Silicon carbide single-photon detector and preparation method thereof

By growing a silicon carbide multiplication layer and an aluminum gallium nitride absorption layer on a silicon carbide substrate, the problem of low responsivity in solar-blind detection of silicon carbide single-photon detectors was solved, achieving high sensitivity and low loss solar-blind photon detection.

CN121310668APending Publication Date: 2026-01-09THE 13TH RES INST OF CHINA ELECTRONICS TECH GRP CORP
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202511722183.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-11-21
Publication Date
2026-01-09

AI Technical Summary

Technical Problem

Existing silicon carbide single-photon detectors have low responsivity in solar-blind detection, mainly due to photon loss caused by filters.

Method used

The structure employs a silicon carbide multiplication layer and an aluminum gallium nitride (AGL) absorption layer grown on a silicon carbide substrate. The AGL absorption layer absorbs photons only in the solar blind band and transmits them in the solar blind outer band, thus avoiding the use of filters. Furthermore, the absorption multiplication separation structure reduces the impact of heteroepitaxial defects.

Benefits of technology

It improves detection responsivity, reduces photon loss, enhances signal-to-noise ratio, and reduces the impact of dark current and breakdown voltage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121310668A_ABST
    Figure CN121310668A_ABST
Patent Text Reader

Abstract

The invention provides a silicon carbide single-photon detector and a preparation method thereof, and relates to the technical field of silicon carbide solar blind detection. The silicon carbide multiplication layer and the aluminum gallium nitrogen absorption layer of different material systems are sequentially grown on the silicon carbide substrate, and the side, far away from the silicon carbide substrate, of the aluminum gallium nitrogen absorption layer is the light incidence side, so that incident light firstly passes through the aluminum gallium nitrogen absorption layer and is excited to generate current carriers, and then the current carriers are multiplied by the multiplication layer to generate internal gain, so that the light emitting efficiency is improved. The detection sensitivity is improved. The forbidden bandwidth range of the aluminum gallium nitrogen absorption layer coincides with the photon energy range of the solar-blind wave band, so that the aluminum gallium nitrogen absorption layer only absorbs the solar-blind wave band and transmits the wave band outside the solar-blind wave band, absorption of photons outside the solar-blind wave band when a silicon carbide absorption layer is adopted is avoided, light filtering in a light filter mode is also avoided, and the detection responsivity is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of silicon carbide solar blind detection technology, and in particular to a silicon carbide single-photon detector and its fabrication method. Background Technology

[0002] Photodetectors based on wide-bandgap semiconductor silicon carbide, such as avalanche ultraviolet single-photon detectors, utilize the collisional ionization avalanche multiplication effect of charge carriers under high electric field conditions to achieve high device gain. This results in advantages such as high sensitivity, high reliability, small size, and ease of integration. They have broad application prospects in fields such as fire detection, communication, corona monitoring, and remote sensing.

[0003] A typical structure for a silicon carbide (SiC) single-photon detector includes a SiC substrate, a SiC absorber layer, and a SiC multiplication layer. Based on homoepitaxy, SiC detectors have a lower epitaxial defect density and outperform heteroepitaxy gallium nitride (GaN) detectors. SiC materials offer advantages in visible-blind detection; however, when applied to solar-blind detection, SiC absorbs photons not only within but also outside the solar-blind band, resulting in a low signal-to-noise ratio (SNR). Existing methods typically involve adding filters, such as optical thin-film interference filters, to filter out incident light outside the solar-blind band, allowing only the incident light in the solar-blind band to pass through, thus improving the SNR. However, the filters themselves introduce photon loss, which reduces the detector's responsivity. Summary of the Invention

[0004] This invention provides a silicon carbide single-photon detector and its fabrication method to solve the problem of low responsivity caused by filters in existing silicon carbide single-photon solar-blind detectors.

[0005] In a first aspect, embodiments of the present invention provide a silicon carbide single-photon detector, comprising: a silicon carbide substrate; a silicon carbide multiplication layer disposed on the silicon carbide substrate; the silicon carbide multiplication layer being obtained by homoepitaxial growth of the silicon carbide substrate; an aluminum gallium nitride (AGL) absorber layer disposed on the silicon carbide multiplication layer; wherein the AGL absorber layer being obtained by heteroepitaxial growth of the silicon carbide multiplication layer; the doping concentration of the AGL absorber layer being no higher than the doping concentration of the silicon carbide multiplication layer, and the thickness of the AGL absorber layer being greater than the thickness of the silicon carbide multiplication layer; the bandgap range of the AGL absorber layer coinciding with the photon energy range of the solar-blind band; and the light incident direction of the detector being the direction from the AGL absorber layer toward the silicon carbide multiplication layer.

