based high-value-added products. Chromium-containing waste liquid can be used to produce chromium powder, chromium hydroxide and other front-end products, and then used in subsequent material production.
[0004] At present, the main production method of chromium formate commonly seen on the market is to use formaldehyde to reduce chromic anhydride, and then add formic acid for acidification. Shandong Chemical Industry has announced a production process called "Optimization of Crystallization and Drying Processes in the Production of Chromium Formate" (Volume 52, 2023), which uses formic acid reduction and acidification of chromic anhydride to prepare chromium formate production methods, and then uses cyclone flash evaporation to dry it. The continuous circulation of the mother liquor produced by this method will cause further enrichment of impurities and affect the quality. At the same time, the production cost of chromic anhydride is relatively high. Patent CN109852741A discloses a method for preparing a non-pickling chrome tanning agent, which uses sulfur dioxide to reduce dichromate to prepare basic chromium sulfate, and then adds 10% to 30% A auxiliary and 20% to 50% B auxiliary relative to the mass of the chromium compound. Auxiliary A is a low-carbon monobasic organic salt such as sodium formate. Finally, after spray drying, a high-quality chrome tanning agent is obtained. This preparation method SO 2Reduction, and adding a monobasic low-carbon organic acid salt, the preparation cost is relatively high. Patent CN116332842A discloses a preparation method for the co-production of chromium formate and chromium propionate, belonging to the field of organic synthesis technology, the method comprises: in a microwave environment, chromium trioxide, propionic acid and hydrogen ion donor material, 2-pyridine formaldehyde and solvent are mixed and reacted, and a solid-liquid mixed reaction liquid is obtained after the reaction is completed; the solid-liquid mixed reaction liquid is subjected to a first separation and purification to obtain 2-pyridine formic acid chromium solid and a first separation liquid; the first separation liquid is subjected to a second separation and purification to obtain chromium propionate solid. This method has high requirements for equipment in the preparation process, and the construction cost is not proportional to the benefits. Patent CN110156587A discloses a process for synthesizing chromium formate from chromium chromate, comprising adding water and chromium chromate to a reactor, turning on ultrasonic waves and stirring and beating, heating and heating; slowly dripping formic acid at a uniform speed to control the temperature; slowly dripping a reducing agent solution, and continuing to keep warm and mature after the reaction liquid is free of hexavalent chromium, cooling and crystallizing to obtain chromium formate. This method involves the use of chromium chromate, one of the three major carcinogens in the chromium salt industry, which is extremely unfriendly to the operator and the environment during the production process. Patent CN101633613B discloses a method for preparing chromium formate, 1) 50 to 60 parts of industrial formic acid are diluted with 150 to 180 parts of water by mass, added to a reactor containing 80 to 100 parts of chromium tanning waste liquid precipitation filter cake, heated from room temperature to 60 to 80°C, and reacted for 20 to 30 minutes; 2) Secondly, the above reaction materials are filtered through a filter cloth to obtain a crude chromium formate solution; 3) Then, the crude chromium formate solution is added to the reactor, heated to 95 to 100°C, and 90 to 120 parts of water are distilled out; 4) Finally, the remaining reaction liquid after distillation is cooled to 10 to 20°C, crystallized for 3 to 4 hours, and filtered through a filter cloth to obtain solid chromium formate. This method involves a distillation process, and the distillation cost is difficult to be proportional to the benefits during the production process. The above methods all have problems in cost, safety and technology in the production process. There is an urgent need for a chromium formate production process with simple process route, low energy consumption and safe and reliable production process. Summary of the invention
[0005] An object of the present invention is to solve at least the above problems and / or disadvantages and to provide at least the advantages which will be described hereinafter.
