A device and method for orifice correction of large-diameter high-strength steel pipe tile assembly

By designing an orthodontic device for large-diameter high-strength steel pipes, and utilizing the sliding fit and wedge-shaped tightening mechanism of the mold outer body, outer mold, inner mold and wedge, the problem of misaligned pipe openings in the assembly of pressure steel pipe tiles in hydropower stations is solved. , achieving efficient tile assembly and welding quality assurance.

CN108607902BActive Publication Date: 2024-10-15CHINA GEZHOUBA GROUP MACHINERY & SHIP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201810532896.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2018-05-29
Publication Date
2024-10-15
Estimated Expiration
2038-05-29

AI Technical Summary

Technical Problem

During the assembly process of high-strength pressure steel pipe tiles in hydropower stations, the problem of misalignment of the pipe mouth is difficult to solve, which increases the difficulty of assembly. Direct welding of high-strength steel materials is not allowed, which affects the welding quality.

Method used

A device including the outer mold body, outer mold, inner mold and wedge is designed. Through sliding fit and wedge-shaped tightening mechanism, the pipe mouth is corrected, avoiding additional welding and ensuring the positioning accuracy and welding quality of the tile assembly.

Benefits of technology

It effectively eliminates dimensional deviations, improves welding quality, reduces costs, and improves production efficiency. It is suitable for orthopedic positioning assembly of large-diameter high-strength steel pipes, ensuring the accuracy of tile assembly and welding quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN108607902B_ABST
    Figure CN108607902B_ABST
Patent Text Reader

Abstract

The present invention discloses a device and method for orthopedic assembly of large-caliber high-strength steel pipe tiles, which comprises a mold outer body, a rectangular through hole is processed in the middle part of the mold outer body, a notch is processed in the bottom edge of the rectangular through hole, a first mounting plate and a second mounting plate are formed on both sides of the notch, an outer mold is slidably mounted on the first mounting plate, an inner mold is slidably mounted on the second mounting plate, a first wedge is arranged between the outer mold and the inner wall of the rectangular through hole, and a second wedge is arranged between the inner mold and the outer wall of the rectangular through hole. It effectively improves the assembly quality of large-caliber steel pipes and high-strength pressure steel pipes before welding, eliminates dimensional deviations, ensures that the ovality of the steel pipe meets the specification requirements, so as to reduce the energy loss of water in the flow of the steel pipe, and effectively ensures the welding quality of the longitudinal seam of the steel pipe.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a device and method for correcting the misalignment of pipe orifices during assembly of large-diameter steel pipe tiles, belonging to the technical field of pre-deformation correction of metal structural parts. The device and method are mainly used for the correction positioning assembly of pipe orifices with large misalignment during assembly of high-strength pressure steel pipe tiles in hydropower stations, and can also be used for the correction of pipe orifices during longitudinal seam assembly of large-diameter steel pipes made of other materials in other industries. Background Art

[0002] Penstock is an important part of the water supply structure of the hydropower station. It connects the water inlet of the power station and the turbine volute, and plays the role of introducing water from the water inlet into the volute and promoting the rotation of the turbine. The common layout forms of penstock are dam-in, tunnel-in and open-air. The diameter of the dam-in penstock is larger, usually composed of 2 to 3 tiles. The maximum diameter of the penstock of the water diversion system of 26 units in the left and right bank powerhouses of the Three Gorges Power Station is 12.8 meters. The maximum diameter of the penstock of the water diversion system of the 4 units in the underground powerhouse on the right bank of the Xiangjiaba Hydropower Station is 14.4 meters, which is the largest diameter penstock in the world so far. This kind of penstock is often manufactured on site, and a single pipe section is composed of 3 tiles. At the same time, the selection of materials for penstocks is gradually developing towards high strength. From the original use of 16Mn materials, it has developed to a large number of 600MPa and 800MPa high-strength steels. The pressure steel pipes of the Wudongde Hydropower Station in China are all made of 800MPa high-strength steel, and the pressure steel pipes of the Baihetan Hydropower Station also use a large amount of 600MPa and 800MPa high-strength steel.

