High reliability wide window super junction MOSFET structure and manufacturing method
By arranging conductive type pillars and well regions in the superjunction MOSFET structure, it is ensured that the breakdown point appears in the active region, which solves the problem of the breakdown point appearing outside the existing technology caused by the deviation of the total amount of impurities, and improves the performance of the device. reliability and reduced manufacturing costs.
Patent Information
- Application Number
- CN202011227243.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-11-06
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2040-11-06
AI Technical Summary
When the total amount of impurities in existing superjunction power MOSFET devices shifts, the breakdown point is likely to appear outside the device, resulting in reduced avalanche resistance and unusability.
A high-reliability, wide-window superjunction MOSFET structure is designed by arranging second conductivity type pillars and first conductivity type pillars in the active area, and arranging second conductivity type first well areas and second conductivity type pillars in between. Type 2 well area ensures that the breakdown point appears in the active area. Specific manufacturing methods include selective etching, deposition, injecting impurities and forming an insulating dielectric layer to ensure the reliability of the device.
When the total amount of impurities shifts, the breakdown point always appears in the active area, which improves the reliability of the device, reduces manufacturing costs, and is compatible with existing processes.
Smart Images

Figure CN112216744B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a semiconductor device and a manufacturing method thereof, in particular to a high-reliability wide-window super junction MOSFET structure and a manufacturing method thereof. Background Art
[0002] At present, there are two manufacturing methods for super junction power devices. The first is multiple epitaxy and multiple impurity injections, and the second is deepening the trench for filling. Both methods have some fluctuations in the process. These fluctuations will cause the total amount of impurities in the second conductive type column 5 and the first conductive type column 4 to shift, resulting in the charge balance being broken.
[0003] like Fig.14 As shown, an existing super junction power MOSFET structure is provided, an active area 001 is provided at the center of the chip, a terminal area 002 is provided on the outside of the active area 001, and no second conductive type first well area 15 and second conductive type second well area 7 are provided in the active area 001. When the total amount of impurities in the second conductive type column 5 is less than the total amount of impurities in the first conductive type column 4 to a certain extent, a breakdown weak point may appear at a position of the terminal close to the surface. When the total amount of impurities in the second conductive type column 5 is greater than the total amount of impurities in the first conductive type column 4 to a certain extent, a breakdown weak point may appear at the bottom of the second conductive type column 5 near the active area 001. When an obvious breakdown weak point appears at the terminal, the avalanche tolerance of the device will be significantly reduced, resulting in the device being unusable. Summary of the invention
[0004] The purpose of the present invention is to overcome the deficiencies in the prior art and to provide a high-reliability wide-window super junction MOSFET structure and a manufacturing method in which the breakdown point still appears in the active region when the total amount of impurities shifts.
[0005] According to the technical solution provided by the present invention, the high-reliability wide-window super junction MOSFET structure includes a drain metal, a first conductive type substrate located on the drain metal, and a first conductive type epitaxial layer located on the first conductive type substrate, a second conductive type column is arranged in the first conductive type epitaxial layer, a first conductive type column is arranged between adjacent second conductive type columns, an active area is arranged in the center area of the device, a transition area is arranged at the periphery of the active area, and a terminal area is arranged at the periphery of the transition area;
[0006] In the terminal region, a field oxide layer is provided above the first conductive type epitaxial layer, a gate bus polysilicon is provided above the field oxide layer near the transition region, an insulating dielectric layer is provided above the gate bus polysilicon, and a source metal is provided above the insulating dielectric layer near the transition region;
[0007] In the active area, a second conductive type body region is provided above the second conductive type column, a first conductive type source region is provided in the second conductive type body region, a gate oxide layer is provided above the first conductive type column, a gate polysilicon is provided above the gate oxide layer, an insulating dielectric layer is provided above the gate polysilicon and the gate oxide layer, a source metal is provided above the insulating dielectric layer, the source metal completely covers the upper surface of the active area, and the source metal is in ohmic contact with the first conductive type source region and the second conductive type body region through a through hole; a block-shaped second conductive type first well region is provided at intervals between corresponding adjacent second conductive type body regions and on the top of the same first conductive type column; a second conductive type second well region is provided in the top of the second conductive type column directly below the corresponding second conductive type body region;
[0008] In the transition zone, a second conductive type body region is provided above the second conductive type column, a first conductive type source region is provided in the second conductive type body region, a gate oxide layer is provided above the first conductive type column, a gate polysilicon is provided above the gate oxide layer, an insulating dielectric layer is provided above the gate polysilicon and the gate oxide layer, and a source metal is provided above the insulating dielectric layer. The source metal completely covers the upper surface of the transition zone, and the source metal is in ohmic contact with the first conductive type source region and the second conductive type body region through a through hole.
