Process methods applied in BSI fabrication

By forming a through-substrate groove and depositing multiple dielectric layers during the BSI manufacturing process, the problem of tungsten residue in metal grid fabrication was solved, improving product yield and equipment utilization.

CN123076040APending Publication Date: 2026-11-10HUA HONG SEMICON WUXI LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610975616.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-01
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

In the back-illuminated image sensor (BSI) manufacturing process, tungsten residue can easily occur during the metal grid fabrication process, leading to decreased product yield and equipment contamination.

Method used

By forming a metal interconnect structure on the front side of the substrate, forming a first groove on the back side to fill the deep trench isolation structure with first and second dielectric layers, forming a second groove through the substrate, and sequentially depositing a third and fourth dielectric layer thereon, planarizing and dry etching to a predetermined depth below the fourth dielectric layer, a flatter morphology is formed to reduce metal residue.

Benefits of technology

It reduces metal residue after metal grid etching, improving product yield and equipment utilization.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123076040A_ABST
    Figure CN123076040A_ABST
Patent Text Reader

Abstract

This application discloses a process method for BSI fabrication, comprising: providing a substrate, wherein a metal interconnect structure is formed on the front side of the substrate, a first groove is formed from the back side of the substrate to a predetermined depth therein, a first dielectric layer is formed on the back side of the substrate and the surface of the first groove, a second dielectric layer is formed on the first dielectric layer, and the second dielectric layer fills the first groove; etching is performed by photolithography to remove the first dielectric layer, the second dielectric layer and the substrate in a target area to form a second groove extending downward from the back side through the substrate; a third dielectric layer is formed on the second dielectric layer, the third dielectric layer fills the second groove, and the third dielectric layer above the second groove has a recessed morphology; a fourth dielectric layer is formed on the third dielectric layer; a fifth dielectric layer is formed on the fourth dielectric layer; planarization is performed, and planarization stops at the fourth dielectric layer; dry etching is performed, and etching stops at a predetermined depth below the fourth dielectric layer; and a metal grid is formed on the back side of the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of semiconductor devices and integrated circuit technology, and in particular to a process method applied in BSI fabrication. Background Technology

[0002] In the back end of line (BEOL) manufacturing process of back illuminated image sensor (BSI), a backside metal grid (BMG) is typically formed to provide a low-resistance path to facilitate the rapid transfer of photogenerated charges, aid in heat dissipation, and reduce color crosstalk.

[0003] In related technologies, the fabrication process of metal grids includes: forming a tungsten (W) metal layer on the back of the chip, and etching it using photolithography to define the grid pattern, thereby forming the metal grid. However, in actual production, during the fabrication of the metal grid, after the tungsten etching process, tungsten residue is often detected in the seal ring area of ​​the chip. This residual tungsten is prone to peeling, which not only contaminates the pixel area and affects image quality, but also contaminates the etching equipment, reducing product yield and equipment utilization.

[0004] Therefore, there is an urgent need to provide a process method for BSI fabrication that can improve the metal residue phenomenon caused during the fabrication of the back metal grid. Summary of the Invention

[0005] This application provides a process method for BSI fabrication that solves the problem of metal residue easily caused after the metal grid is formed in related technologies. The method includes: A substrate is provided, wherein a metal interconnect structure is formed on the front side of the substrate, a first groove is formed from the back side of the substrate to a predetermined depth of the substrate, a first dielectric layer is formed on the back side of the substrate and the surface of the first groove, a second dielectric layer is formed on the first dielectric layer, and the second dielectric layer fills the first groove. The first dielectric layer, the second dielectric layer, and the substrate in the target area are removed by photolithography to form a second groove extending downward from the back side of the substrate and penetrating the substrate, exposing the metal interconnect structure at the bottom of the second groove. A third dielectric layer is formed on the second dielectric layer, the third dielectric layer fills the second groove, and the third dielectric layer above the second groove has a recessed morphology; A fourth dielectric layer is formed on the third dielectric layer; A fifth dielectric layer is formed on the fourth dielectric layer; Perform planarization, which stops at the fourth dielectric layer; Dry etching is performed until the etching stops at a predetermined depth below the fourth dielectric layer; A metal grid is formed on the back side of the substrate.

