Chemically amplified positive photoresist composition for improving pattern profile
By adding specific transmittance to the KrF photoresist to improve the resin additive, the problems of poor contour and insufficient etch resistance in the prior art are solved, and vertical contours and improved sensitivity are achieved under the KrF light source, which is suitable for high integration Chemical semiconductor manufacturing.
Patent Information
- Application Number
- CN201980041217.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-06-18
- Filing Date
- 2019-05-22
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2039-05-22
AI Technical Summary
The existing KrF photoresist has problems such as poor profile, insufficient etch resistance and insufficient sensitivity when forming fine patterns, especially in high-integration and miniaturized semiconductor manufacturing, which is difficult to meet the needs of high resolution and depth of focus margin. .
By adding a chemical amplification type resist transmittance of 2,000 to 20,000 represented by a specific chemical formula 1, the resin additive includes 5 to 60% by weight of polymer resin, and 0.1 to 10% by weight of transmittance of 0.1 to 10% by weight of the polymer resin The resin additive, 0.05 to 10% by weight of the photoacid generator and 0.01 to 5% by weight of the acid diffusion inhibitor improves the transmittance and photosensitiveness of the photoresist.
The vertical profile is formed under the KrF light source, which improves the sensitivity and process margin, improves the resolution and etching performance of the pattern profile, and is suitable for semiconductor manufacturing processes.
Smart Images

Figure BDA0002844729190000031 
Figure BDA0002844729190000043 
Figure BDA0002844729190000044
Abstract
Description
Technical Field
[0001] The invention relates to a chemically amplified positive photoresist composition for improving pattern profile. Background Art
[0002] Recently, with the development of semiconductor manufacturing process technology, the miniaturization and high integration of semiconductor elements are required, and the technology of realizing ultra-fine patterns with line widths below tens of nanometers is required. The progress of the technology for forming such ultra-fine patterns depends on light sources with smaller wavelengths, the development of process technology based on light sources, and the development of photoresists suitable for light sources.
[0003] Photoresist is used in the photolithography process for forming various patterns. Photoresist refers to a photosensitive resin that can change its solubility in a developer under the action of light to obtain an image corresponding to the exposure pattern.
[0004] The photoresist pattern forming method includes: negative tone development (NTD) using a negative tone developer and positive tone development (PTD) using a positive tone developer.
[0005] The pattern forming method using the negative tone developer is a method of forming a pattern by selectively dissolving and removing the non-exposed area using the negative tone developer, while the pattern forming method using the positive tone developer is a method of forming a pattern by selectively dissolving and removing the exposed area using the positive tone developer.
[0006] Compared with the pattern forming method using the positive tone developer, the pattern forming method using the negative tone developer can also realize an inverted pattern in a contact hole pattern or a groove pattern that is difficult to form due to insufficient exposure, so it is easy to form a pattern when realizing the same pattern, and an organic solvent is used as a developer for removing the unexposed part, so that the photoresist pattern can be formed more effectively.
[0007] On the other hand, generally, the photolithography process using the photoresist composition includes: a process of coating the photoresist on a wafer; a soft baking process of heating the coated photoresist to evaporate the solvent; a process of imaging with the help of a light source passing through a photomask; a process of forming a pattern using a developer according to the solubility difference between the exposed part and the non-exposed part; and a process of etching it to complete the circuit.
[0008] The photoresist composition is composed of a photosensitizer (Photo Acid Generator) and a base resin and other additives that generate acid by irradiation with an excimer laser. In the base resin, a polystyrene polymer is basically used as a structure containing a hydroxyl group in a phenol structure. As a photosensitizer, any type of photosensitive agent is acceptable as long as it can generate acid (H+) at a specific wavelength, and mainly uses sulfonium salts, sulfonyl diazos, benzene sulfonyls, iodine, chlorine, carboxylic acid, etc.
[0009] In addition, the light source mainly used in the above-mentioned process is the wavelength region of 365nm to 193nm using I-line, KrF excimer laser, ArF excimer laser light source, and the shorter the wavelength, the finer the pattern can be formed.
