Fully sealed supercapacitor and method for manufacturing the same

By using ceramic rings and metal layer sealing rings in supercapacitors to achieve fully sealed insulation isolation, and adopting automated processes, the problems of poor sealing performance and low production efficiency of traditional supercapacitors are solved, and the sealing strength and service life are significantly improved. Improved production efficiency.

CN107749351BActive Publication Date: 2024-10-18SHANGHAI AOWEI TECH DEV
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN201711156320.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2017-11-20
Publication Date
2024-10-18
Estimated Expiration
2037-11-20

AI Technical Summary

Technical Problem

Traditional supercapacitors have problems with poor sealing performance, short service life, and low production efficiency. This is mainly due to the limited high-temperature resistance of the rubber sealing ring and the high intensity of manual assembly, which leads to reduced sealing performance and increased chances of leakage.

Method used

It adopts a fully sealed supercapacitor design, using a ceramic ring and a metal layer sealing ring to connect the negative terminal and the negative outer cover through soldering to achieve fully sealed insulation isolation of the capacitor cells, and realize the production process through automatic laser welding and vacuum drying. automated operations.

Benefits of technology

The sealing strength and service life are improved, the probability of leakage is reduced, and the supercapacitor production process is automated, significantly improving production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN107749351B_ABST
    Figure CN107749351B_ABST
Patent Text Reader

Abstract

The present invention discloses a fully sealed supercapacitor and a manufacturing method thereof. The fully sealed supercapacitor comprises: a positive outer cover, a negative outer cover, a shell, a capacitor cell, a negative current collector, a negative terminal and a sealing ring. The positive outer cover and the negative outer cover are respectively connected to the two ends of the shell, the capacitor cell and the negative current collector are arranged inside the shell, one end of the capacitor cell is connected to the positive outer cover, the negative current collector is connected to the other end of the capacitor cell, the negative terminal is partially arranged inside the shell and connected to the negative current collector, and partially passes through the negative outer cover and is arranged outside the shell; there is a sealing gap between the negative terminal and the negative outer cover; the sealing ring comprises a ceramic ring and a metal layer arranged on the surface of the ceramic ring, the ceramic ring is arranged in the sealing gap, and is respectively brazed and connected to the negative outer cover and the negative terminal through the metal layer. The fully sealed supercapacitor has high sealing strength and high production efficiency. Accordingly, the present invention also provides a manufacturing method of a fully sealed supercapacitor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of electrochemical energy storage components, and in particular to a fully sealed supercapacitor and a manufacturing method thereof. Background Art

[0002] As an efficient energy storage component, supercapacitors have a series of advantages such as fast charging and discharging speed, high power density, long cycle life, and green environmental protection. They have been widely used in the fields of new energy vehicles, rail transportation, aerospace, and industrial automation. Generally, one end (positive or negative) of the supercapacitor's battery cell is connected to the shell, and the other end is insulated and sealed from the shell by a rubber seal. However, the high temperature resistance of the rubber seal is limited (generally not more than 260°C), and it is easy to age under long-term high temperature load, which greatly reduces the sealing performance and seriously limits the service life of the supercapacitor; and in order to prevent the rubber seal from deforming during the assembly process and increasing the chance of leakage during use, it is necessary to manually assemble the rubber seal and use the shell expansion method to prevent the seal from shifting. The assembly work is labor-intensive and the assembly efficiency is low, which affects the production efficiency of the supercapacitor. Therefore, traditional supercapacitors have technical problems such as poor sealing performance, short service life, and low production efficiency. Summary of the invention

[0003] The purpose of the present invention is to provide a fully sealed supercapacitor to overcome the technical problems of poor sealing performance, short service life and low production efficiency existing in traditional supercapacitors.

[0004] Another object of the present invention is to provide a method for manufacturing a fully sealed supercapacitor, which can realize fully automated operation of the supercapacitor production process and improve the supercapacitor production efficiency.