[0009] Preferably, in the active area, at the top of the same first conductivity type column, the center distance between adjacent second conductivity type first well regions is greater than or equal to 3 um.
[0010] Preferably, in the active area, in the direction in which the second conductivity type column extends, the length of the second conductivity type first well region is greater than or equal to 2 um.
[0011] Preferably, in the active area, a second conductive type first well region is provided on the top of each first conductive type column.
[0012] Preferably, in the active area, the second conductive type first well region is arranged on top of a plurality of first conductive type columns.
[0013] Preferably, in the active area, the doping concentration of the second conductivity type second well region is higher than the doping concentration of the second conductivity type column.
[0014] Preferably, in the active area, the second conductive type second well region is provided in the top of part or all of the second conductive type columns directly below the corresponding second conductive type body region.
[0015] Preferably, for an N-type power semiconductor device, the first conductivity type is N-type conductivity, and the second conductivity type is P-type conductivity; for a P-type power semiconductor device, the first conductivity type is P-type conductivity, and the second conductivity type is N-type conductivity.
[0016] The manufacturing method of the above-mentioned high-reliability wide-window super junction MOSFET structure comprises the following steps:
[0017] Step 1: forming a first conductive type epitaxial layer on a first conductive type substrate, and then selectively etching a deep trench;
[0018] Step 2: depositing a second conductive type semiconductor to fill the deep trench in step 1, and then removing the second conductive type semiconductor above the first conductive type epitaxial layer to form a second conductive type column and a first conductive type column;
[0019] Step 3: selectively injecting second conductivity type impurities and forming a second conductivity type body region after annealing;
[0020] Step 4: injecting second conductivity type impurities into the top of the second conductivity type column in the active area to form a second conductivity type second well region after activation;
[0021] Step 5: forming a field oxide layer on the surface of the device;
[0022] Step 6: Selectively remove the field oxide layer in the active area and transition area;
[0023] Step 7: forming a gate oxide layer on the surface of the device;
[0024] Step 8: After depositing conductive polysilicon, selectively etching the conductive polysilicon to form gate polysilicon and gate bus polysilicon;
[0025] Step nine: selectively injecting first conductivity type impurities to form a first conductivity type source region after activation;
[0026] Step 10: depositing an insulating dielectric layer;
[0027] Step 11: selectively etching the insulating dielectric layer and the semiconductor to form a through hole;
[0028] Step 12: Form source metal and drain metal.
[0029] The manufacturing method of the above-mentioned high-reliability wide-window super junction MOSFET structure comprises the following steps:
[0030] Step 1: forming a first conductive type epitaxial layer on a first conductive type substrate, and then selectively etching a deep trench;
[0031] Step 2: depositing a second conductive type semiconductor to fill the deep trench in step 1, and then removing the second conductive type semiconductor above the first conductive type epitaxial layer to form a second conductive type column and a first conductive type column;
[0032] Step 3: selectively injecting second conductivity type impurities, and forming a second conductivity type body region and a second conductivity type first well region after annealing;
[0033] Step 4: injecting second conductivity type impurities into the top of the second conductivity type column in the active area to form a second conductivity type second well region after activation;
[0034] Step 5: forming a field oxide layer on the surface of the device;
[0035] Step 6: Selectively remove the field oxide layer in the active area and transition area;
[0036] Step 7: forming a gate oxide layer on the surface of the device;
[0037] Step 8: After depositing conductive polysilicon, selectively etching the conductive polysilicon to form gate polysilicon and gate bus polysilicon;
[0038] Step nine: selectively injecting first conductivity type impurities to form a first conductivity type source region after activation;
[0039] Step 10: depositing an insulating dielectric layer;
[0040] Step 11: selectively etching the insulating dielectric layer and the semiconductor to form a through hole;
[0041] Step 12: Form source metal and drain metal.
[0042] The high-reliability wide-window super junction MOSFET structure and manufacturing method provided by the present invention have the following advantages compared with the prior art:
[0043] 1. When the total amount of impurities in the second conductive type column is less than the total amount of impurities in the first conductive type column to a certain extent, a breakdown weak point will appear at the bottom of the second conductive type second well region. When the total amount of impurities in the second conductive type column is greater than the total amount of impurities in the first conductive type column to a certain extent, a breakdown weak point will appear below the second conductive type first well region. The breakdown points can all appear in the active area, ensuring the reliability of the device.
