Electrochemical module, assembly method of electrochemical module, electrochemical device and energy system

By using elastic flat plate components and materials with different thermal expansion rates in fuel cell stacks, the problem of insufficient fastening pressure caused by the expansion of the laminate was solved, realizing miniaturized, lightweight and efficient fuel cell modules.

CN111902989BActive Publication Date: 2024-10-22OSAKA GAS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980023958.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-03-30
Filing Date
2019-03-29
Publication Date
2024-10-22
Estimated Expiration
2039-03-29

AI Technical Summary

Technical Problem

Existing fuel cell stacks suffer from insufficient clamping pressure due to the expansion of the stacked structure at high temperatures, which increases internal resistance and reduces the sealing of reactant gases. Furthermore, traditional solutions have led to the increase in the size and weight of fuel cell stacks.

Method used

A flexible flat plate component is arranged along the plane of the laminate and the plane of the clamping body. The elastic force of the flat plate component is used to uniformly tighten the laminate when it expands. The thermal expansion component is used to compensate for the difference in thermal expansion. Materials with different thermal expansion rates, such as austenitic stainless steel and ferritic stainless steel, are used to form the clamping body.

Benefits of technology

This design achieves proper tightening during the expansion of the laminate, suppressing the increase in internal resistance and the reduction in the sealing of the reactant gas, while also enabling miniaturization and lightweighting, thus improving the durability and reliability of the fuel cell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111902989B_ABST
    Figure CN111902989B_ABST
Patent Text Reader

Abstract

The purpose is to provide a small and lightweight electrochemical module, etc., which can properly tighten the stack even when the stack expands. The electrochemical module M has: an electrochemical element stack S, in which a plurality of electrochemical elements having an electrolyte layer and a first electrode and a second electrode respectively arranged on both sides of the electrolyte layer are stacked along a substrate in a predetermined stacking direction; an elastic flat plate-shaped member 220, which is arranged along at least one of the first plane and the second plane of the electrochemical element stack S; and a clamping body 230, which includes a first clamping body 230T along the first plane and a second clamping body 230B along the second plane in the stacking direction, and clamps the electrochemical element stack S via the flat plate-shaped member 220.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an electrochemical module, an assembling method of the electrochemical module, an electrochemical device and an energy system. Background Art

[0002] In the fuel cell stacks of Patent Documents 1 and 2, a stack is formed by stacking a plurality of power generation units. The stack is clamped by a pair of rectangular end plates arranged at both ends of the stacking direction. Between the pair of end plates, connecting rods extending in the stacking direction of the stack are arranged at four locations supporting the periphery of the pair of end plates. In addition, the two ends of the connecting rod are fixed to each of the pair of end plates by bolts. Therefore, a pair of end plates are supported and fixed by the portions where the connecting rods are fixed at four locations around them, and the stack clamped between the pair of end plates is tightened. Thus, a tightening pressure in the stacking direction is applied to the stack, the increase of the internal resistance is suppressed, and the reduction of the sealing of the reaction gas is suppressed, so that the plurality of power generation units are constituted as an integrated stack.

[0003] Prior art literature

[0004] Patent Literature

[0005] Patent Document 1: Japanese Patent Application Publication No. 2015-153679

[0006] Patent document 2: Japanese Patent Application Publication No. 2016-62852. Summary of the invention

[0007] Problems to be solved by the invention

[0008] The fuel cell stacks of Patent Documents 1 and 2 reach a high temperature during power generation, whereby the stacked body having a plurality of power generation units stacked thereon expands in, for example, the stacking direction. In addition, a pair of end plates are fastened and clamped together in the stacking direction by connecting rods, but the connecting rods also expand in the stacking direction due to the high temperature during power generation.

[0009] Therefore, the distance between the stack and the end plate becomes larger, and the clamping pressure of the stack becomes insufficient, which may lead to an increase in the internal resistance of the stack and a decrease in the sealing performance of the reaction gas.

[0010] Therefore, a pair of thickened end plates for clamping the stacked body is adopted, and the thick end plates are used to bear the expansion of the stacked body. Furthermore, the four corners of the periphery of the pair of thick end plates are supported by connecting rods, and large fastening bolts using springs are used to bear the changes caused by the expansion.

[0011] However, in the above-mentioned structure, the pair of end plates are thick, and the fuel cell stack is formed using large fastening bolts using springs to fasten the thick end plates. Therefore, it is inevitable that the fuel cell stack will be larger and heavier.

[0012] Therefore, the present invention has been made in view of the above-mentioned problems, and an object of the present invention is to provide a small and light electrochemical module and an electrochemical module assembling method, etc., which can appropriately tighten a stacked body even when the stacked body expands.

[0013] Means for solving problems

[0014] [constitute]

[0015] The electrochemical module of the present invention is characterized in that it has:

[0016] A laminated body in which a plurality of electrochemical elements having an electrolyte layer and a first electrode and a second electrode respectively arranged on both sides of the electrolyte layer are formed along a substrate and are laminated in a predetermined lamination direction;

[0017] an elastic flat plate-shaped member disposed along at least one of a first plane of the stacked body in the stacking direction and a second plane opposite to the first plane; and

[0018] The clamping body includes a first clamping body in the form of a flat plate arranged along the first plane and a second clamping body in the form of a flat plate arranged along the second plane in the stacking direction, and clamps the stacked body via the flat plate-shaped member.

[0019] According to this characteristic configuration, a flat plate-shaped member is arranged along the plane of the stacked body and the plane of the clamping body, at least between the first plane in the stacking direction of the stacked body and the first clamping body, and between the second plane opposite to the first plane and the second clamping body. That is, in at least one plane side of the stacked body, the elastic flat plate-shaped member is arranged along the plane of the stacked body and the plane of the clamping body.

[0020] Here, when at least one of the stack and the clamp expands, the distance between the stack and the clamp may change before and after the expansion of the stack, etc. The flat plate-shaped member has elastic force, so even when the distance between the stack and the clamp changes, the stack is elastically clamped between the pair of clamps by its elastic force.

[0021] More specifically, if the interval between the stack and the clamp changes due to the expansion of at least one of the stack and the clamp, the extrusion force applied to the flat plate member also changes due to the change in the interval. The changing extrusion force is elastically received by the flat plate member at a contact portion that is substantially uniformly distributed along the substantially entire plane of the stack and the plane of the clamp.

[0022] Therefore, even if the distance between the stacked body and the clamping body varies due to expansion of the stacked body, the flat plate-like member can provide an appropriate tightening pressure in the stacking direction substantially uniformly along the plane of the stacked body.

[0023] In this way, by simply configuring a flat plate-shaped member between at least one of the first plane and the second plane of the stack and the plane of the clamp, along the planes of the stack and the clamp, an electrochemical module can be configured that takes into account the expansion of the stack, etc. Therefore, a small and lightweight electrochemical module that can appropriately fasten the stack, etc., can be provided even when the stack, etc., expands.

[0024] It should be noted that the configuration in which the first electrode and the second electrode are respectively arranged on both sides of the electrolyte layer includes any one of the configurations in which the first electrode is arranged in contact with the electrolyte layer and the configuration in which the first electrode is arranged facing the electrolyte layer via an interlayer. The relationship between the second electrode and the electrolyte layer is also the same. The interlayer includes, for example, an anti-reaction layer and an intermediate layer.

[0025] [constitute]

[0026] A further characteristic configuration of the electrochemical module according to the present invention is that the flat plate-shaped member is a thermally expandable member that expands by heat.

[0027] For example, when the stack and the clamp are changed from a low temperature state (e.g., about 20°C at room temperature, etc.) when the electrochemical element is not generating electricity to a high temperature state (e.g., about 650°C to about 950°C, etc.) when generating electricity, they expand. At this time, if a difference in thermal expansion occurs between the thermal expansion of the stack and the thermal expansion of the clamp, the interval between the stack and the clamp is different when generating electricity (at high temperature) and when not generating electricity (at low temperature).

[0028] According to this characteristic configuration, the flat plate-shaped member is a thermal expansion member, so the flat plate-shaped member also thermally expands due to the high temperature reached when the electrochemical element generates electricity. Therefore, even if the interval between the stack and the clamping body changes due to thermal expansion, the flat plate-shaped member uses the change of elastic force caused by the thermal expansion of the flat plate-shaped member itself to apply appropriate tightening pressure to the stack using the clamping body as a pressing surface.

[0029] That is, the change in the distance between the stacked body and the clamping body caused by thermal expansion is compensated by the change caused by thermal expansion of the flat plate-like member, so that even after the above-mentioned distance change, an appropriate fastening pressure is applied to the stacked body.

[0030] Furthermore, the flat plate-shaped member is arranged along the plane of the stack and the plane of the clamping body, so that even after the aforementioned interval changes, an appropriate tightening pressure is applied roughly uniformly along the plane of the stack. Therefore, in the electrochemical module, it is possible to suppress an increase in internal resistance and a decrease in the sealing performance of the reaction gas.

[0031] [constitute]

[0032] The electrochemical module according to the present invention has a further characteristic configuration in which the flat plate-shaped member is in contact with at least one of a plane of the stacked body and a plane of the clamping body at a plurality of dispersed locations.

[0033] According to this characteristic configuration, the flat plate-shaped member is disposed between the plane of the stacked body and the plane of the clamping body and along these planes. Furthermore, the flat plate-shaped member contacts at least one of the plane of the stacked body and the plane of the clamping body at a plurality of dispersed locations.

[0034] Here, if the interval between the stack and the clamp changes due to the expansion of at least one of the stack and the clamp, the extrusion force on the flat plate-shaped member due to the change in the interval also changes. The changing extrusion force is elastically supported by the flat plate-shaped member in a state of being roughly uniformly distributed along the plane of the stack and the plane of the clamp. The reason is that the flat plate-shaped member contacts at least one of the plane of the stack and the plane of the clamp at multiple dispersed locations. Furthermore, in the case of thermal changes in the flat plate-shaped member, the change in the interval between the stack and the clamp is supported at the aforementioned multiple locations due to the thermal changes in the flat plate-shaped member.

[0035] Therefore, even if the interval between the stack and the clamp changes due to the expansion of the stack, the flat plate-shaped member can be used to roughly uniformly apply a moderate tightening pressure in the stacking direction along the plane of the stack. Therefore, in the electrochemical module, the increase in internal resistance and the decrease in the sealing performance of the reaction gas can be suppressed, and miniaturization and lightness can be achieved.

[0036] [constitute]

[0037] The electrochemical module according to the present invention is further characterized in that:

[0038] The flat plate-shaped member receives, by its elastic force, a difference in thermal expansion between the stacked body and the sandwiching body when the electrochemical element is generating power and when the electrochemical element is not generating power.

[0039] For example, when the stack and the clamp are changed from a low temperature state (e.g., about 20°C at room temperature, etc.) when the electrochemical element is not generating electricity to a high temperature state (e.g., about 650°C to about 950°C, etc.) when generating electricity, they expand. At this time, if a difference in thermal expansion occurs between the thermal expansion of the stack and the thermal expansion of the clamp, the interval between the stack and the clamp is different when generating electricity (at high temperature) and when not generating electricity (at low temperature).

[0040] According to this characteristic configuration, the flat plate-like member compensates for the change in the distance between the stacked body and the sandwiching body due to thermal expansion by using its elastic force.

[0041] For example, when the flat plate-shaped member is a thermally expandable member, the flat plate-shaped member compensates for the change in the distance between the stacked body and the sandwiching body caused by the thermal expansion by the thermal expansion of the flat plate-shaped member itself.

[0042] In addition, even in the case where the thermal expansion coefficient of the flat plate-shaped member is small, the stack, the flat plate-shaped member, and the clamping body are pre-assembled by a large tightening pressure. In this case, a large repulsive force is generated in the flat plate-shaped member. Therefore, even if the interval between the stack and the clamping body is widened, the repulsive force of the flat plate-shaped member remains to a certain extent, compensating for the widening of the aforementioned interval.

[0043] Thus, even after the above-mentioned interval changes, the flat plate-shaped member can substantially uniformly apply an appropriate tightening pressure along the plane of the stacked body. Therefore, in the electrochemical module, it is possible to suppress an increase in internal resistance and a decrease in sealing performance for reaction gas.

[0044] [constitute]

[0045] The electrochemical module according to the present invention is further characterized in that:

[0046] The clamping pressure applied by the flat plate-shaped member to the stack when the electrochemical element is not generating electricity is applied in advance to a degree that can ensure the clamping pressure applied by the flat plate-shaped member to the stack required when the electrochemical element generates electricity.

[0047] When the temperature changes from the low temperature when the electrochemical device does not generate power to the high temperature when the electrochemical device generates power, the stacked body and the sandwiching body expand, and the interval between the stacked body and the sandwiching body changes.

[0048] According to this characteristic configuration, the flat plate-shaped member is assembled in such a manner that the same or more tightening pressure is applied to the stack at a low temperature when the electrochemical element is not generating electricity than at a high temperature when generating electricity. Therefore, even if the interval between the stack and the clamping body changes due to thermal expansion, the flat plate-shaped member is roughly uniformly loaded with an appropriate tightening pressure along the plane of the stack. Therefore, it is possible to suppress the increase in internal resistance and the reduction in the sealing performance of the reaction gas.

[0049] [constitute]

[0050] The electrochemical module according to the present invention has a further characteristic configuration in which the thermal expansion coefficient of the flat plate-shaped member is larger than the thermal expansion coefficient of a member constituting the clamping body.

[0051] For example, if the thermal expansion amount of the flat plate member is smaller than that of the clamping body, if the distance between the stacked body and the clamping body increases due to thermal expansion, the flat plate member may not be able to apply appropriate clamping pressure to the stacked body even by utilizing its expansion.

[0052] According to this characteristic configuration, the thermal expansion coefficient of the flat plate-shaped member is greater than that of the clamping body. Therefore, the distance between the stacked body and the clamping body, which is expanded due to the expansion of the clamping body, can be compensated by the thermal expansion of the flat plate-shaped member. That is, even if the distance between the stacked body and the clamping body changes in a direction that is greatly widened due to thermal expansion, the flat plate-shaped member that is thermally expanded more can load the stacked body with an appropriate tightening pressure.

[0053] [constitute]

[0054] A further characteristic configuration of the electrochemical module according to the present invention is that the holder is formed of ferritic stainless steel, martensitic stainless steel, or a composite of ferritic stainless steel and ceramics.

[0055] According to this characteristic configuration, the thermal expansion coefficient of the above-mentioned material used in the clamping body is small. Therefore, by forming the clamping body from the above-mentioned material, when a high temperature is reached during power generation, for example, the thermal expansion amount of the clamping body can be suppressed to a small value. As a result, the widening of the gap between the stacked body and the clamping body caused by thermal expansion can be suppressed to a small value. Therefore, even in the case where the thermal expansion coefficient of the flat plate-shaped member is relatively small, an appropriate tightening pressure can be applied to the stacked body after the aforementioned gap change.

[0056] Furthermore, since the amount of thermal expansion of the holder is small, the positional displacement and damage of the substrate of the electrochemical device can be suppressed by the expansion of the holder.

[0057] [constitute]

[0058] A further characteristic configuration of the electrochemical module according to the present invention is that the flat plate-shaped member is formed of austenitic stainless steel.

[0059] According to this characteristic structure, the thermal expansion coefficient of the material used in the flat plate-shaped member is relatively large. Therefore, even if the interval between the stack and the clamp changes due to thermal expansion, the change of the interval can be compensated by the flat plate-shaped member with greater thermal expansion, and the stack can be loaded with appropriate tightening pressure.

[0060] [constitute]

[0061] A further characteristic configuration of the electrochemical module according to the present invention is that the flat plate-like member has a corrugated plate shape when viewed in a direction intersecting with a stacking direction of the stacked body.

[0062] According to this characteristic configuration, the flat plate-shaped member is in a corrugated shape, so that the flat plate-shaped member can have a moderate elastic force. In addition, the flat plate-shaped member contacts the stack and the clamp at a plurality of dispersed locations, so that the stack can be loaded with a tightening pressure in a substantially uniformly dispersed state.

[0063] [constitute]

[0064] A further characteristic configuration of the electrochemical module according to the present invention is that at least one of the first clamping body and the second clamping body is a part of a case surrounding the stacked body.

[0065] According to this characteristic configuration, at least one of the first and second sandwiching bodies is a part of the case, and thus it is possible to easily configure an integrated electrochemical module by surrounding at least one of the stacked bodies.

[0066] [constitute]

[0067] A further characteristic configuration of the electrochemical module according to the present invention is that the electrochemical element is a solid oxide fuel cell.

[0068] According to this characteristic configuration, the electrochemical element is a solid oxide fuel cell, and a high temperature of, for example, about 650°C to about 950°C is reached during power generation. Therefore, the stack and the clamp expand due to exposure to the high temperature. At this time, if a thermal expansion difference occurs between the thermal expansion of the stack and the thermal expansion of the clamp, the interval between the stack and the clamp is different when power generation is performed and when power is not performed.

[0069] The flat plate member uses its elastic force to apply appropriate clamping pressure to the stack between the clamps even when the gap between the stack and the clamp changes due to thermal expansion. This can suppress the increase of internal resistance and the reduction of sealing performance of reaction gas in the electrochemical module.

[0070] [constitute]

[0071] A further characteristic configuration of the electrochemical module according to the present invention is that the electrochemical element is a solid oxide electrolytic cell.

[0072] According to the above-mentioned characteristic configuration, an electrochemical element having excellent durability, reliability and performance can generate gas by electrolytic reaction as a solid oxide electrolytic cell, so a highly durable and high-performance solid oxide electrolytic cell can be obtained.

[0073] [constitute]

[0074] The electrochemical module assembly method according to the present invention is characterized in that:

[0075] In a stacked body, a flat plate-shaped member is arranged along at least one of a first plane in the stacking direction and a second plane opposite to the first plane, wherein a plurality of electrochemical elements including an electrolyte layer formed along a substrate and a first electrode and a second electrode respectively arranged on both sides of the electrolyte layer are stacked in a predetermined stacking direction;

[0076] A first flat plate-shaped clamping body is arranged along the first plane, and a second flat plate-shaped clamping body is arranged along the second plane.

[0077] The first clamping body and the second clamping body are fastened in the stacking direction in such a manner that the fastening pressure applied by the flat plate-shaped member to the stack when the electrochemical element is not generating electricity is equal to or greater than the fastening pressure applied by the flat plate-shaped member to the stack when the electrochemical element is not generating electricity.

[0078] According to this characteristic configuration, the flat plate-shaped member is assembled in such a manner that the same or more tightening pressure is applied to the stack at a low temperature when the electrochemical element is not generating electricity than at a high temperature when generating electricity. Therefore, even if the interval between the stack and the clamping body changes due to thermal expansion, the flat plate-shaped member is roughly uniformly loaded with an appropriate tightening pressure along the plane of the stack. Therefore, it is possible to suppress the increase in internal resistance and the reduction in the sealing performance of the reaction gas.

[0079] It should be noted that the configuration in which the first electrode and the second electrode are respectively arranged on both sides of the electrolyte layer includes any one of the configurations in which the first electrode is arranged in contact with the electrolyte layer and the configuration in which the first electrode is arranged facing the electrolyte layer via an interlayer. The relationship between the second electrode and the electrolyte layer is also the same. The interlayer includes, for example, an anti-reaction layer and an intermediate layer.

[0080] [constitute]

[0081] The electrochemical device according to the present invention is characterized in that:

[0082] The invention comprises at least the electrochemical module and a fuel converter, and comprises a fuel supply unit for flowing the reducing component gas from the fuel converter to the electrochemical module or flowing the reducing component gas from the electrochemical module to the fuel converter.

