Method for manufacturing a semiconductor device

By short-circuiting control pads and sealing semiconductor elements with resin, the method addresses electrostatic damage in semiconductor devices, enhancing yield and reducing manufacturing complexity and cost.

DE102021112974B4Active Publication Date: 2024-11-21MITSUBISHI ELECTRIC CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE102021112974
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-07-22
Filing Date
2021-05-19
Publication Date
2024-11-21
Estimated Expiration
2041-05-19

AI Technical Summary

Technical Problem

Existing semiconductor devices face issues with electrostatic damage in the measuring cell part due to charge absorption by the sealing resin, leading to potential differences and decreased yield, particularly during the grinding process to expose conductor pieces.

Method used

A method involving connecting semiconductor elements to a relay substrate, bonding electrode materials, sealing with resin, and grinding to expose electrode materials while short-circuiting control pads to equalize potential, thereby preventing electrostatic damage.

Benefits of technology

Prevents electrostatic damage to the measuring cell part by equalizing potential differences, improving yield and reducing manufacturing complexity and cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Method for manufacturing a semiconductor device, wherein: - the semiconductor device has: - a plurality of semiconductor elements (1) comprising a semiconductor element (1) having a main cell part and at least one measuring cell part (4) and provided with a plurality of signal pads (6, 7, 8, 9, 10) which each correspond to the main cell part and the measuring cell part (4); and - a relay substrate (2) which is provided with a multitude of control pads (12), - the procedure exhibits: (a) Connect each of the semiconductor elements (1) and the relay substrate (2) on a printed circuit board (3); (b) Connect each signal pad (6, 7, 8, 9, 10) of each of the semiconductor elements (1) and each control pad (12) of the relay substrate (2) by a wire (17); (c) Connecting a first electrode material (18) to each of the semiconductor elements (1); (d) Connecting a second electrode material (19) having a short-circuiting part (21) that short-circuits each of the control pads (12) to the relay substrate (2); (e) Sealing the printed circuit board (3), each of the semiconductor elements (1), the relay substrate (2), the first electrode material (18), and the second electrode material (19) with resin (23); and (f) Grinding the resin (23) and removing the short-circuit part (21) to expose part of the second electrode material (19). - the relay substrate (2) has a plurality of control terminals (14) which are electrically connected to each of the control pads (12), - the second electrode material (19) has a plurality of connecting parts (20) that correspond to each of the control terminals (14) and the short-circuit part (21) which connects each connecting part (20), and - in (d) each of the connecting parts (20) is electrically connected to each of the control terminals (14), and then each of the connecting parts (20) and the short-circuiting parts (21) is electrically connected to each other.
Need to check novelty before this filing date? Find Prior Art

Description

Field of the invention

[0001] The present invention discloses a method for manufacturing a semiconductor device comprising a semiconductor element with a measuring cell part. Description of the state of the art

[0002] Conventionally, a semiconductor device is disclosed which is manufactured by processes of connecting a wiring member (relay substrate) and a plurality of semiconductor elements on a circuit board, connecting a control pad of each semiconductor element in parallel through an internal wiring (wiring pattern) formed on a wiring member, fixing a conductor piece (signal terminal) formed on the wiring member made of copper, sealing the conductor piece by means of a sealing resin, and polishing the sealing resin to expose each conductor piece at a surface (see, for example, International Patent Application WO 2020 / 110170 A1). Summary

[0003] For example, in International Patent Application WO 2020 / 110170 A1, in a case where a semiconductor element comprising a main cell part and a sensing cell part (for example, a current sensing cell part) having a lower flow rate division ratio than the main cell part is sealed by a sealing resin, if the sealing resin covering a surrounding area of ​​the semiconductor element receives a charge, there is a problem that electrostatic damage occurs in the sensing cell part at a time of handling the semiconductor device, particularly at a time of grinding an upper surface of the sealing resin to expose each conductor piece, and a yield of the semiconductor device decreases.For example, the measuring cell part has a thin insulating layer such as a gate oxide layer and an interlayer, and an overvoltage caused by static electricity will destroy such a structural body. Particularly in a state where the control pads of each semiconductor element are independent of each other, when a charge in the sealing resin passes through the control terminal to the outside, a potential difference occurs between the control terminals, and electrostatic damage resistance decreases in some cases.

