Battery
By using the first adhesive paper prepared in a lithium-ion battery to cover the connection position of the protective element and the electrode ear, and applying the second adhesive paper on the side of the housing, the carbon disulfide residue and glue spill caused by the textured paper tape are solved. The problem has improved the safety and protection effect of the battery and met environmental protection requirements.
Patent Information
- Application Number
- CN202411093423.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
AI Technical Summary
The use of American marking tape in existing lithium-ion batteries leads to carbon disulfide residue, which violates environmental protection requirements, and the tape caused by the composite process is prone to overflowing glue in a high humidity environment, affecting the packaging effect and protective performance of the battery.
The first tape, including polyimide or polyethylene terephthalate as the substrate, is prepared by coating process without impregnation, covering the connection position of the protective element and the electrode, avoiding short circuits and improving safety, Meanwhile, the second tape covers the side of the housing to prevent short circuits and dust from entering.
It effectively avoids carbon disulfide residue, solves the problem of glue spills, improves the safety and stability of the battery, ensures the meeting of environmental protection requirements, and improves the protection effect and performance of the battery.
Smart Images

Figure CN119009399A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of batteries, and in particular to a battery. Background Art
[0002] Lithium-ion batteries have the advantages of high energy density and long cycle life. They are not only widely used in portable electronic devices such as mobile phones and laptops, but also in electric vehicles, electric bicycles, energy storage facilities, battery swap stations, smart devices, etc.
[0003] The battery includes a shell and a cell inside the shell. The cell has a tab extending from the shell. The battery is generally provided with a protective element, which is welded to the tab. The welding position of the protective element and the tab usually requires a protective tape to fix the protective element and prevent short circuit. The related technology usually uses masking tape to protect the welding points of the protective element and the tab. However, the masking tape must be made using a composite process, that is, the process needs to go through an impregnation process, resulting in carbon disulfide residue in the produced masking tape, which does not meet environmental protection requirements. Summary of the invention
[0004] In view of this, an embodiment of the present invention is directed to providing a battery to at least to some extent solve the problems of carbon disulfide residue caused by masking tape in the related art.
[0005] The present invention provides a battery, comprising a housing, a battery cell, a protective element and a first adhesive tape;
[0006] The battery cell is located in the shell, the battery cell has a tab, the shell has a sealing portion, and the tab extends from the sealing portion; the protection element is connected to the tab, and the first adhesive tape at least covers the connection position between the protection element and the tab;
[0007] The first adhesive tape comprises a first adhesive layer and a first substrate disposed on one side of the first adhesive layer, wherein the material of the first substrate is selected from at least one of polyimide and polyethylene terephthalate;
[0008] The light transmittance of the first adhesive tape is not greater than 20%.
[0009] Optionally, along the first direction, the total thickness of the first adhesive tape is not greater than 180 μm;
[0010] and / or, along the first direction, the thickness of the first substrate ranges from 45 μm to 70 μm;
[0011] and / or, along the first direction, the thickness of the first adhesive layer ranges from 20 μm to 50 μm;
[0012] And / or, the peeling force of the first adhesive tape is not less than 0.06 kgf / mm.
[0013] Optionally, the material of the first adhesive layer is selected from at least one of acrylate copolymers, polysiloxane resins, and styrene-isoprene block copolymers.
[0014] Optionally, the first glue layer is further doped with a color-adjusting dopant;
[0015] Preferably, the color-adjusting dopant is selected from at least one of titanium dioxide and mica powder.
[0016] Optionally, the dimensional shrinkage of the first adhesive tape along the MD direction is less than 1.5%;
[0017] Preferably, the dimensional shrinkage of the first adhesive tape along the MD direction is less than 0.8%;
[0018] and / or, the dimensional shrinkage of the first adhesive tape along the TD direction is less than 1%;
[0019] Preferably, the dimensional shrinkage rate of the first adhesive tape along the TD direction is less than 0.3%.
[0020] Optionally, the porosity of the first substrate ranges from 1% to 10%;
[0021] and / or, the swelling rate of the first substrate is in the range of 0 to 5%;
[0022] Preferably, the swelling ratio of the first substrate is in the range of 0-1%.
[0023] Optionally, the battery further includes a second adhesive tape, at least a portion of which covers at least one side of the housing along the second direction;
[0024] The second adhesive tape includes a second adhesive layer and a second substrate arranged on one side of the second adhesive layer;
[0025] The material of the second substrate is at least one selected from polyimide and polyethylene terephthalate.
[0026] Optionally, the material of the second adhesive layer is selected from at least one of acrylate copolymers, polysiloxane resins, and styrene-isoprene block copolymers.
[0027] Optionally, the light transmittance of the second adhesive tape is different from the light transmittance of the first adhesive tape;
[0028] Optionally, the light transmittance of the second adhesive tape is not less than 80%.
[0029] Optionally, the total thickness of the second adhesive tape is less than the total thickness of the first adhesive tape;
[0030] and / or, along the second direction, the total thickness of the second adhesive tape is not greater than 45 μm;
[0031] and / or, along the second direction, the thickness of the second substrate ranges from 12 μm to 30 μm;
[0032] and / or, along the second direction, the thickness of the second adhesive layer is in the range of 5 μm to 15 μm;
[0033] And / or, the ratio of the thickness of the second substrate to the thickness of the first substrate is in the range of 1 / 6 to 2 / 3;
[0034] and / or, the ratio of the thickness of the second adhesive layer to the thickness of the first adhesive layer is in a range of 1 / 10 to 3 / 4;
[0035] And / or, the peeling force of the second adhesive tape is in the range of 0.018 kgf / mm to 0.021 kgf / mm.
[0036] Optionally, the battery further comprises a bonding colloid;
[0037] At least a portion of the adhesive colloid covers at least one side of the housing along the second direction.
[0038] Optionally, the material of the adhesive colloid is selected from at least one of polyurethane and polymethyl methacrylate;
[0039] And / or, the bonding colloid is doped with a fluorescent agent;
[0040] Preferably, the material of the fluorescent agent is selected from at least one of a stilbene type fluorescent agent, a coumarin type fluorescent agent, a pyrazoline type fluorescent agent, and a xylylene imine type fluorescent agent;
[0041] And / or, the peeling force of the adhesive colloid ranges from 0.204kgf / mm to 1.22kgf / mm.
