Gallium nitride vertical JFET (Junction Field Effect Transistor) device with channel threshold modulation layer and N-I-P withstand voltage region
By introducing a channel threshold modulation layer and multiple N-I-P withstand voltage zones into the gallium nitride vertical JFET device, the problem that traditional vertical GaN devices cannot obtain high threshold voltage and large forward current at the same time is solved, and higher breakdown resistance is achieved Voltage and operating frequency simultaneously improve device reliability and quality factor.
Patent Information
- Application Number
- CN202411051782.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-08-01
AI Technical Summary
Traditional vertical GaN transistors cannot obtain both high threshold voltage and large forward current, limiting their performance in medium voltage and high power applications.
A gallium nitride vertical JFET device with a channel threshold modulation layer and an N-I-P withstand voltage region is designed. By introducing an N-type ultra-low doped channel threshold modulation layer into the channel region, a plurality of N-I-Ps are formed in the device. Withstand voltage zone to improve the device's breakdown voltage and electron mobility.
The threshold voltage and forward current of the device are significantly improved, the operating frequency is improved, and the on-resistance is reduced through multi-layer doping, which enhances the voltage withstandability and heat dissipation performance of the device.
Smart Images

Figure CN118983345A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of semiconductor technology, and in particular relates to a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region and a preparation method thereof. Background Art
[0002] Today, lateral GaN HEMT devices are developing rapidly and maturing in RF and low-voltage power devices. Enhanced GaN HEMT based on p-GaN cap layer and enhanced GaN HEMT based on cascade structure are gradually being applied. The current commercial GaN HEMT withstand voltage level is usually below 650V, and it has advantages in switching speed in medium and low voltage applications. However, if the withstand voltage level needs to be further improved, vertical GaN will become a new focus, especially homoepitaxial GaN vertical power devices based on GaN bulk material substrates, which will become the future development direction of high voltage and high current.
[0003] Compared with lateral GaN HEMT, vertical GaN devices have the following advantages: (1) For a given chip area, they have higher breakdown voltage and current capability; (2) The electric field peak of vertical GaN devices can be transferred from the surface to the drift region, which can suppress the occurrence of surface breakdown; (3) By using GaN homoepitaxial growth, the thermal mismatch ratio between the substrate and the drift region is reduced, which is beneficial to power dissipation; (4) Since it is less dependent on surface passivation, the dynamic on-resistance is relatively stable; (5) The defect density in the homoepitaxial layer is reduced. These advantages make vertical GaN devices particularly suitable for medium voltage (600-10kV) and high power scenarios.
[0004] So far, several 1.2kV-class vertical GaN transistors have been prepared based on GaN substrates, such as: current aperture vertical electron transistor (CAVFET), junction field effect transistor (JFET), trench MOSFET and fin channel MOSFET. In the conventional structure of junction field effect transistor, since the threshold voltage and forward current are both related to the channel n-type impurity concentration, when the channel n-type impurity concentration is high, the threshold voltage is low and the forward current is large, and when the channel n-type impurity concentration is low, the threshold voltage is high and the forward current is low. In other words, the traditional vertical GaN transistor cannot obtain high threshold voltage and large forward current at the same time. Summary of the invention
[0005] In order to solve the above problems existing in the prior art, the present invention provides a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region and a preparation method thereof. The technical problem to be solved by the present invention is achieved by the following technical solutions:
[0006] In a first aspect, the present invention provides a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region, comprising:
[0007] N++GaN substrate;
[0008] An N-GaN drift region located on a surface of one side of the N++GaN substrate;
[0009] A first I-type insulating region, a second I-type insulating region and an N GaN drift region located on a surface of the N-GaN drift region away from the N++GaN substrate, wherein the first I-type insulating region and the second I-type insulating region are located on both sides of the N-GaN drift region respectively;
[0010] A first heavily doped P-type region, a channel region, and a second heavily doped P-type region are respectively located on the first I-type insulating region, the N GaN drift region, and the second I-type insulating region on a side away from the N++GaN substrate; the channel region includes an N-type ultra-low-doped channel threshold modulation layer, and the channel threshold is in contact with the NGaN;
[0011] A first gate, a source, and a second gate respectively located on the first heavily doped P-type region, the channel region, and the second heavily doped P-type region on a side away from the N++GaN substrate;
[0012] a passivation layer located between the first gate and the source and between the second gate and the source;
[0013] A drain electrode is located on the surface of the N++GaN substrate away from the N-GaN drift region.
