Semiconductor device and method for forming the same
By forming alternating layers on the semiconductor fins and dielectric fins and selectively removing semiconductor materials, forming nanowires and extended dielectric fins, the problem of poor filling of gate spacers in semiconductor devices is solved, and device integration is improved Density and filling efficiency reduce the risk of resistance and electrical short circuit.
Patent Information
- Application Number
- CN202010851257.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-08-23
- Filing Date
- 2020-08-21
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2040-08-21
AI Technical Summary
As the minimum feature size of semiconductor devices decreases, the challenges of creating high density integration increase, especially the problems of poor filling between gate spacers leading to reduced yield and increased resistance.
By forming alternating layers on the semiconductor fins and dielectric fins, the semiconductor material is selectively removed to form nanowires and expanding on the dielectric fins, the central width of the hybrid fins is reduced to increase the dielectric fins and The distance between nanowires simplifies the metal filling process to form an efficient metal gate.
Improves the filling efficiency of the metal gate, reduces resistance, increases device integration density, and provides a large error tolerance to reduce the risk of electrical short circuits.
Smart Images

Figure CN112420614B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductors, and in particular, to semiconductor devices and methods for forming the same. Background Art
[0002] Semiconductor devices are used in a variety of electronic applications, such as personal computers, cell phones, digital cameras, and other electronic devices. Semiconductor devices are typically manufactured by sequentially depositing insulating or dielectric layers, conductive layers, and semiconductor material layers on a semiconductor substrate, and patterning the various material layers using photolithography and etching techniques to form circuit components and elements thereon.
[0003] The semiconductor industry continues to improve the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.) by continuously reducing the minimum feature size, thereby allowing more components to be integrated into a given area. However, as the minimum feature size decreases, other issues arise that should be addressed. Summary of the invention
[0004] An embodiment of the present application provides a method for forming a semiconductor device, the method comprising: forming a semiconductor fin over a substrate, and forming a patterned mask layer over the semiconductor fin, wherein the semiconductor fin comprises an epitaxial layer over a semiconductor strip, wherein the epitaxial layer comprises alternating layers of a first semiconductor material and a second semiconductor material; forming a hybrid fin over an isolation region on opposite sides of the semiconductor fin, wherein each hybrid fin comprises a dielectric fin and a dielectric structure over the dielectric fin; forming a gate structure over the semiconductor fin and over the hybrid fin; removing a first portion of the patterned mask layer, a first portion of the epitaxial layer, and a second portion of the gate structure; and removing a first portion of the patterned mask layer, a first portion of the epitaxial layer, and a second portion of the gate structure. The invention relates to a method of removing a first semiconductor material from a substrate and a second semiconductor material and removing a first portion of a dielectric structure from a substrate, wherein the second semiconductor material forms a nanowire after the selective removal, wherein the second dielectric structure extends further from the substrate than an uppermost surface of the nanowire.
[0005] An embodiment of the present application provides a method for forming a semiconductor device, the method comprising: forming a protruding semiconductor strip over a substrate; forming an isolation region between adjacent semiconductor strips; forming a hybrid fin on the isolation region, the hybrid fin comprising a dielectric fin and a dielectric structure over the dielectric fin; forming a dummy gate structure over the semiconductor strip and the hybrid fin; forming a source / drain region over the semiconductor strip and on opposite sides of the dummy gate structure; forming a nanowire under the dummy gate structure, wherein the nanowire is over and aligned with a corresponding semiconductor strip, and the source / drain region is at opposite ends of the nanowire, wherein the hybrid fin extends farther from the substrate than the nanowire; after forming the nanowire, reducing the width of a central portion of the hybrid fin while maintaining the width of an end portion of the hybrid fin unchanged, wherein the central portion of the hybrid fin is under the dummy gate structure, and the end portion of the hybrid fin is outside the boundary of the dummy gate structure; and forming a conductive material around the nanowire.
[0006] An embodiment of the present application provides a semiconductor device, comprising: a semiconductor strip protruding above a substrate; a first isolation region and a second isolation region, the first isolation region and the second isolation region being located on opposite sides of the semiconductor strip; a nanowire, the nanowire being located above the semiconductor strip and aligned with the semiconductor strip; a source / drain region, the source / drain region being located at opposite ends of the nanowire;
[0007] A first dielectric fin, the first dielectric fin is located on the first isolation region; and a metal gate, the metal gate is located around the nanowire and around a central portion of the first dielectric fin, wherein ends of the first dielectric fin are arranged on opposite sides of the metal gate, and wherein the ends of the first dielectric fin are wider than the central portion of the first dielectric fin.
[0008] The embodiments of the present application provide a gate-all-around field effect transistor device. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] When read in conjunction with the accompanying drawings, various aspects of the present invention can be best understood from the following detailed description. It should be noted that, in accordance with standard practice in the industry, the various components are not drawn to scale. In fact, for clarity of discussion, the size of the various components may be arbitrarily increased or reduced.
[0010] Figure 1-Figure 26 are various views of a gate-all-around (GAA) field effect transistor (FET) device at various stages of fabrication according to one embodiment;
[0011] Fig. 27 is a cross-sectional view of a GAA FET device according to another embodiment;
[0012] Fig.28is a cross-sectional view of a GAA FET device according to yet another embodiment;
[0013] Fig.29 is a flow chart of a method of forming a GAA FET device according to some embodiments. DETAILED DESCRIPTION
[0014] The following disclosure provides many different embodiments or examples for realizing different features of the present invention. Specific examples of components and arrangements are described below to simplify the present invention. Of course, these are merely examples and are not intended to limit the present invention. For example, in the following description, forming a first component above or on a second component may include an embodiment in which the first component and the second component are directly contacted, and may also include an embodiment in which an additional component may be formed between the first component and the second component so that the first component and the second component may not be in direct contact. In addition, the present disclosure may repeat reference numbers and / or letters in various examples. Unless otherwise stated, the same or similar reference numerals in different drawings represent the same or similar components formed by the same or similar (some) processes using the same or similar (some) materials.
[0015] Additionally, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "upper," etc. may be used herein to easily describe the relationship of one element or component to another (or additional) elements or components as shown in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein should likewise be interpreted accordingly.
[0016] In some embodiments, a gate-all-around (GAA) field effect transistor (FET) device includes a semiconductor strip protruding above a substrate, and a first isolation region and a second isolation region located on opposite sides of the semiconductor strip. The GAA FET device also includes a nanowire located above and aligned with the semiconductor strip, and a source / drain region located at opposite ends of the nanowire. The GAA FET device also includes a first dielectric fin located on the first isolation region, and a metal gate surrounding the nanowire and surrounding a central portion of the first dielectric fin, wherein an end of the first dielectric fin is disposed on an opposite side of the metal gate, and the end of the first dielectric fin is wider than the central portion of the first dielectric fin.
[0017] Figure 1-Figure 26 are various views (eg, perspective, cross-sectional, plan views) of a gate-all-around (GAA) field effect transistor (FET) device 100 at various stages of fabrication according to one embodiment. Figure 1-Figure 13 and Fig.23 is a perspective view of a GAA FET device 100 . Figure 14-Figure 22 , Fig.25 ,as well as Fig.26 is a cross-sectional view of a GAA FET device 100, Fig.24 is a top view of the GAA FET device 100. Note that for clarity, Figure 1-Figure 26 Some of the figures may show only a portion of the GAA FET device 100 , but not the entirety.
[0018] refer to Figure 1 , a substrate 101 is provided. The substrate 101 may be a semiconductor substrate, such as a bulk semiconductor (e.g., bulk silicon), a semiconductor on insulator (SOI) substrate, etc., which may be doped (e.g., with a P-type or N-type dopant) or undoped. The substrate 101 may be a wafer, such as a silicon wafer. Typically, an SOI substrate is a semiconductor material layer formed on an insulator layer. The insulator layer may be, for example, a buried oxide (BOX) layer, a silicon oxide layer, etc. The insulator layer is disposed on a substrate, typically a silicon substrate or a glass substrate. Other substrates, such as a multilayer substrate or a gradient substrate may also be used. In some embodiments, the semiconductor material of the substrate 101 includes: silicon; germanium; compound semiconductors, including silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; alloy semiconductors, including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, and / or GaInAsP; or combinations thereof.
