Nano motor for inducing hypertrophic scar copper death and preparation method thereof
By preparing copper and manganese-loaded Janus silica nanoparticles in the hyperplastic scar microenvironment, combining DSF and hyaluronidase, the problem of active transport of nanomotors in hyperplastic scars and induction of copper death in HSF is achieved Efficient HSF killing and alleviating cell hypoxia significantly improve the therapeutic effect.
Patent Information
- Application Number
- CN202411187731.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-12-03
AI Technical Summary
The existing nanomotors lack active transport capabilities in the hyperplastic scar microenvironment and fail to effectively induce copper death in HSF, limiting their application in hyperplastic scar treatment.
Spherical mesoporous silicone nanoparticles were synthesized by cetyl trimethylammonium bromide and diethane, and further processed to form Janus silica nanoparticles, and hydrolyzed by Cu(NO3)2 and MnCl2, and hexamethylene group was added Tetraamine catalysis to form Janus silica nanoparticles supported by copper and manganese, combined with DSF and hyaluronidase, nanomotors that can induce hyperplastic scar copper death.
The prepared nanomotor has a size of 300-400nm, and the loaded copper ions and manganese ions are only dispersed to the Janus rod-shaped tail, with catalytic hydrogen peroxide capability, which can excellently sustain the release of DSF, induce hyperplastic scar copper death, and show the best HSF kills and can relieve cell hypoxia.
Smart Images

Figure CN119055595A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of nanomotor preparation, and in particular to a nanomotor for inducing copper death of hypertrophic scars and a preparation method thereof. Background Art
[0002] Hypertrophic scar is a complex fibrotic disease, the occurrence of which involves multiple cell types and complex molecular mechanisms. Studies have shown that the excessive proliferation and activation of hypertrophic scar fibroblasts (HSF) play a key role in this process, suggesting that promoting the death of HSF may be a potential strategy to reverse scar formation. In this context, copper death, as a newly discovered form of programmed cell death, provides new prospects for treatment. Copper death is different from traditional apoptosis or necrosis. It depends on the accumulation of copper ions in cells, which promotes the abnormal oligomerization of lipoyl proteins. The discovery of this mechanism has opened up a new treatment path for us, that is, to inhibit the excessive proliferation of HSF by inducing copper death, thereby achieving the effect of treating hypertrophic scars.
[0003] At present, the treatment of hypertrophic scars still faces a major challenge, that is, it is difficult for drugs to effectively penetrate deep into scar tissue. The extracellular matrix of hypertrophic scars is dense, which hinders the passive transport of drugs and leads to poor treatment effects. Studies have shown that this property of nanomotors helps the distribution of drugs in complex tissues, thereby improving the efficiency of treatment. However, most nanomotors have not been optimized for the microenvironment of hypertrophic scars and lack the ability to actively transport in this environment. In addition, existing nanomotors have also failed to effectively induce copper death of HSF, which limits their application in the treatment of hypertrophic scars. Therefore, it has become a top priority to develop a nanomotor that can quickly and efficiently induce copper death of HSF. Summary of the invention
[0004] The present invention aims to provide a nanomotor for inducing copper death of hypertrophic scars and a preparation method thereof, so as to solve the problem that the existing nanomotor does not have the ability of active transport in the microenvironment of hypertrophic scars and fails to effectively induce copper death of HSF.
[0005] In order to achieve the above object, the present invention provides the following method:
[0006] Specifically, it relates to a nanomotor that induces copper death in hypertrophic scars and a preparation method thereof, which is characterized by:
[0007] S1: Synthesis of spherical mesoporous organosilica nanoparticles by hexadecyltrimethylammonium bromide and diethane;
[0008] S2: adding the spherical mesoporous organosilicon nanoparticles to a mixture of deionized water, ethanol, and hexadecyltrimethylammonium bromide, subjecting the mixture to ultrasonic and stirring treatment, and then adding tetraethyl orthosilicate to react, thereby obtaining Janus silica nanoparticles;
[0009] S3: dispersing the Janus silica nanoparticles in deionized water to obtain a Janus silica nanoparticle solution, adding a Cu(NO3)2 precursor to the Janus silica nanoparticle solution and stirring, then adding hexamethylenetetramine to the Janus silica nanoparticle solution to which the Cu(NO3)2 precursor has been added to catalyze the hydrolysis of Cu(NO3)2, and finally centrifuging to collect the centrifuge to obtain copper-loaded Janus silica nanoparticles;
[0010] S4: dispersing the copper-loaded Janus silica nanoparticles into deionized water to obtain a Cu-containing Janus silica nanoparticle solution, adding a MnCl2 precursor to the Cu-containing Janus silica nanoparticle solution and stirring, then adding hexamethylenetetramine to catalyze the hydrolysis of the MnCl2 precursor, and collecting to obtain Janus silica nanoparticles M-Cu@J containing Cu and Mn;
[0011] S5: preparing the M-Cu@J into an M-Cu@J ethanol suspension, adding 3-aminopropyltriethoxysilane to the M-Cu@J ethanol suspension, and performing a reaction centrifugation treatment, and washing with water and ethanol for several times to obtain an amino-functionalized M-Cu@J nanomotor;
[0012] S6: the copper-loaded Janus silica nanoparticles, the copper-loaded Janus silica nanoparticles and the amino-functionalized M-Cu@J nanomotor are separated into anhydrous ethanol to obtain a M-Cu@J nanoparticle solution, tetraethylthiuram disulfide is added to the M-Cu@J nanoparticle solution, and then freeze-dried to obtain a DSF-loaded M-CuD@J nanomotor;
[0013] S7: Dissolve EDC and NHS in PBS, add hyaluronidase to react at room temperature to obtain an activated hyaluronidase solution; then add the DSF-loaded M-CuD@J nanomotor to the activated hyaluronidase solution, stir and centrifuge, collect the centrifuge, and obtain the HM-CuD@J nanomotor.
