Diffusion barrier film to achieve lithium stability
By using refractory metal/metal nitride diffusion barrier film and wetting layer in lithium-ion batteries, the instability problem of the interface between lithium metal and copper substrate is solved, and the cycle life and safety of the battery are improved.
Patent Information
- Application Number
- CN201980039543.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-06-21
- Filing Date
- 2019-06-18
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2039-06-18
AI Technical Summary
The unstable interface between lithium metal and copper substrate in lithium-ion batteries leads to lithium diffusion and copper-induced embrittlement, affecting the cycle life and safety of the battery.
Form a refractory metal/metal nitride diffusion barrier film on the copper foil, including titanium, molybdenum, tantalum and other materials, and further form a wetting layer and lithium metal layer on it to ensure the time/thermal stability of the lithium metal/copper foil interface sex.
Improves the interfacial stability of lithium metal batteries, prevents lithium diffusion and copper-induced embrittlement, extends the battery cycle life and enhances mechanical properties.
Smart Images

Figure CN112292775B_ABST
Abstract
Description
background Technical Field
[0002] Implementations described herein relate generally to metal electrodes, and more particularly to lithium-containing anodes, high-performance electrochemical devices including the aforementioned lithium-containing electrodes, and methods of making the lithium-containing anodes and electrochemical devices, the high-performance electrochemical devices such as secondary batteries. Background Art
[0004] Rechargeable electrochemical storage systems are becoming increasingly important in many areas of daily life. High capacity electrochemical energy storage devices, such as lithium-ion (Li-ion) batteries, are used in an increasing number of applications, including portable electronics, medical, transportation, grid-connected large energy storage, renewable energy storage, and uninterruptible power supplies (UPS). Conventional lead / sulfuric acid batteries generally lack the capacity and are generally not cycled adequately for these increasing number of applications. However, lithium-ion batteries are considered the best opportunity.
[0005] Typically, for safety reasons, lithium-ion batteries do not contain any metallic lithium, but use graphite materials as anodes. However, the use of graphite that is chargeable up to the limiting component LiC6 in the charged state brings much lower capacitance values than the use of metallic lithium. Currently, the industry is shifting from graphite-based anodes to graphite blended with silicon to increase energy cell density. However, the graphite anode blended with silicon suffers from first cycle capacity loss. Therefore, what is needed is lithium metal deposition to supplement the first cycle capacity loss of the graphite anode blended with silicon. However, lithium metal faces several device integration challenges. For example, lithium deposition on a copper substrate may cause lithium-induced embrittlement of the copper substrate.
[0006] Therefore, what are needed are methods and systems for depositing and processing lithium metal in energy storage systems. Summary of the invention
[0007] The implementations described herein generally relate to metal electrodes, and more specifically to lithium-containing anodes, high-performance electrochemical devices including the aforementioned lithium-containing electrodes, and methods of manufacturing the lithium-containing anodes and electrochemical devices, the high-performance electrochemical devices, such as secondary batteries. In one implementation, an anode electrode is provided. The anode electrode includes a copper foil. The anode electrode further includes a first diffusion barrier layer, which is formed on the copper foil. The first diffusion barrier layer contains titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta), or a combination thereof. The anode electrode further includes a wetting layer, which is formed on the first diffusion barrier layer. The wetting layer is selected from silicon (Si), tin (Sn), aluminum (Al), germanium (Ge), antimony (Sb), lead (Pb), bismuth (Bi), gallium (Ga), indium (In), zinc (Zn), cadmium (Cd), magnesium (Mg), the above oxides, the above nitrides, or a combination thereof. The anode electrode further includes a lithium metal layer, which is formed on the wetting layer.
[0008] In another implementation, a method for forming an electrode structure is provided. The method includes forming a first diffusion barrier layer on a copper foil. The first diffusion barrier layer includes titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta), or a combination thereof. The method further includes forming a wetting layer on the first diffusion barrier layer. The wetting layer is selected from silicon (Si), tin (Sn), aluminum (Al), germanium (Ge), antimony (Sb), lead (Pb), bismuth (Bi), gallium (Ga), indium (In), zinc (Zn), cadmium (Cd), magnesium (Mg), the above oxides, the above nitrides, or a combination thereof. The method further includes forming a lithium metal layer on the wetting layer.
[0009] In yet another implementation, an integrated processing tool operable to form a lithium-coated negative electrode is provided. The integrated processing tool includes a reel-to-reel system operable to transport a continuous sheet of material through a series of processing chambers. The series of processing chambers further includes a first processing chamber operable to deposit a first diffusion barrier layer on the continuous sheet of material. The series of processing chambers further includes a second processing chamber operable to deposit a second diffusion barrier layer on the first diffusion barrier layer. The series of processing chambers further includes a third processing chamber operable to deposit a wetting layer on the second diffusion barrier layer. The series of processing chambers further includes a fourth processing chamber operable to deposit a thin lithium metal film on the second diffusion barrier layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] The above briefly summarizes the manner in which the above-described features of the present disclosure can be understood in detail, as well as a more specific description of implementations, which can be obtained by reference to implementations, some of which are illustrated in the accompanying drawings. However, it should be noted that the accompanying drawings only illustrate typical implementations of the present disclosure and should not be considered as limiting the scope of the present disclosure, as the present disclosure may allow other equally effective implementations.
[0011] Figure 1 A graph showing the depression of the melting point of lithium is illustrated;
[0012] Figure 2 illustrates a process flow diagram of one implementation of a method of forming an anode electrode structure according to an overview of implementations described herein;
[0013] FIG. 3A to FIG. 3D illustrates cross-sectional views of electrode structures at various stages of fabrication according to implementations described herein;
[0014] Figure 4 illustrates a cross-sectional view of one implementation of a battery structure having an electrode structure formed according to implementations described herein; and
[0015] Figure 5 Illustrated is a schematic diagram of an integrated processing tool operable to form electrode structures according to implementations described herein.