[0004] WO 2019 / 181760 A1 discloses a module in which terminal assemblies having a connecting conductor with larger dimensions than those of other parts are mounted on corner portions of a substrate, thereby improving strength against stresses generated during installation on an external substrate and connection reliability. A high-frequency module is configured with a component mounted on an upper surface of a substrate, a second sealing resin layer laminated to the upper surface of the substrate, a component mounted on a lower surface of the substrate, a first sealing resin layer laminated to the lower surface of the substrate, and first terminal assemblies and a second terminal assembly mounted on the lower surface of the substrate.The first terminal assemblies are mounted at the four corners of the substrate and have connecting conductors that are thicker than the connecting conductors of the second terminal assembly. Each of the terminal assemblies is formed by integrating a plurality of connecting conductors with resin blocks. The resin used in the resin blocks is a liquid polymer resin with a lower dielectric tangent than the first sealing resin layer.

[0005] US 2013 / 0 234 308 A1 describes a manufacturing method for a semiconductor device, in which a newly configured wafer of resin-encapsulated semiconductor packages is obtained by supporting it with a resin. Subsequently, a grinding process is performed on the top and back surfaces to expose only one connection electrode on a surface of a semiconductor chip. Furthermore, a chip-scale package is obtained by a subdivision process along a periphery of the chip.

[0006] DE 21 2018 000 072 U1 discloses an electronic component formed with a substrate having a first main surface on one side and a second main surface on the other side, a chip having a first chip main surface on one side and a second chip main surface on the other side, and a plurality of electrodes formed on the first chip main surface and / or the second chip main surface, wherein the chip is arranged on the first main surface of the substrate, a sealing insulation layer sealing the chip on the first main surface of the substrate such that the second main surface of the substrate is exposed, wherein the sealing insulation layer has a sealing main surface opposite the first main surface of the substrate, and a plurality of external terminals formed to penetrate the sealing insulation layer such thatthat they are exposed from the sealing main surface of the sealing insulation layer, wherein the external terminals are each electrically connected to the plurality of electrodes of the chip.,

[0007] It is an object of the present disclosure to provide a method of manufacturing a semiconductor device capable of preventing electrostatic damage in a configuration including a semiconductor element with a sensing cell part.

[0008] The object underlying the invention is achieved in a method for producing a semiconductor device according to the invention with the features of claim 1 and alternatively with the features of claim 5. Advantageous further developments are the subject of the respective dependent claims.

[0009] A method for manufacturing a semiconductor device according to the present invention includes, among other things: a plurality of semiconductor elements including a semiconductor element having a main cell portion and at least one sense cell portion, and provided with a plurality of signal pads corresponding to the main cell portion and the sense cell portion, respectively; and a relay substrate provided between a plurality of control pads.The method comprises: (a) connecting each of the semiconductor elements and the relay substrate on a circuit board; (b) connecting each of the signal pads of each semiconductor element and each control pad of the relay substrate by a wire; (c) connecting a first electrode material on each of the semiconductor elements; (d) connecting a second electrode material having a short-circuiting part that short-circuits each of the control pads on the relay substrate; (e) sealing the circuit board, each of the semiconductor elements, the relay substrate, the first electrode material, and the second electrode material with resin; and (f) grinding the resin and removing the short-circuiting part to expose a part of the second electrode material.

[0010] According to the present invention, the method for manufacturing the semiconductor device includes the process of bonding the second electrode material having the short-circuiting portion that shorts each of the control pads to the relay substrate, the process of sealing the circuit board, each of the semiconductor elements, the relay substrate, the first electrode material, and the second electrode material with the resin, and the process of grinding the resin and removing the short-circuiting portion to expose the second electrode material portion. Consequently, electrostatic damage can be prevented in the configuration including the semiconductor element with the sensing cell portion.

[0011] These and other objects, features, aspects and advantages of the present disclosure will become more apparent from the following detailed description of the present disclosure when taken in conjunction with the accompanying figures.