[0010] Among them, although the ArF laser (193nm) system was developed later, the KrF laser (248nm) photoresist has also been pursuing research and development of optical micro-processing. The following reasons can be cited as reasons. That is, although the development of the second generation ArF photoresist still has unsatisfactory aspects, if the KrF photoresist is continued to be used, the effect of reducing costs in the mass production of semiconductors is large. With the development of this technology, the performance of KrF photoresist should also be improved. A representative example is that with high integration, the thickness of the photoresist is required to be reduced. Therefore, the development of a photoresist with more enhanced dry etching resistance is urgently needed. In addition, the required characteristics also include: high resolution, wide depth of focus margin (DOF (Depth Of Focus) Margin), formation of defect-free film, adhesion to substrate, high contrast (Contrast), fast sensitivity, chemical stability, etc.
[0011] As mentioned above, previous patent disclosures on the photoresist technology for KrF lasers include Korean Patent Publication No. 10-2010-0047038 "Chemically amplified positive photoresist composition", Korean Authorized Patent Publication No. 10-1363842 "Chemically amplified positive photoresist composition and anti-etching pattern forming method using the same", Korean Authorized Patent Publication No. 10-1204915 "Photoresist polymer, photoresist composition containing the same and photoresist pattern forming method using the same", Korean Authorized Patent Publication No. 10-0273108 "Copolymer for photoresist preparation and chemically amplified positive photoresist composition containing the same", Korean Authorized Patent Publication No. 10-1655947 "Negative photoresist composition for KrF laser with high resolution and high aspect ratio", etc.
[0012] In the above patent, as described above, in order to improve the resolution and sensitivity, polyhydroxystyrene and polystyrene polymers having good transmittance at a wavelength of 248 nm are mainly used as base polymers for KrF photoresists.
[0013] Positive photoresists based on polyhydroxystyrene and polystyrene polymers are limited in their usability in processes based on 248 nm light sources due to slope patterns and footing development, and thus present difficulties in the process.
[0014] (Prior art literature)
[0015] (Patent Document)
[0016] (Patent Document 1) Korean Patent Publication No. 10-2010-0047038
[0017] (Patent Document 2) Korean Patent Publication No. 10-1363842
[0018] (Patent Document 3) Korean Patent Publication No. 10-1204915
[0019] (Patent Document 4) Korean Patent Publication No. 10-0273108
[0020] (Patent Document 5) Korean Patent Publication No. 10-1655947 Summary of the invention
[0021] Technical issues to be solved
[0022] An object of the present invention is to provide a photoresist composition for a KrF light source which exhibits a vertical profile compared to a conventional KrF positive photoresist by adding a resin capable of increasing transmittance.
[0023] Technical solutions to the problem
[0024] In order to achieve the above object, the present invention provides a positive photoresist composition for KrF laser, comprising a transmittance-enhancing resin additive for chemically amplified resist having a weight average molecular weight of 2,000 to 20,000 represented by the following Chemical Formula 1.
[0025]
[0026] The a, b, c, and d are molar ratios of repeating units forming the copolymer, characterized in that each is 1 to 9. In the above structure, R1, R2, and R3 are selected from one or more structures consisting of methyl (R-CH3), ethyl (R-CH2CH3), propyl (R-CH2CH2CH3), butyl (R-CH2CH2CH2CH3) or a combination thereof, and the R1, R2, and R3 are different from each other, and the R represents a binding site.
[0027] In a preferred embodiment of the present invention, the transmittance-enhancing resin additive for resist represented by the above chemical formula and similar structures can be commercially obtained from multiple domestic and foreign suppliers such as Miwon and Meiwa.
[0028] In a preferred embodiment of the present invention, the weight average molecular weight of the anti-etching polymer additive represented by the above Chemical Formula 1 is 2,000 to 20,000.
[0029] In a preferred embodiment of the present invention, it is characterized in that the transmittance-enhancing resin additive for anti-etching comprises, relative to the total weight of the composition, 5 to 60 wt % of a polymer resin, 0.1 to 10 wt % of a transmittance-enhancing resin additive represented by Chemical Formula 1, 0.05 to 10 wt % of a photoacid generator, 0.01 to 5 wt % of an acid diffusion inhibitor, and the remainder a solvent.
[0030] In a preferred embodiment of the present invention, it is characterized in that the polymer resin can be any commonly used photoresist resin, and is one or more selected from the group consisting of the following phenol polymer resins containing hydroxyl groups, Chemical Formula 2 to Chemical Formula 5.
[0031] By repeating unit and The resin formed.
