Single-color, multi-color or color-changing light-storing type light-emitting plant and preparation method thereof
By coating long-afterglow materials and injecting them into plant leaves, the problems of uneven light emission, short afterglow time, and high cost in existing technologies have been solved, enabling the preparation of multi-color luminescent plants and their application in low-brightness landscape lighting.
Patent Information
- Application Number
- CN202411075973.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-11-22
AI Technical Summary
Existing technologies make it difficult to prepare light-storing plants with uniform light emission, long afterglow time, and multiple colors of light emission. Furthermore, long afterglow materials are difficult to exist stably in plants, and the process is complex and costly.
The long-afterglow material was treated with coating technology to improve its biosafety and stability, and large-particle luminescent suspension was injected into plant leaves through a syringe to construct monochromatic, multicolor or color-changing phosphorescent plants.
It achieves uniform light emission and a long afterglow time of up to 2 hours. It can emit light under indoor and outdoor light sources, reducing energy consumption for plants. It is low-cost, easy to operate, and suitable for low-brightness landscape lighting.
Smart Images

Figure CN118985312A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of solid luminescence, functional plants and bioluminescence, and in particular to a single-color, multi-color or color-changing light-storage luminescent plant and a preparation method thereof. Background Art
[0002] Plants play a vital role in the modern urban ecology. With the deepening development of urbanization and the increasing emphasis on land use efficiency, people expect plants to show more functionality. In recent years, people have tried to use living plants to replace traditional plastics and circuit boards to manufacture functional devices, which not only reduces the generation of waste, but also because plants have their own self-repairing ability, these devices are more environmentally friendly and sustainable than traditional products. By giving living plants new optical properties to create functional devices, there are potential applications in plant-based reflective devices, biosensors and living plant light sources. Constructing a light-storing living plant is to give plants the property of afterglow luminescence, which has potential applications in low-brightness energy-saving lighting and landscape lighting.
[0003] At present, there are many methods for constructing light-storing plants using genetic engineering, such as applying bacterial bioluminescent gene clusters, firefly enzyme luciferase or fungal bioluminescent gene clusters. However, the luminescence brightness of the plants obtained by this method is very low, and the luminescence color is single. It is difficult to prepare plants that can emit multiple colors of light or even color-changing luminescence. In addition, the luminescence process consumes the energy of the plant itself, reducing the efficiency of the plant photosynthesis to synthesize organic matter. In addition, the substances such as luciferin or luciferase required in the above prior art need to be expressed and extracted in vivo, which is complicated to operate and difficult to express and extract in large quantities outside the laboratory. It has extremely high requirements for operators and is costly, so it is difficult to promote it on the market.
[0004] There are a few reports on the construction of light-storing plants using long afterglow materials, but there are the following problems: First, because the stomata of plants are small and the intercellular gaps inside plants are small, it is difficult for long afterglow materials with larger particle sizes to enter plants through the surface of the stomata, and it is also difficult to diffuse after entering, so the luminescent plants obtained do not emit light uniformly; second, the smaller the particle size of the long afterglow material, the worse the afterglow performance, and the afterglow performance of the constructed light-storing plants also decreases significantly. At present, most of the long afterglow materials used to construct light-storing plants are below 1μm, with weak afterglow intensity and short afterglow time (within 1h), which are difficult to capture with the naked eye; third, long afterglow materials cannot exist in plants stably and safely for a long time. Long afterglow materials may be decomposed or transported in plants and cannot exist stably for more than a week; fourth, there are few reports on multi-color and color-changing luminous plants. Fifth, there are few reports on light-storing plants that can be excited by sunlight.
[0005] Based on the above-mentioned deficiencies, a monochrome, multi-color or color-changing light-storing luminous plant and its preparation method are urgently needed in the industry, which can effectively solve the defects of light-storing plants such as the inability to be excited by sunlight during actual low-brightness lighting, uneven plant luminescence, short afterglow time and weak afterglow intensity. Summary of the invention
[0006] In view of the problems existing in the prior art, the present invention provides a light-storing luminous plant and a preparation method thereof, so as to solve the problem that the light-storing plants prepared in the related technology need to consume the energy of the plants themselves, reduce the efficiency of photosynthesis, and are difficult to prepare light-storing plants with long afterglow time, strong luminescence, uniform luminescence, multi-color luminescence, and color-changing luminescence.
