Method for inhibiting photoresist blistering after wafer etching

By adding oxygen during the Dechucking process, the visible light generated by oxygen ionization and the ultraviolet light of argon are absorbed by reducing nitrogen generation and carbonization layers, the problem of photoresist foaming in micro-nano manufacturing is solved, and low-cost and efficient The process avoids blistering and apparent damage to the photoresist after etching.

CN118969666APending Publication Date: 2024-11-15NORTH ELECTRON RES INST ANHUI CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410976454.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-20
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

During the micro-nano manufacturing process, the photoresist is prone to bubble after dry etching due to bombardment of argon plasma, forming a dense carbonized layer and a pit caused by the pressure difference between nitrogen. The existing methods are costly and limited, and require additional Increase the Dechucking process and affect process efficiency.

Method used

During the Dechucking process, oxygen is added. By setting the amount of argon, oxygen flow, reaction pressure and radio frequency power, the ionized oxygen emits visible light and the ultraviolet light of argon absorbs each other, reducing nitrogen production, and removing the carbonization layer on the photoresist surface through oxygen ions , avoid bubbles.

Benefits of technology

Effectively suppress the blistering of photoresist after etching, solving the problem of apparent damage to the wafer, the process is simple, the cost is low, and there are no new processes, ensuring the apparent quality and high reliability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure FT_2
    Figure FT_2
  • Figure FT_3
    Figure FT_3
Patent Text Reader

Abstract

The invention relates to a method for inhibiting photoresist blistering after wafer etching, which comprises a Decking process after wafer etching, and is characterized in that oxygen is added into reaction gas argon of Decking, and the process parameters are set as follows: the argon amount is 300-400sccm, the oxygen flow is 10-30sccm, the reaction pressure is 150-250mT, the radio frequency power is 200-300W, and the process time is 30-60s. The method has the beneficial effects that the problem of photoresist blistering after etching can be effectively solved, and wafer appearance damage caused by blistering is solved; the method is simple in process, low in cost, free of newly added procedures, extremely high in reliability and capable of guaranteeing the appearance of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of micro-nano manufacturing technology and relates to a method for suppressing photoresist bubbling after wafer etching. Background Art

[0002] In the process of micro-nano manufacturing, wafers undergo processes such as lithography, etching, implantation, and oxidation to achieve multi-level processing and a complex combination of structures. Among them, dry etching is the main process for wafer patterning. The principle is that glow discharge ionizes the reaction gas to produce plasma, and the etched material undergoes physical and chemical reactions with the plasma and is removed. During the dry etching process, a large number of high-energy particles bombard the wafer surface, causing the wafer surface temperature to rise and affect the etching morphology. Therefore, the wafer needs to be fixed and helium needs to be purged on the back of the wafer to dissipate heat.

[0003] In the early days, wafers were fixed by mechanical clamping. This method had problems such as uneven wafer edges and particles caused by mechanical movement. In order to solve the shortcomings of mechanical clamping, an electrostatic adsorption method, ESC-Electrostatic Chuck, was invented. ESC-Electrostatic Chucking uses the Coulomb attraction of the two electrode plates of the capacitor to fix the wafer. This non-contact fixation method on the front of the wafer solves the problems of uneven wafer edges and particles in mechanical clamping. The ESC-Electrostatic Chucking method has obvious benefits, but an additional Dechucking process is required to release the ESC from the wafer. This process requires an inert gas (argon) plasma bombardment on the wafer surface to reduce or eliminate the electrostatic adsorption force, so that the sample can be easily released from the clamping device. However, argon plasma carries high energy. When it collides with the photoresist surface during the Dechucking process, it will cause some carbon atoms to overflow the photoresist surface and react with surrounding atoms to form a dense carbonized layer. At the same time, when argon gas is ionized, it will emit ultraviolet light, and the ultraviolet light will dissociate or cross-link with the photoresist. The generated nitrogen will be bound in the photoresist by the carbonized layer. Since the pressure in the cavity is extremely low, the generated nitrogen will form a certain pressure difference inside and outside the photoresist, causing the surface of the photoresist to bulge. When the surface of the photoresist is not sufficient to bind the nitrogen, the bulge explodes to form a pit.

[0004] Patent publication number US6207353B1 discloses a method of reducing blistering after etching by changing the composition of photoresist, specifically, changing the ratio of 4-hydroxystyrene, styrene and tert-butyl acrylate in the terpolymer, thereby increasing the adhesion between the photoresist and the substrate material, making it less likely to blister after etching. However, this method has great limitations and high cost. Summary of the invention

[0005] The purpose of the present invention is to make up for the deficiencies of the prior art and provide a method for inhibiting photoresist bubbling after wafer etching, which method has simple process, low cost, safety and high efficiency.

[0006] In order to achieve the above object, the technical solution adopted by the present invention is as follows: A method for suppressing photoresist bubbling after wafer etching includes a Dechucking process after wafer etching, characterized in that oxygen is added to the Dechucking reaction gas argon, and the process parameters are set as follows: argon volume 300-400sccm, oxygen flow rate 10-30sccm, reaction pressure 150-250mT, radio frequency power 200-300W, and process time 30-60s.

