Alignment holder, method for manufacturing semiconductor package, testing device and method

Through the combination of the alignment holder and the force rod, the residual stress problem caused by the thermal expansion coefficient mismatch between the resin and the inserted component in the semiconductor package is solved, the bonding strength and testing accuracy of the composite structure are improved, and higher packaging is achieved. Reliability and cost efficiency.

CN110954398BActive Publication Date: 2024-10-01TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201910648937.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-04-23
Filing Date
2019-07-18
Publication Date
2024-10-01
Estimated Expiration
2040-03-23

AI Technical Summary

Technical Problem

Residual stresses caused by thermal expansion coefficient mismatches between resins and intervening components in semiconductor packages can cause delamination and other damage, affecting the bonding strength and reliability of composite structures.

Method used

Design an alignment holder, including a holder body, a support and a positioning mechanism. It is used to clamp and adjust the clamping position of the composite specimen, and apply a predetermined force through a force rod to test its bonding strength. According to the test As a result, semiconductor process parameters are modified to improve the bonding strength of the package.

Benefits of technology

By precisely controlling the clamping position and applied force, the accuracy of the test and the bonding strength of the composite specimen are improved, manual errors are reduced, product costs are reduced, and the reliability of semiconductor packaging is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110954398B_ABST
    Figure CN110954398B_ABST
Patent Text Reader

Abstract

An alignment holder, a method for manufacturing a semiconductor package, a test device and a method. An alignment holder for holding and testing a composite sample comprises: a holder body, a support member and a positioning mechanism. The holder body is configured to clamp a first side of the composite sample. The support member is detachably connected to a lower portion of the holder body to support a lower surface of the composite sample. The positioning mechanism is configured to lean against a second side of the composite sample and move relative to the holder body to adjust a clamping position of the composite sample clamped by the holder body.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to U.S. Provisional Application Serial No. 62 / 737,114 filed on September 27, 2018. The entire text of the above patent application is incorporated herein by reference and constitutes a part of this specification. Technical Field

[0003] Embodiments of the present disclosure relate to an alignment holder, and more particularly, to an alignment holder, a testing apparatus, and a method of manufacturing a semiconductor package. Background Art

[0004] Semiconductor devices are used in a variety of electronic applications, such as personal computers, cell phones, digital cameras, and other electronic equipment. Semiconductor devices are typically made by sequentially depositing insulating or dielectric layers, conductive layers, and layers of semiconductor material on a semiconductor substrate; and patterning the various material layers using photolithography to form circuit components and elements thereon. Many integrated circuits are typically manufactured on a single semiconductor wafer. The die of a wafer can be processed and packaged at the wafer level, and various techniques have been developed for wafer-level packaging.

[0005] In molded electronic and electrical components that include interposers (e.g., encapsulated semiconductor devices and resin-insulated transformers), the interface between the resin and the interposer is subject to high residual stresses due to the curing shrinkage of the resin and the mismatch in thermal expansion coefficients between the resin and the interposer. These thermal stresses sometimes cause delamination during operation and reliability testing of the components.

[0006] Such delamination at the bonding interface not only causes corrosion and electrical insulation degradation of the wire material, but also causes various other damages, such as resin cracking and wire breaking due to stress concentration caused by delamination. Therefore, evaluating the bonding strength of the composite structure is a key issue to ensure the reliability of such a composite structure. Summary of the invention

[0007] The embodiment of the present disclosure discloses an alignment holder for holding a composite specimen, comprising: a holder body, configured to clamp a first side of the composite specimen; a support member, detachably connected to a lower portion of the holder body to support a lower surface of the composite specimen; and a positioning mechanism, configured to lean against a second side of the composite specimen and move relative to the holder body to adjust a clamping position of the composite specimen clamped by the holder body.

[0008] The embodiments of the present disclosure disclose a testing device for testing the bonding strength of a composite specimen, comprising: a holder body configured to clamp a first side of the composite specimen; a positioning mechanism movably coupled to the holder body, wherein the positioning mechanism is configured to lean against a second side of the composite specimen and move relative to the holder body to adjust the clamping position of the composite specimen clamped by the holder body; and a force applying rod configured to apply force to a portion of the composite specimen exposed by the holder body.

[0009] The embodiments disclosed herein disclose a method for manufacturing a semiconductor package, comprising: performing a semiconductor process to form an encapsulated semiconductor device, wherein the encapsulated semiconductor device comprises an encapsulation material and a semiconductor device encapsulated by the encapsulation material; providing a testing device, wherein the testing device comprises a holder body, a positioning mechanism and a force-applying rod; using the holder body to clamp the encapsulated semiconductor device; using the positioning mechanism to adjust the clamping position of the encapsulated semiconductor device; removing the positioning mechanism; using the force-applying rod to apply a predetermined force to a portion of the encapsulated semiconductor device exposed by the holder body; and if the predetermined force causes the encapsulated semiconductor device to fail, modifying the process parameters of the semiconductor process to form a modified encapsulated semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] The various aspects of the present disclosure will be best understood by reading the following detailed description in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, the various features are not drawn to scale. In fact, the size of the various features may be arbitrarily increased or reduced for clarity of discussion.

[0011] Figure 1 A schematic diagram illustrating a test device according to some embodiments.

[0012] Figure 2 A partial cross-sectional view of an alignment holder is shown in accordance with some embodiments.

[0013] Figure 3 A partial cross-sectional view of an alignment holder is shown in accordance with some embodiments.

[0014] Figure 4 A schematic top view of a lower holder of an alignment holder is shown in accordance with some embodiments.

[0015] Figure 5 A schematic diagram illustrating an alignment holder in an intermediate stage of operation according to some embodiments.

[0016] Figure 6 A schematic diagram illustrating a test device in a testing phase according to some embodiments.

[0017] Figure 7 A schematic diagram illustrating a test device in a testing phase according to some embodiments.

[0018] Figure 8 A partial cross-sectional view of an alignment holder is shown in accordance with some embodiments.

[0019] Fig. 9 A schematic diagram illustrating a test device in a testing phase according to some embodiments.

[0020] Fig.10 A block diagram illustrating a method of manufacturing a semiconductor package according to some embodiments.