[0003] Due to the particularity of high-strength steel materials, when assembling pressure steel pipe tiles, it is strictly forbidden to weld the code directly on the tiles to force fixation, which undoubtedly greatly increases the difficulty of tile assembly and positioning. In particular, the problem of pipe mouth misalignment correction is a difficulty in pressure steel pipe manufacturing. The present invention focuses on solving the problem of assembly correction of such large-diameter high-strength pressure steel pipes. Not only does it protect the material, but it also meets the assembly quality. The production process is low-cost, high-efficiency, and easy to implement on site. Summary of the invention

[0004] The present invention mainly provides a device and method for the pipe mouth correction of large-diameter high-strength steel pipe tile assembly for the commonly used submerged arc welding method, which effectively improves the assembly quality of large-diameter steel pipes and high-strength pressure steel pipes before welding, eliminates dimensional deviations, and ensures that the ovality of the steel pipe meets the requirements of the specifications, so as to reduce the energy loss of water in the flow of the steel pipe, and effectively ensures the welding quality of the longitudinal seam of the steel pipe.

[0005] In order to solve the above technical problems, the present invention proposes the following technical solutions: a device for correcting the pipe orifices of large-diameter high-strength steel pipe tiles for assembly, which includes a mold outer body, a rectangular through hole is processed in the middle part of the mold outer body, a notch is processed in the bottom edge of the rectangular through hole, and a first mounting plate and a second mounting plate are formed on both sides of the notch, an outer mold is slidably mounted on the first mounting plate, and an inner mold is slidably mounted on the second mounting plate, a first wedge block is arranged between the outer mold and the inner wall of the rectangular through hole, and a second wedge block is arranged between the inner mold and the outer wall of the rectangular through hole.

[0006] A quadrangular pyramid head is processed on the top of the mold outer body, a first dovetail slide rail is processed on the top of the first mounting plate, and a second dovetail slide rail is processed on the top of the second mounting plate.

[0007] The outer mold is processed with an outer mold inclined surface, and the surface opposite to the outer mold inclined surface is processed with an outer mold inner arc surface, the outer mold inner arc surface matches the outer circumference of the steel pipe, an outer mold pin hole is processed at the center position of the outer mold, and an outer mold dovetail groove is processed on the outer mold, and the outer mold dovetail groove forms a sliding fit with the first dovetail slide rail of the mold outer body.

[0008] The inner mold is processed with an inner mold inclined surface, and the surface opposite to the inner mold inclined surface is processed with an inner mold outer arc surface, the inner mold outer arc surface matches the inner circumference of the steel pipe, an inner mold pin hole is processed at the center position of the inner mold, and an inner mold dovetail groove is processed on the inner mold, and the inner mold dovetail groove forms a sliding fit with the second dovetail slide rail of the mold outer body.

[0009] The first wedge block and the second wedge block adopt the same structure. The first wedge block includes a wedge-shaped surface, and the wedge-shaped surface forms a wedge-shaped tight fit with the outer mold inclined surface of the outer mold and the inner mold inclined surface of the inner mold. A vertical surface is processed on the surface opposite to the wedge surface, and a wedge pin hole is processed at the center position of the first wedge block.

[0010] The mold outer body, the first wedge block and the second wedge block are made of forged steel material.

[0011] The outer mold and the inner mold are made of the same material as the steel pipe, and the outer surfaces of the outer mold and the inner mold are processed by a quenching process.

[0012] Any method for correcting the orifice of a large-diameter high-strength steel pipe tile assembly device, comprising the following steps:

[0013] Step 1: Determine the misalignment of the tile nozzle;

[0014] Step 2: Select the corresponding correction method according to different misalignment situations;

[0015] Step 3: Use the device to correct the misalignment of the tile pipe opening.