[0042] The battery provided by the embodiment of the present invention uses the first adhesive tape to cover at least the connection position between the protection element and the tab, thereby preventing the connection position from contacting with other components on the housing or the battery top cover to a certain extent and causing a short circuit, thereby improving the safety of the battery. At the same time, by setting the first adhesive tape to include a first adhesive layer and a first substrate located on one side of the first adhesive layer, the material of the first substrate is selected from at least one of polyimide and polyethylene terephthalate. Due to the material characteristics of the first substrate, the first adhesive tape can be formed by directly coating the first adhesive layer on one side of the first substrate using a coating process, that is, the process does not require impregnation, so there will be no solvent residue, that is, the occurrence of carbon disulfide residue is avoided, which meets environmental protection requirements.
[0043] Moreover, by setting the transmittance of the first adhesive tape to no more than 20%, after the first adhesive tape is bonded, it is possible to quickly identify through the transmittance whether the application position of the first adhesive tape is correct and whether the first adhesive tape covers the required protection positions such as the connection position between the protective element and the tab, thereby providing greater convenience for the operator and ensuring that the first adhesive tape effectively covers the required protection positions such as the connection position, thereby further ensuring the safety of the battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] Figure 1 It is a schematic side view of the structure of the first adhesive tape according to an embodiment of the present invention;
[0045] Figure 2 It is a schematic diagram of the three-dimensional structure of the first adhesive tape according to an embodiment of the present invention;
[0046] Figure 3 It is a schematic side view of the structure of the second adhesive tape according to an embodiment of the present invention;
[0047] Figure 4 It is a structural schematic diagram of the back side of a battery according to an embodiment of the present invention;
[0048] Figure 5 A schematic diagram of the structure of the front side of a battery according to an embodiment of the present invention;
[0049] Figure 6 The graph is a result of testing the peeling force between the first adhesive tape and the Nitto 5000NS adhesive tape in one embodiment of the present invention.
[0050] Among them, 1, shell; 11, sealing part; 2, pole ear; 3, protection element; 30, connection position; 4, first adhesive tape; 41, first substrate; 42, first adhesive layer; 5, second adhesive tape; 51, second substrate; 52, second adhesive layer. DETAILED DESCRIPTION
[0051] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0052] The battery includes a housing and a cell in the housing, wherein the cell has a tab extending from the housing. The battery is generally provided with a protection element, such as a temperature switch or a circuit breaker, which will be disconnected when the battery temperature is too high to prevent a short circuit, etc., thereby improving the safety of the battery.
[0053] The protection element and the tab are connected by welding. The related technology uses masking tape to protect the welding points of the protection element and the tab to avoid the risk of thermal runaway caused by the welding position contacting with the shell or other parts on the battery top cover.
[0054] Masking tape is made of masking paper as a substrate, and a double-sided adhesive without a substrate is compounded on the masking paper. However, since the manufacturing process of masking tape must use a composite process, that is, it needs to be impregnated during the process, carbon disulfide residue will be left, which does not meet environmental protection requirements. Based on this, the present invention provides a battery, by setting a first adhesive tape, so that the first adhesive tape includes a first adhesive layer and a first substrate located on one side of the first adhesive layer, and the material of the first substrate is selected from at least one of polyimide and polyethylene terephthalate, and at the same time, the light transmittance of the first adhesive tape is not more than 20%, that is, by utilizing the material characteristics of the first substrate, the first adhesive tape can be prepared directly using a coating process without the need for impregnation, so that there will be no carbon disulfide residue.
[0055] The battery provided by the present invention is described in detail below with reference to the accompanying drawings through specific embodiments:
[0056] Reference Figures 1 to 5 As shown, this embodiment provides a battery, and the battery may be, for example, a lithium-ion battery.
[0057] The battery provided in this embodiment specifically includes: a housing 1 , a battery cell, a protection element 3 and a first adhesive tape 4 .
[0058] The battery cell is located in the housing 1 and has a tab 2. The housing 1 has a sealing portion 11, and the tab 2 extends from the sealing portion 11.
[0059] The housing 1 may be, for example, an aluminum-plastic film housing. Figure 4 and Figure 5 As shown, the sealing portion 11 may specifically include a top sealing portion located at the top of the housing 1. The pole lug 2 may specifically extend from the top sealing portion.
[0060] The protection element 3 is connected to the pole tab 2. Specifically, the protection element 3 can be electrically connected to the pole tab 2. Exemplarily, the protection element 3 can be welded to the pole tab 2, that is, a welding spot is formed at the connection position 30 between the protection element 3 and the pole tab 2.
[0061] Exemplarily, the protection element 3 is, for example, a temperature switch or a circuit breaker. The protection element 3 can be disconnected when the battery temperature is too high to prevent the battery from short-circuiting, thereby improving the safety of the battery.
[0062] If the connection position 30 (such as a welding point) between the protection element 3 and the tab 2 contacts a component on the battery, such as an aluminum-plastic film housing, or contacts a conductive component on the battery top cover, a short circuit will occur, which will lead to risks such as thermal runaway of the battery. Based on this, the first adhesive tape 4 at least covers the connection position 30 between the protection element 3 and the tab 2 to at least protect the connection position 30 and avoid risks such as short circuits.
[0063] Specifically, the first adhesive tape 4 covers at least the connection position 30: the first adhesive tape 4 can only cover the connection position 30 between the protection element 3 and the tab 2 to protect the connection position 30, and also plays a role in fixing the protection element 3, further improving the stability of the protection element 3, and thus improving the stability of the battery. In addition, the first adhesive tape 4 can also cover other positions on the top of the battery except the connection position 30.
[0064] Reference Figure 4 and Figure 5 As shown, at least part of the protection element 3 is specifically located on the top sealing portion. Since the connection position 30 between the protection element 3 and the tab 2 is covered with the first adhesive tape 4, when the protection element 3 is located on the top sealing portion, the connection position 30 between the protection element 3 and the tab will not directly contact the top sealing portion of the housing 1, thereby avoiding the connection position 30 contacting the top sealing portion of the housing 1, etc., and causing a short circuit.