[0021] Fig.11 A cross-sectional view of a semiconductor package according to some embodiments is shown. DETAILED DESCRIPTION

[0022] The following disclosure provides many different embodiments or examples for implementing the different features of the provided subject matter. Specific examples of components and arrangements are set forth below to simplify the present disclosure. Of course, these are merely examples and are not intended to be limiting. For example, in the following description, forming a first feature on or on a second feature may include an embodiment in which the first feature and the second feature are formed to be in direct contact, and may also include an embodiment in which an additional feature may be formed between the first feature and the second feature so that the first feature and the second feature may not be in direct contact. In addition, the present disclosure may reuse reference numbers and / or letters in various examples. This repetition is for simplicity and clarity, and does not itself represent the relationship between the various embodiments and / or configurations discussed.

[0023] Additionally, for ease of description, spatially relative terms such as "beneath," "below," "lower," "above," "upper," etc. may be used herein to describe the relationship of one element or feature to another (other) element or feature as shown in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein should be interpreted accordingly.

[0024] The present disclosure may also include other features and processes. For example, a test structure may be included to help perform verification testing on a three-dimensional (3D) package or a three-dimensional integrated circuit (3DIC) device. The test structure may include, for example, a test pad formed in a redistribution layer or on a substrate to enable testing of the three-dimensional package or the three-dimensional integrated circuit, use of a probe and / or a probe card, etc. Verification testing may be performed on intermediate structures as well as final structures. In addition, the structures and methods disclosed herein may be used in conjunction with a test method including intermediate verification of a known good die to improve yield and reduce cost.

[0025] Figure 1 A schematic diagram illustrating a test device according to some embodiments. Figure 2 A partial cross-sectional view of an alignment retainer according to some embodiments is shown. Figure 1 and Figure 2 , Figure 1 The test apparatus 100 shown in is configured to test the bonding strength of the composite coupon 10. In some embodiments, the composite coupon 10 may be a composite structure including a plurality of components bonded together, and the test apparatus 100 is configured to test / measure the bonding strength between the components around the interface of the composite coupon 10. In some embodiments, the composite coupon 10 may be a semiconductor package including a plurality of components (e.g., encapsulation materials, perforations, semiconductor devices, etc.) bonded to each other, so that the composite coupon 10 includes a plurality of bonding interfaces. The materials of the plurality of components may be different from each other. For example, the composite coupon 10 may include an Integrated Fan Out (InFO) package, a Chip on Wafer on Substrate (CoWoS) package, a flip chip package, and other semiconductor packages.

[0026] In some embodiments, for example, the composite sample 10 may be an encapsulated semiconductor device, the encapsulated semiconductor device comprising a semiconductor device 11 encapsulated by an encapsulation material 12 and a plurality of through holes (conductive pillars) 13 surrounding the semiconductor device 11 and extending through the encapsulation material 12, such as Figure 1 and Figure 2 . The encapsulating material 12 exposes the electrical terminals of the semiconductor device 11 and the end surfaces of the through-holes 13. In the embodiment where the composite coupon 10 is an encapsulated semiconductor device, the composite coupon 10 may be in the form of a wafer. In some embodiments, a testing apparatus 100 is provided to test / measure the bonding strength (i.e., delamination durability) of the composite coupon (encapsulated semiconductor device) 10 at its bonding interface (e.g., the bonding interface between the encapsulating material 12 and the through-hole 13, the bonding interface between the encapsulating material 12 and the semiconductor device 11, etc.).

[0027] In some embodiments, the materials of the components in the composite sample 10 may be different from each other. For example, the material of the encapsulation material 12 may include epoxy resin or other suitable resins. In some embodiments, the encapsulation material 12 may be an epoxy resin containing chemical fillers. The material of the substrate of the semiconductor device 11 may include bulk silicon (doped or undoped) or an active layer including a silicon-on-insulator (SOI) substrate. In general, the SOI substrate includes a semiconductor material (e.g., silicon, germanium, silicon germanium, SOI, silicon germanium on insulator (SGOI) or a combination thereof) layer. Other substrates that can be used include multi-layered substrates, gradient substrates, or mixed orientation substrates. The material of the through-hole 13 may include (Cu) and / or copper alloys, etc. In some embodiments, the materials of some components in the composite sample 10 may be the same, and the test equipment 100 is also configured to test the bonding strength between components having the same material.

[0028] In some embodiments, the test apparatus 100 includes an alignment holder 105 for holding a composite specimen 10 and a force application rod 140 for applying a force to the composite specimen 10. In some embodiments, the alignment holder 105 includes a holder body 110 and a positioning mechanism 130. The holder body 110 is configured to clamp a first side (e.g., right side) of the composite specimen 10. In one embodiment, the holder body 110 may include an upper holder 112 and a lower holder 114, and the first side of the composite specimen 10 is configured to be disposed between the upper holder 112 and the lower holder 114. In some embodiments, the holder body 110 may also include a locking member 118. The locking member 118 is coupled between the upper holder 112 and the lower holder 114, and the distance G1 between the upper holder 112 and the lower holder 114 can be adjusted by the locking member 118. For example, the locking member 118 may be a screw. The upper holder 112 and the lower holder 114 each have a corresponding threaded hole, so that the distance G1 between the upper holder 112 and the lower holder 114 can be adjusted according to the depth of the locking member 118 screwed into the threaded hole of the upper holder 112 and the threaded hole of the lower holder 114.

[0029] Figure 3 A partial cross-sectional view of an alignment holder is shown in accordance with some embodiments. Figure 4 A schematic top view of a lower holder of an alignment holder according to some embodiments is shown. Figure 3 and Figure 4 In some embodiments, the holder body 110 may further include a groove 1141 for accommodating the composite specimen 10. According to some embodiments of the present disclosure, Figure 3 and Figure 4 As shown in , the groove 1141 spans the lower holder 114 so that the composite specimen 10 is configured to move along the movement direction D1 within the groove 1141. In other words, the groove 1141 can be used as a sliding guide to slide the composite specimen 10 along the groove 1141 relative to the holder body. With this arrangement, when the composite specimen 10 is clamped, the upper holder 112 and the lower holder 114 can contact each other. In other embodiments, the groove 1141 can be set on the upper holder 112 and / or the lower holder 114 to serve as a sliding guide for the composite specimen 10. The depth of the groove 1141 can be adjusted according to actual requirements (for example, the thickness of the composite specimen 10, the configuration of the holder body 110, etc.).