[0012] Embodiment 1 described below serves to explain the technical background of the present invention. Embodiments 2 and 3 are the subject matter of the present invention. Short description of the characters Fig. 1 is a bird's-eye view for describing a method of manufacturing a semiconductor device according to Embodiment 1 for explaining the technical background of the present invention. Fig. 2 is a plan view for describing a method of manufacturing the semiconductor device according to Embodiment 1. Fig. 3 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 4 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 5 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 6 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 7 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 8 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 9 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 10 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 11 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 12 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 1. Fig. 13 is a flowchart illustrating an example of the method for manufacturing the semiconductor device according to Embodiment 1. Fig. 14 is a bird's-eye view for describing a method of manufacturing a semiconductor device according to Embodiment 2 of the present invention. Fig. 15 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 16 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 17 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 18 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 19 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 20 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 21 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 22 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 23 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 24 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 25 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 26 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 27 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 28 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 2. Fig. 29 is a diagram for describing a method for producing a second electrode material according to Embodiment 2. Fig. 30 is a diagram for describing the method for manufacturing the second electrode material according to Embodiment 2. Fig. 31 is a diagram for describing the method for manufacturing the second electrode material according to Embodiment 2. Fig. 32 is a bird's-eye view for describing a method of manufacturing a semiconductor device according to Embodiment 3 of the present invention. Fig. 33 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 34 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 35 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 36 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 37 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 38 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 39 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 40 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 41 is a bird's-eye view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 42 is a plan view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 43 is a cross-sectional view for describing the method of manufacturing the semiconductor device according to Embodiment 3. Fig. 44 is a flowchart illustrating an example of the method for manufacturing the semiconductor device according to Embodiment 3. Description of preferred embodiments<Ausführungsform 1 zur Erläuterung des technischen Hintergrunds der vorliegenden Erfindung> <1-1. Manufacturing process>

[0013] The Fig. 1 to 12 are diagrams for describing a method of manufacturing a semiconductor device according to Embodiment 1 for explaining the technical background of the present invention. Fig. 13 is a flowchart illustrating an example of the method for manufacturing the semiconductor device according to Embodiment 1. The method for manufacturing the semiconductor device according to Embodiment 1 is described below with reference to Fig. 1 to 13 described.

[0014] As in the Fig. 1 to 3, in a first connection process of step 11 in Fig. 13 a relay substrate 2 and a plurality of semiconductor elements 1 are connected on a circuit board 3 using a connecting material 16.

[0015] The semiconductor element 1 is a composite semiconductor element formed from SiC, for example, and configured as a metal oxide semiconductor field-effect transistor (MOSFET), for example. In Embodiment 1, the four semiconductor elements 1 are connected on the circuit board 3, and one of the four semiconductor elements 1 includes a main cell portion and a sense cell portion having a smaller flow division ratio than the main cell portion. The other three semiconductor elements 1 do not include the sense cell portion.

[0016] The measuring cell section comprises a current measuring cell section 4 and a temperature measuring diode section 5. In the current measuring cell section 4, a drain potential and a gate potential are jointly at a potential of the main cell section, but the source potential differs from the potential of the main cell section. Accordingly, a source signal pad 10, which corresponds to the source potential of the current measuring cell section 4, is provided in the semiconductor element 1.

[0017] The temperature measuring diode part 5 is formed, for example, from polysilicon and is insulated from the main cell part by an interlayer insulation layer (not shown). The temperature measuring diode part 5 has an anode signal pad 8 and a cathode signal pad 7.

[0018] A source signal pad 6 in the main cell part and a gate signal pad 9 are provided in the semiconductor element 1. The source signal pad 6 may be formed using a part of a region of the main cell part. Hereinafter, the source signal pad 6, the cathode signal pad 7, the anode signal pad 8, the gate signal pad 9, and the source signal pad 10 are collectively referred to as "the signal path" in some cases. An electrode layer (not shown) is provided on an upper surface of each of the source signal pad 6, the cathode signal pad 7, the anode signal pad 8, the gate signal pad 9, the source signal pad 10, and the main cell part. The electrode layer is formed of, for example, Al or Cu and may be formed by a sputtering method.

[0019] A bonding layer 11, which can be sinter-bonded, is provided on the electrode layer. The bonding layer 11 is, for example, a NiP / Pd / Au lamination layer and is formed by a plating process. Alternatively, the bonding layer 11 can be formed from a Ni / Au lamination layer, an Au single layer, or an Ag single layer, for example, by a sputtering process.

