Resistance heating film and method for adjusting resistance of resistance heating film

By dividing the cell areas in the functional area of ​​the resistance heating film and opening resistance adjustment holes, the problem that the resistance heating film is difficult to meet different working conditions under the rated voltage is solved, and flexible resistance adjustment and heating uniformity are achieved, which simplifies the Process.

CN119155828APending Publication Date: 2024-12-17SONGSHAN LAKE MATERIALS LAB
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411437023.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-15
Publication Date
2024-12-17

AI Technical Summary

Technical Problem

The resistance after the resistance heating film is formed is basically determined, and it is difficult to meet the heating power requirements of different working conditions under the rated voltage. The existing adjustment methods increase the difficulty and complexity of the process.

Method used

By dividing the functional area of ​​the resistive heating film into multiple cell areas, and opening resistance adjustment holes in each cell area, the unitary idea is used to adjust the cell cell form square resistance, reduce the film area between electrodes, and realize resistance adjustment. Laser cutting is used to reduce process difficulty and complexity.

Benefits of technology

The same resistance heating film is achieved at the rated voltage to meet the requirements of different working conditions, improve the heating uniformity and resistance uniformity of the resistance heating film, and reduce manufacturing defects and production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119155828A_ABST
    Figure CN119155828A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of resistance heating films, and discloses a resistance heating film and a method for adjusting the resistance of the resistance heating film, and the resistance heating film comprises a positive electrode, a negative electrode and a functional area; the positive electrode and the negative electrode are oppositely arranged, the functional area is located between the positive electrode and the negative electrode, the functional area comprises a plurality of cellular areas, and each cellular area is provided with at least one resistance adjusting hole. According to the invention, the functional area is divided into a plurality of cellular areas, each cellular area is provided with a hole, and the area of the film between the electrodes is reduced, so that a low-sheet-resistance resistance heating film is adjusted to be a high-sheet-resistance resistance heating film, and the same resistance heating film can meet the requirements of different working conditions under rated voltage. In addition, trepanning can be achieved through laser cutting, and the process difficulty and the manufacturing complexity are low.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of resistance heating films, and in particular to a resistance heating film and a method for adjusting the resistance of the resistance heating film. Background Art

[0002] The resistance heating film is a flexible film material that can generate heat when powered on and can be applied to different scenarios and structural surfaces. For example, the resistance heating film can be set in the battery accessories of smartphones to ensure the normal operating temperature of the battery in low temperature environments, thereby improving the charging and discharging efficiency and service life of the battery.

[0003] Different products or the same product at different stages of use may have different requirements for the speed or amount of heat generation. For example, in smartphone battery heating, when the battery is in an extremely cold state and needs to be heated quickly, a resistance heating film with a lower resistance is required to achieve high-power heating; when the battery temperature is close to the normal operating range, the power needs to be reduced. However, the resistance of the resistance heating film is basically determined after it is formed. Therefore, the heating power of the same resistance heating film is difficult to meet the requirements under different working conditions at the rated voltage.

[0004] Currently, the initial square resistance (or initial resistance) of the resistance heating film can be changed by adjusting the surface square resistance of the resistance heating film (for example, etching in the thickness direction of the resistance heating film). However, this method increases the process difficulty and complexity of production. Summary of the invention

[0005] In view of this, the present invention provides a resistance heating film and a method for adjusting the resistance of the resistance heating film, so that the same resistance heating film can meet the requirements of different working conditions under rated voltage with lower process difficulty.

[0006] In the first aspect, the present invention provides a resistive heating film, which includes a positive electrode, a negative electrode and a functional area; the positive electrode and the negative electrode are arranged opposite to each other, the functional area is located between the positive electrode and the negative electrode, the functional area includes a plurality of cell areas, and the cell area is provided with at least one resistance adjustment hole.

[0007] The resistance heating film provided by the present invention extends the adjustment of the unit cell form square resistance to the adjustment of the resistance heating film through the integration concept, and opens a resistance adjustment hole in each unit cell area of ​​the functional area, which can reduce the area of ​​the film between the electrodes, and then adjust the low square resistance resistance heating film to a high square resistance resistance heating film, so that the same resistance heating film can meet the requirements of different working conditions under the rated voltage. Moreover, the opening can be achieved by laser cutting, and the process difficulty and manufacturing complexity are relatively low.

