Paint treatment process for surface of product shell

By grinding, washing and spraying black paint on the surface of the product shell, and forming a transparent pattern layer and a silver paint layer inside, the problem of not being able to display the operation identifier in the prior art is solved, and the identifier is hidden when not operating. And display the effect of the pattern during operation.

CN119456363APending Publication Date: 2025-02-18SHANGHAI AIPERS PURIFICATION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411948557.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-12-27
Publication Date
2025-02-18

AI Technical Summary

Technical Problem

After the existing product shell is sprayed, the operation identifier on the surface cannot be displayed, the identifier cannot be hidden when the product is not operated, and the identifier can be displayed during operation.

Method used

A paint treatment process for the surface of the product shell, including grinding, washing and shocking the surface of the shell; spraying black paint inside the shell and baking to form a black paint surface; laser engraving on the black paint surface to form a transparent pattern and spray white paint; finally spray silver paint on the surface of the shell to form a silver paint layer.

Benefits of technology

It is realized that when the light is not lit, there is no display on the surface of the shell, and the silver paint layer covers the transparent pattern layer; when the light is lit, the light penetrates the silver paint layer to display the content of the transparent pattern layer, thereby hiding and displaying the identifier. effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119456363A_ABST
    Figure CN119456363A_ABST
Patent Text Reader

Abstract

The invention discloses a paint treatment process for the surface of a product shell. The process comprises the following steps that S1, the surface of the shell is subjected to polishing treatment and then is washed and vibrated; s2, after the washed shell is naturally air-dried, black paint is sprayed to the interior of the shell, baking is carried out, and a black paint surface is formed in the shell; s3, laser etching is conducted on the black paint surface to form a needed transparent pattern layer, white paint is sprayed, and then baking is conducted; and S4, silver paint is sprayed on the surface of the shell, and baking is conducted. Through the process provided by the invention, when the product is not lighted up, the surface of the shell has no display under the action of the silver paint layer, and the silver paint layer can cover the transparent pattern layer sprayed with the white paint; the brightness of the light can penetrate through the silver paint layer to display the content of the transparent pattern layer, so that the effect that the surface seems to have no any pattern and the pattern is displayed after the light is lightened is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of paint treatment, and in particular to a paint treatment process for the surface of a product shell. Background Art

[0002] At present, paint is a kind of chemical mixture coating that can firmly cover the surface of objects and other special purposes. It has the functions of anti-corrosion, waterproof, oil-proof, chemical-resistant, light-resistant, and temperature-resistant. Furniture is exposed to the atmosphere and eroded by oxygen, moisture, etc., which will cause wood decay and other damage. Applying paint on the surface of the product shell to form a protective film can prevent or delay the occurrence and development of these damage phenomena and extend the service life of various materials.

[0003] Special graphics or text labels are attached to the surface of the product shell, and users can complete operations according to these labels. Generally, users hope that when the product is not operated, the surface of the shell does not display the operation identifier, and when the product is operated, the surface of the shell can display the operation identifier for easy use. However, after the surface of the existing product shell is painted, the operation identifier on the surface of the product shell cannot achieve the display effect. Summary of the invention

[0004] Therefore, the present invention aims to solve the deficiencies in the prior art to at least a certain extent, thereby proposing a paint treatment process for the surface of a product shell.

[0005] To achieve the above object, a technical solution adopted by the present invention is:

[0006] The present invention provides a paint treatment process for the surface of a product shell, the process comprising the following steps:

[0007] S1. Grinding the surface of the shell, washing and shaking the shell;

[0008] S2, after the washed shell is naturally air-dried, spraying black paint on the inside of the shell and baking it to form a black paint surface on the inside of the shell;

[0009] S3, performing laser engraving on the black painted surface to form a required transparent pattern layer, spraying white paint on the transparent pattern layer, and then baking;

[0010] S4, spraying silver paint on the polished surface of the shell to form a silver paint layer and baking it.

[0011] Furthermore, in the step S1, the surface of the shell is polished by using 800-1000 mesh sandpaper.

[0012] Furthermore, in the step S1, the shell is placed in anhydrous ethanol for washing, and is further shaken and dispersed under 400-500W ultrasonic waves for 10-15 minutes.

[0013] Furthermore, in step S2, the baking temperature is 40-60° C. and the baking time is 20-40 min.

[0014] Furthermore, in step S3, the temperature of the laser engraving is 500-600°C.

[0015] Furthermore, in step S3, the baking temperature is 50-60° C. and the baking time is 30-40 min.

[0016] Furthermore, in step S4, the baking temperature is 60-70° C. and the baking time is 30-40 min.

[0017] Furthermore, the thickness of the silver paint layer is 10-15 μm.