[0065] Exemplary, combined Figure 4 and Figure 5 , the battery cell has a positive terminal ear (such as Figure 4 and Figure 5 The electrode tab 2 shown in the figure and the negative electrode tab (not shown in the figure), for example, the protection element 3 is welded to the negative electrode tab, and a welding spot is formed at the connection position of the protection element 3 and the negative electrode tab. In the specific production, the negative electrode tab needs to be folded back to the top of the battery after being welded to the protection element 3. In the specific implementation, the connection position 30 between the protection element 3 and the electrode tab 2 can be wrapped with the first adhesive tape 4, that is, the first adhesive tape 4 covers and adheres the connection position 30, and then the electrode tab 2 is bent downward, and the protection element 3 is turned over. The protection element 3 is now located on the top sealing part. Since the connection position 30 between the protection element 3 and the electrode tab 2 is covered with the first adhesive tape 4, the connection position 30 between the protection element 3 and the electrode tab will not directly contact the top sealing part of the shell 1, thereby avoiding the connection position 30 from contacting the top sealing part of the shell 1 and causing a short circuit.
[0066] Furthermore, after the protection element 3 is turned over along with the tab 2, Figure 4 and Figure 5A first adhesive tape 4 is affixed to the top of the battery in the left and right directions, thereby further protecting and fixing the protection element 3, further preventing the connection position 30 from contacting other components and causing a short circuit, thereby improving the safety of the battery and improving the fixing effect of the protection element 3.
[0067] The first adhesive tape 4 includes a first adhesive layer 42 and a first substrate 41 disposed on one side of the first adhesive layer 42. For example, the first adhesive layer 42 is in contact with and bonded to the required protection positions such as the connection position 30 between the protection element 3 and the tab 2.
[0068] The material of the first substrate 41 is selected from at least one of polyimide (PI, hereinafter referred to as PI substrate) and polyethylene terephthalate (PET).
[0069] The molecular structure of PI substrate and PET is close, and its surface energy is better matched with the adhesive layer, and it is also resistant to solvent corrosion, unlike the substrate raw paper of masking tape, which needs to be impregnated with solvent before forming the substrate of masking tape, and then the adhesive layer can be coated. That is, the first adhesive tape 4 provided in this embodiment can be directly coated during production, that is, the first adhesive layer 42 is directly coated on the first substrate 41 to form the first adhesive tape 4, and the process does not need to use the impregnation process, thereby effectively avoiding the generation and residue of carbon disulfide, meeting environmental protection requirements.
[0070] Specifically, the light transmittance of the first adhesive tape 4 can be made no greater than 20%. This arrangement can improve the recognition of the first adhesive tape 4, so that after the first adhesive tape 4 is bonded, it can be quickly recognized by the light transmittance whether the application position of the first adhesive tape 4 is correct and whether the first adhesive tape 4 covers the required protection positions such as the connection position 30, thereby providing greater convenience for the operator and ensuring that the first adhesive tape 4 effectively covers the required protection positions such as the connection position 30, thereby further ensuring the safety of the battery.
[0071] The battery provided in this embodiment covers at least the connection position 30 between the protection element 3 and the tab 2 by the first adhesive tape 4, so as to prevent the connection position 30 from contacting with the housing 1 or other components on the battery top cover to a certain extent and causing a short circuit, thereby improving the safety of the battery. At the same time, by setting the first adhesive tape 4 to include a first adhesive layer 42 and a first substrate 41 located on one side of the first adhesive layer 42, the material of the first substrate 41 is selected from at least one of polyimide and polyethylene terephthalate. Due to the material characteristics of the first substrate 41, the first adhesive tape 4 can be formed by directly coating the first adhesive layer 42 on one side of the first substrate 41 using a coating process, that is, the process does not require impregnation, so there will be no solvent residue, that is, the carbon disulfide residue is avoided, and it meets environmental protection requirements.
[0072] At the same time, by setting the transmittance of the first adhesive tape 4 to no more than 20%, after the first adhesive tape 4 is bonded, it is possible to quickly identify through the transmittance whether the application position of the first adhesive tape 4 is correct and whether the first adhesive tape 4 covers the required protection positions such as the connection position 30, thereby providing greater convenience for the operator and ensuring that the first adhesive tape 4 effectively covers the required protection positions such as the connection position 30, thereby further ensuring the safety of the battery.
[0073] In addition, due to the structural composition of the masking tape, a composite process must be used in the manufacturing process, and the adhesive layer in the composite process must be very thick, which causes the masking tape to be prone to serious adhesive overflow in a high-humidity use environment, thereby affecting the protective effect of the masking tape on the battery and the packaging effect of the battery. However, the first adhesive tape 4 in the embodiment of the present invention, since its substrate is at least one of a PI substrate and a PET substrate, can be directly coated with an adhesive layer using a coating process during manufacturing, that is, no composite process is required. Compared with the composite process, the coating process is easier to control the coating of the adhesive layer, so that the thickness of the adhesive layer can be flexibly controlled according to actual needs when coating the adhesive layer, thereby avoiding the occurrence of adhesive overflow caused by an excessively thick adhesive layer.
[0074] That is to say, compared with the masking tape, the first adhesive tape 4 in this embodiment not only achieves no carbon disulfide residue and meets the environmental protection requirements, but also can effectively solve the problems of residual glue and overflow of the masking tape.
[0075] Among them, the specific bonding process when bonding the first adhesive tape 4 to the required protection position of the battery is the same as the bonding process when bonding the masking tape to the battery, that is, the first adhesive tape 4 provided in this embodiment does not need to change the existing gluing process while achieving the above-mentioned technical effects, and is adapted to the existing gluing process.
[0076] Reference Figure 1As shown, in some embodiments, along the first direction, the total thickness H of the first adhesive tape 4 is not greater than 180 μm.
[0077] Among them, refer to Figure 1 , the first direction can be specifically Figure 1 In the up-down direction, the total thickness H of the first adhesive tape 4 is the thickness of the first adhesive tape 4 along the up-down direction, that is, the total thickness H of the first adhesive tape 4 = the thickness h1 of the first substrate 41 in the up-down direction + the thickness h2 of the first adhesive layer 42 in the up-down direction.
[0078] Reference Figure 4 and Figure 5 The first direction may be a direction perpendicular to the paper surface, that is, the first direction is perpendicular to the paper surface. Figure 4 and Figure 5 The up-down direction is perpendicular to Figure 4 and Figure 5 The left and right directions are perpendicular.
[0079] Exemplarily, the total thickness H of the first adhesive tape 4 can be 50μm, 55μm, 60μm, 65μm, 70μm, 80μm, 90μm, 95μm, 100μm, 110μm, 120μm, 130μm, 140μm, 150μm, 160μm, 170μm, or 180μm.