[0020] The relay substrate 2 is, for example, a substrate made of Si. In the relay substrate 2, an insulating layer (not shown) is provided on one surface, and a wiring part 13, which is a plurality of wiring patterns made of, for example, Al and a covering layer (not shown) covering at least a portion of the wiring part 13, is formed on the insulating layer. The covering layer is, for example, a layer made of polyimide.

[0021] An interconnect layer (not shown) is provided on a rear surface of the relay substrate 2. The interconnect layer is, for example, a Ti / Al / Ni / Au lamination layer, and may be formed by a sputtering method. Alternatively, the interconnect layer may be formed by forming a Ti / Au lamination layer by a sputtering method and then forming NiP / Au by a plating method.

[0022] A plurality of first pad portions 12 and a plurality of second pad portions 14 are provided in the wiring portion 13. The first pad portion 12 includes a control pad corresponding to the source signal pad 6, a control pad corresponding to the cathode signal pad 7, a control pad corresponding to the anode signal pad 8, a control pad corresponding to the gate signal pad 9, and a control pad corresponding to the source signal pad 10.

[0023] The second pad portion 14 (control terminal) is primarily used for supplying a signal during a burn-in test of a semiconductor package and for extracting a signal potential during assembly of the semiconductor package into a semiconductor device. An interconnect layer 15, which may be solder-bonded or sinter-bonded, is provided on at least every second pad portion 14. The interconnect layer 15 is, for example, a NiP / Pd / Au lamination layer and is formed by a plating process. Alternatively, the interconnect layer 15 may be formed from a Ni / Au lamination layer, an Au single layer, or an Ag single layer, for example, by a sputtering process.

[0024] The circuit board 3 is a plate material made of Cu, for example. The bonding material 16 is a sintered material made of Ag or Cu, for example. Each semiconductor element 1 and each relay substrate 2 are bonded on the circuit board 3 via the bonding material 16 using a pressure bonding process or a pressureless bonding process.

[0025] As in the Fig. 1 to 3, in a wire connection process of step S12 in Fig. 13, a signal pad provided in each semiconductor element 1, and the first pad part 12 provided in the relay substrate 2 are connected by the wire 17. Specifically, the source signal pad 6 and the control pad corresponding thereto are connected by the wire 17, the cathode signal pad 7 and the control pad corresponding thereto are connected by the wire 17, the anode signal pad 8 and the control pad corresponding thereto are connected by the wire 17, the gate signal pad 9 and the control pad corresponding thereto are connected by the wire 17, and the source signal pad 10 and the control pad corresponding thereto are connected by the wire 17. The wire 17 is formed of Au, Al, or Cu.

[0026] As in the Fig. 4 to 6, in a second connection process of step S13 in Fig. 13, a first electrode material 18 is bonded to the interconnection layer 11 provided on each semiconductor element 1 using a bonding material 22. The bonding material 22 is a sintered material formed, for example, from Ag or Cu. The first electrode material 18 is bonded to the interconnection layer 11 via the bonding material 22 by a pressure bonding process or a pressureless bonding process.

[0027] As in the Fig. 4 to 6, in a third connection process of step S14 in Fig. 13, a second electrode material 19 is bonded to the bonding layer 15 provided on each second pad portion 14 of the relay substrate 2 using the bonding material 22. The second electrode material 19 includes a short-circuit portion 21 and a plurality of bonding portions 20. Each bonding portion 20 corresponds to each second pad portion 14. The short-circuit portion 21 short-circuits each bonding portion 20. Here, the process of short-circuiting each bonding portion 20 indicates a process of bonding each bonding portion 20 such that the potential of each bonding portion 20 is the same among each other.

[0028] The potential of each signal pad of each semiconductor element 1 is independent of each other at the time of completion of the wire bonding process of step S12. That is, the potential of each signal pad of each semiconductor element 1 is electrically open. In the third bonding process of the subsequent step S14, the second electrode material 19 is bonded to the bonding layer 15 provided on each second pad portion 14, thus the potential of each signal pad of each semiconductor element 1 becomes a common potential. That is, the potential of each signal pad of each semiconductor element 1 is electrically short-circuited.

