Method for uniformly curling and unfolding polymer stent structures
By using a crimping device and polymer material resetting technology on the polymer stent structure, the problem of curling and expansion of the polymer stent structure in the balloon catheter is solved, improving the structural integrity and expansion uniformity, and avoiding Balloon overstretch and pinhole leakage.
Patent Information
- Application Number
- CN201980038742.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-06-05
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2039-06-05
AI Technical Summary
When crimping the polymer stent structure to the balloon catheter, it is difficult to ensure structural integrity, safe delivery and uniform expansion, and can easily lead to overstretching of the balloon and pinhole leakage.
Using a crimping device and a crimping barrier or protective sheet, the polymer material is placed between the surface of the stent structure and the crimping blades. Through intermittent crimping and resetting of the polymer material, the diameter of the stent structure is adjusted, and the diameter of the stent structure is adjusted during crimping. The balloon pressure is controlled during the process to ensure the distribution of small wrinkles and avoid the formation of large wrinkles.
It improves the retention force and expansion uniformity of the stent structure on the balloon, reduces the risk of structural damage and shortened fatigue life, and avoids excessive balloon strain and pinhole leakage.
Smart Images

Figure CN112512463B_ABST
Abstract
Description
[0001] Field of the Invention
[0002] The present invention relates to medical devices; more particularly, the present invention relates to methods for uniformly crimping and deploying a medical device (eg, a polymeric scaffold) onto and from a delivery balloon, respectively.
[0003] Description of the Prior Art
[0004] Radially expandable endoprostheses are artificial devices suitable for implantation in anatomical cavities. "Anatomical cavities" refer to cavities or ducts of tubular organs such as blood vessels, urethra, and bile ducts. Stents are examples of usually cylindrical endoprostheses whose function is to keep open anatomical cavities and sometimes expand segments of anatomical cavities. Stents are commonly used to treat atherosclerotic stenosis of blood vessels. "Stenosis" refers to the narrowing or reduction of the diameter of a body passage or orifice. In such treatments, stents reinforce the vessel walls and prevent restenosis of angioplasty in the vascular system. "Restenosis" refers to a significant recurrence of stenosis that occurs in a blood vessel or heart valve after treatment (such as by balloon angioplasty, stenting, or valvuloplasty).
[0005] Treatment of a diseased area or lesion with a stent involves delivery and deployment of the stent. "Delivery" refers to the introduction and transport of the stent through an anatomical cavity to a desired treatment site, such as a lesion. "Deployment" corresponds to expanding the stent within the lumen at the treatment area. Delivery and deployment of a stent is accomplished by positioning the stent around one end of a catheter, inserting the end of the catheter through the skin into the anatomical cavity, advancing the catheter within the anatomical cavity to the desired treatment site, expanding the stent at the treatment site, and removing the catheter from the lumen.
[0006] The stent must be able to meet a number of basic functional requirements. When the stent (or stent structure) supports the vessel wall, the stent (or stent structure) must be able to withstand radial compressive forces. Therefore, the stent must have sufficient radial strength. After deployment, the stent must adequately maintain its size and shape during its service life, despite the various forces it may be subjected to. In particular, the stent must be sufficient to maintain the vessel at a specified diameter for a desired treatment time despite these forces. The treatment time may correspond to the time required for the vessel wall to be remodeled, after which the stent is no longer needed.
[0007] The stent structure can be made of biodegradable, bioabsorbable, bioresorbable or bioerodible polymers. The term biodegradable, bioabsorbable, bioresorbable, biodissolvable or bioerodible refers to the property that the material or stent degrades, absorbs, resorbs or is eroded and leaves the implantation site. The stent structure can also be made of bioerodible metals and alloys. In contrast to durable metal stents, the stent structure is intended to remain in the body only for a limited period of time. In many therapeutic applications, the presence of the stent in the body may require a limited period of time until its intended function, such as maintaining vascular patency and / or drug delivery is completed. In addition, it has been shown that compared with metal stents, biodegradable stent structures improve the healing of anatomical cavities, which may lead to a reduced incidence of late thrombosis. In these cases, it is desirable to use a polymer stent structure, particularly a bioabsorbable or bioresorbable polymer stent structure relative to a metal stent to treat the blood vessel so that the presence of the prosthesis in the blood vessel is temporary.