[0014] Preferably, the step of synthesizing spherical mesoporous organosilicon nanoparticles using hexadecyltrimethylammonium bromide and diethane comprises: dispersing hexadecyltrimethylammonium bromide in a mixed solution comprising deionized water and ethanol to obtain a first solution; adding an aqueous ammonia solution to the first solution under continuous stirring to obtain a dispersion; adding diethane to the dispersion, reacting for 12 hours, and then centrifuging at a speed of 9000 rpm for 10 minutes, collecting the centrifuged product, and washing the centrifuged product several times with water and ethanol to obtain spherical mesoporous organosilicon nanoparticles.
[0015] Preferably, the step of adding the spherical mesoporous organosilicon nanoparticles to a mixture of deionized water, ethanol and hexadecyltrimethylammonium bromide, subjecting the mixture to ultrasonic and stirring treatment, and then adding tetraethyl orthosilicate to react to obtain Janus silica nanoparticles comprises: adding the spherical mesoporous organosilicon nanoparticle powder to a mixture containing deionized water, ethanol and hexadecyltrimethylammonium bromide to obtain a second solution; subjecting the second solution to ultrasonic treatment, and then adding an aqueous ammonia solution and stirring the solution; adding tetraethyl orthosilicate to the second solution after adding the aqueous ammonia solution, reacting for 2 hours, and then centrifuging at a speed of 9000 rpm for 10 minutes, collecting the centrifuge to obtain Janus silica nanoparticles, and washing the solution with water and ethanol for several times.
[0016] Preferably, the step of dispersing the Janus silica nanoparticles in deionized water to obtain a Janus silica nanoparticle solution, and adding a Cu(NO3)2 precursor to the Janus silica nanoparticle solution and stirring comprises: dispersing the Janus silica nanoparticles in deionized water to prepare a Janus silica nanoparticle solution with a concentration of 1 mg / ml; adding a Cu(NO3)2 precursor to the Janus silica nanoparticle solution and stirring for 30 minutes.
[0017] Preferably, the step of adding hexamethylenetetramine to the Janus silica nanoparticle solution to which a Cu(NO3)2 precursor has been added to catalyze the hydrolysis of Cu(NO3)2, and finally centrifuging to collect the centrifuge is the step of producing copper-loaded Janus silica nanoparticles, comprising: adding hexamethylenetetramine to the Janus silica nanoparticle solution to which a Cu(NO3)2 precursor has been added to catalyze the hydrolysis of Cu(NO3)2, reacting in an 85°C oil bath for 10 hours, centrifuging at 9000 rpm for 10 minutes, collecting the centrifuge as the copper-loaded Janus silica nanoparticles, and washing with water and ethanol several times.
[0018] Preferably, the step of dispersing the copper-loaded Janus silica nanoparticles in deionized water to obtain a Janus silica nanoparticle solution containing Cu, adding a MnCl2 precursor to the Janus silica nanoparticle solution containing Cu and stirring, then adding hexamethylenetetramine to catalytically hydrolyze the MnCl2, and collecting to obtain Janus silica nanoparticles M-Cu@J containing Cu and Mn comprises: dispersing the copper-loaded Janus silica nanoparticles in deionized water to a concentration of 1 mg / ml to obtain a Janus silica nanoparticle solution containing Cu; adding a MnCl2 precursor to the Janus silica nanoparticle solution containing Cu and stirring for 30 min to obtain a third solution; adding hexamethylenetetramine to the third solution to catalytically hydrolyze the MnCl2, and then reacting the solution in an oil bath at 85° C. for 10 h. The mixture was centrifuged at 17,726 rpm for 5 min, and the centrifuge was collected to obtain Janus silica nanoparticles M-Cu@J containing Cu and Mn, which were then washed several times with water and ethanol.
[0019] Preferably, the step of preparing the M-Cu@J into an M-Cu@J ethanol suspension, adding 3-aminopropyltriethoxysilane to the M-Cu@J ethanol suspension, performing a reaction centrifugation, and washing with water and ethanol several times to obtain an amino-functionalized M-Cu@J nanomotor comprises: preparing the M-Cu@J into an M-Cu@J ethanol suspension with a concentration of 10 mg / ml; adding 3-aminopropyltriethoxysilane to the M-Cu@J ethanol suspension for reaction, wherein the ratio of the M-Cu@J ethanol suspension to 3-aminopropyltriethoxysilane is 100:1; the reaction conditions are to react in a water bath at 35°C for 10 hours to obtain a fourth solution; and then centrifuging the fourth solution at a speed of 9000 rpm for 10 minutes, collecting the centrifuge, and washing with water and ethanol several times to obtain an amino-functionalized M-Cu@J nanomotor.