[0008] In an optional implementation, a plurality of resistance adjustment holes are arranged in a matrix form.

[0009] In an optional implementation, the shape of the cell region and the shape of the resistance adjustment hole are both square, the number of the resistance adjustment hole in the cell region is one, and the side length of the cell region and the spacing between two adjacent resistance adjustment holes are determined by the following formula:

[0010]

[0011] Among them, a represents the side length of the cell area, b represents the distance between two adjacent resistance adjustment holes, α represents the linear relationship between the square resistance before and after adjustment, R l0 Represents the initial square resistance of the functional area, R li represents the target square resistance of the functional area, β represents the opening limit, and γ represents the test constant.

[0012] In an optional implementation, the target square resistance ranges from 1 times to 10 times the initial square resistance.

[0013] In an optional implementation, the side length of the cell region ranges from 1.5 mm to 5 mm.

[0014] In this embodiment, the side length range of the cell area is limited to 1.5 mm to 5 mm. The square cells are arranged relatively regularly on the plane, which can better ensure the heating uniformity of the resistive heating film. Moreover, this range makes it easier to ensure the shape and size accuracy of the cells during the manufacturing process, reduce manufacturing defects, and improve production efficiency and product quality.

[0015] In an optional implementation, the shape of the cell region is triangular or hexagonal, and the shape of the resistance adjustment hole is triangular or hexagonal.

[0016] In an optional implementation, when the shape of the resistance adjustment hole is triangular, the number of the resistance adjustment holes in the cell region is at least two.

[0017] In this embodiment, two or more triangular resistance adjustment holes are provided in the cell region, so that the current distribution in the cell region can be more uniform, thereby improving the uniformity of the resistance of the resistance heating film after adjustment.

[0018] In an optional embodiment, the material of the resistive heating film includes one or more of nickel, chromium, copper, graphene, graphite and carbon conductive ink.

[0019] In a second aspect, the present invention provides a method for adjusting the resistance of a resistance heating film, the method comprising: obtaining an initial square resistance and a target square resistance of an original resistance heating film; based on the initial square resistance and the target square resistance, determining the size of a cell region, the spacing between resistance adjustment holes in two adjacent cell regions, and the size of the resistance adjustment holes, wherein the original resistance heating film comprises a functional area, the functional area comprises a plurality of cell regions, and the cell region is provided with at least one resistance adjustment hole; based on the size of the cell region, the spacing between resistance adjustment holes in two adjacent cell regions, and the size of the resistance adjustment holes, determining a processing layout, wherein the processing layout is used to characterize the positions of the plurality of resistance adjustment holes in the functional area; based on the processing layout, controlling a laser cutting device to form a plurality of resistance adjustment holes on the original resistance heating film, to obtain the resistance heating film of the first aspect or any corresponding embodiment thereof.

[0020] In an optional embodiment, before obtaining the initial square resistance and the target square resistance of the original resistance heating film, the method further includes: determining the initial square resistance of the original resistance heating film by a square resistance tester. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the specific embodiments of the present invention or the technical solutions in the related technologies, the drawings required for use in the specific embodiments or the related technical descriptions will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0022] Figure 1 is a schematic structural diagram of a resistance heating film according to an embodiment of the present invention;

[0023] Figure 2 is a schematic structural diagram of another resistance heating film according to an embodiment of the present invention;

[0024] Figure 3 is a schematic diagram of a cell region and a resistance adjustment hole according to an embodiment of the present invention;

[0025] Figure 4 is a schematic diagram of another cell region and a resistance adjustment hole according to an embodiment of the present invention;

[0026] Figure 5 is a schematic diagram of another cell region and a resistance adjustment hole according to an embodiment of the present invention;

[0027] Figure 6 is a schematic structural diagram of an original resistance heating film according to an embodiment of the present invention;

[0028] Figure 7is a schematic diagram of the positional relationship between a cell region and a functional region according to an embodiment of the present invention;

[0029] Figure 8 4 is a flow chart of a method for adjusting the resistance of a resistance heating film according to an embodiment of the present invention.

[0030] Attached figure numerals: 110, positive electrode; 120, negative electrode; 130, functional area; 131, cell area; 132, resistance adjustment hole. DETAILED DESCRIPTION

[0031] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.