[0016] The misalignment in Step 2 includes two situations: arc prefabrication transition and arc prefabrication not in place;

[0017] The correction operation method of the arc prefabrication transition comprises the following steps:

[0018] Step 21: Connect the outer mold and the first wedge into a whole through the built-in bayonet pin;

[0019] Step 22: Assemble the outer mold with the first dovetail slide rail of the mold outer body through the dovetail groove of the outer mold, so that it is fixed on the first mounting plate of the mold outer body;

[0020] Step 23: Assemble the inner mold with the second dovetail slide rail of the mold outer body through the dovetail groove of the inner mold, and then pre-install it on the second mounting plate of the mold outer body;

[0021] Step 24: Hoist the entire device to the center of the part of the steel pipe mouth that needs to be corrected, assemble and adjust it in place, ensure that the outer mold and the outer body of the mold are locked in place, and make the outer mold and the outer circumference of the A port side of the steel pipe mouth in good contact;

[0022] Step 25: Adjust the inner mold so that it has good contact with the inner circumference of the B port side of the steel pipe mouth, lock the inner mold horizontally, and it is free in the vertical direction of the pipe mouth;

[0023] Step 26: Pre-tighten the inner ends of the inner mold and the outer mold body with a second wedge, and check to ensure that the inner mold, the outer mold and the outer mold body are firmly assembled;

[0024] Step 27: Use a sledgehammer to discontinuously apply force to the second wedge block on its outer end face. Under the continuous squeezing action of the second wedge block, the outer arc surface of the inner mold and the inner arc surface of the outer mold fit with the outer circumference and inner circumference of the correction part. After the second wedge block is in place, the B port of the steel pipe naturally fits into place with the A port, achieving the purpose of pipe orifice correction.

[0025] The correction operation method for the inadequate prefabrication of the arc comprises the following steps:

[0026] Step 31: Connect the inner mold and the second wedge into a whole through the built-in bayonet pin;

[0027] Step 32: Assemble the inner mold with the second dovetail rail of the mold outer body through the inner mold dovetail groove, so that it is fixed on the second mounting plate of the mold outer body;

[0028] Step 33: Assemble the outer mold with the first dovetail slide rail of the mold outer body through the outer mold dovetail groove, and then pre-install it on the first mounting plate of the mold outer body;

[0029] Step 34: hoist the entire device to the center of the part of the steel pipe mouth that needs to be corrected, assemble and adjust it in place, ensure that the inner mold and the outer body of the mold are locked in place, and make the inner mold and the inner circumference of the D port side of the steel pipe mouth in good contact;

[0030] Step 35: Adjust the outer mold so that it has good contact with the outer circumference of the C-port side of the steel pipe mouth, lock the outer mold horizontally, and it is free in the vertical direction of the pipe mouth;

[0031] Step 36: Pre-tighten the inner ends of the outer mold and the outer body of the mold with the first wedge, and check to ensure that the inner mold, the outer mold and the outer body of the mold are firmly assembled;

[0032] Step 37: Use a sledgehammer to discontinuously apply force to the first wedge block on its outer end face. Under the continuous squeezing action of the first wedge block, the outer arc surface of the inner mold and the inner arc surface of the outer mold fit with the outer circumference and inner circumference of the correction part. After the first wedge block is in place, the C port of the steel pipe naturally fits into place with the D port, achieving the purpose of pipe orifice correction.

[0033] The present invention has the following beneficial effects:

[0034] 1. The structure of the device is simple to manufacture. According to the specific construction conditions on site, the appropriate outer mold, first wedge, inner mold and second wedge are calculated and selected. The operation process is convenient, the cost is low, the practicability is good, and the production efficiency is high. It can be effectively used for large-diameter high-strength pressure steel pipe assembly and correction, ensuring the assembly positioning accuracy of the tile and ultimately ensuring its welding quality.

[0035] 2. By adopting the outer mold and inner mold of the above structure, on the one hand, they can cooperate with the outer circumference or inner circumference of the pressure steel pipe, and on the other hand, they can cooperate with the wedge, thereby clamping the outer mold or the inner mold, and finally realizing the correction of the pipe mouth.

[0036] 3. By slidingly matching the outer mold and the inner film with the outer body of the mold, it can ensure normal sliding during the wedge clamping process, thereby applying pressure to correct the pipe mouth. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] The present invention will be further described below in conjunction with the accompanying drawings and embodiments.

[0038] Figure 1 It is a schematic diagram of the overall assembly structure of the present invention.

[0039] Figure 2 It is a schematic diagram of the outer structure of the mold of the present invention.

[0040] Figure 3 It is a schematic diagram of the outer mold structure of the present invention.