[0016] To facilitate understanding, identical reference numerals have been used, where possible, to designate identical elements that are common to the figures. It is contemplated that elements and / or features of one implementation may be beneficially incorporated in other implementations without further description. DETAILED DESCRIPTION
[0017] The following disclosure describes anode electrodes, high performance electrochemical cells and batteries including the aforementioned anode electrodes, and methods of making the anode electrodes, electrochemical cells and batteries. Figures 1 to 5 Certain details are set forth in order to provide a thorough understanding of various implementations of the present disclosure. Other details describing well-known structures and systems generally associated with electrochemical cells and batteries are not set forth in the following disclosure to avoid unnecessarily obscuring the description of various implementations.
[0018] Many of the details, dimensions, angles, and other features shown in the drawings illustrate only specific implementations. Therefore, other implementations may have other details, components, dimensions, angles, and features without departing from the spirit or scope of the present disclosure. In addition, other implementations of the present disclosure may be practiced without some of the details described below.
[0019] The implementations described herein will be described below with reference to a roll-to-roll coating system, such as a TopMet TM , TopBeam TM , all of which are available from Applied Materials, Inc. of Santa Clara, California. Other tools capable of performing physical vapor deposition processes (e.g., high rate evaporation processes and magnetron sputtering processes) may also be adapted to benefit from the implementations described herein. In addition, any system that implements the physical vapor deposition processes described herein may be advantageously used. The device descriptions described herein are illustrative and should not be understood or interpreted as limiting the scope of the implementations described herein. It should also be understood that, although described as a roll-to-roll process, the implementations described herein may also be performed on discrete substrates.
[0020] Figure 1 A graph 100 showing the reduction in the melting point of lithium from a first heating cycle to a second heating cycle is illustrated. The thermal stability of lithium metal / copper foil samples made using prior art processes was examined by differential scanning calorimetry (DSC). Figure 1 As shown. A 200 μm thick FMC lithium foil is laminated on two 12 μm thick Oak-Mitsui TM Copper foil and packaged with it. The first heating cycle showed a lithium starting melting point of 179.77 degrees Celsius and a peak melting point of 181.88 degrees Celsius. In contrast, the second heating cycle showed lithium melting points of 177.58 degrees Celsius and 179.26 degrees Celsius, respectively. The reduction in the melting point of lithium indicates that impurities (e.g., copper) are incorporated into lithium during lithium heating / melting. Therefore, the lithium metal / copper foil interface is unstable when lithium melts. In addition, the literature shows that lithium accumulation in copper foil current collectors can be measured. Therefore, experimental data confirm the necessity of forming a barrier film between the lithium film and the copper foil current collector, especially during high temperature manufacturing / storage.
[0021] The temporal / thermal stability of the lithium metal / copper foil current collector interface is critical to the operation of lithium metal batteries. Prior art techniques include directly laminating lithium foil or PVD (e.g., evaporating) lithium onto copper foil. Prior art copper foil is treated to produce a passivation-based chromate / zincate film. These passivation-based films are intended to improve corrosion protection properties compared to untreated copper foil, thus resulting in an increased shelf life. However, experience with lithium metal / copper foils has shown that the barrier properties of these passivation-based films are not sufficient to ensure the stability of the lithium metal / copper foil interface. As a result, lithium diffuses into the copper grain boundaries, which causes lithium-induced embrittlement of the copper current collector. In addition, incorporating copper into lithium prevents lithium phase purity and crystallization control (see Figure 1). As a result, the cycle life of the lithium metal anode is reduced. In some implementations of the present disclosure, the deposition of the barrier film described herein between the lithium film / copper foil solves the above-mentioned problem.
[0022] In some implementations of the present disclosure, a refractory metal diffusion barrier film is deposited on the copper foil to prevent / minimize undesirable interdiffusion processes that can cause interface degradation during lithium metal anode manufacturing and battery operation / storage. The deposition of the refractory metal / metal nitride barrier film described herein ensures the temporal / thermal stability of the lithium metal / copper foil current collector interface. Therefore, the lithium film / copper foil does not suffer degradation during operation as an anode in a lithium metal battery. In addition, the barrier film described herein prevents lithium-induced embrittlement of the copper foil, maintains mechanical properties, and minimizes foil tearing. Therefore, the barrier film described herein facilitates roll-to-roll processing of the copper foil.
[0023] Figure 2 Illustrated is a process flow diagram of one implementation of a processing sequence 200 for forming an anode electrode structure in accordance with an overview of implementations described herein. Figure 2 The processing sequence 200 described in FIG. 3A to FIG. 3D The manufacturing stages depicted in , which will be discussed below. FIG. 3A to FIG. 3D Illustrated are cross-sectional views of an anode electrode structure 300 at various stages of fabrication in accordance with implementations described herein. Although the anode electrode structure 300 is a double-sided electrode structure, implementations described herein are also applicable to single-sided electrode structures.
[0024] The processing sequence 200 begins at operation 210 by providing a copper substrate 310. In one implementation, the copper substrate 310 includes a flat plate, foil, or sheet of copper. The copper substrate 310 may have a thickness from about 0.5 μm to about 20 μm (e.g., from about 1 μm to about 10 μm; or from about 5 μm to about 10 μm). The copper substrate 310 may have any shape, such as square, circular, oval, rectangular, etc. In some implementations, the copper substrate 310 may be square or rectangular, or a sheet of x×y square or rectangular units, or a roll of x units wide, where each unit represents a separate, separable substrate for a single electrode structure. In one implementation, the copper substrate 310 includes a copper sheet that is stored on a roll and used in a roll-to-roll tool, such as Figure 5 The roll-to-roll tool shown in FIG.