[0030] Figure 5 A schematic diagram showing an alignment holder in an intermediate stage of operation according to some embodiments. Figure 1 and Figure 5In some embodiments, the alignment holder 105 may further include a support 120, which is detachably connected to the lower portion of the holder body 110 to support the lower surface of the composite specimen 10. In some embodiments, the support 120 may be detachably connected to the lower holder 114. According to some embodiments of the present disclosure, the support 120 is detachably connected to the lower holder 114 by mechanical engagement. For example, the support 120 may include at least one protrusion (e.g., the protrusion 122 shown in FIG. 5 ), and the lower holder 114 may correspondingly include at least one concave (e.g., Figure 5 142 shown in the figure). With this arrangement, the support member 120 can be detachably connected to the lower holder 114 by the engagement of the protrusion 122 of the support member 120 with the recess 1142 of the lower holder 114, but the present disclosure is not limited to this. Any form of mechanical engagement or any suitable connection can be applied to the support member 120 and the lower holder 114. In an alternative embodiment, the support member 120 can be detachably connected to the lower holder 114 by magnetic force. For example, the support member 120 and the lower holder 114 can each include a magnetic component, and the magnetic components in the support member 120 and the lower holder 114 are configured to attract each other.

[0031] In some embodiments, the support 120 may be first attached (connected) to the lower holder 114 when the composite specimen 10 is placed between the upper holder 112 and the lower holder 114, so that the lower surface of the composite specimen 10 may lean against the support 120 to hold and support the composite specimen 10 in an appropriate position. Then, when the composite specimen 10 is adjusted to a desired clamping position, the distance G1 between the upper holder 112 and the lower holder 114 may be adjusted (shortened) by, for example, screwing the locking member 118 into the threaded hole of the upper holder 112 and the threaded hole of the lower holder 114. That is, the locking member 118 may be used to control the tightness of the holder body 110 clamping the composite specimen 10, thereby holding the composite specimen 10 in an appropriate position.

[0032] Now refer to Figure 1In some embodiments, the positioning mechanism 130 is configured to lean against the second side (e.g., the left side) of the composite specimen 10 and move relative to the holder body 110 to adjust the clamping position of the composite specimen 10 clamped by the holder body 110. In some embodiments, the holder body 110 may further include a base 116. The upper holder 112 and the lower holder 114 are disposed on the base 116, and the positioning mechanism 130 is movably coupled to the base 116. According to some embodiments of the present disclosure, the positioning mechanism 130 includes at least one positioning rod 132 (two positioning rods 132 are shown herein, but not limited thereto) and a positioning plate 134 coupled to the positioning rod 132. Accordingly, the base 116 includes at least one positioning hole 1161 (two positioning holes 1161 are shown herein, but not limited thereto), and the positioning rods 132 are movably engaged with the positioning holes 1161, respectively. The positioning plate 134 is configured to lean against the second side (e.g., the left side) of the composite specimen 10 and move along the positioning rod 132. For example, the positioning hole 1161 may be a threaded hole, and the positioning rod 132 may be a threaded rod. Thus, one end of the positioning rod 132 may penetrate the positioning plate 134, and the other end of the positioning rod 132 may be screwed into the positioning hole 1161, so that the positioning rod 132 is configured to drive the positioning plate 134 to move toward or away from the holder body 110. In some embodiments, a protrusion 136 may be provided on the cantilever end of each positioning rod 132 to facilitate the operation of the positioning rod 132.

[0033] Now refer to Figure 2 According to some embodiments of the present disclosure, the length L1 of the support member 120 is substantially shorter than the length L2 of the composite specimen 10 exposed by the upper holder 112 and the lower holder 114 of the holder body 110. Therefore, the positioning mechanism 130 is able to push the second side of the composite specimen 10 toward the holder body 110 without interfering with the support member 120. In some embodiments, the positioning mechanism 130 is configured to lean against the second side of the composite specimen 10, which is opposite to the first side of the composite specimen 10 clamped by the upper holder 112 and the lower holder 114.

[0034] Figure 6 A schematic diagram of a test device in a test phase according to some embodiments is shown. Figure 1 and Figure 6With this arrangement, when the user wants to adjust the clamping position of the composite specimen 10, the user can simply rotate the protrusion 136 along the rotation direction R1 to screw the positioning rod 132 into the positioning hole 1161. Therefore, the positioning plate 134 is driven to move together with the positioning rod 132 and push the composite specimen 10 toward the holder body 110. When the composite specimen 10 moves to the desired clamping position, the user only needs to simply stop the rotation of the protrusion 136 and further screw the locking member 118 into the upper holder 112 and the lower holder 114 to lock the composite specimen 10 in place. Then, the positioning mechanism 130 can be removed by rotating the protrusion 136 in the opposite direction to screw the positioning rod 132 out of the positioning hole 1161. The support member 120 can also be removed by, for example, disengaging the support member 120 from the lower holder 114. Then, the application rod 140 can be used to apply force to a portion of the composite specimen 10 to test the bonding strength of the composite specimen 10. In some embodiments, the force-applying rod 140 may be a cantilever beam. In some embodiments, the cantilever end of the force-applying rod 140 is configured to abut against the upper surface of the composite specimen 10 to apply force on the upper surface of the composite specimen 10. Therefore, the positioning and alignment of the composite specimen 10 can be well controlled using the upper holder 112, the lower holder 114, and the positioning mechanism 130, and manual errors and erroneous test results caused by the offset or misalignment of the composite specimen 10 can be avoided.

[0035] Now refer to Figure 2 According to some embodiments of the present disclosure, the upper holder 112 includes an inclined surface 1121 at the end of the upper holder 112 to align with the first side of the composite specimen 10. In some embodiments, the upper holder 112 may be a wedge. With this arrangement, the user's viewing angle is not blocked by the upper edge of the upper holder 112, so the user can better observe the composite specimen 10 during the adjustment of the clamping position of the composite specimen 10.

