Phosphorus and fluorine removal agent and preparation method thereof

By using phosphorus removal and fluorine removal agents composed of calcium chloride, calcium oxide and activated magnesium oxide, the problems of high cost, poor defluorine removal and heavy pH influence in the prior art are solved, and high efficiency and simplicity are achieved , environmentally friendly phosphorus removal and fluorine removal effect.

CN119409298AActive Publication Date: 2025-02-11GUIZHOU ACAD OF ENVIRONMENTAL SCI & DESIGNING

Patent Information

Application Number
CN202411560797.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-04
Publication Date
2025-02-11
Estimated Expiration
2044-11-04

AI Technical Summary

Technical Problem

In the prior art, when treating phosphogypsum leachate, the manufacturing and use cost of phosphorus removal and fluorine removal agent is relatively high, the defluorination effect is poor, and it is greatly affected by pH, which may lead to secondary contamination.

Method used

Phosphorus removal agent composed of calcium chloride, calcium oxide and activated magnesium oxide is used, and the mass ratio is 1:2:7-12. The activated magnesium oxide can be replaced with activated alumina or hydroxyapatite. This agent can effectively remove fluoride ions under acidic conditions through reasonable component ratios and appropriate amounts of active magnesium oxide, and has no special requirements for environmental pH.

Benefits of technology

It achieves efficient, simple and environmentally friendly phosphorus removal and fluorine removal effects, reduces operation difficulty and economic costs, avoids secondary pollution, and is suitable for the treatment of phosphorus-containing fluorine-containing wastewater in various pH ranges.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119409298A_ABST
    Figure CN119409298A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of phosphorus-containing and fluorine-containing wastewater treatment, provides a phosphorus and fluorine removal agent and a preparation method thereof, and solves the problems that an existing phosphorus and fluorine removal agent is high in manufacturing and using cost, poor in fluorine removal effect and likely to cause secondary pollution due to the fact that the existing phosphorus and fluorine removal agent is greatly influenced by pH. The dephosphorization and defluorination agent is composed of calcium chloride, calcium oxide and active magnesium oxide; the preparation method comprises the following steps: preparing calcium chloride, calcium oxide and active magnesium oxide according to purity and particle size; mixing calcium chloride, calcium oxide and active magnesium oxide according to the molar ratio; adding active magnesium oxide into the premixed calcium chloride and calcium oxide according to the mass ratio of calcium oxide to calcium chloride to active magnesium oxide of 1: 2: (7-12); the mixed powder is subjected to refining treatment through a fine grinding machine, and the refined powder is subjected to secondary screening; and sealing, packaging and storing the refined powder. The use condition is simple, and only active magnesium oxide is required to be mixed with calcium oxide and calcium chloride in proportion.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of phosphorus- and fluorine-containing wastewater treatment, in particular to a simultaneous removal agent for phosphorus- and fluorine-containing wastewater in high, medium and low concentration ranges and pH ranges; in particular, it relates to a phosphorus- and fluorine-removing agent and a preparation method thereof. Background Art

[0002] The phosphorus chemical industry plays an important role in my country and even in the world, but the phosphorus chemical industry will produce a typical by-product - phosphogypsum. Phosphogypsum is a solid waste produced in the wet phosphoric acid process. Every 1t of phosphoric acid produced produces about 4.5-5t of phosphogypsum. The most common way to deal with phosphogypsum is temporary storage; but it not only occupies a large amount of land resources, but once the slag dump leaks wastewater, it will cause the total phosphorus in the water area to exceed the standard, posing a serious environmental risk. At present, the historical phosphogypsum stockpile in Guizhou alone is ≥120 million tons, and about 8 to 12 million tons of phosphogypsum are added each year. Because some slag depots did not have anti-seepage facilities or the anti-seepage measures of the slag depots failed in the early days, karst spring phosphorus pollution represented by the Jiaoyishan slag dump-No. 34 spring in Xifeng County and the Baiji slag dump-Facai Cave in Fuquan City have formed in Guizhou, which in turn affects the water quality of Wujiang River and Yangtze River. The chemical composition of phosphogypsum is very complex. In addition to calcium sulfate, there are also many impurities such as incompletely decomposed phosphate ore, residual phosphoric acid, fluoride, acid insoluble matter, organic matter, alkali metal salts, silicon, iron, magnesium and aluminum. Among the various impurities in phosphogypsum, phosphorus and fluorine have the greatest impact on the performance of phosphogypsum. In addition, the leachate or leaching liquid of phosphogypsum is usually acidic (pH value is 2-6), which limits the treatment and disposal of phosphogypsum. Although the comprehensive utilization of phosphogypsum has been involved in cement retarder, building material raw material, sulfuric acid co-production of cement and soil conditioner, the presence of impurities represented by P and F will continue to be enriched in the phosphogypsum yard, which not only limits the comprehensive utilization of phosphogypsum, but also greatly increases the risk of phosphogypsum storage.

[0003] The leachate from the phosphogypsum reservoir is an acidic wastewater with high phosphorus and fluoride content. At present, the treatment methods for pollutants such as phosphorus, fluorine and organic matter in water mainly include chemical method, ion exchange method, membrane separation method, biological treatment method and adsorption method. The phosphorus removal process in the phosphogypsum leachate generally selects chemical precipitation method and magnesium ammonium phosphate precipitation method. Among them, calcium-magnesium phosphorus removal in the chemical phosphorus removal method uses calcium ions, magnesium ions and phosphate to form insoluble substances, and removes phosphate from the wastewater by precipitation. It is difficult to meet the requirements of emission standards by relying solely on calcium-magnesium chemical phosphorus removal. In actual engineering projects, other chemical agents need to be added for phosphorus removal reaction to ensure that the total phosphorus meets the effluent water quality indicators. The chemical phosphorus removal agents mainly include calcium salts, iron salts and aluminum salts.

[0004] The removal process of fluoride is not much different from that of phosphate, and it competes with phosphorus removal in many processes. For pure high-concentration fluoride-containing wastewater, calcium ions are usually added to remove fluoride precipitation, even if Ca reacts with F to form CaF2 precipitation for fluoride removal; but the limit of calcium-based fluoride removal is limited by the solubility of CaF2. The theoretical minimum residual fluoride concentration of calcium-based fluoride removal at room temperature is about 6.93 mg / L-7.9 mg / L. In the phosphogypsum slag reservoir, due to the continuous enrichment of impurities, it is easy for the leachate to exceed the fluorine discharge standard of 10 mg / L. In addition, due to the inadequate anti-seepage of the phosphogypsum storage site leachate or the treated phosphorus-containing and fluoride-containing wastewater may need to be discharged to the surface and groundwater; therefore, in view of the high phosphorus, high fluoride and low pH wastewater characteristics of the phosphorus chemical industry, the development of safe and efficient phosphorus and fluoride removal agents is of great significance for the pollution prevention and control of the phosphorus chemical industry.

[0005] Prior art 1, Chinese patent, application number: 202410457271.3 discloses a fluorine-fixing and phosphorus-locking system and method for phosphogypsum slag reservoir and wastewater deep treatment, including a fluorine-fixing and phosphorus-locking subsystem for the phosphogypsum slag reservoir, that is, the supporting facilities of the existing phosphogypsum slag reservoir and the continued construction of the phosphogypsum slag reservoir, and also includes: a mineral material dam subsystem is set at the valley mouth downstream of the reservoir body, and the wastewater deep treatment subsystem for combined treatment of the reservoir body leachate and the wastewater discharged from the phosphogypsum factory is composed of a wastewater deep treatment unit, namely a comprehensive regulating tank, a neutralization reaction tank, a mixing reaction tank, a first sedimentation tank, a hydrolysis acidification tank, a biological contact oxidation tank, a second sedimentation tank, a multi-media filter, a clear water tank, a sludge concentration tank, It is composed of a filter press, etc., and uses the fixed fluorine and phosphorus locking technology to fix fluorine and phosphorus in the phosphogypsum slag, and uses the mineral material reaction dam technology to carry out ecological interception and treatment of the leachate; although the comprehensive treatment technology is used to combine the leachate and the wastewater discharged from the phosphogypsum factory for deep treatment, the treatment is comprehensive, the treatment cost is low, and there is no secondary pollution; but although the agent used in this scheme can greatly reduce the phosphorus and fluorine content, the agent requires the use of lanthanum, and the reserves of rare earth materials are scarce and non-renewable, and the separation, purification and processing are difficult, resulting in high prices. In addition, Guizhou has a large reserve of phosphogypsum, but scarce rare earth resources. If this agent is used as an in-situ remediation agent for the phosphogypsum slag depot in Guizhou Province, the economic cost will be huge.