[0006] Secondly, embodiments of the present invention provide a method for fabricating a silicon carbide single-photon detector, comprising: homoepitaxially growing a silicon carbide multiplication layer on a silicon carbide substrate; heteroepitaxially growing an aluminum gallium nitride (AGaN) absorption layer on the silicon carbide multiplication layer; wherein the doping concentration of the AGaN absorption layer is not higher than the doping concentration of the silicon carbide multiplication layer, and the thickness of the AGaN absorption layer is greater than the thickness of the silicon carbide multiplication layer; the bandgap range of the AGaN absorption layer coincides with the photon energy range of the solar blind band; after epitaxially growing the AGaN absorption layer, a silicon carbide single-photon detector is fabricated, wherein the light incident direction of the detector is the direction from the AGaN absorption layer toward the silicon carbide multiplication layer.

[0007] In one possible implementation, before epitaxially growing a silicon carbide multiplication layer on a silicon carbide substrate, the method further includes: epitaxially growing a silicon carbide ohmic contact layer on the front side of the silicon carbide substrate; correspondingly, after epitaxially growing an aluminum gallium nitride (AGaN) absorber layer, fabricating a silicon carbide single-photon detector includes: epitaxially growing an AGaN ohmic contact layer on the AGaN absorber layer; after growing the AGaN ohmic contact layer, etching a mesa until the silicon carbide ohmic contact layer outside the mesa region is exposed; and fabricating ohmic contact electrodes on the AGaN ohmic contact layer within the mesa region and the silicon carbide ohmic contact layer outside the mesa region, respectively, to obtain a silicon carbide single-photon detector.

[0008] In one possible implementation, the silicon carbide ohmic contact layer is P-type and the aluminum gallium nitride ohmic contact layer is N-type; or, the silicon carbide ohmic contact layer is N-type and the aluminum gallium nitride ohmic contact layer is P-type.

[0009] In one possible implementation, after fabricating ohmic contact electrodes on the aluminum gallium nitride ohmic contact layer in the mesa region and the silicon carbide ohmic contact layer outside the mesa region, the method further includes: fabricating a passivation layer outside the ohmic contact electrode region.

[0010] In one possible implementation, after preparing the passivation layer, an anti-reflection layer is prepared on the surface of the silicon carbide single-photon detector.

[0011] In one possible implementation, the aluminum gallium nitride absorber layer is an aluminum composition gradually varying layer; the proportion of aluminum composition gradually decreases from bottom to top.

[0012] In one possible implementation, after epitaxially growing a silicon carbide multiplication layer on a silicon carbide substrate, the method further includes epitaxially growing a silicon carbide charge control layer on the silicon carbide multiplication layer.

[0013] In one possible implementation, the doping concentration of the aluminum gallium nitride absorber layer is in the range of 1 × 10⁻⁶. 15 cm -3 Up to 1×10 16 cm -3 .

[0014] In one possible implementation, the thickness of the aluminum gallium nitride absorber layer ranges from 0.1 to 0.5 micrometers.

[0015] This invention provides a silicon carbide single-photon detector and its fabrication method. By sequentially growing a silicon carbide multiplication layer and an aluminum gallium nitride (AGaN) absorber layer of different material systems on a silicon carbide substrate, with the AGaN absorber layer facing away from the silicon carbide substrate as the light incident side, the incident light first passes through the AGaN absorber layer, exciting carriers, which are then multiplied by the multiplication layer to generate internal gain, thus improving detection sensitivity. The bandgap range of the AGaN absorber layer coincides with the photon energy range of the solar-blind band, allowing the AGaN absorber layer to absorb only the solar-blind band and transmit beyond it. This avoids the absorption of photons outside the solar-blind band as with a silicon carbide absorber layer and also avoids the need for filtering, improving detection responsivity. Having one side of the AGaN absorber layer as the light incident side also avoids absorption of incident light by the silicon carbide substrate during back-incidence, reducing incident light loss and further improving detection responsivity. In addition, by adopting an absorption multiplication separation structure, the voltage division of the aluminum gallium nitride absorption layer is reduced. This not only has the advantages of low dark current and high breakdown voltage of silicon carbide homoepitaxial materials, but also reduces the impact of defects in heteroepitaxially grown aluminum gallium nitride materials on the device's dark current and breakdown voltage. Attached Figure Description

[0016] Figure 1 This is a schematic diagram of the structure of a silicon carbide single-photon detector in the prior art; Figure 2 This is a schematic diagram of the structure of a silicon carbide single-photon detector provided in an embodiment of the present invention; Figure 3 This is a flowchart illustrating the implementation of the silicon carbide single-photon detector fabrication method provided in this embodiment of the invention. Figure 4 This is a schematic diagram of another silicon carbide single-photon detector provided in an embodiment of the present invention; Figure 5 This is a schematic diagram of the structure of the third type of silicon carbide single-photon detector provided in the embodiments of the present invention. Detailed Implementation

[0017] To enable those skilled in the art to better understand this solution, the technical solutions in the embodiments of this solution will be clearly described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this solution, not all of them. Based on the embodiments of this solution, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of this solution.