[0044] 2. The manufacturing process of the present invention is compatible with the existing process and can reduce the manufacturing cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Figure 1 It is a schematic cross-sectional structure diagram of forming a deep groove according to the present invention.
[0046] Figure 2The cross-sectional structure diagram of forming the second conductive type column and the first conductive type column according to the present invention.
[0047] Figure 3 The cross-sectional structure diagram of forming a second conductivity type body region and a second conductivity type first well region of the present invention.
[0048] Figure 4 The cross-sectional structure diagram of forming a second conductive type second well region of the present invention.
[0049] Figure 5 It is a schematic diagram of the cross-sectional structure of forming a field oxide layer in the present invention.
[0050] Figure 6 It is a schematic cross-sectional structure diagram of removing the field oxide layer in the active region and the transition region according to the present invention.
[0051] Figure 7 It is a schematic diagram of the cross-sectional structure of forming a gate oxide layer in the present invention.
[0052] Figure 8 The cross-sectional structure diagram of forming gate polysilicon and gate bus polysilicon according to the present invention.
[0053] Fig. 9 The cross-sectional structure diagram of forming a first conductive type source region of the present invention.
[0054] Fig.10 It is a schematic diagram of the cross-sectional structure of forming an insulating dielectric layer according to the present invention.
[0055] Fig.11 It is a schematic cross-sectional structure diagram of forming a through hole according to the present invention.
[0056] Fig.12 The schematic diagram of the cross-sectional structure of the source metal and the drain metal formed by the present invention is also along the Fig.15 Schematic diagram of the cross-sectional structure cut by the middle dotted line AB.
[0057] Fig.13 For the present invention along Fig.15 Schematic diagram of the cross-sectional structure cut along the middle dotted line CD.
[0058] Fig.14 It is a schematic diagram of the cross-sectional structure of the traditional structure.
[0059] Fig.15 It is a schematic diagram of an implantation window when forming a second conductivity type body region and a second conductivity type first well region according to the present invention.
[0060] Fig.16 It is another schematic diagram of an implantation window when forming a second conductivity type body region and a second conductivity type first well region according to the present invention. DETAILED DESCRIPTION
[0061] The present invention will be further described below in conjunction with specific embodiments.
[0062] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments and with reference to the accompanying drawings. The same parts are represented by the same figure numerals. It should be noted that the words "front", "rear", "left", "right", "up" and "down" used in the following description refer to the directions in the accompanying drawings. The words "inside" and "outside" used refer to the direction toward or away from the geometric center of a specific component, respectively.
[0063] A first aspect of the present invention provides a semiconductor structure for reducing switching losses, which includes the following embodiments. It should be explained that for N-type power semiconductor devices, the first conductivity type described in the present invention is N-type conductivity, and the second conductivity type is P-type conductivity; for P-type power semiconductor devices, the first conductivity type described in the present invention is P-type conductivity, and the second conductivity type is N-type conductivity.
[0064] Example 1
[0065] A high-reliability wide-window super junction MOSFET structure, comprising a drain metal 1, a first conductive type substrate 2 located on the drain metal 1, and a first conductive type epitaxial layer 3 located on the first conductive type substrate 2, a second conductive type column 4 is arranged in the first conductive type epitaxial layer 3, a first conductive type column 5 is arranged between adjacent second conductive type columns 4, an active area 001 is arranged in the center area of the device, a transition area 003 is arranged outside the active area 001, and a terminal area 002 is arranged outside the transition area 003;
[0066] In the terminal region 002, a field oxide layer 13 is provided above the first conductive type epitaxial layer 3, a gate bus polysilicon 14 is provided above the field oxide layer 13 near the transition region 003, an insulating dielectric layer 11 is provided above the gate bus polysilicon 14, and a source metal 12 is provided above the insulating dielectric layer 11 near the transition region 003;
[0067] In the active area 001, a second conductive type body region 6 is provided above the second conductive type column 4, a first conductive type source region 8 is provided in the second conductive type body region 6, a gate oxide layer 9 is provided above the first conductive type column 5, a gate polysilicon 10 is provided above the gate oxide layer 9, an insulating dielectric layer 11 is provided above the gate polysilicon 10 and the gate oxide layer 9, and a source metal 12 is provided above the insulating dielectric layer 11, the source metal 12 completely covers the upper surface of the active area 001, and the source metal 12 is in ohmic contact with the first conductive type source region 8 and the second conductive type body region 6 through a through hole; in the active area 001, a block-shaped second conductive type first well region 15 is provided at intervals between the corresponding adjacent second conductive type body regions 6 and on the top of the same first conductive type column 5; a second conductive type second well region 7 is provided in the top of the second conductive type column 4 directly below the corresponding second conductive type body region 6;
[0068] In the transition zone 003, a second conductive type body region 6 is provided above the second conductive type column 4, a first conductive type source region 8 is provided in the second conductive type body region 6, a gate oxide layer 9 is provided above the first conductive type column 5, a gate polysilicon 10 is provided above the gate oxide layer 9, an insulating dielectric layer 11 is provided above the gate polysilicon 10 and the gate oxide layer 9, and a source metal 12 is provided above the insulating dielectric layer 11. The source metal 12 completely covers the upper surface of the transition zone 003, and the source metal 12 is in ohmic contact with the first conductive type source region 8 and the second conductive type body region 6 through a through hole.