[0083] According to the above-mentioned characteristic configuration, an electrochemical module and a fuel converter are provided, and a fuel supply unit for circulating a gas containing a reducing component between the electrochemical module and the fuel converter is provided. Therefore, when the electrochemical module is operated as a fuel cell, if a configuration is set to generate hydrogen gas through a fuel converter such as a reformer from a natural gas supplied using an existing raw fuel supply infrastructure such as municipal gas, an electrochemical device having an electrochemical module with excellent durability, reliability and performance can be realized. In addition, it is easy to construct a system for recovering unused fuel gas discharged from the electrochemical module, so a highly efficient electrochemical device can be realized.

[0084] When the electrochemical module is operated as an electrolysis unit, a gas containing water vapor and carbon dioxide flows through the electrode layer, and a voltage is applied between the electrode layer and the counter electrode layer. - Reacts with water molecules H2O and carbon dioxide molecules CO2 to form hydrogen molecules H2, carbon monoxide CO and oxygen ions O 2- . Oxygen ion O 2- The oxygen ions O in the counter electrode layer move toward the counter electrode layer through the electrolyte layer. 2- Electrons are released to form oxygen molecules O2. Through the above reaction, water molecules H2O are electrolyzed into hydrogen H2 and oxygen O2. When a gas containing carbon dioxide molecules CO2 is circulated, it is electrolyzed into carbon monoxide CO and oxygen O2.

[0085] When a gas containing water vapor and carbon dioxide molecules CO2 is circulated, a fuel converter can be provided to synthesize various compounds such as hydrocarbons from hydrogen and carbon monoxide generated in the electrochemical module by the above electrolysis. The hydrocarbons generated by the fuel converter are circulated in the electrochemical module or taken out of the system and device through the fuel supply unit, so that they can be used as fuels or chemical raw materials for other purposes.

[0086] [constitute]

[0087] The electrochemical device according to the present invention is characterized in that:

[0088] The invention comprises at least the electrochemical module and a power converter for extracting electric power from the electrochemical module or for transmitting electric power to the electrochemical module.

[0089] According to the above-mentioned characteristic configuration, the power converter extracts the power generated by the electrochemical module, or flows power to the electrochemical module. Thus, as described above, the electrochemical module works as a fuel cell, or works as an electrolysis unit. Therefore, according to the above-mentioned configuration, an electrochemical module or the like that can improve the efficiency of converting chemical energy such as fuel into electrical energy, or converting electrical energy into chemical energy such as fuel, can be provided.

[0090] It should be noted that when an inverter is used as a power converter, for example, the electrical output obtained from an electrochemical module having excellent durability, reliability and performance can be boosted through the inverter, or direct current can be converted into alternating current. Therefore, it is easy to utilize the electrical output obtained from the electrochemical module, which is preferred.

[0091] [constitute]

[0092] The energy system according to the present invention is characterized in that:

[0093] The invention comprises the electrochemical device described above and an exhaust heat utilization unit for reusing the heat exhausted from the electrochemical device or the fuel converter.

[0094] According to the above-mentioned characteristic configuration, an energy system having excellent durability, reliability, and performance and excellent energy efficiency can be realized by including an electrochemical device and an exhaust heat utilization unit for reusing the heat exhausted from the electrochemical device or the fuel converter. It should be noted that a hybrid system with excellent energy efficiency can also be realized by combining with a power generation system that generates electricity by utilizing the combustion heat of unused fuel gas exhausted from the electrochemical device or the fuel converter. BRIEF DESCRIPTION OF THE DRAWINGS

[0095] Figure 1 is a cross-sectional view of an electrochemical module.

[0096] Figure 2 is a top view of the electrochemical module.

[0097] Figure 3 is a side view of the electrochemical module.

[0098] Figure 4 This is a schematic diagram of the electrochemical module.

[0099] Figure 5 This is a cross-sectional view of an electrochemical module according to another embodiment 1.

[0100] Figure 6 This is a cross-sectional view of an electrochemical module according to another embodiment 2.

[0101] Figure 7 yes Figure 6 Top view of the electrochemical module.

[0102] Figure 8 yes Figure 6 Side view of the electrochemical module.

[0103] Fig. 9 This is a schematic diagram of an electrochemical element.

[0104] Fig.10 yes Fig. 9 XX cross-section diagram in.

[0105] Fig.11 yes Fig. 9 XI-XI diagram in .

[0106] Fig.12 yes Fig. 9 Section XII-XII in FIG.

[0107] Fig.13 yes Fig. 9 Section XIII-XIII in FIG.

[0108] Fig.14 yes Fig. 9Section XIV-XIV in the figure.

[0109] Fig.15 yes Fig. 9 Section XV-XV in FIG.

[0110] Fig.16 yes Fig. 9 Section XVI-XVI in FIG.

[0111] Fig.17 yes Fig. 9 Section XVII-XVII in FIG.

[0112] Fig.18 This is an enlarged view of the key parts of the electrochemical reaction unit.

[0113] Fig.19 This is a schematic diagram of the energy system.

[0114] Fig. 20 It is an explanatory diagram of an electrochemical module according to another embodiment.

[0115] Fig.21 This is a schematic diagram of another energy system.

[0116] Fig. 22 is a schematic diagram of another electrochemical element.

[0117] Fig.23 yes Fig. 22 Section XXIII-XXIII in FIG.

[0118] Fig.24 yes Fig. 22 Panel XXIV-XXIV in the figure.

[0119] Fig.25 yes Fig. 22 Section XXV-XXV in.

[0120] Fig.26 yes Fig. 22 Section XXVI-XXVI in FIG.

[0121] Fig. 27 yes Fig. 22 Section XXVII-XXVII in FIG.

[0122] Fig.28 yes Fig. 22 Section XXVIII-XXVIII in FIG.

[0123] Fig.29 yes Fig. 22 Section XXIV-XXIV in.

[0124] Fig.30 yes Fig. 22 XXX-XXX cross-sectional view in FIG.

[0125] Fig.31 yes Fig. 22 Section XXXI-XXXI in FIG.

[0126] Fig.32 yes Fig. 22 Section XXXII-XXXII in FIG.

[0127] Fig.33 yes Fig. 22 Section XXXIII-XXXIII in FIG.

[0128] Fig.34 yes Fig. 22 Section XXXIV-XXXIV in FIG.

[0129] Fig.35 yes Fig. 22 Section XXXV-XXXV in FIG.

[0130] Fig.36 yes Fig. 22 Section XXXVI-XXXVI in FIG.

[0131] Fig.37 yes Fig. 22 Section XXXVII-XXXVII in FIG.

[0132] Fig.38 This is an enlarged view of the key parts of the electrochemical reaction unit.

[0133] Fig.39 It is an explanatory diagram of a supply structure and a discharge structure. DETAILED DESCRIPTION

[0134] [Implementation Method]

[0135] The following describes the electrochemical module M and the assembly method of the electrochemical module M according to the embodiment of the present invention. It should be noted that when indicating the positional relationship of the layers, for example, the electrolyte layer side observed from the electrode layer is referred to as "upper" or "upper side", and the first plate-like body side is referred to as "lower" or "lower side". In addition, the present invention can achieve the same effect even if the electrochemical module M is set in a vertical or horizontal direction, so "upper" and "lower" can be replaced by "left" and "right" respectively.

[0136] (1) Overall structure of the electrochemical module M

[0137] The overall structure of the electrochemical module M is described below. Figure 1As shown, the electrochemical module M includes an electrochemical element stack (stack) S and a substantially rectangular parallelepiped container (housing, first holder, second holder) 200 containing the electrochemical element stack S. Figure 4 ) is a component for generating electricity, formed as Figure 1 In the cross-sectional view of FIG. 1 , the electrochemical element stack S is a plate-shaped body extending from the front of the paper to the inside of the paper. Figure 1 In the cross-sectional view of FIG. , the electrochemical element A is stacked in the vertical stacking direction. In the present embodiment, SOFC (Solid Oxide Fuel Cell) is taken as an example for description.

[0138] Furthermore, the electrochemical module M includes a first gas supply unit 61 for supplying the first gas from the outside of the container 200 to the electrochemical element stack S, and a first gas discharge unit 62 for discharging the first gas after reacting in the electrochemical element stack S.

[0139] In the container 200, Figure 1~Figure 3 As shown, a second gas supply unit 71 is provided to supply the second gas from the outside of the container 200 to the electrochemical element stack S. The second gas reacted in the electrochemical element stack S is discharged to the outside from a second gas discharge unit 72 provided in the container 200 .

[0140] Here, the first gas is, for example, a reducing component gas such as fuel gas, and the second gas is an oxidizing component gas such as air.

[0141] In addition, the electrochemical module M Figure 1 In the cross-sectional view, there are plate members 240 with openings on both sides of the electrochemical element stack S. The plate member 240 with openings corresponds to the two sides of the electrochemical element stack S, and is a plate-shaped member extending along the stacking direction of the electrochemical element A. In order to prevent electrical short circuits (short circuits) in the electrochemical module M, an insulating material such as mica is preferably used. In the plate member 240 with openings, a plurality of openings 240a that penetrate along the plane direction of the electrochemical element stack S are formed.

[0142] Therefore, the electrochemical element stack S receives the supply of fuel gas from the first gas supply part 61, and receives the supply of air from the second gas supply part 71 via the opening 240a of the plate member 240 with an opening, so that the fuel gas and oxygen in the air undergo an electrochemical reaction to generate electricity. The fuel gas after the electrochemical reaction is discharged to the outside from the first gas exhaust part 62. In addition, the air after the electrochemical reaction is introduced into the second gas exhaust part 72 via the opening 240a of the plate member 240 with an opening, and is discharged to the outside from the second gas exhaust part 72.

[0143] It should be noted that, here, the plate members 240 with openings are provided adjacent to both side surfaces of the electrochemical element stack S, but this is not essential, and either one may be provided, or both may be omitted.

[0144] In addition, the electrochemical module M has an upper insulator 210T, an upper flat plate-shaped member 220T, and an upper plate (first clamp) 230T in order from the electrochemical element stack S side to the outside at the upper part of the electrochemical element stack S. Similarly, the electrochemical module M has a lower insulator 210B, a lower flat plate-shaped member 220B, and a lower plate (second clamp) 230B in order from the electrochemical element stack S side to the outside at the lower part of the electrochemical element stack S.

[0145] The electrochemical element stack S will be described in detail later.

[0146] (2) Insulators, flat plate members, plates and containers

[0147] Hereinafter, the insulator (upper and lower insulators 210T and 210B) 210, the flat plate-shaped member (upper and lower flat plate-shaped members 220T and 220B) 220, the plate (upper and lower plates 230T and 230B) 230, and the container 200 will be further described.

[0148] The upper insulator 210T is a plate-shaped member, and is disposed so as to cover the upper plane (first plane) of the electrochemical element stack S. The upper insulator 210T is formed of, for example, hard mica, and electrically insulates the electrochemical element stack S from the outside.

[0149] The upper flat plate-shaped member 220T is disposed on the upper portion of the upper insulator 210T. The upper flat plate-shaped member 220T is an elastic member, and in this embodiment, is formed as, for example, Figure 1 The corrugation extends along the plane of the electrochemical element stack S. Therefore, the upper flat plate-shaped member 220T is arranged so that the top 220Ta of the corrugation contacts the upper insulator 210T.

[0150] The thickness of the corrugated upper flat plate member 220T is not limited thereto, but is, for example, about 0.1 mm to 1 mm. The amplitude (height) of the corrugation is not limited thereto, but is, for example, about 1 mm to 10 mm.

[0151] The function of the upper flat plate-shaped member 220T will be described later.

[0152] The upper plate 230T is a plate-like member, which is arranged on the upper portion of the upper flat plate-like member 220T and is formed of a ceramic material having high bending strength at high temperatures, such as 99 alumina. The upper plate 230T is in contact with at least a portion of the upper flat plate-like member 220T. In this embodiment, the corrugated top 220Tb of the upper flat plate-like member 220T is in contact with the upper plate 230T.

[0153] The upper plate 230T and the lower plate 230B receive a predetermined clamping pressure from the container 200 to clamp the electrochemical element stack S, a pair of upper and lower insulators 210T and 210B, and upper and lower flat plate members 220T and 220B. Here, the clamping pressure refers to, for example, an average of 1 mm 2 Equal pressure per unit area.

[0154] The lower insulator 210B is arranged so as to cover the lower plane (second plane) of the electrochemical element stack S. The lower flat member 220B is arranged at the lower part of the lower insulator 210B, and the lower plate 230B is arranged at the lower part of the lower flat member 220B. The lower insulator 210B, the lower flat member 220B, and the lower plate 230B are respectively the same as the upper insulator 210T, the upper flat member 220T, and the upper plate 230T. It should be noted that the top 220Ba of the corrugated shape of the lower flat member 220B is in contact with the lower plate 230B, and the top 220Bb is in contact with the lower insulator 210B.

[0155] The container 200 containing the electrochemical element stack S is as follows: Figure 1~Figure 3 As shown, it is a substantially rectangular container. The container 200 includes a box-shaped upper cover (first clamping body) 201 opened at the bottom, and a lower cover (second clamping body) 203 opened at the top. A connecting portion 202 is provided on the end surface of the upper cover 201 opposite to the lower cover 203, and a connecting portion 205 is provided on the end surface of the lower cover 203 opposite to the upper cover 201. The connecting portion 202 and the connecting portion 205 are connected by, for example, welding, to form a rectangular space inside.

[0156] In this embodiment, if Figure 1 As shown, the depth of the lower cover 203 in the vertical direction (the stacking direction of the electrochemical element A) is deeper than the depth of the upper cover 201. However, as long as the upper cover 201 and the lower cover 203 can form a space inside as a whole, the depth relationship is not limited to this. For example, the depth of the upper cover 201 can also be deeper than that of the lower cover 203.

[0157] like Figure 1~Figure 3 As shown, a second gas supply portion 71 and a second gas exhaust portion 72 are formed at a central portion in the vertical direction of the container 200 and on a pair of opposing side walls of the lower cover 203 .

[0158] It should be noted that, here, the second gas supply part 71 and the second gas exhaust part 72 are formed on the lower cover 203. However, the formation positions of the second gas supply part 71 and the second gas exhaust part 72 are not limited thereto, and can be formed at any position of the container 200. The second gas supply part 71 and the second gas exhaust part 72 can be formed on the upper cover 201, for example.

[0159] Upper cover 201 Figure 1 , Figure 2 As shown, it has an opening 201c that is smaller than the outer edge of the upper cover 201. Figure 1 In the cross-sectional view, the end facing the inner side of the electrochemical element stack S adjacent to the opening 201c is branched into a first end 201a and a second end 201b. Furthermore, the first end 201a extends in the plane direction toward the inner direction of the container 200 by a predetermined length, and the second end 201b branches from the first end 201a and extends below the container 200 by a predetermined length. The first end 201a and the second end 201b form an approximately 90° angle in the cross-sectional view, forming an L-shaped corner. The corner of the L is at Figure 2 The inner side of the outer edge of the top view of the upper cover 201 shown in FIG. 201 is formed along the outer edge. Thus, through the terminal end of the first end 201a, as shown in FIG. Figure 1 , Figure 2 As shown, as mentioned above, an opening 201 c which is smaller than the outer edge of the upper cover 201 is formed on the upper surface of the upper cover 201 .

[0160] The lower cover 203 is similar to the upper cover 201. Figure 1 In the cross-sectional view shown in FIG. 1 , the first end portion 203a and the second end portion 203b are provided to form an L-shaped corner portion of approximately 90°. Figure 1 As shown, an opening 203 c is formed which is slightly smaller than the outer edge of the lower cover 203 .

[0161] like Figure 1As shown, the upper ends of a pair of plate members 240 with openings, the upper insulator 210T, the upper flat plate member 220T, and the upper plate 230T are embedded in the L-shaped corner formed by the first end 201a and the second end 201b of the upper cover 201. Specifically, in the upper plate 230T along the plane direction of the electrochemical element stack S, the upper surface of its outer peripheral end is in contact with the lower surface of the first end 201a (a part of the inner surface of the corner of the L) and supported. In addition, in the plate member 240 with openings along the side of the electrochemical element stack S, the outer surface of its upper end is in contact with the inner side surface of the second end 201b (a part of the inner surface of the corner of the L) and supported. The upper flat plate member 220T and the upper insulator 210T are supported by the L-shaped corner formed by the first end 201a and the second end 203b via the upper plate 230T and the plate member 240 with openings.

[0162] Similarly, the lower ends of the pair of opening plate members 240 , the lower insulator 210B, the lower flat plate member 220B, and the lower plate 230B are embedded in a pair of L-shaped corners facing the plane direction of the lower cover 203 .

[0163] In addition, the upper surface of the electrochemical element stack S is supported by the upper cover 201 via the upper plate 230T, the upper flat member 220T, and the upper insulator 210T. In addition, the lower surface of the electrochemical element stack S is supported by the lower cover 203 via the lower plate 230B, the lower flat member 220B, and the lower insulator 210B.

[0164] In such a configuration, the upper cover 201 and the lower cover 203 are connected by, for example, welding, the connecting portion 202 and the connecting portion 205 in a state where the electrochemical element stack S, the upper and lower insulators 210T and 210B, the upper and lower flat plate members 220T and 220B, the upper and lower plates 230T and 230B, etc. are sandwiched by the upper and lower parts. During this connection, the upper cover 201 and the lower cover 203 are connected by applying a predetermined tightening pressure to the electrochemical element stack S, etc. That is, in a state where the upper cover 201 and the lower cover 203 are connected, a predetermined tightening pressure is applied to the electrochemical element stack S, the upper and lower insulators 210T and 210B, the upper and lower flat plate members 220T and 220B, and the upper and lower plates 230T and 230B.

[0165] It should be explained, such as Figure 3As shown, an opening 203e is formed on the side of the lower cover 203. Therefore, a part of the side of the electrochemical element stack S is exposed from the opening 203e. In addition, by forming the aforementioned openings 201c, 203c, and opening 203e on the container 200, the container 200 can be made lightweight and the material required for the container 200 can be reduced. It should be noted that in the case where an electrical short circuit (short circuit) may occur due to contact between the side of the electrochemical element stack S and the upper cover 201 or the lower cover 203 or both, a side insulator 245 made of a material such as mica is provided between the side of the electrochemical element stack S and the upper cover 201 or the lower cover 203.

[0166] (3) The composition and function of the flat plate-shaped member and its related members

[0167] Next, the configuration and function of the flat plate-shaped member (upper and lower flat plate-shaped members 220T and 220B) 220 and members associated therewith will be further described.

[0168] As described above, when the upper cover 201 and the lower cover 203 are connected, the electrochemical element stack S and the upper and lower insulators 210T and 210B are loaded with a predetermined tightening pressure via the upper and lower flat plate members 220T and 220B, and are clamped by the upper and lower plates 230T and 230B.

[0169] (3-1) Configuration of the flat plate-shaped member and its related members

[0170] In this embodiment, the flat plate-shaped member 220 is formed of a heat expansion member that expands by heat. It is preferred that the thermal expansion coefficient of the flat plate-shaped member 220 is greater than the thermal expansion coefficient of the members constituting the electrochemical element stack S and the container 200. As a material for such a flat plate-shaped member 220, for example, austenitic stainless steel can be cited.

[0171] Austenitic stainless steel has a high thermal expansion coefficient. For example, the thermal expansion coefficient of austenitic stainless steel is about 23.8×10 -6 / ℃, the thermal expansion coefficient of austenitic stainless steel is about the same as that of aluminum. The thermal expansion coefficient of austenitic stainless steel SUS303 and SUS304 is about 17.3×10 -6 / ℃, SUS316 is about 16×10 -6 / °C. However, the material of the flat plate-shaped member 220 is not limited thereto, and it is preferable to select a member having a higher thermal expansion coefficient than the container 200 and having excellent corrosion resistance.