[0036] According to some embodiments of the present disclosure, a force-applying rod 140 may be used to apply force to an interface between two components of the composite specimen 10. In some embodiments, the force-applying rod 140 is configured to move toward the composite specimen 10 in a direction perpendicular to a surface (e.g., an upper surface) of the composite specimen 10. For example, a force may be applied on the upper surface at an interface between the encapsulation material 12 and the semiconductor device 11 or at an interface between the encapsulation material 12 and the through-hole 13. Thus, the bonding strength between the encapsulation material 12 and the semiconductor device 11 and the bonding strength between the encapsulation material 12 and the through-hole 13 may be tested / measured. Thus, the bonding strength (delamination durability) may be determined by measuring the applied force at the interface during an increase in delamination growth. By applying the alignment holder 105, the clamping position may be well controlled to expose the interface to be tested without offset, so that force may be accurately applied to the interface of the composite specimen 10. For example, the composite specimen 10 is first held by the holder body 110, and then pushed toward the holder body 110 by the positioning mechanism 130 to more accurately adjust the clamping position, thereby avoiding or reducing the misalignment (positional deviation) of the composite specimen 10 caused by manually placing the composite specimen 10. Thus, the accuracy of the test result of the testing apparatus 100 can be improved.

[0037] According to some embodiments of the present disclosure, to perform a bending test, the force-applying rod 140 moves in a direction from the upper holder 112 toward the lower holder 114 to apply a bending force to the composite specimen 10. In some embodiments, the longitudinal axis A1 of the force-applying rod 140 is substantially perpendicular to the application surface (e.g., the upper surface) of the composite specimen 10, and the bending force is applied by the end of the force-applying rod 140, such as Figure 6 as shown in .

[0038] Figure 7 A schematic diagram of a test device in a test phase according to some embodiments is shown. Figure 7 According to some embodiments of the present disclosure, in order to perform a shear test, after removing the positioning mechanism 130 and the support member 120, the holder body 110 can be placed in an upright position, such as Figure 7 As shown in . Thus, the composite specimen 10 clamped by the holder body 110 is also in an upright position. Therefore, the longitudinal axis A1 of the force-applying rod 140 is substantially parallel to the application surface (e.g., the lower surface) of the composite specimen 10, and the shear stress is applied by the side surface of the force-applying rod 140, as shown in Figure 7As shown in . In an embodiment of performing a shear test, the force applying rod 140 moves in a direction from the lower holder 114 toward the upper holder 112 to apply a shear stress to the composite specimen 10. Therefore, the alignment holder 105 provides the test apparatus 100 with a more precise alignment and greater test operation flexibility. With this arrangement, the alignment holder 105 and the test apparatus 100 having the alignment holder 105 can perform a bending test, a shear test, a scratch test, a dent test, or any other suitable test including alignment and force application. Therefore, the application of the test apparatus 100 having the alignment holder 105 is more extensive, and the alignment of the composite specimen 10 and the test results can be more accurate.

[0039] According to some embodiments of the present disclosure, the composite sample 10' may be an encapsulated semiconductor device, which includes a first semiconductor device 11, a second semiconductor device 14, a first encapsulation material 12a, and a second encapsulation material 12b. In some embodiments, the first semiconductor device 11 is encapsulated by the first encapsulation material 12a, and the second semiconductor device 14 is encapsulated by the second encapsulation material 12b. The first encapsulation material 12a and the second encapsulation material 12b are combined with each other. In some embodiments, the structure of the first semiconductor device 11 encapsulated by the first encapsulation material 12a and the structure of the second semiconductor device 14 encapsulated by the second encapsulation material 12b can be formed in different steps.

[0040] For example, a structure of a first semiconductor device 11 encapsulated by a first encapsulating material 12a may be preformed and provided, and then a second encapsulating material 12b may be formed to encapsulate a second semiconductor device 14 and the second encapsulating material 12b may be combined with the first encapsulating material 12a. In some embodiments, the first encapsulating material 12a and the second encapsulating material 12b may be over molded to cover the first semiconductor device 11 and the second semiconductor device 14. Then, a planarization process may be performed on the first encapsulating material 12a and the second encapsulating material 12b to expose the first semiconductor device 11 and the second semiconductor device 14. For example, the planarization process may include mechanical grinding or chemical mechanical polishing (CMP). After the grinding process, a cleaning step may be performed as needed, for example, to clean and remove residues generated by the grinding step. However, the present disclosure is not limited thereto, and the planarization step may be performed by any other suitable method.

[0041] With this arrangement, force can be applied to the interface between the first semiconductor device 11 and the first encapsulation material 12a, the interface between the second semiconductor device 14 and the second encapsulation material 12b, and the interface between the first encapsulation material 12a and the second encapsulation material 12b to test their bonding strength. In some embodiments, the materials of the first encapsulation material 12a and the second encapsulation material 12b may be the same. For example, the materials of the first encapsulation material 12a and the second encapsulation material 12b may include epoxy resin or other suitable resins. In some embodiments, the first encapsulation material 12a and the second encapsulation material 12b may be epoxy resin containing chemical fillers. In alternative embodiments, the materials of the first encapsulation material 12a and the second encapsulation material 12b may be different from each other. The first semiconductor device 11 and / or the second semiconductor device 14 may be a high bandwidth memory (HBM) die or any other suitable semiconductor device. In some embodiments, at least one of the first semiconductor device 11 and the second semiconductor device 14 may be a dummy die used only for testing purposes to further reduce testing costs.

[0042] According to some embodiments of the present disclosure, to perform a bending test, the force-applying rod 140 may be moved in a direction from the upper holder 112 toward the lower holder 114 to apply a bending force to the composite specimen 10. In some embodiments, the longitudinal axis of the force-applying rod 140 is substantially perpendicular to the application surface (e.g., the upper surface) of the composite specimen 10', and the bending force is applied by the end of the force-applying rod 140, such as Figure 8 as shown in .