[0032] The resistance heating film has good flexibility and can be applied to different scenarios and structural surfaces. For example, the resistance heating film can be installed inside the car seat. In cold weather, by energizing the resistance heating film, the seat surface can be quickly heated up, providing a warm and comfortable riding experience for the driver and passengers.

[0033] For another example, the resistance heating film can be attached to the surface of the rearview mirror, and the fog and frost can be quickly eliminated by heating, ensuring that the driver can clearly see the situation behind and improving driving safety. The resistance heating film can also be set on wearable devices such as smart watches and smart bracelets to provide warmth for the wearer's wrist in cold weather and improve the user experience. The resistance heating film can also be attached to the surface of the aircraft wing, and the wing can be heated by electricity to prevent ice from forming on it, ensuring the normal flight of the aircraft.

[0034] After the resistance heating film is formed, the resistance is basically determined. Therefore, the heating power of the same resistance heating film is difficult to meet the requirements under different working conditions at a given rated voltage. The production of resistance heating films with different resistances puts forward more standards for process requirements. On the resistance heating film with the same square resistance, resistance heating films with different resistances are obtained through subsequent processing. This is the key to solving the problem that the same resistance heating film meets the requirements of different working conditions at a rated voltage.

[0035] In view of this, the present invention provides a resistance heating film, which divides the functional area into multiple cell areas, and opens holes in each cell area to reduce the area of ​​the film between the electrodes, thereby adjusting the low-square-resistance resistance heating film to a high-square-resistance resistance heating film, so that the same resistance heating film can meet the requirements of different working conditions under the rated voltage. Moreover, the opening of the holes can be achieved by laser cutting, and the process difficulty and manufacturing complexity are relatively low.

[0036] The resistance heating film provided by the present invention is described in detail below with reference to the accompanying drawings.

[0037] For example, Figure 1 and Figure 2 As shown, the resistive heating film includes a positive electrode 110 , a negative electrode 120 and a functional region 130 .

[0038] The positive electrode 110 and the negative electrode 120 are arranged opposite to each other, the functional area 130 is located between the positive electrode 110 and the negative electrode 120 , and the functional area 130 is divided into a plurality of cell areas 131 , each of which is provided with at least one resistance adjustment hole 132 .

[0039] During operation, the positive electrode 110, the negative electrode 120 and the functional area 130 form a closed loop, and the functional area 130 has a heating effect after current is passed through it. The present invention adjusts the square resistance of the functional area by opening holes, thereby adjusting the resistance of the resistance heating film.

[0040] Specifically, the cell region 131 is a basic unit for constructing a resistive heating film structure, and is arranged and combined on the plane of the functional region 130 according to a preset rule to form a surface structure of the functional region. Figure 2 As shown, the plurality of cell regions 131 are distributed in a matrix form, and two adjacent cell regions 131 are connected to each other, that is, there is no gap between two adjacent cell regions 131 .

[0041] The cell region 131 is the basis for realizing surface resistance adjustment. The surface resistance is related to the electrical characteristics of the cell region 131. By setting the resistance adjustment hole 132 in the cell region 131, the conductive path in the cell region 131 can be changed, which is equivalent to changing the effective cross-sectional area of ​​the conductive material. The change in the cross-sectional area will cause the change in resistance, thereby realizing the adjustment of the resistance and achieving the purpose of changing the resistance of the resistance heating film.

[0042] Specifically, according to the basic theoretical formula of resistance, the resistance value of the resistor is proportional to the distance between the electrodes and inversely proportional to the cross-sectional area of ​​the resistor. In other words, when other factors such as the cross-sectional area remain unchanged, the larger the distance between the electrodes, the larger the resistance value of the resistor; when other factors such as the distance between the electrodes remain unchanged, the smaller the cross-sectional area, the larger the resistance value of the resistor. Therefore, based on the low-square-resistance resistive heating film, the area of ​​the film between the electrodes can be reduced by graphically processing (opening holes) the film, thereby increasing the overall resistance of the resistive heating film.

[0043] The resistance heating film provided by the present invention extends the adjustment of the unit cell form square resistance to the adjustment of the resistance heating film through the integration concept, and opens a resistance adjustment hole in each unit cell area of ​​the functional area, which can reduce the area of ​​the film between the electrodes, and then adjust the low square resistance resistance heating film to a high square resistance resistance heating film, so that the same resistance heating film can meet the requirements of different working conditions under the rated voltage. Moreover, the opening can be achieved by laser cutting, and the process difficulty and manufacturing complexity are relatively low.