[0006] Prior art 2, Chinese patent, application number: 202410262793.8 discloses a deep defluorination agent and a preparation method thereof, the preparation method comprising: adding ferric chloride and aluminum chloride to the acetic acid solution of chitosan to obtain a mixed solution, adjusting the pH of the mixed solution to 4.5-5.0 with ammonia water and stirring for a set time to obtain a first dispersion; dispersing polyacrylamide in the aqueous dispersion of nano calcium carbonate to obtain a second dispersion; adding the second dispersion to the first dispersion to obtain a third dispersion, adjusting the pH value of the third dispersion to 7-7.5 with ammonia water, and the static precipitate is a defluorination agent; although it effectively solves the problem that the current defluorination agent has a high cost if the defluorination effect is good, and the defluorination effect is not ideal if the cost is low, the agent used can stably control the fluoride ion concentration below 1 mg / L. However, the initial fluoride ion concentration is low, and the pH value requirement is high.

[0007] Prior art three, Chinese patent, application number: 202110466372.3 discloses a method for synthesizing a calcium iron magnesium ternary nanocomposite defluoridating agent, the method is as follows: (1) using industrial grade CaC l2 , FeCl3·6H2O, MgCl2·6H2O as calcium salt, iron salt and magnesium salt raw materials; (2) according to the molar ratio of calcium, iron and magnesium of 1:2:1, the addition mass of calcium salt, iron salt and magnesium salt is determined; (3) the weighed calcium salt, iron salt and magnesium salt are added to an appropriate amount of water in turn, and the mixture is fully stirred and added to the reactor; (4) 2 molL-1 NaOH solution is added dropwise to the reactor while stirring until the pH value of the mixed solution is 7-9; (5) stirring is continued for 1 hour at room temperature and pressure, and aging is carried out for 12 hours; (6) the product is taken out and filtered, and washed until the filtrate is neutral; (7) the filter cake is placed in a 100℃ constant temperature drying oven and dried for 24 hours; (8) the product is cooled to room temperature and crushed to obtain a calcium iron magnesium ternary nanocomposite defluoridant. Advantages: at room temperature and pressure, the preparation process is simple and easy to operate, and can be mass-produced and applied. Although the defluorination method of the agent used is relatively single. However, the defluorination effect is difficult to meet the emission standards.

[0008] At present, the existing technologies 1, 2 and 3 have the problems that the existing phosphorus removal and fluorine removal agents have high manufacturing and use costs, poor defluorination effects, are greatly affected by pH, and may cause secondary pollution. Therefore, the present invention provides a phosphorus removal and fluorine removal agent and a preparation method thereof. Summary of the invention

[0009] In order to achieve the above object, the present invention adopts the following technical scheme:

[0010] One aspect of the present invention provides a dephosphorization and defluorination agent, which is composed of calcium chloride, calcium oxide and active magnesium oxide; the mass ratio of calcium oxide, calcium chloride and active magnesium oxide is 1:2:7-12.

[0011] In an alternative embodiment, the activated magnesium oxide is replaced by activated aluminum oxide or hydroxyapatite.

[0012] In an optional embodiment, more than 0.6 g of active magnesium oxide is added per 10 g; and the amount of active magnesium oxide added is not less than 0.5 g / 10 g of phosphogypsum slag.

[0013] Another aspect of the present invention provides a method for preparing a dephosphorization and defluorination agent, which is used to prepare the dephosphorization and defluorination agent, comprising:

[0014] Prepare calcium chloride, calcium oxide and activated magnesium oxide according to purity and particle size;

[0015] Calcium chloride, calcium oxide and active magnesium oxide are mixed according to the molar ratio; calcium chloride and calcium oxide are weighed in proportion and placed in a dry mixer respectively; low-speed stirring is used for premixing to ensure that the two powders are evenly distributed; active magnesium oxide is placed in a dryer for drying; the dried active magnesium oxide is screened through a sieve to remove lumps and impurities;

[0016] Add active magnesium oxide to the premixed calcium chloride and calcium oxide in a molar ratio; mix by high-speed stirring;

[0017] The mixed powder is refined by a fine grinder, and the refined powder is screened again by a sieve; the refined powder is sealed and packaged.

[0018] In an optional embodiment, the rotation speed of the low-speed stirring is ≤50rpm; the drying process is carried out at a temperature of 95°C-100°C for not less than 2 hours; the mesh size of the dried sieve is ≤0.05mm;

[0019] The speed of high-speed stirring is ≥300rpm, and the stirring time is 10-15 minutes.

[0020] In an optional embodiment, the process of placing the activated magnesium oxide in a dryer comprises the following steps:

[0021] Deploy multi-dimensional intelligent sensors in drying equipment and screening equipment, including temperature sensors, humidity sensors, and particle size sensors, to achieve all-round data collection; interconnect drying equipment, screening equipment, temperature controllers, and screen inspection equipment through the Internet of Things, and transmit the data collected by the sensors to the controller in real time;

[0022] Among them, the particle size distribution equation is used to describe the distribution of active magnesium oxide particle size, and its form is:

[0023]

[0024] Where f(r,t) represents the particle size distribution function, which indicates the number or concentration of active magnesium oxide particles with a particle size of r at time t; D p represents the particle size diffusion coefficient, which indicates the diffusion capacity of particle size distribution in space. The diffusion term represents the particle size distribution, which describes the diffusion process of the particle size distribution in space; represents the nonlinear effect term; v represents the particle size change rate, which represents the rate of change of the particle size of the active magnesium oxide particles with time; vf(r,t) represents the convection term of the particle size distribution, which describes the movement process of the particle size distribution with the particle size change rate v;

[0025]

[0026] Represents the diffusion process of particle size distribution in space;

[0027] Intelligent control is used to predict the changing trend of active magnesium oxide at different temperatures and screen apertures, and the control strategy is optimized; the drying temperature and screen aperture are automatically adjusted according to the prediction results;

[0028] Among them, intelligent control includes a generative adversarial network model. The generator of the generative adversarial network model generates a simulated active magnesium oxide production environment, including different parameter combinations such as temperature, humidity and screen aperture. The discriminator determines whether the environment generated by the generator is real, and continuously optimizes the simulation ability of the generator by comparing it with the real data.

[0029] A large amount of simulation data was generated using a generative adversarial network model to expand the historical data set. Multiple simulation experiments were conducted in a virtual environment to explore the effects of different parameter combinations on the activity and particle size of activated magnesium oxide and find the optimal parameter combination.

[0030] In an optional implementation, a reinforcement learning model of adaptive reinforcement learning is established, and the state space is defined, including key parameters of real-time temperature, humidity, particle size distribution and screen aperture; the action space is defined, including operations of adjusting the drying temperature and changing the screen aperture; a reward function is designed, and the agent is given corresponding rewards or penalties according to the activity and particle size consistency of the active magnesium oxide; the agent continuously learns new control strategies during the production process, and dynamically adjusts the control strategies according to the simulated data and real-time data generated by the generative adversarial network; offline training is performed using historical data, and online learning is performed during the production process to continuously optimize the decision-making strategy of the agent; the simulated data generated by the generative adversarial network is used to detect abnormal conditions in the production process, such as temperature fluctuations and screen damage, and timely issue warnings;

[0031] Among them, the expression of the reward function is:

[0032]

[0033] In the formula, R(s,a) represents the reward function, which represents the reward obtained by performing action a in state s, and α i represents the activity consistency weight, which indicates the contribution of the activity consistency of the i-th batch to the reward, β i represents the particle size consistency weight, which indicates the contribution of the particle size consistency of the i-th batch to the reward, γ i represents the anomaly detection weight, indicating the contribution of the anomaly detection of the i-th batch to the reward, δ i represents the energy consumption optimization weight, indicating the contribution of the energy consumption optimization of the i-th batch to the reward, ∈ i represents the production efficiency weight, indicating the contribution of the i-th batch production efficiency to the reward, ζ i represents the equipment life weight, indicating the contribution of the equipment life of the i-th batch to the reward, η i represents the environmental impact weight, which indicates the contribution of the environmental impact of the i-th batch to the reward, θ i Represents the quality control weight, which indicates the contribution of the quality control of the i-th batch to the reward.