[0032] (In the above structure, R4 is a structure selected from the following chemical formula a to chemical formula p, and R represents a binding site.)
[0033]
Chemical formula a
[0034]
[0035]
Chemical formula b
[0036]
[0037]
Chemical formula c
[0038]
[0039]
Chemical formula d
[0040]
[0041]
Chemical formula e
[0042]
[0043]
Chemical formula f
[0044]
[0045]
Chemical formula g
[0046]
[0047]
Chemical formula h
[0048]
[0049]
Chemical formula i
[0050]
[0051]
Chemical formula j
[0052]
[0053]
Chemical formula k
[0054]
[0055]
Chemical formula 1
[0056]
[0057]
Chemical formula m
[0058]
[0059]
Chemical formula n
[0060]
[0061]
Chemical formula o
[0062]
[0063]
Chemical formula p
[0064]
[0065] By repeating unit and The resin formed.
[0066] (In the above structure, R5 is the same as R4 and is a structure selected from the structures of chemical formula a to chemical formula p.)
[0067] By repeating unit and The resin formed.
[0068] (In the aforementioned structure, R6 and R7 are one or more structures selected from the structures of Chemical Formula a to Chemical Formula p.)
[0069] By repeating unit and The resin formed.
[0070] (In the aforementioned structure, R8 and R9 are one or more structures selected from the structures of Chemical Formula a to Chemical Formula p.)
[0071] In a preferred embodiment of the present invention, the phenol polymer resin is one or more selected from the group consisting of the following phenol polymer resins containing hydroxyl groups represented by Chemical Formula 2 to Chemical Formula 5.
[0072] In a preferred embodiment of the present invention, it is characterized in that the photoacid generator comprises a member selected from the group consisting of triphenylsulfonium triflate, triphenylsulfonium antimonate, diphenyliodonium triflate, diphenyliodonium antimonate, methoxydiphenyliodonium triflate, di-t-butyldiphenyliodonium triflate, 2,6-dinitrobenzenesulfonate, and 1,2-dinitrobenzenesulfonate.6-dinitrobenzylsulponate), pyrogalloltrisalkylsulfonate, norbornenedicarboxyimidetriflate, triphenylsulfoniumnonaflate, diphenyliodoniumnonaflate, methoxydiphenyliodoniumnonaflate, di-t-buthyldiphenyliodoniumnonaflate, N-hydroxysuccinimidenonaflate, norbornenedicarboxyimidetriflate, triphenylsulfoniumnonaflate, diphenyliodoniumnonaflate, methoxydiphenyliodoniumnonaflate, di-t-buthyldiphenyliodoniumnonaflate, N-hydroxysuccinimidenonaflate, norbornenedicarboxyimidetriflate, triphenylsulfoniumnonaflate, diphenyliodoniumnonaflate, methoxydiphenyliodoniumnonaflate, di-t-buthyldiphenyliodoniumnonaflate, One or more of the group consisting of norbornenedicarboxyimidenonaflate, triphenylsulfoniumperfluorooctanesulfonate, diphenyliodoniumperfluorooctanesulfonate, methoxydiphenyliodoniumperfluorooctanesulfonate, di-tert-butyldiphenyliodoniumperfluorooctanesulfonate, N-hydroxysuccinimideperfluorooctanesulfonate and norbornenedicarboxyimideperfluorooctanesulfonate.
[0073] In a preferred embodiment of the present invention, the acid diffusion inhibitor is characterized by comprising one or more selected from the group consisting of dimethylamine, diethylamine, trimethylamine, triethylamine, tributhylamine, dimethanolamine, diethanolamine, trimethanolamine, triethanolamine, and tributhanolamine.
[0074] Effects of the Invention
[0075] By adding the transmittance-enhancing resin additive according to the present invention, a vertical profile according to exposure energy can be obtained, and the sensitivity can be increased to improve the process margin compared with the conventional KrF photoresist (PR).
[0076] Best Mode for Carrying Out the Invention
[0077] Unless otherwise defined, all technical and scientific terms used in this specification have the same meaning as those commonly understood by those of ordinary skill in the art to which the invention belongs. Generally, the nomenclature used in this specification is well known and commonly used in the art.
[0078] Throughout the specification of the present invention, when it is considered that a certain part includes a certain structural element, this means that other structural elements are not excluded and other structural elements can be included unless there is a special description to the contrary.