[0172] In addition, it is preferred that the thermal expansion coefficient of the container 200 is smaller than the thermal expansion coefficient of the flat plate-shaped member 220. The container 200 is arranged adjacent to the flat plate-shaped member 220 via the plate 230. Furthermore, by combining the lower cover 203 and the upper cover 201 of the container 200, a tightening pressure is applied to the electrochemical element stack S via the flat plate-shaped member 220. Examples of materials for such a container 200 include ferritic stainless steel, martensitic stainless steel, or composites thereof with ceramics. These materials have a smaller thermal expansion coefficient than austenitic stainless steel. The thermal expansion coefficient of ferritic stainless steel is about 11×10 -6 / ℃. In addition, the thermal expansion coefficient of martensitic stainless steel is about 10.4×10 -6 / ℃, SUS410 and SUS440C are about 10.1×10 -6 / °C. However, the container 200 is not limited thereto, and it is preferable to select a material having a smaller thermal expansion coefficient than the flat plate-shaped member 220 and having excellent corrosion resistance.

[0173] The material of the electrochemical element stack S is preferably the same material as the container 200. In other words, the materials of the electrochemical element stack S and the container 200 preferably have the same thermal expansion coefficient as the container 200. In this case, the substrate of the electrochemical element stack S and the container 200 thermally expand at the same level when, for example, the electrochemical element A reaches high temperature for power generation. Therefore, for example, the thermal expansion difference between the substrate of the electrochemical element A and the container 200 can be suppressed to a small value, and damage to the substrate can be suppressed.

[0174] (3-2) Assembly method of electrochemical module M and compression displacement of flat plate member during assembly

[0175] (a) Assembly method of electrochemical module M

[0176] Next, a method for assembling the electrochemical module M will be described.

[0177] A plurality of electrochemical elements A are stacked to prepare an electrochemical element stack S. The structure and manufacturing method of the electrochemical element stack S will be described later.

[0178] In addition, a container 200 for accommodating the electrochemical element stack S is prepared. Although the container 200 is not limited thereto, it can be manufactured using, for example, a lost wax casting method. When using the lost wax casting method, a hollow mold corresponding to the shape of the container 200 is manufactured by, for example, a thermoplastic material containing beeswax, rosin, etc. The mold is covered with a refractory material containing silica sand, lime powder, etc. Thereafter, the mold covered with the refractory material is heated, and the mold composed of the thermoplastic material is dissolved. Thus, a cavity corresponding to the mold of the shape of the molded container 200 is formed inside the refractory material. The material of the container 200 is injected into the cavity, and after solidification, the refractory material is removed. Thus, a container 200 having an upper cover 201 and a lower cover 203 is manufactured by the lost wax casting method. It should be noted that the upper cover 201 and the lower cover 203 can be manufactured separately.

[0179] Next, for example, a pair of plate members 240 with openings are arranged on both sides of the electrochemical element stack S, and the insulator 210, the flat plate-shaped member 220, and the plate 230 are accommodated in the lower cover 203 in a state of being arranged in sequence on the upper plane and the lower plane of the electrochemical element stack S. The lower cover 203 is covered by the upper cover 201, and the position is adjusted in a manner that a predetermined tightening pressure is applied to the electrochemical element stack S, and the lower cover 203 and the upper cover 201 are welded or the like to be combined. In this way, the electrochemical module M is assembled.

[0180] As described above, when the container 200 is manufactured using the lost wax casting method, it is possible to achieve cost reduction through thinning, precision, and mass production.

[0181] Furthermore, by forming the container 200 in a box shape, in the present embodiment, a space for a line for supplying air from the second gas supply unit 71 to the electrochemical element stack S can be provided.

[0182] (b) Compression displacement of the flat plate member during assembly

[0183] When the lower cover 203 and the upper cover 201 are combined during assembly of the electrochemical module M, a predetermined clamping pressure is applied to the electrochemical element stack S. The clamping pressure is applied by applying a predetermined compressive displacement L to the flat plate-shaped member 220 .

[0184] Hereinafter, the compression displacement L will be described.

[0185] Hereinafter, the container 200 is formed of a predetermined material A, the main parts such as the substrate in the electrochemical element stack S are formed of a predetermined material B, and the flat plate member 220 is formed of a predetermined material C. The thermal expansion coefficient of the material C is greater than that of the material A and the material B.

[0186] Here, the spring constant of the flat plate-shaped member 220 at room temperature (20° C.) is K20. The spring constant K20 is calculated using, for example, the plate thickness of the flat plate-shaped member 220, the amplitude (height) of the corrugated shape, the pitch of the wave, and the like.

[0187] Furthermore, the spring constant at the temperature (for example, 700° C.) when power is generated by the electrochemical element A is K700. It should be noted that K700 is, for example, about 75% of K20.

[0188] Here, the clamping pressure per unit area required for the electrochemical element stack S during power generation (for example, at 700° C.) is denoted as P. Here, P is not limited thereto, but is, for example, about 1 to 3 kgf / cm 2 If the area of ​​the electrochemical device stack S is represented by SB, the weight force F is F=P×SB.

[0189] In addition, when the temperature rises from room temperature (20°C) to a high temperature during power generation (e.g., 700°C), in the weighted direction (here, the stacking direction of the electrochemical element A), the thermal expansion length of the container 200 is recorded as LA, the thermal expansion length of the electrochemical element stack S is recorded as LB, and the thermal expansion length of the flat member 220 is recorded as LC.

[0190] The difference ΔG between the thermal expansion lengths of the container 200 and the electrochemical element stack S is ΔG=LA-LB. Here, as the difference ΔG in the thermal expansion length, the difference in the thermal expansion lengths of the container 200, the electrochemical element stack S, and the flat member 220 can be calculated. In this case, ΔG=LA-(LB+LC). Hereinafter, ΔG=LA-LB is used by assuming that the flat member 220 does not thermally expand, so that even after the container 200 and the like are thermally expanded, the appropriate tightening pressure can be more reliably loaded by the compressive displacement L of the flat member 220 during assembly.

[0191] Here, in order to maintain the clamping pressure P per unit area at a high temperature (eg, 700° C.) during power generation, the compressive displacement L of the flat plate-shaped member 220 at room temperature (20° C.) is calculated by the following formula.

[0192] L=P×SB / (K700)+ΔG

[0193] According to the above, after the electrochemical element stack S and the flat plate-shaped member 220 are accommodated in the container 200, the lower cover 203 and the upper cover 201 are sealed by welding, etc. by adjusting the bonding distance, etc. in a manner that the above-calculated compression displacement L is given to the flat plate-shaped member 220. Thus, the electrochemical element stack S can be loaded with a predetermined tightening pressure.

[0194] (3-3) Function of the flat plate member

[0195] As described above, the flat plate-shaped member 220 formed of a thermal expansion member is disposed on the upper and lower planes of the electrochemical element stack S, and a predetermined clamping pressure is applied from the upper and lower plates 230 to elastically support the electrochemical element stack S.

[0196] Here, for example, if at least one of the electrochemical element stack S and the container 200 expands from a low temperature state (e.g., about 20°C at room temperature, etc.) when the electrochemical element A is not generating electricity to a high temperature state (e.g., about 650°C to about 950°C, etc.) when the electrochemical element A is generating electricity, the electrochemical element stack S and the container 200 expand. At this time, if a thermal expansion difference occurs between the electrochemical element stack S and the container 200, the distance between the electrochemical element stack S and the container 200 is different when generating electricity (at high temperature) and when not generating electricity (at low temperature).

[0197] According to the above configuration, the flat plate-shaped member 220 is a thermal expansion member, and therefore the flat plate-shaped member 220 also thermally expands due to the high temperature of the electrochemical element A during power generation. Therefore, even if the interval between the electrochemical element stack S and the container 200 changes due to thermal expansion, the flat plate-shaped member 220 uses the elastic force generated by the thermal expansion of the flat plate-shaped member 220 itself and the elastic force generated by the pre-given compression displacement L to make the plate 230 act as a pressing surface, and load the electrochemical element stack S with an appropriate tightening pressure.

[0198] That is, the change in the interval between the electrochemical element stack S and the container 200 due to thermal expansion can be compensated by the change caused by the thermal expansion of the flat plate-shaped member 220. Therefore, even after the aforementioned interval change, an appropriate tightening pressure is applied to the electrochemical element stack S. For example, the interval between the electrochemical element stack S and the container 200 increased due to thermal expansion is compensated by the thermal expansion of the flat plate-shaped member 220, and an appropriate tightening pressure is applied to the electrochemical element stack S.

[0199] Furthermore, the flat plate-shaped member 220 is arranged along the plane of the electrochemical element stack S and the plane of the plate 230, so even after the aforementioned interval changes, an appropriate tightening pressure is roughly uniformly applied along the plane of the electrochemical element stack S. Therefore, in the electrochemical module M, the reduction in the contact area between the electrochemical elements A can be suppressed, and the internal resistance can be reduced. In addition, the electrochemical elements A can be properly contacted and the airtightness can be maintained, so the leakage of fuel gas to the outside of the electrochemical element A can be suppressed, and the reduction in the sealing of the reaction gas can be suppressed.

[0200] In this manner, a small, lightweight, and low-cost electrochemical module can be realized in which the electrochemical element stack S and the like can be appropriately fastened even when the electrochemical element stack S and the like expands.

[0201] In particular, in the above-mentioned embodiment, the thermal expansion coefficient of the flat plate-shaped member 220 is greater than the thermal expansion coefficient of the member constituting the container 200. In order to achieve this relationship, as the material of the flat plate-shaped member 220, for example, austenitic stainless steel is used, and as the material of the container 200, ferritic stainless steel, martensitic stainless steel, or a composite of these and ceramics is used. In addition, as the material of the electrochemical element stack S, the same material as the material of the container 200 can be used.

[0202] Here, as described above, in the electrochemical element stack S, when the low temperature state without power generation reaches the high temperature state during power generation, at least one of the electrochemical element stack S and the container 200 thermally expands, and a difference occurs between the amount of thermal expansion of the electrochemical element stack S and the amount of thermal expansion of the container 200. In this way, the distance between the electrochemical element stack S and the container 200 at high temperature is increased compared to that at low temperature. For example, when the amount of thermal expansion of the container 200 is large, the distance between the electrochemical element stack S and the container 200 is further increased.

[0203] In the present embodiment, as described above, the thermal expansion coefficient of the flat plate-shaped member 220 is greater than the thermal expansion coefficient of the member constituting the container 200. Therefore, in particular, the interval between the electrochemical element stack S and the container 200, which is expanded due to the expansion of the container 200, can be compensated by the thermal expansion of the flat plate-shaped member 220. That is, even if the interval between the electrochemical element stack S and the container 200 changes in a direction of significant widening due to thermal expansion, the aforementioned interval can be compensated by the flat plate-shaped member 220 that is thermally expanded more. Therefore, even after the interval changes, by utilizing the elastic force of the compression displacement given in advance to the flat plate-shaped member 220 and the elastic force generated by the thermal expansion of the flat plate-shaped member 220 itself, it is possible to load an appropriate tightening pressure roughly uniformly along the plane of the electrochemical element stack S.

[0204] It should be noted that when the thermal expansion coefficient of the container 200 is small, for example, when a high temperature is reached during power generation, the thermal expansion amount of the container 200 can be suppressed to be small. As a result, the widening of the gap between the electrochemical element stack S and the container 200 due to thermal expansion can be suppressed to be small. Therefore, even when the thermal expansion coefficient of the flat plate-shaped member 220 is small, after the above-mentioned gap change, it is possible to load an appropriate tightening pressure substantially uniformly along the plane of the electrochemical element stack S.

[0205] Furthermore, when the amount of thermal expansion of the container 200 is small, positional displacement, damage, etc. of the substrate of the electrochemical element A can be suppressed by the expansion of the container 200 .

[0206] In the above embodiment, the flat plate member 220 is formed in a corrugated shape. Therefore, the corrugated tops of the flat plate member 220 contact the plane of the plate 230 and the plane of the electrochemical element stack S alternately via the insulator 210 at a plurality of dispersed locations.

[0207] Here, if the interval between the electrochemical element stack S and the container 200 changes due to the expansion of at least one of the electrochemical element stack S and the container 200, the extrusion force applied to the flat member 220 also changes due to the change in the interval. The changing extrusion force is elastically borne in a state of being roughly uniformly dispersed along the plane of the electrochemical element stack S and the plane of the plate 230 through the flat member 220. The reason is that, as mentioned above, the flat member 220 contacts the plane of the electrochemical element stack S and the plane of the plate 230 at multiple dispersed locations. In addition, in the case of thermal changes in the flat member 220, the change in the interval between the electrochemical element stack S and the container 200 is borne at the aforementioned multiple locations by the thermal expansion and elasticity of the flat member 220 itself.

[0208] Therefore, even if the interval between the electrochemical element stack S and the container 200 changes due to the expansion of the electrochemical element stack S, etc., the flat plate-shaped member 220 can be used to roughly uniformly apply a moderate tightening pressure in the stacking direction along the plane of the electrochemical element stack S. As a result, in the electrochemical module M, an increase in internal resistance and a decrease in sealing performance of the reaction gas can be suppressed, and miniaturization and lightness can be achieved.

[0209] In addition, in the present embodiment, the electrochemical element stack S is composed of a SOFC as an electrochemical element. The temperature of the SOFC during power generation reaches a high temperature of about 650°C to about 950°C. Therefore, the expansion amount of the electrochemical element stack S and the container 200, etc., increases by reaching a high temperature (e.g., about 650°C to about 950°C, etc.) during power generation from a low temperature (e.g., about 20°C at room temperature, etc.) during non-power generation. In the present embodiment, the flat member 220 utilizes the change in elastic force caused by the thermal expansion of the flat member 220 itself, and can use the plate 230 as a pressing surface to load the electrochemical element stack S with appropriate tightening pressure. Therefore, in SOFCs that generate electricity in high temperature regions, this embodiment can also be applied to load the electrochemical element stack S with appropriate tightening pressure.

[0210] Further explanation is given for miniaturization of the electrochemical module M. For example, in the case of a configuration in which a tightening pressure is applied to the electrochemical element stack S by tightening the periphery of a pair of thick clamping plates, a large tightening bolt using a spring needs to be arranged outside the electrochemical module M as a tightening member. However, in the above-mentioned embodiment, only the flat plate-shaped member 220 is arranged inside the electrochemical module M, and the electrochemical module M can be miniaturized.

[0211] In addition, when a large protrusion such as a fastening bolt is arranged outside the electrochemical module M, heat is easily released during power generation through the protrusion of the electrochemical module M. The flat plate member 220 of this embodiment is arranged inside the electrochemical module M, so that the heat release surface can be reduced and the power generation efficiency of the electrochemical module M can be improved.

[0212] In addition, in the present embodiment, the tightening pressure is adjusted by the flat plate-shaped member 220, so compared with the case where the tightening pressure of the electrochemical element stack S is adjusted using a large number of tightening bolts, etc., the labor required for adjusting the tightening pressure can be greatly reduced. For example, when the electrochemical element stack S is tightened using a large number of tightening bolts, it is necessary to adjust the pressure while managing the torque of the multiple bolts. However, when the flat plate-shaped member 220 of the present embodiment is used, the flat plate-shaped member 220 roughly evenly loads the tightening pressure on the plane of the electrochemical element stack S, so there is no need for the complex torque management described above.

[0213] (4) Specific structure of electrochemical module M

[0214] Next, use Figure 1 and Figure 4 , the specific structure of the electrochemical module M is described. Figure 1 The details of the electrochemical device stack S are shown in Figure 1 .

[0215] like Figure 1 and Figure 4 As shown, the electrochemical module M has: a container 200 (upper cover 201 and lower cover 203), which contains an electrochemical element stack S; a first gas supply part 61, which supplies a first gas to the internal flow path A1 from the outside of the container 200 via the supply path 4; a first gas exhaust part 62, which exhausts the first gas after the reaction; a second gas supply part 71, which supplies a second gas to the flow part A2 from the outside of the container 200; a second gas exhaust part 72, which exhausts the second gas after the reaction; and, an output part 8, which obtains an output accompanying the electrochemical reaction in the electrochemical reaction part 3;

[0216] The container 200 includes a distribution chamber 9 for distributing and supplying the second gas supplied from the second gas supply unit 71 to the flow portion A2.

[0217] The distribution chamber 9 is a space located on the side of the electrochemical element stack S where the second gas is supplied to the electrochemical element stack S.

[0218] The flow portion A2 is opened on the space side and communicates with the space.

[0219] The electrochemical element stack S is housed relative to the container 200 in a state of being clamped by a pair of current collectors 81, 82, and an output portion 8 is extended on the current collectors 81, 82 to be freely connected to a power supply object outside the container 200. At the same time, at least one of the current collectors 81, 82 is electrically insulated relative to the container 200, and the first gas is contained in a manner that is airtight relative to the container 200.

[0220] Thus, the electrochemical module M is supplied with fuel gas from the first gas supply unit 61 and air from the second gas supply unit 71, so that the fuel gas is Figure 1 , 4 The air enters as shown by the dotted arrows and the air enters as shown by the solid arrows.

[0221] The fuel gas supplied from the first gas supply unit 61 is guided to the supply path 4 from the first penetration portion 41 of the uppermost electrochemical element A of the electrochemical element stack S, and flows from the supply path 4 partitioned by the first annular seal portion 42 to the internal flow paths A1 of all the electrochemical elements A. In addition, the air supplied from the second gas supply unit 71 flows into the flow portion A2 formed between the electrochemical elements A after temporarily flowing into the distribution chamber 9.

[0222] Furthermore, if the second plate-like body 2 (a part of the plate-like support body 10) is used as a reference, the portion of the corrugated second plate-like body 2 that bulges out from the first plate-like body 1 (a part of the plate-like support body 10) forms an internal flow path A1 between the first plate-like body 1 and the second plate-like body 2, and is in contact with the electrochemical reaction portion 3 of the adjacent electrochemical element A to be electrically connected. On the other hand, the portion of the corrugated second plate-like body 2 that contacts the first plate-like body 1 is electrically connected to the first plate-like body 1, and a flow portion A2 is formed between the electrochemical reaction portion 3 of the electrochemical element A adjacent to the second plate-like body 2.

[0223] exist Fig.18 In a part of the drawing, there is a portion where the electrochemical element A including the cross section of the internal flow path A1 and the electrochemical element A including the cross section of the flow section A2 are shown side by side for convenience, but the fuel gas supplied from the first gas supply unit 61 reaches the distribution section A12 (refer to Fig. 9, 12, 15), flows along the width direction of one end side through the distribution portion A12, and reaches each auxiliary flow path A11 in the internal flow path A1 (refer to Fig. 9 , Fig.11 , Fig.15 In this case, the first gas can be evenly distributed to the plurality of sub-flow paths A11 from the distribution portion A12, and electrochemical output can be evenly generated in each electrochemical element.

[0224] In this way, the fuel gas entering the internal flow path A1 can enter the electrode layer 31 and the electrolyte layer 32 through the gas flow allowing portion 1A. In addition, the fuel gas further advances in the internal flow path A1 together with the fuel gas that has completed the electrochemical reaction, passes through the confluence portion A13 and the second penetration portion 51, and advances in the discharge path 5 formed by the second annular sealing portion 52, and is discharged from the first gas discharge portion 62 to the outside of the container 200 together with the fuel gas that has completed the electrochemical reaction from other electrochemical elements A.

[0225] On the other hand, the air supplied from the second gas supply unit 71 enters the circulation unit A2 via the distribution chamber 9, and can enter the counter electrode layer 33 and the electrolyte layer 32. In addition, the air, together with the air that has finished the electrochemical reaction, further advances in the circulation unit A2 along the electrochemical reaction unit 3, and is discharged from the second gas discharge unit 72 to the outside of the container 200.