[0034] In an optional implementation manner, the specific calculation method is:

[0035]

[0036] Among them, the activity standard deviation is the standard deviation of the activity of the i-th batch of active magnesium oxide, and the maximum activity standard deviation is the preset maximum allowable standard deviation;

[0037]

[0038] Among them, the particle size standard deviation is the standard deviation of the particle size of the i-th batch of activated magnesium oxide, and the maximum particle size standard deviation is the preset maximum allowable standard deviation;

[0039]

[0040] Energy consumption optimization = current energy consumption / target energy consumption

[0041] Production efficiency; = current production volume / target production volume;

[0042] Equipment life = current equipment life / target equipment life;

[0043] Environmental impact = current environmental impact / target environmental impact;

[0044] Quality control = current quality control index / target quality control index.

[0045] In an optional embodiment, the control process of mixing by high-speed stirring comprises the following steps:

[0046] In the initial mixing stage, the stirring speed does not exceed 50 rpm; the initial mixing time is set to 5 minutes; after the initial mixing, the stirring speed is kept below 50 rpm; the time of the uniform distribution stage is set to 3 minutes;

[0047] After the low-speed stirring stage is completed, switch to the high-speed stirring stage, and the stirring speed should be no less than 300rpm; the time of the intensive mixing stage is set to 5 minutes; after the intensive mixing, the stirring speed is maintained at 300rpm; the time of the final mixing stage is set to 5-10 minutes;

[0048] During the mixing process, sampling and testing should be carried out every 2 minutes. The sampling points should be evenly distributed in different positions of the mixing container. The uniformity of the mixture should be tested by microscopic observation or chemical analysis methods. The stirring speed should be adjusted according to the sampling and test results.

[0049] In an optional embodiment, if the test results show uneven mixing, the stirring speed is increased or the stirring time is extended; if the test results show excessive mixing, the stirring speed is reduced or the stirring time is shortened; and the stirring time is adjusted according to the sampling test results.

[0050] The dephosphorization and defluorination agent of the present invention has simple use conditions and does not require complex configuration. It only requires active magnesium oxide to be mixed with calcium oxide and calcium chloride in proportion. Most of the defluorination agents currently on the market require a neutral pH range, while phosphogypsum leachate is acidic, and the solution must be adjusted to neutral before use; there is no requirement for the environmental pH value for use, and it can play a good defluorination effect under acidic conditions. BRIEF DESCRIPTION OF THE DRAWINGS

[0051] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:

[0052] Figure 1 This is a flow chart of the preparation method of the dephosphorization and defluorination agent provided in Example 1 of the present invention;

[0053] Figure 2 The fluorine removal effect of phosphogypsum leachate under different calcium oxide addition amounts provided in Example 5 of the present invention;

[0054] Figure 3 This is a diagram showing the phosphorus removal effect of phosphogypsum leachate at different calcium oxide addition amounts provided in Example 5 of the present invention;

[0055] Figure 4 This is a schematic diagram of the chloride ion removal rate provided in Example 5 of the present invention;

[0056] Figure 5 This is a schematic diagram of the total phosphorus removal rate provided in Example 5 of the present invention;

[0057] Figure 6 A schematic diagram showing a comparison of the defluorination effects of different agents provided in Example 5 of the present invention;

[0058] Figure 7 This is a schematic diagram of the simulated adsorption first-order kinetic equation provided in Example 5 of the present invention;

[0059] Figure 8 This is a schematic diagram of the simulated adsorption second-order kinetic equation provided in Example 5 of the present invention;

[0060] Fig. 9 This is a schematic diagram of treating a simulated phosphogypsum leachate using a mixed calcium agent of calcium oxide + calcium chloride in different ratios provided in Example 5 of the present invention;

[0061] Fig.10 The change of the removal rate of P and F by active magnesium oxide in the first 1470 minutes provided in Example 5 of the present invention;

[0062] Fig.11 This is a graph showing the change in the removal rate of P and F by active magnesium oxide in the first 150 minutes provided in Example 5 of the present invention;

[0063] Fig.12 This is a diagram showing the fluoride ion removal effect at various reagent ratios provided in Example 5 of the present invention;

[0064] Fig.13 This is a diagram of total phosphorus removal effects at various reagent ratios provided in Example 5 of the present invention. DETAILED DESCRIPTION

[0065] The technical solutions in the embodiments of the present invention will be described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0066] In the following, the terms "first", "second", etc. are used only for convenience of description and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first", "second", etc. may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "plurality" means two or more.

[0067] The embodiments of the present invention can be used for the control of fixed pollutants containing phosphorus and fluorine, and can also be used for the pollution control of phosphorus and fluorine wastewater; the treated phosphorus and fluorine wastewater is not affected by the initial pH, and is applicable to various pH ranges; it is used for the simultaneous removal of pollutants in phosphorus and fluorine wastewater, and can also be used alone for the treatment of phosphorus or fluorine wastewater; it is applicable to the treatment of phosphorus and fluorine concentration wastewater or solid waste in various concentration ranges of high, medium and low. By compounding different reagents and according to the proportion of the reagents, the optimal use of the reagents is achieved; the calcium oxide, calcium chloride and active magnesium oxide used in the reagents are all common industrial reagents, which are easy to obtain, cheap, and highly operable, and through the development of compound control, no new pollution will be caused to groundwater and surface water.

[0068] The key technical features of the embodiments of the present invention are as follows: calcium oxide, calcium chloride and active magnesium oxide or active aluminum oxide or hydroxyapatite, the mass ratio between different components ensures the synergistic effect of each component in the reaction, and improves the effect of phosphorus removal and fluorine removal; active magnesium oxide can be replaced by active aluminum oxide or hydroxyapatite, which increases the applicability and flexibility of the agent. An appropriate amount of active magnesium oxide can effectively adsorb and remove fluoride ions to ensure the defluorination effect; the added amount is not less than 0.5g / 10g phosphogypsum slag to ensure that a stable defluorination effect can be exerted under acidic conditions. It is only necessary to mix active magnesium oxide with calcium oxide and calcium chloride in proportion, without the need for complex configuration; the agent has no special requirements for the environmental pH value, and can play a good defluorination effect under acidic conditions; the configuration and use process of the agent is simplified, and the difficulty of operation is reduced; there is no need to adjust the pH value of the solution, which is suitable for the treatment of acidic phosphogypsum leachate, and the application range of the agent is expanded. Compared with the prior art, most existing defluorination agents require a neutral pH range, while phosphogypsum leachate is acidic, so the solution must be adjusted to neutral before use; there is no need to adjust the pH value, which reduces additional processing steps and costs; and reduces the consumption of chemicals and environmental pollution caused by adjusting the pH value. The dephosphorization and defluorination agent of this embodiment achieves efficient, simple, and environmentally friendly dephosphorization and defluorination effects through a reasonable component ratio, an appropriate amount of active magnesium oxide addition, and adaptability to the pH value; the key technical features not only improve the defluorination efficiency of the agent, but also simplify the operation process, reduce the cost of use, and have significant technical advantages and application value.

[0069] Embodiment 1:

[0070] like Figure 1 As shown, the embodiment of the present invention provides a dephosphorization and defluorination agent composed of calcium oxide, calcium chloride and active magnesium oxide; the mass ratio is 1:2:7-12;

[0071] The active magnesium oxide may also be active alumina or hydroxyapatite; more than 0.6 g of active magnesium oxide is added per 10 g; and the amount of active magnesium oxide added is not less than 0.5 g / 10 g of phosphogypsum slag.

[0072] In the above embodiment, the dephosphorization and defluorination agent of this embodiment has simple use conditions and does not require complex configuration. It only requires active magnesium oxide to be mixed with calcium oxide and calcium chloride in proportion. Most of the defluorination agents currently on the market require a neutral pH range, while phosphogypsum leachate is acidic, and the solution must be adjusted to neutral before use; there is no requirement for the environmental pH value for use, and it can play a good defluorination role under acidic conditions.