[0005] To achieve this object, the present invention adopts the following technical solutions:

[0006] A fully sealed supercapacitor comprises: a positive outer cover, a negative outer cover, an outer shell, a capacitor cell, a negative current collector, a negative terminal and a sealing ring, wherein the positive outer cover and the negative outer cover are respectively connected to the two ends of the outer shell, the capacitor cell and the negative current collector are arranged inside the outer shell, one end of the capacitor cell is connected to the positive outer cover, the negative current collector is connected to the other end of the capacitor cell, the negative terminal is partially arranged inside the outer shell and connected to the negative current collector, and partially passes through the negative outer cover and is arranged outside the outer shell; a sealing gap is formed between the part of the negative terminal arranged inside the outer shell and the negative outer cover; the sealing ring comprises a ceramic ring and a metal layer arranged on the surface of the ceramic ring, the ceramic ring is arranged in the sealing gap, and is respectively brazed to the negative outer cover and the negative terminal through the metal layer.

[0007] In one embodiment, the metal layer includes a metallization layer and a metal plating layer, and the metallization layer is disposed between the ceramic ring and the metal plating layer.

[0008] In one embodiment, the metallization layer is a molybdenum-manganese powder layer.

[0009] In one embodiment, the metal plating layer is a nickel plating layer.

[0010] In one embodiment, an insulating filling ring is further included, and an insulating gap is provided between the portion of the negative terminal passing through the negative outer cover and the negative outer cover. The insulating filling ring is arranged in the insulating gap and is respectively abutted and connected with the negative outer cover and the negative terminal.

[0011] In one of the embodiments, a sealing nail is further included. A liquid injection hole is opened on the negative electrode outer cover, and the sealing nail is inserted into the liquid injection hole and welded to the negative electrode outer cover.

[0012] In one of the embodiments, it also includes an explosion-proof plate. An exhaust hole is opened on the positive electrode outer cover. The explosion-proof plate is arranged in the exhaust hole and connected to the positive electrode outer cover.

[0013] In one embodiment, the thickness of the explosion-proof disk is 0.1 mm-0.3 mm, and the pressure adjustment range of the explosion-proof disk is 0.6 MPa-1.0 MPa.

[0014] The present invention also provides a method for manufacturing any of the above-mentioned supercapacitors, comprising the following steps:

[0015] Automatic laser welding to assemble the positive electrode cover, negative electrode cover, shell, capacitor core, negative electrode current collector, negative electrode terminal and sealing ring to obtain a fully sealed supercapacitor tooling;

[0016] Vacuum drying of fully sealed supercapacitor tooling;

[0017] The electrolyte is injected into the vacuum dried supercapacitor tooling and an aging operation is performed to obtain a fully sealed supercapacitor.

[0018] In one embodiment, the steps of injecting electrolyte into the vacuum dried supercapacitor tooling and performing an aging operation to obtain a fully sealed supercapacitor include:

[0019] Inject electrolyte into the vacuum dried supercapacitor tooling, and after injection, insert a glue nail into the injection hole to seal the supercapacitor tooling;

[0020] Perform aging treatment on the supercapacitor tooling after sealing with rubber nails;

[0021] After the aging treatment is completed, the rubber nail is pulled out to exhaust the aging gas, the sealing nail is inserted into the injection hole and the sealing nail is welded to the negative electrode outer cover to obtain a fully sealed supercapacitor.

[0022] The above-mentioned fully sealed supercapacitor, the negative terminal and the negative electrode outer cover are sealed by a sealing ring including a ceramic ring and a metal layer, the metal layer is arranged on the surface of the ceramic ring, and the ceramic ring is brazed and connected to the negative terminal and the negative electrode outer cover respectively through the metal layer, so as to realize the fully sealed insulation isolation of the negative electrode of the capacitor cell and the shell, and the sealing strength is high, which can effectively ensure the airtightness and reduce the leakage probability. In addition, the ceramic ring has stable performance and long service life, which can greatly extend the service life of the supercapacitor. At the same time, the sealing ring is brazed and connected to the negative terminal and the negative electrode outer cover, and the sealing ring assembly can realize automatic welding, realize the automatic operation of the entire production process of the supercapacitor, greatly save the labor intensity, and improve the production efficiency of the supercapacitor. Therefore, compared with the traditional supercapacitor, the above-mentioned fully sealed supercapacitor has the beneficial effects of high sealing strength, long service life, high degree of automation and high production efficiency. Accordingly, the above-mentioned fully sealed supercapacitor manufacturing method realizes the fully automated operation of the production process of the fully sealed supercapacitor, greatly reduces the labor intensity, and improves the production efficiency of the supercapacitor. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 is a schematic diagram of the structure of a fully sealed supercapacitor in one embodiment;

[0024] Figure 2 is a schematic structural diagram of a housing in one embodiment;

[0025] Figure 3 is a schematic structural diagram of a sealing ring in an embodiment;

[0026] Figure 4 yes Figure 3 AA structural cross-sectional view of the sealing ring shown;

[0027] Figure 5 is a schematic structural diagram of the connection between the negative electrode outer cover and the negative electrode terminal in one embodiment;

[0028] Figure 6 is a schematic structural diagram of a positive electrode outer cover in one embodiment;

[0029] Figure 7 The present invention is a flow chart of a method for manufacturing a fully sealed supercapacitor in an embodiment.

