Method for improving single crystal particle defect yield and product thereof

By changing the liquid port distance fluctuation at a fixed pull speed during single crystal growth and optimizing the diameter and stress distribution of crystal rods, the problem of low single crystal particle defects is solved, and the quality and yield of single crystal silicon rods are improved to meet the needs of high-integration chips and power devices.

CN120425449APending Publication Date: 2025-08-05FERROTEC (NINGXIA) SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510693663.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-27
Publication Date
2025-08-05

AI Technical Summary

Technical Problem

In the prior art, the partial defect yield of single crystal materials is low, resulting in reduced performance and poor reliability of semiconductor devices, especially in high-integration chips and power devices.

Method used

During the growth of single crystals, the liquid opening distance is changed at a fixed pull speed to make it fluctuate within a certain range. By accurately controlling the fluctuation range and frequency of the liquid opening distance, the diameter and stress distribution of the crystal rod are optimized, and partial defects are reduced.

Benefits of technology

By optimizing the stress distribution and crystal structure inside the crystal rod, the quality and yield of the single crystal silicon rod are significantly improved, and the improvement of the quality and yield of the single crystal silicon rod is about 18%, reducing production costs and improving corporate efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120425449A_ABST
    Figure CN120425449A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of semiconductor material processing, and particularly relates to a method for improving the single crystal particle defect yield and a product thereof, and the method comprises the following steps: under a fixed pulling speed, the condition of a contact interface between a molten silicon liquid and a crystal bar can be changed by deliberately fluctuating a liquid port distance, so that the growth rate and diameter of the crystal bar are influenced, and the yield of the single crystal particle defect is improved. By accurately controlling the fluctuation range of the liquid opening distance, the particle defect in the crystal can be reduced, and the quality and yield of the silicon single crystal rod are improved. Specifically, when the liquid opening distance is increased, the contact area between the molten silicon liquid and the crystal bar is reduced, and the growth rate of the crystal bar is possibly reduced; conversely, when the liquid opening distance is reduced, the contact area is increased, and the growth rate of the crystal bar can be increased. By accurately controlling the fluctuation range and frequency of the liquid port distance, the diameter of the crystal bar can fluctuate within the range of + / -0.3 mm, and the tiny diameter change is beneficial to optimization of stress distribution and crystal structure in the crystal bar, so that generation of particle defects is reduced, and the yield of the particle defects is improved by about 18%.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of semiconductor material processing, and particularly relates to a method for improving the defect yield rate of single crystal particles and a product thereof. Background Art

[0002] High-quality single-crystal materials are the foundation for manufacturing high-performance semiconductor devices. In the integrated circuit field, with the continuous increase in chip integration, the requirements for the purity, crystal integrity, and defect control of single-crystal materials are becoming increasingly stringent. Even tiny defects can lead to reduced chip performance, increased power consumption, or even failure, thus affecting the performance and reliability of the entire electronic device. In power devices, high-quality single-crystal materials can improve the device's voltage resistance and reduce on-resistance, thereby improving energy conversion efficiency and meeting the demand for efficient and reliable power devices in new energy vehicles, smart grids, and other fields. Therefore, improving the quality of single-crystal materials, especially reducing the yield of particle defects, is of great significance to promoting the development of the semiconductor industry.

[0003] V / G (the ratio of pulling speed to axial temperature gradient) is a key parameter influencing the formation of microdefects during single crystal growth. In actual production, to control the ingot diameter, the pulling speed is typically adjusted while maintaining a constant gap (Gap). While this method can maintain ingot diameter within a ±0.1mm range, it results in significant fluctuations in the pulling speed. Fluctuations in pulling speed can significantly alter the V / G value, making it unstable. When the V / G value deviates from the optimal range, it alters the thermodynamic and kinetic conditions of crystal growth, promoting the generation and proliferation of particle defects. For example, excessively high V / G values can lead to excessive vacancies during crystal growth, which aggregate to form particle defects. Excessively low V / G values can lead to the proliferation and aggregation of dislocations, similarly reducing the yield of single crystal particle defects. Particle defects can reduce the performance and reliability of semiconductor devices, such as increasing leakage current, reducing breakdown voltage, and affecting switching speed and stability, severely impacting the quality and market competitiveness of semiconductor products. Summary of the Invention

[0004] In view of this, the present invention provides a method and product for improving the defect yield of single crystal particles to solve the above-mentioned technical problems caused by the low defect yield of single crystal particles in the prior art.