[0007] The present invention utilizes the property of long afterglow materials that can absorb and store light energy. They can be stimulated to emit visible light under sunlight, indoor LED light and other light sources, and store part of the obtained light energy. After the stimulation stops, the energy is slowly released in the form of light. However, the smaller the particle size of the long afterglow material, the lower the luminous efficiency. Therefore, a method is needed to transport luminous particles with larger particle sizes safely and evenly in plant leaves.
[0008] To achieve the above object, the present invention adopts the following technical solutions:
[0009] The present invention first provides a method for preparing a single-color, multi-color or color-changing light-storing luminescent plant, comprising the following steps:
[0010] S1. The commercial inorganic long afterglow material of different particle sizes and light colors is coated to obtain a long afterglow material with good water resistance;
[0011] S2. dispersing the long afterglow material in water to obtain a luminescent suspension;
[0012] S3. Inject the luminescent suspension into the plant via a syringe.
[0013] Furthermore, the step S1 further comprises the following steps:
[0014] S11. Determine the luminous color of the required light-storing plant;
[0015] S12. Select a long afterglow material with a micron particle size of suitable luminous color, an inorganic long afterglow material of different light colors, including but not limited to cyan, blue, blue-purple, green or red; wherein cyan can be selected from: Sr4Al 14 O 25 :Eu 2+ Inorganic long afterglow luminescent materials and other inorganic long afterglow materials with emission bands in the cyan range; blue-purple can be selected from: CaAl2O4:Eu 2+ ,Nd3+ Inorganic long afterglow luminescent materials and other inorganic long afterglow materials with emission bands in the blue-violet range; blue can be selected from: Sr2MgSi2O7:Eu 2+ ,Dy 3+ Inorganic long afterglow luminescent materials and other inorganic long afterglow materials with emission bands in the blue light range; green can be selected from: SrAl2O4:Dy 3+ ,Eu 2+ Inorganic long afterglow luminescent materials and other inorganic long afterglow materials with emission bands in the green light range; red can be selected from: Y2O2S:Eu 3+ Mg 2+ ,Ti 4+ Other inorganic long afterglow materials with emission bands in the red range;
[0016] S13. The long afterglow material is ball-milled for 0-96h to obtain long afterglow materials of different particle sizes (1-20 μm);
[0017] S14. The ball-milled long afterglow material is coated, and the coating includes: oxide coating, fluoride coating, phosphate coating, etc., and the coating method includes: sol-gel method, liquid phase deposition method, high temperature solid phase reaction method, etc. Each method can obtain a long afterglow material that can be stably present in water, air, and inside plants without decomposition;
[0018] S15. Test the cytotoxicity of the coated long afterglow material, preliminarily determine its biosafety, and select materials with low or no cytotoxicity for use in plants.
[0019] Furthermore, the step S2 also includes determining the concentration and particle size of the stable long afterglow material, and the specific steps are:
[0020] S21. The safe and stable long afterglow material is screened to obtain long afterglow materials of different particle sizes;
[0021] S22. Dispersing stable long afterglow materials of different masses and different particle sizes (1-20 μm) in water to obtain luminescent suspensions of different particle sizes and different concentrations (1-200 mg / ml);
[0022] S23. Injecting the luminescent suspension into the plant, selecting a particle size and concentration that can be evenly diffused in the plant leaves;
[0023] S24. Injecting the suspension having the particle size and concentration into a plurality of plants (more than 3 plants) to obtain luminous plants;
[0024] S25. Observe the survival of the luminescent plants for more than 7 days, and test physiological indicators such as chlorophyll content and photosynthetic rate. Compare the physiological indicators with those of plants that have not been treated with the luminescent suspension (i.e., the blank group). If the plants can grow and develop normally, and the physiological indicators are similar to those of the blank group under the same cultivation conditions, determine the injected particle size and concentration.
