Large-scale crossbar switch matrix with smaller series resistance

By designing high aspect ratio electrodes and nail electrodes embedded with curable layers on a flexible substrate, the problem of large series resistance in large-scale cross-switch circuits is solved, and smaller resistance and higher productivity is achieved, suitable for smart-based applications. Wearing devices.

CN111199991BActive Publication Date: 2024-11-01TETRAMEM INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201911120042.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-11-16
Filing Date
2019-11-15
Publication Date
2024-11-01
Estimated Expiration
2039-11-15

AI Technical Summary

Technical Problem

When manufacturing large-scale cross-switch circuits on flexible substrates, series resistance is difficult to reduce, resulting in signal attenuation and heat dissipation problems, affecting the performance and wearability of the device.

Method used

By designing high aspect ratio electrodes and flexible substrates, cross-switch circuits are manufactured using plating and bonding processes to form a nail-shaped upper and lower electrodes, and the upper electrodes are embedded in the curable layer to reduce the series resistance of the electrodes.

Benefits of technology

It realizes reducing series resistance in large-scale cross-switch circuits, improving productivity, preventing layering, providing transparent cladding to adjust the electrical or optical characteristics of the memristor, extending device life, and suitable for smart wearable devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111199991B_ABST
    Figure CN111199991B_ABST
Patent Text Reader

Abstract

The present disclosure discloses a technique for reducing series resistance. An exemplary method includes: forming a first layer on a temporary substrate; forming a second layer on the first layer; etching the first layer and the second layer to form a groove; electroplating an upper electrode through the groove, wherein the upper electrode is partially formed on the upper surface of the second layer; removing the first layer and the second layer; forming a curable layer on the temporary substrate and the upper electrode; removing the temporary substrate from the curable layer and the upper electrode; forming a cross-point device on the curable layer and the upper electrode; forming a lower electrode on the cross-point device; forming a flexible substrate on the lower electrode.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to large-scale crossbar switch circuits with reduced series resistance, and more particularly, to reducing series resistance in flexible crossbar switch circuits by using high aspect ratio electrodes fabricated using electroplating and bonding processes. Background Art

[0002] The crossbar switch matrix may include rows and columns of electrodes (or other electrodes) that cross each other to form a crosspoint device at the intersection. The crossbar switch circuit may be used in a code comparator, a neural network, or other applications (e.g., a wearable device).

[0003] Forming large-scale cross-switch circuits on flexible substrates and reducing series resistance remains a technical challenge. Summary of the invention

[0004] The present disclosure discloses a method for manufacturing a large-scale crossbar switch matrix with a smaller series resistance, and more particularly, relates to the design of electrodes and flexible substrates in the crossbar switch circuit.

[0005] A device includes: a plurality of upper electrodes; and a plurality of cross-point devices connecting the plurality of upper electrodes, wherein each of the plurality of upper electrodes includes a top portion and a tail portion (in a cross-sectional view), the top portion being wider than the tail portion.

[0006] In some implementations, the top portion is dome-shaped in cross-section.

[0007] In some implementations, the tail portion is trapezoidal in cross-section.

[0008] In some implementations, each of the plurality of upper electrodes has a nail shape in a cross-sectional view.

[0009] In some implementations, the plurality of upper electrodes includes a plurality of row electrodes and / or column electrodes.

[0010] In some implementations, each of the plurality of cross-point devices includes a memristor.

[0011] In some implementations, a bottom width of the tail portion is in a nanometer to micrometer range, and a height of each of the plurality of upper electrodes is in a micrometer range.

[0012] In some implementations, a ratio of a bottom width of the tail portion to a height of each of the plurality of upper electrodes is less than 1.

[0013] In some implementations, the apparatus further includes a bottom electrode formed on the plurality of cross-point devices.

[0014] In some implementations, the device further includes a flexible substrate formed on the lower electrode.

[0015] In some implementations, the material of the flexible substrate includes polymer, plastic, rubber, resin, or a combination thereof.

[0016] In some implementations, the memristor includes a memristor system, a floating gate device, a phase change random access memory (PCRAM) device, a resistive random access memory (RRAM or ReRAM), a magnetoresistive random access memory (MRAM), or any device with adjustable resistance.

[0017] A method includes: forming a first layer on a temporary substrate; forming a second layer on the first layer; etching the first layer and the second layer to form a groove; electroplating an upper electrode through the groove, wherein the upper electrode is partially formed on the upper surface of the second layer; removing the first layer and the second layer; forming a curable layer on the temporary substrate and the upper electrode; removing the temporary substrate from the curable layer and the upper electrode; forming a cross-point device on the curable layer and the upper electrode; forming a lower electrode on the cross-point device; and forming a flexible substrate on the lower electrode.