[0226] According to the flow of the fuel gas and air, the electricity generated in the electrochemical reaction unit 3 is connected in series between the collectors 81 and 82 through the contact between the electrochemical reaction unit 3 of the adjacent electrochemical element A and the second plate-like body 2, forming a form in which a synthetic output is extracted from the output unit 8.

[0227] The structure of the electrochemical element stack S will be described in detail later.

[0228] (5) Deformation example of flat plate member

[0229] (a) In the above, the flat plate-shaped member 220 is a thermal expansion member that expands due to heat. However, the flat plate-shaped member 220 is not limited to a thermal expansion member as long as it can roughly uniformly load the tightening pressure on the plane of the electrochemical element stack S when the electrochemical element stack S and the container 200 expand and contract, etc. For example, the flat plate-shaped member 220 can be a member with a small thermal expansion coefficient but a certain degree of elasticity.

[0230] The elastic flat plate member 220 is arranged along the upper and lower planes of the electrochemical device stack S. The flat plate member 220 is loaded with a predetermined clamping pressure from the container 200 via the upper and lower plates 230 to elastically support the electrochemical device stack S.

[0231] Here, when at least one of the electrochemical element stack S and the container 200 expands, the interval between the electrochemical element stack S and the container 200 may change before and after the expansion of the electrochemical element stack S. The flat plate-shaped member 220 has elastic force, so even when the interval between the electrochemical element stack S and the container 200 changes, the electrochemical element stack S is elastically clamped in the container 200 by its elastic force. That is, the flat plate-shaped member 220 receives the tightening pressure from the container 200 and elastically clamps the electrochemical element stack S between the pair of plates 230.

[0232] More specifically, if the interval between the electrochemical element stack S and the container 200 changes due to the expansion of at least one of the electrochemical element stack S and the container 200, the compressive force applied to the flat plate-shaped member 220 also changes due to the change in the interval. The changing compressive force is elastically received by the flat plate-shaped member 220 arranged along the plane of the electrochemical element stack S and the plane of the plate 230 in a state of being substantially uniformly dispersed along the substantially entire plane of the electrochemical element stack S and the plane of the plate 230.

[0233] Therefore, even if the distance between the electrochemical element stack S and the container 200 changes due to expansion of the electrochemical element stack S, etc., the flat plate member 220 can apply an appropriate tightening pressure in the stacking direction substantially uniformly along the plane of the electrochemical element stack S.

[0234] In this way, by configuring a flat plate-like member 220 between the plane of the electrochemical element stack S and the plane of the plate 230, along the plane of the electrochemical element stack S and the plate 230, and storing it in a container 200, this simple structure can form an electrochemical module M that takes into account the expansion of the electrochemical element stack S, etc.

[0235] It should be noted that, when the flat plate-shaped member 220 is a member with a low thermal expansion coefficient, when the flat plate-shaped member 220 and the electrochemical element stack S are accommodated in the container 200 and assembled, it is preferable to increase the fastening pressure compared to the case where the flat plate-shaped member 220 is a member with a high thermal expansion coefficient. In this case, during assembly, a large repulsive force is generated in the flat plate-shaped member 220 by the large fastening pressure. Therefore, the interval between the electrochemical element stack S and the container 200 is widened due to the expansion of the electrochemical element stack S, etc., and even if the fastening pressure is reduced to a certain extent, it is possible to give a moderate fastening pressure to the electrochemical element stack S.

[0236] (b) In the above, the upper and lower flat plate-shaped members 220T and 220B are provided, but it is also possible to provide only one of the flat plate-shaped members 220. However, when the upper and lower flat plate-shaped members 220T and 220B are provided, the electrochemical element stack S can be loaded with a tightening pressure from the upper and lower parts through the flat plate-shaped member 220, so that the tightening pressure can be loaded more uniformly on the plane of the electrochemical element stack S, which is preferred.

[0237] (c) In the above, the flat plate-like member 220 has a corrugated shape, but the present invention is not limited thereto and other structures may be adopted in which the flat plate-like member 220 is in contact with the electrochemical element stack S and the plate 230 at multiple locations. For example, the flat plate-like member 220 may have a metal honeycomb shape.

[0238] Furthermore, the flat plate-like member 220 may be in contact with only one of the plane of the electrochemical element stack S and the plane of the plate 230 at a plurality of dispersed locations.

[0239] For example, the flat plate-shaped member 220 may contact the plane of the electrochemical element stack S at a plurality of dispersed locations and may contact the plane of the plate 230. In this case, the flat plate-shaped member 220 receives the load force generated by the expansion of the electrochemical element stack S etc. in a dispersed manner at the portion in contact with the electrochemical element stack S.

[0240] In addition, for example, the flat plate-shaped member 220 may be in contact with the plane surface of the electrochemical element stack S and in contact with the plane of the plate 230 at multiple locations. In this case, the portion of the flat plate-shaped member 220 in contact with the plane of the plate 230 will bear the load force generated by the expansion of the electrochemical element stack S, etc. in a dispersed manner.

[0241] (d) In the above, the thermal expansion coefficient of the flat plate-shaped member 220 is greater than the thermal expansion coefficient of the members constituting the container 200. However, as long as the distance between the electrochemical element stack S and the container 200 caused by thermal expansion can be compensated by the expansion of the flat plate-shaped member 220, the relationship of thermal expansion coefficient is not limited to this.

[0242] For example, the thermal expansion coefficient of the flat plate-shaped member 220 may be approximately the same as the thermal expansion coefficient of the members constituting the container 200 , or may be smaller.

[0243] (e) In the above description, the flat plate member 220 is described for adjusting the change in the distance between the electrochemical device stack S and the container 200 due to expansion. However, the flat plate member 220 can also be used for the change in the distance between the electrochemical device stack S and the container 200 due to contraction.

[0244] (f) In the above, the flat plate member 220 can also withstand the expansion and contraction of the electrochemical element stack S and the container 200 caused not only by temperature changes associated with power generation, but also by changes such as vibration applied to the electrochemical module M, external pressure, humidity and external temperature.

[0245] (g) In the above, the electrochemical module M is provided with functional layers such as the insulator 210 having insulating properties. The electrochemical module M may be provided with another functional layer in addition to or in place of the functional layers described above.

[0246] (h) In the above description, the lower cover 203 and the upper cover 201 are joined by welding. However, the joining of the lower cover 203 and the upper cover 201 is not limited to welding, and they may be joined by bolts or the like, for example.

[0247] (6) Another Electrochemical Module M

[0248] Hereinafter, an electrochemical module M having a different form from the electrochemical module M of the above-described embodiment will be described by taking another form 1 and another form 2 as examples.

[0249] (6-1) Another method 1

[0250] In the electrochemical module M1 according to another embodiment 1, Figure 5 Another embodiment 1 involves an electrochemical module M1 and Figure 1 The electrochemical module M of the embodiment 1 is different in that a flat plate-shaped member 320 is provided in addition to the flat plate-shaped member 220. That is, in the electrochemical module M1 according to the other embodiment 1, two flat plate-shaped members 220 and 320 are provided.

[0251] like Figure 5 As shown, the electrochemical module M1 has an upper insulator 210T, an upper flat plate-shaped member 320T, an upper flat plate-shaped member 220T, and an upper plate 230T in order from the side of the electrochemical element stack S to the outside. Similarly, the electrochemical module M1 has a lower insulator 210B, a lower flat plate-shaped member 320B, a lower flat plate-shaped member 220B, and a lower plate 230B in order from the side of the electrochemical element stack S to the outside.

[0252] Figure 5 In the embodiment, the flat plate-shaped member 320 (upper and lower flat plate-shaped members 320T and 320B) is a flat plate-shaped member such as a metal honeycomb shape. On the other hand, the flat plate-shaped member 220 (upper and lower flat plate-shaped members 220T and 220B) is a flat plate-shaped member such as a corrugated shape. The electrochemical module M1 has the same effect as the flat plate-shaped member 320 and the flat plate-shaped member 220. Figure 1The other components of the electrochemical module M1 are the same as those of Figure 1 The electrochemical module M is the same as that of FIG. 1 , so the description is omitted.

[0253] It should be explained that Figure 5 In the electrochemical module M1, the flat plate member 320 may be a flat plate member having a corrugated shape, and the flat plate member 220 may be a flat plate member having a metal honeycomb shape.

[0254] (6-2) Another method 2

[0255] In another embodiment 2, the electrochemical module M2 is used. Figure 6 Another embodiment 2 involves an electrochemical module M2 and Figure 5 The electrochemical module M is different mainly in that an upper surface portion 201d and a lower surface portion 203d are provided in a container 200, and the upper and lower plates 230T and 230B are omitted.

[0256] Further, in the electrochemical module M2, as Figure 7 and Figure 8 As shown, the lower cover 203 and the upper cover 201 are connected by bolts. Figure 5 The electrochemical module M is different from that of the embodiment of the present invention. Specifically, the edge of the lower cover 203 is opposite to the edge of the upper cover 201, and multiple bonding members 250 are bonded at multiple locations of the edge. The bonding member 250 is composed of a bolt 251 having a head and a shaft and a nut 253. The shaft of the bolt 251 is inserted into the through holes of the edge of the lower cover 203 and the edge of the upper cover 201, and the nut 253 is bonded to the bolt 251. As a result, the edge of the lower cover 203 is bonded to the upper cover 201.

[0257] However, the lower cover 203 and the upper cover 201 may be Figure 5 They are also joined by welding.

[0258] If for Figure 6 To further describe, the upper cover 201 has an upper surface portion 201d along the plane direction of the electrochemical element stack S. Figure 5 Similarly, the upper cover 201 has a first end 201a and a second end 201b. Also, the upper surface portion 201d extends continuously from the inner terminal of the first end 201a. At a predetermined position between the first end 201a and the upper surface portion 201d, as shown in FIG. Figure 6~Figure 8 As shown, a cylindrical portion 201e is provided which respectively constitutes the first gas supply portion 61 and the first gas discharge portion 62. Figure 6 The other components of the upper cover 201 are Figure 5 The upper cover 201 is the same.

[0259] On the other hand, the lower cover 203 has a lower surface portion 203 d extending along the plane direction of the electrochemical element stack S. Figure 8 The other components of the lower cover 203 are Figure 7 The lower cover 203 is the same.

[0260] In addition, the electrochemical module M2 has an upper insulator 210T, an upper flat plate-shaped member 320T such as a metal honeycomb shape, and an upper flat plate-shaped member 220T such as a corrugated shape in order from the electrochemical element stack S side to the outside, at the upper part of the electrochemical element stack S. In this case, the upper insulator 210T, the upper flat plate-shaped member 320T, and the upper flat plate-shaped member 220T are not arranged in the space surrounded by the cylindrical portion 201e, the first end portion 201a, and the upper surface portion 201d.

[0261] Furthermore, the electrochemical module M2 has, at the bottom of the electrochemical element stack S, a lower insulator 210B, a lower flat plate member 320B such as a metal honeycomb shape, and a lower flat plate member 220B such as a corrugated shape in order from the electrochemical element stack S side toward the outside.

[0262] The upper surface portion 201d of the upper cover 201 is opposite to the upper plane of the electrochemical element stack S, and the lower surface portion 203d of the lower cover 203 is opposite to the lower plane of the electrochemical element stack S. Furthermore, by combining the upper cover 201 and the lower cover 203, the electrochemical element stack S receives the tightening pressure from the upper surface portion 201d and the lower surface portion 203d substantially uniformly along its plane via the flat plate-shaped members 220 and 320.

[0263] It should be noted that the configuration may also include at least one of the upper and lower flat plate-shaped members 320 and the upper and lower flat plate-shaped members 220. In addition, the upper insulator 210T, the upper flat plate-shaped member 320T, and the upper flat plate-shaped member 220T may be disposed in the space surrounded by the cylindrical portion 201e, the first end portion 201a, and the upper surface portion 201d.

[0264] (7) Specific Structure of Electrochemical Element Stack S

[0265] Next, a specific configuration of the electrochemical element stack S will be described. The electrochemical element stack S is formed by stacking a plurality of electrochemical elements A.

[0266] use Figure 9~Figure 18 , electrochemical element A is described.

[0267] (Electrochemical Components)

[0268] like Figure 9~Figure 17As shown, the electrochemical element A has a plate-shaped support 10, and the plate-shaped support 10 has an internal flow path A1 formed between the opposing surfaces of a conductive first plate-shaped body 1 and a conductive second plate-shaped body 2.

[0269] The plate-like support body 10 comprises: a gas flow-allowing portion 1A, which is capable of passing gas across the inner side of the plate-like support body 10, i.e., the internal flow path A1, and the outer side in at least a portion of the first plate-like body 1 and the second plate-like body 2 constituting the plate-like support body 10; and an electrochemical reaction portion 3, which, in a state of covering all or a portion of the gas flow-allowing portion 1A, comprises a film-like electrode layer 31, a film-like electrolyte layer 32, and a film-like counter electrode layer 33 in the order described (see Figure 13~Figure 17 ). In addition, the plate-like support body 10 has a first penetration portion 41 on one end side, which forms a supply path 4 for supplying one of a reducing component gas such as fuel gas and an oxidizing component gas such as air, i.e., a first gas, from the outer side of the surface penetration direction to the internal flow path A1, and a second penetration portion 51 on the other end side, which forms a discharge path 5 for discharging the first gas flowing in the internal flow path A1 to the outer side of the surface penetration direction of the plate-like support body (see Fig. 9 , Fig.11 , Fig.16 , Fig.17 It should be noted that the supply path 4, etc. and the discharge path 5, etc. can also be understood as the same structure in a symmetrical form).

[0270] (Plate-like support)

[0271] The first plate-like body 1 supports the electrochemical reaction unit 3 having the electrode layer 31, the electrolyte layer 32 and the counter electrode layer 33, and has the function of maintaining the strength of the electrochemical element A. As the material of the first plate-like body 1, a material having excellent electronic conductivity, heat resistance, oxidation resistance and corrosion resistance is used. For example, ferritic stainless steel, austenitic stainless steel, nickel-based alloy, etc. are used. In particular, an alloy containing chromium is preferably used. In the present embodiment, the first plate body 1 uses a Fe-Cr alloy containing 18 mass % or more and 25 mass % or less of Cr. It is particularly suitable if it is a Fe-Cr alloy containing 0.05 mass % or more of Mn, a Fe-Cr alloy containing 0.15 mass % or more and 1.0 mass % or less of Ti, a Fe-Cr alloy containing 0.15 mass % or more and 1.0 mass % or less of Zr, a Fe-Cr alloy containing Ti and Zr with a total content of Ti and Zr of 0.15 mass % or more and 1.0 mass % or less, or a Fe-Cr alloy containing 0.10 mass % or more and 1.0 mass % or less of Cu.

[0272] The second plate-like body 2 is welded to the first plate-like body 1 in a state of being overlapped with the first plate-like body 1, and the peripheral edge portion 1a is integrated to form a plate-like support body 10 (see Figure 10~Figure 17 ). The second plate-like body 2 can be divided into a plurality of parts relative to the first plate-like body 1, and vice versa, the first plate-like body 1 can be divided into a plurality of parts relative to the second plate-like body 2. In addition, during integration, instead of welding, other means such as bonding and fitting can be used, and as long as the internal flow path can be separated from the outside, the parts other than the peripheral portion 1a can be integrated.

[0273] The first plate-like body 1 has a gas flow-allowing portion 1A, which is formed by providing a plurality of through holes 11 penetrating through the front surface and the back surface (see Figure 13~Figure 17 ). It should be noted that, for example, the through hole 11 can be provided in the first plate-like body 1 by laser processing or the like. The through hole 11 has a function of allowing gas to pass from the back surface of the first plate-like body 1 to the front surface. The gas flow-allowing portion 1A is preferably provided in an area smaller than the area of ​​the first plate-like body 1 where the electrode layer 31 is provided.

[0274] In the first plate-like body 1, a metal oxide layer 12 (described later, refer to Fig.18 ). That is, a diffusion suppression layer is formed between the first plate-like body 1 and the electrode layer 31 described later. The metal oxide layer 12 is not only provided on the surface of the first plate-like body 1 exposed to the outside, but also on the surface (interface) in contact with the electrode layer 31. In addition, it can also be provided on the surface on the inner side of the through hole 11. Through the metal oxide layer 12, the mutual diffusion of elements between the first plate-like body 1 and the electrode layer 31 can be suppressed. For example, in the case of using ferritic stainless steel containing chromium as the first plate-like body 1, the metal oxide layer 12 mainly becomes chromium oxide. In addition, the metal oxide layer 12 having chromium oxide as the main component suppresses the diffusion of chromium atoms and the like of the first plate-like body 1 to the electrode layer 31 and the electrolyte layer 32. The thickness of the metal oxide layer 12 can be any thickness as long as it can take into account both high diffusion prevention performance and low resistance.

[0275] The metal oxide layer 12 can be formed by various means, and a method of oxidizing the surface of the first plate-like body 1 to form a metal oxide is preferably used. In addition, on the surface of the first plate-like body 1, the metal oxide layer 12 can be formed by spraying (spraying, aerosol deposition, aerosol vapor deposition, powder spray deposition, particle spray deposition, cold spraying, etc.), sputtering, PVD methods such as PLD, CVD methods, etc., or by plating and oxidation treatment. Further, the metal oxide layer 12 can contain a spinel phase with high conductivity.

[0276] When a ferritic stainless steel material is used as the first plate-like body 1, the thermal expansion coefficient is close to that of YSZ (yttria-stabilized zirconia), GDC (also known as gadolinium-doped cerium oxide, CGO) and the like, which are materials of the electrode layer 31 and the electrolyte layer 32. Therefore, the electrochemical element A is also difficult to be damaged in the case of repeated temperature cycles of low temperature and high temperature. Therefore, an electrochemical element A with excellent long-term durability can be achieved, so it is preferred. It should be noted that the first plate-like body 1 has a plurality of through holes 11 that are arranged through the surface on the front side and the surface on the back side. It should be noted that, for example, the through hole 11 can be arranged in the first plate-like body 1 by mechanical, chemical or optical perforation processing. The through hole 11 has the function of allowing gas to pass from the surface on the back side of the first plate-like body 1 to the surface on the front side. In order to make the first plate-like body 1 gas permeable, a porous metal can also be used. For example, a sintered metal, a foamed metal, etc. can also be used for the first plate-like body 1.

[0277] The second plate-like body 2 is formed into a corrugated plate shape in a region of the first plate-like body 1 opposite to the gas flow allowing portion 1A, and the corrugated plate shape forms an internal flow path A1 having a plurality of auxiliary flow paths A11, A11 ... ... from one end side to the other end side (see Fig. 9 , Fig.13 ). In addition, the second plate-like body 2 is formed into a corrugated plate shape on both the front and back surfaces, and the opposite surface of the surface separating the surface forming the internal flow path A1 is electrically connected to the electrochemical reaction part 3 of the adjacent electrochemical element A, and the passage formed near the portion where the corrugated second plate-like body 2 contacts the first plate-like body 1 functions as a flow portion A2. A plurality of the secondary flow paths A11 are arranged in parallel along the long sides of the plate-like support body 10 formed into a rectangle, constituting the internal flow path A1 from the supply path 4 provided at one end to the discharge path 5 provided at the other end. In addition, there is a distribution portion A12, which is formed by making the connection portion between the first penetration portion 41 and the internal flow path A1 bulge downward from the contact portion with the first plate-like body 1, and distributes the first gas supplied from the first penetration portion 41 to each of the secondary flow paths A11 (refer to Fig. 9 ), having a confluence portion A13, which is formed by making the connection portion between the second through-portion 51 and the internal flow path A1 bulge downward from the contact portion with the first plate-like body 1, and the first gas flowing in each auxiliary flow path A11 is collected and introduced into the second through-portion 51 (refer to Fig. 9 , Fig.11 , Fig.12 , Figure 14~Figure 17 It should be noted that the supply path 4 and the exhaust path 5 can also be understood as the same structure in a symmetrical form). In addition, the material of the second plate-like body 2 is preferably a heat-resistant metal. From the perspective of reducing the thermal expansion difference with the first plate-like body 1 and ensuring the reliability of welding and other bonding properties, it is more preferred if it is the same material as the first plate-like body 1.