[0006] In some embodiments, the second dielectric layer, the third dielectric layer, and the fifth dielectric layer comprise a silicon dioxide layer.

[0007] In some embodiments, the fourth dielectric layer includes a silicon nitride layer.

[0008] In some embodiments, the substrate comprises silicon, and the first dielectric layer is formed by a thermal oxidation process on the substrate.

[0009] In some embodiments, the metal grille includes a patterned layer of tungsten metal.

[0010] In some embodiments, the ratio of the depth to the width of the first groove is greater than 6.

[0011] The technical solution of this application has at least the following advantages: By forming a metal interconnect structure on the front side of the substrate during the BSI fabrication process, and then forming a first trench on the back side of the substrate after the first and second dielectric layers fill the first trench of the deep trench isolation structure, a second trench penetrating the substrate is formed. After the third dielectric layer fills the second trench, a fourth dielectric layer and a fifth dielectric layer are formed on the third dielectric layer. In this way, planarization and general dry etching are performed sequentially to a predetermined depth below the fourth dielectric layer, thereby making the dielectric layer above the second trench present a flatter morphology, reducing the metal residue after subsequent metal grid etching, and improving the product yield to a certain extent. Attached Figure Description

[0012] To more clearly illustrate the technical solutions in the specific embodiments of this application or the prior art, the drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this application. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.

[0013] Figure 1 This is a flowchart of a process method applied in BSI fabrication provided by an exemplary embodiment of this application; Figures 2 to 8 This is a schematic diagram illustrating the manufacturing process of an exemplary embodiment of this application. Detailed Implementation

[0014] The technical solutions of this application will now be clearly and completely described with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this application. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0015] In the description of this application, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0016] In the description of this application, it should be noted that, unless otherwise expressly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal connection of two components; and they can refer to a wireless connection or a wired connection. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.

[0017] Furthermore, the technical features involved in the different embodiments of this application described below can be combined with each other as long as they do not conflict with each other.

[0018] refer to Figure 1 It illustrates a flowchart of a process method applied to BSI fabrication provided in an exemplary embodiment of this application, such as... Figure 1 As shown, the method includes: Step S1: A substrate is provided, a metal interconnect structure is formed on the front side of the substrate, a first groove is formed from the back side of the substrate to a predetermined depth of the substrate, a first dielectric layer is formed on the back side of the substrate and the surface of the first groove, a second dielectric layer is formed on the first dielectric layer, and the second dielectric layer fills the first groove.

[0019] refer to Figure 2 This shows a schematic cross-sectional view before the formation of the second groove. For example, as shown... Figure 2 As shown, substrate 210 is a substrate for forming BSI, which contains silicon (Si), and a metal interconnect structure 240 is formed on its front side (the metal interconnect structure 240 includes an insulating layer and a metal layer formed in the insulating layer). Figures 2 to 8 (Not shown in the image) A first groove 211 is formed on the back side of the substrate 210 to a predetermined depth therein (the ratio of the depth to the width of the first groove 211 is greater than 6). A first dielectric layer 221 is formed on the back side of the substrate 210 and the surface of the first groove 211. A second dielectric layer 222 is formed on the first dielectric layer 221. The second dielectric layer 222 fills the first groove 211. The first dielectric layer 221 and the second dielectric layer 222 in the first groove 211 constitute a deep trench isolation (DTI) structure.