[0079] In the present invention, the so-called photoresist is a mixture of a polymer and a photosensitizer, and its chemical properties change with the help of light. Therefore, when exposed to light of a certain wavelength, its solubility in a specific solvent changes, resulting in a difference in the dissolution rate of the exposed part and the non-exposed part of the solvent. When the dissolution time of a specified time has passed, the incompletely dissolved part remains to form a pattern.
[0080] In the present invention, the photolithographic process refers to placing a mask engraved with a semiconductor design drawing between a light source and a photoresist film coated on a silicon wafer using the properties of the photoresist as described above. When the light source is turned on, the circuit engraved on the mask will be transferred to the photoresist as it is.
[0081] In the present invention, KrF laser refers to krypton fluoride (KrF) laser having a wavelength of 248 nm.
[0082] One embodiment of the present invention provides a chemically amplified positive photoresist composition for improving pattern profile, characterized in that it contains a transmittance-enhancing resin additive represented by the following chemical formula 1.
[0083]
Chemical formula 1
[0084]
[0085] The a, b, c, and d are molar ratios of repeating units forming the copolymer, characterized in that each is 1 to 9. In the aforementioned structure, R1, R2, and R3 are one or more structures selected from the structure consisting of methyl (R-CH3), ethyl (R-CH2CH3), propyl (R-CH2CH2CH3), butyl (R-CH2CH2CH2CH3) or a combination thereof, and the R1, R2, and R3 are different from each other, and the R represents a binding site.
[0086] The positive photoresist composition for improving pattern profile containing a transmittance enhancing resin additive according to the present invention may include 5 to 60 wt % of a polymer resin, 0.1 to 10 wt % of a transmittance enhancing resin additive represented by Chemical Formula 1, 1 to 10 wt % of a cross-linking agent, 0.05 to 10 wt % of a photoacid generator, 0.01 to 5 wt % of an acid diffusion inhibitor, and the remainder of a solvent, relative to the total weight of the composition.
[0087] Preferably, the transmittance-enhancing resin additive represented by the above chemical formula 1 contains 0.1 to 10 wt % relative to the total weight of the composition. If the compound is used in an amount less than 0.1 wt %, the amount of the transmittance-enhancing resin additive is too small to have no effect on ensuring a vertical profile, and if it is used in an amount greater than 10 wt %, a vertical profile can be ensured, but it may cause other defects such as scum, poor etching resistance, and poor development, and is therefore not desirable.
[0088] The polymer resin is characterized in that it can be any photoresist resin commonly used, and is one or more selected from the group consisting of the following phenol polymer resins containing a hydroxyl group, Chemical Formula 2 to Chemical Formula 5.
[0089]
Chemical formula 2
[0090] By repeating unit and The resin formed.
[0091] (In the aforementioned structure, R4 is a structure selected from the following chemical formula a to chemical formula p, and R represents a binding site.)
[0092]
Chemical formula a
[0093]
[0094]
Chemical formula b
[0095]
[0096]
Chemical formula c
[0097]
[0098]
Chemical formula d
[0099]
[0100]
Chemical formula e
[0101]
[0102]
Chemical formula f
[0103]
[0104]
Chemical formula g
[0105]
[0106]
Chemical formula h
[0107]
[0108]
Chemical formula i
[0109]
[0110]
Chemical formula j
[0111]
[0112]
Chemical formula k
[0113]
[0114]
Chemical formula 1
[0115]
[0116]
Chemical formula m
[0117]
[0118]
Chemical formula n
[0119]
[0120]
Chemical formula o
[0121]
[0122]
Chemical formula p
[0123]
[0124]
Chemical formula 3
[0125] By repeating unit and The resin formed.
[0126] (In the above structure, R5 is the same as R4 and is a structure selected from the structures of chemical formula a to chemical formula p.)
[0127]
Chemical formula 4
[0128] By repeating unit and The resin formed.
[0129] (In the aforementioned structure, R6 and R7 are one or more structures selected from the structures of Chemical Formula a to Chemical Formula p.)
[0130]
Chemical formula 5
[0131] By repeating unit and The resin formed.
[0132] (In the aforementioned structure, R8 and R9 are one or more structures selected from the structures of Chemical Formula a to Chemical Formula p.)