[0043] Fig. 9 A schematic diagram of a test device in a test phase according to some embodiments is shown. Fig. 9 According to some embodiments of the present disclosure, to perform a shear test, after removing the positioning mechanism 130 and the support member 120, the holder body 110 may be placed in an upright position, such as Fig. 9 As shown in . Thus, the composite specimen 10' clamped by the holder body 110 is also in an upright position. Therefore, the longitudinal axis of the force-applying rod 140 is substantially parallel to the force-applying surface (e.g., the lower surface) of the composite specimen 10', and the shear stress is applied by the side surface of the force-applying rod 140, as shown in FIG. Fig. 9 In the embodiment of performing the shear test, the force applying rod 140 moves in the direction from the lower holder 114 to the upper holder 112 to apply the shear stress to the composite specimen 10'. Generally speaking, when the composite specimen 10' is subjected to high residual stress due to, for example, the curing shrinkage of the encapsulating materials 12a and 12b, the composite specimen 10' including the first encapsulating material 12a and the second encapsulating material 12b bonded to each other is prone to cracking at the lower surface of the composite specimen 10'. Therefore, as Fig. 9The shear test shown in FIG. 1 is unavoidable for the composite specimen 10 ′.

[0044] According to some embodiments of the present disclosure, the alignment holder 105 provides more precise alignment and greater test operation flexibility for the test device 100. With this arrangement, the alignment holder 105 and the test device 100 having the alignment holder 105 can perform bending tests, shear tests, scratch tests, dent tests, or any other suitable tests including alignment and force application.

[0045] Now refer to Figure 1 , Fig.10 and Fig.11 According to some embodiments of the present disclosure, Fig.11 The method for manufacturing a semiconductor package 50 shown in FIG. 5 may include the following steps. It should be noted that the following description is based on an embodiment of the method being applied to Figure 1 The composite sample (encapsulated semiconductor device) 10 is shown, but the present disclosure is not limited thereto. It should be understood that the method and testing apparatus 100 can also be applied to any suitable sample.

[0046] First, step S110 is performed to provide an encapsulated semiconductor device 10, wherein the encapsulated semiconductor device 10 includes an encapsulation material 12 and a semiconductor device 11 encapsulated by the encapsulation material 12. In some embodiments, the encapsulated semiconductor device 10 is formed by a semiconductor process. Such a semiconductor process may include: providing a semiconductor device 11 and a plurality of through-holes (conductive pillars) 13, and then providing an encapsulation material 12 to encapsulate the semiconductor device 11 and the conductive pillars 13. In some embodiments, the semiconductor device 11 and the through-holes (conductive pillars) 13 may be provided on a carrier (not shown), and the carrier may be removed during a subsequent test process. In some embodiments, the carrier may be a glass carrier, a ceramic carrier, etc. The conductive pillars 13 may be pre-formed, and then the conductive pillars 13 may be placed on the carrier. In alternative embodiments, the conductive pillars 13 may be formed by, for example, a plating process. The plating of the conductive pillars 13 may be performed before the placement of the semiconductor device 11. In some embodiments, the encapsulation material 12 may include a molding compound, an epoxy resin, or a resin, etc. In some embodiments, a thinning process (which may be a grinding process) may be performed as needed to thin the encapsulation material 12 so as to expose the through-holes 13 and electrical terminals of the semiconductor device 11 .

[0047] Next, step S120 is performed to provide Figure 1The test apparatus 100 shown in FIG. 1 includes a holder body 110, a positioning mechanism 130, and a force-applying rod 140. The test apparatus 100 is provided to test / measure the bonding strength (i.e., delamination durability) of the encapsulated semiconductor device 10 at its bonding interface (e.g., the bonding interface between the encapsulation material 12 and the through-hole 13, the bonding interface between the encapsulation material 12 and the semiconductor device 11, etc.).

[0048] Next, step S130 is performed to clamp the first side of the encapsulated semiconductor device (composite sample) 10 using the holder body 110. In some embodiments, the first side (e.g., the right side) of the encapsulated semiconductor device 10 is placed between the upper holder 112 and the lower holder 114 of the holder body 110. Figure 1 In the embodiment of the test apparatus 100 shown with the support 120, the support 120 may first be attached (connected) to the lower holder 114 before placing the encapsulated semiconductor device 10 between the upper holder 112 and the lower holder 114. Thus, the lower surface of the encapsulated semiconductor device 10 may rest on the support 120 to hold and support the encapsulated semiconductor device 10 in place. In some embodiments, the support 120 may be detachably connected to the lower holder 114 by mechanical engagement, magnetic force, or any suitable means.

[0049] Next, step S140 is performed to adjust the clamping position of the packaged semiconductor device 10 using the positioning mechanism 130. For example, in some embodiments, the second side of the packaged semiconductor device 10 is pushed toward the holder body 110 using the positioning mechanism 130 to adjust the clamping position of the packaged semiconductor device 10. In some embodiments, the positioning mechanism 130 rests on a second side (e.g., the left side) of the packaged semiconductor device 10 opposite to the first side clamped by the holder body 110, and is configured to push the second side of the packaged semiconductor device 10 toward the holder body 110 in a controllable manner. When the packaged semiconductor device 10 is pushed and adjusted to the desired clamping position, the upper holder 112 and the lower holder 114 can be locked by, for example, screwing the locking member 118 into the threaded hole of the upper holder 112 and the threaded hole of the lower holder 114. That is, the locking member 118 can be used to control the tightness of the holder body 110 clamping the encapsulated semiconductor device 10, thereby holding the encapsulated semiconductor device 10 in a proper position. In other embodiments, the upper holder 112 and the lower holder 114 can be connected by an elastic piece, thereby holding the encapsulated semiconductor device 10 in a proper position.

[0050] Then, step S150 is performed to remove the positioning mechanism 130. In some embodiments, the positioning mechanism 130 can be removed from the holder body by, for example, unscrewing the positioning rod 132 of the positioning mechanism 130 from the positioning hole 1161 of the holder body. In an embodiment of the test device 100 having the support member 120, the support member 120 can also be removed by, for example, disengaging the support member 120 from the lower holder 114.