[0029] Each process of step S12, step S13, and step S14 described above is not necessarily executed in this order, but may be executed in any order.

[0030] As in the Fig. 7 to 9, in a sealing process of step S15 in Fig. 13, each semiconductor element 1, the relay substrate 2, the conductor body 3, the first electrode material 18, and at least a portion of the second electrode material 19 are sealed and fixed by means of the sealing resin 23. In the sealing process, the sealing is carried out, for example, using a transfer molding method. In the example in the Fig. 7 to 9, surfaces of the first electrode material 18 and the second electrode material 19 are exposed, but they may be covered by the sealing resin 23.

[0031] The sealing resin 23 comprises a filler material and a thermosetting resin. The filler material and the thermosetting resin are mixed and then poured into a mold housing the semiconductor device, to which each process from step S11 to step S14 has been performed. When the sealing resin 23 is poured into the mold and the thermosetting resin is heat-treated, pressure is applied to form the sealing resin 23 with a high density.

[0032] As in the Fig. 10 to 12, in the grinding process of step S16 in Fig. 13, the grinding process is performed such that at least a portion of the first electrode material 18 and at least a portion of the second electrode material 19 are exposed. At this time, the short-circuit portion 21 of the second electrode material 19 is removed by grinding, and each connection portion 20 remains as it is. Accordingly, the potential of each signal pad of each semiconductor element 1 is electrically open.

[0033] In a sealing process of step S15, a rear surface of the circuit board 3 is pressed against a lower surface of the mold, thus, the sealing resin 23 is not intended to cover the rear surface of the circuit board 3. However, if a small portion of the sealing resin 23 adheres to the rear surface of the circuit board 3 or is oxidized during the resin process, the sealing resin 23 adhering to the rear surface or an oxidized portion is ground during the grinding process, thus, the mountability of the semiconductor device can be improved.

[0034] The semiconductor device according to Embodiment 1 is completed by the respective processes from step S11 to step S16 as described above.

[0035] A larger circuit can be formed using the semiconductor devices according to Embodiment 1. For example, an equivalent circuit to the semiconductor device according to Embodiment 1 includes a MOSFET for one phase, so a half-bridge circuit can be formed by using and mounting the two semiconductor devices on an insulating substrate with a circuit pattern, and a full-bridge circuit can be formed using the six semiconductor devices. Accordingly, the plurality of semiconductor devices according to Embodiment 1 are combined, so various circuits such as a booster circuit can be achieved.After the semiconductor device according to Embodiment 1 is mounted on the insulating substrate having the circuit pattern, bonding is performed to lead out each signal electrode and main current electrode from each semiconductor device to the outside, and each semiconductor device and the insulating substrate having the circuit pattern are sealed by means of a sealing material, thus a higher-order semiconductor device can be obtained. <1-2. Effect>

[0036] After the sealing process of step S15 in Fig. 13, electrostatic damage to the measuring cell part of the semiconductor element 1 can be prevented as much as possible even when an electrical discharge occurs from the charged sealing resin 23 through each semiconductor device 1 to the outside. The sealing resin 23 is formed of an insulating material. The filler material and the thermosetting resin are stirred and then injected around each semiconductor element 1. Static electricity tends to occur when the filler material and the thermosetting resin are stirred, and the sealing resin 23 easily absorbs a charge because it is the insulating material. At the time of handling the semiconductor element 1, particularly during the grinding process of step S16 in Fig. 13, a potential difference occurs between the first pad portions 12 when the charge in the sealing resin 23 around each semiconductor element 1 passes from the signal pad, the wire 17, and the relay substrate 2, and is discharged to the outside by the second electrode material 19. The voltage due to static electricity is sufficiently high to damage the gate oxide layer and the interlayer insulating layer of the semiconductor element 1 in some cases. Accordingly, the gate oxide layer is damaged in some cases in the semiconductor element 1 having a small effective area ratio, that is, in the semiconductor element 1 having the current measuring cell 4 with a small gate-source capacitance. The temperature measuring diode portion 5 is insulated from the main cell portion by the interlayer insulating layer, and the interlayer insulating layer is damaged in some cases by the static electricity.