[0133] In a preferred embodiment of the present invention, the phenol polymer resin is one or more selected from the group consisting of phenol polymer resins containing hydroxyl groups represented by Chemical Formula 2 to Chemical Formula 5.
[0134] Preferably, the polymer resin is contained in an amount of 5 to 60 wt % relative to the total weight of the composition. If the polymer resin is used in an amount less than 5 wt %, problems such as poor profile, scum, and poor etching resistance may occur, and if the polymer resin is used in an amount exceeding 60 wt %, problems such as poor patterning may occur due to insufficient development.
[0135] The photoacid generator may include a photoacid generator selected from the group consisting of triphenylsulfonium triflate, triphenylsulfonium antimonate, diphenyliodonium triflate, diphenyliodonium antimonate, methoxydiphenyliodonium triflate, di-t-butyldiphenyliodonium triflate, 2,6-dinitrobenzenesulfonate, and 1,2-dinitrobenzenesulfonate.6-dinitrobenzylsulponate), pyrogalloltrisalkylsulfonate, norbornenedicarboxyimidetriflate, triphenylsulfoniumnonaflate, diphenyliodoniumnonaflate, methoxydiphenyliodoniumnonaflate, di-t-buthyldiphenyliodoniumnonaflate, N-hydroxysuccinimidenonaflate, norbornenedicarboxyimidetriflate, triphenylsulfoniumnonaflate, diphenyliodoniumnonaflate, methoxydiphenyliodoniumnonaflate, di-t-buthyldiphenyliodoniumnonaflate, N-hydroxysuccinimidenonaflate, norbornenedicarboxyimidetriflate, triphenylsulfoniumnonaflate, diphenyliodoniumnonaflate, methoxydiphenyliodoniumnonaflate, di-t-buthyldiphenyliodoniumnonaflate, One or more of the group consisting of norbornenedicarboxyimidenonaflate, triphenylsulfoniumperfluorooctanesulfonate, diphenyliodoniumperfluorooctanesulfonate, methoxydiphenyliodoniumperfluorooctanesulfonate, di-tert-butyldiphenyliodoniumperfluorooctanesulfonate, N-hydroxysuccinimideperfluorooctanesulfonate and norbornenedicarboxyimideperfluorooctanesulfonate.
[0136] Preferably, the photoacid generator comprises 0.05 to 10 wt % relative to the total weight of the composition. If the photoacid generator is used in an amount less than 0.05 wt %, the pattern tilt surface becomes excessive compared to the normal level due to insufficient acid generated, and when it exceeds 10 wt %, the photoacid generator absorbs light from the exposure source and reduces transmittance, thereby causing pattern defects such as inability to define.
[0137] The acid diffusion inhibitor may include one or more selected from the group consisting of dimethylamine, diethylamine, trimethylamine, triethylamine, tributhylamine, dimethanolamine, diethanolamine, trimethanolamine, triethanolamine, and tributhanolamine.
[0138] Preferably, the acid diffusion inhibitor comprises 0.01 to 5 wt % relative to the total weight of the composition. If the acid diffusion inhibitor is used in an amount less than 0.01 wt %, pattern defects such as pattern wall or edge defects (line width roughness (LWR), line edge roughness (LER)) may occur due to excessive acid generation, and when the acid diffusion inhibitor is used in an amount greater than 5 wt %, there is a problem that a pattern cannot be formed.
[0139] On the other hand, the thickness of the chemically amplified positive photoresist composition for improving pattern profile containing the transmittance-enhancing resin additive of the present invention can be adjusted according to the type and amount of the solvent used. to It can be used after being dissolved in 10 to 90% by weight relative to the weight of the solvent.
[0140] As the solvent, ethylene glycol monomethyl ether, ethylene glycol monoethyl ether, methyl cellosolve acetate, ethyl cellosolve acetate, diethylene glycol monomethyl ether, diethylene glycol monoethyl ether, propylene glycol monomethyl ... Ether acetate (Propyleneglycolmethyletheracetate), propylene glycol propyletheracetate (Propyleneglycolpropyletheracetate), diethylene glycol dimethyl ether (Diethyleneglycoldimethylether), ethyl lactate (Ethyllactate), toluene (Toluene), xylene (Xylene), methyl ethyl ketone (Methylethylketone), cyclohexanone (Cyclohexanone), 2-heptanone (2-heptanone), 3-heptanone (3-heptanone), 4-heptanone (4-heptanone), etc., and can be used alone or in combination.