[0025] Optionally, at operation 210, the copper substrate is exposed to a pretreatment process. The pretreatment process is generally a pre-cleaning process performed prior to depositing the first diffusion barrier layer at operation 210. The pre-cleaning process may remove, for example, residues from processing raw materials used to prepare the copper substrate 310, residual organic materials, particles, and / or other contaminants that may adversely affect the adhesion of the first diffusion barrier layer 320a, 320b (collectively, 320) to the surface of the copper substrate 310. Pre-cleaning the copper substrate 310 may include wet cleaning and / or dry cleaning.
[0026] Suitable etching techniques for the pre-cleaning process may include a wet etching process (e.g., wet chemical etching) or dry etching (e.g., reactive ion etching or sputter etching). In one implementation, the copper substrate 310 is cleaned by immersing the substrate in a liquid phase cleaner (e.g., a liquid phase cleaner that removes organic residues) and / or rinsing the substrate with it, followed by wet etching using a dilute acid aqueous solution (e.g., a dilute HF aqueous solution that can be buffered with ammonia and / or ammonium fluoride). Alternative acids for wet etching the copper substrate 310 include nitric acid, sulfuric acid, hydrochloric acid, etc., depending on the grade of copper used and the processing temperature of the copper substrate 310. In another implementation, the copper substrate 310 is cleaned by sputter etching. The selection of the gas used in the dry etching process to clean the copper substrate 310 is not particularly limited. Any gas or gas combination that removes substantially all undesirable contaminants from the surface of the copper substrate 310 but does not leave permanent residues can be used. For example, an inert gas such as argon can be used in the sputter cleaning of the copper substrate 310.
[0027] In one implementation, the pre-cleaning process of operation 220 includes annealing the copper substrate 310 in a forming gas (H2 / N2) environment. In another implementation, the pre-cleaning process of operation 220 includes annealing the copper substrate 310 in a hydrogen and argon (H2 / Ar) environment. In one implementation, the processing temperature during the pre-cleaning process of operation 220 is between about 50 degrees Celsius and about 150 degrees Celsius (e.g., between about 80 degrees Celsius and about 150 degrees Celsius; or between about 100 degrees Celsius and about 150 degrees Celsius). In one implementation, the pre-cleaning process of operation 220 includes passing the copper substrate 310 between rollers and pressing it to reduce the roughness of the copper substrate 310.
[0028] Reference now Figure 3AAt operation 230, a first diffusion barrier layer deposition process is performed to deposit first diffusion barrier layers 320a, 320b (collectively referred to as 320) on the copper substrate 310. The first diffusion barrier layer 320 serves as a copper diffusion barrier. The first diffusion barrier layer 320 generally comprises a refractory metal and / or a refractory metal nitride. In one implementation, the refractory metal is selected from molybdenum (Mo), tungsten (W), tantalum (Ta), niobium (Nb), titanium (Ti), or a combination thereof. In one implementation, the refractory metal nitride is selected from titanium nitride (TiN), tungsten nitride (WN), tantalum nitride, or a combination thereof. In one implementation, the first diffusion barrier layer 320 is a tantalum layer. In another implementation, the first diffusion barrier layer 320 is a tantalum nitride layer. The first diffusion barrier layer 320 may have a thickness of from about to about within the range of about to about within the range of about to about within the range of about to about within the range of about to about within the range of about to about within the range of about to about and more narrowly within the range from about to about The first diffusion barrier layer 320 is generally deposited by atomic layer deposition (ALD), plasma enhanced ALD (PE-ALD), chemical vapor deposition (CVD), or physical vapor deposition (PVD) processes. In one implementation, operation 230 is a PVD process performed by a DC magnetron sputtering process. In one implementation, the DC magnetron sputtering process is performed at room temperature. In one implementation of the PVD process, the base pressure is 10 - 7 mbar, the process temperature is in the range between room temperature and 100 degrees Celsius, and the target DC power is in the range of about 2 kW to about 10 kW.
[0029] In one implementation, the first diffusion barrier layer 320 is a tantalum layer deposited by a PVD sputtering process using a tantalum target. In another implementation, the first diffusion barrier layer 320 is a tantalum nitride layer deposited by a PVD sputtering process using a tantalum target in a nitrogen-containing environment or using a tantalum nitride target.
[0030] Reference now Figure 3BOptionally, at operation 240, a second diffusion barrier layer 330 deposition process is performed to deposit the second diffusion barrier layer 330 on the first diffusion barrier layer 320 to form a double barrier layer. The second diffusion barrier layer 330 serves as a lithium diffusion barrier. The second diffusion barrier layer 330 generally comprises a refractory metal and / or a refractory metal nitride. The refractory metal and / or refractory metal nitride of the second diffusion barrier layer 330 is different from the refractory metal and / or refractory metal nitride of the first diffusion barrier layer 320. In one implementation, the refractory metal is selected from molybdenum (Mo), tungsten (W), tantalum (Ta), niobium (Nb), titanium (Ti), or a combination thereof. In one implementation, the refractory metal nitride is selected from titanium nitride (TiN), tungsten nitride (WN), tantalum nitride, or a combination thereof. In one implementation, the second diffusion barrier layer 330 is a titanium layer. In another implementation, the second diffusion barrier layer 330 is a titanium nitride layer. The second diffusion barrier layer 330 may have a thickness of from about to about within the range of about to about within the range of about to about within the range of about to about within the range of about to about within the range of about to about and more narrowly within the range from about to about The second diffusion barrier layer 330 is generally deposited by atomic layer deposition (ALD), plasma enhanced ALD (PE-ALD), chemical vapor deposition (CVD), or physical vapor deposition (PVD) processes. In one implementation, operation 240 is a PVD process performed by a DC magnetron sputtering process performed at room temperature. In one implementation of the PVD process, the base pressure is 10 -7 mbar, the process temperature is in the range between room temperature and 100 degrees Celsius, and the target DC power is in the range of about 2 kW to about 10 kW.