[0041] Figure 4This is a schematic diagram of the first wedge structure of the present invention.

[0042] Figure 5 It is a schematic diagram of the inner mold structure of the present invention.

[0043] Figure 6 This is an operating state diagram of the present invention when the arc is prefabricated in transition.

[0044] Figure 7 This is a diagram of the operating state of the present invention when the curvature is not prefabricated in place.

[0045] In the figure: mold outer body 1, outer mold 2, first wedge block 3, inner mold 4, second wedge block 5, bayonet pin 6;

[0046] A quadrangular pyramid head 101, a rectangular through hole 102, a first dovetail slide rail 103, a first mounting plate 104, a notch 105, a second mounting plate 106, and a second dovetail slide rail 107;

[0047] The outer mold inclined surface 201, the outer mold pin hole 202, the outer mold inner arc surface 203, and the outer mold dovetail groove 204;

[0048] Wedge pin hole 301, vertical surface 302, wedge surface 303;

[0049] Inner mold inclined surface 401, inner mold outer arc surface 402, inner mold pin hole 403, inner mold dovetail groove 404. DETAILED DESCRIPTION

[0050] The embodiments of the present invention are further described below in conjunction with the accompanying drawings.

[0051] Embodiment 1:

[0052] like Figure 1-7 , a device for correcting the pipe mouth of large-diameter high-strength steel pipe tile assembly, which includes a mold outer body 1, a rectangular through hole 102 is processed in the middle part of the mold outer body 1, a notch 105 is processed at the bottom edge of the rectangular through hole 102, a first mounting plate 104 and a second mounting plate 106 are formed on both sides of the notch 105, an outer mold 2 is slidably mounted on the first mounting plate 104, an inner mold 4 is slidably mounted on the second mounting plate 106, a first wedge block 3 is arranged between the outer mold 2 and the inner wall of the rectangular through hole 102, and a second wedge block 5 is arranged between the inner mold 4 and the outer wall of the rectangular through hole 102. By adopting the above-mentioned device, it can be used for the deformation correction of the pipe mouth of the pressure steel pipe, which is simple to operate and easy to use, and can well ensure the correction accuracy. Due to the particularity of the high-strength steel in the manufacturing process, it cannot be forced to assemble by welding codes as arbitrarily as carbon steel and low-alloy structural steel. The codeless assembly method is used as much as possible during the assembly process to ensure that the parent material is not damaged. The use of the above device does not require additional code welding, thus ensuring the quality of the base material.

[0053] Furthermore, a quadrangular pyramid head 101 is processed on the top of the mold outer body 1, a first dovetail slide 103 is processed on the top of the first mounting plate 104, and a second dovetail slide 107 is processed on the top of the second mounting plate 106. By adopting the above mold outer body 1, the outer mold 2 and the inner mold 4 can be assembled to ensure the subsequent correction process.

[0054] Furthermore, the outer mold 2 is processed with an outer mold inclined surface 201, and the surface opposite to the outer mold inclined surface 201 is processed with an outer mold inner arc surface 203, and the outer mold inner arc surface 203 matches the outer circumference of the steel pipe, and an outer mold pin hole 202 is processed at the center position of the outer mold 2, and an outer mold dovetail groove 204 is processed on the outer mold 2, and the outer mold dovetail groove 204 forms a sliding match with the first dovetail slide rail 103 of the mold outer body 1. The outer mold inner arc surface 203 can generate a certain pressing force on the outer circumference of the steel pipe, and cooperate with the outer circle of the steel pipe to correct it.

[0055] Furthermore, the inner mold 4 is processed with an inner mold bevel 401, and the surface opposite to the inner mold bevel 401 is processed with an inner mold outer arc surface 402, the inner mold outer arc surface 402 cooperates with the inner circumference of the steel pipe, an inner mold pin hole 403 is processed at the center position of the inner mold 4, and an inner mold dovetail groove 404 is processed on the inner mold 4, and the inner mold dovetail groove 404 forms a sliding fit with the second dovetail slide rail 107 of the mold outer body 1.

