Metallized safety film

By using a double-sided metallized thin film stacked roll structure and a cross-vertical fuse design, the problem of wasted cell area in existing capacitor grid designs is solved, achieving efficient utilization and long lifespan of the capacitor.

CN109243825BActive Publication Date: 2024-11-08DELIXI ELECTRIC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201811159858.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2018-09-30
Publication Date
2024-11-08
Estimated Expiration
2038-09-30

AI Technical Summary

Technical Problem

The existing full-area grid design of capacitors results in a large waste of cell area after breakdown, leading to significant capacitance loss and short lifespan.

Method used

It adopts a double-sided metallized thin film stacked roll structure, with the conductive grid area occupying half of the fully metallized conductive layer, and is divided into multiple square units by intersecting vertical fuses, combined with a high sheet resistance area to improve self-healing and voltage resistance.

Benefits of technology

This reduces cell area loss after breakdown, improves capacitor utilization and lifespan, and enhances safety and self-healing capabilities.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN109243825B_ABST
    Figure CN109243825B_ABST
Patent Text Reader

Abstract

The present invention relates to a metallized safety film, which is formed by stacking and winding double-sided metallized film layers, wherein the metallized film layers include a base film and a fully metallized conductive layer arranged on the base film, a margin area is arranged on one side of the base film, and a thickened area is arranged on the opposite side of the margin area of ​​the base film, the thickened area and the fully metallized conductive layer are spaced by an isolation area, and a conductive grid area is arranged on the upper side of the fully metallized conductive layer near the thickened area. Compared with the existing double-layer safety film winding, the utilization rate of the base film is increased by 2.5% while ensuring the same safety performance, and the safety performance is improved. The high square resistance fully metallized conductive layer improves self-healing performance, has high voltage resistance, strong ripple resistance, and long service life.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of capacitors, and in particular to a metallized safety film. Background Art

[0002] Chinese patent CN205264515U discloses a safe metallized film for capacitors, wherein the metal layer is arranged on the upper surface of the dielectric layer, a margin is arranged at one end of the dielectric layer, and a thickening layer is arranged at one end of the metal layer; a longitudinal insulating strip is arranged in the middle of the metal layer, and the longitudinal insulating strip divides the metal layer into a fully metallized conductive layer and a partially metallized conductive layer; one end of the transverse insulating strip is connected to the longitudinal insulating strip, and the other end extends to the boundary of the partially metallized conductive layer; the transverse insulating strip is connected to a T-shaped insulating block, and a transverse fuse is arranged between two adjacent T-shaped insulating blocks on the left and right, and a longitudinal fuse is arranged between two adjacent T-shaped insulating blocks on the upper and lower sides and the transverse insulating strip. However, this full-width grid design wastes a large unit area after the product is broken down, the capacitor capacity loss is also large, and the product life is short.

[0003] Most common metallized safety films adopt full-width hexagonal, diamond or T-shaped design structures. When a local breakdown occurs, the entire capacitor will short-circuit and discharge through the breakdown point. Strong currents will rush in from all directions, causing the fuse to blow, effectively protecting the normal operation of other parts from being affected. This is how the safety performance of the product is guaranteed. However, this full-width grid design wastes a large unit area after the product is broken down, and the capacitor capacity loss is also large. The product life will be greatly shortened compared to ordinary film capacitors. Summary of the invention

[0004] The purpose of the present invention is to provide a metallized safety film in order to solve the above problems.

[0005] The purpose of the present invention is achieved through the following technical solutions:

[0006] A metallized safety film is formed by stacking and winding double-sided metallized film layers, wherein the metallized film layers include a base film and a fully metallized conductive layer arranged on the base film, a margin area is provided on one side of the base film, and a thickened area is provided on the side opposite to the margin area of ​​the base film, the thickened area and the fully metallized conductive layer are spaced apart by an isolation area, and a conductive grid area is provided in an area on one side of the upper part of the fully metallized conductive layer close to the thickened area.

[0007] Furthermore, the conductive grid area occupies half of the fully metallized conductive layer.