[0080] By setting the thickness of the first adhesive tape 4 within the above range, the first adhesive tape 4 is not likely to crack, thereby ensuring that the first adhesive tape 4 effectively covers the required protection position, thereby improving the safety of the battery.
[0081] In some embodiments, along the first direction, the thickness h1 of the first substrate 41 may be set between 45 μm and 70 μm, such as 45 μm, 50 μm, 55 μm, 57.5 μm, 60 μm, 65 μm, or 70 μm.
[0082] In specific implementation, if the thickness h2 of the first adhesive layer 42 is too small, it will affect the bonding effect of the first adhesive layer 42, but if the thickness h2 of the first adhesive layer 42 is too large, it will cause the first adhesive layer 42 to crack or warp easily, thereby causing a short circuit risk. Based on this, in some embodiments, the thickness h2 of the first adhesive layer 42 can be set between 20μm and 50μm. For example, it can be 20μm, 25μm, 30μm, 35μm, 40μm, 45μm, and 50μm.
[0083] By setting the thickness h2 of the first adhesive layer 42 within this range, not only the bonding effect between the first adhesive layer 42 and the desired protection position is ensured, but also the first adhesive layer 42 is not prone to cracking or warping, thereby ensuring the safety of the battery.
[0084] The peeling force of the first adhesive tape 4 was tested using a national standard steel plate:
[0085] For example, a 200mm long sample is cut from the first adhesive tape 4 sample, and one end of the first adhesive layer 42 is folded in half along the length direction of the sample to form a folded layer of about 15mm in length. Holding the folded layer, the other end of the sample is pasted on one end of the steel plate, so that the first adhesive tape 4 is naturally placed above the steel plate (not touching the steel plate), and then the roller is rolled back and forth twice manually or mechanically to prevent air from remaining between the first adhesive layer 42 and the steel plate (if there is air, the sample is invalid).
[0086] Specifically, 20 mm of the first adhesive tape 4 is peeled off from the steel plate by one folded end of the first adhesive tape 4, one end of the steel plate is clamped in the clamp of the peeling force testing machine, and the free end of the first adhesive tape 4 is clamped in another clamp. The other clamp continuously peels the first adhesive tape 4 from the steel plate at an angle of 180° at a rate of (5±0.3) mm / s, thereby obtaining the peeling force.
[0087] Make multiple samples, and test each sample one by one, and complete it within 1 minute.
[0088] The average value of the peeling forces measured from a plurality of samples is the peeling force of the first adhesive tape 4 .
[0089] After testing the first adhesive tape 4, the measured peeling force of the first adhesive tape 4 is not less than 0.06 kgf / mm. It can be seen that the first adhesive tape 4 has a large peeling force, which can ensure that the first adhesive tape 4 is not easy to peel off and warp to a certain extent, thereby preventing the battery from short circuiting and improving the safety of the battery.
[0090] In some embodiments, the material of the first adhesive layer 42 is selected from at least one of acrylate copolymer (also known as acrylic, hereinafter referred to as acrylic glue), polysiloxane resin (also known as organic silicone), and styrene-isoprene block copolymer (also known as SIS rubber).
[0091] For example, the first substrate 41 of the first adhesive tape 4 is selected as a PI substrate, and the first adhesive layer 42 is selected as an acrylic adhesive layer. Acrylic adhesive has low cost, is easy to apply, and has good bonding strength.
[0092] In some embodiments, the first adhesive layer 42 is further doped with a color-adjusting dopant. By adding the color-adjusting dopant into the first adhesive layer 42, for example, the chromaticity or light transmittance of the first adhesive tape 4 can be adjusted, wherein the chromaticity can include, for example, hue, color vividness, and color depth, so that on the one hand, production requirements or customized requirements of different customers for the color of the first adhesive tape 4 can be met, and on the other hand, it can be convenient to quickly identify whether the application position of the first adhesive tape 4 is correct and whether the required protection positions such as the connection position 30 are covered in place, thereby providing convenience for operators and further ensuring that the first adhesive tape 4 effectively covers the required protection positions such as the connection position 30, thereby improving the safety of the battery.
[0093] The color-adjusting dopant is, for example, at least one selected from titanium dioxide and mica powder.
[0094] For example, when the first adhesive layer 42 is acrylic adhesive, adding titanium dioxide to the acrylic copolymer can make the first adhesive layer 42 appear bright yellow. For another example, adding mica powder to the acrylic copolymer can make the color of the first adhesive layer 42 more layered, thereby improving the appearance of the first adhesive layer 42.
[0095] According to specific tests, the dimensional shrinkage rate of the first adhesive tape 4 along the MD direction is less than 1.5%, and the dimensional shrinkage rate along the TD direction is less than 1%.
[0096] The MD direction is specifically the longitudinal direction, for example, Figure 2 The length direction of the first adhesive tape 4 is specifically the transverse direction, and the TD direction is perpendicular to the MD direction, for example, it can be Figure 2 The width direction of the first adhesive tape 4.
[0097] That is to say, the first adhesive tape 4 of this embodiment can effectively prevent the first adhesive tape 4 from being deformed and causing debonding under high temperature conditions, thereby preventing the problem of short circuit from occurring, thereby improving the safety of the battery.
[0098] Furthermore, the dimensional shrinkage of the first adhesive tape 4 along the MD direction is less than 0.8%, and the dimensional shrinkage along the TD direction is less than 0.3%, which can further avoid the first adhesive tape 4 from being deformed and causing the adhesive to come apart, further improving the safety of the battery.
[0099] For example, at a temperature of 130° C., the shrinkage rate of the first adhesive tape 4 is tested after the first adhesive tape 4 is stored for 72 hours.
[0100] Exemplarily, the heat resistance of the first adhesive tape 4 in which the first substrate 41 is specifically selected as a PI substrate and the first adhesive layer 42 is specifically selected as an acrylic adhesive is tested:
[0101] Before testing the first adhesive tape 4, the size of the first adhesive tape 4 in the TD direction was 100 mm, and the size in the MD direction was 99 mm. After being stored at a temperature of 130° C. for three days, the measured size of the first adhesive tape 4 in the TD direction was 99.25 mm, and the size in the MD direction was 98.96. That is, after testing, the shrinkage rate of the first adhesive tape 4 in the TD direction was 0.75%, and the shrinkage rate in the MD direction was 0.04%, proving that the first adhesive tape 4 of this embodiment has better heat shrinkage resistance, that is, strong heat resistance, that is, the first adhesive tape 4 provided in the embodiment of the present invention is not easy to deform, thereby ensuring that the first adhesive tape 4 effectively protects the required protection positions such as the connection position 30, thereby improving the safety of the battery.