[0006] In order to achieve these purposes and other advantages according to the present invention, a method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate is provided, comprising the following steps:
[0007] Step 1: using chromium-containing waste liquid or basic chromium sulfate solid as a chromium source, diluting in proportion to obtain a chromium-containing slurry;
[0008] Step 2: adding a neutralizing agent to the chromium-containing slurry, heating and stirring to dissolve, adding sulfuric acid to adjust the pH, and then adding a reducing agent to obtain a reducing solution;
[0009] Step 3: adding caustic soda flakes to the reducing solution to adjust the pH to obtain chromium hydroxide precipitate, and then filtering and washing the precipitate on a plate and frame. After washing, a chromium hydroxide filter cake is obtained for standby use;
[0010] Step 4, adding formic acid into the reaction tank, then turning on steam heating, stirring and fan at the same time, and then adding the chromium hydroxide filter cake obtained in step 3 in batches, stirring and reacting for a period of time after each addition, until the chromium hydroxide filter cake is completely added, reacting for 1 hour after the addition, sampling and filtering, observing whether there are undissolved particles, if there are, continuing to keep warm and react, if the liquid is dark green, and there are no undissolved particles and hexavalent chromium, it is determined that the reaction is completed to obtain a chromium formate solution;
[0011] Step 5: spray-drying the chromium formate solution obtained in step 4 to obtain a high-purity chromium formate product.
[0012] Preferably, in the step 1, the concentration of the chromium-containing waste liquid or basic chromium sulfate is 20-55° Bé, the volume ratio of the chromium-containing waste liquid to water is 1:0.5-1.5, and the mass ratio of basic chromium sulfate to water is 1:1-5.
[0013] Preferably, in step 2, the neutralizing agent is one or more of sodium dichromate, sodium chromate or chromic anhydride.
[0014] Preferably, in step 2, the heating and stirring temperature is 60-85°C, the pH is adjusted to 2.0-3.5, and the reducing agent is persulfate, peroxide, hydrazine hydrate, seawater, sodium pyrosulfite, SO 2 , sodium thiosulfate, organic alcohol, organic aldehyde, sugar, etc. one or more.
[0015] Preferably, in the step 2, when adding the reducing agent, the reducing agent is added according to the volume ratio of hexavalent chromium to the reducing agent in the chromium-containing slurry of 1:0.1-100. When adding, first add part of the reducing agent, stir evenly, then take a sample and titrate to observe whether there is still hexavalent chromium, and then decide whether to continue adding until there is no hexavalent chromium.
[0016] Preferably, in step three, the pH is adjusted to 7.0-7.5.
[0017] Preferably, in step 3, the mass ratio of chromium hydroxide precipitate to water is controlled to be 1:5 during washing, the washing time is more than 20 minutes, the washing times are 1 to 6 times, and the sample is sent for testing of chromium content after the first washing, and the chromium content is measured as Cr 2 O 3 The calculation of the subsequent formic acid addition is based on the sulfate content being less than 1000ppm.
[0018] Preferably, in step 4, the steam heating temperature is 90-100° C., and when the chromium hydroxide filter cake is added in batches, 20% is added each time and stirred for reaction for 10 minutes.
[0019] Preferably, in the step 4, the amount of formic acid added is calculated according to the following formula:
[0020] Y (HCOOH) =X Cr(OH)3 ×a×b×c×d×e×f
[0021] Among them, X Cr(OH)3 is the mass of chromium hydroxide filter cake, Y (HCOOH) is the mass of formic acid that needs to be added theoretically, a is Cr 2 O 3 The relative molecular mass of Cr(OH) 3 The relative molecular mass of Cr 2 O 3 Converted to Cr(OH) 3 The conversion amount of chromium atoms is 2, and d is the Cr(OH) produced when using different waste liquids. 3 Content, its value is 0.12~0.15, e is according to Cr(OH) 3 The ratio of formic acid required by the formic acid reaction equation is 138 / 103, and f is the concentration of formic acid 85wt%;
[0022] Formic acid 20% excess: Z (HCOOH) =Y (HCOOH) ×(1+0.2), where Z (HCOOH) is the actual amount of formic acid added.
[0023] Preferably, in step five, the spray drying has an inlet temperature of 180-220° C., an outlet temperature of 95-105° C., and a feed screw rotation frequency of 6.2-8.9 Hz.
[0024] Preferably, the high-purity chromium formate obtained in step 5 is post-treated, comprising the following steps:
[0025] S1. Disperse collagen in water at a collagen to water mass ratio of 1 to 5:25 to prepare a collagen suspension, fully shake at 20 to 50° C. for 12 to 48 hours, and adjust the pH of the suspension to 2 to 4 with hydrochloric acid for standby use;
[0026] S2. Dissolve high-purity chromium formate in water at a mass ratio of high-purity chromium formate to water of 1:1-1.5, add a small amount of acetic acid thereto, add sodium hydroxide to adjust the pH to 2.8-4, stir for 4-12 hours, and obtain a mixed solution, wherein the molar ratio of acetic acid to chromium formate is 1:3-5.