[0025] Furthermore, step S3 includes the following steps:
[0026] S31. Use the needle of a sterile syringe to shallowly pierce the epidermis of the back leaf of the plant to create a channel for the afterglow material to enter the leaf;
[0027] S32. Use a needle-free syringe to draw in a certain amount (0.1-10 ml) of the luminescent suspension, press it on the position of the leaf punctured by the needle, and gently push the liquid into the leaf through the syringe by pressure infiltration.
[0028] The present invention also discloses a single-color, multi-color or color-changing light-storing luminescent plant prepared according to any of the above-mentioned preparation methods. The afterglow time of the luminescent plant observable by the naked eye is up to 2 hours, and uniform, multi-color and color-changing luminescence can be achieved.
[0029] The beneficial effects brought about by the technical solution provided by the present invention include:
[0030] (1) Use long afterglow materials to store light energy. When this material is combined with plants, it gives the plants afterglow characteristics, enabling them to store light energy. Both indoor LED light and outdoor sunlight can be used as the excitation light source. After the excitation light stops, the plant can release the stored energy, and the whole process does not consume the plant's own energy.
[0031] (2) A suspension transport channel is opened on the plant leaves through a needle, and then the suspension of afterglow material is injected into the plant with a needle-free syringe. This allows materials with larger particle sizes (1μm-20μm) to enter the plant and be passively transported to the entire leaf under external pressure, thereby obtaining a uniformly luminous light-storing plant.
[0032] (3) The uniform luminescence of light-storing plants can be observed with the naked eye. Because the luminescent particles entering the plants are large in size, the afterglow of the plants can last up to 2 hours or even longer after the excitation of the light-storing plants stops. The light emitted by the plants can illuminate the text on a book. Multiple luminous plants can illuminate a portrait together, achieving low-brightness landscape lighting. This is energy-saving and beautiful, and can be applied to living plant lighting.
[0033] (4) Currently, there are many different colors of inorganic long afterglow phosphors available commercially. Their biosafety can be improved by coating, and then light-storing plants that emit light of multiple colors can be constructed. Luminescent materials of different colors can also be mixed together and added to plants to construct color-changing luminescent plants. All of the above can be customized according to people's requirements.
[0034] (5) After being coated, the long afterglow material has good stability in water and will not decompose into harmful acidic and alkaline substances that harm plants. It can also maintain its optical properties and can be repeatedly excited to emit light. Therefore, the light-storing plants constructed with it can maintain normal growth and development and long-term afterglow performance.
[0035] (6) The present invention directly transforms plants, has simple technology, and has low requirements on operators. In addition, the preparation of long afterglow materials is simple and low in cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. The drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0037] Figure 1 A flow chart of the preparation of a light-storing plant in an embodiment of the present invention;
[0038] Figure 2 To test the cytotoxicity of the green long afterglow material (PO4-SA) after coating;
[0039] Figure 3 To characterize the water resistance of the green long afterglow material before and after coating, (a) the pH value of the uncoated material (SA) increases sharply after being soaked in water for 20 minutes, becoming alkaline and causing great damage to plants; (b) the pH value of the material after phosphoric acid coating (PO4-SA) remains at around 7 after being soaked in water for 10 days; (c) the fluorescence of the green long afterglow material (SA) before coating changes from green to blue after being soaked for 8 hours, indicating that the substance has been hydrolyzed. After being soaked in water for 10 days, the green long afterglow material (PO4-SA) coated with phosphoric acid still emits green light and its afterglow performance remains unchanged.
[0040] Figure 4 These are the emission spectra and afterglow decay curves of the coated material after immersion in water for 2, 4, 6, 8, and 10 days. The emission peak position, peak shape, luminous intensity, and decay rate remain basically consistent.