[0014] In one embodiment of the present invention, the doping concentration of the channel region gradually increases from bottom to top.
[0015] In one embodiment of the present invention, the channel region further includes an N GaN channel layer and an N++GaN channel layer, wherein the N++GaN channel layer is located on a side of the channel threshold modulation layer away from the N++GaN substrate, and the N GaN channel layer is located between the channel threshold modulation layer and the N++GaN channel layer.
[0016] In one embodiment of the present invention, the doping concentration of the channel threshold modulation layer is 0.5×10 15 ~1×10 17 cm -3 .
[0017] In one embodiment of the present invention, the doping concentration of the N GaN channel layer is 5×10 16 ~7×10 18 cm -3 .
[0018] In one embodiment of the present invention, the doping concentration of the N++GaN channel layer is 1×10 18 ~5×10 19 cm -3 .
[0019] In one embodiment of the present invention, the doping concentration of the first heavily doped P-type region and the second heavily doped P-type region is 3×10 17 ~5×10 19 cm -3 .
[0020] In one embodiment of the present invention, the doping concentration of the N-GaN drift region is 1×10 15 ~5×10 18 cm -3 .
[0021] In a second aspect, the present invention provides a method for preparing a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region, comprising:
[0022] Providing an N++GaN substrate;
[0023] Depositing an N-GaN drift layer and an N GaN drift region in sequence on one side surface of the N++GaN substrate;
[0024] After etching the first preset regions at both ends of the N GaN drift region, a first I-type insulating region and a second I-type insulating region are grown in the first preset regions at both ends respectively;
[0025] A channel region is grown on the surfaces of the first I-type insulating region, the N GaN drift region and the second I-type insulating region, wherein the doping concentration of the channel region gradually increases from bottom to top;
[0026] After growing an AlN cover layer on the surface of the channel region, etching away the AlN cover layer in the second preset region at both ends of the channel region, and injecting Mg ions to form a first heavily doped P-type region and a second heavily doped P-type region;
[0027] Thinning the N++GaN substrate and forming a drain electrode on the surface thereof away from the N-GaN drift layer;
[0028] A source electrode is fabricated on a surface of the channel region on a side away from the N++GaN substrate, and a first gate and a second gate are fabricated on surfaces of the first heavily doped P-type region and the second heavily doped P-type region on a side away from the N++GaN substrate, respectively;
[0029] After a passivation layer is deposited on the surfaces of the first heavily doped P-type region, the second heavily doped P-type region, the first gate, the second gate and the source, holes are opened in the passivation layer on the surfaces of the source, the first gate and the second gate to lead out electrodes.
[0030] In one embodiment of the present invention, the step of growing a channel region on the surfaces of the first I-type insulating region, the N GaN drift region and the second I-type insulating region comprises:
[0031] A metal organic chemical vapor deposition (MOCVD) process is used to sequentially grow an N-type ultra-low doped channel threshold modulation layer, an N GaN channel layer and an N++GaN channel layer on the surfaces of the first I-type insulating region, the N GaN drift region and the second I-type insulating region.
[0032] Compared with the prior art, the present invention has the following beneficial effects:
[0033] (1) The present invention provides a gallium nitride vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region and a preparation method thereof. In the vertical JFET device, the first heavily doped P-type region, the first I-type insulating region, the N-GaN drift region and the N++GaN substrate constitute the first NIP withstand voltage region, and the second heavily doped P-type region, the second I-type insulating region, the N-GaN drift region and the N++GaN substrate constitute the second NIP withstand voltage region, so that the device's withstand breakdown voltage can be improved, and the electric field area of the high-value electric field in the drift region of the device becomes larger, thereby reducing the electric field strength in the contact area between the P-type region and the N-type drift region. In addition, the present invention introduces a channel threshold modulation layer in the channel region, and its N-type ultra-low doping method can not only significantly improve the threshold voltage of the device, but also improve the electron mobility, thereby improving the operating frequency of the JFET device. At the same time, the forward current can be increased by increasing the doping concentration of the upper part of the channel threshold modulation layer.