[0141] As described above, the chemically amplified positive photoresist composition for improving pattern profiles provided by the present invention, which contains the transmittance-enhancing resin additive of the present invention, is composed by containing the transmittance-enhancing resin additive represented by Chemical Formula 1, and provides a photoresist composition capable of ensuring a vertical profile suitable for use in a semiconductor manufacturing process, thereby being able to provide an excellent process margin. DETAILED DESCRIPTION
[0142] [Example]
[0143] The present invention is described in more detail below by way of examples. These examples are only used to illustrate the present invention and are not to be construed as limiting the scope of the present invention based on these examples, which is obvious to those skilled in the art to which the present invention belongs.
[0144] [Example 1]
[0145] A KrF excimer laser positive photoresist composition was prepared using 100 g of a phenol polymer resin with a weight average molecular weight of 15,000 as a base resin (R8 in Chemical Formula 5 is Chemical Formula a, R9 is Chemical Formula c, and the copolymerization ratios 1, m, and n are 7, 2, and 1, respectively), 0.25 g of a transmittance enhancing resin additive with a weight average molecular weight of 17,000 (R1, R2, and R3 in Chemical Formula 1 are methyl, propyl, and butyl, respectively, and the copolymerization ratios a, b, c, and d are 20, 50, 15, and 15, respectively), 4 g of triphenylsulfonium perfluorobutanesulfonate as a photoacid generator, and 0.6 g of triethanolamine as an acid diffusion inhibitor, and a mixed solution of 104 g of propylene glycol monomethyl ether and 104 g of propylene glycol methyl ether acetate as a solvent. The prepared composition was coated on a silicon wafer using a spin coater and soft-baked at 140°C for 90 seconds, confirming the target thickness of 10um. If the exposure process is completed under a 248nm light source, the baking process is performed at 110°C for 80 seconds, and then a process of developing using 2.38% tetramethylammonium hydroxide is performed to form a pattern. As a result, it was confirmed that the sensitivity was 100mJ / cm 2 , and confirmed the positive slope pattern (Positive Slope Pattern) with a line / space reference resolution of 3.0μm and an inclination angle of 75°.
[0146] [Example 2]
[0147] A KrF excimer laser positive photoresist composition was prepared using 100 g of a phenol polymer resin with a weight average molecular weight of 15,000 as a base resin (R8 in Chemical Formula 5 is Chemical Formula a, R9 is Chemical Formula c, and the copolymerization ratios 1, m, and n are 7, 2, and 1, respectively), 1.5 g of a transmittance-enhancing resin additive with a weight average molecular weight of 17,000 (R1, R2, and R3 in Chemical Formula 1 are methyl, propyl, and butyl, respectively, and the copolymerization ratios a, b, c, and d are 20, 50, 15, and 15, respectively), 4 g of triphenylsulfonium perfluorobutanesulfonate as a photoacid generator, and 0.6 g of triethanolamine as an acid diffusion inhibitor, and a mixed solution of 105 g of propylene glycol monomethyl ether and 105 g of propylene glycol methyl ether acetate as a solvent. The prepared composition was coated on a silicon wafer using a spin coater and soft-baked at 140°C for 90 seconds, confirming the target thickness of 10um. If the exposure process is completed under a 248nm light source, the baking process is performed at 110°C for 80 seconds, and then a process of developing using 2.38% tetramethylammonium hydroxide is performed to form a pattern. As a result, it was confirmed that the sensitivity was 97mJ / cm 2, and confirmed a pattern with a line / space reference resolution of 3.0μm and a nearly vertical slope of 85°.