[0018] In some implementations, the curable layer includes a thermally curable layer, a photocurable layer, an ultraviolet (UV) curable layer, a radiation curable layer, or any layer capable of changing from a liquid phase to a solid phase.

[0019] In some implementations, forming a cross-point device on the curable layer and the upper electrode includes: forming a cross-point device; and bonding the cross-point device to the curable layer and the upper electrode.

[0020] In some implementations, forming the cross-point device on the curable layer and the top electrode further includes forming a bonding layer on the cross-point device before bonding the cross-point device to the curable layer and the top electrode.

[0021] In some implementations, the step of removing the temporary substrate from the curable layer and the upper electrode further comprises: peeling the curable layer and the upper electrode from the temporary substrate. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 is a block diagram illustrating an exemplary crossbar switch circuit according to some embodiments of the present disclosure.

[0023] Figure 2 is a block diagram showing Figure 1 A cross-sectional view of the crossbar switch circuit is shown at section AA'.

[0024] Figures 3A-3H is a block diagram illustrating a process for manufacturing a crossbar switch circuit according to some embodiments of the present disclosure.

[0025] Figure 4 is a flow chart illustrating a method for manufacturing a crossbar switch circuit according to some embodiments of the present disclosure.

[0026] The embodiments disclosed in the present disclosure are illustrated in the accompanying drawings by way of example and not limitation. Reference numerals refer to corresponding parts in the drawings. DETAILED DESCRIPTION

[0027] The present disclosure provides a system and method capable of reducing the series resistance in a large-scale crossbar switch circuit and forming a flexible substrate. The technology described in the present disclosure can bring the following technical advantages. First, as described in the present disclosure, the manufacturing process and structural design of the row electrodes and column electrodes can reduce the series resistance in the large-scale crossbar switch circuit.

[0028] Second, the disclosed technology can improve productivity and prevent delamination when the growth substrate is removed or a flexible substrate is used in place of the growth substrate.

[0029] Third, the disclosed technology can form a transparent overlay on the memristor, so that the electrical or optical properties of the memristor can be tuned by using different wavelengths of light.

[0030] Memristor crossbar circuit matrices can provide technical advantages for a variety of applications, such as smart wearable electronic devices. However, manufacturing large-scale crossbar matrices can be challenging for a variety of reasons. First, high-precision processing of flexible substrates that requires critical dimension control can be very difficult. Second, the manufacturing of highly conductive electrode lines is challenging, especially when fabricated at the nanoscale level. Third, the thermal budget of flexible substrates is limited. To build large-scale crossbar matrices, the electrode resistance must be extremely small. If high packing density and nano-features are required, the line resistance problem will be more serious. On the one hand, the signal propagating along the vertical column line or horizontal row line will be attenuated by the high-resistance line. On the other hand, the high line resistance will also increase the RC constant, making the charging speed of the line slower. The heat generated by the high-resistance lines of the crossbar matrix is ​​usually not easy to dissipate. Therefore, there is a need for systems and methods for reducing the resistance in large-scale crossbar matrices.

[0031] Figure 1 is a block diagram showing an exemplary crossbar switch circuit 100 with a smaller series resistance according to some embodiments of the present disclosure. Figure 1 As shown, the cross-point switch circuit 100 includes a first row electrode 101 , a first column electrode 102 , and a cross-point device 103 .

[0032] The cross-point device 103 may include a memristor. In some implementations, the memristor includes a memristor system, a floating gate device, a phase change random access memory (PCRAM) device, a resistive random access memory (RRAM or ReRAM), a magnetoresistive random access memory (MRAM), or any device with adjustable resistance.

[0033] Figure 2is a block diagram showing a cross-sectional view 200 of the crossbar switch circuit 100, the cross-sectional view 200 being from Figure 1 1. The cross-sectional view 200 shows Figure 1 The cross-point switch circuit shown in the figure includes a flexible substrate 211, a lower electrode 209 formed on the flexible substrate 211, a switching layer 203 formed on the lower electrode 209, a bonding layer 205 formed on the cross-point device 203, an electrode 202 formed on the bonding layer 205, and a curable layer 207 formed on the upper electrode 202 and the bonding layer 205. In some implementations, the curable layer 207 includes: an ultraviolet (UV) curable layer, a heat curable layer, or any layer that can be transformed from a liquid phase to a solid phase.