[0019] exist Figure 1 In the embodiment shown, an epitaxial material stack 104' is formed on a substrate 101, and a hard mask layer 107' is formed on the epitaxial material stack 104'. The epitaxial material stack 104' includes alternating first semiconductor layers 103 and second semiconductor layers 105. The first semiconductor layers 103 are formed of a first semiconductor material, and the second semiconductor layers 105 are formed of a different second semiconductor material. In the embodiment shown, the first semiconductor material is silicon germanium (Si x Ge 1-x , where x can be in the range of 0 to 1), the second semiconductor material is silicon. The epitaxial material stack 104' may include any number of layers. In a subsequent process, the epitaxial material stack 104' will be patterned to form a channel region of the GAA FET. In particular, the epitaxial material stack 104' will be patterned to form horizontal nanowires, and the channel region of the resulting GAA FET includes a plurality of horizontal nanowires.
[0020] The epitaxial material stack 104' can be formed by an epitaxial growth process, which can be implemented in a growth chamber. During the epitaxial growth process, the growth chamber is cyclically exposed to a first set of precursors for growing the first semiconductor layer 103, and to a second set of precursors for growing the second semiconductor layer 105. The first set of precursors includes precursors for a first semiconductor material (e.g., silicon germanium), and the second set of precursors includes precursors for a second semiconductor material (e.g., silicon). The epitaxial material stack 104' can be doped or undoped, depending on the design of the GAA FET device.
[0021] In some embodiments, the first group of precursors includes a silicon precursor (e.g., silane) and a germanium precursor (e.g., germanium), and the second group of precursors includes a silicon precursor but omits the germanium precursor. Thus, the epitaxial growth process may include enabling the silicon precursor to flow continuously to the growth chamber, and then cyclically: (1) enabling the germanium precursor to flow to the growth chamber when growing the first semiconductor layer 103; and (2) disabling the germanium precursor to flow to the growth chamber when growing the second semiconductor layer 105. The cyclic exposure may be repeated until a target number of layers are formed. After the growth cycle is completed, a planarization process may be performed to flatten the top surface of the epitaxial material stack 104'. The planarization process may be a chemical mechanical polishing (CMP), an etch back process, a combination thereof, or the like.
[0022] Next, a hard mask layer 107' is formed over the epitaxial material stack 104'. The hard mask layer 107' may include sublayers, such as a pad oxide layer and an overlying pad nitride layer. The pad oxide layer may be a thin film including silicon oxide formed, for example, using a thermal oxidation process. The pad oxide layer may serve as an adhesion layer between the epitaxial material stack 104' and the pad nitride layer. In some embodiments, the pad nitride layer is formed of silicon nitride, silicon oxynitride, silicon carbonitride, etc., or a combination thereof, and may be formed, by way of example, using low pressure chemical vapor deposition (LPCVD) or plasma enhanced chemical vapor deposition (PECVD).
[0023] Next reference Figure 2 , using techniques such as photolithography and etching, patterning Figure 1 The hard mask layer 107' is patterned to form a patterned hard mask 107, and then the patterned hard mask 107 is used as an etching mask to pattern the substrate 101 and the epitaxial material stack 104'. Thereafter, a liner 109 is formed over the semiconductor fin 102 and the patterned hard mask 107. The details will be discussed below.
[0024] To form the semiconductor fins 102, the hard mask layer 107' may be patterned using photolithography techniques. Typically, photolithography techniques utilize a photoresist material that is deposited, irradiated (exposed), and developed to remove a portion of the photoresist material. The remaining photoresist material protects the underlying material, such as the hard mask layer 107' in this example, from subsequent processing steps such as etching. In this example, the photoresist material is used to pattern the hard mask layer 107' to form a patterned hard mask 107, such as Figure 2 shown.
[0025] The substrate 101 and the epitaxial material stack 104' are then patterned using the patterned hard mask 107 to form trenches 108, thereby defining semiconductor fins 102 between adjacent trenches 108, such as Figure 2 As shown. In the illustrated embodiment, each semiconductor fin 102 includes a semiconductor strip 106 and a patterned epitaxial material stack 104 above the semiconductor strip 106. The semiconductor strip 106 is a patterned portion of the substrate 101 and protrudes above the (recessed) substrate 101. The patterned epitaxial material stack 104 is a patterned portion of the epitaxial material stack 104' and will be used to form a nanowire in subsequent processing, and therefore, may also be referred to as a nanowire structure 104 or a GAA structure 104.
[0026] In some embodiments, trenches in the substrate 101 and in the epitaxial material stack 104' are etched to form semiconductor fins 102 by using, for example, reactive ion etching (RIE), neutral beam etching (NBE), etc., or a combination thereof. The etching process may be anisotropic. In some embodiments, the trenches 108 may be strips parallel to each other (viewed from the top) and closely spaced relative to each other. In some embodiments, the trenches 108 may be continuous and surround the semiconductor fins 102. The semiconductor fins 102 may also be referred to as fins 102 hereinafter.
[0027] The fins 102 may be patterned by any suitable method. For example, the fins 102 may be patterned using one or more photolithography processes, including double patterning or multi-patterning processes. Typically, double patterning or multi-patterning processes combine photolithography and self-alignment processes, allowing for the creation of patterns having a smaller pitch than that obtainable using a single direct photolithography process, for example. For example, in one embodiment, a sacrificial layer is formed over a substrate, and the sacrificial layer is patterned using a photolithography process. Spacers are formed next to the patterned sacrificial layer using a self-alignment process. The sacrificial layer is then removed, after which the remaining spacers or mandrels may be used to pattern the fins.
[0028] After forming the fin 102, a liner 109 is formed along the sidewalls and bottom of the trench 108. The liner 109 may also be formed over the upper surface of the patterned hard mask 107. In an exemplary embodiment, the liner 109 is a silicon liner formed by, for example, CVD, atomic layer deposition (ALD), a combination thereof, or the like.
[0029] Figure 3 The formation of an insulating material between adjacent semiconductor fins 102 is shown to form an isolation region 111. The insulating material can be an oxide, such as silicon oxide, nitride, etc., or a combination thereof, and can be formed by high density plasma chemical vapor deposition (HDP-CVD), flowable CVD (FCVD) (e.g., CVD-based material deposition and post-curing in a remote plasma system to convert it into another material, such as an oxide), etc., or a combination thereof. Other insulating materials and / or other formation processes may be used. In the illustrated embodiment, the insulating material is silicon oxide formed by an FCVD process. Once the insulating material is formed, an annealing process may be performed. Any excess insulating material may be removed from above the top surface of the semiconductor fin 102 by a planarization process such as CMP.
[0030] Next, the isolation region is recessed to form a shallow trench isolation (STI) region 111. The isolation region 111 is recessed so that the upper portion of the semiconductor fin 102 protrudes from between adjacent STI regions 111. The top surface of the STI region 111 may have a flat surface (as shown), a raised surface, a recessed surface (e.g., a depression), or a combination thereof. By appropriate etching, the top surface of the STI region 111 may be formed as a flat, raised, and / or recessed surface. The isolation region 111 may be recessed using an acceptable etching process, such as an etching process that is selective to the material of the isolation region 111. For example, dry etching or wet etching using dilute hydrofluoric acid (dHF) may be performed to recess the isolation region 111. In Figure 3 In FIG. 1 , the upper surface of STI region 111 is shown to be flush with the upper surface of semiconductor strip 106. In other embodiments, the upper surface of STI region 111 is lower than the upper surface of semiconductor strip 106 (eg, closer to substrate 101).
[0031] like Figure 3 As shown, the upper portion of the liner 109 disposed above the upper surface of the STI region 111 is removed. A suitable etching process, such as a wet etching process or a dry etching process, may be used to remove the upper portion of the liner 109. In some embodiments, the liner 109 is removed in the same etching process used to recess the isolation region 111.
[0032] Next, in Figure 4In the embodiment, a capping layer 113 is conformally formed over the GAA structure 104 and over the patterned hard mask 107. In some embodiments, the capping layer 113 is an epitaxial semiconductor layer formed using, for example, a CVD process. In an exemplary embodiment, the capping layer 113 and the first semiconductor layer 103 are formed of the same epitaxial material (e.g., silicon germanium). In some embodiments, an epitaxial growth process is used to form a liner 109 (e.g., a silicon liner, see FIG. 1 ). Figure 3 ) is selectively grown on the exposed surface of the STI region 111, so that the upper surface of the STI region 111 is free of the capping layer 113. As an example, the capping layer 113 may have a thickness of about 5 nm. To avoid confusion, the portion of the liner 109 disposed above the upper surface of the STI region 111 is not shown in FIG. Figure 4 As shown in subsequent figures, it should be understood that a liner 109 may be present between the capping layer 113 and the GAA structure 104 / patterned hard mask 107 .