[0102] In some embodiments, the porosity of the first substrate 41 ranges from 1% to 10%. The swelling ratio of the first substrate 41 ranges from 0 to 5%.
[0103] Exemplarily, after the first substrate 41 is immersed in a solvent for a preset time, the porosity and swelling rate of the first substrate 41 are tested. For example, the solvent can be selected from at least one of N-methyl-2-pyrrolidone (NMP), ethyl acetate, dimethyl carbonate (DMC), methyl ethyl ketone (MEK), and ethanol. The preset time is, for example, seven days.
[0104] After testing, it was found that the porosity of the first substrate 41 was relatively small, that is, the density of the first substrate 41 was still relatively high after immersion, and the swelling rate was relatively low, which proved that the first adhesive tape 4 could effectively prevent the chemical corrosion of the solvent, thereby ensuring the stability of the first adhesive tape 4. Moreover, it was proved that the first adhesive tape 4 could effectively block the solvent, preventing the solvent from penetrating the first adhesive tape 4 and affecting the adhesion of the first adhesive tape 4, thereby affecting the performance of the components in the area covered by the first adhesive tape 4.
[0105] Furthermore, the swelling rate of the first substrate 41 is in the range of 0-1%, which further improves the stability of the first substrate 41, and the first substrate 41 is not easily deformed, thereby further improving the adhesion and stability of the first adhesive tape 4, and ensuring that the first adhesive tape 4 effectively protects the required protection position.
[0106] Exemplarily, the first substrate 41 (taking the first substrate 41 as a PI substrate as an example) is divided into five equal samples, and one sample is immersed in each of the solvents NMP, DMC, MEK, ethyl acetate, and ethanol.
[0107] Meanwhile, a polypropylene PP / polyethylene PE composite substrate and a polypropylene PP porous substrate as the first substrate 41 were selected as comparative examples, and five samples of each were obtained and immersed in the above solvents.
[0108] After soaking for seven days at 25°C, the porosity of the corresponding substrate was measured. The specific test data are shown in Table 1 below:
[0109]
[0110] The above porosity is the average of the porosities of the corresponding substrates finally measured in five solvents.
[0111] It can be seen from the comparison in Table 1 that the porosity of the PI substrate is relatively low, that is, the first adhesive tape 4 using the PI substrate has a compact structure and has a good barrier effect on solvents.
[0112] The masking paper substrate of the masking tape in the related art is easily adhered. In the manufacturing process, in order to unwind, a release agent must be applied on the side of the masking tape that is away from the adhesive layer. After the release agent is applied, the peeling force of the masking tape will be reduced, so that it is easy to be peeled off, thereby achieving unwinding. However, the coating uniformity of the release agent is difficult to control, which will cause residual adhesive to delaminate. The first substrate 41 in the embodiment of the present invention selects at least one of a PI substrate or a PET substrate, and the surface of the substrate is smooth. The side of the substrate that is away from the first adhesive layer 42 is not easy to adhere, and there is no need to apply a release agent.
[0113] For example, refer to Figure 6 As shown, the first adhesive tape 4 of this embodiment is selected and divided into three equal samples ( Figure 6 1, 2, and 3), a Nitto 5000NS tape is coated on the side of the first substrate 41 away from the first adhesive layer 42, and then the peeling force between the first adhesive paper 4 and the Nitto 5000NS tape is tested. The test results are shown in FIG. Figure 6 shown.
[0114] Due to the beginning and end of the test, the instability of the test equipment will cause the first adhesive tape 4 to be unstable. Figure 6 It can be seen from the deformation amount in the force stable section of 20mm~80mm that the peeling force on the side of the first adhesive tape 4 away from the first adhesive layer 42 is relatively large. For example, when the deformation amount is 25mm, the corresponding peeling force is approximately 0.1kgf / mm, which proves that no release agent is added to the side of the first substrate 41 away from the first adhesive layer 42. In other words, the first adhesive tape 4 provided in this embodiment can achieve self-unwinding without coating a release agent on the side of the first substrate 41 away from the first adhesive layer 42, thereby avoiding the residual adhesive delamination phenomenon caused by the coating of the release agent and saving the production cost.
[0115] In actual use, if the side of the shell 1 contacts other parts of the battery, a short circuit will occur, leading to thermal runaway. In addition, if impurities such as dust and dirt adhere to the surface of the shell 1 and then fall into the battery cell, the performance and life of the battery will be affected. Based on this, in some embodiments, refer to Figure 3 , Figure 4 and Figure 5 As shown, the battery provided by the embodiment of the present invention further includes a second adhesive tape 5 , and at least a portion of the second adhesive tape 5 covers at least one side of the housing 1 along the second direction.
[0116] The second direction may be the width direction of the battery, for example Figure 4 and Figure 5 In the left-right direction, at least part of the second adhesive tape 5 covers at least one side of the shell 1. For example, both the left and right sides of the shell 1 are covered with the second adhesive tape 5, or one side of the shell 1 in the left-right direction is covered with the second adhesive tape 5.
[0117] In a specific implementation, the second adhesive tape 5 covers the side of the housing 1, and the top end of the second adhesive tape 5 can extend and cover the top edge of the housing 1, thereby increasing the coverage area of the second adhesive tape 5, further improving the protection effect, and further improving the safety of the battery. In addition, the top end of the second adhesive tape 5 can extend and cover the top edge of the housing 1, and the bottom end of the second adhesive tape 5 can extend and cover part of the bottom surface of the housing 1.
[0118] The second adhesive tape 5 is used to protect at least the side of the shell 1 to prevent the exposed aluminum foil on the side of the shell 1 from coming into contact with other components and causing a short circuit, thereby avoiding thermal runaway of the battery and preventing dust and other impurities from directly adhering to the surface of the shell 1 and then falling into the battery cell, thereby improving the performance and life of the battery. In addition, the second adhesive tape 5 can increase the strength of the battery, thereby ensuring the stability of the battery.
[0119] The second adhesive tape 5 includes a second adhesive layer 52 and a second base material 51 disposed on one side of the second adhesive layer 52 .
[0120] The second substrate 51 is selected from at least one of polyimide and polyethylene terephthalate.