[0278] (Electrochemical reaction part) ((Electrode layer))

[0279] The electrode layer 31 is as follows Figures 13 to 18 As shown, it can be provided in a thin layer state in an area which is the front side of the first plate-like body 1 and is larger than the area where the through holes 11 are provided. In the case of being provided as a thin layer, its thickness can be set to, for example, about 1 μm to 100 μm, preferably 5 μm to 50 μm. If it is set to such a thickness, it is possible to ensure sufficient electrode performance while reducing the amount of expensive electrode layer materials used and achieving cost reduction. The entire area where the through holes 11 are provided is covered by the electrode layer 31. That is, the through holes 11 are formed on the inner side of the area where the electrode layer 31 is formed in the first plate-like body 1. In other words, all the through holes 11 are provided facing the electrode layer 31.

[0280] The electrode layer 31 has a large number of micropores inside and on the surface thereof in order to have gas permeability.

[0281] That is, the electrode layer 31 is formed as a porous layer. The electrode layer 31 is formed, for example, in such a manner that its density reaches 30% or more and less than 80%. The size of the micropores can be appropriately selected to be suitable for the size to smoothly react during the electrochemical reaction. It should be noted that the density refers to the proportion of the material constituting the layer in the space, which can be expressed as (1-porosity), and is the same as the relative density.

[0282] As the material of the electrode layer 31, composite materials such as NiO-GDC, Ni-GDC, NiO-YSZ, Ni-YSZ, CuO-CeO2, Cu-CeO2, etc. can be used. In these examples, GDC, YSZ, and CeO2 can be called the skeleton of the composite material. It should be noted that the electrode layer 31 is preferably formed by a low-temperature calcination method (for example, a wet method using a calcination treatment in a low-temperature region without a calcination treatment in a high-temperature region higher than 1100°C), a spraying method (spraying method, aerosol deposition method, aerosol vapor deposition method, powder spray deposition method, particle spray deposition method, cold spray method, etc.), a PVD method (sputtering method, pulsed laser deposition method, etc.), a CVD method, etc. By these processes that can be used in a low-temperature region, a good electrode layer 31 can be obtained without using, for example, calcination in a high-temperature region higher than 1100°C. Therefore, the first plate body 1 is not damaged, and mutual diffusion of elements between the first plate body 1 and the electrode layer 31 can be suppressed, so that a durable electrochemical element A can be realized. Furthermore, low-temperature calcination is more preferably used because it facilitates the handling of the raw materials.

[0283] (Middle layer)

[0284] The intermediate layer 34 can be formed in a thin layer state on the electrode layer 31 in a state of covering the electrode layer 31. In the case of a thin layer, its thickness can be set to, for example, about 1 μm to 100 μm, preferably about 2 μm to 50 μm, and more preferably about 4 μm to 25 μm. If it is set to such a thickness, it is possible to reduce the amount of expensive materials used in the intermediate layer 34 and achieve cost reduction while ensuring sufficient performance. As the material of the intermediate layer 34, for example, YSZ (yttria-stabilized zirconia), SSZ (scandium-stabilized zirconia), GDC (gadolinium-doped cerium oxide), YDC (yttrium-doped cerium oxide), SDC (samarium-doped cerium oxide), etc. can be used. Ceramics of the cerium oxide system are particularly suitable.

[0285] The intermediate layer 34 is preferably formed by a low-temperature calcination method (for example, a wet method using a calcination treatment in a low-temperature region without performing a calcination treatment in a high-temperature region higher than 1100°C), a spraying method (spraying method, aerosol deposition method, aerosol vapor deposition method, powder jet deposition method, particle jet deposition method, cold spray method, etc.), a PVD method (sputtering method, pulsed laser deposition method, etc.), a CVD method, etc. By these film-forming processes that can be used in a low-temperature region, the intermediate layer 34 is obtained without using calcination in a high-temperature region higher than 1100°C, for example. Therefore, the first plate-like body 1 is not damaged, the mutual diffusion of elements between the first plate-like body 1 and the electrode layer 31 can be suppressed, and an electrochemical element A with excellent durability can be realized. In addition, if a low-temperature calcination method is used, the handling of the raw materials becomes easy, so it is further preferred.

[0286] The intermediate layer 34 preferably has oxygen ion (oxide ion) conductivity. Furthermore, it is more preferable if it has mixed conductivity of oxygen ions (oxide ions) and electrons. The intermediate layer 34 having these properties is suitable for use in the electrochemical element A.

[0287] ((Electrolyte layer))

[0288] like Figure 13~Figure 18 As shown, the electrolyte layer 32 is formed in a thin layer state on the intermediate layer 34 in a state of covering the electrode layer 31 and the intermediate layer 34. In addition, it can also be formed in a thin film state with a thickness of less than 10 μm. In detail, the electrolyte layer 32 is arranged on the first plate-like body 1 across (over) the intermediate layer 34. By configuring like this, the electrolyte layer 32 is joined to the first plate-like body 1, thereby being able to form a structure with excellent firmness as a whole electrochemical element.

[0289] In addition, the electrolyte layer 32 is Fig.13As shown, the through hole 11 may be formed in a region which is the front surface of the first plate-like body 1 and is larger than the region where the through hole 11 is formed. That is, the through hole 11 is formed inside the region where the electrolyte layer 32 is formed in the first plate-like body 1.

[0290] In addition, around the electrolyte layer 32, gas leakage from the electrode layer 31 and the aforementioned intermediate layer (not shown) can be suppressed. If explained, when the electrochemical element A is used as a component of SOFC, when the SOFC is working, gas is supplied to the electrode layer 31 from the back side of the first plate-like body 1 through the through hole 11. At the part where the electrolyte layer 32 contacts the first plate-like body 1, gas leakage can be suppressed without setting another component such as a gasket. It should be noted that in this embodiment, the surrounding of the electrode layer 31 is completely covered by the electrolyte layer 32, but it can also be set to be a structure in which the electrolyte layer 32 is set on the upper part of the electrode layer 31 and the aforementioned intermediate layer 34, and a gasket is set around.

[0291] As the material of the electrolyte layer 32, electrolyte materials that conduct oxygen ions such as YSZ (yttria-stabilized zirconia), SSZ (scandium-stabilized zirconia), GDC (gadolinium-doped cerium oxide), YDC (yttrium-doped cerium oxide), SDC (samarium-doped cerium oxide), and LSGM (strontium-magnesium-doped lanthanum gallate) and electrolyte materials that conduct hydrogen ions such as perovskite-type oxides can be used. Zirconia-based ceramics are particularly suitable. If the electrolyte layer 32 is made of zirconia-based ceramics, the operating temperature of the SOFC using the electrochemical element A can be set higher than that of cerium-based ceramics and various hydrogen ion conductive materials. For example, in the case of using electrochemical element A in SOFC, if a material such as YSZ that can exhibit high electrolyte performance even in a high temperature region above about 650°C is used as the material of the electrolyte layer 32, and a hydrocarbon-based raw fuel such as municipal gas or LPG is used as the raw fuel of the system, and the raw fuel is reformed by steam, etc. to produce the anode gas of the SOFC, then a high-efficiency SOFC system can be constructed in which the heat generated in the SOFC unit stack is used to reform the raw fuel gas.

[0292] The electrolyte layer 32 is preferably formed by a low-temperature calcination method (for example, a wet method using a calcination treatment in a low-temperature region without performing a calcination treatment in a high-temperature region greater than 1100°C), a spraying method (a method such as a spraying method, an aerosol deposition method, an aerosol vapor deposition method, a powder jet deposition method, a particle jet deposition method, a cold spraying method, etc.), a PVD method (a sputtering method, a pulsed laser deposition method, etc.), a CVD (chemical vapor growth) method, etc. By these film-forming processes that can be used in a low-temperature region, a dense electrolyte layer 32 with high airtightness and gas barrier properties is obtained without using, for example, calcination in a high-temperature region greater than 1100°C. Therefore, damage to the first plate-like body 1 can be suppressed, and further, mutual diffusion of elements between the first plate-like body 1 and the electrode layer 31 can be suppressed, and an electrochemical element A with excellent performance and durability can be realized. In particular, if a low-temperature calcination method, a spraying method, etc. are used, a low-cost element can be realized, so it is preferred. Furthermore, the use of the spray coating method is more preferred because a dense electrolyte layer having high airtightness and gas barrier properties can be easily obtained in a low temperature range.

[0293] The electrolyte layer 32 is densely constructed to block gas leakage of the anode gas and the cathode gas and to exhibit high ionic conductivity. The density of the electrolyte layer 32 is preferably 90% or more, more preferably 95% or more, and further preferably 98% or more. In the case where the electrolyte layer 32 is a uniform layer, it is preferred that the density is 95% or more, and more preferably 98% or more. In addition, in the case where the electrolyte layer 32 is constructed as a plurality of layers, it is preferred that at least a portion thereof contains a layer (dense electrolyte layer) with a density of 98% or more, and more preferably a layer (dense electrolyte layer) with a density of 99% or more. The reason is that if such a dense electrolyte layer is contained in a part of the electrolyte layer, even if the electrolyte layer is constructed as a plurality of layers, a dense electrolyte layer with high airtightness and gas barrier properties can be easily formed.

[0294] (Anti-reaction layer)

[0295] The anti-reaction layer 35 can be formed in the state of a thin layer on the electrolyte layer 32. In the case of a thin layer, its thickness can be set to, for example, about 1 μm to 100 μm, preferably about 2 μm to 50 μm, and more preferably about 3 μm to 15 μm. If it is set to such a thickness, it is possible to reduce the use of expensive anti-reaction layer materials and achieve cost reduction while ensuring sufficient performance. As the material of the aforementioned anti-reaction layer, any material that can prevent the reaction between the components of the electrolyte layer 32 and the components of the electrode layer 33 can be used, for example, cerium oxide-based materials are used. In addition, as the material of the anti-reaction layer 35, a material containing at least one of the elements selected from Sm, Gd and Y is suitable. It should be noted that at least one of the elements selected from Sm, Gd and Y may be contained, and the total content of these elements is 1.0 mass% or more and 10 mass% or less. By introducing the reaction prevention layer 35 between the electrolyte layer 32 and the electrode layer 33, the reaction between the constituent material of the electrode layer 33 and the constituent material of the electrolyte layer 32 can be effectively suppressed, and the long-term stability of the performance of the electrochemical element A can be improved. If the reaction prevention layer 35 is formed by a method that can be formed at a processing temperature of 1100°C or less, damage to the first plate-like body 1 can be suppressed, and the mutual diffusion of elements between the first plate-like body 1 and the electrode layer 31 can be suppressed, and an electrochemical element A with excellent performance and durability can be realized, so it is preferred. For example, it can be appropriately performed using a low-temperature calcination method (for example, a wet method using a calcination treatment in a low-temperature region without a calcination treatment in a high-temperature region greater than 1100°C), a spraying method (a method such as a spraying method, an aerosol deposition method, an aerosol vapor deposition method, a powder spray deposition method, a particle spray deposition method, a cold spray method, etc.), a PVD method (a sputtering method, a pulsed laser deposition method, etc.), a CVD method, etc. In particular, it is preferred to use a low-temperature calcination method, a spraying method, or the like, because a low-cost element can be realized. Furthermore, it is further preferred to use a low-temperature calcination method because the handling of the raw material becomes easy.

[0296] ((Counter Electrode Layer))

[0297] like Figure 13~Figure 18As shown, the counter electrode layer 33 can be formed in the state of a thin layer on the electrolyte layer 32 or the anti-reaction layer 35. In the case of a thin layer, its thickness can be set to, for example, about 1 μm to 100 μm, preferably 5 μm to 50 μm. If it is set to such a thickness, it is possible to reduce the use of expensive counter electrode layer materials and achieve cost reduction while ensuring sufficient electrode performance. As materials for the counter electrode layer 33, composite oxides such as LSCF, LSM, cerium oxide-based oxides and mixtures thereof can be used. In particular, the counter electrode layer 33 preferably includes a perovskite-type oxide containing two or more elements selected from La, Sr, Sm, Mn, Co and Fe. The counter electrode layer 33 composed of the above materials functions as a cathode.

[0298] It should be noted that if the formation of the electrode layer 33 is appropriately performed using a method that can be formed at a processing temperature below 1100°C, damage to the first plate-like body 1 can be suppressed. In addition, mutual diffusion of elements between the first plate-like body 1 and the electrode layer 31 can be suppressed, and an electrochemical element A with excellent performance and durability can be realized, so it is preferred. For example, a low-temperature calcination method (for example, a wet method using a calcination treatment in a low-temperature region without a calcination treatment in a high-temperature region greater than 1100°C), a spraying method (spraying method, aerosol deposition method, aerosol vapor deposition method, powder spray deposition method, particle spray deposition method, cold spray method, etc.), a PDV method (sputtering method, pulsed laser deposition method, etc.), a CVD method, etc. can be appropriately used. In particular, if a low-temperature calcination method, a spraying method, etc. are used, a low-cost element can be realized, so it is preferred. Furthermore, if a low-temperature calcination method is used, the handling of the raw materials becomes easy, so it is further preferred.

[0299] By constructing such an electrochemical reaction unit 3, when the electrochemical reaction unit 3 functions as a fuel cell (electrochemical power generation unit), the electrochemical element A can be used as a power generation unit of a solid oxide fuel cell. For example, a fuel gas containing hydrogen as a first gas is supplied to the electrode layer 31 through the through hole 11 from the back side of the first plate-like body 1, and air as a second gas is supplied to the counter electrode layer 33 that serves as the counter electrode of the electrode layer 31, and the operating temperature is maintained at, for example, about 700°C. In this way, oxygen O2 contained in the air in the counter electrode layer 33 reacts with electrons e - The reaction generates oxygen ions O 2- The oxygen ion O 2- The hydrogen gas H2 and the oxygen ions O contained in the supplied fuel gas move to the electrode layer 31 through the electrolyte layer 32. 2- Reaction, producing water H2O and electrons e - .

[0300] When an electrolyte material that conducts hydrogen ions is used in the electrolyte layer 32, hydrogen H2 contained in the fuel gas flowing through the electrode layer 31 releases electrons e - The hydrogen ion H + The hydrogen ion H + The oxygen O2 contained in the air and the hydrogen ions H2 move to the counter electrode layer 33 through the electrolyte layer 32. + 、Electronics - Reaction to produce water H2O.

[0301] The above reaction generates an electromotive force as an electrochemical output between the electrode layer 31 and the counter electrode layer 33. In this case, the electrode layer 31 functions as a fuel electrode (anode) of the fuel cell, and the counter electrode layer 33 functions as an air electrode (cathode).

[0302] also, Figure 13~Figure 17 Omitted, such as Fig.18 As shown, in this embodiment, the electrochemical reaction unit 3 has an intermediate layer 34 between the electrode layer 31 and the electrolyte layer 32. Furthermore, an anti-reaction layer 35 is provided between the electrolyte layer 32 and the counter electrode layer 33.

[0303] (Method for producing electrochemical reaction unit)

[0304] Next, a method for manufacturing the electrochemical reaction unit 3 will be described. Figure 13~Figure 17 In the description of the intermediate layer 34 and the anti-reaction layer 35 described below are omitted, so the main description is used here. Fig.18 To explain.

[0305] (Electrode layer forming step)

[0306] In the electrode layer forming step, the electrode layer 31 is formed in a thin film state in an area wider than the area where the through hole 11 is provided on the surface of the front side of the first plate-like body 1. The through hole 11 of the first plate-like body 1 can be provided by laser processing or the like. The formation of the electrode layer 31 can be performed as described above using a low-temperature calcination method (a wet method of performing a calcination treatment in a low-temperature region below 1100°C), a spraying method (a method such as a spraying method, an aerosol deposition method, an aerosol vapor deposition method, a powder jet deposition method, a particle jet deposition method, a cold spraying method, etc.), a PVD method (a sputtering method, a pulsed laser deposition method, etc.), a CVD method, or the like. When any of the methods is used, in order to suppress the degradation of the first plate-like body 1, it is desirable to perform the process at a temperature below 1100°C.

[0307] When the electrode layer formation step is performed by low temperature calcination, it is specifically performed as follows: First, the material powder of the electrode layer 31 is mixed with a solvent (dispersion medium) to prepare a material paste, which is applied to the front surface of the first plate-like body 1 and calcined at 800°C to 1100°C.

[0308] (Diffusion Suppression Layer Formation Step)

[0309] During the calcination step in the above-mentioned electrode layer forming step, a metal oxide layer 12 (diffusion suppression layer) is formed on the surface of the first plate-like body 1. It should be noted that, in the above-mentioned calcination step, if a calcination step is included in which the calcination atmosphere is set to an atmosphere condition with a low oxygen partial pressure, the mutual diffusion suppression effect of the elements is high, and a high-quality metal oxide layer 12 (diffusion suppression layer) with a low resistance value is formed, so it is preferred. Including the case where the electrode layer forming step is set as a coating method without calcination, another diffusion suppression layer forming step may also be included. In either case, it is desired to be implemented at a processing temperature of 1100°C or less that can suppress damage to the first plate-like body 1.

[0310] (Intermediate Layer Formation Step)

[0311] In the intermediate layer forming step, the intermediate layer 34 is formed in a thin layer on the electrode layer 31 in the form of covering the electrode layer 31. The intermediate layer 34 can be formed as described above by a low-temperature calcination method (a wet method in which a calcination treatment is performed in a low-temperature region below 1100°C), a spraying method (a method such as a spraying method, an aerosol deposition method, an aerosol vapor deposition method, a powder spray deposition method, a particle spray deposition method, a cold spray method, etc.), a PVD method (a sputtering method, a pulsed laser deposition method, etc.), a CVD method, etc. When any method is used, it is desirable to perform the process at a temperature below 1100°C in order to suppress the degradation of the first plate-like body 1.

[0312] When the intermediate layer forming step is performed by the low temperature calcination method, it is specifically performed as in the following example.

[0313] First, the material powder of the intermediate layer 34 and the solvent (dispersion medium) are mixed to make a material paste, and the material paste is applied to the surface on the front side of the first plate-like body 1. Then, the intermediate layer 34 is compression molded (intermediate layer smoothing step) and calcined at a temperature below 1100°C (intermediate layer calcining step). The rolling of the intermediate layer 34 can be performed by, for example, CIP (Cold Isostatic Pressing) molding, roller press molding, RIP (Rubber Isostatic Pressing) molding, etc. In addition, it is suitable to calcine the intermediate layer 34 at a temperature above 800°C and below 1100°C. The reason is that, at such a temperature, it is possible to form a high-strength intermediate layer 34 while suppressing damage and deterioration of the first plate-like body 1. In addition, it is more preferred to calcine the intermediate layer 34 at a temperature below 1050°C, and it is further preferred to calcine the intermediate layer 34 at a temperature below 1000°C. The reason for this is that the lower the firing temperature of the intermediate layer 34 is, the more the electrochemical element A can be formed while further suppressing damage and degradation of the first plate-like body 1. The order of the intermediate layer smoothing step and the intermediate layer firing step may be reversed.

[0314] The intermediate layer smoothing step may also be performed by stretch molding, leveling treatment, surface cutting and polishing treatment, and the like.