[0033] Next, in Figure 5 In the embodiment, a dielectric layer 114 is conformally formed over the cap layer 113 and over the upper surface of the STI region 111. Next, a dielectric layer 115 is formed over the dielectric layer 114 to fill the trench 108. The dielectric layer 114 and the dielectric layer 115 are then etched back to form a dielectric fin 116, details of which will be discussed below.
[0034] In some embodiments, dielectric layer 114 is formed by forming a conformal layer of silicon nitride along cap layer 113 and along the upper surface of STI region 111 using a suitable deposition method such as CVD. Dielectric layer 115 is then formed on dielectric layer 114. In the illustrated embodiment, dielectric layer 115 is formed using a low-K dielectric material (e.g., having a dielectric constant K of less than about 7, such as less than about 3.9) such as SiO2, SiN, SiCN, or SiOCN.
[0035] Next, the dielectric layer 115 (e.g., a low-K dielectric material) is etched back using, for example, a dry etching process or a wet etching process. For example, the dielectric layer 115 can be etched back using a dry etching process using a fluoride-containing gas. After etching back the dielectric layer 115, the dielectric layer 114 exposed through the recessed dielectric layer 115 is removed by a suitable etching process such as a dry etching process or a wet etching process. For example, a wet etching process using H3PO4 as an etchant can be performed to remove the exposed dielectric layer 114. The remaining portion of the dielectric layer 114 and the remaining portion of the dielectric layer 115 form a dielectric fin 116. In Figure 5In the example of , the upper surface of the remaining portion of the dielectric layer 114 and the upper surface of the remaining portion of the dielectric layer 115 are flush with each other. Since both the dielectric layer 114 and the dielectric layer 115 are formed of low-K dielectric materials, the dielectric fin 116 can also be referred to as a low-K dielectric fin. Figure 5 As shown, the dielectric fin 116 is formed on the STI region 111 and physically contacts the capping layer 113 disposed on opposite sides of the dielectric fin 116 .
[0036] Next, in Figure 6 In the process, a dielectric structure 118 is formed to fill the remaining portion of the trench 108. Figure 6 In the example, by Figure 5 A dielectric layer 117 is conformally formed over the structure of the hard mask 107, and then a dielectric layer 119 is formed over the dielectric layer 117 to form a dielectric structure 118. A planarization process such as CMP is then performed to remove a portion of the capping layer 113, a portion of the dielectric layer 117, and a portion of the dielectric layer 119 from the upper surface of the patterned hard mask 107.
[0037] In some embodiments, aluminum oxide (e.g., AlO) is deposited using a suitable deposition method such as CVD, PVD, combinations thereof, or the like. x ) to form the dielectric layer 117. The thickness of the dielectric layer 117 may be, for example, about 2 nm. x 、HfSiO x , or Al2O3 (e.g., having a dielectric constant K greater than about 7) to form dielectric layer 119. Since both dielectric layer 117 and dielectric layer 119 are formed of high-K dielectric materials, dielectric structure 118 may also be referred to as a high-K dielectric structure. In addition, since dielectric fin 116 is formed of a low-K dielectric material, and since dielectric structure 118 is formed of a high-K dielectric material, each dielectric fin 116 and the corresponding overlying dielectric structure 118 may be collectively referred to as a hybrid fin 112.
[0038] Next reference Figure 7 , in the semiconductor fin 102 (reference Figure 6 A dummy gate structure 122 is formed above the hybrid fin 112 and above the hybrid fin 112. In some embodiments, each dummy gate structure 122 includes a gate dielectric 121 and a gate electrode 123.
[0039] In order to form the dummy gate structure 122, Figure 6A dielectric layer is formed on the structure shown. The dielectric layer can be, for example, silicon oxide, silicon nitride, multiple layers thereof, etc., and can be deposited or thermally grown. Next, a gate layer is formed over the dielectric layer, and then a mask layer is formed over the gate layer. The gate layer can be deposited over the dielectric layer and then planarized, for example, by a CMP process. A mask layer can be deposited over the gate layer. The gate layer can be formed, for example, by polysilicon, but other materials can also be used. The mask layer can be formed, for example, by silicon oxide, silicon nitride, combinations thereof, etc.
[0040] After forming the layers (eg, dielectric layer, gate layer, and mask layer), the mask layer may be patterned using acceptable photolithography and etching techniques to form mask 126. Figure 7 In the example of , mask 126 includes a first mask 125 (e.g., silicon oxide) and a second mask 127 (e.g., silicon nitride). The pattern of mask 126 is then transferred to the gate layer and the dielectric layer by an acceptable etching technique to form a gate electrode 123 and a gate dielectric 121, respectively. The gate electrode 123 and the gate dielectric 121 are located above (e.g., directly above) the corresponding channel region of the GAA FET device to be formed. The gate electrode 123 may also have a length direction substantially perpendicular to the length direction of the semiconductor fin 102 or the length direction of the hybrid fin 112.
[0041] Next, in Figure 8 In the embodiment, a gate spacer 129 is formed on the sidewalls of the gate electrode 123 and the gate dielectric 121. Figure 7 A gate spacer layer is conformally deposited on the structure shown to form a gate spacer 129. The gate spacer layer can be silicon nitride, silicon carbonitride, a combination thereof, or the like. In some embodiments, the gate spacer layer includes multiple sub-layers. For example: a first sub-layer (sometimes referred to as a gate sealing spacer layer), which can be formed by thermal oxidation or deposition; and a second sub-layer (sometimes referred to as a main gate spacer layer), which can be conformally deposited on the first sub-layer. The gate spacer 129 can be formed by anisotropically etching the gate spacer layer. The anisotropic etching can remove the horizontal portion of the gate spacer layer (e.g., above the patterned hard mask 107, the hybrid fin 112, and the mask 126), and the remaining vertical portion of the gate spacer layer (e.g., along the sidewalls of the gate electrode 123 and the sidewalls of the gate dielectric 121) forms the gate spacer 129. In the discussion herein, the gate spacer 129 may also be referred to as a portion of the dummy gate structure 122.
[0042] Next, an anisotropic etching process is performed to remove portions of the dielectric structure 118 located outside the boundary of the dummy gate structure 122 (e.g., outside the outer sidewalls of the gate spacer 129), portions of the GAA structure 104 (e.g., 103 and 105), and portions of the patterned hard mask 107. The anisotropic etching process can be performed using the dummy gate structure 122 as an etching mask. After the anisotropic etching, in some embodiments, due to the anisotropic etching, the sidewalls 129S of the gate spacer 129 are aligned with the corresponding sidewalls 105S of the second semiconductor layer 105.
[0043] In some embodiments, the anisotropic etching process is a dry etching process (e.g., a plasma etching process) using (some) etchants that are selective (e.g., have a higher etching rate) to the materials of the patterned hard mask 107 and the GAA structure 104. In an exemplary embodiment, the dry etching process has an average etching rate of E1 for the dielectric structure 118 (e.g., high-K material) and an average etching rate of E2 (E2>E1) for the combination of the patterned hard mask 107 (e.g., low-K material) and the GAA structure 104 (e.g., semiconductor material), and the ratio between E1 and E2 can be selected as E1 / E2=H1 / H2, where H1 is the height of the dielectric structure 118, and H2 is the sum of the height of the patterned hard mask 107 and the height of the GAA structure 104. With the above relationship between the ratios, when the dielectric structure 118 is removed (e.g., outside the boundaries of the dummy gate structure 122) to expose the underlying dielectric fins 116, the patterned hard mask 107 and the GAA structure 104 are also removed (e.g., outside the boundaries of the dummy gate structure 122) to expose the underlying semiconductor strips 106.
[0044] Next, in Fig. 9 In the embodiment of the present invention, a lateral etching process is performed to recess the exposed portion of the first semiconductor material using an etchant selective to the first semiconductor material. Fig. 9 In the example of , both the capping layer 113 and the first semiconductor layer 103 are formed of a first semiconductor material (e.g., SiGe), and therefore, the lateral etching recesses both the capping layer 113 and the first semiconductor layer 103. After the lateral etching process, the first semiconductor material is recessed from the sidewalls 129S of the gate spacer 129, from the sidewalls 105S of (the remaining portion) of the second semiconductor layer 105, and from the sidewalls of (the remaining portion) of the patterned hard mask 107. For example, Fig. 9 An offset R between the sidewall 105S of the second semiconductor layer 105 and the sidewall of the recessed first semiconductor layer 103 is shown.