[0030] In the figure: 10-positive electrode outer cover, 20-negative electrode outer cover, 30-housing, 40-capacitor core, 50-negative electrode current collector, 60-negative electrode terminal, 70-sealing ring, 80-insulating filling ring, 90-sealing nail, 100-explosion-proof disk;

[0031] 11-exhaust hole, 21-liquid injection hole, 71-ceramic ring, 72-metal layer;

[0032] 721 -metallization layer, 722 -metal plating layer. DETAILED DESCRIPTION

[0033] The technical solution of the present invention is further described below with reference to the accompanying drawings and through specific implementation methods.

[0034] In the description of the present invention, it should be understood that the terms "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0035] Please also see Figures 1 to 4 A fully sealed supercapacitor of one embodiment includes: a positive electrode outer cover 10, a negative electrode outer cover 20, a shell 30, a capacitor cell 40, a negative electrode current collector 50, a negative electrode terminal 60 and a sealing ring 70. The positive electrode outer cover 10 and the negative electrode outer cover 20 are respectively connected to both ends of the shell 30, the capacitor cell 40 and the negative electrode current collector 50 are arranged inside the shell 30, one end of the capacitor cell 40 is connected to the positive electrode outer cover 10, and the negative electrode current collector 50 is connected to the other end of the capacitor cell 40. The negative electrode terminal 60 is partially arranged inside the shell 30 and connected to the negative electrode current collector 50, and partially passes through the negative electrode outer cover 20 and is arranged outside the shell 30; there is a sealed gap between the part of the negative electrode terminal 60 arranged inside the shell 30 and the negative electrode outer cover 20; the sealing ring 70 includes a ceramic ring 71 and a metal layer 72 arranged on the surface of the ceramic ring 71, the ceramic ring 71 is arranged in the sealed gap, and is brazed and connected to the negative electrode outer cover 20 and the negative electrode terminal 60 respectively through the metal layer 72.

[0036] Specifically, the capacitor cell 4 is filled with electrolyte, the negative electrode cover 20 and the negative electrode terminal 60 are made of aluminum, copper and its alloy or copper-plated nickel, the outer shell 30 is integrated with the positive electrode current collector, the outer shell 30 and the positive electrode current collector are integrally stamped, the positive electrode cover 10 is integrally formed with the positive electrode terminal, and the positive electrode cover 10 and the outer shell 30 are made of aluminum or aluminum alloy. The capacitor cell 40 and the positive electrode current collector are connected by laser welding, the positive electrode cover 10 is closely contacted with the positive electrode current collector by interference fit, and is sealed and connected with the outer shell 30 by laser welding, the negative electrode current collector 50 is laser welded and connected with the capacitor cell 40, the negative electrode terminal 60 is laser welded and connected with the negative electrode current collector 50, the negative electrode cover 20 is laser welded and connected with the outer shell 30, and the negative electrode terminal 60 and the negative electrode cover 20 are brazed and sealed as one by a sealing ring.

[0037] In the above-mentioned fully sealed supercapacitor, the surface of the ceramic ring 71 is provided with a metal layer 72, and the ceramic ring 71 is brazed and connected to the negative electrode outer cover 20 and the negative terminal 60 respectively through the metal layer 72. During the brazing process, the solder alloy melted at high temperature and the metal layer 72, the metal surface of the negative electrode outer cover 20 and the negative electrode terminal 60 all have good wettability, and high-strength and highly reliable sealing welding can be achieved. When the sealing ring 70 of the fully sealed supercapacitor is assembled, the negative terminal 60 and the sealing ring 70, and the sealing ring 70 and the negative electrode outer cover 20 are respectively brazed at high temperature under an inert atmosphere by brazing solder, and the integrated sealed negative terminal and negative electrode outer cover structure can be obtained, and the negative electrode of the capacitor cell 40 and the shell 30 are fully sealed and insulated, and the sealing strength is high, and the automatic welding of the sealing ring 70 can be achieved, which can greatly improve the production efficiency of the supercapacitor.