[0005] To achieve the above objectives, this application adopts the following scheme: A method for improving the defect yield of single crystal particles involves varying the standard liquid nozzle distance at a fixed pulling speed during the constant diameter process, causing the standard liquid nozzle distance to fluctuate. This fluctuation in the standard liquid nozzle distance allows the diameter of the crystal rod to fluctuate within a range of ±0.3 mm. This slight diameter change helps optimize the stress distribution and crystal structure within the crystal rod, suppressing the generation of particle defects.

[0006] Preferably, the fixed pulling speed is 0.43 mm / min-0.44 mm / min.

[0007] Preferably, the standard liquid port distance is 60±0.1 mm.

[0008] Preferably, the standard liquid port distance fluctuates within a range of ±1 mm.

[0009] Preferably, the standard liquid port distance fluctuates within a range of ±0.3 mm.

[0010] Preferably, during the equal diameter process, the crucible rotation speed is 1.1 rpm-1.2 rpm, and the crystal rod rotation speed is 6.5 rpm-8 rpm.

[0011] Preferably, during the iso-diameter process, the furnace pressure is 4KPa-8KPa, and the argon flow rate is 100slm-150slm.

[0012] Preferably, during the equal diameter process, the magnetic field strength is 3000Gs-3500Gs.

[0013] Preferably, during the iso-diameter process, the water flow rate of the water-cooling jacket is fixed at 50±2 SLM / min, and the temperature is fixed at 24±1.5°C.

[0014] The single crystal product is prepared according to the above method for improving the defect yield of single crystal particles.

[0015] In the above-mentioned method for improving the yield rate of single crystal particle defects, by intentionally fluctuating the liquid nozzle distance at a fixed pulling speed, the conditions of the contact interface between the molten silicon liquid and the crystal rod can be changed, thereby affecting the growth rate and diameter of the crystal rod. By precisely controlling the fluctuation range of the liquid nozzle distance, the particle defects in the crystal can be reduced, and the quality and yield of the single crystal silicon rod can be improved. Specifically, when the liquid nozzle distance increases, the contact area between the molten silicon liquid and the crystal rod decreases, which may slow down the growth rate of the crystal rod; conversely, when the liquid nozzle distance decreases, the contact area increases, which may accelerate the growth rate of the crystal rod. By precisely controlling the fluctuation range and frequency of the liquid nozzle distance, the diameter of the crystal rod can be made to fluctuate within the range of ±0.3mm. This slight diameter change helps to optimize the stress distribution and crystal structure inside the crystal rod, thereby reducing the generation of particle defects and improving the particle defect yield by about 18%. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 This is a diagram of the crystal simulation results under the first condition in the embodiment.

[0017] Figure 2 This is a diagram of the crystal simulation results under the second condition in the embodiment.

[0018] Figure 3 1 is a comparison chart of the yield of the crystal rods prepared in the embodiment and the comparative example. DETAILED DESCRIPTION

[0019] To facilitate understanding of the present application, a more comprehensive description of the present application will be provided below with reference to the accompanying drawings. Preferred embodiments of the present application will also be described. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided to provide a more thorough and comprehensive understanding of the disclosure of the present application.

[0020] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this application pertains. The terms used herein in the specification of this application are for the purpose of describing specific embodiments only and are not intended to limit this application. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.

[0021] A method for improving the defect yield of single crystal particles involves varying the standard liquid nozzle distance at a fixed pulling speed during the constant diameter process, causing the standard liquid nozzle distance to fluctuate. This fluctuation in the standard liquid nozzle distance allows the diameter of the crystal rod to fluctuate within a range of ±0.3 mm. This slight diameter change helps optimize the stress distribution and crystal structure within the crystal rod, suppressing the generation of particle defects.

[0022] During the pulling process of the single crystal silicon rod, especially in the isodiameter growth stage, the specific operation process of this method is as follows: First, determine and fix the crystal pulling speed (pulling rate), which is a key parameter for controlling the growth rate of the crystal rod. At the same time, set a standard liquid mouth distance, that is, the distance between the molten silicon liquid and the seed crystal or the bottom of the grown crystal rod, which is an important factor affecting the diameter and growth quality of the crystal rod. Under the condition of a fixed pulling speed, begin to consciously change the standard liquid mouth distance so that it fluctuates within a certain range. For example, the size of the liquid mouth distance can be changed by changing the lifting and lowering of the crucible. While the liquid mouth distance fluctuates, the diameter of the crystal rod is monitored in real time using an online diameter measuring device (such as a laser diameter gauge). The goal is to control the fluctuation range of the crystal rod diameter within ±0.3mm. The method provided in this application can change the conditions of the contact interface between the molten silicon liquid and the crystal rod by intentionally fluctuating the liquid mouth distance at a fixed pulling speed, thereby affecting the growth rate and diameter of the crystal rod. By precisely controlling the fluctuation range of the liquid mouth distance, particle defects in the crystal can be reduced and the quality and yield of the single crystal silicon rod can be improved. Specifically, when the nozzle distance increases, the contact area between the molten silicon and the crystal ingot decreases, potentially slowing the ingot's growth rate. Conversely, when the nozzle distance decreases, the contact area increases, potentially accelerating the ingot's growth rate. By precisely controlling the fluctuation range and frequency of the nozzle distance, the ingot's diameter can be adjusted to within a ±0.3mm range. This slight diameter variation helps optimize the stress distribution and crystal structure within the ingot, suppressing the generation of particle defects.