[0045] Next, in Fig.10In the embodiment, a dielectric material 131 is formed to fill the above reference Fig. 9 The space left by the removal (e.g., recessing) of the first semiconductor material discussed. The dielectric material 131 can be a low-K dielectric material, such as SiO2, SiN, SiCN, or SiOCN, and can be formed by a suitable deposition method such as ALD. After the deposition of the dielectric material 131, an anisotropic etching process can be performed to trim the deposited dielectric material 131 so that only the portion of the deposited dielectric material 131 that fills the space left by the removal of the first semiconductor material remains. After the trimming process, the remaining portion of the deposited dielectric material 131 forms an internal spacer 131. The internal spacer 131 is used to isolate the metal gate from the source / drain region formed in subsequent processing. Fig. 9 In the example shown in FIG. 4 , the front sidewall of the inner spacer 131 is aligned with the sidewall 129S of the gate spacer 129 .
[0046] Next, in Fig.11 In the embodiment of the present invention, source / drain regions 133 are formed over semiconductor strips 106. Source / drain regions 133 are formed by epitaxially growing a material over semiconductor strips 106 using a suitable method such as metal organic CVD (MOCVD), molecular beam epitaxy (MBE), liquid phase epitaxy (LPE), vapor phase epitaxy (VPE), selective epitaxial growth (SEG), etc., or a combination thereof.
[0047] like Fig.11 As shown, the epitaxial source / drain regions 133 fill the spaces between adjacent dielectric fins 116. The epitaxial source / drain regions 133 may include surfaces that are raised from the surfaces of the dielectric fins 116 and may include facets. The source / drain regions 133 above adjacent semiconductor strips 106 may merge to form a continuous epitaxial source / drain region 133, as shown. Fig.11 As shown. In some embodiments, the source / drain regions 133 above adjacent semiconductor strips 106 are not merged together, but separate source / drain regions 133 are maintained. The (some) materials of the source / drain regions 133 can be tuned according to the type of device to be formed. In some embodiments, the resulting GAA FET is an n-type FinFET, and the source / drain regions 133 include silicon carbide (SiC), silicon phosphorus (SiP), phosphorus-doped silicon carbon (SiCP), etc. In some embodiments, the resulting GAA FET is a p-type FinFET, and the source / drain regions 133 include SiGe and p-type impurities such as boron or indium.
[0048] The epitaxial source / drain regions 133 may be implanted with dopants and then subjected to an annealing process. The implantation process may include forming and patterning a mask, such as a photoresist, to cover areas of the GAA FET device that need to be protected from the implantation process. The source / drain regions 133 may have a thickness of approximately 1E19 cm -3 to about 1E21cm -3 The impurity (e.g., dopant) concentration may be within a range of . P-type impurities such as boron or indium may be implanted in the source / drain regions 133 of a P-type transistor. N-type impurities such as phosphorus or arsenide may be implanted in the source / drain regions 133 of an N-type transistor. In some embodiments, the epitaxial source / drain regions may be in-situ doped during growth.
[0049] Next, in Fig.12 in Fig.11 A contact etch stop layer (CESL) 135 is formed over the structure shown, and an interlayer dielectric (ILD) layer 137 is formed over the CESL 135. The CESL 135 serves as an etch stop layer in a subsequent etching process, and may include a suitable material such as silicon oxide, silicon nitride, silicon oxynitride, a combination thereof, and may be formed by a suitable formation method such as CVD, PVD, a combination thereof, or the like.
[0050] An ILD layer 137 is formed over the CESL 135 and around the dummy gate structure 122. In some embodiments, the ILD layer 137 is formed of a dielectric material such as silicon oxide, phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), etc., and may be deposited by any suitable method such as CVD, PECVD, or FCVD. A planarization process such as a CMP process may be performed to remove the mask 126 (see FIG. 1 ). Fig.11 ), and removing a portion of the CESL 135 disposed above the gate electrode 123. Fig.12 As shown, after the planarization process, the top surface of the ILD layer 137 is flush with the top surface of the gate electrode 123 .
[0051] Next, in Fig.13 In the etching step (some), the gate electrode 123 of the dummy gate structure is removed (refer to Fig.12 ) and gate dielectric 121 (reference Fig.12), thereby forming grooves 128 between the gate spacers 129. Each groove exposes a remaining portion of the patterned hard mask 107 disposed under the dummy gate structure. After removing the gate electrode 123 and the gate dielectric 121, a cut metal gate (CMG) pattern 139 is formed in the groove 128. The top surface of the CMG pattern 139 may extend above the upper surface of the ILD layer 137. The patterned hard mask layer 139A (see FIG. 1 ) may be formed by depositing a photoresist layer in the groove 128 and forming a patterned hard mask layer 139A (see FIG. 1 ) above the photoresist layer. Fig.14 ), a CMG pattern 139 is formed by patterning the photoresist layer using the patterned hard mask layer 139A to form a patterned photoresist 139B.
[0052] Figure 14-Figure 22 Shown along Fig.13 1 is a cross-sectional view of the GAA FET device 100 at various processing stages, wherein the cross-section BB is located between the gate spacers 129 (eg, in the groove 128 ) and along the longitudinal direction of the dummy gate structure 122 . Fig.14 A cross-sectional view of the GAA FET device 100 along the cross section BB after forming the CMG pattern 139 is shown, as described above with reference to FIG. Fig.13 described.
[0053] Next, in Fig.15 In the embodiment of the present invention, the dielectric structure 118 exposed by the CMG pattern 139 is removed, for example, by an etching process. The etching process may use an etchant that is selective to the material of the dielectric structure 118. For example, a dry etching process using a chlorine-containing etchant may be performed to remove the exposed dielectric structure 118. After the dielectric structure 118 is removed, the CMG pattern 139 is removed by a suitable method such as an etching process, an ashing process, a combination thereof, or the like. The recess 136 is formed at the location of the dielectric structure 118 that was once removed.
[0054] Next reference Fig.16 For example, the upper surface of the patterned hard mask 107 is recessed by a dry etching process, so that the upper surface of the patterned hard mask 107 is located below the upper surface of the dielectric structure 118 (for example, closer to the substrate 101). The upper surface of the capping layer 113 may also be recessed by an etching process. Fig.16 In the example of FIG. 1 , after the etching process, the remaining portion of the patterned hard mask 107 remains. In subsequent processing, the remaining portion of the patterned hard mask 107 can protect the underlying nanowires 110 (see FIG. 1 ). Figure 17-Figure 19 ) to prevent it from being overetched by the subsequent (some) etching process. In other embodiments, the etching process completely removes (see, for example, Fig. 27 ) patterned hard mask 107.
[0055] Next, in Fig.17 In the process, the first semiconductor layer 103 and the capping layer 113 are removed to release the second semiconductor layer 105, so that the central portion of the second semiconductor layer 105 (for example, the portion between the inner spacer 131 and the bottom of the groove 128) is suspended. After removing the first semiconductor layer 103 and the capping layer 113, the second semiconductor layer 105 forms a plurality of nanowires 110. In other words, the second semiconductor layer 105 may also be referred to as a nanowire 110 in subsequent processing.
[0056] Since the first semiconductor layer 103 and the capping layer 113 are both formed of a first semiconductor material (e.g., SiGe), a selective etching process such as dry etching or wet etching selective to the first semiconductor material may be performed to form the nanowires 110. The selective etching process for removing the first semiconductor material may also slightly etch the second semiconductor layer 105, which may cause the sidewalls of the second semiconductor layer 105 to be slightly etched on each side (e.g., Fig.17 The left and right sides in FIG. 1 are recessed by, for example, about 0.5 nm, thereby increasing the distance D between the nanowire 110 and the dielectric fin 116 (reference Fig.18 ), the details of which are described below.
[0057] Note that the central portion of the nanowire 110 is suspended, with empty spaces 134 between adjacent nanowires 110 and between the dielectric fins 116 and the nanowires 110. Other portions of the nanowire 110 (which may be referred to as ends), such as portions below the gate spacer 129 and portions outside the boundaries of the gate spacer 129, are not released by the above-described selective etching process. Instead, the nanowire 110 is surrounded by the inner spacer 131, as described below with reference to Fig.25 described.