[0038] like Figure 4 As shown, in one embodiment, the metal layer 72 includes a metallization layer 721 and a metal plating layer 722, and the metallization layer 721 is disposed between the ceramic ring 71 and the metal plating layer 722. Specifically, as Figure 4 As shown, the metal layers 72 are arranged on two opposite sides of the ceramic ring 71, and the two oppositely arranged metal layers 72 are spaced apart, thereby forming an insulating section on the ceramic ring 71 to ensure the sealing performance of the sealing ring 70 while ensuring the insulation performance of the sealing ring 70, and to ensure stable insulation between the negative terminal 60 and the negative outer cover 20.

[0039] In one embodiment, the metallization layer 721 is a molybdenum-manganese powder layer, and the metal plating layer 722 is a nickel plating layer. Specifically, the sealing ring 70 is obtained by screen printing a molybdenum-manganese electronic conductive paste on the surface of the ceramic ring 71, sintering at high temperature to form a molybdenum-manganese powder layer, and then chemically plating nickel to form a nickel plating layer. Further, the ceramic ring 71 is sintered and formed by mixing Al2O3, ZrO2, a modifier, and a sintering aid. After the ceramic ring 71 is sintered, the molybdenum-manganese electronic conductive paste is printed on the opposite sides of the ceramic ring 71 by screen printing. After vacuum high-temperature sintering, the ceramic ring 71 and the molybdenum-manganese powder on the surface are firmly combined to form a molybdenum-manganese powder layer, and then chemically nickel is plated in the aqueduct to form a nickel plating layer on the surface of the molybdenum-manganese powder layer. In this embodiment, the metallization layer 721 is a molybdenum-manganese powder layer, and the conductive paste uses molybdenum-manganese powder and a small amount of binder, and the particle size of the molybdenum powder does not exceed 3um. In other embodiments, the metallization layer can also be other metal powder layers, such as a silver powder layer, a palladium powder layer or a gold powder layer, and the corresponding electronic conductive paste can be silver paste, palladium paste or gold paste. Therefore, the above metallization layer 721 using a molybdenum manganese powder layer is only an embodiment and is not used to limit the present invention.

[0040] like Figure 1 , Figure 5As shown, in one embodiment, the fully sealed supercapacitor further includes an insulating filling ring 80, and there is an insulating gap between the portion of the negative terminal 60 passing through the negative outer cover 20 and the negative outer cover 20, and the insulating filling ring 80 is arranged in the insulating gap, and is respectively abutted and connected with the negative outer cover 20 and the negative terminal 60. The diameter of the insulating filling ring 80 is smaller than the diameter of the sealing ring 70. The insulating filling ring 80 is arranged in the insulating gap, which can further improve the insulation performance between the negative outer cover 20 and the negative terminal 60, and ensure the insulation stability between the negative terminal 60 and the shell 30. In this embodiment, a small-diameter insulating filling ring 80 is used to fill the insulating gap, so that the sealing ring 70 can adopt a common ring design, which is conducive to enhancing the mechanical strength of the sealing ring 70 and improving the mechanical strength of the insulation structure as a whole. In one embodiment, in order to be consistent with the material of the sealing ring 70, the insulating filling ring 80 is a ceramic filling ring. However, in other embodiments, the insulating filling ring can also be a rubber filling ring, a silicone filling ring or a plastic filling ring.

[0041] Furthermore, in one embodiment, an injection hole 21 is provided on the negative electrode outer cover 20, and the fully sealed supercapacitor also includes a sealing nail 90. The injection hole 21 is used to inject electrolyte during the generation process. The sealing nail 90 is inserted into the injection hole 21 and welded to the negative electrode outer cover 20 to seal the injection hole 21 after the electrolyte injection is completed.

[0042] like Figure 1 , Figure 6 As shown, in one embodiment, the fully sealed supercapacitor further includes an explosion-proof disc 100 , a vent hole 11 is opened on the positive electrode outer cover 10 , and the explosion-proof disc 100 is arranged in the vent hole 11 and connected to the positive electrode outer cover 10 .