[0044] The present embodiment does not limit the shape of the cell region 131 and the shape of the resistance adjustment hole 132. For example, the shape of the cell region 131 may be as follows: Figure 3 As shown, it is a square, but it can also be Figure 4 As shown in the figure, it is a triangle, and it can also be Figure 5 Correspondingly, the resistance adjustment hole 132 can also be as shown in FIG. Figure 3 As shown in square Figure 4 As shown in triangle or Figure 5 Shown as a hexagon.

[0045] When resistance adjustment holes 132 of different shapes or sizes are opened in cell regions 131 of different shapes and sizes, factors such as the internal current path length and cross-sectional area are different, and the degree of influence on the adjustment resistance is different. The shape and size of the cell region 131 and the resistance adjustment hole 132 can be selected by the designer according to the needs.

[0046] Specifically, when the shape of the resistance adjustment hole is triangular, the number of resistance adjustment holes in the cell region is at least two. A single triangular resistance adjustment hole may cause a great change in the local current density in the cell region, resulting in uneven resistance distribution. When there are at least two triangular resistance adjustment holes, these resistance adjustment holes can be reasonably arranged (such as symmetrically arranged) to make the current distribution in the cell region more uniform, thereby improving the uniformity of the resistance of the resistance heating film after adjustment.

[0047] The following takes the case where the shape of the cell region and the shape of the resistance adjustment hole are both square as an example to explain the size of the cell region and the size of the resistance adjustment hole in the functional area.

[0048] Specifically, Figure 1 and Figure 2 As shown, the shape of the cell region 131 and the shape of the resistance adjustment hole 132 are both square, the number of the resistance adjustment hole 132 in the cell region 131 is one, and the multiple resistance adjustment holes are arranged in a matrix form. The side length of the cell region 131 and the distance between two adjacent resistance adjustment holes are determined by formula (1).

[0049]

[0050] Wherein, α represents the side length of the cell region 131, b represents the spacing between two adjacent resistance adjustment holes, and α represents the linear relationship between the square resistance before and after adjustment. α can be determined by testing. l0 Represents the initial square resistance of the functional area, R li It represents the target resistance of the functional area, β represents the opening limit, which can be determined by testing, and γ represents the test constant, which can be determined by fitting the test data.

[0051] Specifically, the initial square resistance R of the resistance heating film l0 Refers to the actual square resistance of the resistance heating film before the hole is opened. The actual square resistance of the resistance heating film before the hole is opened can be determined by a square resistance tester. li It refers to the square resistance that needs to be achieved after the resistance heating film is opened. The target square resistance can be determined by the designer according to actual needs.

[0052] Exemplarily, the target square resistance may range from 1 times to 10 times the initial square resistance. For example, the target square resistance may be 1 times, 2.5 times, 4 times, 6 times, 8 times, or 10 times the initial square resistance.

[0053] In some embodiments, the side length of the cellular region 131 can range from 1.5 mm to 5 mm, that is, the side length of the cellular region 131 can be any value between 1.5 mm and 5 mm, for example, the side length of the cellular region 131 is 1.5 mm, 2 mm, 2.5 mm, 4 mm or 5 mm.

[0054] In this embodiment, the side length of the cell region 131 is limited to a range of 1.5 mm to 5 mm. The square cells are arranged relatively regularly on the plane, which can better ensure the heating uniformity of the resistive heating film. Moreover, this range makes it easier to ensure the shape and size accuracy of the cells during the manufacturing process, reduce manufacturing defects, and improve production efficiency and product quality.

[0055] For example, the side length of the cell region 131 may be Figure 3As shown in a, the spacing between two adjacent resistance adjustment holes can be Figure 3 As shown in b, if the center of the resistance adjustment hole 132 coincides with the center of the cell region, the side length of the resistance adjustment hole is (ab).

[0056] Specifically, after the side length of the cell region 131 is determined, the number of the cell regions 131 in the length direction of the functional area, that is, the number of the cell regions in each row, can be determined according to formula (2).

[0057]

[0058] Among them, S L represents the number of cell regions 131 distributed in the length direction, L represents the length of the functional area, and the length of the functional area can be as follows: Figure 6 L shown.