[0020] The first dielectric layer 221 and the second dielectric layer 222 may include a silicon dioxide (SiO2) layer. The first dielectric layer 221 containing the silicon dioxide layer can be formed on the back side of the substrate 210 and the surface of the first groove 211 by a thermal oxidation process. The second dielectric layer 222 can be formed by depositing the silicon dioxide layer by a chemical vapor deposition (CVD) process to fill the first groove 211.

[0021] Step S2: Etching is performed using photolithography to remove the first dielectric layer, the second dielectric layer, and the substrate in the target area, forming a second groove extending downward from the back side of the substrate and penetrating the substrate, exposing the metal interconnect structure at the bottom of the second groove.

[0022] refer to Figure 3 This shows a cross-sectional view after the second groove has been formed. For example, as shown... Figure 3 As shown, step S2 includes, but is not limited to: covering the second dielectric layer 222 with photoresist ( Figure 3 (Not shown in the image) The photoresist in the target area is removed sequentially by exposure and development, followed by etching to remove the second dielectric layer 222, the first dielectric layer 221, and the substrate 210 in the target area, forming a second groove 212 extending downward from the back side of the substrate 210. The metal interconnect structure 240 at the bottom of the second groove 212 is exposed. After etching, the photoresist is removed. Optionally, the width of the second groove 212 is 350 nanometers (nm) to 500 nanometers, and the depth of the second groove 212 is 2 micrometers (μm) to 4 micrometers. The second groove 212 is used to form a deep trench isolation structure.

[0023] Step S3: A third dielectric layer is formed on the second dielectric layer. The third dielectric layer fills the second groove, and the third dielectric layer above the second groove has a recessed morphology.

[0024] refer to Figure 4 This shows a schematic cross-sectional view after the formation of the third dielectric layer. For example, as shown... Figure 4As shown, a silicon dioxide layer can be deposited using atomic layer deposition (ALD) to form a third dielectric layer 223. The third dielectric layer 223 fills the second groove 212 and has a thickness of 2000 Å to 3000 Å. The third dielectric layer 223 above the third groove 212 has a recessed morphology (e.g., Figure 4 (As shown by the dashed line area).

[0025] The applicant discovered that the generation of metal residue is closely related to the top morphology of the deep trench isolation structure. In the manufacturing process of the deep trench isolation structure provided by the relevant technology, after the formation of the third dielectric layer, a planarization process is directly performed, resulting in a V-shaped depression at the top of the second trench. During the subsequent metal layer formation and metal grid etching process, this area is prone to insufficient filling and etching residue.

[0026] Step S4: Form a fourth dielectric layer on the third dielectric layer.

[0027] Step S5: Form a fifth dielectric layer on the fourth dielectric layer.

[0028] refer to Figure 5 It shows a schematic cross-sectional view after the formation of the fifth dielectric layer. For example, as shown... Figure 5 As shown, a fourth dielectric layer 224 can be formed by depositing a silicon nitride (Si3N4) layer using a CVD process, and a fifth dielectric layer 225 can be formed by plasma-enhanced chemical vapor deposition of silicon dioxide (PEOX). Optionally, the thickness of the fourth dielectric layer 224 is less than the thickness of the fifth dielectric layer 225; the thickness of the fourth dielectric layer 224 is 800 to 1000 angstroms, and the thickness of the fifth dielectric layer 225 is 5000 to 10000 angstroms.

[0029] Step S6: Perform planarization, which stops at the fourth dielectric layer.

[0030] refer to Figure 6 This shows a schematic cross-sectional view after flattening. For example, as shown... Figure 6 As shown, planarization can be achieved through a chemical mechanical polishing (CMP) process until the fourth dielectric layer 224 is exposed, thereby removing the fifth dielectric layer 225.

[0031] Step S7: Perform dry etching until the etching stops at a predetermined depth below the fourth dielectric layer.