[0041] Figure 5(a) is a light-storing plant transformed with green long afterglow materials in the embodiment of the present invention. After being irradiated with a 365nm ultraviolet lamp (6W) for 2 minutes, it can emit green afterglow in a dark environment. The visible luminescence time is up to 2 hours, and the luminescence is relatively uniform; (b) is the luminescence of the plant after 10 days. After 10 days, the afterglow performance remains basically unchanged, and it can still maintain luminescence for 2 hours, and the plant can still survive normally. The above photos were taken with the same equipment and the same parameters.
[0042] Figure 6 The light-storing plant transformed from the green long afterglow material in the embodiment of the present invention can illuminate the words on the book and make them clearly visible;
[0043] Figure 7 A luminous plant wall constructed of multiple light-storing plants transformed from green long-afterglow materials in an embodiment of the present invention can illuminate text and images in a book;
[0044] Figure 8 The light-storing plant transformed with the green long afterglow material in the embodiment of the present invention can emit green afterglow light after being irradiated with (a) 360lx indoor white light LED, (b) 1500lx white light LED, or (c) 10000lx sunlight for 5 minutes, with a light emission time of 60-120 minutes. It can have a longer afterglow light emission time under stronger and longer white light excitation;
[0045] Fig. 9 (a) is a luminescent plant modified by a mixture of cyan, red and green long afterglow materials in the embodiment of the present invention. After being irradiated by a 365nm (6W) ultraviolet lamp for 10s, it emits warm white light in a dark environment, and changes to greenish white light over time; (b) is a luminescent plant modified by a cyan long afterglow material in the embodiment of the present invention. After being irradiated by a 365nm ultraviolet lamp (6W) for 10s, it emits cyan light in a dark environment; (c) is a luminescent plant modified by a red long afterglow material in the embodiment of the present invention. After being irradiated by a 365nm ultraviolet lamp (6W) for 10s, it emits red light in a dark environment; (d) is a luminescent plant modified by a blue long afterglow material in the embodiment of the present invention. After being irradiated by a 365nm ultraviolet lamp (6W) for 10s, it emits blue light in a dark environment; (e) is a luminescent plant modified by a blue-violet long afterglow material in the embodiment of the present invention. After being irradiated by a 365nm ultraviolet lamp (6W) for 10s, it emits blue-violet light in a dark environment.
[0046] In order to more clearly illustrate the purpose, technical solution and advantages of the present invention, the technical solution of the present invention will be described in detail below in conjunction with the drawings in the embodiments. It should be noted that the embodiments only represent some examples of the present invention, not all. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work belong to the scope of protection of the present invention.
[0047] The embodiment of the present invention provides a luminous plant and a preparation method thereof, which can solve the problems in the related art that the prepared light-storage plants have weak light emission, short light emission time, uneven light emission, consume their own energy, reduce the photosynthesis efficiency of the plants, and cannot prepare light-storage plants with multiple colors. Example
[0048] Reference Figure 1 The present invention provides a method for preparing a luminescent suspension, which specifically includes:
[0049] S1. Coating long afterglow materials improves stability in water and plant environments.
[0050] Purchase commercially available long-lasting glow material of the desired light color.
[0051] Some long afterglow materials that cannot exist stably in water will be coated, such as phosphoric acid coating, silica coating, etc.
[0052] In order to obtain samples with average particle sizes of 1, 3, 5, 7, 10, 15, and 20 μm, ball milling was performed for 12-96 h before coating and sieving was performed after coating.
[0053] The cytotoxicity of the coated long afterglow material is tested to preliminarily determine its biosafety, and materials with low or no cytotoxicity are selected for use in plants.
[0054] S2. The long afterglow material is dispersed in water to form suspensions of different concentrations and particle sizes, and the suspension is injected into the plant in step S3, and the concentration of the long afterglow material in the suspension is determined, and the specific steps are:
[0055] S21. Dispersing stable long afterglow materials of different masses and different particle sizes in water to obtain luminescent suspensions of different particle sizes and different concentrations;
[0056] S22. Injecting the luminescent suspension into the plant, selecting a particle size and concentration that can be evenly diffused in the plant leaves; injecting the suspension of the particle size and concentration into a plurality of plants (more than 3 plants) to obtain a luminescent plant;
[0057] S23. Observe the survival of the luminous plants for more than 10 days and test physiological indicators such as chlorophyll content and photosynthetic rate. If the plants can grow and develop normally, determine the injected particle size and concentration.