[0018] The term "comprising" and any other variations thereof in the specification, claims, and accompanying drawings of this invention mean "including but not limited to," and are intended to cover a non-exclusive inclusion, not limited to the examples listed herein. Furthermore, the terms "first" and "second," etc., are used to distinguish different objects, not to describe a specific order.

[0019] The implementation of the present invention will be described in detail below with reference to the accompanying drawings: The application scenario of this invention is a solar-blind photodetector. For example, an avalanche ultraviolet single-photon detector.

[0020] Figure 1 This is a schematic diagram of the structure of a silicon carbide single-photon detector in the prior art; see reference. Figure 1 A silicon carbide (SiC) single-photon detector, from bottom to top, comprises a SiC substrate, a SiC multiplication layer, and a SiC absorber layer. This structure is a homoepitaxial SiC detector, meaning the substrate, absorber layer, and multiplication layer are all made of the same material. Homoepitaxial SiC detectors have a lower epitaxial defect density, which improves carrier transport efficiency, reduces dark current and noise, and enhances device stability and lifetime. For reference, gallium nitride (GaN) detectors typically grow a GaN epitaxial layer on a sapphire substrate, which is heteroepitaxial and has a higher epitaxial defect density. Therefore, in the field of detectors, SiC materials have advantages over GaN materials.

[0021] Solar-blind detection requires detectors to respond only to solar-blind wavelengths. For example, the solar-blind wavelength range typically refers to deep ultraviolet light in the 200–280 nm range. When silicon carbide is used in solar-blind detection, because silicon carbide absorbs photons not only within but also outside the solar-blind wavelength range, the detected signal contains both solar-blind wavelength signals and noise from outside the range, resulting in a low signal-to-noise ratio for the detector.

[0022] In existing methods, filters are typically mounted on the light incident path of the detector. For example, a filter is mounted between the optical lens and the detector chip. The filter filters out incident light except in the solar-blind band, transmitting only the incident light in the solar-blind band. This allows the silicon carbide absorption layer to absorb only photons in the solar-blind band, resulting in only solar-blind band signals being detected, thus improving the detector's signal-to-noise ratio. The disadvantage of adding a filter is increased photon loss, causing a decrease in detector responsivity, especially in single-photon detection applications. For example, the incident light intensity must be at least greater than the filter's loss to be detected.

[0023] The present invention addresses the problem of low responsivity of silicon carbide single-photon detectors by combining a silicon carbide multiplication layer with an aluminum gallium nitride absorption layer that absorbs only the solar blind band.

[0024] Figure 2 This is a schematic diagram of the structure of a silicon carbide single-photon detector provided in an embodiment of the present invention; see reference. Figure 2 This invention provides a silicon carbide single-photon detector, comprising: a silicon carbide substrate; a silicon carbide multiplication layer disposed on the silicon carbide substrate; the silicon carbide multiplication layer being obtained by homoepitaxial growth of the silicon carbide substrate; an aluminum gallium nitride (AGL) absorption layer disposed on the silicon carbide multiplication layer; wherein the AGL absorption layer is obtained by heteroepitaxial growth of the silicon carbide multiplication layer; the doping concentration of the AGL absorption layer is not higher than the doping concentration of the silicon carbide multiplication layer, and the thickness of the AGL absorption layer is greater than the thickness of the silicon carbide multiplication layer; the bandgap range of the AGL absorption layer coincides with the photon energy range of the solar-blind band; and the light incident direction of the detector is the direction from the AGL absorption layer toward the silicon carbide multiplication layer.

[0025] It should be noted that the detector in this embodiment of the invention, with the silicon carbide substrate side as the bottom, sequentially includes a silicon carbide substrate, a silicon carbide multiplication layer, and an aluminum gallium nitride (AGaN) absorber layer from bottom to top. The silicon carbide multiplication layer is obtained by homoepitaxial growth based on the silicon carbide substrate. The AGaN absorber layer is obtained by heteroepitaxial growth based on the silicon carbide multiplication layer. The purpose of setting the AGaN absorber layer is to absorb photons only in the solar blind band, as described in detail in the following embodiments.

[0026] In some embodiments, the bandgap range of the aluminum gallium nitride (AGaN) absorber layer coincides with the photon energy range of the solar blind band, thereby ensuring that the AGaN absorber layer only absorbs photons in the solar blind band and does not absorb photons outside the solar blind band.

