A method for removing the PTH hole ring of a multilayer board by etching technology
Direct removal of multilayer board PTH hole rings through etching technology solves the problems of depth control and process complexity of traditional backdrilling technology, achieves simplified processes and low-cost signal transmission effects, and improves product yield and signal Integrity.
Patent Information
- Application Number
- CN202011039538.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-28
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2040-09-28
AI Technical Summary
Traditional back-drilling technology has accuracy problems when controlling the depth of copper in PTH holes. The process is complex and costly, and the resin easily overflows and affects signal transmission when the hole is plugged after etching.
Etching technology is used to directly remove the PTH hole ring of the multi-layer board on the outer layer. Through blanking, copper foil plating, drilling, electroplating, resin hole plugging, etching, ink printing and other steps, the process is simplified and avoids secondary drilling and plating. Tin process, using vacuum hole plugging machine and optimizing etching pressure to protect the copper in the hole.
It achieves a simple process and low cost, reduces the product scrap rate, improves the integrity and accuracy of signal transmission, and avoids the problem of uneven hole rings caused by resin overflow.
Abstract
Description
Technical Field
[0001] The invention relates to the field of PCB board processing, and in particular to a method for removing PTH hole rings of a multilayer board by using an etching technology. Background Art
[0002] The development of electronic products towards miniaturization and high speed requires PCB to have high transmission speed and precise circuit layout. PTH (PLATING Through Hole) is used to conduct each conductive layer, also known as a through hole. Due to signal requirements, some useless metallized PTH holes on the PCB board will affect the signal transmission of the line and increase signal loss. The hole mouth of some through holes requires the removal of hole rings. At present, the industry often uses back drilling to remove a certain length of useless hole copper to reduce its signal transmission on the PCB board. Traditional back drilling is to remove the hole copper part that is not conducive to signal transmission in the electroplated PTH hole through secondary drilling.
[0003] The back drilling technology currently used is actually a depth-controlled drilling technology, which constructs the drilling zero height and then sets a certain drilling depth value to complete the back drilling. When the board thickness fluctuates, accurate back drilling copper retention control cannot be achieved. The process flow is complicated and the drilling depth is difficult to control.
[0004] Chinese patent CN110572947A discloses a method of controlling deep etching to replace back drilling, including the following steps: S1: cutting, drilling and electroplating, forming at least one PTH hole on the board, and determining the etching hole that needs controlled deep etching; S2: controlling the deep etching pattern, covering the etching hole with the hole ring, and compensating the dry film width of the etching hole mouth according to the alignment ability of LDI, and then exposing and developing, except for the pad on the surface of the PTH hole, the copper layer in the remaining area of the board surface is removed; S3: tinning, tinning the etching hole; S4: etching, etching the etching hole, removing the excess copper PAD in the etching hole, and slicing to determine the etching effect; S5: resin plugging and grinding. The present invention adopts controlled deep etching to avoid the problems of easy drilling deviation and broken needle in the back drilling process, and the produced PCB board has good quality, simple process, reduced cost, removes excess conductors in the etching hole, avoids signal interference, and improves the integrity and accuracy of signal transmission.
[0005] However, this method first requires electroplating, dry film application, exposure, development, tinning, and etching to remove excess copper. The process is cumbersome and complicated. When the resin is plugged into the hole after etching, resin overflows. Since the hole ring is etched away, the overflowed resin covers the periphery of the hole. During grinding, the resin around the hole ring will be unevenly ground, and even the substrate will be worn, affecting the signal transmission of the finished circuit board. Summary of the invention
[0006] To solve the above problems, the present invention proposes a method for removing the hole ring of the PTH hole of a multilayer board by etching technology. The method does not require secondary depth-controlled drilling and directly removes unnecessary copper during the outer layer etching. The method has the advantages of simple process, convenient operation and low cost.
[0007] The main contents of the present invention include: a method for removing the PTH hole ring of a multilayer board by etching technology, comprising the following steps: the multilayer board includes a signal layer and multiple conductive layers from bottom to top; comprising the following steps:
[0008] S1, blanking and copper foil plating: plating copper foil on the outer surface of the signal layer to form an outer copper foil layer;
[0009] S2, drilling to form a through hole on the multilayer board, wherein the through hole penetrates the multiple conductive layers, the signal layer and the outer copper foil layer;
[0010] S3, electroplating: copper is plated in the through hole obtained in S2 to obtain a PTH hole, and the PTH hole penetrates the multiple conductive layers and the signal layer;
[0011] S4, plugging the PTH holes with resin and grinding;
[0012] S5, dry film pasting, exposure, development, etching: removing the outer copper foil layer during etching;
[0013] S6, ink printing, when printing ink, use 43T screen on the back-drilled side, print, expose and develop 4 times;
[0014] S7, molding, surface treatment, final inspection, etc. complete the production of circuit boards.
[0015] Preferably, in step S3, the copper thickness in the PTH hole is not less than 25 μm.
[0016] Preferably, in step S4, a vacuum plugging machine is used to plug the holes with resin to ensure that the holes are plugged in one go.
