Eddy current detection probe and method for gas turbine blade gas film inclined hole inner surface cracks
By designing an eddy current detection probe containing an excitation coil and a curved magnetic core, the problem of crack detection in the inner surface of the oblique hole of the gas turbine blade is solved, and high sensitivity and high accuracy detection is achieved, ensuring the integrity evaluation of the oblique hole structure .
Patent Information
- Application Number
- CN202411340780.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-25
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-09-25
AI Technical Summary
The existing vortex current detection methods are difficult to effectively detect cracks in the inner surface of the oblique hole of the gas membrane of the gas turbine blades, resulting in the inability to accurately evaluate the integrity and reliability of the parts, increasing the risk of failure and accidents.
An eddy current detection probe including an excitation coil and a bent magnetic core is designed. By adjusting the inclination angle of the magnetic core and the arrangement of the coil, the magnetic field can be effectively introduced to the inner wall of the inclined hole, improving the signal-to-noise ratio, and judging cracks by using differential signal detection method. The presence of the micro cracks ensures efficient detection.
High sensitivity detection of cracks on the inner surface of the oblique hole of the gas membrane of the gas turbine blade is realized, which enhances the detection signal quality and precise positioning ability, can accurately judge the existence and location of the cracks, reduces errors, and improves the accuracy and efficiency of detection.
Smart Images

Figure CN118980741A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an eddy current nondestructive testing probe, in particular to an eddy current testing probe and method for inner surface cracks of an inclined air film hole of a gas turbine blade. Background Art
[0002] Gas turbine blades rely on air film cooling holes to maintain their performance and life. Air film hole cooling technology uses cooling air to pass through specially designed small holes on the blade to form a protective cooling air film. This air film can reduce the temperature of the blade surface and reduce heat conduction to the blade material itself, thereby protecting the blade from damage by high-temperature gases. However, existing manufacturing technologies may introduce damage when processing these cooling holes, leading to the formation of cracks. These cracks may cause stress concentration during the service life of the blade, increase the risk of damage to the blade in harsh working environments, and shorten its service life. Compared with straight holes, inclined holes are more likely to produce stress concentration, which in turn produces defects. These defects may have an adverse effect on the performance and service life of the parts and may cause blade failure or more serious accidents. In addition, long-term complex service conditions, stress concentration, structural aging, etc., may also cause fatigue cracks around the holes. These damages seriously reduce the service life of parts. Therefore, it is very necessary to conduct production inspections on the inclined hole structure parts and regularly conduct integrity assessments and reliability inspections on the parts of the air film hole structure in service.
[0003] Eddy current nondestructive testing technology has high sensitivity for defect detection, and its non-contact characteristics mean that it does not need to consider coupling agents. It is the most common nondestructive testing method in the inspection of key components of major equipment. Traditional eddy current testing methods will encounter many problems in the inspection process of the gas turbine blade air film inclined hole structure. Due to the particularity of the inclined hole structure, cracks mostly exist on the inner surface. At this time, the traditional eddy current detection probe cannot detect whether there are defects due to the eddy current skin characteristics. In summary, considering the harmfulness of the crack defects of the gas turbine blade air film inclined hole structure to aircraft engine components, the design and development of an eddy current detection probe for the cracks on the inner surface of the gas turbine blade air film inclined hole is of great significance in practical engineering. Summary of the invention
[0004] In order to solve the problems existing in the above-mentioned prior art, the purpose of the present invention is to provide an eddy current detection probe structure and method for cracks on the inner surface of the inclined air film holes of gas turbine blades, so as to achieve high-sensitivity detection of cracks on the inner surface of the inclined air film holes of gas turbine blades.