[0051] Next, step S160 is performed, and a predetermined force may be applied to a portion of the encapsulated semiconductor device 10 using the force-applying rod 140 to test the bonding strength of the encapsulated semiconductor device 10. In some embodiments, the force-applying rod 140 may be used to apply force to the interface between two bonding components of the encapsulated semiconductor device 10. For example, a predetermined force may be applied at the interface between the encapsulation material 12 and the semiconductor device 11 or at the interface between the encapsulation material 12 and the through-hole 13. Therefore, the bonding strength between the encapsulation material 12 and the semiconductor device 11 and the bonding strength between the encapsulation material 12 and the through-hole 13 may be tested and measured. By applying the alignment holder 105, the alignment holder 105 may be well controlled to hold the encapsulated semiconductor device 10 and expose the interface to be tested, so that force may be accurately applied to the interface of the encapsulated semiconductor device 10 without displacement. Therefore, the positioning and alignment of the packaged semiconductor device 10 can be well controlled using the upper holder 112 , the lower holder 114 , and the positioning mechanism 130 , and manual errors and erroneous test results due to the shift or misalignment of the packaged semiconductor device 10 can be avoided.

[0052] Next, step S170 is performed. If the predetermined force applied by the force-applying rod 140 causes the encapsulated semiconductor device 10 to fail, the process parameters of the semiconductor process are modified to form a modified encapsulated semiconductor device 10a. In some embodiments, if the bonding strength between the interfaces of the encapsulated semiconductor device 10 does not meet the requirements, when the force-applying rod 140 applies the predetermined force to the encapsulated semiconductor device 10, the encapsulated semiconductor device 10 may fail around the interface (e.g., crack, deform, etc.). Thus, the process parameters of the semiconductor process for forming the encapsulated semiconductor device 10 may be modified to form a modified encapsulated semiconductor device 10a. For example, the process parameters may include the curing temperature of the encapsulation material 12, the reactant concentration of the plating process for forming the conductive pillars 13 and / or conductors of the semiconductor device 11, etc. The test process may be repeated until the bonding strength of the modified encapsulated semiconductor device meets the requirements, and then a subsequent process (e.g., forming a redistribution structure 20 on the modified encapsulated semiconductor device 10a, etc.) may be performed on the modified encapsulated semiconductor device 10a to form a semiconductor package 50. Of course, if the bonding strength of the encapsulated semiconductor device 10 originally meets the requirements, a subsequent process (e.g., forming a redistribution structure 20 on the encapsulated semiconductor device 10, etc.) may be performed on the encapsulated semiconductor device 10 to form a semiconductor package 50 without modifying any process parameters.

[0053] In some embodiments, for the subsequent process, a rewiring structure 20 may be formed on the encapsulation material 12 and the semiconductor device 11, and the rewiring structure 20 is electrically connected to the semiconductor device 11 and the through-hole 13 of the encapsulated semiconductor device 10 / 10a. The rewiring structure 20 may be formed by, for example, depositing a conductive layer, patterning the conductive layer to form a rewiring line 21, using a dielectric layer 22 to partially cover the rewiring line 21, and filling the gaps between the rewiring lines 21. The material of the rewiring line 21 may include a metal or a metal alloy including aluminum, copper, tungsten and / or an alloy thereof. The dielectric layer 22 may be formed of a dielectric material (e.g., oxide, nitride, carbide, carbon nitride, a combination thereof and / or a multilayer thereof). The rewiring line 21 is formed in the dielectric layer 22 and is electrically connected to the semiconductor device 11 and the through-hole 13. In addition, an Under Bump Metallurgy (UBM) layer 23 may be formed on the rewiring structure 20 by sputtering, evaporation or electroless plating.

[0054] Next, according to some exemplary embodiments, a plurality of electrical connectors 30 and at least one integrated passive device (IPD) 32 are disposed on the rewiring structure 20. The formation of the electrical connectors 30 may include placing solder balls on the UBM layer 23 (or on the rewiring structure 20), and then reflowing the solder balls. In alternative embodiments, the formation of the electrical connectors 30 may include performing a plating process to form solder areas on the UBM layer 23 (or on the rewiring structure 20), and then reflowing the solder areas. The electrical connectors 30 may also include conductive pillars or conductive pillars with solder caps, which may also be formed by plating. The IPD 32 may be fabricated using standard wafer fabrication techniques (e.g., thin film and photolithography processing), and may be mounted on the rewiring structure 20 by, for example, flip chip bonding or wire bonding.

[0055] According to some embodiments of the present disclosure, once the encapsulation material 12 is formed (i.e., the molding process), a method and a testing device for testing the bonding strength of the encapsulated semiconductor device 10 can be applied. In other words, once the molding process is performed, the delamination durability of the encapsulated semiconductor device 10 can be obtained without waiting for the entire semiconductor packaging process to be completed. That is, the testing method and the testing device can be applied to the encapsulated semiconductor device 10, but not to the semiconductor package that may include the encapsulated semiconductor device and the rewiring structure. Thus, the delamination durability of the encapsulated semiconductor device 10 can be obtained more immediately, so that the recipe of the encapsulated semiconductor device 10 can be modified immediately to prevent the risk of delamination without waiting for the entire semiconductor packaging process to be completed. Therefore, the product cost can be reduced and the process efficiency can be improved.

[0056] Based on the above discussion, it can be seen that the present disclosure provides various advantages. However, it should be understood that not all advantages must be discussed herein, and other embodiments may provide different advantages, and not all embodiments require specific advantages.

[0057] According to some embodiments of the present disclosure, an alignment holder for holding a composite specimen comprises a holder body, a support member, and a positioning mechanism. The holder body is configured to clamp a first side of the composite specimen. The support member is detachably connected to a lower portion of the holder body to support a lower surface of the composite specimen. The positioning mechanism is configured to lean against a second side of the composite specimen and move relative to the holder body to adjust a clamping position of the composite specimen clamped by the holder body.

[0058] According to some embodiments of the present disclosure, a test device for testing the bonding strength of a composite specimen includes a holder body, a positioning mechanism, and a force-applying rod. The holder body is configured to clamp a first side of the composite specimen. The positioning mechanism is movably coupled to the holder body, wherein the positioning mechanism is configured to lean against a second side of the composite specimen and move relative to the holder body to adjust the clamping position of the composite specimen clamped by the holder body. The force-applying rod is configured to apply force to a portion of the composite specimen exposed by the holder body.