[0037] In Embodiment 1 for explaining the technical background of the present invention, the second electrode material 19 is provided with the short-circuiting part 21, thus the first pad parts 12 are short-circuited to each other during the sealing process. Accordingly, it is possible to prevent, as much as possible, the potential difference between the first pad parts 12, which occurs when the charge in the sealing resin 23 around the semiconductor element 1 penetrates the second electrode material 19 and is discharged to the outside. Accordingly, it is possible to prevent, as much as possible, damage to the insulating layer in the current measuring cell part 4 and the temperature measuring diode part 5.

[0038] The second electrode material 19 includes not only the connecting part 20 but also the short-circuiting part 21. Accordingly, each connecting part 20 corresponding to each second pad part 14 can be integrally formed, and operability and positional accuracy at the time of connecting the second electrode material 19 to the relay substrate 2 can be improved. A pattern pitch is usually determined by photoengraving in the second pad part 14, so a tolerance is quite small, and a tolerance regarding location of the second electrode material 19 is large. The second pad part 14 is small in terms of the tolerance in locating the second electrode material 19, so it is necessary to also control rotation of the second electrode material 19. In a state where the second electrode material 19 is obliquely connected for each second pad part 14, rotation must also be prevented.For example, when each connection part 20 of the second electrode material 19 is an independently configured component (when the second electrode material 19 does not include the short-circuit part 21), there is a problem that a size of the second pad part 14 increases due to the above-described tolerance, a connection tolerance of the second electrode material 19 is reduced, and the number of processes required for assembling the second electrode material 19 increases. According to Embodiment 1, the second electrode material 19 is a component in which each connection part 20 and the short-circuit part 21 are integrally formed, thus the above problem can be solved, and the semiconductor device can be easily manufactured.

[0039] Cost per unit area is higher in SiC than in Si, so the cost of the semiconductor device can be reduced by making the first pad portion 12 small. The second pad portion 14 needs to be made large for positional tolerance to be connected to an electrode material, but the first pad portion 12 connecting the wire 17 can be made small, thus reducing the cost of the semiconductor device. <Ausführungsform 2 der vorliegenden Erfindung> <2-1. Manufacturing process>

[0040] The Fig. 14 to 28 are diagrams for describing a method of manufacturing a semiconductor device according to Embodiment 2 of the present invention. The method of manufacturing the semiconductor device according to Embodiment 2 will be described below with reference to Fig. 14 to 28, however, the description mainly focuses on a process that differs from the method for manufacturing the semiconductor device according to Embodiment 1 for explaining the technical background of the present invention. Each process for manufacturing the semiconductor device according to Embodiment 2 is similar to that shown in the flowchart in Fig. 13 is illustrated.

[0041] As in the Fig. 17 to 19, in a third connection process of step S14 in Fig. 13, a second electrode material 24 is bonded to the bonding layer 15 provided on each second pad portion 14 of the relay substrate 2 using the bonding material 22. The second electrode material 24 includes an insulating material 25 and the plurality of bonding portions 20. The bonding portions 20 are integrally formed by the insulating material 25 and are electrically open.

[0042] Below, as in the Fig. 20 to 22, the adjacent connecting parts 20 are connected by a short-circuit wire 26 to short-circuit each connecting part 20. The connection is performed in the wire connection process of step S12 in Fig. 13. In this case, the wire connection process of step S12 is executed after the third connection process of step S14.

[0043] As in the Fig. 23 to 25, in the sealing process S15 in Fig. 13 each semiconductor element 1, the relay substrate 2, the conductor body 3, the first electrode material 18, and at least a part of the second electrode material 24 are sealed and fixed by means of the sealing resin 23. In the example in the Fig. 23 to 25, surfaces of the first electrode material 18 and the second electrode material 24 are exposed, but they may be covered by the sealing resin 23.

[0044] As in the Fig. 26 to 28, in the grinding process of step S16 in Fig. 13, the grinding process is performed such that at least a portion of the first electrode material 18 and at least a portion of the second electrode material 24 are exposed. At this time, the short-circuit wire 26 is removed by grinding, and each connection part 20 remains as it is. Accordingly, the potential of each signal pad of each semiconductor element 1 is electrically open.

[0045] Here, a method for producing the second electrode material 24 is described. Fig. 29 to 31 are diagrams for describing the method for producing the second electrode material.