[0018] The present invention provides a paint treatment process for the surface of a product shell, and the process includes the following steps: S1, grinding the surface of the shell, washing and shaking the shell; S2, after the washed shell is naturally air-dried, black paint is sprayed on the inside of the shell and baked to form a black paint surface inside the shell; S3, laser engraving is performed on the black paint surface to form a required transparent pattern layer, and white paint is sprayed on the transparent pattern layer, and then baked; S4, silver paint is sprayed on the surface of the shell after grinding to form a silver paint layer and baked. Through the process provided by the present invention, when the product is not lit, the surface of the shell can be made to have no display under the action of the silver paint layer, and the silver paint layer will cover the transparent pattern layer sprayed with white paint. When the light is turned on, the brightness of the light will penetrate the silver paint layer to display the content of the transparent pattern layer, so as to achieve the effect that the surface seems to have no pattern, and the pattern is displayed after the light is turned on. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.

[0020] Figure 1 The figure is a schematic flow chart of the paint treatment process for the surface of the product shell of the present invention. DETAILED DESCRIPTION

[0021] In order to make the purpose, features and advantages of the invention more obvious and easy to understand, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.

[0022] Example 1

[0023] The present application embodiment provides a paint treatment process for the surface of a product shell, the process comprising the following steps:

[0024] S1. The surface of the housing is polished smooth with 800-mesh sandpaper, and the housing is washed in anhydrous ethanol and continuously shaken under 400W ultrasonic wave for 10 minutes;

[0025] S2, after the washed shell is naturally air-dried, spray black paint on the inside of the shell and bake at 40° C. for 20 minutes to form a black paint surface on the inside of the shell;

[0026] S3, performing laser laser engraving at 500° C. on the black painted surface to form a required transparent pattern layer, spraying white paint on the transparent pattern layer, and then baking at 50° C. for 30 minutes;

[0027] S4, spraying silver paint on the polished surface of the shell to form a silver paint layer with a thickness of 10 μm and baking it at a temperature of 60° C. for 30 minutes.

[0028] In this embodiment, the above steps can make the overall effect of the product shell more beautiful than existing products. When the light inside the product in the embodiment of the present application is off, no icon will be displayed on the shell, and only when the light inside the product is on will a pattern be displayed on the shell.

[0029] Specifically, the outer surface includes an outer surface and an inner surface. A silver paint layer is sprayed on the outer surface, while black paint is first sprayed on the inner surface. After forming a black paint surface, a transparent pattern layer of the pattern content to be displayed is formed on the black paint surface by laser engraving, and then white paint is sprayed on the transparent pattern layer. In this way, the outer shell will not display anything when there is no light inside the product. The silver paint layer will cover the transparent pattern layer inside the outer shell sprayed with white paint. When the light inside the product is on, the brightness of the light will penetrate the silver paint layer to display the values ​​and icons displayed by the transparent pattern layer.

[0030] Among them, the transparent pattern layer is the numerical value and icon that needs to be displayed on the product shell, which is set according to the needs of the user. The content of the transparent pattern layer is not limited here and is set according to actual production needs.

[0031] Among them, white paint is sprayed on the transparent pattern layer so that the light can better and evenly display the content on the transparent pattern layer on the product shell.

[0032] Example 2

[0033] The present application embodiment provides a paint treatment process for the surface of a product shell, the process comprising the following steps:

[0034] S1. The surface of the housing is polished smooth with 900-grit sandpaper, and the housing is washed in anhydrous ethanol and continuously shaken under 450W ultrasonic wave for 15 minutes;

[0035] S2, after the washed shell is naturally air-dried, black paint is sprayed on the inside of the shell and baked at a temperature of 45° C. for 30 minutes to form a black paint surface on the inside of the shell;

[0036] S3, performing laser laser engraving at 550° C. on the black painted surface to form a required transparent pattern layer, spraying white paint on the transparent pattern layer, and then baking at 55° C. for 35 minutes;

[0037] S4, spraying silver paint on the polished surface of the shell to form a silver paint layer with a thickness of 12 μm and baking it at a temperature of 65° C. for 35 minutes.

[0038] Example 3

[0039] The present application embodiment provides a paint treatment process for the surface of a product shell, the process comprising the following steps:

[0040] S1. The surface of the housing is polished smooth with 950-mesh sandpaper, and the housing is washed in anhydrous ethanol and continuously shaken under 500W ultrasonic wave for 13 minutes;

[0041] S2, after the washed shell is naturally air-dried, spray black paint on the inside of the shell and bake at a temperature of 55° C. for 35 minutes to form a black paint surface on the inside of the shell;

[0042] S3, performing laser laser engraving at 500° C. on the black painted surface to form a required transparent pattern layer, spraying white paint on the transparent pattern layer, and then baking at 58° C. for 38 minutes;

[0043] S4, spraying silver paint on the polished surface of the shell to form a silver paint layer with a thickness of 10 μm and baking it at a temperature of 68° C. for 37 minutes.