[0059] According to some embodiments of the present disclosure, a method for manufacturing a semiconductor package includes the following steps. Perform a semiconductor process to form an encapsulated semiconductor device, wherein the encapsulated semiconductor device includes an encapsulation material and a semiconductor device encapsulated by the encapsulation material. Provide a test device, which includes a holder body, a positioning mechanism, and a force-applying rod. Use the holder body to clamp the encapsulated semiconductor device. Use the positioning mechanism to adjust the clamping position of the encapsulated semiconductor device. Remove the positioning mechanism. Use the force-applying rod to apply a predetermined force to a portion of the encapsulated semiconductor device exposed by the holder body. If the predetermined force causes the encapsulated semiconductor device to fail, modify the process parameters of the semiconductor process to form a modified encapsulated semiconductor device.

[0060] According to aspects of the present disclosure, an alignment holder for holding a composite specimen is provided, comprising: a holder body configured to clamp a first side of the composite specimen; a support member detachably connected to a lower portion of the holder body to support a lower surface of the composite specimen; and a positioning mechanism configured to lean against a second side of the composite specimen and move relative to the holder body to adjust a clamping position of the composite specimen clamped by the holder body. The holder body comprises an upper holder and a lower holder, and the first side of the composite specimen is configured to be disposed between the upper holder and the lower holder. The holder body further comprises a locking member coupled between the upper holder and the lower holder, and a distance between the upper holder and the lower holder is adjusted by the locking member. The upper holder comprises an inclined surface at a distal end of the upper holder to align with the first side of the composite specimen. The holder body further comprises a base, and the positioning mechanism is movably coupled to the base. The base includes at least one positioning hole, and the positioning mechanism includes: at least one positioning rod movably engaged with the positioning hole; and a positioning plate configured to lean against the second side of the composite sample and move together with the positioning rod. The length of the support member is substantially shorter than the length of the composite sample exposed by the holder body. The holder body includes a groove for accommodating the composite sample, and the composite sample is configured to move along the groove.

[0061] According to another aspect of the present disclosure, a testing device for testing the bonding strength of a composite specimen is provided, comprising: a holder body configured to clamp a first side of the composite specimen; a positioning mechanism movably coupled to the holder body, wherein the positioning mechanism is configured to lean against a second side of the composite specimen and move relative to the holder body to adjust the clamping position of the composite specimen clamped by the holder body; and a force-applying rod configured to apply force to a portion of the composite specimen exposed by the holder body. The holder body comprises an upper holder and a lower holder, and the first side of the composite specimen is configured to be disposed between the upper holder and the lower holder. The holder body further comprises a locking member coupled between the upper holder and the lower holder, and the distance between the upper holder and the lower holder is adjusted by the locking member. The testing device further comprises a support member, which is detachably connected to the lower holder to support the lower surface of the composite specimen. The upper holder includes an inclined surface at the end of the upper holder to align with the first side of the composite specimen. The holder body also includes a base, and the positioning mechanism is movably coupled to the base. The base includes at least one positioning hole, and the positioning mechanism includes: at least one positioning rod that is movably engaged with the positioning hole; and a positioning plate that is configured to lean against the second side of the composite specimen and move with the positioning rod. The holder body includes a groove for accommodating the composite specimen, and the composite specimen is configured to move along the groove. The force rod is configured to move toward the composite specimen in a direction perpendicular to the surface of the composite specimen.

[0062] According to another aspect of the present disclosure, a method for manufacturing a semiconductor package is provided, comprising: performing a semiconductor process to form an encapsulated semiconductor device, wherein the encapsulated semiconductor device comprises an encapsulation material and a semiconductor device encapsulated by the encapsulation material; providing a test device, wherein the test device comprises a holder body, a positioning mechanism and a force-applying rod; using the holder body to clamp the encapsulated semiconductor device; using the positioning mechanism to adjust the clamping position of the encapsulated semiconductor device; removing the positioning mechanism; using the force-applying rod to apply a predetermined force to a portion of the encapsulated semiconductor device exposed by the holder body; and if the predetermined force causes the encapsulated semiconductor device to fail, modifying the process parameters of the semiconductor process to form a modified encapsulated semiconductor device. The method for manufacturing a semiconductor package further comprises: providing a support member on a lower portion of the holder body, wherein the encapsulated semiconductor device rests on the support member when being clamped by the holder body; and removing the support member before applying the force to the portion of the encapsulated semiconductor device exposed by the holder body. The method for manufacturing a semiconductor package further includes: forming a redistribution structure on the modified encapsulated semiconductor device.

[0063] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the present disclosure. Those skilled in the art will appreciate that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to implement the same purposes and / or achieve the same advantages as the embodiments described herein. Those skilled in the art will also recognize that these equivalent constructions do not depart from the spirit and scope of the present disclosure, and that they can make various changes, substitutions, and modifications herein without departing from the spirit and scope of the present disclosure.

Claims

1. An alignment holder for holding a composite sample, characterized in that: include: a holder body configured to clamp a first end of the composite specimen; a support member detachably connected to a lower portion of the holder body to support a lower surface of the composite specimen; as well as A positioning mechanism is configured to lean against a second end of the composite specimen relative to the first end and move relative to the holder body to adjust a clamping position of the composite specimen clamped by the holder body, wherein the holder body includes an upper holder and a lower holder, and the first end of the composite specimen is configured to be disposed between the upper holder and the lower holder. 2 . The alignment holder according to claim 1 , wherein the holder body further comprises a locking member coupled between the upper holder and the lower holder, and a distance between the upper holder and the lower holder is adjusted by the locking member. 3 . The alignment holder of claim 1 , wherein the upper holder includes an inclined surface at a distal end of the upper holder to align with the first end of the composite specimen. 4 . The alignment holder of claim 1 , wherein the holder body further comprises a base, and the positioning mechanism is movably coupled to the base.

5. The alignment holder according to claim 4, wherein the base comprises at least one positioning hole, and the positioning mechanism comprises: at least one positioning rod, movably engaged with the positioning hole; and a positioning plate configured to rest on the second end of the composite specimen and move together with the positioning rod. 6 . The alignment holder of claim 1 , wherein a length of the support member is substantially shorter than a length of the composite specimen exposed by the holder body. 7 . The alignment holder of claim 1 , wherein the holder body comprises a groove for accommodating the composite specimen, and the composite specimen is configured to move along the groove.