[0020] Preferably, the step of separating the copper-loaded Janus silica nanoparticles, the copper-loaded Janus silica nanoparticles and the amino-functionalized M-Cu@J nanomotor into anhydrous ethanol to obtain a M-Cu@J nanoparticle solution, adding tetraethylthiuram disulfide to the M-Cu@J nanoparticle solution, and then freeze-drying to obtain the DSF-loaded M-CuD@J nanomotor comprises: separating the copper-loaded Janus silica nanoparticles, the copper-loaded Janus silica nanoparticles and the amino-functionalized M-Cu@J nanomotor into anhydrous ethanol to obtain a M-Cu@J nanoparticle solution; adding tetraethylthiuram disulfide to the M-Cu@J nanoparticle solution; and then freeze-drying the solution to obtain the DSF-loaded M-CuD@J nanomotor. The amino-functionalized M-Cu@J nanomotor was divided into anhydrous ethanol to prepare a M-Cu@J nanoparticle solution with a concentration of 11 mg / ml; tetraethylthiuram disulfide was added to the M-Cu@J nanoparticle solution, and stirred at room temperature for 10 hours to obtain a fifth solution; the fifth solution was centrifuged at a speed of 9000 rpm for 10 minutes, the centrifuge was collected, and washed with water and ethanol for 2-3 times to obtain M-CuD@J nanoparticles; and the obtained M-CuD@J nanoparticles were freeze-dried.
[0021] Preferably, the steps of dissolving EDC and NHS in PBS, adding hyaluronidase and reacting at room temperature to obtain an activated hyaluronidase solution; then adding the DSF-loaded M-CuD@J nanomotor to the activated hyaluronidase solution for stirring and centrifugation, collecting the centrifuge, and obtaining the HM-CuD@J nanomotor include: dissolving EDC and NHS in PBS, adding hyaluronidase and reacting at room temperature for 2 hours to obtain an activated hyaluronidase solution; adding the DSF-loaded M-CuD@J nanomotor to the activated hyaluronidase solution and reacting for 4 hours under stirring to obtain a sixth solution; centrifuging the sixth solution at a speed of 9000 rpm for 10 minutes, collecting the centrifuge, and obtaining the HM-CuD@J nanomotor.
[0022] Preferably, the ratio of EDC, NHS and hyaluronidase is 30:40:2.
[0023] The present invention has the following beneficial effects: the motor size of the present invention is basically between 300-400nm, presenting a monodisperse state, and the loaded copper ions and manganese ions are only dispersed to the Janus rod tail, wherein the copper is Cu + and Cu 2+ It exists in two valence states, and manganese splits as a spin-orbit peak between the Mn2p 3 / 2 and Mn2p 1 / 2 peaks, and has the ability to catalyze hydrogen peroxide. DSF forms a metal chelate complex with copper and manganese on the surface of nanomotor nanoparticles, has excellent DSF sustained-release ability, can induce copper death in hypertrophic scars, and has the best HSF lethality. Since Mn can consume H2O2 to produce O2, it is beneficial to alleviate cell hypoxia. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the following is a brief introduction to the drawings required for the specific embodiments or the description of the prior art. In all the drawings, similar elements or parts are generally identified by similar reference numerals. In the drawings, the elements or parts are not necessarily drawn according to the actual scale.
[0025] Figure 1 It is a transmission electron microscope image of the HM-CuD@J nanomotor provided in an embodiment of the present invention.
[0026] Figure 2 This is a mapping element analysis diagram of the HM-CuD@J nanomotor provided in an embodiment of the present invention.
[0027] Figure 3 It is the SDS gel electrophoresis diagram of HAase, HM@J and HM-CuD@J nanomotors provided in the embodiments of the present invention.
[0028] Figure 4 This is an XPS spectrum diagram of the HM-CuD@J nanomotor provided in an embodiment of the present invention.
[0029] Figure 5 It is the ultraviolet-visible spectrum and infrared absorption spectrum of the HM-CuD@J nanomotor loaded with DSF provided by the embodiment of the present invention.
[0030] Figure 6 This is a kinetic curve diagram of the release of DSF by the HM-CuD@J nanomotor provided in an embodiment of the present invention.
[0031] Figure 7 3 is a degradation ability curve diagram of the HM-CuD@J nanomotor provided in an embodiment of the present invention.
[0032] Figure 8 This is an oxygen concentration curve of the four nanomotors, CuD@J, H-CuD@J, Mn-CuD@J, and HMn-CuD@J, provided in an embodiment of the present invention under 10 mM H2O2 conditions.
[0033] Fig. 9 This is the motion tracking diagram of the four nanomotors CuD@J, H-CuD@J, Mn-CuD@J, and HMn-CuD@J provided in the embodiment of the present invention under the conditions of 200mM H2O2+0.1% HA solution (10mg / ml)
[0034] Fig.10 These are fluorescence images of four nanomotors, CuD@J, M-CuD@J, H-CuD@J and HM-CuD@J, provided in the embodiments of the present invention, capturing different materials.