[0034] In some implementations, the upper electrode 202 can be a row electrode (e.g., the first row electrode 101) and / or a column electrode (e.g., the first column electrode 102). In some implementations, the upper electrode 202 is the first column electrode 102, and the lower electrode 209 is the first row electrode 101. In some implementations, the curable layer 207 covers or encapsulates the entire upper electrode 202.

[0035] like Figure 2 As shown, the upper electrode 202 may be in the shape of a nail and embedded in the curable layer 207. The nail shape is essential for the manufacturing process using a flexible substrate instead of a growth substrate, see Figures 3A-3H Discuss this.

[0036] In some implementations, the upper electrode 202 includes a top portion 2022 and a tail portion 2021. In some implementations, the top portion 2022 may be dome-shaped, such as Figure 2 In some implementations, the tail portion 2021 may be a trapezoid or an inverted trapezoid, such as Figure 2 shown.

[0037] In one embodiment of the present disclosure, Figure 2 As shown, the tail portion 2021 is in an inverted trapezoidal shape, and its bottom width w1 is narrower than its top width. In addition, the height h1 of the upper electrode is the distance between the highest surface of the top portion 2022 and the lowest surface of the tail portion 2021 .

[0038] In some implementations, the bottom width of the tail is in the range of nanometers to micrometers, and the height h1 of each of the plurality of upper electrodes is in the range of micrometers. Nanometers can be defined as a range between 0.5 nanometers and 500 nanometers; micrometers are defined as a range between 0.5 micrometers and 500 micrometers.

[0039] In some implementations, a ratio of a bottom width of the tail portion to a height h1 of each of the plurality of upper electrodes is less than 1. This approach reduces the series resistance of the electrodes.

[0040] The material of the upper electrode 202 includes Cu, Au, Ag, Ni, Sn or a combination or alloy thereof. In some implementations, the material of the bonding layer 205 may be made of one of the following materials: In, Pb, Sn, Au, Ag and alloys thereof. The exchange layer 203 may be a blank layer, or may be Figure 2 and 3A -Style shown in 3H.

[0041] In some implementations, the lower electrode 209 may be an electrode (e.g., a row electrode or a column electrode) connected to the cross-point device 203. The lower electrode 209 may have the same structure as the upper electrode 202 rotated 90 degrees, and may be manufactured by the same process as the upper electrode 202. The lower electrode 209 may also have a spike-shaped structure and a high aspect ratio like the upper electrode 202 to achieve a desired low resistance.

[0042] In some implementations, the flexible substrate 211 is made of a polymer, plastic, rubber, resin or a combination thereof. In some implementations, the curable layer 207 is made of an acrylate resin, an epoxy resin or a combination thereof. In some implementations, the curable layer 207 is bendable and transparent. For example, if a Ge2Sb2Te5 (GST) material is used as an exchange layer in a memristor of a crosspoint device 203, the phase change can be locally controlled by light. The flexible substrate 211 together with the lower electrode 209 can be collectively referred to as a curable layer 213. The curable layer 213 can have the same structure, composition and other characteristics as the curable layer 207. The curable layer 213 can be the same as the curable layer 207, but in different positions, for example, one is placed horizontally and the other is placed vertically. In some implementations, the curable layer 213 covers or encapsulates the electrode matrix embedded therein.

[0043] Figures 3A-3H is a block diagram illustrating a process 300 for manufacturing a crossbar switch circuit, according to some embodiments of the present disclosure. Figure 4 is a flow chart illustrating a method 400 for manufacturing a crossbar switch circuit according to some embodiments of the present disclosure.

[0044] like Figure 3A As shown, a temporary substrate 301 is provided. In some implementations, the temporary substrate 301 includes silicon, silicon carbide, gallium, sapphire, glass, or any other material capable of growing or supporting other materials throughout the manufacturing process. A first layer 303 may be formed on the temporary substrate 301, and a second layer 305 may be formed on the first layer 303 (step 402). In some implementations, the first layer 303 is a transfer layer, and the second layer 305 is an image layer for enhancing the aspect ratio.

[0045] like Figure 3B As shown, a photolithography and etching process may be performed on the second layer 305 to form an unetched portion of the second layer 305'. Figure 3C As shown, the first layer 303 may be etched according to the pattern of the unetched portion of the second layer 305 of the temporary substrate 301. The unetched portion of the first layer 303' and the trench are formed (step 404).

[0046] Then, if Figure 3C As shown, the upper electrode 202 is electroplated through the groove, and the electroplating is completed when the groove is full (step 406). In some implementations, the upper electrode 202 covers a portion (but not all) of the upper surface of the second layer 305'. Then, the first layer 303' and the second layer 305' can be removed by wet etching with chemicals, such as Figure 3D (Step 408).