[0017] Preferably, in step S5, the etching pressure is 3.0 kg / cm 2 , down pressure 2.6kg / cm 2 , the etching times are two times.
[0018] Preferably, in step S6, the ink thickness is controlled to be above 100 μm. The purpose of tin plating in the reference document is to protect the copper in the hole from being etched. The present invention does not require a tin plating process. The present invention uses resin plug holes to protect the copper in the PTH through hole from being corroded during etching. In the reference document, secondary copper plating is required to meet the finished copper thickness. In the present invention, only one copper plating is required, and the process is relatively simple.
[0019] The beneficial effects of the present invention are:
[0020] 1. Use etching to remove unnecessary copper from the target signal layer without adding a back-drilling process. The process is simple and the cost is low.
[0021] 2. Back drilling requires controlling the drilling depth. Unstable depth control will cause product scrapping. Using etching instead of back drilling can reduce scrapping caused by back drilling and improve product yield. DETAILED DESCRIPTION
[0022] The technical solution protected by the present invention will be described in detail below.
[0023] The present invention discloses a method for removing the hole ring of a PTH hole of a multilayer board by etching technology. The multilayer board includes a signal layer and multiple conductive layers from bottom to top. The purpose of the present invention is to remove the hole ring of the conductive hole on the surface of the signal layer. Specifically, the present invention includes the following steps:
[0024] S1: blanking and copper foil plating, that is, plating copper foil on the outer surface of the signal layer to form an outer copper foil layer.
[0025] For a five-layer circuit board, from top to bottom, there are the first conductive layer, the second conductive layer, the third conductive layer, the fourth conductive layer and the fifth conductive layer, wherein the fifth conductive layer is the signal layer, and the copper foil is added to the lower surface of the fifth conductive layer, which is called the sixth conductive layer, and the sixth conductive layer is the outer copper foil layer. There is a dielectric layer between the fifth conductive layer and the sixth conductive layer.
[0026] S2: drilling, drilling the multilayer board to obtain a through hole, the through hole passes through the multilayer board, that is, passes through the multiple conductive layers, the signal layer and the outer copper foil layer;
[0027] S3: electroplating, that is, plating copper in the through hole in the board to obtain a PTH hole. This step ensures that the hole copper thickness is at least 25μm; so that the hole ring is formed on the sixth conductive layer, that is, the outer copper foil layer.
[0028] S4: The PTH hole is plugged with resin and ground. The resin plugging machine is used to plug the hole with a vacuum plugging machine to ensure that the hole is plugged with one knife, thereby ensuring that there are no bubbles in the resin in the hole;
[0029] S5: Dry film pasting, exposure, development, etching. When etching, remove the outer copper layer where the PTH hole is needed and the copper layer that is not needed on the board surface; the etching pressure is 3.0kg / cm 2 , down pressure 2.6kg / cm 2 , etched twice to ensure uniformity of line width;
[0030] S6: Ink printing, when printing ink, use 43T screen on one side of the PTH hole, print, expose and develop 4 times, and control the ink thickness to be more than 100μm;
[0031] S7: Forming, surface treatment, final inspection, etc. complete the production of circuit boards.
[0032] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A method for removing PTH hole rings of a multilayer board using etching technology, wherein the multilayer board includes a signal layer and multiple conductive layers from bottom to top; It is characterized in that The method is to remove the hole ring of the via hole on the surface of the signal layer, comprising the following steps: S1, blanking and copper foil plating: copper foil is plated on the outer surface of the signal layer to form an outer copper foil layer, and a dielectric layer is provided between the outer copper foil layer and the signal layer; S2, drilling to form a through hole on the multilayer board, wherein the through hole penetrates the multiple conductive layers, the signal layer and the outer copper foil layer; S3, electroplating: copper is plated in the through hole obtained in S2 to obtain a PTH hole, and the PTH hole penetrates the multiple conductive layers and the signal layer; S4, plugging the PTH holes with resin and grinding; S5, dry film pasting, exposure, development, etching: removing the outer copper foil layer during etching; S6, ink printing, when printing ink, use 43T screen on the back-drilled side, print, expose and develop 4 times; S7, molding, surface treatment and final inspection complete the production of circuit boards.
2. A method for removing the PTH hole ring of a multilayer board by etching technology according to claim 1, It is characterized in that In step S3, the copper thickness in the PTH hole is not less than 25 μm.
3. A method for removing the PTH hole ring of a multilayer board by etching technology according to claim 1, It is characterized in that In step S4, a vacuum plugging machine is used to plug the holes with resin to ensure that the holes are plugged in one go.
4. A method for removing PTH hole rings of multilayer boards by etching technology according to claim 1, It is characterized in that In step S5, the etching pressure is increased to 3.0 kg / cm 2 , down pressure 2.6kg / cm 2 , the etching times are two times.
5. A method for removing PTH hole rings of multilayer boards by etching technology according to claim 1, It is characterized in that In step S6, the ink thickness is controlled to be above 100 μm.