[0031] In one implementation, the second diffusion barrier layer 330 is a titanium layer deposited by a PVD sputtering process using a titanium target. In another implementation, the second diffusion barrier layer 330 is a titanium nitride layer deposited by a PVD sputtering process using a titanium target in a nitrogen-containing environment or using a titanium nitride target.
[0032] Reference now Figure 3COptionally, at operation 250, a wetting layer deposition process is performed to deposit wetting layers 340a, 340b (collectively 340) on the underlying first diffusion barrier layer 320 or the underlying second diffusion barrier layer 330 (if present). The wetting layer 340 generally enhances the adhesion of the lithium metal layer 350a, 350b (collectively 350) to the underlying barrier material. The wetting layer 340 generally comprises a lithium alloying element or compound. In one implementation, the wetting layer 340 may be made of a material that can directly bond with lithium or have a high contact angle. For example, Si, Sn, Al all form alloys with lithium and oxides (e.g., SiO x SnO x and AlO x (x varies from 0 to a certain number to match the highest oxidation state to achieve charge balance). In one implementation, the wetting layer 340 is composed of a material selected from the group consisting of silicon (Si), tin (Sn), aluminum (Al), germanium (Ge), antimony (Sb), lead (Pb), bismuth (Bi), gallium (Ga), indium (In), zinc (Zn), cadmium (Cd), magnesium (Mg), carbon (C), oxides thereof, nitrides thereof, or combinations thereof. In one implementation, the wetting layer 340 is composed of a material selected from the group consisting of silicon (Si), tin (Sn), aluminum (Al), silicon oxide, tin oxide, or combinations thereof. In one implementation, the wetting layer 340 has a thickness from about 1 nm to about 200 nm (e.g., from about 5 nm to about 50 nm; from about 5 nm to about 20 nm; or from about 5 nm to about 10 nm). In one implementation, the wetting layer 340 is silicon or a silicon-containing film.
[0033] Reference now Figure 3DAt operation 260, a lithium metal layer deposition process is performed to deposit a lithium metal layer 350 on the underlying barrier layer or wetting layer 340 (if present) to form the anode electrode structure 300. In some implementations where the optional wetting layer 340 is present, the lithium metal layer 350 is formed on the wetting layer 340. In some implementations, the lithium metal layer 350 is formed directly on the underlying first diffusion barrier layer 320 or the underlying second diffusion barrier layer 330 (if present). The lithium metal layer 350 may be composed of lithium metal, lithium metal foil or lithium alloy foil (e.g., lithium aluminum alloy), or a mixture of lithium metal and / or lithium alloy with materials such as carbon (e.g., coke, graphite), nickel, copper, tin, indium, silicon, oxides of the foregoing, or combinations thereof. In one implementation, the lithium metal layer 350 is a lithium metal alloy layer that forms an alloy with the underlying wetting layer 340 (if present). In one implementation, the lithium metal layer 350 typically includes an intercalation compound containing lithium or an insertion compound containing lithium. In one implementation, a printing method can be used to deposit the lithium metal layer 350. In one implementation, the lithium metal layer 350 is laminated to the underlying structure to form the anode structure 300. In one implementation, the lithium metal layer 350 is a lithium foil that is laminated to the underlying structure, which includes a barrier film formed on a copper foil by passing the lithium foil and the underlying structure between two rollers. In some implementations, the lithium metal layer 350 can be formed by physical or chemical thin film techniques, such as sputtering, electron beam evaporation, thermal evaporation, chemical vapor deposition (CVD), three-dimensional printing, etc. In one implementation, the lithium metal layer 350 has a thickness of from about 1 μm to about 50 μm (e.g., from about 3 μm to about 40 μm; from about 3 μm to about 20 μm; or from about 20 μm to about 40 μm).
[0034] In some implementations, the formed anode electrode structure 300 is exposed to additional processing, such as depositing a protective film on the anode electrode structure.
[0035] Figure 4 A cross-sectional view of one implementation of a battery structure 400 having an electrode structure 300 formed according to the implementations described herein is illustrated. In some implementations, the battery structure 400 is a rechargeable battery cell. In some implementations, the battery structure 400 is a capacitor (e.g., a supercapacitor or ultracapacitor). In some implementations, the battery structure 400 is a solid-state battery structure. In some implementations, the battery structure 400 is combined with other battery cells to form a rechargeable battery or capacitor. The battery structure 400 includes a cathode electrode structure 410 and an anode electrode structure 300 separated by a separator 420. The cathode electrode structure 410 includes a cathode current collector 440 and a cathode film 430 formed thereon. In Figure 4It should be noted that although the current collector and separator are shown extending beyond the stack, the current collector and / or separator do not have to extend beyond the stack, and the portions extending beyond the stack may serve as tabs.
[0036] The cathode current collector 440 may be composed of aluminum (Al), copper (Cu), zinc (Zn), nickel (Ni), cobalt (Co), tin (Sn), silicon (Si), manganese (Mn), magnesium (Mg), a coating material, an alloy of the above, or a combination thereof. In one implementation, the cathode current collector 440 is aluminum. In one implementation, the cathode current collector 440 is perforated. In addition, the current collector may have any form factor (e.g., metal foil, sheet or plate), shape, and micro / macro structure. Generally speaking, in prismatic batteries, the tabs are formed of the same material as the current collector and may be formed during the manufacture of the stack or added thereafter. In some implementations, all components except the copper substrate 310 and the cathode current collector 440 contain a lithium ion electrolyte. In one implementation, the cathode current collector 440 is aluminum. In some implementations, the cathode current collector 440 has a thickness from about 2 μm to about 20 μm.