[0035] Fig.11 This is a CCK8 activity test graph of four nanomotors, namely CuD@J, M-CuD@J, H-CuD@J and HM-CuD@J, provided in an embodiment of the present invention.
[0036] Fig.12 (A) Western Blot strips of HSF treated with the four nanomotors, CuD@J, M-CuD@J, H-CuD@J and HM-CuD@J, provided in the embodiments of the present invention; (B) JC-1 fluorescence staining; (C) HPF fluorescence staining.
[0037] Fig.13 These are photos of New Zealand rabbit ear scar treatment using different groups of four nanomotors, namely CuD@J, M-CuD@J, H-CuD@J and HM-CuD@J, provided in the embodiments of the present invention. DETAILED DESCRIPTION
[0038] In order to make the technical personnel in the technical field better understand the scheme of the present invention, the technical scheme in the embodiment of the present invention will be clearly and completely described below in combination with the drawings in the embodiment of the present invention. Obviously, the described embodiment is only a part of the embodiment of the present invention, not all the embodiments. Based on the embodiment of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0039] The terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish different objects rather than to describe a specific order. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions. For example, a process, method, device, product or end including a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units that are not listed, or may optionally include other steps or units inherent to these processes, methods, products or ends.
[0040] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present invention. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0041] At present, the treatment of hypertrophic scars still faces a major challenge, that is, it is difficult for drugs to effectively penetrate deep into scar tissue. The extracellular matrix of hypertrophic scars is dense, which hinders the passive transport of drugs and leads to poor treatment effects. Studies have shown that this property of nanomotors helps the distribution of drugs in complex tissues, thereby improving the efficiency of treatment. However, most nanomotors have not been optimized for the microenvironment of hypertrophic scars and lack the ability to actively transport in this environment. In addition, existing nanomotors have also failed to effectively induce copper death of HSF, which limits their application in the treatment of hypertrophic scars. Therefore, it has become a top priority to develop a nanomotor that can quickly and efficiently induce copper death of HSF.
[0042] The present invention aims to provide a nanomotor for inducing copper death of hypertrophic scars and a preparation method thereof, so as to solve the problem that the existing nanomotor does not have the ability of active transport in the microenvironment of hypertrophic scars and fails to effectively induce copper death of HSF.
[0043] The features and performance of the present invention are further described in detail below in conjunction with the embodiments.
[0044] like Figure 1-13 As shown, this embodiment provides a nanomotor that induces copper death of hypertrophic scars and a preparation method thereof, characterized in that:
[0045] S1: Synthesis of spherical mesoporous organosilica nanoparticles by hexadecyltrimethylammonium bromide and diethane.
[0046] In an embodiment of the present invention, hexadecyltrimethylammonium bromide is dispersed in a mixed solution comprising deionized water and ethanol to obtain a first solution; an aqueous ammonia solution is added to the first solution under continuous stirring to obtain a dispersion; diethane is added to the dispersion, reacted for 6-12 hours, and then centrifuged at a speed of 5000-11000 rpm for 5-20 minutes, the centrifuged product is collected, and the centrifuged product is washed with water and ethanol several times to obtain spherical mesoporous organosilicon nanoparticles, wherein the ratio of deionized water to ethanol is 25:4-1:1.
[0047] S2: adding the spherical mesoporous organosilicon nanoparticles to a mixture of deionized water, ethanol and hexadecyltrimethylammonium bromide, subjecting the mixture to ultrasonic and stirring treatment, and then adding tetraethyl orthosilicate to react, thereby obtaining Janus silica nanoparticles.
[0048] In an embodiment of the present invention, the spherical mesoporous organosilicon nanoparticle powder is added to a mixture containing deionized water, ethanol and hexadecyltrimethylammonium bromide to obtain a second solution; the second solution is subjected to ultrasonic treatment, and then an ammonia solution is added and stirred; tetraethyl orthosilicate is added to the second solution after the ammonia solution is added, and after reacting for 2-6 hours, the solution is centrifuged at a speed of 5000-11000 rpm for 5-20 minutes, and the centrifuge is collected to obtain Janus silica nanoparticles, which are washed several times with water and ethanol; the mass ratio of the spherical mesoporous organosilicon nanoparticle powder to the spherical mesoporous organosilicon nanoparticle powder is 1:60-1:10.
[0049] S3: The Janus silica nanoparticles are dispersed in deionized water to obtain a Janus silica nanoparticle solution, a Cu(NO3)2 precursor is added to the Janus silica nanoparticle solution and stirred, and then hexamethylenetetramine is added to the Janus silica nanoparticle solution to catalyze the hydrolysis of Cu(NO3)2, and finally centrifugation is performed to collect the centrifuge to obtain copper-loaded Janus silica nanoparticles.
[0050] In an embodiment of the present invention, the Janus silica nanoparticles are dispersed in deionized water to prepare a Janus silica nanoparticle solution with a concentration of 1 mg / ml; a Cu(NO3)2 precursor is added to the Janus silica nanoparticle solution and stirred for 30 minutes; hexamethylenetetramine is added to the Janus silica nanoparticle solution to catalyze the hydrolysis of Cu(NO3)2, and then the mixture is reacted in an 85°C oil bath for 10 hours, centrifuged at a speed of 5000-11000 rpm for 5-20 minutes, and the centrifuge is collected as copper-loaded Janus silica nanoparticles, which are washed several times with water and ethanol, and the dosage ratio of the Cu(NO3)2 precursor to the hexamethylenetetramine is 15:1-1:1.