[0315] (Electrolyte layer forming step)

[0316] In the electrolyte layer forming step, the electrolyte layer 32 is formed in the form of a thin layer on the intermediate layer 34 while covering the electrode layer 31 and the intermediate layer 34. In addition, it can also be formed in the form of a thin film with a thickness of less than 10 μm. The formation of the electrolyte layer 32 can be performed as described above using a low-temperature calcination method (a wet method of calcination treatment in a low-temperature region below 1100°C), a spraying method (spraying method, aerosol deposition method, aerosol vapor deposition method, powder spray deposition method, particle spray deposition method, cold spray method, etc.), a PVD method (sputtering method, pulsed laser deposition method, etc.), a CVD method, and the like. When using any of the methods, in order to suppress the degradation of the first plate-like body 1, it is desired to be performed at a temperature below 1100°C.

[0317] In order to form a high-quality electrolyte layer 32 that is dense and has high airtightness and gas barrier properties in a temperature range below 1100° C., it is desirable to perform the electrolyte layer forming step by spraying. In this case, the material of the electrolyte layer 32 is sprayed toward the intermediate layer 34 on the first plate-like body 1 to form the electrolyte layer 32.

[0318] (Anti-reaction layer forming step)

[0319] In the anti-reaction layer formation step, the anti-reaction layer 35 is formed in the form of a thin layer on the electrolyte layer 32. The formation of the anti-reaction layer 35 can be performed as described above using a low-temperature calcination method (a wet method in which a calcination treatment is performed in a low-temperature region below 1100°C), a spraying method (a method such as a spraying method, an aerosol deposition method, an aerosol vapor deposition method, a powder jet deposition method, a particle jet deposition method, a cold spraying method, etc.), a PVD method (a sputtering method, a pulsed laser deposition method, etc.), a CVD method, and the like. When any method is used, in order to suppress the degradation of the first plate-like body 1, it is desirable to perform the process at a temperature below 1100°C. It should be noted that in order to make the upper surface of the anti-reaction layer 35 flat, for example, a leveling treatment may be performed after the formation of the anti-reaction layer 35, a cutting / grinding treatment may be performed on the surface, or a press processing may be performed after the wet formation and before the calcination.

[0320] (Counter Electrode Layer Formation Step)

[0321] In the step of forming the counter electrode layer, the counter electrode layer 33 is formed in the form of a thin layer on the reaction prevention layer 35. As described above, the formation of the counter electrode layer 33 can be performed using a low-temperature calcination method (a wet method in which a calcination treatment is performed in a low-temperature region below 1100°C), a spraying method (a method such as a spraying method, an aerosol deposition method, an aerosol vapor deposition method, a powder spray deposition method, a particle spray deposition method, a cold spray method, etc.), a PVD method (a sputtering method, a pulsed laser deposition method, etc.), a CVD method, etc. When any method is used, it is desirable to perform the process at a temperature below 1100°C in order to suppress the degradation of the first plate-like body 1.

[0322] In the above-described manner, the electrochemical reaction unit 3 can be manufactured.

[0323] It should be noted that in the electrochemical reaction section 3, it is also possible to have a form without either or both of the intermediate layer 34 and the anti-reaction layer 35. That is, it is also possible to have a form in which the electrode layer 31 is in contact with the electrolyte layer 32, or a form in which the electrolyte layer 32 is in contact with the counter electrode layer 33. In this case, in the above-mentioned manufacturing method, the intermediate layer forming step and the anti-reaction layer forming step are omitted. It should be noted that the step of forming other layers can also be added, or a plurality of layers of the same type can be stacked. In either case, it is desirable to perform at a temperature below 1100°C.

[0324] (Electrochemical device laminate)

[0325] like Figure 4As shown, the electrochemical element stack S has a plurality of electrochemical elements A, and the plurality of electrochemical elements A are stacked and arranged in a form in which the plate-like support 10 constituting one electrochemical element A is opposite to the plate-like support 10 constituting another electrochemical element A, and the outer surface of the second plate-like body 2 different from the first plate-like body 1 having the electrochemical reaction part 3 in the plate-like support 10 constituting one electrochemical element A is electrically connected to the outer surface of the first plate-like body 1 in the plate-like support 10 constituting another electrochemical element A, and a flow portion A2 for the flow of the second gas is formed in the adjacent space between the two outer surfaces along the two outer surfaces. For electrical connection, in addition to simply contacting the conductive surface portions with each other, a method of applying surface pressure to the contact surface or reducing the contact resistance through a highly conductive material can also be adopted. Specifically, each rectangular electrochemical element is arranged with the first penetration portion 41 at one end aligned with the second penetration portion 51 at the other end, with the electrochemical reaction portion of each electrochemical element facing upward, and the first penetration portion 41 and the second penetration portion 51 are stacked with the first annular sealing portion and the second annular sealing portion interposed therebetween, thereby forming the above-mentioned structure.

[0326] In the plate-like support body 10, a first penetration portion 41 is provided at one end side in the longitudinal direction of the rectangular plate-like support body 10, which forms a supply path 4 for supplying a first gas, which is one of a reducing component gas and an oxidizing component gas, from the outer side in the surface penetration direction to the internal flow path A1; a first annular sealing portion 42 is provided as an annular sealing portion in the flow path A2, which separates the first penetration portions 41 formed on the two outer sides of the plate-like support body 10 from the flow path A2; the supply path 4 for supplying the first gas to the internal flow path A1 is formed by the first penetration portion 41 and the first annular sealing portion 42. It should be noted that an annular bulge a is provided on the side opposite to the internal flow path A1 of the first plate-like body 1 around the portion of the first plate-like body 1 connected to the first annular sealing portion 42, so that the positioning of the first annular sealing portion 42 in the direction along the surface of the first plate-like body 1 becomes easy.

[0327] In addition, the plate-like support body 10 has a second through-portion 51 on the other end side, which forms an exhaust path 5 for exhausting the first gas flowing in the internal flow path A1 to the outside in the surface penetration direction of the plate-like support body 10; the second through-portion 51 is a structure for allowing the first gas to flow while being separated from the second gas, and within the circulation portion A2, there is a second annular sealing portion 52 as an annular sealing portion, which separates the second through-portions 51 formed on the two outer sides of the plate-like support body 10 from the circulation portion A2; through the second through-portion 51 and the second annular sealing portion 52, an exhaust path 5 for exhausting the first gas flowing in the internal flow path A1 is formed.

[0328] The first and second annular sealing portions 42 and 52 are made of an insulating material such as a ceramic material such as alumina, mica, or a metal coated thereon, and function as insulating sealing portions that electrically insulate adjacent electrochemical elements from each other.

[0329] (8) Energy systems and electrochemical devices

[0330] Next, for energy systems and electrochemical devices, use Fig.19 Provide explanation.

[0331] The energy system Z includes the electrochemical device 100 and a heat exchanger 190 as a waste heat utilization unit for reusing the heat exhausted from the electrochemical device 100 .

[0332] The electrochemical device 100 has an electrochemical module M, and a fuel converter including a desulfurizer 101 and a reformer 102, a fuel supply unit 103 that supplies fuel gas containing reducing components to the electrochemical module M, and an inverter (an example of a power converter) 104 as an output unit 8 that extracts power from the electrochemical module M.

[0333] Specifically, the electrochemical device 100 includes a desulfurizer 101 , a reforming water tank 105 , a gasifier 106 , a reformer 102 , a blower 107 , a combustion unit 108 , an inverter 104 , a control unit 110 , and an electrochemical module M.

[0334] The desulfurizer 101 removes (desulfurizes) sulfur compounds contained in hydrocarbon-based raw fuels such as municipal gas. When the raw fuel contains sulfur compounds, the desulfurizer 101 can suppress the negative impact of the sulfur compounds on the reformer 102 or the electrochemical element A. The gasifier 106 generates steam from the reforming water supplied from the reforming water tank 105. The reformer 102 steam-reforms the raw fuel desulfurized by the desulfurizer 101 using the steam generated by the gasifier 106, and generates a reformed gas containing hydrogen.

[0335] The electrochemical module M generates electricity by electrochemical reaction using the reformed gas supplied from the reformer 102 and the air supplied from the blower 107. The combustion unit 108 mixes the reaction exhaust gas discharged from the electrochemical module M with the air to burn the combustible components in the reaction exhaust gas.

[0336] The inverter 104 adjusts the output power of the electrochemical module M to have the same voltage and frequency as the power received from the commercial system (not shown). The control unit 110 controls the operation of the electrochemical device 100 and the energy system Z.

[0337] The reformer 102 performs a reforming process of the raw fuel using the combustion heat generated by the combustion of the reaction exhaust gas in the combustion unit 108 .

[0338] The raw fuel is supplied to the desulfurizer 101 through the raw fuel supply path 112 by the operation of the booster pump 111. The reforming water in the reforming water tank 105 is supplied to the gasifier 106 through the reforming water supply path 114 by the operation of the reforming water pump 113. The raw fuel supply path 112 merges with the reforming water supply path 114 at a location on the downstream side of the desulfurizer 101, and the reforming water and the raw fuel that merge outside the container 200 are supplied to the gasifier 106.

[0339] The reforming water is vaporized by the vaporizer 106 to form water vapor. The raw fuel containing water vapor generated by the vaporizer 106 is supplied to the reformer 102 through the raw fuel supply path 115 containing water vapor. The raw fuel is steam-reformed by the reformer 102 to generate a reformed gas (a first gas having a reducing component) having hydrogen as a main component. The reformed gas generated by the reformer 102 is supplied to the electrochemical module M through the fuel supply unit 103.

[0340] The reaction exhaust gas is burned in the combustion unit 108 to form combustion exhaust gas, which is sent to the heat exchanger 190 from the combustion exhaust gas discharge path 116. The combustion catalyst unit 117 (for example, a platinum catalyst) is arranged in the combustion exhaust gas discharge path 116 to burn and remove reducing components such as carbon monoxide and hydrogen contained in the combustion exhaust gas.

[0341] The heat exchanger 190 generates warm water by exchanging heat between the combustion exhaust gas generated by the combustion in the combustion unit 108 and the supplied cold water. That is, the heat exchanger 190 operates as an exhaust heat utilization unit that reuses the heat exhausted from the electrochemical device 100.

[0342] It should be noted that, instead of the exhaust heat utilization unit, a reaction exhaust utilization unit that utilizes the reaction exhaust gas discharged from the electrochemical module M (unburned) may be provided. In addition, at least a portion of the reaction exhaust gas that flows from the first gas exhaust unit 62 to the outside of the container 200 may be discharged to the outside of the container 200. Fig.19 The reaction exhaust gas is combined at any of 100, 101, 103, 106, 112, 113, and 115 and reused. The reaction exhaust gas contains residual hydrogen that is not used for the reaction in the electrochemical element A. In the reaction exhaust gas utilization unit, the residual hydrogen is utilized to utilize heat from combustion, generate electricity using a fuel cell, etc., and effectively utilize energy.

[0343] [Other embodiments]

[0344] It should be noted that the configuration disclosed in the above-mentioned embodiment (including other embodiments, the same below) can be combined with the configuration disclosed in other embodiments when no contradiction occurs. In addition, the embodiments disclosed in this specification are illustrative, and the embodiments of the present invention are not limited to this and can be appropriately changed within the scope of the purpose of the present invention.

[0345] (1) In the above embodiment, the flat plate member 220 is applied to the electrochemical module M in which the electrochemical element A is a SOFC. However, the flat plate member 220 may also be applied to a SOEC (Solid Oxide Electrolyzer Cell) or a secondary battery.

[0346] (2) In the above embodiment, the electrochemical element A is used in a solid oxide fuel cell as the electrochemical device 100, but the electrochemical element A may also be used in a solid oxide electrolysis unit, an oxygen sensor using a solid oxide, etc. In addition, the electrochemical element A is not limited to being used in combination as an electrochemical element stack S or an electrochemical module M, but may also be used alone.

[0347] That is, in the above-mentioned embodiment, the configuration that can improve the efficiency of converting chemical energy such as fuel into electrical energy has been described.

[0348] That is, in the above embodiment, the electrochemical element A and the electrochemical module M are operated as a fuel cell, hydrogen is circulated to the electrode layer 31, and oxygen is circulated to the counter electrode layer 33. In this way, the oxygen molecules O2 in the counter electrode layer 33 react with the electrons e - The reaction generates oxygen ions O 2- The oxygen ion O 2- The hydrogen molecules H2 and the oxygen ions O 2- Reaction, producing water H2O and electrons e - Through the above-mentioned reaction, an electromotive force is generated between the electrode layer 31 and the counter electrode layer 33, and power generation is performed.

[0349] On the other hand, when the electrochemical element A and the electrochemical module M are operated as an electrolysis unit, a gas containing water vapor and carbon dioxide flows through the electrode layer 31, and a voltage is applied between the electrode layer 31 and the counter electrode layer 33. - Reacts with water molecules H2O and carbon dioxide molecules CO2 to form hydrogen molecules H2, carbon monoxide CO and oxygen ions O 2- . Oxygen ion O 2- The oxygen ions O in the counter electrode layer 33 move toward the counter electrode layer 33 through the electrolyte layer 32. 2-Electrons are released to form oxygen molecules O2. Through the above reaction, water molecules H2O are electrolyzed into hydrogen H2 and oxygen O2. When a gas containing carbon dioxide molecules CO2 is circulated, it is electrolyzed into carbon monoxide CO and oxygen O2.

[0350] In the case of circulating a gas containing water vapor and carbon dioxide molecules CO2, a fuel converter 25 ( Fig.21 ). The hydrocarbons etc. generated by the fuel converter 25 can be circulated in the electrochemical element A and the electrochemical module M through a fuel supply unit (not shown), or extracted to the outside of the system / device and used as fuel or chemical raw materials for other purposes.

[0351] Fig.21 , an example of an energy system Z and an electrochemical device 100 in which the electrochemical reaction unit 3 is operated as an electrolysis unit is shown. In this system, water and carbon dioxide supplied are electrolyzed in the electrochemical reaction unit 3 to generate hydrogen and carbon monoxide. Furthermore, hydrocarbons are synthesized in the fuel converter 25. Fig.21 The heat exchanger 24 operates as a waste heat utilization unit that exchanges heat generated by the reaction in the fuel converter 25 with water to vaporize the reaction heat. Fig.21 The heat exchanger 23 in the embodiment functions as an exhaust heat utilization unit that performs heat exchange between the exhaust heat generated by the electrochemical element A and steam and carbon dioxide for preheating. By setting the configuration as described above, energy efficiency can be improved.

[0352] Furthermore, the power converter 93 supplies electric power to the electrochemical element A. Thus, the electrochemical element A functions as an electrolytic unit as described above.

[0353] Therefore, according to the above configuration, it is possible to provide the electrochemical device 100 and the energy system Z, etc., which can improve the efficiency of converting electrical energy into chemical energy such as fuel.

[0354] (3) In the above embodiment, as the material of the electrode layer 31, NiO is used. - GDC、Ni - GDC、NiO - YSZ、Ni - YSZ、CuO - CeO2、Cu -CeO2 and other composite materials, as the material of the electrode layer 33, composite oxides such as LSCF and LSM are used. In the electrochemical element A constructed like this, hydrogen is supplied to the electrode layer 31 and it is set as the fuel electrode (anode), and air is supplied to the electrode layer 33 and it is set as the air electrode (cathode), which can be used as a solid oxide fuel cell unit. The structure can also be changed to form the electrochemical element A in a way that the electrode layer 31 can be used as the air electrode and the electrode layer 33 can be used as the fuel electrode. That is, composite oxides such as LSCF and LSM are used as the material of the electrode layer 31, and composite materials such as NiO-GDC, Ni-GDC, NiO-YSZ, Ni-YSZ, CuO-CeO2, Cu-CeO2 are used as the material of the electrode layer 33. If it is an electrochemical element A constructed like this, air is supplied to the electrode layer 31 and it is used as the air electrode, and hydrogen is supplied to the electrode layer 33 and it is used as the fuel electrode, and the electrochemical element A can be used as a solid oxide fuel cell unit.

[0355] (4) In the above embodiment, the electrode layer 31 is provided between the first plate-like body 1 and the electrolyte layer 32, and the counter electrode layer 33 is arranged on the opposite side of the first plate-like body 1 when viewed from the electrolyte layer 32. Alternatively, the electrode layer 31 and the counter electrode layer 33 may be arranged opposite to each other. In other words, the counter electrode layer 33 may be arranged between the first plate-like body 1 and the electrolyte layer 32, and the electrode layer 31 may be arranged on the opposite side of the first plate-like body 1 when viewed from the electrolyte layer 32. In this case, the supply of gas to the electrochemical element A also needs to be changed.

[0356] That is, with respect to the order of the electrode layer 31 and the counter electrode layer 33, and whether either the first gas or the second gas is one or the other of a reducing component gas and an oxidizing component gas, various forms may be adopted as long as they are configured to be supplied in a form in which the first gas and the second gas react appropriately in the electrode layer 31 and the counter electrode layer 33.

[0357] (5) In the above embodiment, the electrochemical reaction unit 3 is provided on the side of the first plate-like body 1 opposite to the second plate-like body 2 by covering the gas flow allowing portion 1A, but it may be provided on the second plate-like body 2 side of the first plate-like body 1. That is, even if the electrochemical reaction unit 3 is arranged in the internal flow path A1, the present invention is also established.

[0358] (6) In the above-mentioned embodiment, the first through-portion 41 and the second through-portion 51 are provided as a pair at both ends of the rectangular plate-shaped support body, but the configuration is not limited to the configuration at both ends. In addition, the configuration may be provided in two or more pairs. In addition, the first through-portion 41 and the second through-portion 51 do not need to be provided in pairs. Therefore, more than one first through-portion 41 and one second through-portion 51 may be provided.

[0359] Furthermore, the plate-shaped support body is not limited to a rectangular shape, and may also be in various shapes such as a square or a circle.

[0360] (7) The first and second annular sealing portions 42, 52 may have any shape as long as they are structures that allow the first and second penetration portions 41, 51 to communicate with each other and prevent gas leakage. That is, the first and second annular sealing portions 42, 52 may be structures that seal adjacent electrochemical elements A with an endless structure having an opening that communicates with the penetration portion inside. The first and second annular sealing portions 42, 52 are, for example, annular. The annular shape may also be any shape such as circular, elliptical, square, polygonal, etc.

[0361] (8) In the above description, the plate-like support body 10 is composed of the first plate-like body 1 and the second plate-like body 2. Here, the first plate-like body 1 and the second plate-like body 2 may be composed of different plate-like bodies, or may be composed of Fig. 20 As shown in FIG. 1 , it is composed of a plate-like body. Fig. 20 In the case of, by bending one plate-like body, the first plate-like body 1 and the second plate-like body 2 overlap. And, by welding the peripheral edge portion 1a, the first plate-like body 1 and the second plate-like body 2 are integrated. It should be noted that the first plate-like body 1 and the second plate-like body 2 can be composed of a series of seamless plate-like bodies, or a series of plate-like bodies can be bent, such as Fig. 20 Shaped like that.

[0362] As will be described later, the second plate-like body 2 may be composed of one member or two or more members. Similarly, the first plate-like body 1 may be composed of one member or two or more members.

[0363] (9) The second plate-shaped body 2 forms an internal flow path A1 together with the first plate-shaped body 1. The internal flow path A1 includes a distribution portion A12, a plurality of sub-flow paths A11, and a confluence portion A13. The first gas supplied to the distribution portion A12 is as follows: Fig. 9 As shown, the first gas is distributed and supplied to each of the plurality of sub-flow paths A11, and merges at the confluence portion A13 at the outlets of the plurality of sub-flow paths A11. Therefore, the first gas flows from the distribution portion A12 along the gas flow direction toward the confluence portion A13.