[0056] Furthermore, the first wedge block 3 and the second wedge block 5 adopt the same structure. The first wedge block 3 includes a wedge surface 303. The wedge surface 303 forms a wedge-shaped tight fit with the outer mold inclined surface 201 of the outer mold 2 and the inner mold inclined surface 401 of the inner mold 4. A vertical surface 302 is processed on the surface opposite to the wedge surface 303, and a wedge pin hole 301 is processed at the center position of the first wedge block 3.

[0057] Furthermore, the mold outer body 1, the first wedge block 3 and the second wedge block 5 are made of forged steel, which ensures the structural strength.

[0058] Furthermore, the outer mold 2 and the inner mold 4 are made of the same material as the steel pipe, and the outer surfaces of the outer mold 2 and the inner mold 4 are quenched. The quenching process ensures the strength of the surface and increases the wear resistance of the surface.

[0059] Embodiment 2:

[0060] Any method for correcting the orifice of a large-diameter high-strength steel pipe tile assembly device, comprising the following steps:

[0061] Step 1: Determine the misalignment of the tile nozzle;

[0062] Step 2: Select the corresponding correction method according to different misalignment situations;

[0063] Step 3: Use the device to correct the misalignment of the tile pipe opening.

[0064] Embodiment 3:

[0065] like Figure 6 , 7 The misalignment in Step 2 includes two situations: arc prefabrication transition and arc prefabrication not in place;

[0066] like Figure 6 When two tiles are assembled, the B port is prefabricated too large. To eliminate the misalignment, the B end needs to be pushed outward in the diameter direction. The correction operation method of the arc prefabrication transition includes the following steps:

[0067] Step 21: Connect the outer mold 2 and the first wedge block 3 into a whole through the built-in bayonet 6;

[0068] Step 22: Assemble the outer mold 2 with the first dovetail rail 103 of the mold outer body 1 through the outer mold dovetail groove 204 to fix it on the first mounting plate 104 of the mold outer body 1;

[0069] Step 23: Assemble the inner mold 4 with the second dovetail rail 107 of the mold outer body 1 through the inner mold dovetail groove 404, and then pre-install it on the second mounting plate 106 of the mold outer body 1;

[0070] Step 24: hoist the entire device to the center of the part of the steel pipe mouth that needs to be corrected, assemble and adjust it in place, ensure that the outer mold 2 and the mold outer body 1 are locked in place, and make the outer mold 2 and the outer circumference of the A port side of the steel pipe mouth in good contact;

[0071] Step 25: Adjust the inner mold 4 so that the inner mold 4 is in good contact with the inner circumference of the B port side of the steel pipe mouth, and lock the inner mold 4 horizontally so that it is free in the vertical direction to the pipe mouth;

[0072] Step 26: Pre-tighten the inner ends of the inner mold 4 and the outer mold body 1 with the second wedge 5, and check to ensure that the inner mold 4, the outer mold 2 and the outer mold body 1 are firmly assembled;

[0073] Step 27: Use a sledgehammer to discontinuously apply force to the second wedge block 5 on the outer end face of the second wedge block 5. Under the continuous squeezing action of the second wedge block 5, the outer arc surface 402 of the inner mold and the inner arc surface 203 of the outer mold fit with the outer circumference and inner circumference of the correction part. After the second wedge block 5 is pushed into place, the B port of the steel pipe naturally fits into place with the A port, thereby achieving the purpose of pipe orifice correction.

[0074] Embodiment 4:

[0075] like Figure 7 When two tiles are aligned, the C-port prefabricated arc is not in place. To eliminate the misalignment, the C-end needs to be pushed in toward the diameter. The correction method for the prefabricated arc not in place includes the following steps:

[0076] Step 31: Connect the inner mold 4 and the second wedge block 5 into a whole through the built-in bayonet 6;

[0077] Step 32: Assemble the inner mold 4 with the second dovetail rail 107 of the mold outer body 1 through the inner mold dovetail groove 404 to fix it on the second mounting plate 106 of the mold outer body 1;

[0078] Step 33: Assemble the outer mold 2 with the first dovetail guide rail 103 of the mold outer body 1 through the outer mold dovetail groove 204, and then pre-install it on the first mounting plate 104 of the mold outer body 1;