[0023] Specifically, the fixed pulling speed is 0.43 mm / min-0.44 mm / min.

[0024] The method provided in the present application fixes the pulling speed within the range of 0.43 mm / min to 0.44 mm / min during the equal-diameter process, which can ensure that the thermal stress and mechanical stress to which the crystal rod is subjected during the growth process are relatively uniform, and reduce growth defects caused by fluctuations in the pulling speed. Within this pulling speed range, the growth rate of the crystal rod is moderate, which is conducive to the formation of a uniform and dense crystal structure. This structure helps to reduce defects such as dislocations and vacancies in the crystal, especially particle defects, thereby improving the quality and yield of single crystal silicon rods.

[0025] In order to provide a clear and precise liquid nozzle distance standard during the pulling process of single crystal silicon rods, especially in the isodiameter growth stage, to ensure the stability and consistency of the crystal rod growth environment, specifically, the standard liquid nozzle distance is 60±0.1mm.

[0026] Specifically, the standard liquid port distance fluctuates within a range of ±1 mm.

[0027] By allowing the standard liquid nozzle distance to fluctuate within a range of ±1mm, a certain amount of growth disturbance can be introduced. This disturbance helps to break the local imbalance that may form during the growth process, promotes uniform mixing of the molten silicon liquid and uniform crystal growth. These optimized growth conditions help reduce impurities and particle defects in the crystal, helping to improve the yield of single crystal silicon rods. An increase in yield means more qualified products, thereby reducing production costs and improving the company's economic benefits.

[0028] Preferably, the standard liquid port distance fluctuation is within the range of ±0.3 mm, which has a better effect.

[0029] During the calibrating process, the crucible speed is 1.1-1.2 rpm, and the ingot speed is 6.5-8 rpm. This specific range of crucible speed of 1.1-1.2 rpm and ingot speed of 6.5-8 rpm provides precise process parameter guidance for the calibrating process of single crystal growth. This precise control helps stabilize the growth environment, reduces the adverse effects of speed fluctuations, and makes the single crystal growth process more controllable.

[0030] During the isobaric process, the furnace pressure is 4KPa-8KPa, and the argon flow rate is 100slm-150slm. Controlling the furnace pressure within this specific range creates a relatively stable and suitable physical environment for single crystal growth. Stable furnace pressure helps maintain uniform gas distribution within the furnace and reduces disturbances to the single crystal growth interface caused by pressure fluctuations. The appropriate argon flow rate ensures stable flow of the furnace atmosphere, removing impurities and heat generated during the growth process, creating favorable conditions for single crystal growth. Growing single crystals within this range optimizes thermal convection and material transfer between the melt and the crystal, reduces the accumulation and aggregation of impurities at the crystal growth interface, avoids particle defects caused by impurities or abnormal growth, and significantly improves the yield of single crystal particle defects.

[0031] In a specific embodiment, during the isodiametric process, the magnetic field strength is 3000-3500 Gs. A magnetic field strength within this range can promote the growth of atoms or molecules within the crystal according to a more regular lattice arrangement, improving the crystallization quality of the crystal. By suppressing disordered growth and defect formation during crystal growth, the magnetic field helps reduce defects such as dislocations and stacking faults within the crystal, while also indirectly reducing the generation of particle defects, thereby improving the overall yield of the single crystal.

[0032] In a specific embodiment, during the isodiameter process, the water flow rate of the water-cooling jacket is fixed at 50±2SLM / min and the temperature is fixed at 24±1.5°C. Fixing the water flow rate of the water-cooling jacket at 50±2SLM / min and the temperature at 24±1.5°C can provide a stable and predictable cooling effect for the single crystal growth area. Stable cooling conditions help to form a uniform and suitable temperature gradient near the crystal growth interface, which is crucial for the orderly growth of single crystals. The appropriate temperature gradient can guide the crystal to grow in a predetermined crystal direction, reduce the growth direction deviation and structural disorder caused by temperature changes, and thus reduce the generation of particle defects.