[0058] S3. Injecting the luminescent suspension into the plant, the step S3 comprises the following steps:
[0059] S31. Use the needle of a sterile syringe to shallowly pierce the epidermis of the plant leaf to create a channel for the afterglow material to enter the leaf;
[0060] S32. Use a needle-free syringe to draw in a certain amount of luminescent suspension, press it on the position of the leaf punctured by the needle, and gently push the liquid through the syringe into the leaf.
[0061] Through the above steps, a light-storing plant with single-color, multi-color, or color-changing light can be constructed. In some examples, when the injected material is strontium aluminate with an average particle size of 7 μm, the light-storing plant can emit afterglow that can be observed by the naked eye for up to 2 hours, and can absorb and store sunlight during the day and release it at night for nighttime landscape lighting.
[0062] Figure 2 In the cytotoxicity test of the green long afterglow material after coating, the survival rate of cells at each concentration was not less than 95%, indicating that the material has good biocompatibility.
[0063] Figure 3 The water resistance of the green afterglow material before and after coating is characterized. (a) After the uncoated material (SA) is soaked in water for 20 minutes, the pH value increases sharply and becomes alkaline, which causes great damage to plants; (b) After the coated material (PO4-SA) is soaked in water for 10 days, the pH value remains at about 7. This shows that the chemical stability of the green afterglow material is improved after coating, so that it can remain stable in water, and the pH of the suspension is neutral. It can be applied to plants with rich water content, and will not cause damage to plants due to excessive alkalinity, and has good biocompatibility; (c) After the green afterglow material (SA) is soaked for 8 hours before coating, the fluorescence changes from green to blue, indicating that the substance has been hydrolyzed. After the green afterglow material (PO4-SA) coated with phosphoric acid is soaked in water for 10 days, the luminescent color is still green, and the afterglow performance remains unchanged, indicating that the coated material has good water resistance.
[0064] Figure 4 The emission spectra and afterglow decay curves of the coated material after immersion in water for 2, 4, 6, 8, and 10 days are shown. The emission peak position, peak shape, luminous intensity, and decay rate are basically consistent. This shows that the coated material has good stability and stable optical properties in water. It can be applied to plants with high water content and maintain stable optical properties.
[0065] Figure 5 (a) is a light-storing plant transformed with green long afterglow materials in the embodiment of the present invention. After being irradiated with a 365nm ultraviolet lamp (6W) for 2 minutes, it can emit green afterglow in a dark environment. The luminescence time visible to the naked eye is up to 2 hours, and the luminescence is relatively uniform; (b) is the luminescence of the plant after 10 days. After 10 days, the afterglow performance remains basically unchanged, and it can still maintain luminescence for 2 hours, and the plant can still survive normally. The above photos were taken with the same equipment and the same parameters. The luminous plant has a long afterglow time visible to the naked eye.
[0066] Figure 6 The light-storing plant modified from the green long afterglow material in the embodiment of the present invention can illuminate the words on the book, indicating that the luminous plant has a higher brightness.
[0067] Figure 7 The luminous plant wall constructed by multiple light-storing plants modified with green long afterglow materials in the embodiment of the present invention can illuminate the text and images on the book, which shows that the method is easy to repeat and the constructed luminous plants have higher brightness.
[0068] Figure 8 The light-storing plant modified from the green long afterglow material in the embodiment of the present invention can emit green afterglow light after being irradiated with (a) 360lx indoor white light LED, (b) 1500lx white light LED, and (c) 10000lx sunlight for 5 minutes, with a luminescence time of 60-120 minutes. It can have a longer afterglow luminescence time under stronger and longer white light excitation. The luminous plant can be excited to emit light by ordinary indoor lights and sunlight, and is a low-carbon, environmentally friendly and sustainable light source with a wider range of application scenarios.