[0059] Specifically, if the dimension L in the length direction cannot be divided by the side length a of the cell region 131, the quotient is determined as the number of cell regions 131 distributed in the length direction, and the length obtained by dividing the remainder in half is set on both sides of the two cell regions 131 at the edge in the length direction. Figure 7 As shown, the sum of the first length L1 and the second length L2 is the remainder of (L÷a).

[0060] After the side length of the cell region 131 is determined, the number of the cell regions 131 in the width direction of the functional area, that is, the number of the cell regions in each column, can be determined according to formula (3).

[0061]

[0062] Among them, S W represents the number of cell regions 131 in the width direction, W represents the length of the functional area, and the width of the functional area can be as follows: Figure 6 W shown.

[0063] Specifically, if the dimension W in the width direction cannot be divided by the side length a of the cell region 131, the quotient is determined as the number of cell regions 131 distributed in the width direction, and the length obtained by dividing the remainder in half is set on both sides of the two cell regions 131 at the edge in the width direction. Figure 7 As shown, the sum of the first width W1 and the second width W2 is the remainder of (W÷a).

[0064] After the target square resistance is determined, the resistance of the resistance heating film can be determined according to formula (4).

[0065]

[0066] Wherein, R represents the resistance of the resistance heating film after the hole is opened.

[0067] The present invention does not limit the type of resistance heating film. For example, the resistance heating film can be a metal heating film, in which case the material of the resistance heating film includes one or more of nickel, chromium or copper; the resistance heating film can also be a carbon material system heating film, in which case the material of the resistance heating film includes one or more of graphene, graphite and carbon conductive ink.

[0068] In this embodiment, a method for adjusting the resistance of a resistance heating film is also provided, which can be used for adjusting the resistance of a resistance heating film. The device for adjusting the resistance of the resistance heating film can be a computer or a tablet computer, etc. Figure 8 FIG. 1 is a schematic diagram of a process for adjusting the resistance of a resistance heating film according to an embodiment of the present invention. Figure 8 As shown, the method comprises the following steps:

[0069] Step S801, obtaining the initial square resistance and target square resistance of the original resistance heating film.

[0070] Specifically, Figure 6 As shown, the original resistance heating film can be a resistance heating film without holes.

[0071] Exemplarily, the initial square resistance of the original resistance heating film can be determined by a square resistance tester, and the square resistance uniformity of the original resistance heating film is within ±5%.

[0072] Exemplarily, the target square resistance can be determined by the staff according to the needs, and the initial square resistance and the target square resistance can be input by the user through a human-computer interaction device (such as a mouse, keyboard or touch screen, etc.) into the device for adjusting the resistance of the resistance heating film, so that the device for adjusting the resistance of the resistance heating film can obtain the initial square resistance and the target square resistance.

[0073] Step S802 : determining the size of the cell region, the spacing between the resistance adjustment holes in two adjacent cell regions, and the size of the resistance adjustment holes based on the initial square resistance and the target square resistance.

[0074] The original resistance heating film includes a functional area, the functional area includes a plurality of cellular areas, and the cellular area is provided with at least one resistance adjustment hole.

[0075] Specifically, when the shape of the cell region and the shape of the resistance adjustment hole are square, after determining the initial square resistance and the target square resistance, the size of the cell region and the spacing between the resistance adjustment holes in two adjacent cell regions can be determined by the above formula (1). The side length of the cell region ranges from 1.5 mm to 5 mm.

[0076] If the shape of the cell region and the shape of the resistance adjustment hole are square, and the center of the cell region coincides with the center of the resistance adjustment hole, then the size of the resistance adjustment hole is (ab).

[0077] Step S803 , determining a processing layout based on the size of the cell region, the spacing between the resistance adjustment holes in two adjacent cell regions, and the size of the resistance adjustment holes.

[0078] The processing layout is used to characterize the positions of multiple resistance adjustment holes in the functional area.

[0079] Specifically, after determining the size of the cell region, the spacing between the resistance adjustment holes in two adjacent cell regions, and the size of the resistance adjustment holes, the number of cell regions in each row can be determined based on formula (2), and the number of cell regions in each column can be determined based on formula (3). Then, based on the spacing between the resistance adjustment holes in two adjacent cell regions and the size of the resistance adjustment holes, the positions of multiple resistance adjustment holes can be set to obtain a processing layout.