[0027] In some embodiments, the light incident direction of the detector is from the aluminum gallium nitride (AGaN) absorption layer toward the silicon carbide (SiC) multiplication layer, that is, the incident light passes sequentially through the AGaN absorption layer, the SiC multiplication layer, and the SiC substrate. Solar-blind wavelengths in the incident light are fully absorbed by the AGaN absorption layer.

[0028] Light outside the solar-blind band passes through the aluminum gallium nitride (AGaN) absorber layer and incident on the silicon carbide (SiC) multiplier layer and the SiC substrate. The AGaN absorber layer is positioned on the light incident side, which avoids absorption of the solar-blind band light by the SiC substrate in back-incidence cases, reducing solar-blind band light loss and improving detection responsivity. Conversely, if the light is back-incidence, the SiC epitaxial layer absorbs photons outside the solar-blind band before the incident light passes through the AGaN absorber layer, generating a detection signal. This signal constitutes background noise for solar-blind detection applications, resulting in high noise and a low signal-to-noise ratio.

[0029] The above explains how an aluminum gallium nitride (AGaN) absorber layer can replace a light filter. In other words, the AGaN absorber layer effectively replaces both the light filter and the silicon carbide absorber layer, thus performing both filtering and absorption functions. The following explains how to specifically address the problem of high defect density in the AGaN heteroepitaxial layer.

[0030] Based on silicon carbide (SiC) substrates, AlGaN (AlGaN-Nitrogen) is a heteroepitaxial layer, with a defect density far greater than that of homoepitaxial SiC layers. For example, when directly growing AlGaN epitaxial material on SiC, the defect density of the AlGaN layer is much higher than that of the SiC epitaxial layer due to lattice and thermal mismatches. Furthermore, different epitaxial furnaces are typically required to grow SiC and AlGaN layers separately, making the process complex. Therefore, current technologies typically employ homoepitaxial growth of SiC combined with optical filters to fabricate SiC single-photon detectors.

[0031] In some embodiments, the doping concentration of the aluminum gallium nitride absorber layer is not higher than the doping concentration of the silicon carbide multiplier layer, and the thickness of the aluminum gallium nitride absorber layer is greater than the thickness of the silicon carbide multiplier layer. It should be noted that the embodiments of the present invention employ an absorption multiplication separation structure, specifically using an aluminum gallium nitride (AGaN) absorber layer and a silicon carbide (SiC) multiplication layer. Since the electric field is mainly concentrated in the SiC multiplication layer, the voltage carrying capacity of the AGaN absorber layer is reduced, and the influence of AGaN material defects on dark current and breakdown voltage is also reduced. Therefore, the embodiments of the present invention possess the advantages of low dark current and high breakdown voltage of silicon carbide homoepitaxial materials, while also reducing the influence of defects in heteroepitaxially grown AGaN materials on the device's dark current and breakdown voltage.

[0032] Therefore, the embodiments of the present invention improve the device responsivity by using an aluminum gallium nitride (AGL) absorber layer instead of a filter, and avoid the adverse effects of a high AGL defect density by reducing the voltage drop across the AGL absorber layer.

[0033] This invention, in its embodiments, sequentially grows a silicon carbide multiplication layer and an aluminum gallium nitride (AGaN) absorber layer on a silicon carbide substrate, with the AGaN absorber layer, furthest from the silicon carbide substrate, as the light incident side. This allows incident light to first pass through the AGaN absorber layer, exciting carriers, which are then multiplied by the multiplication layer to generate a detection signal. The bandgap of the AGaN absorber layer coincides with the photon energy range of the solar-blind band, ensuring that the AGaN absorber layer only absorbs the solar-blind band and transmits beyond it. This avoids the absorption of photons outside the solar-blind band as with a silicon carbide absorber layer and also avoids the need for light filtering, thus improving detection responsivity. Having one side of the AGaN absorber layer as the light incident side also prevents absorption of incident light by the silicon carbide substrate during back-incidence, reducing incident light loss and further improving detection responsivity. In addition, by adopting an absorption multiplication separation structure, the voltage division of the aluminum gallium nitride absorption layer is reduced. This not only has the advantages of low dark current and high breakdown voltage of silicon carbide homoepitaxial materials, but also reduces the impact of defects in heteroepitaxially grown aluminum gallium nitride materials on the device's dark current and breakdown voltage.

[0034] Figure 3 This is a flowchart illustrating the implementation of the silicon carbide single-photon detector fabrication method provided in this embodiment of the invention; see also... Figure 3This invention provides a method for fabricating a silicon carbide single-photon detector, comprising: Step 301: Homoepitaxial growth of a silicon carbide multiplication layer on a silicon carbide substrate; Silicon carbide substrates provide mechanical support and lattice matching, typically high-purity, low-defect SiC single crystal wafers, such as 4H-SiC and 6H-SiC.