[0046] As in Fig. 29, a conductive material 27 provided with slit-like holes is prepared. As shown in Fig. 30, a surrounding area of ​​the conductive material 27 is next covered by the insulating material 25. As in Fig. 31, the conductive material 27 and the insulating material 25 are subsequently cut out in a vertical direction with respect to an extension direction of the holes in the conductive material 27. The second electrode material 19 is thereby formed. <2-2. Effect>

[0047] The second electrode material 24 does not have the short-circuit parts 21 described in Embodiment 1 for explaining the technical background of the present invention. Accordingly, it is sufficient that the short-circuit wire 26 and a redundant part of the sealing resin 23 are formed in Fig. 13 can be ground, thus reducing the amount of the second electrode material 19 to be ground as much as possible. The processing time and the frequency of replacing a grindstone can be reduced, thus improving the productivity of the semiconductor device.

[0048] In the wire connection process of step S12 in Fig. 13, not only the wire 17 but also the short-circuit wire 26 is connected at the same time, thus it is not necessary to newly add a process for connecting the short-circuit wire 26.

[0049] The second electrode material 19 is in each in the Fig. 29 to 31, thus, the positional tolerance can be reduced as much as possible, and the plurality of second electrode materials 19 can be formed from a conductive material 27. The second electrode material 19 is formed in such a manner as to have a positional accuracy similar to that in Embodiment 1 for explaining the technical background of the present invention. <Ausführungsform 3 der vorliegenden Erfindung> <3-1. Manufacturing process>

[0050] The Fig. 32 to 43 are diagrams for describing a method of manufacturing a semiconductor device according to Embodiment 3 of the present invention. Fig. 44 is a flowchart illustrating an example of the method for manufacturing the semiconductor device according to Embodiment 3. The method for manufacturing the semiconductor device according to Embodiment 3 will be described below with reference to Fig. 32 to 44, however, the description mainly focuses on a process different from the method of manufacturing the semiconductor device according to Embodiment 1 for explaining the technical background of the present invention.

[0051] The semiconductor device according to Embodiment 3 does not include the relay substrate 2. Accordingly, each Fig. 44 does not include a process that is related to the wire connecting process of step S12 in Fig. 13 corresponds.

[0052] As in the Fig. 32 to 34, in a first connection process of step S21 in Fig. 44, the semiconductor element 1 is connected to the circuit board 3 using the connecting material 16. The semiconductor element 1 includes the main cell part and the measuring cell part. The semiconductor element 1 has a plurality of signal terminals 28, and each signal terminal 28 is provided with a connecting layer 29.

[0053] As in the Fig. 35 to 37, in a second connection process of step S22 in Fig. 44 the first electrode material 18 is connected to the connection layer 11 provided on the semiconductor element 1 using the connection material 22.

[0054] As in the Fig. 35 to 37, in a third connection process of step S23 in Fig. 44, the second electrode material 19 is connected to the connection layer 29 provided on each signal terminal 28 of the semiconductor element 1 using the connection material 22. Accordingly, the potential of each signal terminal 28 is electrically short-circuited.

[0055] Each process of step S22 and step S23 described above is not necessarily executed in this order, but may be executed in a reverse order.

[0056] As in the Fig. 38 to 40, in the sealing process of step S24 in Fig. 44, the semiconductor element 1, the circuit board 3, the first electrode material 18, and the second electrode material 19 are sealed and fixed by means of the sealing resin 23. In the example in the Fig. 38 to 40, surfaces of the first electrode material 18 and the second electrode material 19 are exposed, but they may be covered by the sealing resin 23.

[0057] As in the Fig. 41 to 43, in the grinding process of step S25 in Fig. 44, the grinding process is performed such that at least a portion of the first electrode material 18 and at least a portion of the second electrode material 19 are exposed. At this time, the short-circuit portion 21 of the second electrode material 19 is removed by grinding, and each connection portion 20 remains as it is. Accordingly, the potential of the signal terminal 28 of the semiconductor element 1 is electrically open. <3-2. Effect>

[0058] The semiconductor device according to Embodiment 3 includes a semiconductor element 1 including the main cell part and the sense cell part. The semiconductor device is manufactured by the above manufacturing method, thus achieving an effect similar to that of Embodiment 1 for explaining the technical background of the present invention.