[0008] Polymer materials that may be considered for use as polymer stent structures, such as poly(L-lactide) ("PLLA"), poly(D-lactide) ("PDLA"), poly(D,L-lactide-co-glycolide), poly(D-lactide-co-glycolide) or poly(L-lactide-co-D-lactide) having less than 10% D-lactide, poly(L-lactide-co-caprolactone), poly(caprolactone), PLLD / PDLA stereocomplexes, and blends of the foregoing polymers may be described in some of the following ways by comparison to metallic materials used to form stents. Polymeric materials generally have a lower strength to volume ratio than metals, meaning that more material is required to provide equivalent mechanical properties. As a result, the struts must become thicker and wider in order for the stent to have the required strength to support the lumen wall at the required radius. Stent structures made from such polymers are also prone to brittleness or limited fracture toughness. The inherent anisotropy and rate-dependent inelastic properties of the material (i.e., the change in strength / stiffness of the material depends on the rate at which the material deforms, in addition to the material's inherent temperature, hydration level, thermal history) only add to this complexity when using polymers, especially bioresorbable polymers such as PLLA or PLGA.
[0009] Stent structures and stents are traditionally classified into two broad categories: balloon-expandable stents and self-expanding stents. The latter type expands (at least partially) within a vessel to a deployed or expanded state when radial constraints are removed, whereas the former rely on externally applied forces to configure them from a crimped or collapsed state to a deployed or expanded state.
[0010] Self-expanding stents are designed to expand significantly when radial constraints are removed, so that a balloon is generally not required to deploy the stent. Self-expanding stents do not experience or are relatively free of plastic or inelastic deformation when they are stowed in a sheath or expanded within a lumen (with or without an auxiliary balloon). In contrast, a balloon-expandable stent or stent structure will experience significant plastic or inelastic deformation when it is crimped and later deployed by a balloon.
[0011] In the case of a balloon expandable stent, the stent is mounted around the balloon portion of a balloon catheter. The stent is compressed or crimped onto the balloon. The crimping may be accomplished using an iris or sliding wedge or other form of crimper. When a balloon expandable stent or stent structure is crimped and later deployed by a balloon, a great deal of plastic or inelastic deformation occurs. At the treatment site within the cavity, the stent is expanded by inflating the balloon. The expanded state is achieved and maintained substantially, if not entirely, by irreversible or inelastic strain at the crown of the stent structure or stent caused by balloon expansion. In contrast, a self-expanding stent or stent structure achieves and maintains its expanded state in the vessel by elastic radially outward forces.
[0012] The stent has been crimped to the balloon using a film-headed crimper. Referring to FIG. 1A , a perspective view of a crimping assembly 20 is shown, which includes three rollers 123, 124, 125 for disposing a clean sheet of non-stick material between the crimping blades and the stent prior to crimping. For example, the upper roller 125 secures the sheet to a backing sheet. The sheet is withdrawn from the backing sheet by a rotating mechanism (not shown) within the crimping head 21. A second sheet is dispensed by the middle roller 124. After crimping, the first and second (used) sheets are collected by the lower roller 123. As an alternative to the rollers dispensing the non-stick sheet, the stent may be covered with a thin, flexible protective sheath prior to crimping.
[0013] 1B shows the positioning of the first sheet 125a and the second sheet 124a within the aperture of the crimping assembly 20 relative to the wedge 22 and the bracket 100. As shown, each of the two sheets passes between two blades 22 on opposite sides of the bracket 100, and as the iris of the crimping assembly is reduced in size by the converging blades 22, tensions T1 and T2 are applied to collect excess sheet material.
[0014] The dispensed sheet of non-stick material is used to avoid buildup of coating material on the crimper blades when the stent is coated with a therapeutic agent. After each crimping procedure, the sheets 125a, 124a are replaced with new sheets. By advancing a clean sheet after each crimping, buildup of contaminated coating material from previously crimped stents is avoided. By using replaceable sheets, the same crimping assembly can be used to crimp stents with different drug coatings without the risk of contamination or buildup of coating material from previous stent crimpings.