[0148] [Example 3]
[0149] A KrF excimer laser positive photoresist composition was prepared using 100 g of a phenol polymer resin with a weight average molecular weight of 15,000 as a base resin (R8 in Chemical Formula 5 is Chemical Formula a, R9 is Chemical Formula c, and the copolymerization ratios 1, m, and n are 7, 2, and 1, respectively), 25.0 g of a transmittance enhancing resin additive with a weight average molecular weight of 17,000 (R1, R2, and R3 in Chemical Formula 1 are methyl, propyl, and butyl, respectively, and the copolymerization ratios a, b, c, and d are 20, 50, 15, and 15, respectively), 4 g of triphenylsulfonium perfluorobutanesulfonate as a photoacid generator, and 0.6 g of triethanolamine as an acid diffusion inhibitor, and a mixed solution of 129 g of propylene glycol monomethyl ether and 129 g of propylene glycol methyl ether acetate as a solvent. The prepared composition was coated on a silicon wafer using a spin coater and soft-baked at 140°C for 90 seconds, confirming the target thickness of 10um. If the exposure process is completed under a 248nm light source, the baking process is performed at 110°C for 80 seconds, and then a process of developing using 2.38% tetramethylammonium hydroxide is performed to form a pattern. As a result, it was confirmed that the sensitivity was 91mJ / cm 2 , and confirmed a pattern with a line / space reference resolution of 2.5μm and a nearly vertical slope of 87°.
[0150] [Example 4]
[0151] A KrF excimer laser positive photoresist composition was prepared using 100 g of a phenol polymer resin with a weight average molecular weight of 15,000 as a base resin (R8 in Chemical Formula 5 is Chemical Formula a, R9 is Chemical Formula c, and the copolymerization ratios 1, m, and n are 7, 2, and 1, respectively), 50.0 g of a transmittance enhancing resin additive with a weight average molecular weight of 17,000 (R1, R2, and R3 in Chemical Formula 1 are methyl, propyl, and butyl, respectively, and the copolymerization ratios a, b, c, and d are 20, 50, 15, and 15, respectively), 4 g of triphenylsulfonium perfluorobutanesulfonate as a photoacid generator, and 0.6 g of triethanolamine as an acid diffusion inhibitor, and a mixed solution of 154 g of propylene glycol monomethyl ether and 154 g of propylene glycol methyl ether acetate as a solvent. The prepared composition was coated on a silicon wafer using a spin coater and soft-baked at 140°C for 90 seconds, confirming the target thickness of 10um. If the exposure process is completed under a 248nm light source, the baking process is performed at 110°C for 80 seconds, and then a process of developing using 2.38% tetramethylammonium hydroxide is performed to form a pattern. As a result, it was confirmed that the sensitivity was 80mJ / cm 2 , and was able to confirm a nearly vertical pattern with a line / space reference resolution of 2.0μm and a pattern slope of 90°, but scum and residual defects were confirmed at the bottom of the wafer.
[0152] [Comparative Example 1]
[0153] The experiment was conducted in the same manner as in Example 1 except that the transmittance-enhancing resin additive was not added. As a result, it was confirmed that the sensitivity was 110 mJ / cm 2 , the line / space reference resolution is 3.5μm, the pattern slope (PatternSlope) has a positive slope pattern (Positive Slope Pattern) with an inclination angle of 70°.
[0154] Characteristic determination
[0155] The characteristics of the chemically amplified positive photoresist composition for improving pattern profile prepared in the same manner as in Examples 1 to 4 and Comparative Example 1 were measured.
[0156] In terms of resolution, a scanning electron microscope (CD-SEM) capable of observing the line width (Critical Dimension) of a pattern was used to observe and confirm the minimum line width (resolution) based on L / S (Line / Space). In terms of sensitivity, the energy (Energy) that can determine the minimum line width (resolution) was measured as the sensitivity.
[0157] The results of the above measurements are shown in Table 1 below.
[0158]
Table 1
[0159]
[0160]
[0161] As can be seen from Table 1 above, it can be confirmed that Examples 2 and 3 have superior sensitivity compared to Comparative Example 1, and the resolution as the minimum line width and the vertical pattern slope (Pattern Slope) are also improved, but in the case of Example 1, when it is compared with Comparative Example 1, there is no improvement effect in resolution and vertical pattern slope (Pattern Slope). In the case of Example 4, when it is compared with Comparative Example 1, the sensitivity, the resolution as the minimum line width and the vertical pattern slope (Pattern Slope) are improved, but defects such as scum and residue are confirmed.
[0162] As a result, it was confirmed that when the transmittance-enhancing resin additive of the structure of Chemical Formula 1 is contained at an optimal content, the sensitivity and transmittance of the formed pattern can be improved to provide a KrF light source photoresist composition showing a vertical profile compared to conventional KrF positive photoresists.