[0058] Next, in Fig.18 In the embodiment of the present invention, the dielectric layer 117 (e.g., aluminum oxide) disposed along the sidewall of the dielectric layer 119 is removed by an etching process. For example, a wet etching process using a mixture of hydrogen peroxide (H2O2) and ammonia (NH3) may be performed to remove the dielectric layer 117. After the etching process, a portion of the dielectric layer 117 below the dielectric layer 119 remains, such as Fig.18 shown.
[0059] In addition, the dielectric layer 114 (eg, silicon nitride layer) disposed along the sidewall of the dielectric layer 115 is removed by an etching process. For example, a wet etching process using H3PO4 may be performed to remove the dielectric layer 114. Fig.18 As shown, after the etching process, a portion of the dielectric layer 114 beneath the dielectric layer 115 remains.
[0060] After removing the sidewall portions of dielectric layer 117 and the sidewall portions of dielectric layer 114, the thickness T1 of dielectric fin 116 is reduced (eg, Fig.18 , about 1 nm on the left side and about 1 nm on the right side). This increases the distance D between the dielectric fin 116 and the adjacent nanowire 110. The increased distance D is beneficial to the metal filling process, which forms the gate electrode 143 in subsequent processing (see Fig.21 ), which illustrates the advantages of the present disclosure. As feature sizes continue to shrink in advanced process nodes, the recesses 128 (refer to Fig.13 ) becomes increasingly smaller, making it difficult to fill the groove 128 with a conductive material to form the gate electrode 143. Poorly filled grooves 128 may reduce yield and / or increase the resistance of the formed metal gate. By increasing the distance D, the present invention makes it easier to fill the groove 128, thereby improving yield and reducing the resistance of the formed metal gate. In addition, since the increased distance D allows for easy filling of the filling metal, a smaller spacing S (e.g., between about 20 nm and about 40 nm) between adjacent semiconductor strips 106 is made possible by the present invention, which advantageously reduces the size of the formed device (e.g., cell height) and increases the integration density of the device.
[0061] Next, in Fig.19 In the embodiment of the present invention, an optional hybrid fin trimming process is performed to further reduce the width of the hybrid fin 112 (e.g., the width T1 of the dielectric fin 116, which may be the same as the width of the dielectric structure 118), and further increase the distance D. The hybrid fin trimming process may be any suitable etching process, such as dry etching or wet etching. In some embodiments, the hybrid fin trimming process is omitted.
[0062] Next reference Fig. 20 , an interface layer 142 is formed over the surface of the nanowire 110. The interface layer 142 is a dielectric layer, such as an oxide, and can be formed by a thermal oxidation process or a deposition process. In the illustrated embodiment, a thermal oxidation process is performed to convert the outer portion of the nanowire 110 into an oxide to form the interface layer 142, and as a result, the interface layer 142 is not formed over the dielectric fin 116 or the dielectric structure 118.
[0063] After forming the interface layer 142, a gate dielectric layer 141 is formed around the nanowires 110, on the dielectric fins 116, on the dielectric structure 118, and on the patterned hard mask 107. The gate dielectric layer 141 is also formed on the upper surface of the STI region 111, as shown in FIG. Fig. 20In some embodiments, the gate dielectric layer 141 includes a high-k dielectric material (e.g., having a K value greater than about 7.0), and may include a metal oxide, or a silicate of Hf, Al, Zr, La, Mg, Ba, Ti, Pb, or a combination thereof. For example, the gate dielectric layer 141 may include HfO2, ZrO2, HfAlO x 、HfSiO x , Al2O3, or a combination thereof. The gate dielectric layer 141 may be formed by molecular beam deposition (MBD), ALD, PECVD, or the like.
[0064] exist Fig. 20 In the example of FIG. 1 , the portion of the gate dielectric layer 141 formed around the nanowire 110 merges with the adjacent gate dielectric layer 141. As a result, the gate dielectric layer 141 completely fills the gap between the vertically adjacent nanowires 110, and fills the gap between the topmost nanowire 110 and the corresponding overlying patterned hard mask 107. In addition, the gate dielectric layer 141 completely fills the gap between the bottommost nanowire 110 and the underlying semiconductor strip 106, as shown in FIG. Fig. 20 In some embodiments, the merged gate dielectric layer 141 can prevent the gate electrode 143 (see FIG. Fig. 22 In other embodiments, the portion of the gate dielectric layer 141 surrounding the nanowires 110 is not merged, and thus, the gap between, for example, vertically adjacent nanowires 110 is filled by a subsequently formed gate electrode, such as Fig.28 As shown in the embodiments.
[0065] Next, in Fig.21 In the embodiment of the present invention, a conductive material (also referred to as a filling metal) is formed in the groove 128 to form a gate electrode 143. The gate electrode 143 may be made of a metal-containing material such as Cu, Al, W, or the like, a combination thereof, or a multilayer thereof, and may be formed by, for example, electroplating, electroless plating, or other suitable methods. After the gate electrode 143 is formed, a planarization process such as CMP may be performed to planarize the upper surface of the gate electrode 143.
[0066] Although not shown, a barrier layer and a work function layer may be formed over the gate dielectric layer 141 and around the nanowires 110 before forming the conductive material. The barrier layer may include a conductive material, such as titanium nitride, but other materials, such as tantalum nitride, titanium, tantalum, etc., may be used alternatively. The barrier layer may be formed using a CVD process such as PECVD. However, other alternative processes, such as sputtering, metal organic chemical vapor deposition (MOCVD), or ALD may be used alternatively. In some embodiments, after forming the barrier layer, a work function layer is formed on the barrier layer.
[0067] exist Fig.21 In the example of , the GAA FET device has an N-type device region 510 and a P-type device region 520. Therefore, an N-type work function layer can be formed above the barrier layer in the N-type device region 510 and around the nanowire 110, and a P-type work function layer can be formed above the barrier layer in the P-type device region 520 and around the nanowire 110. Exemplary P-type work function metals included in the gate structure for P-type devices may include TiN, TaN, Ru, Mo, Al, WN, ZrSi2, MoSi2, TaSi2, NiSi2, WN, other suitable P-type work function materials, or combinations thereof. Exemplary N-type work function metals included in the gate structure for N-type devices may include Ti, Ag, TaAl, TaAlC, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, other suitable N-type work function materials, or combinations thereof. The work function value is associated with the material composition of the work function layer, and therefore, the material of the work function layer can be selected to adjust its work function value to achieve a target threshold voltage Vt in the device to be formed. The work function layer(s) can be deposited by CVD, physical vapor deposition (PVD), and / or other suitable processes.
[0068] In order to form different work function layers in the N-type device region 510 and the P-type device region 520, a patterned mask layer, such as a patterned photoresist, can be formed to cover the first region (e.g., 510) while forming a work function layer in the second region (e.g., 520) exposed by the patterned mask layer. Next, a fill metal can be formed on the work function layer in the second region (e.g., 520) to form a gate electrode 143P (e.g., a portion of the gate electrode 143 in region 520). A similar process can be repeated to cover the second region (e.g., 520) while forming a work function layer in the first region (e.g., 510), and a fill metal can be formed on the work function layer in the first region to form a gate electrode 143N (e.g., a portion of the gate electrode 143 in region 510). In Fig.21 In the example of FIG. 1 , there is an interface 144 between the gate electrodes 143N and 143P, wherein the barrier layer and the work function layer may extend along the interface 144. For example, the N-type work function layer may extend along the left side of the interface 144, and the P-type work function layer may extend along the right side of the interface 144. In other embodiments, after forming the N-type work function layer and the P-type work function layer, a fill metal may be formed in both the N-type device region 510 and the P-type device region 520 in a single step, in which case the interface 144 may not be formed.