[0051] S4: The copper-loaded Janus silica nanoparticles are dispersed in deionized water to obtain a Cu-containing Janus silica nanoparticle solution, a MnCl2 precursor is added to the Cu-containing Janus silica nanoparticle solution and stirred, and then hexamethylenetetramine is added to catalyze the hydrolysis of the MnCl2 precursor, and Janus silica nanoparticles M-Cu@J containing Cu and Mn are collected.
[0052] In an embodiment of the present invention, the copper-loaded Janus silica nanoparticles are dispersed in deionized water at a concentration of 0.5-5 mg / ml to obtain a Cu-containing Janus silica nanoparticle solution; a MnCl2 precursor is added to the Cu-containing Janus silica nanoparticle solution and stirred for 30 minutes to obtain a third solution; hexamethylenetetramine is added to the third solution to catalytically hydrolyze the MnCl2, and then the solution is reacted in an oil bath at 85°C for 10 hours. Centrifuge at a speed of 5000-11000 for 5-20 minutes, collect the centrifuge, and obtain Janus silica nanoparticles M-Cu@J containing Cu and Mn, which are washed with water and ethanol several times, and the amount ratio of MnCl2 to hexamethylenetetramine is 15:1-1:1.
[0053] S5: The M-Cu@J is prepared into an M-Cu@J ethanol suspension, 3-aminopropyltriethoxysilane is added to the M-Cu@J ethanol suspension, and a reaction centrifugation treatment is performed. After washing with water and ethanol for several times, an amino-functionalized M-Cu@J nanomotor is obtained.
[0054] In an embodiment of the present invention, the M-Cu@J is prepared into an M-Cu@J ethanol suspension with a concentration of 10 mg / ml; 3-aminopropyltriethoxysilane is added to the M-Cu@J ethanol suspension for reaction, and the ratio of the M-Cu@J ethanol suspension to 3-aminopropyltriethoxysilane is 100:1-20:1; the reaction conditions are to react in a 35°C water bath for 10 hours to obtain a fourth solution; then the fourth solution is centrifuged at a speed of 9000 rpm for 10 minutes, the centrifuge is collected, and washed with water and ethanol several times to obtain an amino-functionalized M-Cu@J nanomotor.
[0055] S6: The copper-loaded Janus silica nanoparticles, the copper-loaded Janus silica nanoparticles and the amino-functionalized M-Cu@J nanomotor are separated into anhydrous ethanol to obtain a M-Cu@J nanoparticle solution, tetraethylthiuram disulfide is added to the M-Cu@J nanoparticle solution, and then freeze-dried to obtain a DSF-loaded M-CuD@J nanomotor.
[0056] In an embodiment of the present invention, the copper-loaded Janus silica nanoparticles, the copper-loaded Janus silica nanoparticles and the amino-functionalized M-Cu@J nanomotor are divided into anhydrous ethanol to prepare a M-Cu@J nanoparticle solution with a concentration of 11 mg / ml; tetraethylthiuram disulfide is added to the M-Cu@J nanoparticle solution, and stirred at room temperature for 10 hours to obtain a fifth solution; the fifth solution is centrifuged at a speed of 9000 rpm for 10 minutes, the centrifuge is collected, and washed with water and ethanol 2-3 times to obtain M-CuD@J nanoparticles; and the obtained M-CuD@J nanoparticles are freeze-dried.
[0057] S7: Dissolve EDC and NHS in PBS, add hyaluronidase to react at room temperature to obtain an activated hyaluronidase solution; then add the DSF-loaded M-CuD@J nanomotor to the activated hyaluronidase solution, stir and centrifuge, collect the centrifuge, and obtain the HM-CuD@J nanomotor.
[0058] In an embodiment of the present invention, EDC and NHS are dissolved in PBS, hyaluronidase is added and reacted at room temperature for 2 hours to obtain an activated hyaluronidase solution; the DSF-loaded M-CuD@J nanomotor is added to the activated hyaluronidase solution and reacted for 4 hours under stirring to obtain a sixth solution; the sixth solution is centrifuged at 9000 rpm for 10 minutes, and the centrifuge is collected to obtain HM-CuD@J nanomotor; the ratio of EDC, NHS and hyaluronidase is 30:40:2.
[0059] like Figure 1 The figure shows the transmission electron micrograph of the HM-CuD@J nanomotor. The motor size is basically between 300-400nm and is monodispersed.
[0060] like Figure 2 Figure 2 shows the mapping element analysis of the HM-CuD@J nanomotor, which shows that the loaded copper ions and manganese ions are only dispersed in the Janus rod tail.
[0061] like Figure 3 Shown are SDS gel electrophoresis of HAase, HM@J and HM-CuD@J nanomotors; the results show that HAase was successfully synthesized on the surface of HM@J and HM-CuD@J materials.