[0034] (2) The present invention adds a first type I insulating layer and a second type I insulating layer with high thermal conductivity to the pn junction, which is beneficial to improving the heat dissipation capacity of the JFET device, reducing the junction temperature, and preventing the JFET device from being damaged due to excessively high junction temperature, thereby significantly improving reliability.
[0035] (3) The present invention adopts a multi-layer doping method in the channel region, which can reduce the on-resistance and improve the quality factor of the JFET device.
[0036] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1It is a structural schematic diagram of a gallium nitride vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region provided by an embodiment of the present invention;
[0038] Figure 2 It is a schematic flow chart of a method for preparing a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region provided by an embodiment of the present invention;
[0039] Figures 3a to 3j It is a schematic diagram of a process for preparing a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region provided by an embodiment of the present invention;
[0040] Figure 4a It is the transfer curve diagram of conventional device and GaN vertical JFET device with channel threshold modulation layer and NIP withstand voltage region;
[0041] Figure 4b It is the transfer curve diagram of the conventional device and the GaN vertical JFET device with the channel threshold modulation layer and the NIP withstand voltage region in the semi-logarithmic coordinates;
[0042] Figure 5a It is a schematic diagram of the electric field distribution of a conventional device;
[0043] Figure 5b It is a schematic diagram of the electric field distribution of a GaN vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region;
[0044] Figure 6 This is a comparison chart of the breakdown voltage of a conventional device and a gallium nitride vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region. DETAILED DESCRIPTION
[0045] The present invention is further described in detail below with reference to specific embodiments, but the embodiments of the present invention are not limited thereto.
[0046] Figure 1 1 is a schematic diagram of a structure of a gallium nitride vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region provided by an embodiment of the present invention. Figure 1 As shown, an embodiment of the present invention provides a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region, characterized in that it includes:
[0047] N++GaN substrate;
[0048] An N-GaN drift region located on one surface of an N++GaN substrate;
[0049] A first I-type insulating region, a second I-type insulating region and an NGaN drift region located on a surface of the N-GaN drift region away from the N++GaN substrate, wherein the first I-type insulating region and the second I-type insulating region are located on both sides of the N-GaN drift region respectively;
[0050] The first heavily doped P-type region, the channel region and the second heavily doped P-type region are respectively located on the first I-type insulating region, the N GaN drift region, the second I-type insulating region and the surface of the side away from the N++GaN substrate; the channel region includes an N-type ultra-low doped channel threshold modulation layer, and the channel threshold is in contact with the N GaN;
[0051] A first gate, a source, and a second gate, respectively located on the first heavily doped P-type region, the channel region, and the second heavily doped P-type region on a surface away from a side of the N++GaN substrate;
[0052] a passivation layer between the first gate and the source and between the second gate and the source;
[0053] The drain is located on the surface of the N++GaN substrate away from the N-GaN drift region.
[0054] Specifically, the gallium nitride JFET device in this embodiment includes: an N++GaN substrate, an N-GaN drift region located on the surface of the N++GaN substrate, a first I-type insulating region located on the surface of the N-GaN drift region, a second I-type insulating region and an N GaN drift region, a first heavily doped P-type region located on the surface of the first I-type insulating region, a channel region located on the surface of the N GaN drift region, and a second heavily doped P-type region located on the surface of the second I-type insulating region, wherein the N GaN drift region is located between the first I-type insulating region and the second I-type insulating region, so that two NIP withstand voltage regions can be formed in the device, namely: a first NIP withstand voltage region composed of the first heavily doped P-type region, the first I-type insulating region, the N-GaN drift region and the N++GaN substrate, and a second NIP withstand voltage region composed of the second heavily doped P-type region, the second I-type insulating region, the N-GaN drift region and the N++GaN substrate. The two NIP withstand voltage regions in this embodiment are beneficial to improving the breakdown voltage of the device. The electric field area of the high-value electric field in the drift region of the device becomes larger, thereby reducing the electric field strength in the contact area between the P-type region and the N-type drift region.