[0121] That is to say, the second substrate 51 is made of the same material as the first substrate 41. The first substrate 41 and the second substrate 51 are made of the same material, including but not limited to: the first substrate 41 and the second substrate 51 are both made of polyimide, or the first substrate 41 and the second substrate 51 are both made of polyethylene terephthalate, or the first substrate 41 is made of polyimide and the second substrate 51 is made of polyethylene terephthalate.
[0122] In some embodiments, the material of the second adhesive layer 52 is selected from at least one of acrylate copolymer, polysiloxane resin, and styrene-isoprene block copolymer.
[0123] That is to say, the second adhesive layer 52 and the first adhesive layer 42 are made of the same material. The second adhesive layer 52 and the first adhesive layer 42 are made of the same material, including but not limited to: the first adhesive layer 42 and the second adhesive layer 52 are both made of acrylate copolymers; or the first adhesive layer 42 and the second adhesive layer 52 are both made of polysiloxane resins; or the first adhesive layer 42 is made of acrylate copolymers, and the second adhesive layer 52 is made of polysiloxane resins, etc., that is, the first adhesive layer 42 and the second adhesive layer 52 are made of the same material.
[0124] Therefore, the second adhesive tape 5 can achieve the above-mentioned corresponding technical effects of the first adhesive tape 4, which will not be described in detail here. For details, please refer to the description of the first adhesive tape 4 in the above embodiment.
[0125] In some embodiments, the light transmittance of the second adhesive tape 5 can be different from that of the first adhesive tape 4. This arrangement can distinguish the first adhesive tape 4 and the second adhesive tape 5 from the appearance of the adhesive tape, thereby achieving effective foolproofing, avoiding the mixing of the first adhesive tape 4 and the second adhesive tape 5 when used at the same time, and improving production and assembly efficiency.
[0126] In specific implementation, the light transmittance of the second adhesive tape 5 can be set to be no less than 80%.
[0127] Exemplarily, the light transmittance of the first adhesive tape 4 is not greater than 20%, and the light transmittance of the second adhesive tape 5 is not less than 80%, so that the difference in light transmittance between the first adhesive tape 4 and the second adhesive tape 5 is more obvious, thereby further improving the convenience during assembly and use.
[0128] Of course, in other implementations, the light transmittance of the second adhesive tape 5 and the light transmittance of the first adhesive tape 4 may also be the same.
[0129] In the specific implementation, in consideration of safety and to avoid the first adhesive tape 4 from cracking, the first adhesive tape 4 may be made thicker. At the same time, if the total thickness of the second adhesive tape 5 is too thick, the energy density per unit volume of the battery will be reduced, and the second adhesive tape 5 will bend and warp, which will lead to the risk of aluminum leakage on the side of the battery. Based on this, in some embodiments, refer to Figure 1 and Figure 3 As shown, the total thickness D of the second adhesive tape 5 can be made smaller than the thickness H of the first adhesive tape 4 .
[0130] Specifically, in some embodiments, along the second direction, the total thickness D of the second adhesive tape 5 can be set to be no greater than 45 μm, for example, 15 μm, 17 μm, 20 μm, 25 μm, 30 μm, 35 μm, 40 μm, or 45 μm.
[0131] Reference Figure 3 As shown, the second direction is Figure 3 In the vertical direction, the total thickness D of the second adhesive tape 5 is the thickness dimension of the second adhesive tape 5 in the vertical direction. That is, the total thickness D of the second adhesive tape 5 = the thickness d1 of the second substrate 51 in the vertical direction + the thickness d2 of the second adhesive layer 52 in the vertical direction.
[0132] Reference Figure 4 and Figure 5 As shown, the second direction can be specifically Figure 4 and Figure 5 In the left-right direction, the total thickness D of the second adhesive tape 5 is the size of the second adhesive tape 5 along the left-right direction.
[0133] By setting the total thickness D of the second adhesive tape 5 to be no more than 45 μm and the total thickness H of the first adhesive tape 4 to be no more than 180 μm, this ensures that the total thickness H of the first adhesive tape 4 is thicker to avoid the risk of short circuit caused by cracking of the first adhesive tape 4, thereby improving the safety of the battery, and at the same time ensures that the total thickness D of the second adhesive tape 5 is not too thick, thereby avoiding the situation where the second adhesive tape 5 is too thick and causes the energy density per unit volume of the battery to decrease. That is, this setting takes into account both the safety of the battery and the energy density per unit volume of the battery.
[0134] Of course, in other implementations, the total thickness D of the second adhesive tape 5 may be the same as the total thickness H of the first adhesive tape 4 .
[0135] In some embodiments, reference Figure 3 As shown, along the second direction, the thickness d1 of the second substrate 51 can be set between 12 μm and 30 μm, such as 12 μm, 15 μm, 18 μm, 20 μm, 21 μm, 25 μm, 26 μm, 28 μm, and 30 μm.
[0136] In some embodiments, the ratio of the thickness h1 of the second substrate 51 to the thickness h2 of the first substrate 41 may be set between 1 / 6 and 2 / 3, for example, the ratio may be 1 / 6, 2 / 5, 1 / 2, or 2 / 3.
[0137] Such a configuration can further prevent the second adhesive tape 5 from being too thick and causing cracking and warping.
[0138] In specific implementation, if the thickness d2 of the second adhesive layer 52 is too small, it will affect the bonding effect of the second adhesive layer 52, but if the thickness d2 of the second adhesive layer 52 is too large, it will cause the second adhesive layer 52 to crack or warp easily, thereby causing a short circuit risk. Based on this, in some embodiments, the thickness d2 of the second adhesive layer 52 can be set between 5μm and 15μm. For example, it can be 5μm, 6μm, 7μm, 8μm, 9μm, 10μm, 11μm, 12μm, 13μm, and 15μm.
[0139] By setting the thickness d2 of the second adhesive layer 52 within this range, not only the bonding effect between the second adhesive layer 52 and the side of the shell 1 is ensured, but also the second adhesive layer 52 is not easy to crack or warp, thereby ensuring the safety of the battery.
[0140] In some embodiments, the ratio of the thickness d2 of the second adhesive layer 52 to the thickness h2 of the first adhesive layer 42 may be set between 1 / 10 and 3 / 4, for example, the ratio may be 1 / 10, 2 / 7, or 3 / 4.
[0141] In specific implementation, for example, an international steel plate is used to test the peeling force of the second adhesive tape 5, the second adhesive layer 52 of the second adhesive tape 5 is pasted on the steel plate, and the second adhesive tape 5 is tested using a peeling force testing machine. The measured peeling force of the second adhesive tape 5 ranges from 0.018kgf / mm to 0.021kgf / mm, which proves that the second adhesive tape 5 has a good bonding effect with the side of the shell 1 and is not easy to debond, thereby improving the safety of the battery.