[0005] To achieve the above object, the present invention adopts the following technical solution:
[0006] An eddy current detection probe for cracks on the inner surface of an inclined hole of a gas turbine blade film, the eddy current detection probe comprises an excitation coil 2 and a bent magnetic core 6 of the excitation coil disposed therein, a first detection coil 3 and a bent magnetic core 7 of the first detection coil disposed therein, a second detection coil 4 and a bent magnetic core 8 of the second detection coil disposed therein; during detection, the first detection coil 3 and the second detection coil 4 are located on both sides of the excitation coil 2, and the three coils are closely attached to a test piece 1, and for array inclined holes with different inclination angles, the inclination angle of the bent magnetic core is changed to be inserted into the inclined hole, wherein the bent magnetic core is located inside the pancake coil Along the axis direction of the bending coil, the inner part of the inclined hole is along the axial direction of the inclined hole. By inserting the bent magnetic cores of the excitation coil and the detection coil into the inclined hole of the array air film, the magnetic field is effectively introduced into the inner wall of the inclined hole, thereby improving the signal-to-noise ratio of the detection signal and realizing the precise positioning of the relative position of the probe and the inclined hole structure. Taking advantage of the fact that cracks around the hole are mostly scattered along the radius, the arrangement of the excitation coil of the probe makes the direction of the eddy current completely perpendicular to the direction of the crack around the hole, the crack defect has the greatest disturbance to the eddy current field, and the resulting detection signal has the greatest signal-to-noise ratio, thereby realizing effective detection of tiny cracks along the radial direction of the inclined hole.
[0007] The inner diameters of the excitation coil 2, the first detection coil 3 and the second detection coil 4 are equal to or greater than the outer diameters of the corresponding bent magnetic cores. The vertical section of the bent magnetic core is inserted into the corresponding coils and fixed. The vertical section of the bent magnetic core is consistent with the height of the corresponding coil, and the length of the bent section of the bent magnetic core is less than or equal to the length along the inclined direction of the inclined hole, so as to avoid excessive constraint of the bent magnetic core on the magnetic field, which may lead to the magnetic field being derived from the test piece.
[0008] The probe can meet the detection requirements for inclined holes with different inclination angles and test pieces with different thicknesses by changing the number of coil turns, core length and inclination angle.
[0009] The exciting coil 2, the first detecting coil 3 and the second detecting coil 4 are pancake-shaped coils.
[0010] The detection method of the eddy current detection probe for the inner surface cracks of the inclined hole of the gas turbine blade air film is a differential signal detection method. After the probe is arranged, an excitation signal is first introduced into the excitation coil 2. The excitation signal is a sinusoidal AC voltage signal. The current generated by the alternating voltage signal will generate an alternating magnetic field around the excitation coil, which is recorded as the first magnetic field. Its frequency is related to the frequency of the sinusoidal AC voltage signal. Since the excitation coil 2 contains a central excitation coil bent magnetic core 6 made of ferromagnetic material and has soft magnetic properties, it can introduce more magnetic lines of force into the test piece 1, thereby increasing the magnetic induction intensity of the test piece and generating an eddy current field. The density will also be greater, greatly improving the signal-to-noise ratio of the detection; the eddy current field generated by the alternating first magnetic field on the surface of the test piece will induce another magnetic field, recorded as the second magnetic field, and the second magnetic field has a direct effect on the detection signals of the first detection coil 3 and the second detection coil 4; when there are cracks on the inner surface of the inclined hole of the gas turbine blade air film, it will affect the eddy current field generated by the first magnetic field, and then change the second magnetic field, resulting in the voltage signals detected by the first detection coil 3 and the second detection coil 4 being different in size when there is a defect or not. The voltage detection signal of the first detection coil 3 is recorded as V1, and the voltage detection signal of the second detection coil 4 is recorded as V2, V 1 and V2 are complex numbers, and the difference between the two is recorded as ΔV, that is, ΔV=|V1-V2|. In the absence of defects, the excitation coil 2 will generate an induced eddy current field around the inclined hole structure under the excitation. At this time, the voltage detection signals of the first detection coil 3 and the second detection coil 4 are exactly the same, that is, V1=V2. When there is a crack defect on the inner surface of the inclined hole of the gas turbine blade air film, the induced eddy current field will be disturbed, making V1≠V2, that is, ΔV≠0. By calculating the voltage signal difference, it can be judged whether there is a crack defect on the inner surface of the inclined hole of the gas turbine blade air film; in the actual service process of the probe, when the gas turbine blade When there is no defect on the inner surface of the inclined air film hole, the values of V1 and V2 may not be completely equal due to slight differences in the structure. Therefore, a crack-free standard gas turbine blade inclined air film hole is taken for inspection, and the difference ΔV between V1 and V2 is denoted as ΔV0. The relative error Δ=(ΔV / ΔV0)×100% between the inspection results ΔV and ΔV0 of the inclined hole structure to be tested is used as the judgment standard for whether the inclined hole structure has defects. When Δ≤200%, it is judged that the structural integrity is good and there is no crack on the inner surface of the inclined air film hole of the gas turbine blade. When Δ>200%, it is judged that the structural integrity is poor and there are cracks on the inner surface of the inclined air film hole of the gas turbine blade.