[0062] like Figure 4Figure 2 shows the XPS spectrum of the HM-CuD@J nanomotor. The overall spectrum is subjected to peak separation to analyze the valence states of copper and manganese, thereby providing reliable evidence for the catalysis of hydrogen peroxide as an ion. From the spectrum, it can be seen that copper exists in two valence states, Cu+ and Cu2+, and manganese exists in the form of spin-orbit peak splitting between the Mn2p 3 / 2 and Mn2p 1 / 2 peaks, confirming that the prepared nanomotor has the ability to catalyze hydrogen peroxide.
[0063] like Figure 5 Shown are the UV-visible spectra and infrared absorption spectra of the nanomotor loaded with DSF, proving that DSF forms metal chelate complexes with copper and manganese on the surface of the nanomotor nanoparticles.
[0064] like Figure 6 Shown are the kinetic curves of DSF release from HM-CuD@J nanomotor, proving that the prepared nanomotor has excellent DSF sustained-release ability in an environment containing H2O2 as the material disintegrates; kinetics of DSF release from HM-CuD@J nanomotor; (A) DSF sustained-release from HM-CuD@J under 0mM and 200mM H2O2 conditions; (B) DSF sustained-release from four Janus nanomotors under 200mM H2O2 conditions.
[0065] like Figure 7 The figure shows the degradation curve of Janus nanomotor. The sustained release curves of copper ions, manganese ions, and silicon ions prove that the nanomotor has good degradation ability under the condition of H2O2. At the same time, the release of copper ions also provides conditions for inducing copper death of hypertrophic scars.
[0066] like Figure 8 The figure shows the oxygen concentration curves of the four nanomotors under 10 mM H2O2 conditions. It proves that the prepared M-CuD@J and HM-CuD@J nanomotors have the ability to catalyze the decomposition of hydrogen peroxide to produce oxygen.
[0067] like Fig. 9 As shown, the movement tracking of the four prepared nanomotors CuD@J, H-CuD@J, Mn-CuD@J, and HMn-CuD@J in 200mMH2O2+0.1% HA solution (10mg / ml) was performed. Under the action of the dual-power engine, HM-CuD@J traveled a longer displacement and moved faster in the same time.
[0068] like Fig.10As shown in the figure, the uptake of different materials by HSF was investigated by fluorescence imaging; first, HSF was spread in a 24-well plate, and sealed with hyaluronic acid gel after adherence; RhB-labeled CuD@J, M-CuD@J, H-CuD@J and HM-CuD@J were synthesized, and then different materials and HSF were co-cultured in a 37-degree incubator for 6 hours. Finally, the uptake of different materials by cells was observed under a fluorescence microscope. In the same period of time, HSF took up the most HM-CuD@J and had the strongest fluorescence intensity; this was due to the enzymatic reaction between HAase and HA to generate power, and Mn consumed H2O2 to generate O2 power. The dual power engine caused HSF to internalize the most HM-CuD@J.
[0069] like Fig.11 As shown, the effects of powered drug-free nanomotor HM@J, unpowered drug-containing nanomotor CuD@J and powered drug-containing nanomotor HM-CuD@J on the activity of HSF (human hypertrophic scar fibroblasts) were tested by CCK8. It can be seen that HM-CuD@J has the best HSF killing ability; this proves that a simple powered nanomotor carrier has no killing effect on HSF, while a simple drug has a certain killing effect on HSF, but the powered and drug-containing nanomotor has the best HSF killing effect.
[0070] like Fig.12 As shown in the figure, after different materials were co-cultured with HSF for 12 hours, the protein of HSF was extracted and tested by WB. It was found that the DLAT, LIAS, SDHB, and FDX1 of the cells in the HM-CuD@J material group were significantly downregulated, which once again proved that HSF had serious copper death. And HIF1a was also downregulated in the HM@J group and the HM-CuD@J group. This is because Mn catalyzes H2O2 to produce O2, which effectively alleviates cell hypoxia. In addition, JC-1 staining showed that the mitochondrial membrane potential of the HM-CuD@J material group decreased the most, and HPF staining showed that the HM-CuD@J material group produced the most OH reactive oxygen.
[0071] like Fig.13 As shown in the figure, HM@J has no anti-scarring effect, and the scar degree of rabbit ears is similar to that of the PBS group. The CuD@J group has a certain anti-scarring effect, but the effect is not good. There are still scars that are clearly visible to the naked eye after the fourth week. The anti-scarring effect of HM-CuD@J is the most obvious. After four weeks of treatment, the scars almost disappeared.
[0072] The present invention has the following beneficial effects: the motor size of the present invention is basically between 300-400nm, presenting a monodisperse state, and the loaded copper ions and manganese ions are only dispersed to the Janus rod tail, wherein the copper is Cu + and Cu 2+It exists in two valence states, and manganese splits as a spin-orbit peak between the Mn2p 3 / 2 and Mn2p 1 / 2 peaks, and has the ability to catalyze hydrogen peroxide. DSF forms a metal chelate complex with copper and manganese on the surface of nanomotor nanoparticles, has excellent DSF sustained-release ability, can induce copper death in hypertrophic scars, and has the best HSF lethality. Since Mn can consume H2O2 to produce O2, it is beneficial to alleviate cell hypoxia.