[0055] Optionally, the doping concentration of the N-GaN drift region is 1×10 15 ~5×10 18 cm -3 The doping concentration of the first heavily doped P-type region and the second heavily doped P-type region is 3×10 17 ~5×10 19 cm -3 .
[0056] Furthermore, the channel region of the gallium nitride vertical JFET device includes an N-type ultra-low doping (N--) channel threshold modulation layer, which is located on the surface of the N GaN drift region away from the N++GaN substrate, that is, Figure 1 From the perspective of the channel threshold modulation layer, the channel threshold modulation layer is located on the upper surface of the N GaN drift region.
[0057] It should be understood that for GaN vertical JFET devices, when the gate is zero volts, because the electrons in the N-type region in the channel are one order of magnitude lower than the holes in the P-type region, the electrons in the N-type region will be depleted by the holes in the P-type region, resulting in a space charge region, and the space charge region of the N-type region is large. The two P-type regions will deplete the entire N-type region channel, preventing the drain current from flowing to the source. When the gate voltage of the GaN vertical JFET device is greater than the threshold voltage, the space charge region of the N-type region decreases and the drain current flows to the source. Since both the threshold voltage and the forward current are related to the N-type doping concentration of the channel, in conventional JFET devices, when the concentration of N-type impurities is high, the forward current is large but the threshold voltage is low; similarly, when the concentration of N-type impurities is low, the threshold voltage is high but the forward current is small. In this embodiment, by introducing a channel threshold modulation layer in the channel region, its N-type ultra-low doping method can significantly improve the threshold voltage of the device.
[0058] Optionally, the doping concentration of the channel region gradually increases from bottom to top, and the forward current is increased by increasing the doping concentration of the upper part of the channel threshold modulation layer. The electric field is concentrated in the insulating region through the withstand voltage of the first I-type insulating region and the second I-type insulating region. After the high electric field region is changed, the electric field strength of the contact region between the P-type region and the N-type drift region can be reduced, thereby obtaining a GaN vertical JFET that simultaneously meets high threshold voltage, large forward current and high withstand voltage. Exemplarily, the channel region also includes an N GaN channel layer and an N++GaN channel layer, wherein the N++GaN channel layer is located on the side of the channel threshold modulation layer away from the N++GaN substrate, and the NGaN channel layer is located between the channel threshold modulation layer and the N++GaN channel layer, and the doping concentration of the channel threshold modulation layer is 0.5×10 15 ~1×10 17 cm -3 , the doping concentration of the N GaN channel layer is 5×10 16 ~7×10 18 cm -3 , the doping concentration of the N++GaN channel layer is 1×10 18 ~5×10 19 cm -3 .
[0059] Figure 2The present invention provides a flow chart of a method for preparing a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region. Figures 3a to 3j Schematic diagram of the process of preparing a GaN vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region provided by an embodiment of the present invention. Figure 2 , 3a ~3j, the embodiment of the present invention further provides a method for preparing a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region, comprising:
[0060] S1. providing an N++GaN substrate;
[0061] S2, depositing an N-GaN drift layer and an N GaN drift region in sequence on one side surface of the N++GaN substrate;
[0062] S3, after etching the first preset regions at both ends of the N GaN drift region, respectively growing a first I-type insulating region and a second I-type insulating region in the first preset regions at both ends;
[0063] S4, growing a channel region on the surface of the first I-type insulating region, the N GaN drift region and the second I-type insulating region, wherein the doping concentration of the channel region gradually increases from bottom to top;
[0064] S5, after growing an AlN cover layer on the surface of the channel region, etching away the AlN cover layer in the second preset region at both ends of the channel region, and injecting Mg ions to form a first heavily doped P-type region and a second heavily doped P-type region;
[0065] S6, thinning the N++GaN substrate, and forming a drain on the surface thereof away from the N-GaN drift layer;
[0066] S7, fabricating a source electrode on a surface of a side of the channel region away from the N++GaN substrate, and fabricating a first gate and a second gate on a surface of a side of the first heavily doped P-type region and a second heavily doped P-type region away from the N++GaN substrate, respectively;
[0067] S8. After a passivation layer is deposited on the surfaces of the first heavily doped P-type region, the second heavily doped P-type region, the first gate, the second gate and the source, holes are opened in the passivation layer on the surfaces of the source, the first gate and the second gate to lead out electrodes.