[0080] For example, the processing layout can be determined by two-dimensional drawing software (such as CAD, etc.), and the processing layout can be as follows: Figure 1 Specifically, in CAD, the processing layout can be obtained by taking the functional area as the boundary and performing operations such as offset and array according to the size of the cell area.

[0081] The resistance of the resistance heating film after the hole is opened can be determined by formula (4). The square resistance R of the resistance heating film after the hole is opened li Greater than the square resistance R of the resistance heating film before opening l0 , that is, R li >R l0 Accordingly, the resistance of the resistance heating film after the holes are opened is greater than the resistance of the resistance heating film before the holes are opened.

[0082] Step S804, based on the processing layout, controlling the laser cutting device to form a plurality of resistance adjustment holes on the original resistance heating film to obtain the resistance heating film.

[0083] The resistance heating film is the resistance heating film provided by any of the above embodiments.

[0084] Specifically, after determining the processing layout, a laser processing path can be generated, and then the laser cutting device can be controlled to move along the laser processing path to cut holes in the functional area. Figure 1 The resistance heating film shown is to convert the original resistance heating film into a resistance heating film.

[0085] During the cutting process, the product shape remains consistent with the designed shape, and the size difference between the processing layout and the actual product during the cutting process does not exceed the tolerance range of 0.5×b.

[0086] The method for adjusting the resistance of the resistive heating film provided in this embodiment is based on the idea of ​​integration and applies the unit cell square resistance adjustment to the thin film material square resistance adjustment. By opening holes in the unit cell region, not only the square resistance of the thin film material can be fine-tuned, but also the low square resistance film can be adjusted to a high square resistance film. The resistance adjustment range can reach 1000% of the original square resistance, or even higher.

[0087] After the sheet resistance of the thin film material is adjusted, the data is more accurate. Under ideal manufacturing process and cutting environment, the error between the adjusted sheet resistance and the theoretical value is within 5%.

[0088] The embodiment of the present invention also provides a computer device, which includes: one or more processors, a memory, and an interface for connecting various components, including a high-speed interface and a low-speed interface. The various components are connected to each other using different buses for communication, and can be installed on a common mainboard or installed in other ways as needed. The processor can process instructions executed in the computer device, including instructions stored in or on the memory to display graphical information of a GUI on an external input / output device (such as a display device coupled to the interface). In some optional embodiments, if necessary, multiple processors and / or multiple buses can be used together with multiple memories and multiple memories. Similarly, multiple computer devices can be connected, and each device provides some necessary operations (for example, as a server array, a group of blade servers, or a multi-processor system).

[0089] The processor may be a central processing unit, a network processor or a combination thereof. The processor may further include a hardware chip. The hardware chip may be a dedicated integrated circuit, a programmable logic device or a combination thereof. The programmable logic device may be a complex programmable logic device, a field programmable gate array, a general purpose array logic or any combination thereof.

[0090] The memory stores instructions executable by at least one processor, so that the at least one processor executes the method shown in the above embodiment.

[0091] The memory may include a program storage area and a data storage area, wherein the program storage area may store an operating system, an application required for at least one function; the data storage area may store data created according to the use of the computer device, etc. In addition, the memory may include a high-speed random access memory, and may also include a non-transient memory, such as at least one disk storage device, a flash memory device, or other non-transient solid-state storage device. In some optional embodiments, the memory may optionally include a memory remotely arranged relative to the processor, and these remote memories may be connected to the computer device via a network. Examples of the above-mentioned network include, but are not limited to, the Internet, an intranet, a local area network, a mobile communication network, and combinations thereof.

[0092] The memory may include volatile memory, such as random access memory; the memory may also include non-volatile memory, such as flash memory, hard disk or solid state drive; the memory may also include a combination of the above types of memory.

[0093] The computer device also includes an input device and an output device. The processor, memory, input device and output device can be connected via a bus or other methods.

[0094] The input device can receive input digital or character information, and generate key signal input related to the user settings and function control of the computer device, such as a touch screen, a keypad, a mouse, a track pad, a touch pad, an indicator bar, one or more mouse buttons, a trackball, a joystick, etc. The output device may include a display device, an auxiliary lighting device (e.g., an LED) and a tactile feedback device (e.g., a vibration motor), etc. The above-mentioned display device includes but is not limited to a liquid crystal display, a light emitting diode, a display and a plasma display. In some optional embodiments, the display device may be a touch screen.