[0073] The above is only an embodiment of the present invention, and the common knowledge such as the known specific technical solutions or characteristics in the solution is not described in detail here. It should be pointed out that for those skilled in the art, without departing from the solution of the present invention, several modifications and improvements can be made, which should also be regarded as the protection scope of the present invention, and these will not affect the effect of the present invention and the practicality of the patent. The scope of protection required by this application shall be based on the content of its claims, and the specific implementation methods and other records in the specification can be used to interpret the content of the claims.
Claims
1. A nanomotor for inducing copper death in hypertrophic scars and a preparation method thereof, characterized in that: The method comprises: S1: Synthesis of spherical mesoporous organosilica nanoparticles by hexadecyltrimethylammonium bromide and diethane; S2: adding the spherical mesoporous organosilicon nanoparticles to a mixture of deionized water, ethanol, and hexadecyltrimethylammonium bromide, subjecting the mixture to ultrasonic and stirring treatment, and then adding tetraethyl orthosilicate to react, thereby obtaining Janus silica nanoparticles; S3: dispersing the Janus silica nanoparticles in deionized water to obtain a Janus silica nanoparticle solution, adding a Cu(NO3)2 precursor to the Janus silica nanoparticle solution and stirring, then adding hexamethylenetetramine to the Janus silica nanoparticle solution to which the Cu(NO3)2 precursor has been added to catalyze the hydrolysis of Cu(NO3)2, and finally centrifuging to collect the centrifuge to obtain copper-loaded Janus silica nanoparticles; S4: dispersing the copper-loaded Janus silica nanoparticles into deionized water to obtain a Cu-containing Janus silica nanoparticle solution, adding a MnCl2 precursor to the Cu-containing Janus silica nanoparticle solution and stirring, then adding hexamethylenetetramine to catalyze the hydrolysis of the MnCl2 precursor, and collecting to obtain Janus silica nanoparticles M-Cu@J containing Cu and Mn; S5: preparing the M-Cu@J into an M-Cu@J ethanol suspension, adding 3-aminopropyltriethoxysilane to the M-Cu@J ethanol suspension, and performing a reaction centrifugation treatment, and washing with water and ethanol for several times to obtain an amino-functionalized M-Cu@J nanomotor; S6: the copper-loaded Janus silica nanoparticles, the copper-loaded Janus silica nanoparticles and the amino-functionalized M-Cu@J nanomotor are separated into anhydrous ethanol to obtain a M-Cu@J nanoparticle solution, tetraethylthiuram disulfide is added to the M-Cu@J nanoparticle solution, and then freeze-dried to obtain a DSF-loaded M-CuD@J nanomotor; S7: Dissolve EDC and NHS in PBS, add hyaluronidase to react at room temperature to obtain an activated hyaluronidase solution; then add the DSF-loaded M-CuD@J nanomotor to the activated hyaluronidase solution, stir and centrifuge, collect the centrifuge, and obtain the HM-CuD@J nanomotor.
2. A nanomotor for inducing copper death of hypertrophic scar and a preparation method thereof according to claim 1, characterized in that: The step of synthesizing spherical mesoporous organosilicon nanoparticles by using hexadecyltrimethylammonium bromide and diethane comprises: dispersing hexadecyltrimethylammonium bromide in a mixed solution comprising deionized water and ethanol to obtain a first solution; adding an aqueous ammonia solution to the first solution under continuous stirring to obtain a dispersion; Diethane was added to the dispersion, and the mixture was reacted for 12 hours. The mixture was then centrifuged at 9000 rpm for 10 minutes. The centrifuged product was collected and washed with water and ethanol for several times to obtain spherical mesoporous organosilicon nanoparticles.
3. A nanomotor for inducing copper death of hypertrophic scars and a preparation method thereof according to claim 2, characterized in that: The step of adding the spherical mesoporous organosilicon nanoparticles to a mixture of deionized water, ethanol, and hexadecyltrimethylammonium bromide, subjecting the mixture to ultrasonic and stirring treatment, and then adding tetraethyl orthosilicate to react to obtain Janus silica nanoparticles comprises: adding the spherical mesoporous organosilicon nanoparticle powder into a mixture containing deionized water, ethanol and hexadecyltrimethylammonium bromide to obtain a second solution; The second solution is subjected to ultrasonic treatment, and then an aqueous ammonia solution is added and stirred; Tetraethyl orthosilicate was added to the second solution after adding the ammonia solution. After reacting for 2 hours, the solution was centrifuged at 9000 rpm for 10 minutes. The centrifuged product was collected to obtain Janus silica nanoparticles, which were then washed with water and ethanol several times.
4. The nanomotor for inducing copper death of hypertrophic scar and the preparation method thereof according to claim 1, characterized in that: The steps of dispersing the Janus silica nanoparticles in deionized water to obtain a Janus silica nanoparticle solution, and adding a Cu(NO3)2 precursor to the Janus silica nanoparticle solution and stirring the solution include: Dispersing the Janus silica nanoparticles in deionized water to prepare a Janus silica nanoparticle solution with a concentration of 1 mg / ml; Cu(NO3)2 precursor was added to the Janus silica nanoparticle solution and stirred for 30 minutes.