[0043] Generally, during the use of supercapacitors, due to the catalytic decomposition of the electrolyte by the activated carbon electrode, gas will be continuously generated inside the capacitor and a certain internal pressure will be generated. Once there is too much gas and the internal pressure is too high, an explosion is likely to occur, which makes the supercapacitor a safety hazard. In this embodiment, an explosion-proof plate 100 is installed on the positive electrode outer cover 10. When the internal pressure reaches the preset pressure value of the explosion-proof plate 100, the explosion-proof plate 100 will rupture and exhaust in time to avoid explosion, thereby reducing the danger of the supercapacitor during use, ensuring safe use, and greatly improving product reliability. In one embodiment, the thickness of the explosion-proof plate 100 is 0.1mm-0.3mm, and the pressure adjustment range of the explosion-proof plate is 0.6MPa-1.0MPa. Furthermore, the explosion-proof plate 100 is made of PP (Polypropylene) film.

[0044] The above-mentioned fully sealed supercapacitor, the negative terminal 60 and the negative outer cover 20 are sealed by a sealing ring 70 including a ceramic ring 71 and a metal layer 72, the metal layer 72 is arranged on the surface of the ceramic ring 71, and the ceramic ring 71 is brazed and connected to the negative terminal 60 and the negative outer cover 20 respectively through the metal layer 72, so as to achieve fully sealed insulation isolation between the negative electrode of the capacitor cell 40 and the shell 30, with high sealing strength, which can effectively ensure airtightness and reduce the probability of leakage. The leakage rate during the use of the product is reduced from the original 1.5% to zero leakage, which can meet the high-quality reliability requirements of industrial fields such as new energy vehicles / aerospace, and has a wide range of applications. In addition, the ceramic ring 71 has stable performance and long service life, which can greatly extend the service life of the supercapacitor. At the same time, the sealing ring 70 is brazed with the negative terminal 60 and the negative outer cover 20. The sealing ring 70 assembly can realize automatic welding, realize the automatic operation of the entire production process of the supercapacitor, greatly save the labor intensity, and improve the production efficiency from 1PPM (1 supercapacitor / lithium-ion capacitor per minute) of the traditional supercapacitor to more than 10PPM, greatly improving the production efficiency of the supercapacitor. Compared with the traditional supercapacitor, the above-mentioned fully sealed supercapacitor has the beneficial effects of high sealing strength, long service life, high degree of automation, high production efficiency, and a wide range of applications.

[0045] See also Figure 7 The present invention also provides a method for manufacturing a fully sealed supercapacitor, comprising the following steps:

[0046] S110: Automatic laser welding to assemble the positive electrode outer cover 10, the negative electrode outer cover 20, the housing 30, the capacitor cell 40, the negative electrode current collector 50, the negative electrode terminal 60 and the sealing ring 70 to obtain a fully sealed supercapacitor tooling.

[0047] Specifically, the negative terminal 60 and the sealing ring 70 are first connected by high-temperature brazing, and then the sealing ring 70 and the negative outer cover 20 are brazed at high temperature to obtain the negative terminal 60 and the negative outer cover 20 that are sealed and connected, and the negative terminal 60 and the negative terminal and the sealing ring 70 are assembled; further, in one embodiment, after the sealing ring 70 and the negative terminal 60 and the negative terminal 60 are laser brazed, the insulating filling ring 80 is also sleeved on the negative terminal 60 to fill the insulating gap between the negative terminal 60 and the negative outer cover 20 to insulate The filling ring 80 is assembled; thereafter, the capacitor cell 40 is first connected to the negative electrode collector 50 by laser welding, and then the negative electrode collector 50 is connected to the negative electrode terminal 60 by laser welding; then, the negative electrode outer cover 20 and the outer shell 30 are sealed by laser welding, the capacitor cell 40 and the outer shell 30 are connected by laser welding, and then the positive electrode outer cover 10 is made to be closely contacted with the positive electrode collector integrated with the outer shell 30 by interference fit, and the positive electrode outer cover 10 and the outer shell 30 are sealed by laser welding to obtain a fully sealed supercapacitor tooling.

[0048] Furthermore, during the assembly process of the negative terminal 60, the negative outer cover 10 and the sealing ring 70, the negative terminal 60 and the sealing ring 70 and the sealing ring 70 and the negative outer cover 20 are brazed at high temperature in an inert atmosphere by brazing solder to obtain an integrated sealed negative terminal 60 and negative outer cover 10 sealing structure. Generally, the negative terminal 10 contains aluminum, and the melting point of aluminum is 660 degrees. Therefore, the brazing solder uses a low melting point alloy, such as a silver-copper alloy with a melting point between 540°C and 850°C, and the inert gas can be nitrogen, argon or helium.