[0027] S3, adding 5-7wt% of the total mass of chromium formate in a collagen suspension to the mixed solution, stirring evenly and aging for 24-48h, and finally spray drying at 75-90°C to obtain protein-modified chromium formate.
[0028] The present invention has at least the following beneficial effects:
[0029] (1) The present invention utilizes multiple by-products to recycle and recycle low-value-added chromium-containing waste liquid or basic chromium sulfate in an efficient and low-cost manner to convert it into high-value-added and high-performance chromium hydroxide, and then prepares it into chromium formate. Compared with the preparation of chromium formate using chromium chromate as raw material, the production process of this patent does not involve carcinogens.
[0030] (2) The present invention utilizes the sodium thiosulfate wastewater as a resource for the reduction of hexavalent chromium.
[0031] (3) The present invention obtains refined chromium hydroxide by reducing and washing chromium-containing waste liquid or basic chromium sulfate, and obtains high-purity chromium formate by directly mixing and reacting chromium hydroxide with formic acid. The reaction can be carried out without microwave or specific conditions, and hexavalent chromium reduction is not involved, which greatly reduces the reaction time and cost. The preparation method is simple, cost-saving, and easy to implement in the production line.
[0032] (4) Compared with the distillation method, the present invention introduces spray drying, which saves product output time and reduces energy costs, and has great advantages in large-scale production.
[0033] (5) Chromium formate is modified with collagen so that the chromium formate is in full contact with the elastic fibers in the collagen, and the elastic fibers and the chromium formate are combined. The obtained modified chromium formate can make the tanned leather have better leather softness and lower chromium absorption rate when used as a chrome tanning agent.
[0034] Other advantages, objectives and features of the present invention will be embodied in part through the following description, and in part will be understood by those skilled in the art through study and practice of the present invention. DETAILED DESCRIPTION
[0035] The present invention is described in further detail below so that those skilled in the art can implement it according to the description.
[0036] It should be understood that terms such as “having”, “including” and “comprising” used herein do not specify the existence or addition of one or more other elements or combinations thereof.
[0037] It should be noted that in the description of the present invention, the orientation or position relationship indicated by the term is the orientation or position relationship shown, which is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.
[0038] Example 1
[0039] Step 1: Add 1m 3 Add 1m 3 Dilute with water, at which point the chromium-containing waste liquid concentration is about 30°Bé, to obtain a chromium-containing slurry;
[0040] Step 2: add sulfuric acid to the chromium-containing slurry to adjust the pH to 2.5, heat to 70°C, stir for 20 minutes, and then add 0.6m 3 Haibo wastewater, add 0.5m 3 Haibo wastewater, after stirring evenly, take a sample and titrate to observe whether there is hexavalent chromium, and then decide whether to continue adding until there is no hexavalent chromium and obtain the reduced solution;
[0041] Step 3: Add caustic soda flakes to the reducing solution to adjust the pH to 7.0 to obtain chromium hydroxide precipitate, and then filter the precipitate on a plate and frame for washing. During washing, the mass ratio of chromium hydroxide precipitate to water is controlled to be 1:5, and the washing time is 25 minutes to obtain a chromium hydroxide filter cake for standby use; after the first washing is completed, send the sample to detect the chromium content, and the Cr 2 O 3 The chromium content is 12.5%;
[0042] Step 4, take 1000kg of chromium hydroxide filter cake for standby use, add 378kg of formic acid with a concentration of 85wt% into the reaction tank, then turn on steam heating, raise the temperature to 90°C, turn on stirring and fan at the same time, and then add chromium hydroxide filter cake in batches, add 200kg for the first time, stir and react for 10min, observe the dissolution in the tank, add 200kg of chromium hydroxide filter cake to the tank for the second time after dissolution, stir and react for 10min, observe the situation in the tank, and cycle in this way until all 1000kg of chromium hydroxide filter cake is added, react for 1 hour after adding, take samples and filter, observe whether there are undissolved particles, if there are, continue to keep warm and react, if the liquid is dark green, and there are no undissolved particles and hexavalent chromium, it is determined that the reaction is over to obtain a chromium formate solution;
[0043] Step 5: spray drying the chromium formate solution obtained in step 4 to obtain a high-purity chromium formate product. The spray drying inlet temperature is 180° C., the outlet temperature is 95° C., and the feed screw rotation frequency is 8 Hz.