[0073] Embodiment 2:

[0074] like Figure 2 As shown, based on Example 1, the preparation method of the dephosphorization and defluorination agent provided in the embodiment of the present invention comprises the following steps:

[0075] Step S100: preparing calcium chloride, calcium oxide and activated magnesium oxide according to purity and particle size;

[0076] Among them, the purity of calcium chloride is ≥98%, and the particle size is ≤0.1mm; the purity of calcium oxide is ≥95%, and the particle size is ≤0.2mm; the purity of active magnesium oxide is ≥99%, and the particle size is ≤0.05mm;

[0077] Step S200: Mixing calcium chloride, calcium oxide and active magnesium oxide according to the mass ratio; weighing calcium chloride and calcium oxide in proportion and placing them in a dry mixer respectively; premixing by low-speed stirring (speed ≤ 50 rpm) to ensure that the two powders are evenly distributed; placing the active magnesium oxide in a dryer for drying at a temperature of 95° C.-100° C. for a period of not less than 2 hours; screening the dried active magnesium oxide through a sieve (sieve hole size ≤ 0.05 mm) to remove lumps and impurities;

[0078] Step S300: adding active magnesium oxide to the premixed calcium chloride and calcium oxide in a mass ratio of calcium oxide, calcium chloride and active magnesium oxide of 1:2:7-12; mixing by high-speed stirring (speed ≥ 300 rpm); the high-speed stirring time is controlled within 10-15 minutes to ensure that the components are fully mixed to form a uniform powder mixture;

[0079] Step S400: The mixed powder is refined by a fine grinder, and the particle size is controlled to be ≤0.05 mm; the refined powder is screened again by a sieve (sieve hole size ≤0.05 mm); the refined powder is sealed and packaged and stored in a dry and cool environment.

[0080] In the above embodiment, step S100 raw material preparation ensures the high purity of raw materials and improves the reaction efficiency and stability of the agent; controls the particle size of raw materials to ensure mixing uniformity and reaction activity. Significance: Provide high-quality raw materials for mixing and reaction to ensure the overall performance of the agent. Step S200 Mixing ratio setting and premixing, accurately weigh according to the molar ratio to ensure the stoichiometric relationship of each component; use low-speed stirring for premixing to ensure the uniform distribution of calcium chloride and calcium oxide; dry active magnesium oxide to remove moisture and impurities and improve its activity. Significance: Improve the uniformity and stability of the mixture through premixing and drying; dry and screen active magnesium oxide to improve its reaction activity in an acidic environment. Step S300 Addition of active magnesium oxide and high-speed mixing, add active magnesium oxide at a molar ratio of 0.5 to ensure its uniform distribution in the mixture; use high-speed stirring to ensure that active magnesium oxide is fully mixed with other components. Significance: Improve the contact area and reaction efficiency of each component through high-speed mixing; ensure that active magnesium oxide is evenly dispersed in the mixture and enhance the overall performance of the agent. Step S400: Refining and packaging and storage: Refining is performed by a fine grinder to improve the reactivity of the powder; secondary screening is performed by a screen to remove lumps and impurities to ensure the uniformity and fineness of the powder; the powder after refinement is sealed and packaged to prevent moisture and oxidation. Significance: Refining improves the reactivity of the powder and enhances its defluorination effect in an acidic environment; sealed packaging and storage conditions ensure the long-term stability and effectiveness of the agent.

[0081] In summary, the dephosphorization and defluorination agent of this embodiment not only simplifies the conditions of use, but also significantly improves the defluorination effect in an acidic environment. The specific meanings are as follows: simplifying the conditions of use, without the need for a complicated configuration process, only mixing in proportion is required; acidic environment adaptability, it can still effectively play a defluorination role under acidic conditions, without the need to adjust the solution to neutrality; by precisely controlling the amount of activated magnesium oxide added and the refinement treatment, the reaction efficiency and stability of the agent are improved, and it has high innovation and practicality. The dephosphorization and defluorination agent of this embodiment has significant advantages and potential in practical applications. Through the above-mentioned preparation process, the dephosphorization and defluorination agent of this embodiment not only simplifies the conditions of use, but also significantly improves the defluorination effect in an acidic environment, and it has high innovation and practicality.

[0082] Embodiment 3:

[0083] Based on Example 2, the process of placing the active magnesium oxide in a dryer in step S200 provided in the embodiment of the present invention comprises the following steps:

[0084] Step S201: deploy multi-dimensional intelligent sensors in the drying equipment and the screening equipment, including temperature sensors, humidity sensors, and particle size sensors, etc., to realize all-round data collection; interconnect the drying equipment, the screening equipment, the temperature controller, and the screen inspection equipment through the Internet of Things technology, and transmit the data collected by the sensors to the controller in real time;

[0085] Among them, the particle size distribution equation is used to describe the distribution of active magnesium oxide particle size, and its form is:

[0086]

[0087] Where f(r,t) represents the particle size distribution function, which indicates the number or concentration of active magnesium oxide particles with a particle size of r at time t; D p represents the particle size diffusion coefficient, which indicates the diffusion capacity of particle size distribution in space. The diffusion term represents the particle size distribution, which describes the diffusion process of the particle size distribution in space; represents the nonlinear effect term; v represents the particle size change rate, which represents the rate of change of the particle size of the active magnesium oxide particles with time; vf(r,t) represents the convection term of the particle size distribution, which describes the movement process of the particle size distribution with the particle size change rate v;

[0088]

[0089] Represents the diffusion process of particle size distribution in space;

[0090] Step S202: using intelligent control to predict the changing trend of active magnesium oxide at different temperatures and screen apertures, and optimizing the control strategy; automatically adjusting the drying temperature and screen aperture according to the prediction results;

[0091] Among them, intelligent control includes a generative adversarial network model. The generator of the generative adversarial network model generates a simulated active magnesium oxide production environment, including different parameter combinations such as temperature, humidity and screen aperture. The discriminator determines whether the environment generated by the generator is real, and continuously optimizes the simulation ability of the generator by comparing it with the real data.

[0092] Step S203: Generate a large amount of simulation data using a generative adversarial network model to expand the historical data set; conduct multiple simulation experiments in a virtual environment to explore the effects of different parameter combinations on the activity and particle size of activated magnesium oxide and find the best parameter combination;

[0093] Establish a reinforcement learning model for adaptive reinforcement learning, define the state space, including key parameters such as real-time temperature, humidity, particle size distribution and screen aperture; define the action space, including operations such as adjusting the drying temperature and changing the screen aperture; design a reward function to give the agent corresponding rewards or penalties based on the activity of the activated magnesium oxide and the consistency of the particle size; the agent continuously learns new control strategies during the production process, and dynamically adjusts the control strategy based on the simulated data and real-time data generated by the generative adversarial network; use historical data for offline training, and conduct online learning during the production process to continuously optimize the agent's decision-making strategy; use the simulated data generated by the generative adversarial network to detect abnormal conditions in the production process, such as temperature fluctuations, screen damage, etc., and issue early warnings in a timely manner;

[0094] Among them, the expression of the reward function is:

[0095]

[0096] In the formula, R(s,a) represents the reward function, which represents the reward obtained by performing action a in state s, and α i represents the activity consistency weight, which indicates the contribution of the activity consistency of the i-th batch to the reward, β i represents the particle size consistency weight, which indicates the contribution of the particle size consistency of the i-th batch to the reward, γ i represents the anomaly detection weight, indicating the contribution of the anomaly detection of the i-th batch to the reward, δ i represents the energy consumption optimization weight, indicating the contribution of the energy consumption optimization of the i-th batch to the reward, ∈ i represents the production efficiency weight, indicating the contribution of the i-th batch production efficiency to the reward, ζ i represents the equipment life weight, indicating the contribution of the equipment life of the i-th batch to the reward, η i represents the environmental impact weight, which indicates the contribution of the environmental impact of the i-th batch to the reward, θ i represents the quality control weight, which indicates the contribution of the quality control of the i-th batch to the reward;

[0097] Specific calculation method:

[0098]

[0099] Among them, the activity standard deviation is the standard deviation of the activity of the i-th batch of active magnesium oxide, and the maximum activity standard deviation is the preset maximum allowable standard deviation;

[0100]

[0101] Among them, the particle size standard deviation is the standard deviation of the particle size of the i-th batch of activated magnesium oxide, and the maximum particle size standard deviation is the preset maximum allowable standard deviation;

[0102]

[0103] Energy consumption optimization = current energy consumption / target energy consumption

[0104] Production efficiency; = current production volume / target production volume;

[0105] Equipment life = current equipment life / target equipment life;

[0106] Environmental impact = current environmental impact / target environmental impact;

[0107] Quality control = current quality control index / target quality control index;

[0108] The advantages of the reward function comprehensively consider the activity consistency, particle size consistency, anomaly detection, energy consumption optimization, production efficiency, equipment life, environmental impact and quality control of activated magnesium oxide to ensure the comprehensive optimization of the production process; by adjusting the weights, the focus of the reward function can be flexibly adjusted according to actual production needs; the anomaly detection mechanism ensures the safety and stability of the production process, and timely warns of abnormal situations to avoid production accidents; energy consumption optimization, equipment life and environmental impact considerations ensure the sustainability and long-term benefits of the production process; the introduction of quality control indicators ensures product quality in the production process and improves customer satisfaction; through this complex reward function design, the intelligent agent can continuously optimize the control strategy during the production process to improve the production quality and efficiency of activated magnesium oxide.