[0035] Epitaxial growth is a technique for directionally growing single-crystal thin films on a substrate surface. For example, chemical vapor deposition (CVD) is commonly used. By precisely controlling parameters such as temperature, gas source ratio, and growth rate, the homogeneous SiC thin film is made to have a lattice structure consistent with the substrate. Regarding homoepitaxial growth, since the SiC substrate and the SiC multiplication layer are made of the same material, the lattice mismatch is smaller, reducing defects such as dislocations and vacancies in the epitaxial layer. This ensures high crystal quality of the multiplication layer, which is beneficial for reducing multiplication noise and improving multiplication efficiency.

[0036] The silicon carbide multiplication layer is an epitaxially grown SiC thin film that serves as the functional layer responsible for carrier multiplication in a device. For example, when photons generate electron-hole pairs in the absorption layer, the carriers are accelerated by an electric field and enter the multiplication layer. Through collisional ionization, more carriers are generated, amplifying the electrical signal and improving the detector sensitivity.

[0037] Step 302: Heteroepitaxically grow an aluminum gallium nitride (AGL) absorber layer on a silicon carbide (SiC) multiplication layer; wherein the doping concentration of the AGL absorber layer is not higher than the doping concentration of the SiC multiplication layer, and the thickness of the AGL absorber layer is greater than the thickness of the SiC multiplication layer; the bandgap range of the AGL absorber layer coincides with the photon energy range of the solar blind band; It should be noted that the aluminum gallium nitride (AlGaN) absorber layer is the core layer for photon trapping and carrier generation in the detector. Solar-blind photons are incident on the absorber layer, absorbed, and then excited to excite carriers, providing the basis for subsequent carrier multiplication. For example, the solar-blind band is typically 200–300 nm, corresponding to a photon energy range of approximately 4.13–6.20 eV. The bandgap of AlGaN can be controlled by the aluminum composition; for example, a higher aluminum composition results in a larger bandgap. Adjusting the aluminum composition during epitaxial growth ensures that the bandgap of the absorber layer falls within the 4.13–6.20 eV range, thus coinciding with the photon energy range of the solar-blind band. The specific bandgap range of the absorber layer can be determined based on the target solar-blind band energy range.

[0038] Furthermore, only when photon energy is greater than or equal to the band gap can charge carriers be excited. The photon energy of solar-blind light just meets the requirement, while the photon energy of stray light such as visible light and near-infrared light is lower than the band gap and cannot be absorbed, thus achieving selective detection of solar-blind light at the material level.

[0039] In one possible implementation, the aluminum gallium nitride absorber layer is an aluminum composition gradually varying layer; the proportion of aluminum composition gradually decreases from bottom to top.

[0040] The design employs a gradually decreasing aluminum composition layer from bottom to top. Through compositional gradient modulation, this results in a gradient bandgap in the absorption layer that gradually narrows from top to bottom. For example, with the silicon carbide substrate facing downwards, the direction from the silicon carbide substrate to the aluminum gallium nitride (AGaN) absorption layer is considered bottom-to-top. Photons incident from the front of the substrate are first absorbed by the low-aluminum-composition, wide-bandgap layer for short-wavelength solar-blind light, and then by the high-aluminum-composition, narrow-bandgap layer for long-wavelength solar-blind light, avoiding insufficient absorption in certain wavelength bands due to a single composition. This ultimately forms a gradient bandgap structure, ensuring that the bandgap width of the absorption layer completely covers the photon energy range of the solar-blind wavelength band.

[0041] Step 303: After epitaxially growing the aluminum gallium nitride absorption layer, a silicon carbide single-photon detector is prepared, wherein the light incident direction of the detector is from the aluminum gallium nitride absorption layer toward the silicon carbide multiplication layer.

[0042] It should be noted that the incident light path from the AlGaN absorber layer towards the SiC multiplication layer ensures that the solar-blind light is first captured by the absorber layer, and then the charge carriers enter the multiplication layer to amplify the signal. The excited charge carriers, under the influence of the electric field, propagate towards the bonding surface and directly enter the adjacent SiC multiplication layer. The optical path is aligned with the charge carrier propagation direction, and since the SiC multiplication layer is located behind the absorber layer, it does not block the incident light, ensuring absorption efficiency.