[0044] The obtained high-purity chromium formate product was tested, and the chromium formate content was 99.5%, the moisture content was 0.4%, and the hexavalent chromium content was 9.0 ppm.
[0045] The high-purity chromium formate prepared in this embodiment is used to tan leather. 10 kg of animal fur is placed in a drum, 15 kg of water is added, the temperature is adjusted to 55°C, and then 0.5 kg of high-purity chromium formate is added. The drum is rotated for 6 hours for tanning. The chromium absorption rate is calculated to be 81.35% according to the chromium absorption rate = (the actual weight of chromium absorbed by the leather / the weight of chromium used in the tanning process) * 100%. The softness of the tanned leather is tested according to the flat push method in QB / T5155-2017, and the softness is measured to be 21.6 mm.
[0046] Example 2
[0047] Step 1: mixing 1 ton of basic chromium sulfate and water in a mass ratio of 1:5 and heating them to obtain a chromium-containing slurry;
[0048] Step 2: add sodium chromium to the chromium-containing slurry to adjust the concentration of the chromium-containing slurry to about 40°Bé, add sulfuric acid to the chromium-containing slurry to adjust the pH to 2.5, heat to 70°C, stir for 20 minutes, and then add 2.5 ml of chromium to the chromium-containing slurry at a volume ratio of 1:0.5. 3 Haibo wastewater, add 2.4m 3 Haibo wastewater, after stirring evenly, take a sample and titrate to observe whether there is hexavalent chromium, and then decide whether to continue adding until there is no hexavalent chromium and obtain the reduced solution;
[0049] Step 3: Add caustic soda flakes to the reducing solution to adjust the pH to 7.2 to obtain chromium hydroxide precipitate, and then filter the precipitate on a plate and frame for washing. During washing, the mass ratio of chromium hydroxide precipitate to water is controlled to be 1:5, and the water washing time is 25 minutes to obtain a chromium hydroxide filter cake for standby use; after the first washing is completed, send the sample to detect the chromium content, and the Cr 2 O 3 The chromium content is 14.4%;
[0050] Step 4: Take 1000 kg of chromium hydroxide filter cake for standby use, add 434 kg of formic acid with a concentration of 85 wt % into the reaction tank, then turn on steam heating, raise the temperature to 90 ° C, turn on stirring and fan at the same time, and then add the chromium hydroxide filter cake obtained in step 3 in batches, add 200 kg for the first time, stir and react for 10 minutes, observe the dissolution in the tank, add 200 kg of chromium hydroxide filter cake to the tank for the second time after dissolution, stir and react for 10 minutes, observe the situation in the tank, and repeat this cycle until all 1000 kg of chromium hydroxide filter cake is added, react for 1 hour after adding, take samples and filter, observe whether there are undissolved particles, if there are, continue to keep warm and react, if the liquid is dark green, and there are no undissolved particles and hexavalent chromium, it is determined that the reaction is over, and a chromium formate solution is obtained;
[0051] Step 5: spray drying the chromium formate solution obtained in step 4 to obtain a high-purity chromium formate product. The spray drying inlet temperature is 180° C., the outlet temperature is 95° C., and the feed screw rotation frequency is 8 Hz.
[0052] The obtained high-purity chromium formate product was tested and the chromium formate content was 99.6%, the moisture content was 0.3%, and the hexavalent chromium content was 9.0 ppm.
[0053] The high-purity chromium formate prepared in this embodiment is used to tan leather. 10 kg of animal fur is placed in a drum, 15 kg of water is added, the temperature is adjusted to 55 ° C, and then 0.5 kg of high-purity chromium formate is added. The drum is rotated for 6 hours for tanning. The chromium absorption rate is calculated to be 81.42% according to the chromium absorption rate = (actual weight of chromium absorbed by the leather / weight of chromium used in the tanning process) * 100%; the softness of the tanned leather is tested according to the flat push method in QB / T5155-2017, and the softness is measured to be 21.8 mm.