[0008] Furthermore, the conductive grid area is provided with a plurality of cross-vertical fuses, and the fuses divide the conductive grid area into a plurality of square units.

[0009] Furthermore, the diameter of the fuse is 0.1-2 mm.

[0010] Furthermore, the fully metallized conductive layer is obtained by evaporating metal aluminum or zinc on the base film, and has a square resistance of 15-100Ω.

[0011] Furthermore, the sheet resistance of the evaporated conductive grid area is 7-12Ω.

[0012] Furthermore, the thickened area is obtained by evaporating metal aluminum or zinc on the base film, and the square resistance is 2-6Ω.

[0013] Furthermore, the width of the margin area is the same as that of the thickened area, and the isolation area is composed of a plurality of grooves arranged in a straight line.

[0014] Furthermore, when the double-sided metallized film layers are stacked and wound, the thickened area, conductive grid area, fully metallized conductive layer and margin area of ​​the upper metallized film layer are respectively arranged relative to the margin area, fully metallized conductive layer, conductive grid area and thickened area of ​​the lower metallized film layer.

[0015] The present invention designs the structure of the metallized film layer, and a conductive grid area is provided in a side area near the thickened area on the upper part of the fully metallized conductive layer, and the thickened area, the conductive grid area, the fully metallized conductive layer and the margin area of ​​the upper metallized film layer are arranged relative to the margin area, the fully metallized conductive layer, the conductive grid area and the thickened area of ​​the lower metallized film layer, respectively, to form a double-layer metallized safety film structure, and a structure in which half of the two layers are safety films and the other half are high square resistance films is formed in the middle. After the product is punctured, the unit area is small, and the capacitor capacity loss is small. After evaporation, the film in the high square resistance area has high withstand voltage and good self-healing performance. After evaporation, the safety film area mainly provides safety protection, can take into account safety and practicality, has strong self-healing ability, high withstand voltage, strong ripple resistance, and long service life.

[0016] Compared with the existing double-layer safety film winding, the utilization rate of the base film is increased by 2.5% while ensuring the same safety performance. Compared with the solution of single-layer metallized safety film with metallized ordinary film, the safety performance is improved. The high-square-resistance fully metallized conductive layer improves self-healing, high voltage resistance, strong ripple resistance, and long service life. The vapor-deposited conductive grid area is arranged in a grid with carefully calculated patterns. The fuses in the connecting parts between the grids are safer and have a longer service life than the hexagonal, diamond or T-shaped design structures on the market, and can meet various models and specifications. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of the structure of the metallized film layer of the present invention;

[0018] Figure 2 for Figure 1 Side view of

[0019] Figure 3 is a schematic diagram of the three-dimensional structure of the metallized film layer;

[0020] Figure 4-6 It is a schematic diagram of the assembly of the metallized safety film structure;

[0021] In the figure: 1-thickened area; 2-isolation area; 3-conductive grid area; 4-fully metallized conductive layer; 5-margin area. DETAILED DESCRIPTION

[0022] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.

[0023] Example 1

[0024] A metallized safety film, such as Figure 4-6 , which is made of double-sided metallized film layers stacked and wound, refer to Figure 1-3 The metallized film layer includes a base film and a fully metallized conductive layer 4 disposed on the base film. A margin area 5 is disposed on one side of the base film. A thickened area 1 is disposed on the opposite side of the margin area 5. The thickened area 1 and the fully metallized conductive layer 4 are separated by an isolation area 2. A conductive grid area 3 is disposed on the upper side of the fully metallized conductive layer 4 near the thickened area 1. The conductive grid area 3 occupies half of the fully metallized conductive layer 4. The conductive grid area 3 is provided with a plurality of cross-vertical fuses, which divide the conductive grid area 3 into a plurality of square units. The fully metallized conductive layer 4 is obtained by evaporating metal aluminum or zinc on the base film, and the square resistance is 15Ω / □ (i.e., Ω / mm 2 ), the square resistance of the vapor-deposited conductive grid area 3 is 7Ω, the thickened area 1 is obtained by vapor-depositing metal aluminum or zinc on the base film, and the square resistance is 2Ω, the width of the margin area 5 is the same as that of the thickened area 1, and the isolation area 2 is composed of a plurality of grooves arranged in a straight line. When the double-sided metallized film layers are stacked and wound, the thickened area 1, the conductive grid area 3, the fully metallized conductive layer 4 and the margin area 5 of the upper metallized film layer are arranged opposite to the margin area 5, the fully metallized conductive layer 4, the conductive grid area 3 and the thickened area 1 of the lower metallized film layer, respectively, forming a two-layer structure in the middle, half of which is a safety film and the other half is a high square resistance film. After the product is broken down, the unit area is small, the capacitor capacity loss is small, and safety and practicality can be taken into account. It has strong self-healing ability, high voltage resistance, strong ripple resistance, and long service life.