[0109] In the above embodiment, step S201 multi-dimensional intelligent sensor deployment and data acquisition, by deploying multi-dimensional intelligent sensors such as temperature sensors, humidity sensors and particle size sensors, to achieve comprehensive monitoring of the production environment of active magnesium oxide; using the Internet of Things technology, the drying equipment, screening equipment, temperature controller and screen inspection equipment are interconnected to ensure that the data collected by the sensor can be transmitted to the controller in real time, and the data can be processed and analyzed immediately. The significance achieved: All-round data collection and real-time transmission ensure the accuracy and timeliness of the data, and provide a solid foundation for intelligent control and optimization; real-time monitoring and data recording improve the transparency of the production process, help to timely discover and solve problems, and improve production efficiency. Step S202 intelligent control and optimization strategy, using intelligent control to predict the change trend of active magnesium oxide at different temperatures and screen apertures, optimize the control strategy, and ensure the stability and efficiency of the production process; according to the prediction results, the drying temperature and screen aperture are automatically adjusted to reduce human intervention and improve the consistency and controllability of production. The significance achieved: through intelligent control and automatic adjustment of parameters, the time and cost of manual operation are reduced, and production efficiency is improved; production parameters are accurately controlled to ensure the stable quality of active magnesium oxide and meet high-standard production requirements. Step S203 generates adversarial network models and adaptive reinforcement learning, using the generated adversarial network model to generate a large amount of simulation data, expand the historical data set, and provide rich data support for virtual experiments; conduct multiple simulation experiments in a virtual environment to explore the effects of different parameter combinations on the activity and particle size of active magnesium oxide, and find the best parameter combination; establish a reinforcement learning model for adaptive reinforcement learning, define the state space and action space, and design a reward function. The intelligent agent continuously learns new control strategies during the production process and dynamically adjusts the control strategy. Significance achieved: Through the generation of adversarial networks and adaptive reinforcement learning, the intelligent agent can dynamically adjust the control strategy according to the simulation data and real-time data, and improve the intelligence and flexibility of decision-making; use the simulation data generated by the generative adversarial network to detect abnormal conditions in the production process, such as temperature fluctuations, screen damage, etc., and issue early warnings in time to enhance the robustness and safety of the system.

[0110] In summary, the production process of active magnesium oxide in this embodiment realizes intelligence, automation and high efficiency, which not only improves production efficiency and product quality, but also enhances the safety and controllability of the production process. The production of active magnesium oxide is made more scientific, accurate and sustainable, meeting the high standards of modern industrial production. For the first time, the generative adversarial network (GAN) is applied to the simulation and data enhancement of the active magnesium oxide production process to improve the diversity and training effect of the data set; combined with the adaptive reinforcement learning mechanism, the dynamic adjustment and optimization of the intelligent body in the production process are realized, and the flexibility and accuracy of the control strategy are improved; through GAN anomaly detection and reinforcement learning anomaly handling, intelligent early warning and real-time decision support are realized, and the stability and safety of the production process are improved. Through this innovative solution, the intelligent and adaptive control of the active magnesium oxide production process can be realized, the product quality and production efficiency can be improved, while reducing human intervention and reducing production costs. Not only the latest AI technology is combined, but also a higher level of intelligent and adaptive control is achieved through the combination of GAN and adaptive reinforcement learning.

[0111] Embodiment 4:

[0112] On the basis of Example 2, the control process of high-speed stirring and mixing provided in the embodiment of the present invention comprises the following steps:

[0113] S301: In the initial mixing stage, the stirring speed does not exceed 50 rpm; the initial mixing time is set to 5 minutes; after the initial mixing, the stirring speed is kept below 50 rpm; the time of the uniform distribution stage is set to 3 minutes;

[0114] Step S302: After the low-speed stirring stage is completed, switch to the high-speed stirring stage, and the stirring speed should be not less than 300 rpm; the time of the intensive mixing stage is set to 5 minutes; after the intensive mixing, the stirring speed is maintained at 300 rpm; the time of the final mixing stage is set to 5-10 minutes;

[0115] Step S303: During the mixing process, sampling and testing are performed every 2 minutes, and the sampling points should be evenly distributed at different positions of the mixing container; the uniformity of the mixture is tested by microscopic observation or chemical analysis methods; the stirring speed is adjusted according to the sampling and testing results; if the test results show uneven mixing, the stirring speed is increased or the stirring time is extended; if the test results show excessive mixing, the stirring speed is reduced or the stirring time is shortened; according to the sampling and testing results, the stirring time is adjusted.

[0116] In the above embodiment, in the initial mixing stage of step S301, low-speed stirring helps to avoid the particles in the mixture from being broken or generating too many bubbles due to high-speed stirring, thereby maintaining the integrity of the particles and the stability of the mixture; the initial mixing time is set to 5 minutes, which is enough for the mixture to be initially mixed, but will not cause excessive mixing or particle breakage; the time of the uniform distribution stage is set to 3 minutes, and after the initial mixing, the low-speed stirring is continued to ensure that the mixture is evenly distributed in the container to avoid local concentration differences. The significance achieved: to ensure the initial uniformity of the mixture, through low-speed stirring and appropriate initial mixing time, to ensure that the mixture reaches basic uniformity in the initial stage, and lay a good foundation for subsequent high-speed stirring. In the high-speed stirring stage of step S302, high-speed stirring (not less than 300rpm) can significantly improve the mixing efficiency, so that the particles in the mixture can be dispersed and mixed more quickly; the time of the enhanced mixing stage is set to 5 minutes, which is enough for the mixture to reach a more uniform state under high-speed stirring and enhance the mixing effect; the time of the final mixing stage is set to 5-10 minutes, and the mixing is continued under high-speed stirring to ensure that the mixture reaches the final uniform state. The setting of the time range can be adjusted according to actual conditions. Significance achieved: Through high-speed stirring, the mixing efficiency is significantly improved, so that the mixture can reach a high uniformity in a shorter time; the uniformity of the final mixture is ensured, and by setting a reasonable final mixing time, the mixture is ensured to reach the final uniform state under high-speed stirring to meet production requirements. Step S303 sampling detection and adjustment, sampling detection is performed every 2 minutes, and regular sampling detection can monitor the uniformity of the mixture in real time and find problems in the mixing process in time; the sampling points are evenly distributed to ensure the uniform distribution of the sampling points and avoid inaccurate detection results caused by sampling point deviations; the uniformity of the mixture is detected by microscopic observation or chemical analysis methods, which can accurately evaluate the uniformity of the mixture and provide a basis for adjustment; the stirring speed and time are adjusted according to the test results, and the stirring speed and time are dynamically adjusted according to the test results to ensure that the mixture reaches the best uniform state. Significance achieved: Through regular sampling detection and dynamic adjustment, the mixing process is always in the best state to avoid problems of over-mixing or under-mixing; through real-time monitoring and adjustment, the uniformity of the final mixture is significantly improved to meet high-standard production requirements. During the high-speed stirring process, sampling detection is performed every 2 minutes. Assume that when sampling at the 4th minute, microscopic observation shows that the powder particles are unevenly distributed in some areas. At this point, the test results show that the mixing is uneven, so it is decided to increase the stirring speed to 380rpm and extend the stirring time to 10 minutes to ensure the mixing uniformity. Sampling at the 6th minute: Through chemical analysis methods, it is found that the chemical composition of the mixture is still uneven in some areas.At this time, continue to increase the stirring speed to 400rpm, and extend the final mixing stage time to 12 minutes; take samples at the 8th minute: microscopic observation and chemical analysis results show that the mixing uniformity has been significantly improved, but there is still slight unevenness. At this time, keep the stirring speed at 400rpm and extend the final mixing stage time to 15 minutes; take samples at the 10th minute: the final test results show that the uniformity of the mixture meets the expected standard, and the stirring process ends.