[0043] This invention, in its embodiments, sequentially grows a silicon carbide multiplication layer and an aluminum gallium nitride (AGaN) absorber layer on a silicon carbide substrate, with the AGaN absorber layer, furthest from the silicon carbide substrate, as the light incident side. This allows incident light to first pass through the AGaN absorber layer, exciting carriers, which are then multiplied by the multiplication layer to generate a detection signal. The bandgap of the AGaN absorber layer coincides with the photon energy range of the solar-blind band, ensuring that the AGaN absorber layer only absorbs the solar-blind band and transmits beyond it. This avoids the absorption of photons outside the solar-blind band as with a silicon carbide absorber layer and also avoids the need for light filtering, thus improving detection responsivity. Having one side of the AGaN absorber layer as the light incident side also prevents absorption of incident light by the silicon carbide substrate during back-incidence, reducing incident light loss and further improving detection responsivity. In addition, by adopting an absorption multiplication separation structure, the voltage division of the aluminum gallium nitride absorption layer is reduced. This not only has the advantages of low dark current and high breakdown voltage of silicon carbide homoepitaxial materials, but also reduces the impact of defects in heteroepitaxially grown aluminum gallium nitride materials on the device's dark current and breakdown voltage.

[0044] The above highlights the main epitaxial layer fabrication steps for the device. After the epitaxial growth of the aluminum gallium nitride absorber layer, a series of processes are required to complete the device fabrication. These include electrode fabrication, dicing, and packaging and testing. The steps for fabricating the device electrodes are described below.

[0045] In one possible implementation, before epitaxially growing the silicon carbide multiplication layer on the silicon carbide substrate, the method further includes: epitaxially growing a silicon carbide ohmic contact layer on the front side of the silicon carbide substrate. Accordingly, after epitaxially growing an aluminum gallium nitride absorber layer, a silicon carbide single-photon detector is fabricated, including: Step 3031: Epitaxially grow an aluminum gallium nitride ohmic contact layer on the aluminum gallium nitride absorber layer; Step 3032: After growing the aluminum gallium nitride ohmic contact layer, etch the mesa until the silicon carbide ohmic contact layer outside the mesa area is exposed; Step 3033: Prepare ohmic contact electrodes on the aluminum gallium nitride ohmic contact layer in the mesa region and the silicon carbide ohmic contact layer outside the mesa region to obtain a silicon carbide single-photon detector.

[0046] The ohmic contact layer serves as a transition layer between the functional layer and the electrode. Its early epitaxial growth addresses the resistance issue arising from direct contact between the metal electrode and the semiconductor. The doping concentration of the ohmic contact layer is significantly higher than that of the functional layer, substantially reducing the interface barrier. A silicon carbide ohmic contact layer grown between the SiC substrate and the SiC multiplication layer allows for a low-resistance ohmic contact between the subsequent metal electrode and the SiC multiplication layer, reducing carrier transport losses from the multiplication layer to the electrode. An aluminum gallium nitride (AlGaN) ohmic contact layer grown on top of the AlGaN absorber layer adapts to the semiconductor properties of AlGaN, avoiding high-resistance Schottky contacts formed by direct metal-AlGaN contact and ensuring efficient carrier extraction.

[0047] Etching the mesa enables physical isolation of the electrodes, with one electrode connecting to the AlGaN ohmic contact layer and the other to the silicon carbide ohmic contact layer. The area outside the mesa is etched until the silicon carbide ohmic contact layer outside the mesa is exposed. This silicon carbide ohmic contact layer outside the mesa, located below the multiplication layer, is physically separated from the AlGaN ohmic contact layer within the mesa, preventing short circuits in subsequent electrodes.

[0048] Ohmic contact electrodes are fabricated to form a complete circuit. For example, the cathode electrode is fabricated on a SiC ohmic contact layer outside the mesa region to collect multiplied charge carriers. The anode electrode is fabricated on an AlGaN ohmic contact layer within the mesa region, serving as the input terminal of the AlGaN absorber layer and forming an electric field circuit with the cathode. The electrodes, in conjunction with the ohmic contact layer, construct a conductive path connecting the anode, SiC multiplication layer, AlGaN absorber layer, and cathode, enabling the collection and output of charge carriers.

[0049] In one possible implementation, the silicon carbide ohmic contact layer is P-type and the aluminum gallium nitride ohmic contact layer is N-type; or, the silicon carbide ohmic contact layer is N-type and the aluminum gallium nitride ohmic contact layer is P-type.

[0050] In one possible implementation, after fabricating ohmic contact electrodes on the aluminum gallium nitride ohmic contact layer in the mesa region and the silicon carbide ohmic contact layer outside the mesa region, the method further includes: fabricating a passivation layer outside the ohmic contact electrode region.

[0051] In one possible implementation, after preparing the passivation layer, an anti-reflection layer is prepared on the surface of the silicon carbide single-photon detector.

[0052] For example, the antireflective layer is a multilayer dielectric film. Through the film interference effect, the phase difference between the incident light and the reflected light is canceled out, allowing the reflected light to cancel each other out and the incident light to pass through to the maximum extent, thereby reducing reflection loss.