[0079] Step 34: hoist the entire device to the center of the part of the steel pipe mouth that needs to be corrected, assemble and adjust it in place, ensure that the inner mold 4 and the mold outer body 1 are locked in place, and make the inner mold 4 and the inner circumference of the D port side of the steel pipe mouth in good contact;

[0080] Step 35: Adjust the outer mold 2 so that the outer mold 2 is in good contact with the outer circumference of the C-port side of the steel pipe mouth, and lock the outer mold 2 horizontally so that it is free in the vertical direction to the pipe mouth;

[0081] Step 36: Pre-tighten the inner ends of the outer mold 2 and the mold outer body 1 with the first wedge 3, and check to ensure that the inner mold 4, the outer mold 2 and the mold outer body 1 are firmly assembled;

[0082] Step 37: Use a sledgehammer to discontinuously apply force to the first wedge block 3 on the outer end face of the first wedge block 3. Under the continuous squeezing action of the first wedge block 3, the outer arc surface 402 of the inner mold and the inner arc surface 203 of the outer mold fit with the outer circumference and inner circumference of the correction part. After the first wedge block 3 is in place, the C port of the steel pipe naturally fits into place with the D port, thereby achieving the purpose of pipe orifice correction.

[0083] Through the above description, those skilled in the art can make various changes and modifications within the scope of the technical concept of the present invention without departing from the scope of the present invention. Matters not covered in the present invention belong to the common knowledge of those skilled in the art.