[0033] The single crystal product is prepared according to the above method for improving the defect yield of single crystal particles.

[0034] The following is a detailed description of the technical solutions and effects of the present invention. It should be noted that the following examples are only intended to further explain the present invention and do not limit the technical solutions of the present invention. Example

[0035] First, the crystal pulling conditions are designed and simulated using the crystal ANSYS simulation software for analysis. The simulated crystal pulling conditions are divided into the first condition and the second condition, which are as follows: The first condition is: GAP=A; SL=B-0.6, SL=B, SL=B+0.6, where GAP is the liquid nozzle distance, SL is the casting speed, A is the standard liquid nozzle distance, and B is the fixed casting speed; The second condition is: SL=B; GAP=A-0.3, GAP=A, GAP=A+0.3, where GAP is the liquid nozzle distance, SL is the casting speed, A is the standard liquid nozzle distance, and B is the fixed casting speed; The above two conditions are used to simulate the effects of casting speed fluctuation and GAP fluctuation on V / G. The simulation results under the first condition are as follows: Figure 1 As shown in the second condition, the simulation results are as follows Figure 2 As shown, by comparison Figure 1 and Figure 2 It can be seen that under the second condition, the change in V / G value is smaller than that under the first condition, that is, under the second condition, the influence of V / G is smaller than that under the first condition. Therefore, crystal pulling can be performed using the method under the second condition.

[0036] In the constant diameter stage, the pulling speed is fixed at 0.43mm / min-0.44mm / min, the standard liquid nozzle distance is 60±0.1mm, and the standard liquid nozzle distance fluctuation is within the range of ±0.3mm. The other steps are the same as the traditional process steps. Under this condition, the crystal rod is pulled and repeated ten times. The particle defect yield is calculated. Figure 3 shown.

[0037] Comparative Example In the equal diameter stage, the same furnace as in the above embodiment is used, but the pulling speed is not fixed. The pulling speed is fluctuated within the range of 0.6 mm / min. Then the standard liquid mouth distance is fixed, that is, the standard liquid mouth distance does not fluctuate, and the standard liquid mouth distance is 60±0.1 mm. The other steps are the same as the traditional process steps. Under this condition, a crystal rod is pulled and repeated ten times. The particle defect yield is calculated. Figure 3 shown.

[0038] From the particle yield results ( Figure 3 ), compared with the comparative example, the method provided by the present application in the embodiment not only greatly improves the yield by about 18%, but also improves the stability of the yield.

[0039] The above description is only a specific embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any technician familiar with this technical field can easily think of various equivalent modifications or replacements within the technical scope disclosed by the present invention, and these modifications or replacements should all be included in the scope of protection of the present invention.

Claims

1. A method for improving the defect yield of single crystal particles, characterized in that: During the equal diameter process, at a fixed pulling speed, the standard liquid nozzle distance is changed to fluctuate. The fluctuation of the standard liquid nozzle distance makes the diameter of the crystal rod fluctuate within the range of ±0.3mm. This slight diameter change helps to optimize the stress distribution and crystal structure inside the crystal rod and suppress the generation of particle defects.

2. The method for improving the defect yield of single crystal particles according to claim 1, characterized in that: The fixed pulling speed is 0.43 mm / min-0.44 mm / min.

3. The method for improving the defect yield of single crystal particles according to claim 1, characterized in that: The standard liquid port distance is 60±0.1 mm.

4. The method for improving the defect yield of single crystal particles according to claim 3, characterized in that: The standard liquid port distance fluctuates within the range of ±1 mm.

5. The method for improving the defect yield of single crystal particles according to claim 3, characterized in that: The standard liquid port distance fluctuates within the range of ±0.3 mm.

6. The method for improving the defect yield of single crystal particles according to claim 1, characterized in that: During the equal diameter process, the crucible rotation speed is 1.1rpm-1.2rpm, and the crystal rod rotation speed is 6.5rpm-8rpm.

7. The method for improving the defect yield of single crystal particles according to claim 1, characterized in that: During the equal diameter process, the furnace pressure is 4Kpa-8Kpa, and the argon flow rate is 100slm-150slm.

8. The method for improving the defect yield of single crystal particles according to claim 1, characterized in that: During the equal diameter process, the magnetic field strength is 3000Gs-3500Gs.

9. The method for improving the defect yield of single crystal particles according to claim 1, characterized in that: During the isodiameter process, the water flow rate of the water-cooling jacket is fixed at 50±2SLM / min and the temperature is fixed at 24±1.5℃.

10. A single crystal product prepared according to the method for improving the defect yield of single crystal particles according to any one of claims 1 to 9.