[0053] In this embodiment of the invention, an anti-reflection layer is provided to reduce the reflection loss of solar blind light on the back side of the substrate, allowing more photons to penetrate the substrate and enter the aluminum gallium nitride absorption layer, thereby further improving the detection sensitivity.

[0054] In one possible implementation, after epitaxially growing a silicon carbide multiplication layer on a silicon carbide substrate, the method further includes epitaxially growing a silicon carbide charge control layer on the silicon carbide multiplication layer.

[0055] The charge control layer buffers the doping concentration gradient, allowing the electric field to be uniformly distributed within the multiplication layer. The charge control layer is grown on the side of the SiC multiplication layer away from the substrate, and will come into contact with the AlGaN absorber layer or silicon bonding layer during subsequent bonding.

[0056] In one possible implementation, the doping concentration of the aluminum gallium nitride absorber layer is in the range of 1 × 10⁻⁶. 15 cm -3 Up to 1×10 16 cm -3 .

[0057] In one possible implementation, the thickness of the aluminum gallium nitride absorber layer ranges from 0.1 to 0.5 micrometers.

[0058] The following is an illustration using a comprehensive example.

[0059] Figure 4 This is a schematic diagram of another silicon carbide single-photon detector provided in an embodiment of the present invention; see reference. Figure 4 In one possible implementation, the present invention provides a silicon carbide single-photon detector structure, which, from bottom to top, mainly comprises a silicon carbide substrate, a P-type silicon carbide substrate, and a silicon carbide substrate. + Type SiC ohmic contact layer, N - SiC multiplication layer, N + Type SiC charge control layer, N - AlGaN absorber layer, N +AlGaN ohmic contact layer, first electrode, second electrode, passivation layer.

[0060] N + The Al composition of the AlGaN ohmic contact layer is ≥0.6, the thickness is between 0.1 and 0.3 μm, and the doping concentration is 1×10⁻⁶. 18 cm -3 ~1×10 20 cm -3 between.

[0061] N - The Al composition of the AlGaN absorber layer is ≥0.4, the thickness is between 0.1 and 0.5 μm, and the doping concentration is 1×10⁻⁶. 15 cm -3 ~1×10 16 cm -3 between.

[0062] Optionally, N - The AlGaN absorber layer is an Al composition layer with a gradual change, where the Al composition decreases from top to bottom.

[0063] N + The thickness of the SiC charge-controlled layer is between 0.05 and 0.2 μm, and the doping concentration is between 1 × 10⁻⁶. 18 cm -3 ~1×10 20 cm -3 between.

[0064] N - The thickness of the SiC multiplication layer is between 0.1 and 0.5 μm, and the doping concentration is between 1 × 10⁻⁶. 15 cm -3 ~1×10 16 cm -3 between.

[0065] P + The thickness of the SiC ohmic contact layer is between 0.1 and 0.3 μm, and the doping concentration is between 1 × 10⁻⁶. 18 cm -3 ~1×10 20 cm -3 between.

[0066] The device structure includes an isolation mesa with a depth at P. + Type SiC ohmic contact layer.

[0067] The first electrode is located on the SiC ohmic contact layer, and the second electrode is located on the AlGaN ohmic contact layer. Both the first and second electrodes are ohmic contact electrodes.

[0068] The passivation layer consists of SiO2, Al2O3, HfO2, Y2O3, and SiN. x One or any combination of materials, with a thickness between 50 nm and 10 μm.

[0069] Optionally, the device surface has an anti-reflective layer. The anti-reflective layer is made of SiO2, Al2O3, HfO2, Y2O3, or SiN. x One or any combination of materials, with a thickness between 20 nm and 2 μm.

[0070] Figure 5 This is a schematic diagram of the structure of the third type of silicon carbide single-photon detector provided in the embodiments of the present invention, with reference to... Figure 5 Optionally, the conductivity type of each epitaxial layer of the detector can be changed from P-type to N-type or from N-type to P-type.

[0071] In this embodiment of the invention, the AlGaN absorption layer achieves selective absorption of the incident wavelength, filters out interference signals, and enables "solar-blind" detection. This avoids the influence of the filter on the detector responsivity. Furthermore, AlGaN serves only as the absorption layer of the device, and the absorption multiplication separation structure allows the AlGaN absorption layer to bear only a lower voltage during device operation, while the SiC multiplication layer bears a higher voltage. This effectively reduces the impact of AlGaN material defects on the device's dark current and breakdown voltage.

[0072] SiC, as a device layer, has a low material defect density, which can reduce the dark current of the detector on the one hand, and the SiC multiplication layer can withstand a high electric field intensity on the other hand, thereby realizing the accelerated movement and avalanche multiplication of charge carriers, improving the internal gain and detection sensitivity of the detector.