[0117] In summary, this embodiment ensures that the mixture can reach the best uniform state at different stages through reasonable speed and time settings, as well as real-time monitoring and adjustment. Not only the mixing efficiency is improved, but also the quality of the final product is guaranteed, which has important technical significance and economic value. This embodiment can ensure the uniformity of the agent during the mixing process through a hierarchical stirring speed and time control process, thereby improving the effect of phosphorus removal and fluorine removal. The specific control process includes four stages: initial mixing, uniform distribution, intensive mixing and final mixing. Each stage has a clear stirring speed and time setting, and the mixing uniformity is ensured by sampling detection and adjustment control.

[0118] Embodiment 5:

[0119] like Figure 3 As shown, based on Example 1, the test process of the dephosphorization and defluorination agent provided in the embodiment of the present invention includes:

[0120] 1. Component Description:

[0121] 1. Calcium oxide: The pollutants in phosphogypsum leachate are mainly soluble phosphorus and fluorine, among which soluble phosphorus is mainly in the form of H2PO4 - 、HPO4 2- PO4 3- Soluble fluoride exists in the form of fluoride ions. When calcium ions are added, soluble phosphorus combines with calcium ions to form calcium phosphate precipitation, thereby reducing the concentration of soluble phosphorus in the system. - With the addition of calcium oxide, it can be combined with Ca 2+ A reaction occurs to generate CaF2 precipitation, and the reaction equation is shown below. In addition, phosphogypsum usually contains sulfuric acid and other acidic substances left over from the phosphoric acid production process. Because the phosphogypsum leachate is significantly acidic, the pH value is usually between 2-5. The addition of calcium oxide can effectively adjust the pH of the leachate to facilitate the precipitation and removal of phosphorus and fluorine.

[0122] Ca 2+ +2H2PO4 - →Ca(H2PO4)2

[0123] Ca 2+ +HPO4 2- →CaHPO4

[0124] 3Ca 2+ +2PO4 3- →Ca3(PO4)2

[0125] H + +F - →HF

[0126] Ca 2+ +2F - →CaF2

[0127] The removal of soluble phosphorus and soluble fluorine in phosphogypsum leachate is closely related to the amount of calcium oxide added. The greater the amount of calcium oxide added, the greater the calcium ion concentration, the greater the binding rate of soluble phosphorus and soluble fluorine with calcium in the leachate, and the higher the removal rate. However, excessive addition of calcium oxide will lead to too high pH of the leachate, which not only increases the economic cost, but also affects the surrounding surface and groundwater environment when used in the field. In order to determine the optimal amount of calcium oxide added, phosphogypsum stored for more than 3 years was used to prepare the leachate, with a fluoride ion concentration of 57.23 mg / L, a total phosphorus concentration of 6.544 mg / L, and a pH value of 4.68. Since the reaction of phosphorus, fluorine and calcium ions is closely related to pH conditions, under acidic conditions, the hydrogen ions in the system will compete with fluoride ions to form hydrofluoric acid, thereby affecting the precipitation of fluoride ions. Therefore, in the experiment, the pH of the leachate was adjusted to 9 using NaOH before adding the drug, and then the drug was added according to the mass ratio of phosphogypsum of 0.2%-4%, and the results were shown in Table 1. The addition of calcium oxide has a good effect on total phosphorus removal (see Appendix Figure 2 and attached Figure 3 ), the total phosphorus concentration can be stably maintained below 0.1 mg / L, and the removal rate can be stably maintained above 98%. With the increase of calcium oxide addition, the total phosphorus removal effect no longer increases significantly. In terms of fluoride ions, the fluoride removal effect of calcium oxide is weaker than the phosphorus removal effect. With the increase of calcium oxide addition, the fluoride ion removal rate increases significantly, but when the addition amount reaches 4%, the fluoride ion concentration is 10.09 mg / L, and the removal rate is only 82.37%. This shows that the addition of calcium oxide can completely achieve the removal of soluble phosphorus, but cannot completely achieve the removal of fluoride ions.

[0128] Table 1 Phosphorus and fluorine removal effect of phosphogypsum leachate at different calcium oxide addition amounts

[0129]

[0130]

[0131] 2. Calcium chloride: Although the addition of calcium oxide is beneficial to the removal of phosphate and fluoride ions, excessive addition of calcium oxide will cause the system pH to be too high. Therefore, the common ion effect is used to use calcium chloride as a calcium supplement in the mixed reagent to promote the precipitation reaction of soluble phosphorus, soluble fluoride and calcium ions. In order to determine the phosphorus and fluoride removal effect of calcium chloride, the test also used the leaching solution of phosphogypsum old residue, that is, the fluoride ion concentration was 57.23 mg / L, the total phosphorus concentration was 6.544 mg / L, and the pH value was 4.68. Before adding the drug, the pH of the leachate was adjusted to 9 with NaOH, and then the drug was added according to the mass ratio of phosphogypsum of 0.4%-8%, and the results were shown in Table 2. As can be seen from the chart, with the addition of calcium chloride alone, the total phosphorus concentration can be stably maintained below 0.08 mg / L, and the removal rate can be stably maintained above 98%, indicating that the addition of calcium chloride can achieve the system phosphorus removal effect, but the fluoride ion removal effect is not as good as that of calcium oxide. When the addition amount reaches 8%, the removal rate is only 70.23% and the concentration is 17.04 mg / L (see attached Figure 4 and attached Figure 5 ).

[0132] Table 2 Phosphorus and fluorine removal effect of phosphogypsum leachate at different calcium chloride addition amounts

[0133]

[0134] 3. Activated magnesium oxide: Activated magnesium oxide is a high-performance metal-based adsorbent with a high specific surface area, large adsorption capacity, non-toxic and harmless, green and safe. It has a strong chemical adsorption effect on fluoride ions in fluoride-containing wastewater to form insoluble magnesium fluoride. Although calcium oxide and calcium chloride can effectively remove soluble phosphorus in the leachate, the fluoride removal effect is not good. In order to solve the problem of fluoride removal by chemical agents, the test used activated alumina, activated magnesium oxide, hydroxyapatite, magnesium oxide, and alumina to compare the fluoride removal effects. The fluoride ion concentration of the leachate was 24.71 mg / L, the amount of chemical added was 0.3 g / 100 ml, and the pH of the leachate was not adjusted. The results are shown in the following chart. It can be seen from the chart that among several agents, activated magnesium oxide has the best fluoride removal effect. The fluoride removal rates of the two activated magnesium oxides are both above 95%, and the fluoride ion concentration is not more than 1 mg / L (refer to the attached Figure 6 ).

[0135] Table 3 Comparison of defluorination effects of different agents

[0136]

[0137]

[0138] In order to further study the adsorption mechanism of active magnesium oxide, isothermal adsorption tests and adsorption kinetics studies were carried out on active magnesium oxide. The P of the 1:20 leachate of fresh phosphogypsum produced by the factory was tested to be 105 mg / L, 55 mg / L of fluorine, pH 3.01, 1520 mg / L of sulfate, and no chloride ion was detected. Sodium fluoride, potassium dihydrogen phosphate, and anhydrous sodium sulfate were used to prepare a solution to simulate fresh phosphogypsum leachate to carry out isothermal adsorption experiments. The amount of active magnesium oxide added was 0.5 g / 100 mL, stirred for 30 minutes, and filtered and monitored after standing for 20 hours. The experimental data were fitted with Langmuir and Freundlich equations, respectively, and the results are as follows:

[0139] Table 4 Isothermal adsorption fitting results of activated magnesium oxide (total phosphorus)

[0140]

[0141] Table 5 Isothermal adsorption fitting results of activated magnesium oxide (fluoride ion)

[0142]

[0143] The analysis of the fitting results shows that the Freundlich adsorption isotherm model fitting correlation coefficient R2 of active magnesium oxide for phosphorus and fluorine is greater than the Langmuir adsorption isotherm model fitting correlation coefficient, indicating that the adsorption of active magnesium oxide for phosphorus and fluorine is more inclined to non-uniform surface and multilayer adsorption. In the Freundlich adsorption isotherm model, the value of 1 / n indicates the degree of adsorption favorability, 0<1 / n<1, which is favorable for adsorption, 1 / n=1, the adsorption is irreversible, 1 / n>1, which is not conducive to adsorption. It can be seen from the table that the 1 / n values ​​of active magnesium oxide for phosphorus and fluorine are 0.57 and 0.65 respectively, which are in the range of greater than 0 and less than 1, indicating that active magnesium oxide has good adsorption strength for both phosphorus and fluorine.