8. A testing device for testing the bonding strength of a composite specimen, characterized in that: include: a holder body configured to clamp a first end of the composite specimen; a positioning mechanism movably coupled to the holder body, wherein the positioning mechanism is configured to lean against a second end of the composite specimen relative to the first end and to move relative to the holder body to adjust a clamping position of the composite specimen clamped by the holder body; as well as The force-applying rod is configured to apply force to a portion of the composite sample exposed by the holder body, wherein the holder body includes an upper holder and a lower holder, and the first end of the composite sample is configured to be disposed between the upper holder and the lower holder. 9 . The testing apparatus according to claim 8 , wherein the holder body further comprises a locking member coupled between the upper holder and the lower holder, and the distance between the upper holder and the lower holder is adjusted by the locking member.

10. The testing apparatus of claim 8, further comprising a support member detachably connected to the lower holder to support a lower surface of the composite specimen.

11. The test apparatus of claim 8, wherein the upper holder includes an inclined surface at a distal end of the upper holder to align with the first end of the composite specimen.

12. The testing apparatus of claim 8, wherein the holder body further comprises a base, and the positioning mechanism is movably coupled to the base.

13. The test device of claim 12, wherein the base comprises at least one positioning hole, the positioning mechanism comprising: at least one positioning rod, movably engaged with the positioning hole; and a positioning plate configured to rest on the second end of the composite specimen and move together with the positioning rod.

14. The testing apparatus of claim 8, wherein the holder body comprises a groove for receiving the composite specimen, and the composite specimen is configured to move along the groove.

15. The testing apparatus of claim 8, wherein the force applying rod is configured to move toward the composite specimen in a direction perpendicular to a surface of the composite specimen.

16. A method for manufacturing a semiconductor package, characterized in that: include: performing a semiconductor process to form an encapsulated semiconductor device; Providing a testing device, the testing device comprising a holder body, a positioning mechanism and a force application rod; clamping a first end of the encapsulated semiconductor device using the holder body; Using the positioning mechanism to lean against a second end of the encapsulated semiconductor device relative to the first end to adjust a clamping position of the encapsulated semiconductor device; removing the positioning mechanism; as well as A predetermined force is applied to a portion of the encapsulated semiconductor device exposed by the holder body using the force applying rod.

17. The method according to claim 16, further comprising: A support is provided on a lower portion of the holder body, wherein the encapsulated semiconductor device rests on the support when clamped by the holder body.

18. The method according to claim 17, further comprising: The support is removed before applying the force to the portion of the encapsulated semiconductor device exposed by the holder body.

19. The method of claim 16, wherein performing a semiconductor process to form the encapsulated semiconductor device further comprises: providing a semiconductor device and a plurality of through holes on a carrier; Providing an encapsulation material to encapsulate the semiconductor device and the through-hole; as well as The carrier is removed.

20. The method of claim 19, wherein the predetermined force is applied at an interface between the encapsulation material and the semiconductor device.

21. The method of claim 19, wherein the predetermined force is applied at an interface between the encapsulating material and the perforation.

22. The method of claim 16, further comprising: When the predetermined force causes the encapsulated semiconductor device to fail, process parameters of the semiconductor process are modified to form a modified encapsulated semiconductor device.

23. The method according to claim 22, further comprising: providing a support on a lower portion of the holder body, wherein the encapsulated semiconductor device rests on the support when clamped by the holder body; as well as The support is removed before applying the force to the portion of the encapsulated semiconductor device exposed by the holder body.

24. The method of claim 22, further comprising: If the modified encapsulated semiconductor device satisfies the predetermined force test, a redistribution structure is formed over the modified encapsulated semiconductor device.

25. A method for testing the bonding strength of a composite sample, characterized in that: include: clamping the first end of the composite specimen by a holder body; Pushing the second end of the composite specimen toward the holder body by a positioning mechanism to adjust a clamping position of the composite specimen clamped by the holder body, wherein the second end is relative to the first end; removing the positioning mechanism; and A force is applied to a portion of the composite specimen exposed by the holder body.

26. The method according to claim 25, further comprising: A support is provided on a lower portion of the holder body, wherein the composite specimen rests on the support when clamped by the holder body.

27. The method according to claim 26, further comprising: The support is removed before the force is applied to the portion of the composite specimen exposed by the holder body.

28. The method of claim 25, wherein the holder body comprises an upper holder and a lower holder, and the first end of the composite specimen is configured to be clamped between the upper holder and the lower holder.

29. The method of claim 28, wherein clamping the first end of the composite specimen by the holder body further comprises: disposing the first end of the composite specimen between the upper holder and the lower holder; as well as The distance between the upper holder and the lower holder is adjusted by a locking member coupled between the upper holder and the lower holder.

30. The method of claim 25, wherein the composite specimen is configured to move along a groove extending across the holder body.

31. The method of claim 25, wherein the force is applied to a bonding interface between multiple components of the composite specimen.

32. The method of claim 25, wherein applying the force to the portion of the composite specimen exposed by the holder body further comprises: The force is applied through a distal end of a force application rod, wherein the longitudinal axis of the force application rod is perpendicular to the application surface of the composite specimen.

33. The method of claim 25, wherein applying the force to the portion of the composite specimen exposed by the holder body further comprises: The force is applied through a side surface of a force-applying rod, wherein a longitudinal axis of the force-applying rod is parallel to an applied surface of the composite specimen.

34. A method for testing the bonding strength of a composite sample, characterized in that: include: clamping one end of the composite specimen by a holder body; pushing opposite ends of the composite specimen toward the holder body to a testing position via a positioning mechanism coupled to the holder body; removing the positioning mechanism; and A force is applied to bonding interfaces between the plurality of components of the composite specimen exposed by the holder body.

35. The method of claim 34, further comprising: Before the opposite ends of the composite specimen are pushed toward the holder body by the positioning mechanism, a support is connected to the lower holder to support a bottom surface of the composite specimen.

36. The method of claim 35, further comprising: The support is removed before the force is applied to the composite specimen.