[0011] Compared with the prior art, the present invention has the following advantages:
[0012] The probe of the present invention adjusts the inclination angle of the magnetic core to adapt to the angle of the inclined hole. A specially designed curved magnetic core is used, which is arranged along the axial direction of the coil inside the probe coil and along the axial direction of the inclined hole inside the inclined hole. By using the magnetic cores of the excitation coil and the detection coil to penetrate into the inclined hole, the detection magnetic field can be effectively introduced into the inner wall of the inclined hole, thereby enhancing the quality of the detection signal and improving the signal-to-noise ratio. In addition, the design of the probe of the present invention allows for precise relative positioning, reducing the influence of probe layout errors. In particular, considering that cracks usually spread along the radial direction, the configuration of the excitation coil makes the generated eddy current perpendicular to the diffusion direction of the crack, which helps to effectively detect small cracks along the radial direction of the inclined hole. Compared with traditional detection probes, the probe of the present invention is not limited by the inclined hole structure and can detect cracks on the inner surface of the inclined hole of the gas turbine blade air film.
[0013] In order to accurately detect cracks in inclined holes, the probe design of the present invention includes an excitation coil and two detection coils, whose inner diameters are equal to or slightly larger than the outer diameter of the central curved magnetic core inside the probe. When assembling the probe, the vertical part of the central curved magnetic core is inserted into the interior of the excitation coil and the detection coil, and ensures that it is fixed. The curved part of the curved magnetic core is accurately inserted into the inclined hole to be detected to achieve accurate positioning of the inner wall of the inclined hole. When designing the probe, attention should also be paid to the length selection of the central curved magnetic core. The length of the vertical section of the magnetic core should match the height of the pancake coil in the probe, while the length of the curved section should be consistent with or slightly shorter than the depth of the inclined hole along the inclined direction. This is done to avoid excessive constraint of the magnetic core on the magnetic field, prevent excessive concentration of the magnetic field in the inclined hole, thereby affecting the effective distribution of the magnetic field and the accuracy of crack detection. Through this design, the probe can not only adapt to the specific structure of the inclined hole, but also ensure the reasonable distribution of the magnetic field during crack detection, improve the signal-to-noise ratio of detection, and achieve high efficiency and high precision detection of tiny cracks.
[0014] The probe excitation coil and the detection coils on both sides are closely attached to the test piece during detection. Different coils for excitation and detection can effectively eliminate the influence of uneven probe lifting. At the same time, close to the test piece can make the induced eddy current field stronger, greatly improving the ability of the probe to detect defects. Taking advantage of the fact that cracks around the hole are mostly scattered along the radius, the arrangement of the probe excitation coil makes the direction of the eddy current completely perpendicular to the direction of the crack around the hole. At this time, the crack defect has the greatest disturbance to the eddy current field, and the signal-to-noise ratio of the resulting detection signal is the largest.
[0015] Traditional eddy current detection probes are limited by the influence of eddy current detection skin depth and are still unable to effectively detect cracks on the inner surface of the oblique holes of the air film of gas turbine blades. In response to this problem, the present invention proposes a new probe configuration to solve such problems, which can achieve effective detection of cracks on the inner surface of the oblique holes of the air film of gas turbine blades. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 The present invention is a schematic diagram of an eddy current detection probe for cracks on the inner surface of an inclined air film hole of a gas turbine blade.
[0017] Figure 2 It is a schematic diagram of the structure of the excitation coil and the bent magnetic core therein of the present invention.
[0018] Figure 3 It is a schematic diagram of the structure of the first detection coil and the second detection coil and their respective centrally placed bent magnetic cores of the present invention.