Claims

1. A method for correcting the pipe opening of a large-diameter high-strength steel pipe tile assembly, comprising a correction device, the device comprising a mold outer body (1), a rectangular through hole (102) processed in the middle portion of the mold outer body (1), a notch (105) processed at the bottom edge of the rectangular through hole (102), a first mounting plate (104) and a second mounting plate (106) formed on both sides of the notch (105), an outer mold (2) slidably mounted on the first mounting plate (104), an inner mold (4) slidably mounted on the second mounting plate (106), a first wedge block (3) provided between the outer mold (2) and the inner wall of the rectangular through hole (102), and a second wedge block (5) provided between the inner mold (4) and the outer wall of the rectangular through hole (102); The top of the mold outer body (1) is processed with a quadrangular pyramid head (101), the top of the first mounting plate (104) is processed with a first dovetail slide rail (103), and the top of the second mounting plate (106) is processed with a second dovetail slide rail (107); The outer mold (2) is processed with an outer mold inclined surface (201), and the surface opposite to the outer mold inclined surface (201) is processed with an outer mold inner arc surface (203), and the outer mold inner arc surface (203) matches the outer circumference of the steel pipe. An outer mold pin hole (202) is processed at the center position of the outer mold (2), and an outer mold dovetail groove (204) is processed on the outer mold (2), and the outer mold dovetail groove (204) forms a sliding fit with the first dovetail slide rail (103) of the mold outer body (1); The inner mold (4) is processed with an inner mold inclined surface (401), and the surface opposite to the inner mold inclined surface (401) is processed with an inner mold outer arc surface (402), the inner mold outer arc surface (402) is matched with the inner circumference of the steel pipe, an inner mold pin hole (403) is processed at the center position of the inner mold (4), and an inner mold dovetail groove (404) is processed on the inner mold (4), and the inner mold dovetail groove (404) forms a sliding fit with the second dovetail slide rail (107) of the mold outer body (1); The first wedge block (3) and the second wedge block (5) have the same structure. The first wedge block (3) includes a wedge-shaped surface (303). The wedge-shaped surface (303) forms a wedge-shaped tight fit with the outer mold inclined surface (201) of the outer mold (2) and the inner mold inclined surface (401) of the inner mold (4). A vertical surface (302) is machined on the surface opposite to the wedge-shaped surface (303). A wedge pin hole (301) is machined at the center position of the first wedge block (3). It is characterized by: The correction method comprises the following steps: Step 1: Determine the misalignment of the tile nozzle; Step 2: Select the corresponding correction method according to different dislocation situations; Step 3: Correct the misalignment of the tile nozzle through the device; The misalignment in Step 2 includes two situations: arc prefabrication transition and arc prefabrication not in place; The correction operation method of the radian prefabricated transition comprises the following steps: Step 21: Connect the outer mold (2) and the first wedge (3) into a whole through the built-in bayonet (6); Step 22: Assemble the outer mold (2) with the first dovetail slide rail (103) of the mold outer body (1) through the outer mold dovetail groove (204) so ​​that the outer mold (2) is fixed on the first mounting plate (104) of the mold outer body (1); Step 23: Assemble the inner mold (4) with the second dovetail guide rail (107) of the mold outer body (1) through the inner mold dovetail groove (404), and then pre-install it on the second mounting plate (106) of the mold outer body (1); Step 24: Hoist the entire device to the center of the portion of the steel pipe mouth that needs to be corrected, assemble and adjust it in place, ensure that the outer mold (2) and the mold outer body (1) are locked in place, and make sure that the outer mold (2) is in good contact with the outer circumference of the A port side of the steel pipe mouth; Step 25: Adjust the inner mold (4) so ​​that the inner mold (4) is in good contact with the inner circumference of the B-port side of the steel pipe nozzle, and lock the inner mold (4) horizontally so that it is free in the vertical direction to the pipe nozzle; Step 26: Pre-tighten the inner ends of the inner mold (4) and the outer mold body (1) with a second wedge (5), and check to ensure that the inner mold (4), the outer mold (2) and the outer mold body (1) are firmly assembled; Step 27: A sledgehammer is used to discontinuously apply force to the second wedge block (5) on the outer end surface of the second wedge block (5). Under the continuous squeezing action of the second wedge block (5), the outer arc surface (402) of the inner mold and the inner arc surface (203) of the outer mold are fitted with the outer circumference and inner circumference of the correction part. After the second wedge block (5) is pushed into place, the B port of the steel pipe is naturally fitted into place with the A port, thereby achieving the purpose of pipe orifice correction. The correction method for the inadequate prefabrication of the arc comprises the following steps: Step 31: Connect the inner mold (4) and the second wedge (5) into a whole through the built-in bayonet (6); Step 32: Assemble the inner mold (4) with the second dovetail guide rail (107) of the mold outer body (1) through the inner mold dovetail groove (404) so ​​that the inner mold (4) is fixed on the second mounting plate (106) of the mold outer body (1); Step 33: Assemble the outer mold (2) with the first dovetail slide rail (103) of the mold outer body (1) through the outer mold dovetail groove (204), and then pre-install it on the first mounting plate (104) of the mold outer body (1); Step 34: hoist the entire device to the center of the portion of the steel pipe orifice to be corrected, assemble and adjust it in place, ensure that the inner mold (4) and the outer mold body (1) are locked in place, and make sure that the inner mold (4) is in good contact with the inner circumference of the D-port side of the steel pipe orifice; Step 35: Adjust the outer mold (2) so that the outer mold (2) is in good contact with the outer circumference of the C-port side of the steel pipe nozzle, and lock the outer mold (2) in the horizontal direction so that it is free in the vertical direction of the pipe nozzle; Step 36: Pre-tighten the inner ends of the outer mold (2) and the mold outer body (1) with the first wedge (3), and check to ensure that the inner mold (4), the outer mold (2) and the mold outer body (1) are firmly assembled; Step 37: A sledgehammer is used to discontinuously apply force to the first wedge block (3) on the outer end surface thereof. Under the continuous squeezing action of the first wedge block (3), the outer arc surface (402) of the inner mold and the inner arc surface (203) of the outer mold are fitted with the outer circumference and the inner circumference of the correction part. After the first wedge block (3) is pushed into place, the C port of the steel pipe is naturally fitted into place with the D port, thereby achieving the purpose of pipe orifice correction.

2. The method for correcting the orifice of a large-diameter, high-strength steel pipe tile assembly according to claim 1, characterized in that: The mold outer body (1), the first wedge block (3) and the second wedge block (5) are made of forged steel material.

3. The method for correcting the orifice of a large-diameter, high-strength steel pipe tile assembly according to claim 1, characterized in that: The outer mold (2) and the inner mold (4) are made of the same material as the steel pipe, and the outer surfaces of the outer mold (2) and the inner mold (4) are treated by a quenching process.