[0163] Simple modifications or changes of the present invention can be easily realized by ordinary technicians in the technical field to which the present invention belongs, and it can be considered that such modifications or changes are included in the field of the present invention.
Claims
1. A chemically amplified positive photoresist composition for improving pattern profile, characterized in that: The photoresist composition can be exposed with a light source having a wavelength of 248 nm, and the whole composition comprises 5 to 60 wt % of a polymer resin, 0.1 to 10 wt % of a transmittance-enhancing resin additive represented by the following chemical formula 1, 0.05 to 10 wt % of a photoacid generator, 0.01 to 5 wt % of an acid diffusion inhibitor, and the remaining solvent. The polymer resin is one or more selected from the group consisting of phenol polymer resins containing hydroxyl groups represented by Chemical Formula 2 to Chemical Formula 5, 【Chemical formula 1】 Wherein, a, b, c, d are molar ratios of repeating units forming the copolymer and are each 1 to 9; in the structure described above, R1, R2, and R3 are selected from one or more structures formed by methyl (R-CH3), ethyl (R-CH2CH3), propyl (R-CH2CH2CH3), butyl (R-CH2CH2CH2CH3) and combinations thereof, and R1, R2, and R3 are different from each other, and R represents a binding site. 【Chemical formula 2】 By repeating unit and The resin formed In the aforementioned structure, R4 is a structure selected from the following chemical formula a to chemical formula p, R represents a binding site, 【Chemical formula a】 【Chemical formula b】 【Chemical formula c】 【Chemical formula d】 【Chemical formula e】 【Chemical formula f】 【Chemical formula g】 【Chemical formula h】 【Chemical formula i】 【Chemical formula j】 【Chemical formula k】 【Chemical formula 1】 【Chemical formula m】 【Chemical formula n】 【Chemical formula o】 【Chemical formula p】 【Chemical formula 3】 By repeating unit and The resin formed In the above structure, R5 is the same as R4 and is a structure selected from the structures of chemical formula a to chemical formula p. 【Chemical formula 4】 By repeating unit and The resin formed In the aforementioned structure, R6 and R7 are one or more structures selected from the structures of chemical formula a to chemical formula p, 【Chemical formula 5】 By repeating unit and The resin formed In the aforementioned structure, R8 and R9 are one or more structures selected from the structures of Chemical Formula a to Chemical Formula p.
2. The chemically amplified positive photoresist composition for improving pattern profile according to claim 1, characterized in that: The transmittance enhancing resin additive represented by Chemical Formula 1 has a weight average molecular weight of 2,000 to 20,000.
3. The chemically amplified positive photoresist composition for improving pattern profile according to claim 1, characterized in that: The photoacid generator comprises a photoacid generator selected from the group consisting of triphenylsulfonium trifluoromethanesulfonate, triphenylsulfonium antimonate, diphenyliodonium trifluoromethanesulfonate, diphenyliodonium antimonate, methoxydiphenyliodonium trifluoromethanesulfonate, di-tert-butyldiphenyliodonium trifluoromethanesulfonate, 2,6-dinitrobenzenesulfonate, pyrogallol trialkylsulfonate, norbornene dicarboxylic imide trifluoromethanesulfonate, triphenylsulfonium perfluorobutylsulfonate, diphenyliodonium perfluorobutylsulfonate, methoxydiphenyliodonium perfluorobutylsulfonate, At least one of the group consisting of iodine sulfonate, di-tert-butyldiphenyliodonium perfluorobutylsulfonate, N-hydroxysuccinimide perfluorobutylsulfonate, norbornene dicarboxy imide perfluorobutylsulfonate, triphenylsulfonium perfluorooctane sulfonate, diphenyl iodonium perfluorooctane sulfonate, methoxydiphenyl iodonium perfluorooctane sulfonate, di-tert-butyldiphenyliodonium perfluorooctane sulfonate, N-hydroxysuccinimide perfluorooctane sulfonate and norbornene dicarboxy imide perfluorooctane sulfonate.
4. The chemically amplified positive photoresist composition for improving pattern profile according to claim 1, characterized in that: The acid diffusion inhibitor includes at least one selected from the group consisting of dimethylamine, diethylamine, trimethylamine, triethylamine, tributylamine, dimethanolamine, diethanolamine, trimethanolamine, triethanolamine, and tributanolamine.