[0047] In addition, if Figure 3E As shown, an ultraviolet curable layer 207 may be formed on the temporary substrate 301 and the upper electrode 202 (step 410). In some implementations, the UV curable layer 207 is formed by coating a liquid layer on the temporary substrate 301 and the upper electrode 202, and then exposing the liquid layer to ultraviolet light to cure the liquid layer. Thus, the upper electrode 202 having sufficient mechanical strength is embedded in the curable layer 207 to keep the upper electrode 202 in the curable layer 207 during the subsequent substrate transfer process.

[0048] like Figure 3F As shown, the temporary substrate 301 is removed from the curable layer 207 and the upper electrode 202 (step 412). In some implementations, the UV curable layer and the upper electrode are peeled off from the temporary substrate using a high viscosity glue or other wafer transfer techniques to remove the temporary substrate 301. Figure 3F As shown at the top, when the curable layer 207 is flipped and rotated 90 degrees, it can be combined with another curable layer 207 to form a crossbar switch.

[0049] In addition, as shown in Figure Figure 3G As shown, a flexible substrate 211 may be provided; a lower electrode 209 may be formed on the flexible substrate 211, and a cross-point device 203 may be formed on the lower electrode 209. In some implementations, a bonding layer 205 may be formed on the cross-point device 203.

[0050] Therefore, if Figure 3H As shown, the cross-point device 203 is connected to and aligned with the upper electrode 202. The cross-point device 203 is formed on the curable layer 207 and the upper electrode 202 (step 414). The lower electrode 209 is formed on the cross-point device 203 (step 416), and the flexible substrate 211 is formed on the lower electrode 209 (step 418).

[0051] pass Figures 3A-3HThe crossbar circuit formed by the illustrated process can operate on a flexible (eg, bendable or stretchable) surface and provide reduced series resistance.

[0052] Furthermore, devices within a crossbar circuit formed in this manner are flat at the junctions, which increases device lifetime. The surface of the exposed metal lines is typically extremely smooth; therefore, the interface between the switching layer and the electrodes is also very smooth, continuing the smooth surface of the original carrier substrate (e.g., high-quality silicon).

[0053] The etching step may result in a sloped sidewall, which is generally to be avoided. However, in the present disclosure, a sloped sidewall is advantageous because it allows for better anchoring to the transferred photoresist, which is Figure 3F and 3G The critical dimension is located at the bottom of the trench (ref. Figure 3C to be explained), which can be well controlled by the etching process.

[0054] In addition, the “nail-shaped” metal structure after electroplating (e.g. Figure 3E ) also improves the mechanical bonding between the flexible substrate layer and the metal electrodes, so delamination does not occur even during bending of the flexible substrate. The unique metal line structure reduces resistance without increasing the size of the nodes within the crossbar switch circuit.

[0055] The cured UV resist (or other material) can be made flexible, stretchable or transparent, so the junction can be exposed to light to further tune the device performance. For example, if the GST material is used as a switching layer, the phase change can be locally controlled by light.

[0056] Designated waveguides can be integrated into each node, allowing personalized control of the optical and electrical properties at each node. Driver circuits can be placed on a flexible substrate and directly integrated into a crossbar switch matrix.

[0057] Multiple instances may be provided for components, operations, or structures described as single instances in this disclosure. Finally, the boundaries between various components, operations, and data stores are somewhat arbitrary, and specific operations are described in the context of a specific illustrative configuration. Other functional allocations are foreseeable and may fall within the scope of implementation. Generally, structures and functions presented as separate components in the exemplary configuration may be implemented as a combined structure or component. Similarly, structures and functions presented as single components may also be implemented as separate components. These and other changes, modifications, additions, and improvements fall within the scope of implementation.

[0058] It should also be understood that although the present disclosure uses the terms "first," "second," etc. to describe various elements, these elements should not be limited by these terms. These terms are only used to distinguish one element from another. For example, the first column can be called the second column, and likewise, the second column can be called the first column without changing the meaning of the description, as long as all occurrences of "first column" are renamed consistently, and all occurrences of "second column" are also renamed consistently. The first column and the second column are still the original two columns, but each column is different from the original column.

[0059] The terms used in this disclosure are only used to describe specific implementations and are not intended to limit the claims. As used in the description of the various described embodiments and in the appended claims, the singular forms "a" and "the" also cover the plural forms unless the context clearly indicates otherwise. It should also be understood that the term "and / or" used in this disclosure includes any and all combinations of one or more related listed items. In addition, it should be further understood that the terms "including" and / or "comprising" used in this disclosure specify the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or sets.