[0364] The plurality of auxiliary flow paths A11 are formed by forming the portion of the second plate-like body 2 from the distribution portion A12 except for the confluence portion A13 into a corrugated plate shape. Fig.13 As shown, the plurality of auxiliary flow paths A11 are formed in a corrugated plate shape in a cross-sectional view in a flow intersecting direction intersecting the gas flow direction of the first gas. Fig. 9The corrugated plate is formed by extending in the gas flow direction shown in the figure. The plurality of side flow paths A11 can be formed by a series of corrugated plate-like bodies between the distribution part A12 and the confluence part A13, or can be composed of more than two corrugated plate-like bodies. The plurality of side flow paths A11 can be composed of, for example, more than two corrugated plate-like bodies separated along the direction according to the gas flow direction, or can be composed of more than two corrugated plate-like bodies separated along the direction according to the flow cross direction.

[0365] In addition, a plurality of secondary flow paths A11 are provided. Fig.13 As shown in the figure, the second plate-like body 2 is formed into a waveform by repeatedly forming mountains and valleys of the same shape. However, the second plate-like body 2 may also have a plate-like portion in the region where the plurality of secondary flow paths A11 are formed. For example, the plurality of secondary flow paths A11 may be formed by alternately forming a plate-like portion and a protruding portion. Furthermore, the protruding portion may be set as a portion where a fluid such as the first gas flows.

[0366] (10) The portion of the second plate-like body 2 corresponding to the plurality of secondary flow paths A11 does not need to be formed in a corrugated plate shape over the entire surface, and at least a portion thereof may be formed in a corrugated plate shape. For example, the second plate-like body 2 may be formed in a flat plate shape in a portion in the gas flow direction between the distribution portion A12 and the confluence portion A13, and in a corrugated plate shape in the remainder. In addition, the second plate-like body 2 may be formed in a flat plate shape in a portion in the flow cross direction, and in a corrugated plate shape in the remainder. (11)

[0368] A structure capable of improving power generation efficiency may be provided in the internal flow passage A1. Such a structure will be described below. The description of the parts overlapping with the above embodiment will be simplified or omitted.

[0369] (I) Specific structure of electrochemical module M

[0370] Next, use Figure 22 to Figure 39 The specific structure of the electrochemical module M is described below. The electrochemical module M includes Figure 4 The electrochemical element stack S shown.

[0371] Here, if Figure 22 to Figure 39As shown in FIG. 1 , the stacking direction of the electrochemical element stack S is the +Z direction and the -Z direction (Z direction). In addition, the direction in which the first gas flows from the first gas supply part 61 side to the first gas exhaust part 62 side between the first plate-like body 1 and the second plate-like body 2, and similarly, the direction in which the second gas flows from the second gas supply part 71 side to the second gas exhaust part 72 side between the first plate-like body 1 and the second plate-like body 2 is the +X direction and the -X direction (X direction) intersecting with the +Z direction and the -Z direction (Z direction). In addition, the direction intersecting with the +Z direction and the -Z direction (Z direction) and the +X direction and the -X direction (X direction) is the +Y direction and the -Y direction (Y direction). Furthermore, the XZ plane, the XY plane, and the YZ plane are substantially perpendicular to each other.

[0372] like Figure 4 and Fig. 22 As shown in the figures, the electrochemical module M comprises: a first gas supply section 61, which supplies a first gas to the internal flow path A1 via a supply path 4; a first gas exhaust section 62, which exhausts the first gas after the reaction; a second gas supply section 71, which supplies a second gas to the flow section A2 from the outside; a second gas exhaust section 72, which exhausts the second gas after the reaction; and an output section 8, which obtains an output associated with the electrochemical reaction in the electrochemical reaction section 3; in the container 200, there is a distribution chamber 9, which distributes the second gas supplied from the second gas supply section 71 to the flow section A2.

[0373] Thus, the electrochemical module M is supplied with fuel gas (sometimes also referred to as the first gas) from the first gas supply unit 61, and air (sometimes also referred to as the second gas) from the second gas supply unit 71, so that the fuel gas is Figure 4 , 22 The liquid enters as shown by the dotted arrows, and the air enters as shown by the solid arrows.

[0374] The fuel gas supplied from the first gas supply unit 61 is guided to the supply path 4 from the first penetration portion 41 of the electrochemical element A at the top of the electrochemical element stack S, and flows from the supply path 4 partitioned by the first annular sealing portion 42 to the internal flow path A1 of all electrochemical elements A. In addition, the air supplied from the second gas supply unit 71 flows into the flow portion A2 formed between the electrochemical elements A after temporarily flowing into the distribution chamber 9. In the present embodiment, the flow direction of the fuel gas in the internal flow path A1 along the plane of the plate-like support 10 is from the +X direction toward the -X direction. Similarly, the flow direction of the air in the flow portion A2 along the plane of the plate-like support 10 is from the +X direction toward the -X direction.

[0375] Furthermore, if the second plate-like body 2 (a part of the plate-like support body 10) is used as a reference, the portion of the corrugated second plate-like body 2 that bulges out from the first plate-like body 1 (a part of the plate-like support body 10) forms an internal flow path A1 between the first plate-like body 1 and the second plate-like body 2, and is in contact with the electrochemical reaction portion 3 of the adjacent electrochemical element A to be electrically connected. On the other hand, the portion of the corrugated second plate-like body 2 that contacts the first plate-like body 1 is electrically connected to the first plate-like body 1, and a flow portion A2 is formed between the electrochemical reaction portion 3 of the electrochemical element A adjacent to the second plate-like body 2.

[0376] exist Fig.38 In the part of FIG. 1 and FIG. 2 , there is a part where the electrochemical element A including the cross section of the internal flow path A1 and the electrochemical element A including the cross section of the flow section A2 are shown side by side for convenience, but the fuel gas supplied from the first gas supply unit 61 reaches the distribution unit A12 (refer to FIG. 1 ). Figures 22 to 25 etc.), flows along the width direction of one end side through the distribution portion A12, and reaches each auxiliary flow path A11 in the internal flow path A1 (see Figure 22~Figure 25 wait).

[0377] Here, if Fig. 22 As shown in FIG. 1 , the internal flow path A1 includes a distribution portion A12, a plurality of sub-flow paths A11, and a confluence portion A13 described later. In addition, the internal flow path A1 includes a supply buffer portion 144 between the distribution portion A12 and the plurality of sub-flow paths A11, and a discharge buffer portion 154 between the plurality of sub-flow paths A11 and the confluence portion A13.

[0378] The internal flow path A1 is formed by a space where the first plate-like body 1 and the second plate-like body 2 are opposite to each other. In the present embodiment, the first plate-like body 1 is in the shape of a flat plate, forming a gas flow allowing portion 1A described later. The second plate-like body 2 has a portion protruding upward relative to the stacking direction, and a portion recessed downward. Therefore, by relatively combining the first plate-like body 1 and the second plate-like body 2, the portion of the second plate-like body 2 protruding upward abuts against the first plate-like body 1. Furthermore, a space is formed by the portion of the second plate-like body 2 recessed downward and the first plate-like body 1 to separate the distribution portion A12, the supply buffer portion 144, the plurality of auxiliary flow paths A11, the discharge buffer portion 154, and the confluence portion A13.

[0379] As described in detail later, a supply structure 140 is provided between the distribution section A12 and the plurality of auxiliary flow paths A11 in the direction along the flow direction of the fuel gas (+X direction and -X direction (X direction)). The supply structure 140 temporarily stores the fuel gas in the distribution section A12, and limits the supply of the fuel gas from the distribution section A12 to the plurality of auxiliary flow paths A11.

[0380] Furthermore, a discharge structure 150 is provided between the plurality of sub-flow paths A11 and the junction A13 in the direction along the flow direction of the fuel gas. The discharge structure 150 restricts discharge of the fuel gas from the plurality of sub-flow paths A11 to the junction A13.

[0381] The fuel gas flows through the first gas supply portion 61, the first annular seal portion 42, the first penetration portion 41, etc., and is supplied to the distribution portion A12 of each electrochemical element A. The fuel gas supplied to the distribution portion A12 passes through the supply structure 140 and is temporarily stored in the distribution portion A12. Thereafter, the fuel gas is introduced from the distribution portion A12 into the plurality of secondary flow paths A11.

[0382] The fuel gas entering each secondary flow path A11 flows through each secondary flow path A11 and enters the electrode layer 31 and the electrolyte layer 32 through the gas flow allowing portion 1A. In addition, the fuel gas further advances in the secondary flow path A11 together with the fuel gas that has finished the electrochemical reaction. The fuel gas that has reached the terminal of the flow direction of the plurality of secondary flow paths A11 advances to the confluence portion A13 while the flow to the confluence portion A13 is partially restricted by the discharge structure 150. The fuel gas that has advanced to the confluence portion A13 flows through the confluence portion A13, the second penetration portion 51, the second annular sealing portion 52, etc. And, together with the fuel gas that has finished the electrochemical reaction from other electrochemical elements A, it is discharged to the outside from the first gas discharge portion 62.

[0383] On the other hand, the air supplied from the second gas supply unit 71 enters the circulation unit A2 via the distribution chamber 9 and can enter the counter electrode layer 33 and the electrolyte layer 32. In addition, the air, together with the air that has finished the electrochemical reaction, further advances in the circulation unit A2 along the electrochemical reaction unit 3 and is discharged to the outside from the second gas discharge unit 72.

[0384] According to the flow of the fuel gas and air, the electricity generated in the electrochemical reaction unit 3 is connected in series between the collectors 81 and 82 through the contact between the electrochemical reaction unit 3 of the adjacent electrochemical element A and the second plate-like body 2, forming a form in which a synthetic output is extracted from the output unit 8.

[0385] The structure of the electrochemical element stack S will be described in detail later.

[0386] (II) Configuration of Internal Flow Path and Second Plate-Shaped Body

[0387] The structure of the internal flow path A1 formed by the first plate-shaped body 1 and the second plate-shaped body 2 facing each other will be further described.

[0388] In this embodiment, a first plate-like body 1 in a flat plate shape and a second plate-like body 2 formed in a concave-convex manner in a manner of protruding upward (+Z direction) along the stacking direction or recessed downward (-Z direction) along the stacking direction are opposite to each other, and an internal flow path A1 is formed on the inner surface obtained by the combination. The internal flow path A1 includes a distribution portion A12, a supply buffer portion 144, a plurality of secondary flow paths A11, a discharge buffer portion 154, and a confluence portion A13. In addition, the internal flow path A1 also includes a supply passage portion 141 (a part of the supply structure 140) and a discharge passage portion 151 (a part of the discharge structure 150) through which the first gas passes.

[0389] It should be noted that the supply path 4 side provided with the first gas supply part 61, the first annular seal part 42, the first penetration part 41, etc. and the exhaust path 5 side provided with the first gas exhaust part 62, the second annular seal part 52, the second penetration part 51, etc. are symmetrical structures. Figure 23~Figure 25 , Figure 27~Figure 30 In FIG. 1 , a cross-sectional view of the exhaust passage 5 side where the first gas exhaust portion 62 , the second annular seal portion 52 , the second penetration portion 51 , etc. are provided is shown. On the other hand, Figure 31~Figure 37 In FIG. 4 , a cross-sectional view of the supply path 4 side where the first gas supply portion 61, the first annular seal portion 42, the first penetration portion 41, etc. are provided is shown. Figure 23~Figure 25 , Figure 27~Figure 30 In the cross-sectional view of the discharge path 5, the first gas flows in a direction of being discharged from the plurality of sub-flow paths A11 through the confluence portion A13 to the second penetration portion 51. Figure 31~Figure 37 In the cross-sectional view on the supply path 4 side, the first gas flows through the first penetration portion 41 and the like in the direction of supply from the distribution portion A12 to the plurality of sub-flow paths A11.

[0390] The distribution part A12 is provided corresponding to each electrochemical element A. The distribution part A12 is provided on the supply path 4 side and is a buffer part for supplying the first gas to each electrochemical element A. In addition, the distribution part A12 is provided on the upstream side of the plurality of auxiliary flow paths A11 in the internal flow path A1 in the flow direction of the first gas (from the +X direction to the -X direction). Fig. 22 , Fig.39 As shown in the figures, in the distribution part A12, a first penetration part 41 penetrating the second plate-like body 2 is formed in the approximate center of the directions intersecting the flow direction (+Y direction and -Y direction (Y direction)) and the flow direction (+X direction and -X direction (X direction)). The first gas is circulated in the first gas supply part 61, the first annular sealing part 42, the first penetration part 41, etc., and is supplied to the distribution part A12 of each electrochemical element A.

[0391] The first plate-like body 1 and the second plate-like body 2 are as follows Figure 23~Figure 37As shown in FIG. 1 , the edge of the first plate-like body 1 and the edge of the second plate-like body 2 are welded at the peripheral edge 1a to form an integrated structure. The distribution portion A12 is formed by processing the second plate-like body 2 in a manner that is recessed downward (-Z direction) in the stacking direction compared to the peripheral edge 1a. Further, the distribution portion A12 is formed in a manner that is different from the supply blocking portion 142 (a part of the supply structure 140) in the stacking direction. That is, as Fig.34 As shown in FIG. 1 and FIG. 2 , in the stacking direction, the upper surface of the distribution portion A12 is located lower than the upper surface of the supply blocking portion 142. Furthermore, the upper surface of the supply blocking portion 142 abuts against the lower surface of the first plate-like body 1. Thus, the first gas introduced into the distribution portion A12 is restricted from being discharged from the distribution portion A12 by the supply blocking portion 142 protruding upward in the stacking direction, and is temporarily stored in the distribution portion A12 formed in a concave shape.

[0392] In addition, the distribution portion A12 is shown in the top view. Fig. 22 As shown in FIG. 1 , the length of the distribution portion A12 in the Y direction corresponds to the length of the region of the plurality of auxiliary flow paths A11 arranged in parallel with intervals in the Y direction.

[0393] The plurality of secondary flow paths A11 through which the first gas flows are as follows Figure 22 to Figure 39 As shown in FIG. 1 and FIG. 2 , the second plate-like body 2 extends in the flow direction, that is, in the +X direction and the -X direction (X direction). In addition, as described above, the plurality of secondary flow paths A11 are arranged in parallel with each other in the Y direction. Figure 22 to Figure 39 As shown in FIG. 1 and FIG. 2 , the plurality of auxiliary flow path forming portions 160 are provided to form the plurality of auxiliary flow paths A11, and the plurality of partitioning portions 161 are provided between the adjacent auxiliary flow path forming portions 160 to separate the adjacent auxiliary flow paths A11. Fig.38 As shown in FIG. 1 , the secondary flow path forming portion 160 is formed into a concave shape having a bottom surface, and the upper surface of the partition portion 161 is located above the bottom surface of the secondary flow path forming portion 160 in the stacking direction. In addition, the upper surface of the partition portion 161 abuts against the lower surface of the first plate-like body 1. Thus, each secondary flow path A11 is separated, and each first gas flows in each secondary flow path A11 along the flow direction.

[0394] It should be noted that the secondary flow path A11 is Fig. 22 In the embodiment of the present invention, the auxiliary flow path A11 extends from the vicinity of the supply structure 140 to the vicinity of the discharge structure 150 along the flow direction. However, the auxiliary flow path A11 is not limited to this, and may be formed only in a portion from the vicinity of the supply structure 140 to the vicinity of the discharge structure 150. In other words, the auxiliary flow path forming portion 160 forming the auxiliary flow path A11 may be disposed only in a portion from the vicinity of the supply structure 140 to the vicinity of the discharge structure 150.

[0395] like Fig.38 , Fig.39 As shown, in the +Y direction and the -Y direction (Y direction, the direction intersecting the flow direction), the length L3 of the partition 161 is smaller than the length L4 of the auxiliary flow path forming portion 160 (L3 < L4). Fig.38 As shown in the figure, the contact area between the upper surface of the partition 161 and the lower surface of the first plate-like body 1 can be reduced. That is, the space of the secondary flow path A11 of the first plate-like body 1 forming the gas flow allowing portion 1A can be increased, and the amount of the first gas from the secondary flow path A11 toward the electrochemical reaction unit 3 can be increased.

[0396] The second plate-like body 2 is Fig. 22 , Figure 31~Figure 39 As shown in FIG. 1 , a supply structure 140 is provided between the distribution section A12 and the plurality of auxiliary flow paths A11 in the direction along the flow direction (+X direction and -X direction (X direction)). The supply structure 140 temporarily stores the first gas in the distribution section A12 and limits the supply of the first gas from the distribution section A12 to the plurality of auxiliary flow paths A11.

[0397] The supply structure 140 has a plurality of supply passages 141 and a plurality of supply blocking portions 142. The supply passages 141 allow the first gas to pass from the distribution portion A12 to the plurality of secondary flow paths A11. The supply blocking portions 142 block the first gas from passing from the distribution portion A12 to the plurality of secondary flow paths A11. Fig.33 As shown in FIG. 1 and FIG. 2 , the upper surface of the supply blocking portion 142 is located above the upper surface of the supply passing portion 141 in the stacking direction and abuts against the lower surface of the first plate-like body 1. Therefore, the first gas in the distribution portion A12 is blocked from flowing in the flow direction by the supply blocking portion 142, and on the other hand, flows in the flow direction via the supply passing portion 141 and flows to the plurality of auxiliary flow paths A11.

[0398] In this embodiment, each supply blocking portion 142 is, for example, Fig. 22 , Fig.39 As shown in FIG. 1 and FIG. 2 , the supply blocking portions 142 are formed into a substantially rectangular shape. Furthermore, each rectangular supply blocking portion 142 is arranged along the Y direction in such a manner that the long sides are along the +Y direction and the -Y direction (Y direction). The supply passage portion 141 is provided between adjacent supply blocking portions 142. That is, the supply passage portion 141 is provided in the interval where the short sides of adjacent supply blocking portions 142 are opposite.

[0399] like Fig.39As shown, in the +Y direction and the -Y direction (Y direction, the direction intersecting the flow direction), the length L2 of the supply blocking portion 142 is greater than the length L1 of the supply passage portion 141 (L2>L1). In addition, the length L1 of the supply passage portion 141 is preferably less than the length L3 of the partition portion 161 (L1<L3). Thus, the first gas squeezed out from the distribution portion A12 through the supply passage portion 141 can collide with the end of the partition portion 161 on the +X direction side, and can be temporarily stored in the supply buffer portion 144 described later.

[0400] The relationship between L1 and L2 is determined based on, for example, the amount of the first gas supplied to the distribution section A12 per unit time, the amount of the first gas to be supplied to the multiple auxiliary flow paths A11 per unit time, the number of supply blocking sections 142, the length L3 of the partition section 161 in the Y direction, the length L4 of the auxiliary flow path A11 in the Y direction, etc.

[0401] As described above, each auxiliary flow path A11 is partitioned by each partition 161. In the flow direction (+X direction and -X direction (X direction)), any partition 161 among the plurality of partitions 161 is arranged corresponding to the supply passage portion 141.

[0402] Furthermore, in the flow direction, at least one of the plurality of sub-flow paths A11 is arranged to correspond to the supply blocking portion 142 .

[0403] Here, the first gas is introduced from the distribution section A12 to the plurality of secondary flow paths A11 via the supply passage 141. According to the above configuration, in the flow direction, any partition 161 is arranged corresponding to the supply passage 141, so that the first gas squeezed out from the distribution section A12 to the supply passage 141 advances along the flow direction and collides with the partition 161 protruding upward in the stacking direction. By colliding with the partition 161, the first gas advances in a cross direction that intersects with the flow direction. That is, the first gas that flows from the distribution section A12 through the supply passage 141 is not immediately introduced into the plurality of secondary flow paths A11, but collides with the partition 161 in front of the secondary flow path A11 and advances in the cross direction. Furthermore, the first gas that advances in the cross direction passes through the supply blocking section 142 protruding upward in the stacking direction without returning to the distribution section A12, and is temporarily stored between the supply structure 140 and the plurality of secondary flow paths A11. Thereafter, the first gas is introduced into the plurality of auxiliary flow paths A11 formed by the plurality of auxiliary flow path forming portions 160 along the extrusion from the distribution portion A12 .