[0037] The cathode film 430 or cathode may be any material compatible with the anode and may include an intercalation compound, an insertion compound, or an electrochemically active polymer. Suitable intercalation materials include, for example, lithium-containing metal oxides, MoS2, FeS2, MnO2, TiS2, NbSe3, LiCoO2, LiNiO2, LiMnO2, LiMn2O4, V6O 13 and V2O5. Suitable polymers include, for example, polyacetylene, polypyrrole, polyaniline, and polythiophene. The cathode film 430 or cathode may be made of a layered oxide such as lithium cobalt oxide; an olivine such as lithium iron phosphate; or a spinel such as lithium manganate. Exemplary lithium-containing oxides may be layered metal oxides such as lithium cobalt oxide (LiCoO2), or may be mixed metal oxides such as LiNi x Co 1-2x MnO2, LiNiMnCoO2 (“NMC”), LiNi 0.5 Mn 1.5 O4、Li(Ni 0.8 Co 0.15 Al 0.05 )O2, LiMn2O4 and doped lithium-rich layered materials, where x is zero or a non-zero number. Exemplary phosphates may be olivine iron (LiFePO4) and its variants (such as LiFe (1-x) Mg x PO4), LiMoPO4, LiCoPO4, LiNiPO4, Li3V2(PO4)3, LiVOPO4, LiMP2O7 or LiFe 1.5P2O7, where x is zero or a non-zero number. Exemplary fluorophosphates may be LiVPO4F, LiAlPO4F, Li5V(PO4)2F2, Li5Cr(PO4)2F2, Li2CoPO4F, or Li2NiPO4F. Exemplary silicates may be Li2FeSiO4, Li2MnSiO4, or Li2VOSiO4. Exemplary non-lithium compounds are Na5V2(PO4)2F3. Cathode film 430 may be formed by physical or chemical thin film techniques, such as sputtering, electron beam evaporation, chemical vapor deposition (CVD), and other processes. In one implementation, cathode film 430 has a thickness from about 10 μm to about 100 μm (e.g., from about 30 μm to about 80 μm; or from about 40 μm to about 60 μm). In one implementation, cathode film 430 is a LiCoO2 film. In some implementations in which the energy storage device is an electrochemical capacitor, high surface area carbon is used as an electrode.
[0038] The electrolyte injected into the battery components 320, 330, 350, 420 and 430 may be composed of liquid / gel or solid polymer, and may be different. In some embodiments, the electrolyte mainly includes a salt and a medium (e.g., in a liquid electrolyte, the medium may be referred to as a solvent; in a gel electrolyte, the medium may be a polymer matrix). The salt may be a lithium salt. The lithium salt may include, for example, LiPF6, LiAsF6, LiCF3SO3, LiN(CF3SO3)3, LiBF6 and LiClO4, lithium bis(trifluoromethyl)sulfonyl imide acid (e.g., LiTFSI), BETTE electrolyte (available from 3M Corp. of Minneapolis, MN), or a combination thereof. The solvent may include, for example, ethylene carbonate (EC), propylene carbonate (PC), EC / PC, 2-MeTHF (2-methyltetrahydrofuran) / EC / PC, EC / DMC (dimethyl carbonate), EC / DME (dimethyl ethane), EC / DEC (diethyl carbonate), EC / EMC (ethyl methyl carbonate), EC / EMC / DMC / DEC, EC / EMC / DMC / DEC / PE, PC / DME, and DME / PC. The polymer matrix may include, for example, PVDF (polyvinylidene fluoride), PVDF:THF (PVDF:tetrahydrofuran), PVDF:CTFE (PVDF:chlorotrifluoroethylene), PAN (polyacrylonitrile), and PEO (polyethylene oxide).
[0039] Figure 5A schematic diagram of a flexible substrate coating apparatus 500 for forming an anode electrode structure according to an implementation described herein is illustrated. According to a typical implementation, the flexible substrate coating apparatus 500 can be used to manufacture an anode electrode structure, and in particular, to form a diffusion barrier layer structure on a copper substrate. The flexible substrate coating apparatus 500 is configured as a roll-to-roll system, including an unwinding module 502, a processing module 504, and a winding module 506. In certain implementations, the processing module 504 includes a plurality of processing modules or chambers 510, 520, 530, and 540 arranged in sequence, each processing module or chamber being configured to perform a processing operation on a continuous material sheet 550 or a material web. In one implementation, as Figure 5 As depicted, the process chambers 510-540 are radially disposed about the coating drum 555. Other arrangements besides radial are also contemplated. For example, in another implementation, the process chambers may be positioned in a linear configuration.
[0040] In one implementation, the processing chambers 510 to 540 are independent modular processing chambers, wherein each modular processing chamber is structurally separated from the other modular processing chambers. Therefore, each independent modular processing chamber can be arranged, rearranged, replaced or maintained separately without affecting each other. Although four processing chambers 510 to 540 are shown, it should be understood that any number of processing chambers can be included in the flexible substrate coating apparatus 500.
[0041] The processing chambers 510 to 540 may include any suitable structure, configuration, arrangement and / or components that enable the flexible substrate coating apparatus 500 to deposit a lithium anode device according to an implementation of the present disclosure. For example, but not limited to, the processing chamber may include a suitable deposition system, which includes a coating source, a power source, a separate pressure control, a deposition control system, and a temperature control. In some implementations, the chamber is provided with a separate gas source. The chambers are typically separated from each other to provide good gas separation. The flexible substrate coating apparatus 500 according to the implementation described herein is not limited in the number of deposition chambers. For example, but not limited to, the flexible substrate coating apparatus 500 may include 3, 6, or 12 processing chambers.
[0042] The processing chambers 510 to 540 typically include one or more deposition units 512, 522, 532 and 542. In general, one or more deposition units as described herein can be selected from the group having the following items: CVD source, PECVD source and PVD source. One or more deposition units may include an evaporation source, a sputtering source, such as a magnetron sputtering source, a DC sputtering source, an AC sputtering source, a pulsed sputtering source, and radio frequency (RF) sputtering or medium frequency (MF) sputtering can be provided. For example, MF sputtering with a frequency in the range of 5kHz to 100kHz, for example, 30kHz to 50kHz can be provided. One or more deposition units may include an evaporation source. In one implementation, the evaporation source is a thermal evaporation source or an electron beam evaporation device. In one implementation, the evaporation source is a lithium (Li) source. In addition, the evaporation source can also be an alloy of two or more metals. The material to be deposited (e.g., lithium) can be provided in a crucible. Lithium can be evaporated, for example, by thermal evaporation technology, electron beam evaporation technology or lamination technology.