[0069] Next, in Fig. 22In the embodiment, the gate electrode 143 is recessed below the upper surface of the dielectric structure 118 (e.g., the upper surface of the dielectric layer 119). An etching process that is selective to the material (e.g., metal) of the gate electrode 143 may be performed to remove the top layer of the gate electrode 143 without substantially corroding the dielectric layer 119. Fig. 22 In the example of , after the gate electrode 143 is recessed, the dielectric structure 118 separates the gate electrode 143 into three separate parts, so that three separate gate structures 145 (e.g., 145A, 145B, and 145C) are formed in a self-aligned manner, wherein each gate structure 145 includes a gate dielectric layer 141, a barrier layer, at least one work function layer, and a gate electrode 143. Fig. 22 In the example of , gate structure 145A is formed in N-type device region 510 and has an N-type work function layer. Gate structure 145C is formed in P-type device region 520 and has a P-type work function layer. However, gate structure 145B has its left portion (e.g., the left side of interface 144) in N-type device region 510 and its right portion (e.g., the right side of interface 144) in P-type device region 520, and therefore, the work function layer of gate structure 145B includes a left portion formed by an N-type work function layer and a right portion formed by a P-type work function layer.
[0070] The self-aligned metal gate formation method disclosed herein provides advantages over the reference cut metal gate (CMG) process, in which the gate electrode 143 is cut into separate metal gates by forming an opening in the gate electrode 143 and filling the opening with a dielectric material. For advanced process nodes, the reference CMG process may have difficulty filling the openings due to the high aspect ratio of the openings. Poorly filled openings may cause electrical shorts between gate structures and may cause device failure. The present invention allows easy separation of metal gates in a self-aligned manner, thereby preventing device failure and improving yield.
[0071] After forming the gate structure 145, an etch stop layer 147 is formed (e.g., selectively formed) over the gate electrode 143. In some embodiments, the etch stop layer 147 is a fluorine-free tungsten (FFW) layer. The etch stop layer 147 (e.g., tungsten) can be used as an etch stop layer in a subsequent etching process, and further, can help reduce the resistance of the gate structure 145 and / or gate contact plug formed thereafter. After forming the etch stop layer 147, a dielectric layer 149 is formed over the etch stop layer 147. In some embodiments, a planarization process is performed to planarize the upper surface of the dielectric layer 149.
[0072] exist Fig. 22In the example of FIG. 1 , a height H3 of the dielectric layer 119 of the dielectric structure 118 is between about 10 nm and about 40 nm, and the dielectric layer 119 extends a distance H4 above the upper surface of the etch stop layer 147, which is greater than about 4 nm. The range of the distance H4 ensures a sufficiently large safety margin to avoid electrical shorts between adjacent gate structures 145, which may occur if the upper surface of the dielectric layer 119 is lower than the upper surface of the gate electrode 143.
[0073] Fig.23 Shown in Fig. 22 FIG. 1 is a perspective view of a GAA FET device 100 after processing. Fig.23 In the embodiment, the patterned hard mask 107 has a U-shaped cross section, which is due to the anisotropic etching. Fig.16 The patterned hard mask 107 discussed above is recessed to form the anisotropic etching. The anisotropic etching also removes the top portion of the gate spacer 129 and causes the height of the gate spacer 129 to be reduced, as shown in FIG. Fig.23 As shown. Since the interface layer 142 surrounds the nanowire 110, Fig.23 The position of the interface layer 142 in FIG. 1 corresponds to the position of the nanowire 110 (as shown by reference numeral 142 / 110 ). Fig.23 Also shown is an inner spacer 131 disposed below the gate spacer 129. The source / drain regions 133 are connected to opposite ends of the nanowire 110, such as Fig.23 shown.
[0074] Fig.24 Shows Fig. 22 and Fig.23 1 is a plan view of a GAA FET device 100. For clarity, not all features are shown. Fig.24 The semiconductor strip 106, the gate electrode 143, and the gate spacer 129 are shown. Cross section BB (also see Fig.13 ) is along the longitudinal direction of the gate electrode 143 and passes through the gate electrode 143. The cross section AA (also refer to Fig.10 ) is parallel to cross section BB, but passes through gate spacer 129. Cross section CC (also refer to Fig.13 ) is parallel to cross section BB, but between two adjacent gate structures and passes through source / drain region 133 ( Fig.24 not shown).
[0075] Fig.25 Shows Fig. 22 and Fig.23 A cross-sectional view of the GAA FET device 100 along the cross-section AA. Note that Fig.25In the cross-sectional view of FIG. 1 , the inner spacer 131 surrounds the portion of the nanowire 110 disposed below (eg, directly below) the gate spacer 129. In contrast, in FIG. Fig. 22 , the gate dielectric layer 141 and the interfacial layer 142 surround the portion of the nanowire 110 below the gate electrode 143 (eg, between a pair of gate spacers 129). The gate electrode 143 also at least partially surrounds the nanowire 110. In addition, Fig.28 In the embodiment of FIG. 1 , the gate electrode 143 completely surrounds (eg, in a full circle) the nanowire 110 .
[0076] Fig.26 After forming the source / drain contacts 151, Fig. 22 and Fig.23 A cross section of the GAA FET device 100 along the cross section CC after processing of . The source / drain contacts 151 may be formed by forming openings in the ILD layer 137 to expose the underlying source / drain regions 133, forming silicide regions 153 over the source / drain regions 133, and filling the openings with a conductive material (e.g., Cu, W, Co, Al).
[0077] An opening for the source / drain contact 151 may be formed by performing a photolithography and etching process to etch through the CESL 135, thereby exposing the source / drain region 133. Over the exposed portion of the source / drain region 133, the silicide region 153 may be formed by first depositing a metal that can react with a semiconductor material (e.g., silicon, germanium) to form a silicide region or a germanide region, such as nickel, cobalt, titanium, tantalum, platinum, tungsten, other precious metals, other refractory metals, rare earth metals, or alloys thereof, and then performing a thermal annealing process to form the silicide region 153. Unreacted portions of the deposited metal are then removed, for example, by an etching process. Next, a barrier layer may be formed lining the sidewalls and bottom of the opening in the ILD layer 137, and then a fill metal may be formed to fill the opening. Fig.26 After the processing, additional processing may be performed to complete the GAA FET device 100, as will be readily appreciated by those skilled in the art, and therefore the details will not be discussed herein.
[0078] Note that Fig.26 , the width of the dielectric fin 116 beyond the boundary of the gate structure 145 (e.g., directly below the source / drain region 133) is T2, which is greater than the width T1 of the dielectric fin 116 below (e.g., directly below) the gate electrode 143 (refer to Fig.18 and Fig.19 ). In some embodiments, the difference between T2 and T1 is between about 2 nm and about 20 nm.
[0079] The larger width T2 of the dielectric fin 116 below the source / drain region 133 allows for a larger error tolerance (or less stringent requirements) regarding the lithography and etching processes. For example, if the source / drain contact 151 is shifted (e.g., to the left or to the right) due to inaccuracies in the lithography and etching processes used to form the contact openings, then the source / drain region 133 (e.g., Fig.26 The larger width T2 of the dielectric fin 116 can allow for a large amount of shifting before an electrical short occurs between the source / drain regions 133A and 133B (e.g., in the top surface of the dielectric fin 116). As another example, consider the doping (e.g., implantation process) of the source / drain regions 133 in different regions (e.g., N-type device region 510 and P-type device region 520) for transistors of different types (e.g., N-type, or P-type), where a patterned mask can be used to cover the source / drain regions 133 in one region (e.g., 510) while exposing another region (e.g., 520) for doping. The larger width T2 allows for a larger error tolerance about the boundary of the mask layer, which can be on the top surface of the dielectric fin 116. In addition, the larger width T2 of the dielectric fin 116 reduces or prevents bridging of adjacent source / drain regions (e.g., bridging between source / drain regions 133A and 133B). In addition, the larger width T2 of the dielectric fin 116 improves the time-dependent dielectric breakdown (TDDB) performance of the formed device (e.g., from the source / drain contact 151A to the source / drain region 133B, or from the source / drain contact 151B to the source / drain region 133A). On the other hand, the smaller width T1 of the dielectric fin 116 under the gate electrode 143 (refer to Fig.18 and Fig.19 ) allows the groove 128 to be easily filled with a filling metal, thereby improving the yield and reducing the resistance of the formed gate structure.
[0080] Modifications or variations to the disclosed embodiments are possible and are fully intended to be included within the scope of this disclosure. Fig. 27 and Fig.28 Some examples are shown in . Fig. 27 is a cross-sectional view of a GAA FET device 100A according to another embodiment. The GAA FET device 100A is similar to Fig. 22 The GAA FET device 100 in FIG. 1 is shown in FIG. 1 , but the patterned hard mask 107 is completely removed (see, for example, Fig. 22 ).