[0049] S112: vacuum drying the fully sealed supercapacitor tooling. Specifically, the welded fully sealed supercapacitor tooling is placed in a tunnel vacuum oven for drying and dehydration.

[0050] S114: injecting electrolyte into the vacuum dried supercapacitor tooling and performing aging operation to obtain a fully sealed supercapacitor.

[0051] Specifically, the supercapacitor tooling after vacuum drying and dehydration is placed on the liquid injection machine and vacuum injected through the liquid injection hole 217, and a quantitative electrolyte is injected and sealed for aging to obtain a fully sealed supercapacitor. Further, the fully sealed supercapacitor is laser-coded and then enters the automatic testing machine to test the product capacity and internal resistance. After the test is completed, the code is automatically scanned and sorted into the warehouse, completing the test and packaging of the fully sealed supercapacitor.

[0052] In one embodiment, step S140 includes the following steps: injecting electrolyte into the supercapacitor tooling after vacuum drying, and after injection, inserting the glue nail into the injection hole to seal the supercapacitor tooling; performing aging treatment on the supercapacitor tooling sealed with the glue nail; after the aging treatment is completed, pulling out the glue nail, exhausting the aging gas, inserting the sealing nail into the injection hole and welding the sealing nail to the negative electrode outer cover to obtain a fully sealed supercapacitor.

[0053] Specifically, during the aging process, due to the catalytic decomposition of the electrolyte by the activated carbon electrode, a large amount of gas will be generated inside the supercapacitor, which will have a certain internal pressure. Once there is too much gas, it is easy to explode, posing a safety hazard. In this embodiment, during the aging process, the supercapacitor is first pre-sealed with glue nails and then put into the automatic aging machine for aging. After aging, the glue nails are pulled out to discharge the gas generated during the aging stage of the supercapacitor, and then the sealing nails 90 are inserted for sealing, thereby minimizing the gas production and internal pressure of the supercapacitor during subsequent use, further reducing the danger during the use of the supercapacitor, and improving product reliability. In one embodiment, the glue nails are plastic glue nails.

[0054] In the manufacturing method of the fully sealed supercapacitor, all parts of the fully sealed supercapacitor tooling are welded and sealed by laser welding. During the production process, the conveyor belt and the mechanical arm are used to realize the fully automated operation of the fully sealed supercapacitor tooling assembly and sealing, which can greatly improve the production efficiency of the supercapacitor. The production efficiency can be increased from 1PPM (1 supercapacitor / lithium-ion capacitor per minute) of the traditional supercapacitor to more than 10PPM. In addition, the sealing structure of the fully sealed supercapacitor and the manufacturing method of the fully sealed supercapacitor are also applicable to products such as lithium-ion capacitors, secondary batteries and traditional capacitors, and have a wide range of applications.

[0055] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0056] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A fully sealed supercapacitor, characterized in that: include: A positive electrode outer cover (10), a negative electrode outer cover (20), an outer shell (30), a capacitor cell (40), a negative electrode current collector (50), a negative electrode terminal (60) and a sealing ring (70), wherein the positive electrode outer cover (10) and the negative electrode outer cover (20) are respectively connected to two ends of the outer shell (30), the capacitor cell (40) and the negative electrode current collector (50) are arranged inside the outer shell (30), one end of the capacitor cell (40) is connected to the positive electrode outer cover (10), the negative electrode current collector (50) is connected to the other end of the capacitor cell (40), and the negative electrode terminal (60) is partially arranged inside the outer shell (30) and connected to the negative electrode current collector ( 50), part of which passes through the negative electrode outer cover (20) and is arranged outside the housing (30); a sealing gap is formed between the part of the negative electrode terminal (60) arranged inside the housing (30) and the negative electrode outer cover (20); the sealing ring (70) comprises a ceramic ring (71) and a metal layer (72) arranged on the surface of the ceramic ring (71); the ceramic ring (71) is arranged in the sealing gap, and the ceramic ring (71) is respectively connected to the negative electrode outer cover (20) and the negative electrode terminal (60) by brazing through the metal layer (72), thereby reducing the probability of liquid leakage and realizing automatic welding of the sealing ring (70); The metal layers (72) are arranged on two opposite surfaces of the ceramic ring (71), and the two oppositely arranged metal layers (72) are arranged at an interval, thereby forming an insulating section on the ceramic ring (71), so as to ensure the sealing performance of the sealing ring (70) while ensuring the insulation performance of the sealing ring (70); The metal layer (72) comprises a metallized layer (721) and a metal plating layer (722), wherein the metallized layer (721) is arranged between the ceramic ring (71) and the metal plating layer (722); It also includes an insulating filling ring (80), wherein an insulating gap is formed between the portion of the negative electrode terminal (60) that passes through the negative electrode outer cover (20) and the negative electrode outer cover (20), and the insulating filling ring (80) is arranged in the insulating gap and is respectively abutted and connected to the negative electrode outer cover (20) and the negative electrode terminal (60).