[0044] Example 4

[0045] The present application embodiment provides a paint treatment process for the surface of a product shell, the process comprising the following steps:

[0046] S1. The surface of the housing is polished smooth with 1000-mesh sandpaper, and the housing is washed in anhydrous ethanol and continuously shaken under 500W ultrasonic wave for 15 minutes;

[0047] S2, after the washed shell is naturally air-dried, spray black paint on the inside of the shell and bake at 60° C. for 40 minutes to form a black paint surface on the inside of the shell;

[0048] S3, performing laser laser engraving at 600° C. on the black painted surface to form a required transparent pattern layer, spraying white paint on the transparent pattern layer, and then baking at 60° C. for 40 minutes;

[0049] S4, spraying silver paint on the polished surface of the shell to form a silver paint layer with a thickness of 15 μm and baking it at a temperature of 70° C. for 40 minutes.

[0050] In summary, the present invention provides a paint treatment process for the surface of a product shell, and the process includes the following steps: S1, grinding the surface of the shell, washing and shaking the shell; S2, after the washed shell is naturally air-dried, black paint is sprayed on the inside of the shell and baked to form a black paint surface inside the shell; S3, laser engraving is performed on the black paint surface to form the required transparent pattern layer, and white paint is sprayed on the transparent pattern layer, and then baked; S4, silver paint is sprayed on the surface of the shell after grinding to form a silver paint layer and baked. Through the process provided by the present invention, when the light of the product is not turned on, the surface of the shell can be made to have no display under the action of the silver paint layer, and the silver paint layer will cover the transparent pattern layer sprayed with white paint. When the light is turned on, the brightness of the light will penetrate the silver paint layer to display the content of the transparent pattern layer, so as to achieve the effect that the surface seems to have no pattern, and the pattern is displayed after the light is turned on.

[0051] Each functional module in each embodiment of the present invention may be integrated into a processing module, or each module may exist physically separately, or two or more modules may be integrated into one module. The above-mentioned integrated module may be implemented in the form of hardware or in the form of a software functional module. If the integrated module is implemented in the form of a software functional module and sold or used as an independent product, it may be stored in a computer-readable storage medium.

[0052] Based on this understanding, the technical solution of the specification of the present invention, in essence or in other words, the part that contributes to the prior art or the whole or part of the technical solution can be embodied in the form of a software product, which is stored in a storage medium and includes several instructions for enabling a computer device (which can be a personal computer, a server, or a network device, etc.) to perform all or part of the steps of the process described in each embodiment of the present invention. The aforementioned storage medium includes: U disk, mobile hard disk, read-only memory (ROM, Read-Only Memory), random access memory (RAM, Random Access Memory), disk or optical disk, etc., various media that can store program codes.

[0053] It should be noted that, for the aforementioned method embodiments, for the sake of simplicity of description, they are all expressed as a series of action combinations, but those skilled in the art should be aware that the present invention is not limited by the described order of actions, because according to the present invention, certain steps can be performed in other orders or simultaneously. Secondly, those skilled in the art should also be aware that the embodiments described in the specification are all preferred embodiments, and the actions and modules involved are not necessarily required by the present invention. In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, please refer to the relevant description of other embodiments.

[0054] For those skilled in the art, according to the concept of the embodiments of the present application, there may be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as limiting the present invention.

Claims

1. A paint treatment process for the surface of a product shell, characterized in that: The process comprises the following steps: S1, grinding the surface of the shell, washing and shaking the shell; S2, after the washed shell is naturally air-dried, spraying black paint on the inside of the shell and baking it to form a black paint surface on the inside of the shell; S3, performing laser engraving on the black painted surface to form a required transparent pattern layer, spraying white paint on the transparent pattern layer, and then baking; S4, spraying silver paint on the polished surface of the shell to form a silver paint layer and baking it.

2. The paint treatment process for the product shell surface according to claim 1 is characterized in that: In the step S1, the surface of the housing is polished using 800-1000 mesh sandpaper.

3. The paint treatment process for the product shell surface according to claim 1 is characterized in that: In the step S1, the shell is placed in anhydrous ethanol for washing, and is further shaken and dispersed under 400-500W ultrasonic waves for 10-15 minutes.

4. The paint treatment process for the product shell surface according to claim 1, characterized in that: In step S2, the baking temperature is 40-60° C. and the baking time is 20-40 minutes.

5. The paint treatment process for the product shell surface according to claim 1, characterized in that: In step S3, the temperature of the laser engraving is 500-600°C.

6. The paint treatment process for the product shell surface according to claim 1, characterized in that: In step S3, the baking temperature is 50-60° C. and the baking time is 30-40 minutes.

7. The paint treatment process for the product shell surface according to claim 1, characterized in that: In step S4, the baking temperature is 60-70° C. and the baking time is 30-40 minutes.

8. The paint treatment process for the product shell surface according to claim 1, characterized in that: The thickness of the silver paint layer is 10-15 μm.