[0081] Fig.28 FIG. 1 is a cross-sectional view of a GAA FET device 100B according to another embodiment. The GAA FET device 100B is similar to Fig. 27100A, but the gate dielectric layer 141 around the vertically adjacent nanowires 110 is not merged. Instead, the gaps between the vertically adjacent nanowires 110 are filled by the filling metal of the gate electrode 143. Similarly, the filling metal of the gate electrode 143 fills the gap between the bottommost nanowire 110 and the semiconductor strip 106.
[0082] Fig.29 is a flow chart of a method for forming a GAA FET device according to some embodiments. It should be understood that Fig.29 The embodiment methods shown in are merely examples of many possible embodiment methods. Those skilled in the art will recognize many variations, substitutions, and modifications. For example, the following may be added, removed, replaced, rearranged, and repeated. Fig.29 The various steps shown.
[0083] refer to Fig.29 In step 1010, semiconductor fins are formed over a substrate, and a patterned mask layer is formed over the semiconductor fins, wherein the semiconductor fins include an epitaxial layer over the semiconductor strips, wherein the epitaxial layer includes alternating layers of a first semiconductor material and a second semiconductor material. In step 1020, hybrid fins are formed over isolation regions on opposite sides of the semiconductor fins, wherein each hybrid fin includes a dielectric fin and a dielectric structure over the dielectric fin. In step 1030, a gate structure is formed over the semiconductor fins and over the hybrid fins. In step 1040, a first portion of the patterned mask layer, a first portion of the epitaxial layer, and a first portion of the dielectric structure disposed outside the sidewalls of the gate structure are removed, but the dielectric fins are substantially not removed. In step 1050, an interlayer dielectric (ILD) layer is formed over the dielectric fins and around the gate structure. In step 1060, a gate electrode of the gate structure is removed to form an opening in the gate structure, the opening exposing a second portion of the patterned mask layer and a second portion of the dielectric structure disposed under the gate structure. At step 1070, a first dielectric structure of the dielectric structure is removed while a second dielectric structure of the dielectric structure remains. At step 1080, the first semiconductor material is selectively removed, wherein after the selective removal, the second semiconductor material forms a nanowire, wherein the second dielectric structure extends further from the substrate than an uppermost surface of the nanowire.
[0084] Embodiments can achieve advantages. For example, the dielectric fin 116 has a larger width T2 below the source / drain region 133 and a smaller width T1 below the gate electrode 143. The larger width T2 provides a higher error tolerance for the lithography and etching processes used to form the contact openings, and helps to reduce the electrical short circuit between adjacent source / drain regions 133. The smaller width T1 makes it easier for the fill metal to fill the grooves between the gate spacers 129 used to form the gate electrode 143, thereby improving the yield and reducing the resistance of the gate electrode. In addition, the dielectric fin 116 improves the time-varying dielectric breakdown (TDDB) performance of the formed device. In addition, the separation of different metal gates (e.g., 145A, 145B, 145C) is achieved by self-aligning the dielectric structure 118. Although the present invention is discussed in the context of GAA FET devices (e.g., nanowire devices), the principles of the present invention can be applied to other types of devices, such as nanosheet devices or Fin field effect (FinFET) devices.
[0085] According to one embodiment, a method of forming a semiconductor device includes: forming a semiconductor fin over a substrate, and forming a patterned mask layer over the semiconductor fin, wherein the semiconductor fin includes an epitaxial layer over a semiconductor strip, wherein the epitaxial layer includes alternating layers of a first semiconductor material and a second semiconductor material; forming hybrid fins over isolation regions on opposite sides of the semiconductor fins, wherein each hybrid fin includes a dielectric fin and a dielectric structure over the dielectric fin; forming a gate structure over the semiconductor fin and over the hybrid fin; removing a first portion of the patterned mask layer, a first portion of the epitaxial layer, and a second portion of the gate structure; and removing a first portion of the patterned mask layer, a first portion of the epitaxial layer, and a second portion of the gate structure. The method further comprises: removing the first semiconductor material from the substrate and the second dielectric structure from the substrate, removing the first semiconductor material from the substrate and the second dielectric structure from the substrate, and removing the first semiconductor material from the substrate and the second dielectric structure from the substrate, but substantially not removing the dielectric fin; forming an interlayer dielectric (ILD) layer over the dielectric fin and around the gate structure; removing the gate electrode of the gate structure to form an opening in the gate structure, the opening exposing a second portion of the patterned mask layer and a second portion of the dielectric structure disposed below the gate structure; removing the first dielectric structure of the dielectric structure while retaining the second dielectric structure of the dielectric structure; selectively removing the first semiconductor material, wherein after the selective removal, the second semiconductor material forms a nanowire, wherein the second dielectric structure extends further from the substrate than the uppermost surface of the nanowire. In one embodiment, the method further comprises: filling the opening with a conductive material; recessing the upper surface of the conductive material below the upper surface of the second dielectric structure. In one embodiment, the method further comprises: forming a gate dielectric material around the nanowire before filling the opening. In one embodiment, the method further comprises: removing at least the upper layer of the second portion of the patterned mask layer exposed by the opening before filling the opening. In one embodiment, the method further comprises: after selectively removing the first semiconductor material and before filling the opening, reducing a first width of a first portion of the dielectric fin disposed below the gate structure while maintaining a second width of a second portion of the dielectric fin disposed outside the sidewall of the gate structure. In one embodiment, the method further comprises: after the recessing, forming a tungsten layer on the conductive material. In one embodiment, removing the first portion of the patterned mask layer, the first portion of the epitaxial layer, and the first portion of the dielectric structure comprises: performing anisotropic etching using the gate structure as an etching mask. In one embodiment, the method further comprises: before forming the hybrid fin, forming a capping layer comprising the first semiconductor material along the sidewall of the epitaxial layer and along the sidewall of the patterned mask layer, wherein the hybrid fin is formed to contact the capping layer. In one embodiment, the dielectric fin is formed by one or more dielectric materials having a first dielectric constant, and the dielectric structure is formed by one or more dielectric materials having a second dielectric constant greater than the first dielectric constant.In one embodiment, the method further includes: forming a source / drain region above the semiconductor strip after removing the first portion of the patterned mask layer, the first portion of the epitaxial layer, and the first portion of the dielectric structure, and before forming the ILD layer. In one embodiment, the method further includes: replacing the first semiconductor material disposed under the gate spacer of the gate structure with the first dielectric material after removing the first portion of the patterned mask layer, the first portion of the epitaxial layer, and the first portion of the dielectric structure, and before forming the source / drain region. In one embodiment, the replacing includes: performing a lateral etching process to remove the first semiconductor material disposed under the gate spacer; filling a space left by removing the first semiconductor material with the first dielectric material.
[0086] According to one embodiment, a method for forming a semiconductor device includes: forming a protruding semiconductor strip over a substrate; forming an isolation region between adjacent semiconductor strips; forming a hybrid fin on the isolation region, the hybrid fin including a dielectric fin and a dielectric structure over the dielectric fin; forming a dummy gate structure over the semiconductor strip and the hybrid fin; forming a source / drain region over the semiconductor strip and on opposite sides of the dummy gate structure; forming a nanowire under the dummy gate structure, wherein the nanowire is over and aligned with a corresponding semiconductor strip, and the source / drain region is at opposite ends of the nanowire, wherein the hybrid fin extends farther from the substrate than the nanowire; after forming the nanowire, reducing the width of a central portion of the hybrid fin while maintaining the width of an end portion of the hybrid fin unchanged, wherein the central portion of the hybrid fin is under the dummy gate structure, and the end portion of the hybrid fin is outside the boundary of the dummy gate structure; and forming a conductive material around the nanowire. In one embodiment, forming a nanowire includes: forming alternating layers of a first semiconductor material and a second semiconductor material over the semiconductor strip before forming a dummy gate structure; removing the first semiconductor material and the second semiconductor material disposed outside the boundary of the dummy gate structure after forming the dummy gate structure; forming an interlayer dielectric layer over the source / drain region and around the dummy gate structure; removing the gate electrode of the dummy gate structure after forming the interlayer dielectric layer to form an opening in the dummy gate structure, the opening exposing the first semiconductor material disposed below the dummy gate structure; and selectively removing the first semiconductor material disposed below the dummy gate structure. In one embodiment, forming a nanowire also includes: forming a capping layer between the hybrid fin and the alternating layers of the first semiconductor material and the second semiconductor material before forming the dummy gate structure, using the first semiconductor material to form the capping layer. In one embodiment, the method also includes: recessing the first semiconductor material from the sidewalls of the remaining portion of the second semiconductor material after removing the first semiconductor material and the second semiconductor material disposed outside the boundary of the dummy gate structure; and filling the space left by the recessing of the first semiconductor material with a dielectric material. In one embodiment, the method also includes: recessing the upper surface of the conductive material below the upper surface of the dielectric structure. In one embodiment, the method further comprises: before forming the conductive material, forming a gate dielectric material around the nanowires.