[0404] It should be noted that the region where the first gas is temporarily stored between the supply structure 140 and the plurality of sub-flow paths A11 is the supply buffer portion 144 .

[0405] In the present embodiment, in the flow direction, one partition 161 is arranged corresponding to one supply passage 141. However, the present invention is not limited thereto, and a plurality of partitions 161 may be arranged corresponding to one supply passage 141. In addition, instead of arranging the partition 161 corresponding to one supply passage 141, the partition 161 may be arranged corresponding to another supply passage 141.

[0406] In addition, the supply blocking portion 142 is provided in the flow direction corresponding to the first penetration portion 41. This can prevent the first gas introduced from the first penetration portion 41 into the distribution portion A12 from immediately heading toward the plurality of sub-flow paths A11. Therefore, the first gas can be temporarily stored in the distribution portion A12.

[0407] The number of the supply blocking portions 142 is not limited thereto, but is, for example, 2 or more. In addition, the number of the supply blocking portions 142 is preferably set according to the number of the plurality of auxiliary flow paths A11.

[0408] In addition, the supply blocking portions 142 are arranged in a row in the direction intersecting the flow direction in the above text. However, as long as the first gas is temporarily stored in the distribution portion A12 and the first gas can be supplied to the plurality of secondary flow paths A11 approximately uniformly, the arrangement is not limited thereto. For example, the plurality of supply blocking portions 142 may be arranged offset from the intersecting direction. In addition, the plurality of supply blocking portions 142 may be arranged along the intersecting direction or offset from the intersecting direction.

[0409] In the above description, the supply blocking portion 142 is rectangular. However, the shape of the supply blocking portion 142 is not limited thereto as long as the gas can be uniformly supplied from the distribution portion A12 to the plurality of secondary flow paths A11. For example, the supply blocking portion 142 may be formed in various shapes such as square, circular, elliptical, or triangular.

[0410] In addition, but not limited to this, such as Fig. 22 , Fig.39 As shown in the above-mentioned embodiments, it is preferred that two of the multiple supply blocking portions 142 are each provided at a position corresponding to the end of the distribution portion A12 in the +Y direction and the end of the -Y direction. The first gas diffuses in the distribution portion A12 in a manner that widens the space of the distribution portion A12 from the first penetration portion 41 of the distribution portion A12, and collides with the end face of the distribution portion A12. Therefore, the first gas that sometimes collides with the end face of the distribution portion A12 changes direction at the end face and flows toward the multiple auxiliary flow paths A11. Therefore, by pre-arranging the supply blocking portion 142 at a position corresponding to the end of the distribution portion A12, it is possible to suppress the first gas from immediately flowing out of the distribution portion A12 to the multiple auxiliary flow paths A11. Thereby, as described later, the first gas can be supplied from the distribution portion A12 to each auxiliary flow path A11 approximately evenly.

[0411] Next, the merging portion A13 and the discharge structure 150 will be described. The merging portion A13 and the discharge structure 150 have the same configuration as the distribution portion A12 and the supply structure 140, respectively.

[0412] The confluence portion A13 is provided on the discharge path 5 side and is a buffer portion for discharging the first gas flowing in the plurality of sub-flow paths A11. The confluence portion A13 is provided on the downstream side of the plurality of sub-flow paths A11 in the internal flow path A1 in the flow direction of the first gas. Fig. 22 , Fig.39 As shown in FIG. 1 and FIG. 2 , in the confluence portion A13, a second penetration portion 51 penetrating the second plate-like body 2 is formed at a substantially central portion in the flow direction and the cross direction thereof. The first gas passing through the plurality of secondary flow paths A11 is introduced into the confluence portion A13, and is discharged to the outside via the second penetration portion 51, the second annular sealing portion 52, the first gas discharge portion 62, and the like.

[0413] In addition, the confluence portion A13 is formed in a manner that the position in the stacking direction is different in the discharge blocking portion 152 (a part of the discharge structure 150). Fig. 27 As shown in the figures, in the stacking direction, the upper surface of the confluence portion A13 is located lower than the upper surface of the discharge blocking portion 152. In addition, the upper surface of the discharge blocking portion 152 abuts against the lower surface of the first plate-like body 1. Thus, the first gas from the plurality of auxiliary flow paths A11 toward the confluence portion A13 is restricted from being discharged toward the confluence portion A13 by the discharge blocking portion 152 protruding upward in the stacking direction, and is temporarily stored in the plurality of auxiliary flow paths A11.

[0414] In addition, the confluence portion A13 is shown in the top view. Fig. 22 As shown in FIG. 1 , it is long in the +Y direction and the −Y direction (Y direction). The length of the merging portion A13 in the Y direction corresponds to the length of the region of the plurality of auxiliary flow paths A11 arranged in parallel with intervals in the Y direction.

[0415] The second plate-like body 2 is Fig. 22 , Figure 26~Figure 30 , Fig.39 As shown in FIG. 1 , a discharge structure 150 is provided between the plurality of sub-flow paths A11 and the confluence portion A13 in the direction along the flow direction (+X direction and -X direction (X direction)). The discharge structure 150 restricts discharge of the first gas from the plurality of sub-flow paths A11 to the confluence portion A13.

[0416] The discharge structure 150 includes a plurality of discharge passages 151 and a plurality of discharge blocking portions 152. The discharge passages 151 allow the first gas to pass from the plurality of auxiliary flow paths A11 to the confluence portion A13. The discharge blocking portions 152 block the first gas from passing from the plurality of auxiliary flow paths A11 to the confluence portion A13. Fig. 27As shown in the figures, the upper surface of the discharge blocking portion 152 is located above the upper surface of the discharge passing portion 151 in the stacking direction, and abuts against the lower surface of the first plate-like body 1. Therefore, the discharge blocking portion 152 blocks the first gas in the plurality of auxiliary flow paths A11 from flowing in the flow direction, while the first gas flows in the flow direction through the discharge passing portion 151 and flows toward the confluence portion A13.

[0417] In this embodiment, the discharge blocking portion 152 is similar to the supply blocking portion 142, such as Fig. 22 , Fig.39 As shown in FIG. 1 and FIG. 2 , the drain blocking portions 152 are formed into a substantially rectangular shape. Furthermore, each rectangular drain blocking portion 152 is arranged along the Y direction in such a manner that the long sides are along the +Y direction and the -Y direction (Y direction). A drain passage portion 151 is provided between adjacent drain blocking portions 152. That is, the drain passage portion 151 is provided in the interval where the short sides of adjacent drain blocking portions 152 are opposite.

[0418] like Fig.39 As shown, in the +Y direction and the -Y direction (Y direction, the direction intersecting the flow direction), the length L12 of the discharge blocking portion 152 is greater than the length L11 of the discharge passage portion 151 (L12>L11). In addition, the length L12 of the discharge blocking portion 152 is preferably greater than the length L4 of the auxiliary flow path forming portion 160 (L12>L3). Thus, the first gas from the plurality of auxiliary flow paths A11 toward the confluence portion A13 can collide with the discharge blocking portion 152, and can be temporarily stored and discharged in the discharge buffer portion 154 described later.

[0419] The relationship between L11 and L12 is determined based on, for example, the amount of the first gas supplied to the multiple auxiliary flow paths A11 per unit time, the amount of the first gas to be discharged from the confluence section A13 per unit time, the number of discharge blocking sections 152, the length L3 of the partition section 161 in the Y direction, the length L4 of the auxiliary flow path A11 in the Y direction, etc.

[0420] In the flow direction, at least one of the plurality of sub-flow paths A11 is arranged corresponding to the discharge blocking portion 152 .

[0421] Furthermore, in the flow direction, any one of the plurality of partitions 161 is disposed corresponding to the discharge passage 151 .

[0422] According to the above configuration, the first gas squeezed out from the plurality of auxiliary flow paths A11 advances along the flow direction and collides with the discharge blocking portion 152 protruding upward in the stacking direction. By colliding with the discharge blocking portion 152, the first gas advances in the intersecting direction intersecting with the flow direction. That is, the first gas flowing from the plurality of auxiliary flow paths A11 is not immediately introduced into the confluence portion A13, but collides with the discharge blocking portion 152 before the confluence portion A13 and advances in the intersecting direction. Thereafter, the first gas is introduced into the confluence portion A13 through the discharge passage 151 along the squeezed out from the plurality of auxiliary flow paths A11.

[0423] It should be noted that the region where the first gas is temporarily stored between the plurality of sub-flow paths A11 and the discharge structure 150 is the discharge buffer portion 154 .

[0424] In addition, the discharge blocking portion 152 is provided in the flow direction corresponding to the second penetration portion 51. This can prevent the first gas flowing through the plurality of auxiliary flow paths A11 from being immediately introduced into the confluence portion A13 and discharged from the second penetration portion 51. Therefore, the first gas can be temporarily stored in the plurality of auxiliary flow paths A11.

[0425] The shape, size, arrangement, number, etc. of the discharge passage portion 151 and the discharge blocking portion 152 are the same as those of the supply passage portion 141 and the supply blocking portion 142. Fig.39 The length L12 of the discharge blocking portion 152 and the length L11 of the discharge passage portion 151 in the +Y direction and -Y direction (Y direction, the intersecting direction with the flow direction) are the same as the length L1 of the supply blocking portion 142 and the length L2 of the supply passage portion 141 mentioned above.

[0426] However, the shape, size, arrangement, number, etc. of the discharge passage 151 and the discharge blocking portion 152 may be different from those of the supply passage 141 and the supply blocking portion 142. For example, the size of the discharge passage 151 may be larger than that of the supply passage 141. Thus, the discharge pressure from the plurality of auxiliary flow paths A11 to the confluence portion A13 may be lower than the supply pressure when the first gas is supplied from the distribution portion A12 to the plurality of auxiliary flow paths A11. The first gas can be supplied from the distribution portion A12 to the plurality of auxiliary flow paths A11 at a certain supply pressure, so that the flow distribution between the plurality of auxiliary flow paths A11 is constant, and at the same time, when the first gas is discharged, it is smoothly introduced into the confluence portion A13.

[0427] (b) Roles of the supply structure and the discharge structure

[0428] (b1) Function of supply structure

[0429] Next, the function of the supply structure 140 will be described.

[0430] The supply blocking portion 142 of the supply structure 140 constructed as described above is arranged between the distribution portion A12 and the plurality of secondary flow paths A11, forming a barrier to the flow of the first gas from the distribution portion A12 to the plurality of secondary flow paths A11. Therefore, the pressure loss of the first gas when flowing from the distribution portion A12 to the plurality of secondary flow paths A11 becomes higher, and the first gas introduced into the distribution portion A12 diffuses in a manner that fills the distribution portion A12 and is temporarily stored. Therefore, a substantially uniform pressure (equalized pressure) is achieved throughout the distribution portion A12. That is, the differential pressures of the distribution portion A12 and the plurality of secondary flow paths A11 are substantially the same. On this basis, the first gas is supplied from the distribution portion A12 to the plurality of secondary flow paths A11 via the supply passage portion 141, so that the first gas is supplied in a state of substantially equalized pressure in each secondary flow path A11. As a result, the flow distribution (flow velocity, flow rate, pressure, etc.) of the first gas along the flow direction between the respective secondary flow paths A11 is substantially uniform.

[0431] In addition, the first gas flows through the plurality of sub-flow paths A11 divided from the distribution portion A12. By utilizing the rectifying effect of the flow divided into the plurality of flow paths, the flow distribution (flow velocity, flow rate, pressure, etc.) of the first gas is substantially constant compared to the case where the first gas flows in the internal flow path without forming the plurality of flow paths.

[0432] As described above, the flow distribution of the first gas along the flow direction between each of the secondary flow paths A11 is substantially uniform. For example, when observing a certain position in the flow direction between each of the secondary flow paths A11, the flow velocity, flow rate, and pressure of the first gas in each of the secondary flow paths A11 are substantially constant in the intersecting direction intersecting the one position. As a result, in the electrochemical reaction unit 3, the difference between the portion where the first gas is insufficient and the portion where the first gas flows excessively is reduced, thereby improving the utilization rate of the first gas in the entire electrochemical element A, thereby improving the reaction efficiency of the electrochemical reaction.

[0433] It should be noted that, when the above-mentioned distribution part A12, multiple sub-flow paths A11 and supply structure 140 are not used, the flow distribution of the first gas in each sub-flow path A11 is different, and sometimes the flow rate of the first gas in a certain sub-flow path A11 is fast, and the flow rate of the first gas in another sub-flow path A11 is slow. The first gas is consumed by the electrochemical reaction in the sub-flow path A11 with a slow flow rate of the first gas, and the first gas is insufficient. As a result, the concentration of the first gas decreases, and the electrode layer of the electrochemical reaction unit 3 is oxidized and degraded, which may lead to a decrease in electrode performance and mechanical strength. On the other hand, in the sub-flow path A11 with a fast flow rate of the first gas, the first gas is discharged before being consumed in the electrochemical reaction. That is, when the first gas is a fuel gas such as hydrogen, the first gas with a still high concentration is discharged, and the fuel utilization rate is reduced. Here, it is also possible to consider the shortage of the first gas in the sub-flow path A11 with a slow flow rate of the first gas, and increase the supply amount of the first gas supplied to each sub-flow path A11. However, in this case, in the secondary flow path A11 where the flow rate of the first gas is fast, the amount of the first gas discharged before being consumed in the electrochemical reaction further increases, and the fuel utilization rate further decreases. Accordingly, when the flow distribution of the first gas in each secondary flow path A11 is different, the reaction efficiency of the electrochemical reaction decreases, and the power generation efficiency decreases.

[0434] (b2) Role of emission structure

[0435] Next, the function of the discharge structure 150 will be described.

[0436] According to the above configuration, not only is a supply structure 140 provided for supplying the first gas from the distribution section A12 to the plurality of auxiliary flow paths A11 with a substantially uniform flow distribution, but an exhaust structure 150 is also provided at the portion where the first gas from the plurality of auxiliary flow paths A11 merges at the confluence section A13. The plurality of auxiliary flow paths A11 are sandwiched between the supply structure 140 and the exhaust structure 150, so that the flow distribution (flow velocity, flow rate, pressure, etc.) of the first gas in the plurality of auxiliary flow paths A11 can be made substantially uniform, while improving the reaction efficiency of the electrochemical reaction.

[0437] To be more specific, the emission blocking portion 152 of the emission structure 150 constructed as described above is arranged between the plurality of side flow paths A11 and the confluence portion A13, forming a barrier to the flow of the first gas from the side flow path A11 to the confluence portion A13. Therefore, the pressure loss of the first gas when flowing from the plurality of side flow paths A11 to the confluence portion A13 becomes higher. Therefore, it is difficult for the first gas introduced into the plurality of side flow paths A11 to be immediately introduced into the confluence portion A13 from the plurality of side flow paths A11, and diffuses in a manner that fills the plurality of side flow paths A11. Thus, the flow distribution (flow velocity, flow rate, pressure, etc.) of the first gas along the flow direction can be made substantially uniform between the side flow paths A11. In addition, the first gas diffuses in a manner that fills the plurality of side flow paths A11, so that the electrochemical reaction is fully carried out in the plurality of side flow paths A11. Thus, the reaction efficiency of the electrochemical reaction can be improved.

[0438] (12) In the above embodiment, the electrochemical device includes the electrochemical module M including a plurality of electrochemical elements A. However, the electrochemical device of the above embodiment can also be applied to a configuration including one electrochemical element.

[0439] Description of Reference Numerals

[0440] 31: Electrode layer

[0441] 32: Electrolyte layer

[0442] 33: Counter electrode layer

[0443] 100: Electrochemical devices

[0444] 101: Desulfurizer

[0445] 102: Reformer

[0446] 103: Fuel supply unit

[0447] 104: Inverter

[0448] 220: Flat plate member

[0449] 230: Board

[0450] 245: Side insulator

[0451] 320: Flat plate member

[0452] A: Electrochemical components

[0453] M: Electrochemical module

[0454] S: Electrochemical element stack

[0455] Z: Energy system.

Claims

1. An electrochemical module having: Laminated body, in, A plurality of electrochemical elements each having an electrolyte layer and a first electrode and a second electrode disposed on both sides of the electrolyte layer are stacked in a predetermined stacking direction along a substrate; an elastic flat plate-shaped member disposed along at least one of a first plane of the stacked body in the stacking direction and a second plane opposite to the first plane; and a clamping body, which includes a first clamping body in the form of a flat plate arranged along the first plane and a second clamping body in the form of a flat plate arranged along the second plane in the stacking direction, and clamps the stacked body via the flat plate-shaped member, The plate-like member has a thickness of 0.1 mm to 1 mm, is a thermal expansion member that expands due to heat, has a thermal expansion coefficient greater than that of the member constituting the clamping body, and is formed of austenitic stainless steel. The clamping body is formed of ferritic stainless steel, martensitic stainless steel, or a composite of ferritic stainless steel and ceramics. The flat plate-like member has a corrugated plate shape when viewed in a direction intersecting with a stacking direction of the stacked body.

2. The electrochemical module according to claim 1, in, The flat plate-shaped member is in contact with at least one of the plane of the stacked body and the plane of the sandwiching body at a plurality of dispersed locations.

3. The electrochemical module according to claim 1, in, The flat plate-shaped member receives, by its elastic force, a difference in thermal expansion between the stacked body and the sandwiching body when the electrochemical element is generating electricity and when the electrochemical element is not generating electricity.

4. The electrochemical module according to claim 3, in, The fastening pressure applied by the flat plate-shaped member to the stacked body when the electrochemical element is not generating electricity is applied in advance to a degree that can ensure the fastening pressure required when the electrochemical element generates electricity.

5. The electrochemical module according to claim 1, in, At least one of the first clamping body and the second clamping body is a part of a case surrounding the stacked body.

6. The electrochemical module according to claim 1, in, The aforementioned electrochemical element is a solid oxide fuel cell.

7. The electrochemical module according to claim 1, in, The aforementioned electrochemical element is a solid oxide type electrolytic cell.

8. Assembly method of electrochemical module, in, A flat plate-like member having a thickness of 0.1 mm to 1 mm and being a heat-expandable member that expands due to heat is arranged along at least one of a first plane in a stacking direction of a stacked body and a second plane opposite to the first plane, wherein a plurality of electrochemical elements each having an electrolyte layer formed along a substrate and a first electrode and a second electrode respectively arranged on both sides of the electrolyte layer are stacked in a predetermined stacking direction; A first flat plate-shaped clamping body is arranged along the first plane, and a second flat plate-shaped clamping body is arranged along the second plane, and the first clamping body and the second clamping body are fastened in the stacking direction so as to ensure the degree of fastening pressure applied by the flat plate-shaped member to the stacking body required when the electrochemical element generates electricity, and the fastening pressure applied by the flat plate-shaped member to the stacking body when the electrochemical element does not generate electricity is applied in advance, The flat plate-shaped member has a thermal expansion coefficient greater than that of the members constituting the first clamping body and the second clamping body, and is formed of austenitic stainless steel. The first clamping body and the second clamping body are formed of ferritic stainless steel, martensitic stainless steel, or a composite of ferritic stainless steel and ceramics.

9. An electrochemical device comprising at least an electrochemical module and a fuel converter as described in any one of claims 1 to 7, and having a fuel supply unit for flowing a reducing component gas from the fuel converter to the aforementioned electrochemical module, or flowing a reducing component gas from the aforementioned electrochemical module to the fuel converter.

10. An electrochemical device comprising at least the electrochemical module according to any one of claims 1 to 7 and a power converter for extracting electric power from the electrochemical module or for transmitting electric power to the electrochemical module.

11. An energy system comprising the electrochemical device according to claim 9 or 10, and an exhaust heat utilization unit for reusing heat exhausted from the electrochemical device or a fuel converter.