[0059] The above describes the case of manufacturing the semiconductor device using the second electrode material 19 described in Embodiment 1 for explaining the technical background of the present invention, but the method for manufacturing the semiconductor device is not limited thereto. The semiconductor device can be manufactured using the second electrode material 24 described in Embodiment 2, and in this case, the effect similar to that in Embodiment 2 is obtained.

Claims

[1] A method of manufacturing a semiconductor device, wherein: - the semiconductor device comprises: - a plurality of semiconductor elements (1) comprising a semiconductor element (1) having a main cell part and at least one measuring cell part (4) and being provided with a plurality of signal pads (6, 7, 8, 9, 10) each corresponding to the main cell part and the measuring cell part (4); and - a relay substrate (2) provided with a plurality of control pads (12), - the procedure has: (a) connecting each of the semiconductor elements (1) and the relay substrate (2) on a circuit board (3); (b) connecting each signal pad (6, 7, 8, 9, 10) of each of the semiconductor elements (1) and each control pad (12) of the relay substrate (2) by a wire (17); (c) bonding a first electrode material (18) on each of the semiconductor elements (1); (d) bonding a second electrode material (19) having a short-circuiting part (21) that short-circuits each of the control pads (12) on the relay substrate (2); (e) sealing the circuit board (3), each of the semiconductor elements (1), the relay substrate (2), the first electrode material (18), and the second electrode material (19) by resin (23); and (f) grinding the resin (23) and removing the short-circuit part (21) to expose a part of the second electrode material (19). - the relay substrate (2) has a plurality of control terminals (14) which are electrically connected to each of the control pads (12), - the second electrode material (19) has a plurality of connecting parts (20) corresponding to each of the control terminals (14) and the short-circuit part (21) connecting each connecting part (20), and - in (d) each of the connecting parts (20) is electrically connected to each of the control terminals (14), and then each of the connecting parts (20) and the short-circuit parts (21) are electrically connected to each other. [2] The method according to claim 1, wherein the semiconductor element (1) is formed of SiC and the relay substrate (2) is formed of Si. [3] The method of claim 1, wherein: - the short-circuit part (21) is a plurality of wires (26) which connect the adjacent connecting parts (20) to one another, and - in (d) each of the connecting parts (20) is electrically connected to each of the control terminals (14), and then each of the wires (26) is wire-connected to electrically connect each of the connecting parts (20). [4] The method according to claim 1, wherein each of the connecting parts (20) is formed by covering a surrounding portion of a conductive material (27) provided with a plurality of slit-like holes with an insulating material (25), and then cutting out the conductive material (27) and the insulating material (25) in a vertical direction with respect to an extending direction of the holes. [5] A method of manufacturing a semiconductor device, wherein: - the semiconductor device comprises a semiconductor element (1) which has a main cell part and at least one measuring cell part (4) and which is provided with a plurality of signal terminals (28) which respectively correspond to the main cell part and the measuring cell part (4), and - the procedure has: (a) connecting the semiconductor element (1) to a circuit board (3); (b) bonding a first electrode material (18) to the semiconductor element (1); (c) bonding a second electrode material (19) having a short-circuiting part (21) that short-circuits each of the signal terminals (28) on the semiconductor element (1); (d) sealing the circuit board (3), the semiconductor element (1), the first electrode material (18), and the second electrode material (19) by means of resin (23); and (e) grinding the resin (23) and removing the short-circuit part (21) to expose a part of the second electrode material (19), - the second electrode material (19) has a plurality of connecting parts (20) corresponding to each of the signal terminals (28) and the short-circuit part (21) connecting each connecting part (20), and - in (c) each of the connecting parts (20) is electrically connected to each of the signal terminals (28), and then each of the connecting parts (20) and the short-circuit parts (21) are electrically connected to each other.

Citation Information

Patent Citations

  • Electronic component and semiconductor device

    DE212018000072U1

  • Method of manufacturing semiconductor device, semiconductor integrated device and method of manufacturing the same

    US20130234308A1

  • High-frequency module

    WO2019181760A1

  • Semiconductor package and production method therefor, and semiconductor device

    WO2020110170A1