[0068] Specifically, see Figure 3a-3bIn steps S1 to S2, the N++GaN substrate is first ultrasonically cleaned to eliminate dangling bonds on the surface, then blow-dried and heat-treated, and then a metal organic chemical vapor deposition (MOCVD) process is used to deposit and grow an N-GaN drift layer with a thickness of 1μm to 3μm and an N GaN drift region with a thickness of 5μm to 7μm on the surface of the N++GaN substrate to obtain an epitaxial wafer. The obtained epitaxial wafer is ultrasonically cleaned in acetone for 2 minutes to remove the residual organic matter on the surface, and then ultrasonically cleaned in ethanol for 3 minutes, and then the residual acetone and ethanol are washed away with deionized water, and then dried with N2.
[0069] In step S3, Figure 3c~3d As shown, after the glue is applied, the first preset areas at both ends of the N GaN drift region are etched, and AlN is grown in the first preset areas at both ends using the MOCVD process to form a first I-type insulating region and a second I-type insulating region on both sides of the N GaN drift region.
[0070] For further information, see Figure 3e In step S4, a channel region with a thickness of 1 μm to 3 μm is grown on the surface of the N GaN drift region, the first I-type insulating region and the second I-type insulating region by using an MOCVD process, including:
[0071] By adopting the metal organic chemical vapor deposition (MOCVD) process, an N-type ultra-low doped channel threshold modulation layer, an NGaN channel layer and an N++GaN channel layer are sequentially grown on the surfaces of the first I-type insulating region, the N GaN drift region and the second I-type insulating region.
[0072] In fact, the materials of the first type I insulating region and the second type I insulating region may also include silicon nitride, silicon oxide, etc., which is not limited in the present application.
[0073] In step S5, a substrate such as Figure 3f After the AlN cover layer is removed by etching, Mg ions are implanted into the second preset areas at both ends of the channel region (i.e., the areas on both sides not covered by the AlN cover layer), and the concentration may be 1×10 20 ~5×10 21 cm -3 , and then annealed at high temperature and high pressure to form Figure 3g The first heavily doped P-type region and the second heavily doped P-type region are shown.
[0074] Please continue to see Figure 3h~3jIn steps S6 to S7, the N++GaN substrate is first thinned, and then Ti / Al / Ni / Au metal is deposited on the surface of the N++GaN substrate away from the N-GaN drift layer by electron beam evaporation, and then high-temperature annealing is performed in a rapid annealing furnace to form a good ohmic contact with the substrate to form a drain. Similarly, Ti / Al / Ni / Au metal is deposited on the surface of the channel region away from the N++GaN substrate by electron beam evaporation, and Ni / Au metal is deposited on the surface of the first heavily doped P-type region and the second heavily doped P-type region away from the N++GaN substrate. After high-temperature annealing, the source, the first gate, and the second gate are formed.
[0075] Finally, a plasma chemical vapor deposition (PECVD) process is used to deposit SiNX or SiO2 with a thickness of about 50 nm on the source, the first gate, the second gate, the first heavily doped P-type region, and the second heavily doped P-type region to form a passivation layer, wherein the nitrogen (N) source is provided by ammonia (NH3) and the silicon (Si) source is provided by silane (SiH4), thereby avoiding direct contact between the first gate, the second gate and the source. A hole is opened in the passivation layer above the source, the first gate, and the second gate to lead out the electrode, and the Figure 1 A GaN vertical JFET transistor with a channel threshold modulation layer and a NIP region is shown.