[0144] Sodium fluoride, potassium dihydrogen phosphate, and anhydrous sodium sulfate were used to prepare a solution with a fluoride ion concentration of 100 mg / L, a total phosphorus concentration of 100 mg / L, and a sulfate ion concentration of 1500 mg / L. The amount of active magnesium oxide added was 0.5 g / 100 ml. The solution was stirred for 30 minutes, filtered after standing for different periods of time, and the total phosphorus and fluoride ion concentrations were monitored. The adsorption kinetic equation was simulated. The results are as follows: Figure 7 and Figure 8 shown.

[0145] In the initial stage of adsorption, the adsorption rate is fast, and then the adsorption rate gradually decreases until the adsorption reaches equilibrium. Comparing the two figures, it can be seen that the linear relationship of the secondary kinetic model has a higher correlation coefficient than the primary kinetic model, and the fitting R2 of fluoride ion and total phosphorus is greater than 0.99, indicating that the adsorption of fluorine and phosphorus by active magnesium oxide is more suitable for the secondary kinetic model.

[0146] 2. Research on drug ratio

[0147] (1) Mixed calcium agent for phosphorus and fluoride removal

[0148] The solubility of CaF2 in solution is 7.9 mg / L expressed as F ions, which can be understood as the lowest theoretical value of calcium-based fluoride removal. Removing F and P requires providing as many free calcium ions as possible, so calcium oxide, which is relatively inexpensive and can increase the pH of the system but has relatively low solubility, and calcium chloride, which has good solubility and can enhance the common ion effect of calcium, are used as the basis for this agent for research.

[0149] During the study, the total amount of calcium oxide required to completely react with the soluble P and F in the phosphogypsum leachate was 1. The total amount of calcium chloride required to completely react with the soluble P and F in the phosphogypsum leachate was 1.

[0150] The simulated phosphogypsum leachate was treated with a mixture of calcium oxide and calcium chloride in different ratios. Fig. 9 ; From the experimental results, it can be seen that too high or too low ratio of calcium oxide and calcium chloride is not conducive to the simultaneous removal of phosphorus and fluorine. And too high calcium chloride is easy to cause excessive chloride ions in groundwater, and too high calcium oxide will make the pH too high. Therefore, the mass ratio of calcium oxide: calcium chloride mixed calcium agent is 1:2 times.

[0151] (2) Removal of phosphorus and fluorine by activated magnesium oxide

[0152] Active magnesium oxide was used alone to adsorb the new phosphogypsum slag and the old slag stored in the slag storage. The solid-liquid ratio of the leaching liquid was 1:20. The adsorption results are shown in Table 6:

[0153] Table 6 Adsorption results

[0154]

[0155] Active magnesium oxide was used to conduct adsorption tests on the old slag from the Da'ao slag yard and the new slag from Kailin Company. The removal rate of phosphorus by active magnesium oxide reached more than 99%, and the removal rate of fluorine increased with the increase of the added amount.

[0156] (3) Study the reaction time of calcium and active magnesium oxide.

[0157] By studying the difference in the reaction time of calcium and magnesium, the feasibility of compounding mixed calcium agent with activated magnesium oxide is explored. After using the mixed calcium agent to remove high-concentration phosphorus and fluorine, active magnesium oxide is used to adsorb low-concentration phosphorus and low-concentration fluorine, achieving overall efficient removal. Fig.10Using new slag leaching solution, 1:2 times of calcium oxide + calcium chloride, the mixed agent was studied for the removal of P and F in the simulated mixed solution at different reaction times, of which the first 30 minutes were magnetic stirring, and then the time was static. The effect of reaction time on the removal of phosphorus and fluorine was verified by experiments. The calcium agent of calcium oxide + calcium chloride, which mainly uses chemical reaction, has removed most of the phosphorus within 1 minute (removal rate of more than 99%), and the removal of fluorine is mainly in the first 10 minutes. The adsorption removal of phosphorus by active magnesium oxide is mainly in the first 5 minutes, and the adsorption removal of fluorine is significantly improved from 30 minutes.

[0158] Fig.11 It can be seen from the removal rate that the adsorption and removal of phosphorus by activated magnesium oxide is mainly in the first 5 minutes, and the adsorption and removal of fluorine increases significantly from 30 minutes.

[0159] Therefore, by utilizing the different removal efficiencies of calcium and activated magnesium oxide for phosphorus and fluoride removal, it is possible to use calcium to quickly remove high-concentration phosphorus and fluorine, and then use activated magnesium oxide to re-adsorb low-concentration phosphorus and low-concentration fluorine, thereby achieving the goal of overall efficient removal while saving the amount of activated magnesium oxide.

[0160] (4) Research on different proportions of mixed drugs

[0161] The active magnesium oxide multiple is determined based on the fluorine concentration in the phosphogypsum leachate. The corresponding concentration range is found on the adsorption isotherm of the simulated mixed solution. The amount of magnesium oxide required for complete adsorption of F ions is determined as 1 according to its saturated adsorption capacity.

[0162] In order to find the best ratio of several reagents, a reagent ratio test was carried out. 10g of new phosphogypsum residue was weighed, 200ml of water was added, and magnetic stirring was performed for 30 minutes. The phosphogypsum leachate was obtained by filtering with filter paper. The supernatant was taken to measure the fluoride ion concentration of 105mg / L, the total phosphorus concentration of 55.3mg / L, the sulfate ion concentration of 1520mg / L, and the pH value of 3.01. Calcium oxide, calcium chloride, and active magnesium oxide powder were weighed and mixed according to different proportions, added to the phosphogypsum leachate, magnetic stirring was performed for 30 minutes, and the solution was left to stand for 24 hours. The supernatant was taken to measure the fluoride and total phosphorus concentrations in the water. The results are shown in Table 7.

[0163] Table 7 Phosphorus and fluorine removal effects under various reagent ratios

[0164]

[0165] Depend on Fig.12 and Fig.13It can be seen that under different reagent ratios, the total phosphorus removal rate can stably reach more than 99%. In terms of fluoride removal, when the reagent mass ratio is 1:2:27, the fluoride removal effect is best, the fluoride ion concentration is only 1.62 mg / L, and the removal rate is 96.77%. When the reagent mass ratio is 1:2:18, the fluoride ion concentration is higher than the former, which is 2.64 mg / L, and the removal rate is 94.74%.

[0166] The pH, chloride ion and sulfate ion content of the new slag leaching solution of phosphogypsum were tested by adding different proportions of slag. The pH of the new slag leaching solution was 3.08, the chloride ion content was not detected, and the sulfate ion content was 1520 mg / L. After adding different proportions of reagents, the results are shown in Table 8: the sulfate ion rate relative to the original slag in each group was reduced, the pH rate was higher than 9.0, the chloride ion in the reagent mass ratio of 1:2:18 slightly exceeded the standard, and the chloride ion in the mass ratio of 1:2:9 was lower than the requirement of 250 mg / L for groundwater. However, the dosage of active magnesium oxide can be reduced, and the trial cost of the reagent can be reduced. Therefore, this reagent is used in a ratio of CaO, CaCl2, and active magnesium oxide of 1:1.1:0.5.

[0167] Table 8

[0168]

[0169] (5) Verification of the suitability of reagents and proportions for phosphogypsum slag

[0170] The phosphogypsum slag from the Da'ao slag field was selected, and the fluoride content was measured to be 32.3 mg / L, and the total phosphorus concentration was 3.81 mg / L. The phosphogypsum slag was treated according to the ratio of calcium oxide: calcium chloride = 1:2, and different amounts of active magnesium oxide were added. The results are as follows, as shown in Table 9:

[0171] Table 9

[0172]

[0173] The effects of different addition amounts of calcium oxide + calcium chloride + active magnesium oxide on the new slag of Kailin Company and the old slag of Da'ao slag field were studied. The data showed that the mixed reagents of each ratio had a good removal rate for P. On the contrary, the calcium oxide with a lower addition amount had a better effect on the removal of F. It may be that more calcium oxide caused the pH of the solution to increase, which was not conducive to fluoride removal. It is recommended to add more than 0.6g of active magnesium oxide per 10g. Combined with the results of chloride ion dissolution in calcium chloride, in order to avoid excessive chloride ions, it is recommended to use a reagent mass ratio of calcium oxide: calcium chloride: active magnesium oxide = 2:1:7-12, and the addition of active magnesium oxide should not be less than 0.5g / 10g phosphogypsum slag.