5. The nanomotor for inducing copper death of hypertrophic scar and the preparation method thereof according to claim 4, characterized in that: The step of adding hexamethylenetetramine to the Janus silica nanoparticle solution to which the Cu(NO3)2 precursor has been added to catalyze the hydrolysis of Cu(NO3)2, and finally centrifuging to collect the centrifuge, is the step of preparing the copper-loaded Janus silica nanoparticles, comprising: After adding hexamethylenetetramine to the Janus silica nanoparticle solution to which Cu(NO3)2 precursor was added to catalyze the hydrolysis of Cu(NO3)2, the mixture was reacted in an 85°C oil bath for 10 hours, centrifuged at 9000 rpm for 10 minutes, and the centrifuged product was collected as copper-loaded Janus silica nanoparticles, which were washed several times with water and ethanol.
6. The nanomotor for inducing copper death of hypertrophic scar and the preparation method thereof according to claim 1, characterized in that: The steps of dispersing the copper-loaded Janus silica nanoparticles into deionized water to obtain a Cu-containing Janus silica nanoparticle solution, adding a MnCl2 precursor to the Cu-containing Janus silica nanoparticle solution and stirring, then adding hexamethylenetetramine to catalyze the hydrolysis of the MnCl2 precursor, and collecting to obtain Janus silica nanoparticles M-Cu@J containing Cu and Mn, include: Dispersing the copper-loaded Janus silica nanoparticles in deionized water to a concentration of 1 mg / ml to obtain a Cu-containing Janus silica nanoparticle solution; Adding a MnCl2 precursor to the Cu-containing Janus silica nanoparticle solution and stirring for 30 minutes to obtain a third solution; Hexamethylenetetramine was added to the third solution to catalyze the hydrolysis of MnCl2, and then the solution was reacted in an oil bath at 85°C for 10 hours. The solution was centrifuged at 9000 rpm for 5 minutes, and the centrifuge was collected to obtain Janus silica nanoparticles M-Cu@J containing Cu and Mn, which were washed with water and ethanol several times.
7. A nanomotor for inducing copper death of hypertrophic scar and a preparation method thereof according to claim 6, characterized in that: The step of preparing the M-Cu@J into an M-Cu@J ethanol suspension, adding 3-aminopropyltriethoxysilane to the M-Cu@J ethanol suspension, performing a reaction centrifugal treatment, and washing with water and ethanol for several times to obtain an amino-functionalized M-Cu@J nanomotor comprises: The M-Cu@J is prepared into an M-Cu@J ethanol suspension with a concentration of 10 mg / ml; Adding 3-aminopropyltriethoxysilane to the M-Cu@J ethanol suspension for reaction, wherein the ratio of the M-Cu@J ethanol suspension to 3-aminopropyltriethoxysilane is 100:1; the reaction conditions are to react in a water bath at 35° C. for 10 hours to obtain a fourth solution; Then, the fourth solution was centrifuged at 9000 rpm for 10 min, the centrifuged product was collected, and washed with water and ethanol several times to obtain amino-functionalized M-Cu@J nanomotors.
8. The nanomotor for inducing copper death of hypertrophic scar and the preparation method thereof according to claim 7, characterized in that: The step of separating the copper-loaded Janus silica nanoparticles, the copper-loaded Janus silica nanoparticles and the amino-functionalized M-Cu@J nanomotor into anhydrous ethanol to obtain a M-Cu@J nanoparticle solution, adding tetraethylthiuram disulfide to the M-Cu@J nanoparticle solution, and then freeze-drying to obtain a DSF-loaded M-CuD@J nanomotor comprises: The copper-loaded Janus silica nanoparticles, the copper-loaded Janus silica nanoparticles and the amino-functionalized M-Cu@J nanomotor are separated into anhydrous ethanol to prepare a M-Cu@J nanoparticle solution with a concentration of 11 mg / ml; Adding tetraethylthiuram disulfide to the M-Cu@J nanoparticle solution and stirring at room temperature for 10 hours to obtain a fifth solution; The fifth solution was centrifuged at 9000 rpm for 10 min, the centrifuged product was collected, and washed with water and ethanol 2-3 times to obtain M-CuD@J nanoparticles; The obtained M-CuD@J nanoparticles were then freeze-dried.
9. The nanomotor for inducing copper death of hypertrophic scar and the preparation method thereof according to claim 8, characterized in that: The steps of dissolving EDC and NHS in PBS, adding hyaluronidase to react at room temperature to obtain an activated hyaluronidase solution; then adding the DSF-loaded M-CuD@J nanomotor to the activated hyaluronidase solution, stirring, centrifuging, and collecting the centrifuged product to obtain the HM-CuD@J nanomotor include: Dissolve EDC and NHS in PBS, add hyaluronidase and react at room temperature for 2 hours to obtain an activated hyaluronidase solution; Adding the DSF-loaded M-CuD@J nanomotor to the activated hyaluronidase solution and reacting for 4 hours under stirring to obtain a sixth solution; The sixth solution was centrifuged at 9000 rpm for 10 min, and the centrifuged material was collected to obtain the HM-CuD@J nanomotor.
10. The nanomotor for inducing copper death of hypertrophic scar and the preparation method thereof according to claim 9, characterized in that: The ratio of EDC, NHS and hyaluronidase is 30:40:2.
Citation Information
Cited By
Morphology-controllable mesoporous copper-based nano material and preparation method thereof
CN122424813A