[0087] According to one embodiment, a semiconductor device includes: a semiconductor strip protruding above a substrate; a first isolation region and a second isolation region, the first isolation region and the second isolation region being located on opposite sides of the semiconductor strip; a nanowire, the nanowire being located above and aligned with the semiconductor strip; a source / drain region, the source / drain region being located at opposite ends of the nanowire; a first dielectric fin, the first dielectric fin being located on the first isolation region; and a metal gate, the metal gate being located around the nanowire and around a central portion of the first dielectric fin, wherein an end of the first dielectric fin is disposed on opposite sides of the metal gate, wherein the end of the first dielectric fin is wider than the central portion of the first dielectric fin. In one embodiment, the semiconductor device also includes a first dielectric structure, the first dielectric structure being located above the first dielectric fin, wherein the first dielectric structure extends above an upper surface of the metal gate away from the substrate.
[0088] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the present disclosure. Those skilled in the art should understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures for performing the same or similar purposes and / or achieving the same or similar advantages as the present disclosure. Those skilled in the art should also be aware that such equivalent structures do not depart from the spirit and scope of the present disclosure, and various changes, substitutions and modifications can be made without departing from the spirit and scope of the present disclosure.
Claims
1. A method for forming a semiconductor device, the method comprising: forming a semiconductor fin over a substrate and forming a patterned mask layer over the semiconductor fin, wherein the semiconductor fin comprises an epitaxial layer over the semiconductor strip, wherein the epitaxial layer comprises alternating layers of a first semiconductor material and a second semiconductor material; forming hybrid fins over the isolation regions on opposite sides of the semiconductor fins, wherein each of the hybrid fins includes a dielectric fin and a dielectric structure over the dielectric fin; forming a gate structure over the semiconductor fin and over the hybrid fin; removing a first portion of the patterned mask layer, a first portion of the epitaxial layer, and a first portion of the dielectric structure disposed outside of a sidewall of the gate structure, but not removing the dielectric fin; forming an interlayer dielectric layer over the dielectric fin and around the gate structure; removing a gate electrode of the gate structure to form an opening in the gate structure, the opening exposing a second portion of the patterned mask layer and a second portion of the dielectric structure disposed below the gate structure; removing a first dielectric structure of the dielectric structure that is not blocked in the opening, while retaining a second dielectric structure of the dielectric structure that is blocked in the opening; and The first semiconductor material is selectively removed, wherein after the selective removal, the second semiconductor material forms a nanowire, wherein the second dielectric structure extends further from the substrate than an uppermost surface of the nanowire.
2. The method according to claim 1, further comprising: filling the opening with a conductive material; as well as An upper surface of the conductive material is recessed below an upper surface of the second dielectric structure.
3. The method according to claim 2, further comprising: Prior to filling the openings, a gate dielectric material is formed around the nanowires.
4. The method according to claim 2, further comprising: Prior to filling the opening, at least an upper layer of the second portion of the patterned mask layer exposed through the opening is removed.
5. The method according to claim 2, further comprising: After selectively removing the first semiconductor material and before filling the opening, a first width of a first portion of the dielectric fin disposed under the gate structure is reduced while maintaining a second width of a second portion of the dielectric fin disposed outside a sidewall of the gate structure.
6. The method according to claim 2, further comprising: After the recessing, a tungsten layer is formed on the conductive material.
7. The method according to claim 1, wherein: Removing the first portion of the patterned mask layer, the first portion of the epitaxial layer, and the first portion of the dielectric structure includes performing an anisotropic etch using the gate structure as an etch mask.
8. The method according to claim 1, further comprising: Before forming the hybrid fin, a capping layer including the first semiconductor material is formed along sidewalls of the epitaxial layer and along sidewalls of the patterned mask layer, wherein the hybrid fin is formed to contact the capping layer.
9. The method according to claim 1, wherein: The dielectric fins are formed of one or more dielectric materials having a first dielectric constant, and the dielectric structure is formed of one or more dielectric materials having a second dielectric constant greater than the first dielectric constant.
10. The method according to claim 1, further comprising: After removing the first portion of the patterned mask layer, the first portion of the epitaxial layer, and the first portion of the dielectric structure, and before forming the interlayer dielectric layer, source / drain regions are formed over the semiconductor strips.
11. The method according to claim 10, further comprising: After removing the first portion of the patterned mask layer, the first portion of the epitaxial layer, and the first portion of the dielectric structure, and before forming the source / drain regions, the first semiconductor material disposed under the gate spacer of the gate structure is replaced with a first dielectric material.
12. The method according to claim 11, wherein: The replacement includes: performing a lateral etching process to remove the first semiconductor material disposed under the gate spacer; and The space left by removing the first semiconductor material is filled with the first dielectric material.
13. A method of forming a semiconductor device, the method comprising: forming a protruding semiconductor strip above the substrate; forming an isolation region between adjacent semiconductor strips; forming a hybrid fin on the isolation region, the hybrid fin comprising a dielectric fin and a dielectric structure above the dielectric fin; forming a dummy gate structure over the semiconductor strips and the hybrid fins; forming source / drain regions over the semiconductor strips and on opposite sides of the dummy gate structure; forming a nanowire below the dummy gate structure, wherein the nanowire is located above and aligned with a corresponding semiconductor strip, and the source / drain regions are located at opposite ends of the nanowire, wherein the hybrid fin extends further from the substrate than the nanowire; After forming the nanowire, reducing a width of a central portion of the hybrid fin while maintaining a width of an end portion of the hybrid fin, wherein the central portion of the hybrid fin is located below the dummy gate structure and the end portion of the hybrid fin is located outside a boundary of the dummy gate structure; and A conductive material is formed around the nanowires.
14. The method according to claim 13, wherein: Forming the nanowires comprises: Prior to forming the dummy gate structure, forming alternating layers of a first semiconductor material and a second semiconductor material over the semiconductor strip; After forming the dummy gate structure, removing the first semiconductor material and the second semiconductor material disposed outside a boundary of the dummy gate structure; forming an interlayer dielectric layer above the source / drain region and around the dummy gate structure; After forming the interlayer dielectric layer, removing the gate electrode of the dummy gate structure to form an opening in the dummy gate structure, wherein the opening exposes the first semiconductor material disposed under the dummy gate structure; and The first semiconductor material disposed under the dummy gate structure is selectively removed.
15. The method according to claim 14, wherein: Forming the nanowires further comprises: Before forming the dummy gate structure, a capping layer is formed between the hybrid fin and the alternating layers of the first semiconductor material and the second semiconductor material, and the capping layer is formed using the first semiconductor material.
16. The method according to claim 15, further comprising: After removing the first semiconductor material and the second semiconductor material disposed outside the boundary of the dummy gate structure, recessing the first semiconductor material from the sidewalls of the remaining portion of the second semiconductor material; as well as The space left by the recess of the first semiconductor material is filled with a dielectric material.
17. The method according to claim 13, further comprising: An upper surface of the conductive material is recessed below an upper surface of the dielectric structure.
18. The method according to claim 13, further comprising: Prior to forming the conductive material, a gate dielectric material is formed around the nanowires.
19. A semiconductor device comprising: a semiconductor strip protruding above the substrate; a first isolation region and a second isolation region, the first isolation region and the second isolation region being located on opposite sides of the semiconductor strip; a nanowire located above and aligned with the semiconductor strip; source / drain regions located at opposite ends of the nanowire; a first dielectric fin, the first dielectric fin being located on the first isolation region; as well as A metal gate is positioned around the nanowire and around a central portion of the first dielectric fin, wherein ends of the first dielectric fin are disposed on opposite sides of the metal gate, wherein the ends of the first dielectric fin are wider than the central portion of the first dielectric fin.
20. The semiconductor device according to claim 19, further comprising a first dielectric structure located above the first dielectric fin, wherein The first dielectric structure extends over an upper surface of the metal gate away from the substrate.