[0032] refer to Figure 7 It shows a schematic cross-sectional view after dry etching. For example, as shown... Figure 7As shown, the fourth dielectric layer 224 can be removed by blanket dry etching to a predetermined depth below the fourth dielectric layer 224. After etching, the dielectric layer thickness on the back side of the substrate 210 (the thickness of the first dielectric layer 221 and the second dielectric layer 222, or the thickness of the first dielectric layer 221, the second dielectric layer 222 and the third dielectric layer 223, the remaining dielectric layer thickness can be retained according to actual needs) is 1000 angstroms and 1500 angstroms. After planarization and dry etching in sequence, the dielectric layer above the second groove 212 presents a flatter morphology, so that metal layers are less likely to remain in the subsequent metal grid fabrication process.

[0033] Step S8: Form a metal grid on the back side of the substrate.

[0034] refer to Figure 8 It shows a schematic cross-sectional view after the metal grille has been formed. For example, such as... Figure 8 As shown, after forming a metal layer 231 and a hard mask layer 232 sequentially, the metal layer 231 and the hard mask layer 232 in the target area are etched away using a photolithography process. The remaining patterned metal layer 231 forms a metal grid. The metal layer 231 may include a tungsten metal layer. Because the dielectric layer above the second groove 212 has a flatter morphology, this (e.g., ...) Figure 8 (As shown in the dashed area) No residual metal layer.

[0035] In summary, in the embodiments of this application, during the fabrication of BSI, a metal interconnect structure is formed on the front side of the substrate, and a first trench is formed on the back side of the substrate after the first dielectric layer and the second dielectric layer are filled with the deep trench isolation structure. Then, a second trench is formed that penetrates the substrate. After the third dielectric layer is filled with the second trench, a fourth dielectric layer and a fifth dielectric layer are formed on the third dielectric layer. In this way, planarization and general dry etching are performed sequentially to a predetermined depth below the fourth dielectric layer, thereby making the dielectric layer above the second trench present a flatter morphology, reducing the metal residue after subsequent metal grid etching, and improving the product yield to a certain extent.

[0036] Obviously, the above embodiments are merely illustrative examples for clear explanation and are not intended to limit the implementation. Those skilled in the art will recognize that other variations or modifications can be made based on the above description. It is neither necessary nor possible to exhaustively list all possible implementations here. However, obvious variations or modifications derived therefrom are still within the scope of protection of this application.

Claims

1. A process method applied in BSI fabrication, characterized in that, include: A substrate is provided, wherein a metal interconnect structure is formed on the front side of the substrate, a first groove is formed from the back side of the substrate to a predetermined depth of the substrate, a first dielectric layer is formed on the back side of the substrate and the surface of the first groove, a second dielectric layer is formed on the first dielectric layer, and the second dielectric layer fills the first groove. The first dielectric layer, the second dielectric layer, and the substrate in the target area are removed by photolithography to form a second groove extending downward from the back side of the substrate and penetrating the substrate, exposing the metal interconnect structure at the bottom of the second groove. A third dielectric layer is formed on the second dielectric layer, the third dielectric layer fills the second groove, and the third dielectric layer above the second groove has a recessed morphology; A fourth dielectric layer is formed on the third dielectric layer; A fifth dielectric layer is formed on the fourth dielectric layer; Perform planarization, which stops at the fourth dielectric layer; Dry etching is performed until the etching stops at a predetermined depth below the fourth dielectric layer; A metal grid is formed on the back side of the substrate.

2. The method according to claim 1, characterized in that, The second dielectric layer, the third dielectric layer, and the fifth dielectric layer each comprise a silicon dioxide layer.

3. The method according to claim 2, characterized in that, The fourth dielectric layer includes a silicon nitride layer.

4. The method according to claim 3, characterized in that, The substrate comprises silicon, and the first dielectric layer is formed by a thermal oxidation process on the substrate.

5. The method according to any one of claims 1 to 4, characterized in that, The metal grille includes a patterned layer of tungsten metal.

6. The method according to claim 5, characterized in that, The ratio of the depth to the width of the first groove is greater than 6.