[0076] Figure 4a The transfer curves of conventional devices and GaN vertical JFET devices with channel threshold modulation layer and NIP withstand voltage region are shown in Figure 2. Figure 4b It is a transfer curve diagram of a conventional device and a gallium nitride vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region in semi-logarithmic coordinates. It should be noted that the conventional JFET device includes, from bottom to top, a drain, a substrate located on the surface of the drain, an N-GaN drift region located on the surface of the substrate, a channel region located on the surface of the N-GaN drift region, and a first P+GaN region and a second P+GaN region located on both sides of the channel, a first gate and a second gate located on the surfaces of the first and second P+GaN regions, respectively, and a source located on the surface of the channel region. Figure 4a As shown in Figure 2, when the threshold voltages of the conventional device and the GaN vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region are both 2.8 V, the electron concentration in the channel region of the conventional device is 0.6×10 16 cm -3 , the forward current is smaller than that of the GaN vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region. Figure 4b As shown in Figure 2, when the forward current of the conventional device and the GaN vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region are both 0.6A, the electron concentration in the channel region of the conventional device is 2.5×10 16cm -3 , the threshold voltage is lower than that of the device with a channel threshold modulation layer.
[0077] Figure 5a is a schematic diagram of the electric field distribution of a conventional device. Figure 5b This is a schematic diagram of the electric field distribution of a GaN vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region. Figure 5a-5b , when the voltage is 1800V, the I-type insulation region makes the electric field distribution in the drift region of the device more uniform, reducing the electric field strength in the contact area between the P-type region and the N-type drift region.
[0078] Figure 6 This is a comparison chart of the breakdown voltage of a conventional device and a GaN vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region. Figure 6 As shown, the breakdown voltage of conventional devices is about 1200V, while the breakdown voltage of the gallium nitride vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region is about 1800V, and the withstand breakdown voltage has been significantly improved.
[0079] It can be seen from the above embodiments that the beneficial effects of the present invention are:
[0080] (1) The present invention provides a gallium nitride vertical JFET device with a channel threshold modulation layer and a NIP withstand voltage region and a preparation method thereof. In the vertical JFET device, the first heavily doped P-type region, the first I-type insulating region, the N-GaN drift region and the N++GaN substrate constitute the first NIP withstand voltage region, and the second heavily doped P-type region, the second I-type insulating region, the N-GaN drift region and the N++GaN substrate constitute the second NIP withstand voltage region, so that the device's withstand breakdown voltage can be improved, and the electric field area of the high-value electric field in the drift region of the device becomes larger, thereby reducing the electric field strength in the contact area between the P-type region and the N-type drift region. In addition, the present invention introduces a channel threshold modulation layer in the channel region, and its N-type ultra-low doping method can not only significantly improve the threshold voltage of the device, but also improve the electron mobility, thereby improving the operating frequency of the JFET device. At the same time, the forward current can be increased by increasing the doping concentration of the upper part of the channel threshold modulation layer.
[0081] (2) The present invention adds a first type I insulating layer and a second type I insulating layer with high thermal conductivity to the pn junction, which is beneficial to improving the heat dissipation capacity of the JFET device, reducing the junction temperature, and preventing the JFET device from being damaged due to excessively high junction temperature, thereby significantly improving reliability.
[0082] (3) The present invention adopts a multi-layer doping method in the channel region, which can reduce the on-resistance and improve the quality factor of the JFET device.
[0083] In the description of this specification, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0084] The description with reference to the terms "one embodiment", "some embodiments", "examples", "specific examples", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine different embodiments or examples described in this specification.
[0085] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.
Claims
1. A gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region, It is characterized in that include: N++GaN substrate; An N-GaN drift region located on a surface of one side of the N++GaN substrate; A first I-type insulating region, a second I-type insulating region and an NGaN drift region located on a surface of the N-GaN drift region away from the N++GaN substrate, wherein the first I-type insulating region and the second I-type insulating region are respectively located on two sides of the N-GaN drift region; A first heavily doped P-type region, a channel region, and a second heavily doped P-type region are respectively located on the first I-type insulating region, the N GaN drift region, and the second I-type insulating region on a side away from the N++GaN substrate; the channel region includes an N-type ultra-low-doped channel threshold modulation layer, and the channel threshold is in contact with the NGaN; A first gate, a source, and a second gate respectively located on the first heavily doped P-type region, the channel region, and the second heavily doped P-type region on a side away from the N++GaN substrate; a passivation layer located between the first gate and the source and between the second gate and the source; A drain electrode is located on the surface of the N++GaN substrate away from the N-GaN drift region.