[0043] In some implementations, any of the processing chambers 510 to 540 of the flexible substrate coating apparatus 500 may be configured for performing deposition by sputtering, such as magnetron sputtering. As used herein, "magnetron sputtering" refers to sputtering performed using a magnet assembly, i.e., a unit capable of generating a magnetic field. Typically, such a magnet assembly includes a permanent magnet. This permanent magnet is typically arranged in a rotatable target or coupled to a planar target so that free electrons are trapped in a magnetic field generated below the surface of the rotatable target. Such a magnet assembly may also be arranged to be coupled to a planar cathode.
[0044] Magnetron sputtering can also be achieved with a dual magnetron cathode such as, but not limited to, the TwinMag TM Cathode assembly. In some implementations, the cathodes in the processing chambers may be interchangeable. Thus, a modular design of the apparatus is provided, which facilitates optimization of the apparatus for specific manufacturing requirements. In some implementations, the number of cathodes in the chamber for sputtering deposition is selected to optimize the best productivity of the flexible substrate coating apparatus 500.
[0045] In some implementations, one or some of the processing chambers 510-540 can be configured to perform sputtering without a magnetron assembly. In some implementations, one or some of the chambers can be configured to perform deposition by other methods, such as, but not limited to, chemical vapor deposition, atomic laser deposition, or pulsed laser deposition. In some implementations, one or some of the chambers can be configured to perform a plasma treatment process, such as a plasma oxidation or plasma nitridation process.
[0046] In some implementations, the processing chambers 510 to 540 are configured to process both sides of the continuous material sheet 550. Although the flexible substrate coating apparatus 500 is configured to process a horizontally oriented continuous material sheet 550, the flexible substrate coating apparatus 500 can be configured to process substrates positioned in different orientations, such as a vertically oriented continuous material sheet 550. In some implementations, the continuous material sheet 550 is a flexible conductive substrate. In some implementations, the continuous material sheet 550 includes a conductive substrate having one or more layers formed thereon. In some implementations, the conductive substrate is a copper substrate, such as FIG. 3A to FIG. 3D The copper substrate 310 is shown in FIG.
[0047] In certain implementations, the flexible substrate coating apparatus 500 includes a conveying mechanism 552. The conveying mechanism 552 may include any conveying mechanism capable of moving a continuous material sheet 550 through the processing areas of the processing chambers 510 to 540. The conveying mechanism 552 may include a common transport architecture. The common transport architecture may include a roll-to-roll system and have a common take-up reel 554 positioned in the winding module 506, a coating roller 555 positioned in the processing module 504, and a feed reel 556 positioned in the unwinding module 502. The take-up reel 554, the coating roller 555, and the feed reel 556 may be heated separately. The take-up reel 554, the coating roller 555, and the feed reel 556 may be heated separately using an internal heat source positioned within each reel or using an external heat source. The common transport architecture may further include one or more auxiliary transport reels 553a, 553b positioned between the take-up reel 554, the coating roller 555, and the feed reel 556. Although the flexible substrate coating apparatus 500 is depicted as having a single processing area, in certain implementations, each individual processing chamber 510 to 540 may advantageously have a separate or discrete processing area. For implementations with discrete processing areas, modules, or chambers, the common transport architecture may be a roll-to-roll system, wherein each chamber or processing area has a separate take-up reel and feed reel, and one or more optional intermediate transfer reels positioned between the take-up reel and the feed reel.
[0048] The flexible substrate coating apparatus 500 may include a feed reel 556 and a take-up reel 554 for moving a continuous material sheet 550 through different processing chambers 510 to 540. In one implementation, the first processing chamber 510 is configured to deposit a first diffusion barrier film. The second processing chamber 520 is configured to deposit a second diffusion barrier film. The third processing chamber 530 is configured to deposit a wetting film. The fourth processing chamber 540 is configured to deposit a lithium metal film. In another implementation in which the continuous material sheet 550 is a polymer material, the first processing chamber 510 is configured to deposit a copper film on the polymer material. The second processing chamber 520 and the third processing chamber 530 are each configured to deposit a diffusion barrier film or a wetting film. The fourth processing chamber 540 is configured to deposit a lithium metal film. In some implementations, the completed anode will not be collected on the take-up reel 554 as shown, but can be directly used for integration with separators and positive electrodes to form battery cells.
[0049] In one implementation, the first processing chamber 510 is configured to deposit a first diffusion barrier layer. In one implementation, the first diffusion barrier layer is a tantalum layer deposited by a PVD sputtering process using a tantalum target. In another implementation, the first diffusion barrier layer is a tantalum nitride layer deposited by a PVD sputtering process using a tantalum target in a nitrogen-containing environment or using a tantalum nitride target.
[0050] In one implementation, the second processing chamber 520 is configured to deposit a second diffusion barrier layer. In one implementation, the second diffusion barrier layer is a titanium layer deposited by a PVD sputtering process using a titanium target. In another implementation, the second diffusion barrier layer is a titanium nitride layer deposited by a PVD sputtering process using a titanium target in a nitrogen-containing environment or using a titanium nitride target.
[0051] In one implementation, the third processing chamber 530 is configured to deposit a wetting layer on the underlying barrier layer. In one implementation, the wetting layer is a silicon layer deposited by a PVD sputtering process using a silicon target.