[0069] In the active area 001, at the top of the same first conductive type column 5, the center distance between adjacent second conductive type first well regions 15 is greater than or equal to 3um; and in the extension direction of the second conductive type column 4, the length of the second conductive type first well region 15 is greater than or equal to 2um.
[0070] In the active area 001 , the second conductive type first well region 15 may be disposed on the top of each first conductive type column 5 .
[0071] In the active area 001 , the second conductive type first well region 15 may also be disposed on top of a plurality of first conductive type columns 5 .
[0072] In the active area 001 , the doping concentration of the second conductivity type second well region 7 is higher than the doping concentration of the second conductivity type column 4 .
[0073] In the active area 001 , the second conductive type second well region 7 is provided in the top of part or all of the second conductive type columns 4 directly below the corresponding second conductive type body region 6 .
[0074] For an N-type power semiconductor device, the first conductivity type is N-type conductivity and the second conductivity type is P-type conductivity; for a P-type power semiconductor device, the first conductivity type is P-type conductivity and the second conductivity type is N-type conductivity.
[0075] The manufacturing method of the above-mentioned high-reliability wide-window super junction MOSFET structure comprises the following steps:
[0076] Step 1: forming a first conductive type epitaxial layer 3 on a first conductive type substrate 2, and then selectively etching a deep trench;
[0077] Step 2: depositing a second conductive type semiconductor to fill the deep trench in step 1, and then removing the second conductive type semiconductor above the first conductive type epitaxial layer 3 to form a second conductive type column 4 and a first conductive type column 5;
[0078] Step 3: selectively injecting second conductivity type impurities, and forming a second conductivity type body region 6 and a second conductivity type first well region 15 after annealing;
[0079] Step 4: injecting second conductivity type impurities into the top of the second conductivity type column 4 in the active area 001 to form a second conductivity type second well region 7 after activation;
[0080] Step 5: forming a field oxide layer 13 on the surface of the device;
[0081] Step 6: selectively removing the field oxide layer 13 of the active area 001 and the transition area 003;
[0082] Step 7: forming a gate oxide layer 9 on the surface of the device;
[0083] Step 8: After depositing conductive polysilicon, selectively etching the conductive polysilicon to form gate polysilicon 10 and gate bus polysilicon 14;
[0084] Step nine: selectively injecting first conductivity type impurities to form first conductivity type source regions 8 after activation;
[0085] Step 10: depositing an insulating dielectric layer 11;
[0086] Step 11: selectively etching the insulating dielectric layer 11 and the semiconductor to form a through hole;
[0087] Step 12: Forming source metal 12 and drain metal 1.
[0088] Those skilled in the art should understand that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit of the present invention should be included in the protection scope of the present invention.