[0019] Figure 4 Schematic diagram of the inclined hole structure (including cracks) to be tested.
[0020] Figure 5 It is a schematic diagram of the relative position of the probe of the present invention and the inclined hole structure to be measured (including cracks) during service. Specific implementation methods
[0022] The present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0023] like Figure 1 As shown, the present invention is an eddy current detection probe for cracks on the inner surface of the inclined hole of the air film of a gas turbine blade. The probe includes an excitation unit composed of an excitation coil 2 and a bent magnetic core 6 of the excitation coil disposed therein, a first detection coil 3 and a first detection coil bent magnetic core 7 disposed therein, and a second detection coil 4 and a second detection coil bent magnetic core 8 disposed therein to constitute a detection unit.
[0024] like Figure 2 and Figure 3 As shown, the inner diameter of the excitation coil 2 used by the probe and the first detection coil 3 and the second detection coil 4 on both sides are equal to or slightly larger than the outer diameter of the corresponding bent magnetic core. The vertical section of the bent magnetic core is inserted into the corresponding coil and fixed; the bent part of the bent magnetic core is inserted into the inclined hole of the test piece to achieve precise positioning. It is worth mentioning that the length of the bent magnetic core should not be too long. The vertical section of the bent magnetic core should be consistent with the coil height of the pancake coil, and the bent section of the bent magnetic core should be consistent with or smaller than the length of the inclined hole along the inclined direction to avoid the bent magnetic core from constraining the magnetic field too strongly, resulting in the magnetic field being derived from the test piece.
[0025] like Figure 4 As shown, the characteristic of the crack of the inclined hole structure in the air film hole mostly appears in the center connection direction of the hole. The coil arrangement of the probe of the present invention generates an induced eddy current field which can be guaranteed to be perpendicular to the crack direction at all times. At this time, the crack defect has the greatest disturbance to the eddy current field, and the detection signal is the most obvious.
[0026] like Figure 5The figure shows the relative position of the probe of the present invention and the inclined hole structure to be tested (including cracks) during service. The excitation coil 2 and the first detection coil 3 and the second detection coil 4 on both sides are close to the test piece 1 during detection. The different coils for excitation and detection can effectively eliminate the influence of uneven probe lifting. At the same time, close contact with the test piece 1 can make the induced eddy current field stronger, greatly improving the ability of the probe to detect defects. The central curved magnetic core of the excitation-detection unit is respectively inserted into the inclined hole, which can achieve precise positioning and reduce the occurrence of detection errors.
[0027] The working principle of the present invention is as follows: The present invention is to achieve high-sensitivity detection of cracks on the inner surface of the inclined hole of the gas film of the gas turbine blade, and the specific implementation steps are as follows:
[0028] Step 1: Adjust the angle of the central curved magnetic core, insert the vertical section into the probe excitation-detection unit, make the bending angle of the curved section consistent with the inclination angle of the inclined hole, and insert the curved section into the inclined hole to achieve positioning, press the upper part of the probe tightly to minimize the impact of lift-off;
[0029] Step 2: Arrange the excitation-detection unit according to step 1, and pass an alternating excitation current into the excitation coil 2. The alternating excitation current will generate a primary magnetic field in the space. Under the action of the central curved magnetic core, the alternating primary magnetic field will introduce the magnetic field into the inclined hole structure. The inner wall of the inclined hole structure will excite an induced eddy current field, which will generate a secondary magnetic field. The secondary magnetic field will in turn act on the first detection coil 3 and the second detection coil 4 to generate voltage signals, namely V1 and V2. At this time, the size of the induced signal is ΔV=V1-V2.
[0030] Step 3: In the absence of defects, the excitation coil 2 will generate an induced eddy current field around the inclined hole structure under the action of excitation. At this time, the voltage detection signals of the first detection coil 3 and the second detection coil 4 are exactly the same, that is, V1=V2, ΔV=0. When there is a crack defect on the inner surface of the gas turbine blade film inclined hole, the induced eddy current field will be disturbed, so that V1≠V2, that is, ΔV≠0. By calculating the voltage signal difference, it can be determined whether there is a crack defect on the inner surface of the gas turbine blade film inclined hole. When there is no defect, ΔV=0, and when there is a defect, ΔV≠0. At the same time, according to the positive and negative of the voltage signals generated by the first detection coil 3 and the second detection coil 4, namely V1 and V2, the approximate location of the crack can be determined.