2. The gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region according to claim 1, It is characterized in that The doping concentration of the channel region increases gradually from bottom to top.
3. The gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region according to claim 2, It is characterized in that The channel region further includes an N GaN channel layer and an N++GaN channel layer, wherein the N++GaN channel layer is located on a side of the channel threshold modulation layer away from the N++GaN substrate, and the N GaN channel layer is located between the channel threshold modulation layer and the N++GaN channel layer.
4. The gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region according to claim 3, It is characterized in that The doping concentration of the channel threshold modulation layer is 0.5×10 15 ~1×10 17 cm -3 .
5. The gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region according to claim 3, It is characterized in that The doping concentration of the N GaN channel layer is 5×10 16 ~7×10 18 cm -3 .
6. The gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region according to claim 3, It is characterized in that The doping concentration of the N++GaN channel layer is 1×10 18 ~5×10 19 cm -3 .
7. The gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region according to claim 1, It is characterized in that The doping concentration of the first heavily doped P-type region and the second heavily doped P-type region is 3×10 17 ~5×10 19 cm -3 .
8. The gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region according to claim 1, It is characterized in that The doping concentration of the N-GaN drift region is 1×10 15 ~5×10 18 cm -3 .
9. A method for preparing a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region, It is characterized in that include: Providing an N++GaN substrate; Depositing an N-GaN drift layer and an N GaN drift region in sequence on one side surface of the N++GaN substrate; After etching the first preset regions at both ends of the N GaN drift region, a first I-type insulating region and a second I-type insulating region are grown in the first preset regions at both ends respectively; A channel region is grown on the surfaces of the first I-type insulating region, the N GaN drift region and the second I-type insulating region, wherein the doping concentration of the channel region gradually increases from bottom to top; After growing an AlN cover layer on the surface of the channel region, etching away the AlN cover layer in the second preset region at both ends of the channel region, and injecting Mg ions to form a first heavily doped P-type region and a second heavily doped P-type region; Thinning the N++GaN substrate and forming a drain electrode on the surface thereof away from the N-GaN drift layer; A source electrode is fabricated on a surface of the channel region on a side away from the N++GaN substrate, and a first gate and a second gate are fabricated on surfaces of the first heavily doped P-type region and the second heavily doped P-type region on a side away from the N++GaN substrate, respectively; After a passivation layer is deposited on the surfaces of the first heavily doped P-type region, the second heavily doped P-type region, the first gate, the second gate and the source, holes are opened in the passivation layer on the surfaces of the source, the first gate and the second gate to lead out electrodes.
10. The method for preparing a gallium nitride vertical JFET device having a channel threshold modulation layer and a NIP withstand voltage region according to claim 9, It is characterized in that The step of growing a channel region on the surfaces of the first I-type insulating region, the N GaN drift region and the second I-type insulating region comprises: A metal organic chemical vapor deposition (MOCVD) process is used to sequentially grow an N-type ultra-low doped channel threshold modulation layer, an N GaN channel layer and an N++GaN channel layer on the surfaces of the first I-type insulating region, the N GaN drift region and the second I-type insulating region.
Citation Information
Patent Citations
High-frequency low-consumption power junction type field effect transistor
CN1812132A
Vertical jfet (Junction field-effect transistor) and method of manufacturing the same
JP2003209123A
Cited By
Power MOS device and preparation method thereof
CN120091598A
A power mos device and a method of manufacturing the same
CN120091598B
Power MOS device and preparation method thereof
CN120091599A
A power MOS device and its fabrication method
CN120091599B
JFET device and manufacturing method thereof
CN121194499A