[0060] As used in this disclosure, the term "if" may be interpreted as "when" or "once" or "in response to determining" or "according to determining" or "in response to detecting" that the stated antecedent is true, depending on the context. Similarly, the phrase "if it is determined that (the stated antecedent is true)" or "if (the stated antecedent is true)" or "when (the stated antecedent is true)" may be interpreted as "once determined" or "in response to determining" or "according to determining" or "once detected" or "in response to detecting" that the stated antecedent is true, depending on the context.

[0061] The above description includes exemplary systems, methods, techniques, instruction sequences, and computer programs that embody the illustrative embodiments of the present disclosure. For illustrative purposes, numerous specific details are described in order to provide an understanding of various embodiments of the subject matter of the present invention. However, it is obvious to those skilled in the art that the subject matter of the present invention can be practiced without these specific details. Typically, well-known instruction instances, protocols, structures, and techniques are not necessarily shown in detail.

[0062] For illustrative purposes, the above description has been described with reference to specific embodiments. However, the above illustrative discussion is not intended to be exhaustive or to limit the embodiments to the precise forms disclosed. In view of the above teachings, many modifications and variations are possible. The embodiments selected and described are intended to best explain the principles of the invention and its practical application, thereby enabling others skilled in the art to best utilize the embodiments and various modifications suitable for the specific use contemplated.

Claims

1. A device comprising: Flexible substrate; a lower electrode formed on the flexible substrate; a plurality of upper electrodes; a curable layer, wherein the plurality of upper electrodes are embedded in the curable layer; as well as A plurality of cross-point devices are connected to the plurality of upper electrodes, wherein each of the plurality of upper electrodes comprises a top portion and a tail portion, and the top portion is wider than the tail portion; wherein the plurality of cross-point devices are formed on the lower electrode; and each of the plurality of cross-point devices comprises a memristor.

2. The device as claimed in claim 1, wherein the plurality of upper electrodes comprises a plurality of row electrodes and / or a plurality of column electrodes.

3. The device as claimed in claim 1, wherein the top is dome-shaped.

4. The device as claimed in claim 1, wherein the tail portion is trapezoidal in shape.

5. The device as claimed in claim 1, wherein each of the plurality of upper electrodes is in the shape of a nail. 6 . The device as claimed in claim 1 , wherein a bottom width of the tail portion is in a nanometer to micrometer order, and a height of each of the plurality of upper electrodes is in a micrometer order.

7. The device of claim 1, wherein a ratio of a bottom width of the tail portion to a height of each of the plurality of upper electrodes is less than 1.

8. The device as claimed in claim 1, wherein the material of the flexible substrate comprises polymer, plastic, rubber, resin or a combination thereof.

9. The apparatus of claim 1, wherein the memristor comprises: Memristive systems, floating gate devices, phase change random access memory (PCRAM) devices, resistive random access memory (RRAM or ReRAM), magnetoresistive random access memory (MRAM), or any device with adjustable resistance.

10. The device of claim 1, wherein the curable layer comprises a UV curable layer, a thermal curable layer, a photocurable layer, or a radiation curable layer.

11. The device of claim 1, wherein the curable layer is curved and transparent.

12. The device of claim 1, wherein the curable layer comprises a resin.

13. The device as claimed in claim 1, wherein the device further comprises a bonding layer, wherein the upper electrode and the curable layer are formed on the bonding layer.

14. A method for reducing series resistance, comprising: forming a first layer on a temporary substrate; forming a second layer on the first layer; etching the first layer and the second layer to form a trench; electroplating an upper electrode through the trench, wherein the upper electrode is partially formed on an upper surface of the second layer; Remove the first and second layers; Forming a curable layer on the temporary substrate and the upper electrode; removing the temporary substrate from the curable layer and the upper electrode; forming a cross-point device on the curable layer and the upper electrode; forming a lower electrode on the cross-point device; and forming a flexible substrate on the lower electrode.

15. The method for reducing series resistance according to claim 14, wherein the curable layer comprises: A UV curable layer, a heat curable layer, a photocurable layer or a radiation curable layer.

16. The method for reducing series resistance according to claim 14, wherein forming a cross-point device on the curable layer and the upper electrode comprises: forming a cross-point device; as well as A cross point device is bonded to the curable layer and the top electrode.

17. The method for reducing series resistance according to claim 14, wherein the step of forming a cross-point device on the curable layer and the upper electrode further comprises: Prior to bonding the cross-point device to the curable layer and the top electrode, a bonding layer is formed on the cross-point device.

18. The method for reducing series resistance according to claim 15, wherein the step of removing the temporary substrate from the curable layer and the upper electrode further comprises: The curable layer and the upper electrode are peeled off from the temporary substrate.