[0031] Step 4: During the actual service of the probe, when there is no defect in the inclined hole, the values of V1 and V2 may not be completely equal due to slight differences in the inclined hole structure. Therefore, a standard inclined hole structure without cracks is taken for detection, and the difference ΔV between V1 and V2 is denoted as ΔV0. The relative error Δ between the detection results ΔV and ΔV0 of the inclined hole structure to be tested (Δ=ΔV / ΔV0)×100%) is used as the criterion for judging whether the inclined hole structure has defects. When Δ≤200%, it is judged that the structural integrity is good and there is no crack on the inner surface of the inclined hole of the gas turbine blade air film. When Δ>200%, it is judged that the structural integrity is poor and there is a crack on the inner surface of the inclined hole of the gas turbine blade air film.
[0032] The present invention inserts three coils with a central curved magnetic core into the inclined hole structure of a gas turbine blade air film array at the same inclination angle, passes a sinusoidal AC voltage signal into the excitation coil, generates eddy currents in the test piece, gathers magnetic lines of force through the ferromagnetic properties of the central curved magnetic core, and introduces the magnetic field into the inner wall of the inclined hole, thereby improving the probe's detection capability for fine cracks; a central curved magnetic core is arranged in the detection coil to increase the detection signal and improve the defect detection capability; due to the specific arrangement of the two detection coils, the interference of the inclined hole structure can be effectively eliminated through differential detection signals; compared with traditional probes for gas turbine blade air film hole crack detection, the present invention achieves precise positioning of the probe for the array inclined hole structure, and at the same time, the special probe configuration can eliminate the interference signal generated by the array inclined hole structure, the central curved magnetic core can greatly improve the defect detection signal signal-to-noise ratio, and multiple detection coils can also effectively avoid the interference of lift-off and jitter, thereby achieving high-precision detection of cracks on the inner surface of the gas turbine blade air film array inclined hole.
Claims
1. An eddy current detection probe for cracks on the inner surface of the inclined air film hole of a gas turbine blade, characterized in that: The eddy current detection probe comprises an excitation coil (2) and a bent magnetic core (6) disposed therein, a first detection coil (3) and a bent magnetic core (7) disposed therein, and a second detection coil (4) and a bent magnetic core (8) disposed therein; during detection, the first detection coil (3) and the second detection coil (4) are located on both sides of the excitation coil (2), and the three coils are closely attached to a test piece (1); for array inclined holes with different inclined angles, the inclined angle of the bent magnetic core is changed and inserted into the inclined hole, wherein the bent magnetic core in the inner part of the pancake coil is along the curved direction. The direction of the coil axis is along the axial direction of the inclined hole in the inner part of the inclined hole. By inserting the bent magnetic cores of the excitation coil and the detection coil into the inclined hole of the array air film, the magnetic field is effectively introduced into the inner wall of the inclined hole, thereby improving the signal-to-noise ratio of the detection signal and realizing the precise positioning of the relative position of the probe and the inclined hole structure. Taking advantage of the fact that most cracks around the hole are scattered along the radius, the arrangement of the excitation coil of the probe makes the direction of the eddy current completely perpendicular to the direction of the crack around the hole. The crack defect has the greatest disturbance to the eddy current field, and the signal-to-noise ratio of the detection signal is the largest, thereby realizing effective detection of tiny cracks along the radial direction of the inclined hole.
2. The eddy current detection probe for cracks on the inner surface of the inclined air film hole of a gas turbine blade according to claim 1, characterized in that: The inner diameters of the excitation coil (2), the first detection coil (3) and the second detection coil (4) are equal to or greater than the outer diameters of the corresponding bent magnetic cores, and the vertical sections of the bent magnetic cores are inserted into the corresponding coils and fixed; the vertical sections of the bent magnetic cores are in line with the height of the corresponding coils, and the length of the bent sections of the bent magnetic cores is less than or equal to the length in the inclined direction of the inclined hole, so as to avoid excessive constraint of the bent magnetic core on the magnetic field, resulting in the magnetic field being led out of the test piece.