Claims
1. A high-reliability wide-window super junction MOSFET structure, comprising a drain metal (1), a first conductive type substrate (2) located on the drain metal (1), and a first conductive type epitaxial layer (3) located on the first conductive type substrate (2), a second conductive type column (4) being arranged in the first conductive type epitaxial layer (3), a first conductive type column (5) being arranged between adjacent second conductive type columns (4), an active region (001) being arranged in a device center region, a transition region (003) being arranged at the periphery of the active region (001), and a terminal region (002) being arranged at the periphery of the transition region (003); In the terminal region (002), a field oxide layer (13) is provided above the first conductive type epitaxial layer (3), a gate bus polysilicon (14) is provided above the field oxide layer (13) and near the transition region (003), an insulating dielectric layer (11) is provided above the gate bus polysilicon (14), and a source metal (12) is provided above the insulating dielectric layer (11) near the transition region (003); In the active area (001), a second conductive type body region (6) is provided above the second conductive type column (4), a first conductive type source region (8) is provided in the second conductive type body region (6), a gate oxide layer (9) is provided above the first conductive type column (5), a gate polysilicon (10) is provided above the gate oxide layer (9), an insulating dielectric layer (11) is provided above the gate polysilicon (10) and the gate oxide layer (9), a source metal (12) is provided above the insulating dielectric layer (11), the source metal (12) completely covers the upper surface of the active area (001), and the source metal (12) is in ohmic contact with the first conductive type source region (8) and the second conductive type body region (6) through a through hole; the invention is characterized in that: In the active area (001), a block-shaped second conductive type first well region (15) is provided at intervals between corresponding adjacent second conductive type body regions (6) and on the top of the same first conductive type column (5); and a second conductive type second well region (7) is provided in the top of the second conductive type column (4) directly below the corresponding second conductive type body region (6); In the transition region (003), a second conductive type body region (6) is provided above the second conductive type column (4), a first conductive type source region (8) is provided in the second conductive type body region (6), a gate oxide layer (9) is provided above the first conductive type column (5), a gate polysilicon (10) is provided above the gate oxide layer (9), an insulating dielectric layer (11) is provided above the gate polysilicon (10) and the gate oxide layer (9), a source metal (12) is provided above the insulating dielectric layer (11), the source metal (12) completely covers the upper surface of the transition region (003), and the source metal (12) is in ohmic contact with the first conductive type source region (8) and the second conductive type body region (6) through a through hole; In the active area (001), at the top of the same first conductive type column (5), the center spacing between adjacent second conductive type first well regions (15) is greater than or equal to 3 um; In the active area (001), in the direction in which the second conductive type column (4) extends, the length of the second conductive type first well region (15) is greater than or equal to 2 um; In the active area (001), the doping concentration of the second conductive type second well area (7) is higher than the doping concentration of the second conductive type column (4); In the active area (001), the second conductive type second well area (7) is provided in the top of part or all of the second conductive type columns (4) directly below the corresponding second conductive type body area (6).
2. The high reliability wide window super junction MOSFET structure according to claim 1, characterized in that: In the active area (001), the second conductive type first well area (15) is arranged on the top of each first conductive type column (5).
3. The high reliability wide window super junction MOSFET structure according to claim 1, characterized in that: For an N-type power semiconductor device, the first conductivity type is N-type conductivity and the second conductivity type is P-type conductivity; for a P-type power semiconductor device, the first conductivity type is P-type conductivity and the second conductivity type is N-type conductivity.
4. The method for manufacturing the high reliability wide window super junction MOSFET structure according to claim 1 comprises the following steps: Step 1: forming a first conductivity type epitaxial layer (3) on a first conductivity type substrate (2), and then selectively etching a deep trench; Step 2: depositing a second conductive type semiconductor to fill the deep trench in step 1, and then removing the second conductive type semiconductor above the first conductive type epitaxial layer (3) to form a second conductive type column (4) and a first conductive type column (5); Step 3: selectively injecting second conductivity type impurities, and forming a second conductivity type body region (6) and a second conductivity type first well region (15) after annealing; Step 4: injecting second conductivity type impurities into the top of the second conductivity type column (4) in the active area (001), and forming a second conductivity type second well region (7) after activation; Step 5: forming a field oxide layer (13) on the surface of the device; Step 6: selectively removing the field oxide layer (13) of the active region (001) and the transition region (003); Step 7: forming a gate oxide layer (9) on the surface of the device; Step 8: After depositing conductive polysilicon, selectively etching the conductive polysilicon to form gate polysilicon (10) and gate bus polysilicon (14); Step nine: selectively injecting first conductivity type impurities to form a first conductivity type source region (8) after activation; Step 10: depositing an insulating dielectric layer (11); Step 11: selectively etching the insulating dielectric layer (11) and the semiconductor to form a through hole; Step 12: Forming source metal (12) and drain metal (1).
Citation Information
Patent Citations
Multi-epitaxial super-junction terminal structure and manufacturing method thereof
CN109509784A
High-reliability wide-window super-junction MOSFET structure
CN213150785U