[0054] Example 3
[0055] Step 1: Add 1m 3 Add 1m 3 Dilute with water, at which point the chromium-containing waste liquid concentration is about 30°Bé, to obtain a chromium-containing slurry;
[0056] Step 2: add sulfuric acid to the chromium-containing slurry to adjust the pH to 2.5, heat to 70°C, stir for 20 minutes, add 100 kg of sodium pyrosulfite to the chromium-containing slurry at a volume mass ratio of 1:50, add 80 kg of Haibo first, stir evenly, take a sample and titrate to observe whether there is hexavalent chromium, and then decide whether to continue adding until there is no hexavalent chromium to obtain a reducing solution;
[0057] Step 3: Add caustic soda to the reducing solution to adjust the pH to 7.5 to obtain chromium hydroxide precipitate, and then filter the precipitate on a plate and frame for washing. During washing, the mass ratio of chromium hydroxide precipitate to water is controlled to be 1:5, and the washing time is 25 minutes to obtain a chromium hydroxide filter cake for standby use; after the first washing is completed, send the sample to detect the chromium content, and the Cr 2 O 3 The chromium content is 15%;
[0058] Step 4: Take 1000 kg of chromium hydroxide filter cake for standby use, add 453 kg of formic acid with a concentration of 85 wt % into the reaction tank, then turn on steam heating, raise the temperature to 90 ° C, turn on stirring and fan at the same time, and then add the chromium hydroxide filter cake obtained in step 3 in batches, add 200 kg for the first time, stir and react for 10 minutes, observe the dissolution in the tank, add 200 kg of chromium hydroxide filter cake to the tank for the second time after dissolution, stir and react for 10 minutes, observe the situation in the tank, and repeat this cycle until all 1000 kg of chromium hydroxide filter cake is added, react for 1 hour after adding, take samples and filter, observe whether there are undissolved particles, if there are, continue to keep warm and react, if the liquid is dark green, and there are no undissolved particles and hexavalent chromium, it is determined that the reaction is over to obtain a chromium formate solution;
[0059] Step 5: spray drying the chromium formate solution obtained in step 4 to obtain a high-purity chromium formate product. The spray drying inlet temperature is 180° C., the outlet temperature is 95° C., and the feed screw rotation frequency is 8 Hz.
[0060] The obtained high-purity chromium formate product was tested and the chromium formate content was 99.7%, the moisture content was 0.3%, and the hexavalent chromium content was 8.0 ppm.
[0061] The high-purity chromium formate prepared in this embodiment is used to tan leather. 10 kg of animal fur is placed in a drum, 15 kg of water is added, the temperature is adjusted to 55 ° C, and then 0.5 kg of high-purity chromium formate is added. The drum is rotated for 6 hours for tanning. The chromium absorption rate is calculated to be 81.43% according to the chromium absorption rate = (the actual weight of chromium absorbed by the leather / the weight of chromium used in the tanning process) * 100%; the softness of the tanned leather is tested according to the flat push method in QB / T5155-2017, and the softness is measured to be 21.9 mm.
[0062] Example 4
[0063] The difference between this embodiment and embodiment 1 is that the high-purity chromium formate obtained in step 5 is post-treated, comprising the following steps:
[0064] S1. Disperse 80 g of collagen in 1 kg of water to prepare a collagen suspension, fully shake at 30°C for 36 hours, adjust the pH of the suspension to 3 with hydrochloric acid, and set aside;
[0065] S2. Dissolve 10 kg of high-purity chromium formate in 12 L of water, add a small amount of acetic acid thereto, add sodium hydroxide to adjust the pH to 3, and stir for 8 hours to obtain a mixed solution, wherein the molar ratio of acetic acid to chromium formate is 1:3.
[0066] S3, adding a collagen suspension containing 5 wt% of the total mass of chromium formate to the mixed solution, stirring evenly and aging for 36 hours, and finally spray drying at 80° C. to obtain protein-modified chromium formate.