2. The fully sealed supercapacitor according to claim 1, characterized in that: The metallization layer (721) is a molybdenum-manganese powder layer.

3. The fully sealed supercapacitor according to claim 1, characterized in that: The metal plating layer (722) is a nickel plating layer.

4. The fully sealed supercapacitor according to claim 1, characterized in that: It also includes a sealing nail. The negative electrode outer cover is provided with a liquid injection hole. The sealing nail is inserted into the liquid injection hole and is welded to the negative electrode outer cover.

5. The fully sealed supercapacitor according to claim 1, characterized in that: It also comprises an explosion-proof sheet (100), the positive electrode outer cover (10) is provided with an exhaust hole (11), and the explosion-proof sheet (100) is arranged in the exhaust hole (11) and connected to the positive electrode outer cover (10).

6. The fully sealed supercapacitor according to claim 5, characterized in that: The thickness of the explosion-proof disk (100) is 0.1 mm-0.3 mm, and the pressure adjustment range of the explosion-proof disk (100) is 0.6 MPa-1.0 MPa.

7. A method for manufacturing a fully sealed supercapacitor according to any one of claims 1 to 6, characterized in that: The following steps are involved: First, the negative terminal (60) and the sealing ring (70) are connected by high-temperature brazing, and then the sealing ring (70) and the negative outer cover (20) are brazed at high temperature to obtain a sealed negative terminal (60) and a negative outer cover (20), and the negative terminal (60) and the sealing ring (70) are assembled. Then, the insulating filling ring (80) is sleeved on the negative terminal (60) to fill the insulating gap between the negative terminal (60) and the negative outer cover (20), and the insulating filling ring (80) is assembled. Then, the capacitor cell ( 40) is connected to the negative electrode current collector (50) by laser welding, and the negative electrode current collector (50) and the negative electrode terminal (60) are connected by laser welding; then, the negative electrode outer cover (20) and the outer shell (30) are sealed by laser welding, and the capacitor cell (40) and the outer shell (30) are connected by laser welding, and then the positive electrode outer cover (10) is tightly contacted with the positive electrode current collector integrated with the outer shell (30) by interference fit, and the positive electrode outer cover (10) and the outer shell (30) are sealed by laser welding to obtain a fully sealed supercapacitor tooling; vacuum drying the fully sealed supercapacitor tooling; The electrolyte is injected into the vacuum dried supercapacitor tooling and an aging operation is performed to obtain a fully sealed supercapacitor.

8. The method for manufacturing a fully sealed supercapacitor according to claim 7, characterized in that: The step of injecting electrolyte into the vacuum dried supercapacitor tooling and performing aging operation to obtain a fully sealed supercapacitor comprises: Inject electrolyte into the vacuum dried supercapacitor tooling, and after injection, insert a glue nail into the injection hole to seal the supercapacitor tooling; Perform aging treatment on the supercapacitor tooling after sealing with rubber nails; After the aging treatment is completed, the rubber nail is pulled out to exhaust the aging gas, the sealing nail is inserted into the injection hole and the sealing nail is welded to the negative electrode outer cover to obtain a fully sealed supercapacitor.

Citation Information

Patent Citations

  • Super capacitor with two extracted ends

    CN102074358A

  • Ceramic sealed battery

    CN103441224A

  • Super capacitor with positive electrode and negative electrode at same end

    CN202796465U

  • Totally enclosed ultracapacitor system

    CN207425642U

  • Sealing means for terminal section of sealed type storage battery

    US4337302A