3. The eddy current detection probe for cracks on the inner surface of the inclined air film hole of a gas turbine blade according to claim 1, characterized in that: The probe can meet the detection requirements for inclined holes with different inclination angles and test pieces with different thicknesses by changing the number of coil turns, core length and inclination angle.
4. The eddy current detection probe for cracks on the inner surface of the inclined air film hole of a gas turbine blade according to claim 1, characterized in that: The excitation coil (2), the first detection coil (3) and the second detection coil (4) are pancake-shaped coils.
5. A detection method for an eddy current detection probe for cracks on the inner surface of an inclined air film hole of a gas turbine blade according to any one of claims 1 to 4, characterized in that: The detection method is a differential signal detection method. After the probe is arranged, an excitation signal is first introduced into the excitation coil (2). The excitation signal is a sinusoidal alternating voltage signal. The current generated by the alternating voltage signal will generate an alternating magnetic field around the excitation coil, which is recorded as the first magnetic field. The frequency of the first magnetic field is related to the frequency of the sinusoidal alternating voltage signal. Since the excitation coil (2) contains a central excitation coil bent magnetic core (6) made of ferromagnetic material and having soft magnetic properties, more magnetic lines of force can be introduced into the test piece (1), thereby increasing the magnetic induction intensity of the test piece and generating a greater eddy current field density, thereby greatly improving the signal-to-noise ratio of the detection. The eddy current field generated by the field on the surface of the test piece will induce another magnetic field, which is recorded as the second magnetic field. The second magnetic field has a direct effect on the detection signals of the first detection coil (3) and the second detection coil (4). When there is a crack on the inner surface of the inclined hole of the gas turbine blade, it will affect the eddy current field generated by the first magnetic field, thereby changing the second magnetic field, resulting in the voltage signals detected by the first detection coil (3) and the second detection coil (4) being different in size when there is a defect or not. The voltage detection signal of the first detection coil (3) is recorded as V1, and the voltage detection signal of the second detection coil (4) is recorded as V2. V1 and V2 are plural numbers. The difference is recorded as ΔV, that is, ΔV = |V1-V2|. In the absence of defects, the excitation coil (2) will generate an induced eddy current field around the inclined hole structure under the excitation. At this time, the voltage detection signals of the first detection coil (3) and the second detection coil (4) are exactly the same, that is, V1 = V2. When there is a crack defect on the inner surface of the gas turbine blade air film inclined hole, the induced eddy current field will be disturbed, so that V1≠V2, that is, ΔV≠0. By calculating the voltage signal difference, it can be determined whether there is a crack defect on the inner surface of the gas turbine blade air film inclined hole. In the actual service process of the probe, when the gas turbine blade air film inclined hole has a crack defect, the induced eddy current field will be disturbed, so that V1≠V2, that is, ΔV≠0. When there are no defects on the inner surface of the hole, the values of V1 and V2 may not be completely equal due to slight differences in the structure. Therefore, a crack-free standard gas turbine blade air film inclined hole is taken for inspection, and the difference ΔV between V1 and V2 is denoted as ΔV0. The relative error Δ=(ΔV / ΔV0)×100% between the inspection results ΔV and ΔV0 of the inclined hole structure to be tested is used as the judgment standard for whether the inclined hole structure has defects. When Δ≤200%, it is judged that the structural integrity is good and there are no cracks on the inner surface of the gas turbine blade air film inclined hole. When Δ>200%, it is judged that the structural integrity is poor and there are cracks on the inner surface of the gas turbine blade air film inclined hole.
Citation Information
Patent Citations
Eddy current detecting sensor with high spatial resolution
CN109682882A
Inclined axial array circumferential eccentric eddy current probe and method for small-diameter tube detection
CN112067690A
Flexible rotating eddy current detection probe and method for high-precision detection of cracks around micro holes
CN116337994A
In-situ eddy current detection sensor for cracks of blade air film hole
CN203688500U
Multi-probe type eddy current examination and eddy current test equipment
JP2000227420A
Cited By
Gas turbine wheel disc blade root groove array eddy current coil arrangement and excitation method and device
CN119901806A