[0067] The protein-modified chromium formate prepared in this embodiment is used to tan leather. 10 kg of animal fur is placed in a drum, 15 kg of water is added, the temperature is adjusted to 55°C, and then 0.5 kg of protein-modified chromium formate is added. The drum is rotated for 6 hours for tanning. The chromium absorption rate is calculated to be 87.25% according to the chromium absorption rate = (actual weight of chromium absorbed by the leather / weight of chromium used in the tanning process) * 100%. The softness of the tanned leather is tested according to the flat push method in QB / T5155-2017, and the softness is measured to be 15.4 mm.
[0068] Example 5
[0069] The difference between this embodiment and embodiment 2 is that the high-purity chromium formate obtained in step 5 is post-treated, comprising the following steps:
[0070] S1. Disperse 80 g of collagen in 1 kg of water to prepare a collagen suspension, fully shake at 30°C for 36 hours, adjust the pH of the suspension to 3 with hydrochloric acid, and set aside;
[0071] S2. Dissolve 10 kg of high-purity chromium formate in 12 L of water, add a small amount of acetic acid thereto, add sodium hydroxide to adjust the pH to 3, and stir for 8 hours to obtain a mixed solution, wherein the molar ratio of acetic acid to chromium formate is 1:3.
[0072] S3, adding a collagen suspension containing 6 wt% of the total mass of chromium formate to the mixed solution, stirring evenly and aging for 36 hours, and finally spray drying at 80° C. to obtain protein-modified chromium formate.
[0073] The protein-modified chromium formate prepared in this embodiment is used to tan leather. 10 kg of animal fur is placed in a drum, 15 kg of water is added, the temperature is adjusted to 55°C, and then 0.5 kg of protein-modified chromium formate is added. The drum is rotated for 6 hours for tanning. The chromium absorption rate is calculated to be 87.34% according to the chromium absorption rate = (actual weight of chromium absorbed by the leather / weight of chromium used in the tanning process) * 100%. The softness of the tanned leather is tested according to the flat push method in QB / T5155-2017, and the softness is measured to be 15.2 mm.
[0074] Example 6
[0075] The difference between this embodiment and embodiment 3 is that the high-purity chromium formate obtained in step 5 is post-treated, comprising the following steps:
[0076] S1. Disperse 80 g of collagen in 1 kg of water to prepare a collagen suspension, fully shake at 30°C for 36 hours, adjust the pH of the suspension to 3 with hydrochloric acid, and set aside;
[0077] S2. Dissolve 10 kg of high-purity chromium formate in 12 L of water, add a small amount of acetic acid thereto, add sodium hydroxide to adjust the pH to 3, and stir for 8 hours to obtain a mixed solution, wherein the molar ratio of acetic acid to chromium formate is 1:3.
[0078] S3, adding a collagen suspension containing 7 wt% of the total mass of chromium formate to the mixed solution, stirring evenly and aging for 36 hours, and finally spray drying at 80° C. to obtain protein-modified chromium formate.
[0079] The protein-modified chromium formate prepared in this embodiment is used to tan leather. 10 kg of animal fur is placed in a drum, 15 kg of water is added, the temperature is adjusted to 55°C, and then 0.5 kg of protein-modified chromium formate is added. The drum is rotated for 6 hours for tanning. The chromium absorption rate is calculated to be 87.37% according to the chromium absorption rate = (actual weight of chromium absorbed by the leather / weight of chromium used in the tanning process) * 100%. The softness of the tanned leather is tested according to the flat push method in QB / T5155-2017, and the softness is measured to be 15.1 mm.
[0080] It can be seen from the results of Examples 1 to 6 that the protein-modified chromium formate obtained by post-treatment can effectively improve the softness and chromium absorption rate of leather during tanning.
[0081] Although the embodiments of the present invention have been disclosed as above, they are not limited to the applications listed in the specification and the implementation modes, and they can be fully applied to various fields suitable for the present invention. For those familiar with the art, additional modifications can be easily implemented. Therefore, without departing from the general concept defined by the claims and the scope of equivalents, the present invention is not limited to the specific details and the illustrations shown and described herein.