[0069] Fig. 9(a) is a luminescent plant modified by a mixture of cyan, red and green long afterglow materials in the embodiment of the present invention. After being irradiated by a 365nm (6W) ultraviolet lamp for 10s, it emits warm white light in a dark environment, and changes to greenish white light over time; (b) is a luminescent plant modified by a cyan long afterglow material in the embodiment of the present invention. After being irradiated by a 365nm ultraviolet lamp (6W) for 10s, it emits cyan light in a dark environment; (c) is a luminescent plant modified by a red long afterglow material in the embodiment of the present invention. After being irradiated by a 365nm ultraviolet lamp (6W) for 10s, it emits red light in a dark environment; (d) is a luminescent plant modified by a blue long afterglow material in the embodiment of the present invention. After being irradiated by a 365nm ultraviolet lamp (6W) for 10s, it emits blue light in a dark environment; (e) is a luminescent plant modified by a blue-violet long afterglow material in the embodiment of the present invention. After being irradiated by a 365nm ultraviolet lamp (6W) for 10s, it emits blue-violet light in a dark environment; the present invention successfully constructs luminescent plants of various colors and color changes.
[0070] It should be noted that, in the present invention, relational terms such as "first" and "second" are merely used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any actual relationship or order between these entities or operations.
[0071] The foregoing is only a specific embodiment of the present invention, and is intended to enable those skilled in the art to understand or implement the present invention. Various modifications to these embodiments will be apparent to those skilled in the art. The general principles defined herein can be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention should not be limited to these embodiments shown herein, but should conform to the widest range consistent with the principles and novel features applied for herein.
Claims
1. A method for preparing a monochrome, multi-color or color-changing light-storing luminescent plant, comprising the following steps: S1. The inorganic long afterglow materials of different particle sizes and different light colors are coated to obtain a long afterglow material with good water resistance; S2. dispersing the long afterglow material with good water resistance in water to obtain luminescent suspensions of different concentrations; S3. Inject a certain amount of luminescent suspension into the plant to obtain a single-color, multi-color or color-changing light-storing luminescent plant.
2. The preparation method according to claim 1, wherein: The particle sizes of the inorganic long afterglow materials of different particle sizes in step S1 include: 1-20 μm; The inorganic long afterglow materials of different light colors include: cyan, blue, blue-purple, green or red.
3. The preparation method according to claim 2, wherein: The cyan color is selected from: Sr4Al 14 O 25 :Eu 2+ Inorganic long afterglow luminescent materials; The blue-purple color is selected from: CaAl2O4:Eu 2+ ,Nd 3+ Inorganic long afterglow luminescent materials; The blue color is selected from: Sr2MgSi2O7:Eu 2+ ,Dy 3+ Inorganic long afterglow luminescent materials; The green color is selected from: SrAl2O4:Dy 3+ ,Eu 2+ Inorganic long afterglow luminescent materials; The red color is selected from: Y2O2S:Eu 3+ Mg 2+ ,Ti 4+ Inorganic long afterglow materials.
4. The preparation method according to claim 1, wherein: The coating method in step S1 includes: Sol-gel method, liquid phase deposition method, high temperature solid phase reaction method.
5. The preparation method according to claim 4, wherein: The coating comprises: Oxide coating, fluoride coating, phosphate coating.
6. The preparation method according to claim 1, wherein: The concentration of the luminescent suspension in step S2 is 1-200 mg / ml.
7. The preparation method according to claim 1, wherein: The amount of the luminescent suspension injected into the plant in step S3 is 0.1-10 ml.
Citation Information
Patent Citations
Preparation method for green light-excited long afterglow phosphor with warm color
CN102492419A
Molded nanoparticle phosphor for light emitting applications
CN104066814A
Blue-red light long-afterglow luminescent material for promoting plant growth as well as preparation method and application of blue-red light long-afterglow luminescent material
CN116120934A
Luminous plant and preparation method thereof
CN117243015A