[0052] In one implementation, the fourth processing chamber 540 is configured to deposit a thin lithium metal film on the underlying layer. Any suitable lithium deposition process for depositing a thin lithium metal film can be used to deposit the thin lithium metal film. The deposition of the thin lithium metal film can be performed by a PVD process, such as evaporation, a slot die process, a transfer process, a lamination process, or a three-dimensional lithium printing process. The chamber for depositing the thin lithium metal film may include: a PVD system, such as an electron beam evaporator; a thin film transfer system including a large area pattern printing system, such as a gravure printing system); a lamination system or a slot die deposition system.
[0053] In operation, a continuous material sheet 550 is unwound from a feed reel 556, as indicated by the direction of substrate movement shown by arrow 508. The continuous material sheet 550 may be guided via one or more auxiliary transport reels 553a, 553b. The continuous material sheet 550 may also be guided by one or more substrate guide control units (not shown) that should control the correct travel of the flexible substrate, for example by finely adjusting the orientation of the flexible substrate.
[0054] After being unwound from the feed reel 556 and traveling over the auxiliary transport reel 553a, the continuous material sheet 550 is then moved through a deposition area provided at the coating drum 555 and corresponding to the positions of the deposition units 512, 522, 532 and 542. During operation, the coating drum 555 rotates about the axis 551 so that the flexible substrate moves in the direction of the arrow 508.
[0055] Implementation:
[0056] Item 1. An anode electrode structure comprising: a copper foil; a first diffusion barrier layer, the first diffusion barrier layer being formed on the copper foil, wherein the first diffusion barrier layer comprises titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta) or a combination thereof; a wetting layer, the wetting layer being formed on the first diffusion barrier layer, wherein the wetting layer is selected from silicon (Si), tin (Sn), aluminum (Al), germanium (Ge), antimony (Sb), lead (Pb), bismuth (Bi), gallium (Ga), indium (In), zinc (Zn), cadmium (Cd), magnesium (Mg), the above oxides, the above nitrides or a combination thereof; and a lithium metal layer, the lithium metal layer being formed on the wetting layer.
[0057] Item 2. The anode electrode structure of Item 1, further comprising a second diffusion barrier layer formed between the first diffusion barrier layer and the wetting layer, wherein the second diffusion barrier layer is different from the first diffusion barrier layer.
[0058] Item 3. The anode electrode structure of Item 2, wherein the second diffusion barrier layer comprises titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta), or a combination thereof.
[0059] Clause 4. The anode electrode structure of Clause 2 or 3, wherein the first diffusion barrier layer is a tantalum layer and the second diffusion barrier layer is a titanium layer.
[0060] Item 5. The anode electrode structure of Item 2 or 3, wherein the first diffusion barrier layer is a tantalum nitride layer and the second diffusion barrier layer is a titanium layer.
[0061] Item 6. The anode electrode structure of any one of Items 1 to 5, wherein the lithium metal layer forms an alloy with the wetting layer.
[0062] Item 7. The anode electrode structure of any one of Items 1 to 6, wherein the first diffusion barrier layer has a thickness of about 100 nanometers to about 200 nanometers.
[0063] Item 8. The anode electrode structure of any one of Items 1 to 7, wherein the wetting layer has a thickness of about 5 nanometers to about 20 nanometers.
[0064] Clause 9. A battery incorporating the anode electrode structure of any one of Clauses 1 to 8.
[0065] Item 10. A method for forming an electrode structure, comprising: forming a first diffusion barrier layer on a copper foil, wherein the first diffusion barrier layer comprises titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta) or a combination thereof; forming a wetting layer on the first diffusion barrier layer, wherein the wetting layer is selected from silicon (Si), tin (Sn), aluminum (Al), germanium (Ge), antimony (Sb), lead (Pb), bismuth (Bi), gallium (Ga), indium (In), zinc (Zn), cadmium (Cd), magnesium (Mg), the above oxides, the above nitrides or a combination thereof; and forming a lithium metal layer on the wetting layer.
[0066] Item 11. The method of Item 10, further comprising: before forming the wetting layer, forming a second diffusion barrier layer on the first diffusion barrier layer, wherein the second diffusion barrier layer is different from the first diffusion barrier layer.
[0067] Item 12. The method of Item 11, wherein the second diffusion barrier layer comprises titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta), or combinations thereof.
[0068] Item 13. The method of any one of Items 10 to 12, wherein the first diffusion barrier layer is a tantalum layer deposited by a PVD sputtering process using a tantalum target.
[0069] Item 14. The method of any one of Items 10 to 13, wherein the first diffusion barrier layer is a tantalum nitride layer deposited by a PVD sputtering process using a tantalum target in a nitrogen-containing environment.
[0070] Clause 15. The method of any one of Clauses 11 to 14, wherein the second diffusion barrier layer is a titanium layer deposited by a PVD sputtering process using a titanium target.
[0071] Item 16. The method of any one of Items 11 to 14, wherein the second diffusion barrier layer is a titanium nitride layer deposited by a PVD sputtering process using a titanium target in a nitrogen-containing environment.
[0072] Clause 17. The method of any one of Clauses 10 to 16, wherein the wetting layer is a silicon layer deposited by a PVD sputtering process using a silicon target.
[0073] Clause 18. The method of any of Clauses 10 to 17, further comprising guiding the copper foil in the vacuum chamber using a roller arrangement.
[0074] Item 19. An integrated processing tool operable to form a lithium-coated electrode, comprising: a reel-to-reel system operable to transport a continuous sheet of material through the following processing chambers: a first processing chamber operable to deposit a first diffusion barrier layer on the continuous sheet of material; a second processing chamber operable to deposit a second diffusion barrier layer on the first diffusion barrier layer; a third processing chamber operable to deposit a wetting layer on the second diffusion barrier layer; and a fourth processing chamber operable to deposit a thin lithium metal film on the second diffusion barrier layer.
[0075] Clause 20. The integrated processing tool of Clause 19, wherein the continuous sheet of material is copper foil.