Claims
1. A method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate, It is characterized in that The following steps are involved: Step 1: using chromium-containing waste liquid or basic chromium sulfate solid as a chromium source, diluting in proportion to obtain a chromium-containing slurry; Step 2: adding a neutralizing agent to the chromium-containing slurry, heating and stirring to dissolve, adding sulfuric acid to adjust the pH, and then adding a reducing agent to obtain a reducing solution; Step 3: adding caustic soda flakes to the reducing solution to adjust the pH to obtain chromium hydroxide precipitate, and then filtering and washing the precipitate on a plate and frame. After washing, a chromium hydroxide filter cake is obtained for standby use; Step 4, adding formic acid into the reaction tank, then turning on steam heating, stirring and fan at the same time, and then adding the chromium hydroxide filter cake obtained in step 3 in batches, stirring and reacting for a period of time after each addition, until the chromium hydroxide filter cake is completely added, sampling and filtering after the reaction, observing whether there are undissolved particles, if there are, continuing to keep warm and react, if the liquid is dark green, and there are no undissolved particles and hexavalent chromium, it is determined that the reaction is completed, and a chromium formate solution is obtained; Step 5: spray-drying the chromium formate solution obtained in step 4 to obtain a high-purity chromium formate product.
2. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step 1, the concentration of the chromium-containing waste liquid is 20-55° Bé, the volume ratio of the chromium-containing waste liquid to water is 1:0.5-1.5, and the mass ratio of basic chromium sulfate to water is 1:1-5.
3. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step 2, the neutralizing agent is one or more of sodium dichromate, sodium chromate or chromic anhydride, and the volume ratio of the added neutralizing agent to the chromium-containing slurry is 0 to 100:
1.
4. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step 2, the heating and stirring temperature is 60-85°C, the pH is adjusted to 2.0-3.5, and the reducing agent is persulfate, peroxide, hydrazine hydrate, seawater wastewater, sodium metabisulfite, SO 2 , sodium thiosulfate, organic alcohol, organic aldehyde, sugar, etc. one or more.
5. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step 2, when adding the reducing agent, the reducing agent is added according to the molar ratio of hexavalent chromium to the reducing agent in the chromium-containing slurry of 1:0.1-100. When adding, first add part of the reducing agent, stir evenly, then take a sample and titrate to observe whether there is still hexavalent chromium, and then decide whether to continue adding until there is no hexavalent chromium.
6. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step 3, the pH is adjusted to 7.0-7.
5.
7. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step three, the mass ratio of chromium hydroxide precipitate to water is controlled to be 1:5 during washing, the washing time is more than 20 minutes, the number of washings is 1 to 6 times, and the sample is sent for detection of chromium content after the first washing, which is used to calculate the subsequent formic acid addition amount, based on the detection of sulfate content less than 1000ppm.
8. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step 4, the formic acid concentration is 85wt%, the steam heating temperature is 90-100°C, and when the chromium hydroxide filter cake is added in batches, 20% is added each time and stirred for reaction for 10 minutes.
9. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step 4, the amount of formic acid added is calculated according to the following formula: AND (HCOOH) =X Cr(OH)3 ×a×b×c×d×e×f Among them, X Cr(OH)3 is the mass of chromium hydroxide filter cake, Y (HCOOH) is the mass of formic acid that needs to be added theoretically, a is Cr 2 O 3 The relative molecular mass of Cr(OH) 3 The relative molecular mass of Cr 2 O 3 Converted to Cr(OH) 3 The conversion amount of chromium atoms is 2, and d is the Cr(OH) produced when using different waste liquids. 3 Content, its value is 0.12~0.15, e is according to Cr(OH) 3 The ratio of formic acid required by the formic acid reaction equation is 138 / 103, and f is the concentration of formic acid 85wt%; Formic acid 20% excess: Z (HCOOH) =Y (HCOOH) ×(1+0.2), where Z (HCOOH) is the actual amount of formic acid added.
10. The method for preparing chromium formate from chromium-containing waste liquid or basic chromium sulfate according to claim 1, It is characterized in that In the step 5, spray drying is performed, the inlet temperature is 180-220° C., the outlet temperature is 95-105° C., the feed screw rotation frequency is 6.2-8.9 Hz, and the chromium formate content in the obtained high-purity chromium formate is ≥99.3%.