[0007] Furthermore, the components used for wafer etching are a radio frequency power supply, a radio frequency electrode and an E-chuck.

[0008] Furthermore, the argon gas volume is 320-350 sccm, the oxygen flow rate is 10-15 sccm, the reaction pressure is 200-250 mT, the RF power is 250-300 W, and the process time is 30-45 s.

[0009] Furthermore, the argon gas volume is 350-400 sccm, the oxygen flow rate is 15-25 sccm, the reaction pressure is 180-200 mT, the RF power is 250-300 W, and the process time is 45-55 s.

[0010] The method for solving the problem of photoresist bubbling after etching described in the present invention has the following principle: oxygen is added during the Dechucking process, and visible light is emitted when the oxygen is ionized. The visible light and ultraviolet light generated by ionized argon gas absorb and radiate each other, weakening the ultraviolet light of the argon gas, thereby reducing the reaction between ultraviolet light and photoresist during the Dechucking process, reducing the generation of nitrogen, and thus avoiding the bubbling of the photoresist; at the same time, the ionized oxygen ions will also react with the surface of the photoresist, removing the carbonized layer on the surface of the photoresist, allowing the residual nitrogen to overflow, thereby achieving the purpose of solving the problem of photoresist bubbling after etching.

[0011] The beneficial effects of the present invention are as follows: the method described in the present invention can effectively solve the problem of photoresist bubbling after etching and solve the apparent damage to the wafer caused by the bubbling; the method has simple process, low cost, no additional process, extremely high reliability, and ensures the device appearance. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 A schematic diagram of a wafer structure with photoresist bubbles after etching, wherein 1 is the photoresist, 2 is the dielectric film layer, 3 is the silicon substrate, and 4 is the bubbles caused by nitrogen; Figure 2 This is a photoresist blistering image after wafer etching; Figure 3 The surface image of the photoresist after etching using the method of Example 1; Figure 4 The surface image of the photoresist after etching using the method of Example 2; Figure 5 The surface image of the photoresist after etching using the method of Example 3; Figure 6 This is a photoresist surface image after etching using the method of Comparative Example 1. DETAILED DESCRIPTION

[0013] A method for inhibiting photoresist bubbling after wafer etching, the specific implementation steps are as follows: Example

[0014] (1) Take a six-inch double-polished silicon wafer and grow silicon dioxide on the surface with a thickness of 300nm; (2) Coating photoresist 1.0µm, photolithography, development, and hardening; (3) Silicon dioxide etching; (4) Dechucking after etching, argon volume 350sccm, oxygen flow 10sccm, reaction pressure 220mT, RF power 300W, process time 30s. Example

[0015] (1) Take a six-inch double-polished silicon wafer and grow silicon dioxide on the surface with a thickness of 500nm; (2) Coating photoresist 1.5µm, photolithography, development, and hardening; (3) Silicon dioxide etching; (4) Dechucking after etching, argon volume 375sccm, oxygen flow 15sccm, reaction pressure 200mT, RF power 300W, process time 40s. Example

[0016] (1) Take a six-inch double-polished silicon wafer and grow silicon dioxide on the surface with a thickness of 1000nm; (2) Coating photoresist 2.0µm, photolithography, development, and hardening; (3) Silicon dioxide etching; (4) Dechucking after etching, argon volume 375sccm, oxygen flow 15sccm, reaction pressure 200mT, RF power 300W, process time 60s.

[0017] Comparative Example 1 (1) Take a six-inch double-polished silicon wafer and grow silicon dioxide on the surface with a thickness of 1000nm; (2) Coating photoresist 2.0µm, photolithography, development, and hardening; (3) Silicon dioxide etching; (4) Dechucking after etching, argon volume 375sccm, oxygen flow 0sccm, reaction pressure 200mT, RF power 300W, process time 60s.

Claims

1. A method for inhibiting photoresist blistering after wafer etching, comprising a post-wafer etching dechucking process, characterized in that: Oxygen was added to the argon gas used in Dechucking reaction, and the process parameters were set as follows: argon volume 300-400sccm, oxygen flow rate 10-30sccm, reaction pressure 150-250mT, RF power 200-300W, and process time 30-60s.

2. A method for suppressing photoresist bubbling after wafer etching according to claim 1, characterized in that: The argon volume is 320-350sccm, the oxygen flow rate is 10-15sccm, the reaction pressure is 200-250mT, the RF power is 250-300W, and the process time is 30-45s.

3. A method for suppressing photoresist bubbling after wafer etching according to claim 1, characterized in that: The argon gas volume is 350-400 sccm, the oxygen flow rate is 15-25 sccm, the reaction pressure is 180-200 mT, the RF power is 250-300 W, and the process time is 45-55 s.

4. A method for suppressing photoresist bubbling after wafer etching according to any one of claims 1 to 3, characterized in that: The components used for wafer etching are a radio frequency power supply, a radio frequency electrode and an E-chuck.