[0142] The peeling force test conditions and test method of the second adhesive tape 5 may be the same as the peeling force test conditions and test method of the first adhesive tape 4 on the steel plate, and the details may refer to the above description.
[0143] It can be seen from the above embodiments that the peeling force of the first adhesive tape 4 is not less than 0.06kgf / mm, and the peeling force of the second adhesive tape 5 is in the range of 0.018kgf / mm to 0.021kgf / mm, that is, the peeling force of the first adhesive tape 4 can be greater than the peeling force of the second adhesive tape 5, so that adhesive tapes with different bonding strengths can be set according to the safety hazards existing in different positions of the battery, especially ensuring the safety of the top of the battery while taking into account the energy density and other performance of the battery.
[0144] In some embodiments, the battery further comprises an adhesive colloid. At least a portion of the adhesive colloid covers at least one side of the housing 1 along the second direction. The second direction is as described in the above embodiment and will not be described again here.
[0145] By using the adhesive colloid to protect at least the side of the shell 1, it is prevented that the surface of the shell 1 contacts other parts and causes a short circuit, thus avoiding thermal runaway of the battery. It can also prevent dust and other impurities from directly adhering to the surface of the shell 1 and then falling into the battery cell, thereby improving the performance and life of the battery. In addition, the adhesive colloid can increase the strength of the battery, thereby ensuring the stability of the battery.
[0146] In a specific implementation, glue may be applied on the side of the housing 1 by dispensing glue, and then the glue is cured to form the above-mentioned adhesive colloid.
[0147] By applying glue at least on the side of the shell 1 by dispensing to form a bonding colloid, it is easier to control the thickness of the glue, which is conducive to the thin design of the bonding colloid, thereby further ensuring the energy density of the battery. Moreover, by applying glue at least on the side of the shell 1 by dispensing, the process operation of dispensing is simpler than the solution of sticking adhesive tape on the side of the shell 1, thereby improving the production efficiency of the battery. In addition, the peeling force of the bonding colloid formed by dispensing and curing is greater than the peeling force of the adhesive tape, thereby improving the bonding strength of the bonding colloid, making the bonding colloid not easy to fall off, thereby ensuring the effective protective effect of the bonding colloid on the shell 1.
[0148] In some embodiments, the material of the adhesive colloid can be selected from at least one of polyurethane (Polyurethane Rwactive, referred to as PUR) and polymethylmethacrylate (Polymethylmethacrylate, referred to as PMMA, commonly known as organic glass).
[0149] Taking the adhesive colloid selected from PUR hot melt glue as an example, in the specific implementation, PUR hot melt glue is coated on at least one side of the shell 1 along the second direction, thereby forming a PUR hot melt glue layer covering the side of the shell 1, and the PUR hot melt glue layer is cured to form the above-mentioned adhesive colloid.
[0150] If too much glue is dispensed during the coating process, it will cause glue overflow. Or when the material of the adhesive colloid is transparent PUR or PMMA, it will be difficult to identify the position of the glue coating, which will lead to incorrect application of the adhesive colloid. Based on this, in some embodiments, a fluorescent agent can be doped into the adhesive colloid.
[0151] By adding fluorescent agent, it is easy to identify the position of glue when applying the adhesive colloid, thereby facilitating the identification of the coating size and coating position of the glue, preventing the problem of glue overflow caused by excessive glue dispensing on the side, and ensuring the coating effect and appearance quality.
[0152] Specifically, a fluorescent light source can be used to illuminate during the coating process to identify the glue dot line and determine the size of the glue line, thereby providing convenience for the coating operation and enabling the adhesive colloid formed by the coating to be effectively adhered to the required protective position, thereby ensuring the safety of the battery.
[0153] Exemplarily, the material of the fluorescent agent can be selected from at least one of a stilbene-type fluorescent agent, a coumarin-type fluorescent agent, a pyrazoline-type fluorescent agent, and a xylylene-type fluorescent agent.
[0154] In the specific implementation, a silver aluminum-plastic film test plate is used to test the peeling force of the adhesive colloid:
[0155] For example, a bonding colloid is formed on a silver aluminum-plastic film test plate by dispensing and curing, and a 200 mm long sample is cut from the silver aluminum-plastic film test plate sample with the bonding colloid formed thereon. One end of the bonding colloid is folded in half along the length direction of the sample and pasted into a folded layer of about 15 mm in length.
[0156] Specifically, 20 mm of the adhesive colloid was peeled off from the silver aluminum-plastic film test plate by one folded end of the adhesive colloid, one end of the silver aluminum-plastic film test plate was clamped in the clamp of the peeling force tester, and the free end of the adhesive colloid was clamped in another clamp. The other clamp continuously peeled the adhesive colloid from the silver aluminum-plastic film test plate at a rate of (5±0.3) mm / s at an angle of 180°, thereby obtaining the peeling force.
[0157] Make multiple samples, and test each sample one by one, and complete it within 1 minute.
[0158] The average value of the peeling forces measured on multiple samples is the peeling force of the adhesive.
[0159] According to the test, the peeling force of the adhesive colloid is between 50 and 300 N / 25 mm, that is, between 0.204 kgf / mm and 1.22 kgf / mm.
[0160] At the same time, the peeling force of the first adhesive tape 4 was tested using a silver aluminum-plastic film test plate:
[0161] For example, a 200 mm long sample is cut from the first adhesive tape 4 sample, and one end of the first adhesive layer 42 is folded in half along the length direction of the sample to form a folded layer of about 15 mm in length. Holding the folded layer, the other end of the sample is pasted on one end of the silver aluminum-plastic film test plate, so that the first adhesive tape 4 is naturally placed above the silver aluminum-plastic film test plate (not touching the silver aluminum-plastic film test plate), and then the roller is rolled back and forth twice manually or mechanically to prevent air from remaining between the first adhesive layer 42 and the silver aluminum-plastic film test plate (if there is air, the sample is invalid).
[0162] Specifically, 20 mm of the first adhesive tape 4 was peeled off from the silver aluminum-plastic film test plate by one folded end of the first adhesive tape 4, and one end of the silver aluminum-plastic film test plate was clamped in the clamp of the peeling force testing machine, and the free end of the first adhesive tape 4 was clamped in another clamp. The other clamp continuously peeled the first adhesive tape 4 from the silver aluminum-plastic film test plate at a rate of (5±0.3) mm / s at an angle of 180°, thereby obtaining the peeling force.