[0095] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0096] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0097] It should be understood that the various parts of the present invention can be implemented by hardware, software, firmware or a combination thereof. In the above-mentioned embodiments, a plurality of steps or methods can be implemented by software or firmware stored in a memory and executed by a suitable instruction execution system. For example, if implemented by hardware, as in another embodiment, it can be implemented by any one of the following technologies known in the art or their combination: a discrete logic circuit having a logic gate circuit for implementing a logic function for a data signal, a dedicated integrated circuit having a suitable combination of logic gate circuits, a programmable gate array (PGA), a field programmable gate array (FPGA), etc.

[0098] In the description of this specification, the description with reference to the terms "this embodiment", "one embodiment", "some embodiments", "example", "specific example", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, unless they are contradictory.

[0099] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0100] Although the embodiments of the present invention have been described in conjunction with the accompanying drawings, those skilled in the art may make various modifications and variations without departing from the spirit and scope of the present invention, and such modifications and variations are all within the scope defined by the present invention.

Claims

1. A resistance heating film, characterized in that: The resistance heating film includes a positive electrode, a negative electrode and a functional area; The positive electrode and the negative electrode are arranged opposite to each other, the functional area is located between the positive electrode and the negative electrode, the functional area includes a plurality of cell areas, and the cell area is provided with at least one resistance adjustment hole.

2. The resistance heating film according to claim 1, characterized in that: The plurality of resistance adjustment holes are arranged in a matrix form.

3. The resistance heating film according to claim 2, characterized in that: The shape of the cell region and the shape of the resistance adjustment hole are both square, the number of the resistance adjustment hole in the cell region is one, and the side length of the cell region and the spacing between two adjacent resistance adjustment holes are determined by the following formula: Wherein, a represents the side length of the cell region, b represents the distance between two adjacent resistance adjustment holes, α represents the linear relationship between the square resistance before and after adjustment, R l0 represents the initial square resistance of the functional area, R li represents the target resistance of the functional area, β represents the opening limit, and γ represents the test constant.

4. The resistance heating film according to claim 3, characterized in that: The target square resistance has a value range of 1 times to 10 times of the initial square resistance.

5. The resistance heating film according to any one of claims 1 to 4, characterized in that: The side length of the cell region ranges from 1.5 mm to 5 mm.

6. The resistance heating film according to claim 1 or 2, characterized in that: The shape of the cell region is triangular or hexagonal, and the shape of the resistance adjustment hole is triangular or hexagonal.

7. The resistance heating film according to claim 6, characterized in that: When the shape of the resistance adjusting hole is triangular, the number of the resistance adjusting holes in the cell region is at least two.

8. The resistance heating film according to any one of claims 1 to 4, characterized in that: The material of the resistive heating film includes one or more of nickel, chromium, copper, graphene, graphite and carbon conductive ink.

9. A method for adjusting the resistance of a resistance heating film, characterized in that: The method comprises: Obtaining the initial square resistance and target square resistance of the original resistance heating film; Based on the initial square resistance and the target square resistance, determining the size of the cell region, the spacing between the resistance adjustment holes in two adjacent cell regions, and the size of the resistance adjustment holes, wherein the original resistance heating film includes a functional area, the functional area includes a plurality of the cell regions, and the cell region is provided with at least one resistance adjustment hole; Determine a processing layout based on the size of the cell region, the spacing between the resistance adjustment holes in two adjacent cell regions, and the size of the resistance adjustment holes, wherein the processing layout is used to characterize the positions of the plurality of resistance adjustment holes in the functional area; Based on the processing layout, a laser cutting device is controlled to form a plurality of the resistance adjustment holes on the original resistance heating film, thereby obtaining the resistance heating film according to any one of claims 1 to 8.

10. The method according to claim 9, characterized in that Before obtaining the initial sheet resistance and the target sheet resistance of the original resistance heating film, the method further includes: The initial square resistance of the original resistance heating film is determined by a square resistance tester.

Citation Information

Cited By

  • Manufacturing method of multi-temperature-zone heating device

    CN120692696A