[0073] The device structure uses a SiC substrate to grow SiC and AlGaN layers sequentially from bottom to top. Epitaxially growing the SiC layer first and then the AlGaN layer can effectively reduce the defect density of the epitaxial material, and it is compatible with existing mature epitaxial material growth technology, making the device fabrication process simple.

[0074] The above embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit it. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A silicon carbide single-photon detector, characterized in that, include: silicon carbide substrate; A silicon carbide multiplication layer is provided on the silicon carbide substrate; the silicon carbide multiplication layer is obtained by homoepitaxial growth on the silicon carbide substrate; An aluminum gallium nitride (AGL) absorber layer is provided on the silicon carbide multiplication layer; wherein, the AGL absorber layer is obtained by heteroepitaxial growth of the silicon carbide multiplication layer; the doping concentration of the AGL absorber layer is not higher than the doping concentration of the silicon carbide multiplication layer, and the thickness of the AGL absorber layer is greater than the thickness of the silicon carbide multiplication layer; the bandgap range of the AGL absorber layer coincides with the photon energy range of the solar blind band. The light incident direction of the detector is from the aluminum gallium nitride absorption layer toward the silicon carbide multiplication layer.

2. A method for fabricating a silicon carbide single-photon detector, characterized in that, include: Homoetropic growth of silicon carbide multiplication layers on silicon carbide substrates; An aluminum gallium nitride (AGL) absorber layer is heteroepitaxially grown on a silicon carbide (SiC) multiplication layer; wherein the doping concentration of the AGL absorber layer is not higher than the doping concentration of the SiC multiplication layer, and the thickness of the AGL absorber layer is greater than the thickness of the SiC multiplication layer; the bandgap range of the AGL absorber layer coincides with the photon energy range of the solar blind band. After epitaxially growing an aluminum gallium nitride (AGL) absorber layer, a silicon carbide (SiC) single-photon detector is prepared, wherein the light incident direction of the detector is from the AGL absorber layer toward the SiC multiplication layer.

3. The method for fabricating a silicon carbide single-photon detector as described in claim 2, characterized in that, Before the epitaxial growth of a silicon carbide multiplication layer on a silicon carbide substrate, the following steps are also included: A silicon carbide ohmic contact layer is epitaxially grown on the front side of a silicon carbide substrate; Accordingly, after epitaxially growing an aluminum gallium nitride absorber layer, a silicon carbide single-photon detector is fabricated, including: An aluminum gallium nitride ohmic contact layer is epitaxially grown on the aluminum gallium nitride absorber layer; After growing the aluminum gallium nitride ohmic contact layer, the mesa is etched until the silicon carbide ohmic contact layer outside the mesa area is exposed; Ohmic contact electrodes were fabricated on the aluminum gallium nitride ohmic contact layer in the mesa region and on the silicon carbide ohmic contact layer outside the mesa region, respectively, to obtain a silicon carbide single-photon detector.

4. The method for fabricating a silicon carbide single-photon detector as described in claim 3, characterized in that, The silicon carbide ohmic contact layer is P-type, and the aluminum gallium nitride ohmic contact layer is N-type; Alternatively, the silicon carbide ohmic contact layer may be N-type, and the aluminum gallium nitride ohmic contact layer may be P-type.

5. The method for fabricating a silicon carbide single-photon detector as described in claim 3, characterized in that, After fabricating ohmic contact electrodes on the aluminum gallium nitride ohmic contact layer within the mesa region and the silicon carbide ohmic contact layer outside the mesa region, the process further includes: A passivation layer is prepared outside the ohmic contact electrode region.

6. The method for fabricating a silicon carbide single-photon detector as described in claim 5, characterized in that, After preparing the passivation layer, the following steps are also included: An anti-reflection layer is fabricated on the surface of a silicon carbide single-photon detector.

7. The method for fabricating a silicon carbide single-photon detector as described in claim 2, characterized in that, The aluminum gallium nitrogen absorber layer is an aluminum composition gradually varying layer; the proportion of aluminum composition gradually decreases from bottom to top.

8. The method for fabricating a silicon carbide single-photon detector as described in claim 2, characterized in that, After epitaxially growing a silicon carbide multiplication layer on a silicon carbide substrate, the process also includes: A silicon carbide charge control layer is epitaxially grown on a silicon carbide multiplication layer.

9. The method for fabricating a silicon carbide single-photon detector as described in claim 2, characterized in that, The doping concentration range of the aluminum gallium nitride absorber layer is 1×10⁻⁶. 15 cm -3 Up to 1×10 16 cm -3 .

10. The method for fabricating a silicon carbide single-photon detector as described in claim 2, characterized in that, The thickness of the aluminum gallium nitride absorber layer ranges from 0.1 to 0.5 micrometers.

Citation Information

Cited By

  • Electronically integratable double-sided framework silicon carbide thin film device and preparation method thereof

    CN121772401A