[0163] Make multiple samples, and test each sample one by one, and complete it within 1 minute.
[0164] The average value of the peeling forces measured from a plurality of samples is the peeling force of the first adhesive tape 4 .
[0165] According to the test, the peeling force of the first adhesive tape 4 on the aluminum-plastic film is between 10 and 20 N / 25 mm, that is, between 0.041 kgf / mm and 0.082 kgf / mm.
[0166] It can be seen that the peeling force of the first adhesive tape 4 on the aluminum-plastic film is smaller than the peeling force of the adhesive colloid on the aluminum-plastic film. In this way, if the battery has thermal runaway, an opening is first generated at the top of the battery, thereby avoiding the thermal runaway phenomenon from being aggravated and improving the safety of the battery.
[0167] In this article, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, or it can be indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances. In addition, the orientation or position relationship indicated by the terms "upper", "lower", "left", "right", "front", "back", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc. are based on the orientation or position relationship shown in the accompanying drawings, which is only for the convenience of describing the present application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application.
[0168] In this article, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "comprises", "comprising" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the statement "comprising a ..." does not exclude the presence of other identical elements in the process, method, article or device including the element.
[0169] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A battery, characterized in that: It comprises a housing (1), a battery cell, a protective element (3) and a first adhesive tape (4); The battery cell is located in the shell (1), the battery cell has a pole ear (2), the shell (1) has a sealing portion (11), and the pole ear (2) extends from the sealing portion (11); the protection element (3) is connected to the pole ear (2), and the first adhesive tape (4) at least covers the connection position (30) between the protection element (3) and the pole ear (2); The first adhesive tape (4) comprises a first adhesive layer (42) and a first substrate (41) arranged on one side of the first adhesive layer (42), wherein the material of the first substrate (41) is selected from at least one of polyimide and polyethylene terephthalate; The light transmittance of the first adhesive tape (4) is not greater than 20%.
2. The battery according to claim 1, characterized in that The total thickness of the first adhesive tape (4) along the first direction is not greater than 180 μm; and / or, along the first direction, the thickness of the first substrate (41) ranges from 45 μm to 70 μm; And / or, along the first direction, the thickness of the first adhesive layer (42) ranges from 20 μm to 50 μm; And / or, the peeling force of the first adhesive tape (4) is not less than 0.06 kgf / mm.
3. The battery according to claim 1, characterized in that The material of the first adhesive layer (42) is selected from at least one of acrylate copolymer, polysiloxane resin, and styrene-isoprene block copolymer.
4. The battery according to claim 1, characterized in that The first glue layer (42) is also doped with a color-changing dopant; Preferably, the color-adjusting dopant is selected from at least one of titanium dioxide and mica powder.
5. The battery according to claim 1, characterized in that The dimensional shrinkage rate of the first adhesive tape (4) along the MD direction is less than 1.5%; Preferably, the dimensional shrinkage rate of the first adhesive tape (4) along the MD direction is less than 0.8%; and / or, the dimensional shrinkage rate of the first adhesive tape (4) along the TD direction is less than 1%; Preferably, the dimensional shrinkage rate of the first adhesive tape (4) along the TD direction is less than 0.3%.
6. The battery according to claim 1, characterized in that The porosity of the first substrate (41) is in the range of 1% to 10%; and / or, the swelling rate of the first substrate (41) is in the range of 0 to 5%; Preferably, the swelling ratio of the first substrate (41) is in the range of 0 to 1%.
7. The battery according to any one of claims 1 to 6, characterized in that: The battery further comprises a second adhesive tape (5), at least a portion of the second adhesive tape (5) covers at least one side of the housing (1) along the second direction; The second adhesive tape (5) comprises a second adhesive layer (52) and a second base material (51) arranged on one side of the second adhesive layer (52); The material of the second substrate (51) is selected from at least one of polyimide and polyethylene terephthalate.
8. The battery according to claim 7, characterized in that The material of the second adhesive layer (52) is selected from at least one of acrylate copolymer, polysiloxane resin and styrene-isoprene block copolymer.
9. The battery according to claim 7, characterized in that The light transmittance of the second adhesive tape (5) is different from the light transmittance of the first adhesive tape (4); Preferably, the light transmittance of the second adhesive tape (5) is not less than 80%.
10. The battery according to claim 7, characterized in that The total thickness of the second adhesive tape (5) is less than the total thickness of the first adhesive tape (4); and / or, along the second direction, the total thickness of the second adhesive tape (5) is not greater than 45 μm; and / or, along the second direction, the thickness of the second substrate (51) ranges from 12 μm to 30 μm; and / or, along the second direction, the thickness of the second adhesive layer (52) ranges from 5 μm to 15 μm; and / or, the ratio of the thickness of the second substrate (51) to the thickness of the first substrate (41) is in the range of 1 / 6 to 2 / 3; And / or, the ratio of the thickness of the second adhesive layer (52) to the thickness of the first adhesive layer (42) is in the range of 1 / 10 to 3 / 4; And / or, the peeling force of the second adhesive tape (5) is in the range of 0.018kgf / mm to 0.021kgf / mm.
11. The battery according to any one of claims 1 to 6, characterized in that: The battery also includes a bonding colloid; At least a portion of the adhesive colloid covers at least one side of the housing (1) along the second direction.
12. The battery according to claim 11, characterized in that The material of the bonding colloid is selected from at least one of polyurethane and polymethyl methacrylate; And / or, the bonding colloid is doped with a fluorescent agent; Preferably, the material of the fluorescent agent is selected from at least one of a stilbene type fluorescent agent, a coumarin type fluorescent agent, a pyrazoline type fluorescent agent, and a xylylene imine type fluorescent agent; And / or, the peeling force of the adhesive colloid ranges from 0.204kgf / mm to 1.22kgf / mm.
Citation Information
Patent Citations
Gummed paper
CN110380122A
Adhesive, gummed paper, electrochemical device and electric device
CN117121248A
Pole piece surface rubberizing detection method, device and equipment and pole piece rubberizing machine
CN117178399A
Porous high temperature insulation adhesive tape that lithium ion battery used
CN206163599U
Battery cell dispensing detection system, battery manufacturing equipment and battery
CN215415048U