[0174] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A dephosphorization and defluorination agent, characterized in that: It is composed of calcium chloride, calcium oxide and active magnesium oxide; the mass ratio of calcium oxide, calcium chloride and active magnesium oxide is 1:2:7-12.

2. The dephosphorization and defluorination agent according to claim 1, characterized in that: Active magnesium oxide is replaced by active alumina and hydroxyapatite.

3. The dephosphorization and defluorination agent according to claim 1, characterized in that: More than 0.6g of active magnesium oxide is added for every 10g; and the amount of active magnesium oxide added is not less than 0.5g / 10g of phosphogypsum slag.

4. A method for preparing a dephosphorization and defluorination agent, for producing the dephosphorization and defluorination agent as claimed in any one of claims 1 to 3, characterized in that: Include: Prepare calcium chloride, calcium oxide and activated magnesium oxide according to purity and particle size; Calcium chloride, calcium oxide and active magnesium oxide are mixed according to the mass ratio; calcium chloride and calcium oxide are weighed in proportion and placed in a dry mixer respectively; low-speed stirring is used for premixing to ensure that the two powders are evenly distributed; active magnesium oxide is placed in a dryer for drying; the dried active magnesium oxide is screened through a sieve to remove lumps and impurities; Add active magnesium oxide to the premixed calcium chloride and calcium oxide in a molar ratio; mix by high-speed stirring; The mixed powder is refined by a fine grinder, and the refined powder is screened again by a sieve; the refined powder is sealed and packaged.

5. The method for preparing the dephosphorization and defluorination agent according to claim 4, characterized in that: The speed of low-speed stirring is ≤50rpm; the drying temperature is 95℃-100℃, and the time is not less than 2 hours; the mesh size of the sieve after drying is ≤0.05mm; The speed of high-speed stirring is ≥300rpm, and the stirring time is 10-15 minutes.

6. The method for preparing the dephosphorization and defluorination agent according to claim 4, characterized in that: The process of placing activated magnesium oxide in a dryer includes the following steps: Deploy multi-dimensional intelligent sensors in drying equipment and screening equipment, including temperature sensors, humidity sensors, and particle size sensors, to achieve all-round data collection; interconnect drying equipment, screening equipment, temperature controllers, and screen inspection equipment through the Internet of Things, and transmit the data collected by the sensors to the controller in real time; Among them, the particle size distribution equation is used to describe the distribution of active magnesium oxide particle size, and its form is: Where f(r,t) represents the particle size distribution function, which indicates the number or concentration of active magnesium oxide particles with a particle size of r at time t; D p represents the particle size diffusion coefficient, which indicates the diffusion capacity of particle size distribution in space. The diffusion term represents the particle size distribution, which describes the diffusion process of the particle size distribution in space; represents the nonlinear effect term; v represents the particle size change rate, which represents the rate of change of the particle size of the active magnesium oxide particles with time; vf(r,t) represents the convection term of the particle size distribution, which describes the movement process of the particle size distribution with the particle size change rate v; Represents the diffusion process of particle size distribution in space; Intelligent control is used to predict the changing trend of active magnesium oxide at different temperatures and screen apertures, and the control strategy is optimized; the drying temperature and screen aperture are automatically adjusted according to the prediction results; Among them, intelligent control includes a generative adversarial network model. The generator of the generative adversarial network model generates a simulated active magnesium oxide production environment, including different parameter combinations such as temperature, humidity and screen aperture. The discriminator determines whether the environment generated by the generator is real, and continuously optimizes the simulation ability of the generator by comparing it with the real data. A large amount of simulation data was generated using a generative adversarial network model to expand the historical data set. Multiple simulation experiments were conducted in a virtual environment to explore the effects of different parameter combinations on the activity and particle size of activated magnesium oxide and find the optimal parameter combination.

7. The method for preparing the dephosphorization and defluorination agent according to claim 6, characterized in that: Establish a reinforcement learning model for adaptive reinforcement learning, define the state space, including key parameters of real-time temperature, humidity, particle size distribution and mesh aperture; define the action space, including operations such as adjusting the drying temperature and changing the mesh aperture; Design a reward function to give the agent corresponding rewards or penalties based on the activity and particle size consistency of the active magnesium oxide; the agent continuously learns new control strategies during the production process and dynamically adjusts the control strategy based on the simulated data and real-time data generated by the generative adversarial network; use historical data for offline training and conduct online learning during the production process to continuously optimize the agent's decision-making strategy; Use simulated data generated by generative adversarial networks to detect abnormal conditions in the production process, such as temperature fluctuations and screen damage, and issue early warnings in a timely manner; Among them, the expression of the reward function is: In the formula, R(s,a) represents the reward function, which represents the reward obtained by performing action a in state s, and α i represents the activity consistency weight, which indicates the contribution of the activity consistency of the i-th batch to the reward, β i represents the particle size consistency weight, which indicates the contribution of the particle size consistency of the i-th batch to the reward, γ i represents the anomaly detection weight, indicating the contribution of the anomaly detection of the i-th batch to the reward, δ i represents the energy consumption optimization weight, indicating the contribution of the energy consumption optimization of the i-th batch to the reward, ∈ i represents the production efficiency weight, indicating the contribution of the i-th batch production efficiency to the reward, ζ i represents the equipment life weight, indicating the contribution of the equipment life of the i-th batch to the reward, η i represents the environmental impact weight, which indicates the contribution of the environmental impact of the i-th batch to the reward, θ i Represents the quality control weight, which indicates the contribution of the quality control of the i-th batch to the reward.

8. The method for preparing the dephosphorization and defluorination agent according to claim 7, characterized in that: Specific calculation method: Among them, the activity standard deviation is the standard deviation of the activity of the i-th batch of active magnesium oxide, and the maximum activity standard deviation is the preset maximum allowable standard deviation; Among them, the particle size standard deviation is the standard deviation of the particle size of the i-th batch of activated magnesium oxide, and the maximum particle size standard deviation is the preset maximum allowable standard deviation; Energy consumption optimization = current energy consumption / target energy consumption Production efficiency; = current production volume / target production volume; Equipment life = current equipment life / target equipment life; Environmental impact = current environmental impact / target environmental impact; Quality control = current quality control index / target quality control index.

9. The method for preparing the dephosphorization and defluorination agent according to claim 4, characterized in that: The control process of high-speed stirring for mixing includes the following steps: In the initial mixing stage, the stirring speed does not exceed 50 rpm; the initial mixing time is set to 5 minutes; after the initial mixing, the stirring speed is kept below 50 rpm; the time of the uniform distribution stage is set to 3 minutes; After the low-speed stirring stage is completed, switch to the high-speed stirring stage, and the stirring speed should be no less than 300rpm; the time of the intensive mixing stage is set to 5 minutes; after the intensive mixing, the stirring speed is maintained at 300rpm; the time of the final mixing stage is set to 5-10 minutes; During the mixing process, sampling and testing should be carried out every 2 minutes. The sampling points should be evenly distributed in different positions of the mixing container. The uniformity of the mixture should be tested by microscopic observation or chemical analysis methods. The stirring speed should be adjusted according to the sampling and test results.

10. The method for preparing the dephosphorization and defluorination agent according to claim 9, characterized in that: If the test results show uneven mixing, increase the stirring speed or extend the stirring time; if the test results show excessive mixing, reduce the stirring speed or shorten the stirring time; adjust the stirring time based on the sampling test results.

Citation Information

Patent Citations

  • Synthesis method of calcium-iron-magnesium ternary nano-composite fluorine removal agent

    CN113274968A

  • Deep defluorination agent and preparation method thereof

    CN118164602A

  • Fluorine fixing and phosphorus locking and wastewater advanced treatment system and method for ardealite slag warehouse

    CN118184065A

  • Novel deep defluorinating agent and application thereof

    CN110054275A

  • Composite calcium salt fluorine removal agent as well as preparation method and application method thereof

    CN116239197A

Cited By

  • Method for jointly controlling dissolution and release of phosphorus and fluorine in phosphogypsum

    CN120391289A

  • Intelligent preparation process control method and system of compound lidocaine nano-loaded drug

    CN120595617A

  • Phosphorus and fluorine treating agent based on dolomite

    CN121222797A

  • Semiconductor fluorine-containing wastewater treatment method and system

    CN121449188A

  • Semiconductor fluorine-containing wastewater treatment method and system

    CN121449188B