[0076] In summary, some of the benefits of the present disclosure include the use of refractory metal / metal nitride barrier films to ensure temporal / thermal stability of the lithium metal / copper foil interface. Thus, the lithium metal / copper foil interface does not suffer degradation during operation as an anode in a lithium metal battery. Additionally, the barrier films described herein help prevent lithium-induced embrittlement of the copper foil, maintain the mechanical properties of the copper foil, and minimize tearing of the copper foil. Thus, the barrier films described herein facilitate roll-to-roll processing of the copper foil.
[0077] When introducing elements of the present disclosure or exemplary aspects or implementations of the present disclosure, the articles "a," "an," "the," and "said" are intended to mean that there are one or more of the referenced elements.
[0078] The terms “comprising,” “including,” and “having” are intended to be inclusive and mean that there may be additional elements other than the listed elements.
[0079] While the foregoing is directed to implementations of the present disclosure, other and further implementations of the disclosure may be envisaged without departing from the basic scope of the disclosure, and the scope of the disclosure is determined by the claims that follow.
Claims
1. An anode electrode structure, comprising: Copper foil; a first diffusion barrier layer, the first diffusion barrier layer being formed on the copper foil, wherein the first diffusion barrier layer comprises titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta) or a combination thereof, or the first diffusion barrier layer comprises titanium nitride (TiN), tungsten nitride (WN), tantalum nitride or a combination thereof; a second diffusion barrier layer formed on the first diffusion barrier layer, wherein the second diffusion barrier layer is different from the first diffusion barrier layer, wherein the first diffusion barrier layer serves as a copper diffusion barrier layer, and the second diffusion barrier layer serves as a lithium diffusion barrier layer; a wetting layer formed on the second diffusion barrier layer, wherein the wetting layer is selected from silicon (Si), tin (Sn), aluminum (Al), germanium (Ge), antimony (Sb), lead (Pb), bismuth (Bi), gallium (Ga), indium (In), zinc (Zn), cadmium (Cd), magnesium (Mg), oxides of the above materials, nitrides of the above materials, or combinations thereof; and A lithium metal layer is formed on the wetting layer.
2. The anode electrode structure of claim 1, wherein the second diffusion barrier layer comprises titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta), or a combination thereof. 3 . The anode electrode structure of claim 2 , wherein the first diffusion barrier layer is a tantalum layer and the second diffusion barrier layer is a titanium layer. 4 . The anode electrode structure of claim 2 , wherein the first diffusion barrier layer is a tantalum nitride layer and the second diffusion barrier layer is a titanium layer.
5. The anode electrode structure of claim 1, wherein the lithium metal layer forms an alloy with the wetting layer. The anode electrode structure of claim 1 , wherein the first diffusion barrier layer has a thickness of 100 nm to 200 nm. 7 . The anode electrode structure of claim 6 , wherein the wetting layer has a thickness of 5 nm to 20 nm.
8. A battery comprising the anode electrode structure according to claim 1.
9. A method for forming an electrode structure, comprising: forming a first diffusion barrier layer on the copper foil, wherein the first diffusion barrier layer comprises titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta), or a combination thereof, or the first diffusion barrier layer comprises titanium nitride (TiN), tungsten nitride (WN), tantalum nitride, or a combination thereof; forming a second diffusion barrier layer on the first diffusion barrier layer, wherein the second diffusion barrier layer is different from the first diffusion barrier layer, wherein the first diffusion barrier layer serves as a copper diffusion barrier layer, and the second diffusion barrier layer serves as a lithium diffusion barrier layer; forming a wetting layer on the second diffusion barrier layer, wherein the wetting layer is selected from silicon (Si), tin (Sn), aluminum (Al), germanium (Ge), antimony (Sb), lead (Pb), bismuth (Bi), gallium (Ga), indium (In), zinc (Zn), cadmium (Cd), magnesium (Mg), oxides of the above materials, nitrides of the above materials, or combinations thereof; and A lithium metal layer is formed on the wetting layer.
10. The method of claim 9, wherein the second diffusion barrier layer comprises titanium (Ti), molybdenum (Mo), tungsten (W), zirconium (Zr), hafnium (Hf), niobium (Nb), tantalum (Ta), or a combination thereof.
11. The method of claim 9, wherein the first diffusion barrier layer is a tantalum layer deposited by a PVD sputtering process using a tantalum target.
12. The method of claim 9, wherein the first diffusion barrier layer is a tantalum nitride layer deposited by a PVD sputtering process using a tantalum target in a nitrogen-containing environment.
13. The method of claim 9, wherein the second diffusion barrier layer is a titanium layer deposited by a PVD sputtering process using a titanium target.
14. The method of claim 9, wherein the second diffusion barrier layer is a titanium nitride layer deposited by a PVD sputtering process using a titanium target in a nitrogen-containing environment.
15. The method of claim 9, wherein the wetting layer is a silicon layer deposited by a PVD sputtering process using a silicon target.
16. The method of claim 9, further comprising: The copper foil was guided in the vacuum chamber using a roller arrangement.
17. An integrated processing tool operable to form a lithium coated electrode, comprising: A reel-to-reel system operable to transport a continuous sheet of material through the following processing chambers: a first processing chamber operable to deposit a first diffusion barrier layer on the continuous sheet of material, wherein the continuous sheet of material is a copper foil; a second processing chamber operable to deposit a second diffusion barrier layer on the first diffusion barrier layer, wherein the second diffusion barrier layer is different from the first diffusion barrier layer, wherein the first diffusion barrier layer functions as a copper diffusion barrier layer, and the second diffusion barrier layer functions as a lithium diffusion barrier layer; a third processing chamber operable to deposit a wetting layer on the second diffusion barrier layer; and A fourth processing chamber is operable to deposit a thin lithium metal film on the second diffusion barrier layer, the wetting layer enhancing adhesion of the thin lithium metal film to an underlying barrier material.