[0025] Example 2

[0026] In this embodiment, the square resistance of the fully metallized conductive layer 4 is 100Ω / □, the square resistance of the evaporated conductive grid area 3 is 12Ω, the thickened area 1 is obtained by evaporating metal aluminum or zinc on the base film, and the square resistance is 6Ω, and the rest is the same as in Example 1.

[0027] Example 3

[0028] In this embodiment, the square resistance of the fully metallized conductive layer 4 is 50Ω / □, the square resistance of the evaporated conductive grid area 3 is 9Ω, the thickened area 1 is obtained by evaporating metal aluminum or zinc on the base film, and the square resistance is 4Ω, and the rest is the same as in Example 1.

[0029] The above description of the embodiments is to facilitate the understanding and use of the invention by those skilled in the art. It is obvious that those skilled in the art can easily make various modifications to these embodiments and apply the general principles described herein to other embodiments without creative work. Therefore, the present invention is not limited to the above embodiments, and improvements and modifications made by those skilled in the art based on the disclosure of the present invention without departing from the scope of the present invention should be within the scope of protection of the present invention.

Claims

1. A metallized safety film, formed by stacking and winding double-sided metallized film layers, the metallized film layers comprising a base film and a fully metallized conductive layer (4) disposed on the base film, a margin region (5) being disposed on one side of the base film, and a thickened region (1) being disposed on a side opposite to the margin region (5). It is characterized in that The thickened area (1) and the fully metallized conductive layer (4) are spaced apart by an isolation area (2), and a conductive mesh area (3) is provided on one side of the upper part of the fully metallized conductive layer (4) close to the thickened area (1); When the double-sided metallized film layers are stacked and wound, the thickened area (1), the conductive grid area (3), the fully metallized conductive layer (4) and the margin area (5) of the upper metallized film layer are arranged relative to the margin area (5), the fully metallized conductive layer (4), the conductive grid area (3) and the thickened area (1) of the lower metallized film layer, respectively, to form a double-layer metallized safety film structure, forming a structure in which two layers are formed in the middle, half of which is a safety film and the other half is a high square resistance film.

2. A metallized safety film according to claim 1, It is characterized in that The conductive grid area (3) occupies half of the fully metallized conductive layer (4).

3. A metallized safety film according to claim 1, It is characterized in that The conductive grid area (3) is provided with a plurality of cross-vertical fuses, and the fuses divide the conductive grid area (3) into a plurality of square units.

4. A metallized safety film according to claim 3, It is characterized in that The diameter of the fuse is 0.1-2 mm.

5. The metallized safety film according to claim 1, It is characterized in that The fully metallized conductive layer (4) is obtained by vapor-depositing metal aluminum or zinc on the base film, and has a square resistance of 15-100Ω.

6. The metallized safety film according to claim 1, It is characterized in that The sheet resistance of the conductive grid area (3) is 7-12Ω.

7. The metallized safety film according to claim 1, It is characterized in that The thickened area (1) is obtained by evaporating metal aluminum or zinc on the base film, and has a square resistance of 2-6Ω.

8. The metallized safety film according to claim 1, It is characterized in that The width of the margin area (5) is the same as the width of the thickened area (1), and the isolation area (2) is composed of a plurality of grooves arranged in a straight line.