[0015] There is a continuing need for improved methods of crimping medical devices, particularly polymeric stent structures, onto delivery balloons to improve uniformity of deployment of the polymeric stent structure from the balloon, to increase retention between the stent structure and the balloon, and to achieve a minimal cross-profile for delivery of the stent structure to a target site. Summary of the Invention
[0016] The present invention provides a method for crimping a balloon expandable stent structure onto a balloon catheter. According to one embodiment, the inventive method disclosed herein is used to improve the crimping process of a thin-walled stent structure. Alternatively, the method can be used to improve the crimping process for crimping a stent structure with a thicker wall.
[0017] With reference to the case of thin-walled stent structures, the need for various modifications and improvements to the crimping process has been achieved through testing, and the crimping process does not cause significant problems when the same method is used to crimp stent structures with higher wall thicknesses. Examples of stent structures with higher wall thicknesses are recorded in US 2010 / 0004735. Studies have found that existing crimping methods have proven unsatisfactory when the wall thickness is significantly reduced (e.g., from 158 microns or about 160 microns of wall thickness to 100 microns or less of wall thickness). When applied to thin-walled stent structures, those existing crimping methods can produce a large number of twisted, cracked or broken struts.
[0018] According to the present invention, it has been determined that modifications and improvements to the crimping process can better ensure that all four of the following objectives are met:
[0019] • Structural Integrity : Avoid damaging the structural integrity of the stent structure when the stent structure is crimped to the balloon or expanded by the balloon.
[0020] • Safe delivery to implant site : During delivery to the implantation site, the stent structure is prevented from falling off or separating from the balloon, and the catheter is prevented from having a smaller cross profile.
[0021] • Expansion uniformity : Avoid uneven expansion of the stent structure ring, which may lead to structural damage and / or shorten fatigue life.
[0022] • Avoid overstretching the balloon : The relationship between monitoring balloon pressure and reducing the size of the stent structure to avoid excessive strain or possible pinhole leaks in the balloon without compromising the three existing requirements.
[0023] According to the embodiment, a polymer stent structure is curled to the balloon of a balloon catheter using a curling device and a curling barrier or protective sheet (e.g., a polymer material, hereinafter referred to as polymer material). The polymer material is disposed between the surface of the stent structure and the surface of a curling blade, which is pressed against the stent structure during the curling process. In a preferred embodiment, the polymer material is a sheet provided with a membrane head curling device. According to this embodiment, the stent structure is curled in an intermittent manner. Between one or more curling stages, the polymer sheet is adjusted to remove slack or excess accumulated sheet material. After this resetting of the polymer sheet, the stent structure diameter is further reduced, and then another resetting of the polymer sheet may be performed subsequently as needed or required. The number of resets of the polymer sheet will generally depend on the degree of diameter reduction during curling, and more specifically will depend on the curling result, the type of stent structure being curled, and the material of the stent structure.
[0024] In an alternative embodiment, the polymeric material is a sheath disposed on the stent structure. According to this embodiment, a sheath having a first size is disposed on the stent structure. The stent structure diameter is then reduced by a crimping device. After the stent structure diameter is partially reduced, the first sheath is replaced with a smaller second sheath that matches the reduced diameter of the stent structure. The first sheath is replaced with the smaller second sheath to avoid interference with the crimping process.
[0025] In addition to the aforementioned resetting of the polymer material during the crimping process, in some embodiments, the crimping process further includes varying the balloon pressurization during the crimping process to control the distribution of the balloon material supporting the stent structure. The goal is to maintain a distribution of small wrinkles in the balloon material supporting the stent structure during the crimping process, both when the crimping head applies pressure to the stent structure and when the holes are opened to allow the polymer material to reposition. To achieve this goal, the time between when the crimping blades apply pressure to the stent structure and when the holes are opened may require adjusting the pressure applied to the balloon.
[0026] When the balloon material supporting the inner diameter of the stent structure is distributed primarily in small folds (not a mixture of small and large folds), the stent structure expands more uniformly when the balloon is inflated. When the stent structure is compressed during crimping onto the balloon material formed into mostly or predominantly small folds, the balloon material formed into mostly or predominantly small folds will then expand (when inflated) while applying a relatively uniform radially outward pressure to the stent structure. This relatively uniform radially outward pressure produces the desired uniformity of expansion.
[0027] If instead the stent structure is compressed onto a balloon having a material formed into a combination of large and small folds, the balloon material will not apply uniform radial pressure to the stent structure when inflated. This is because areas of the balloon having small folds will expand faster than areas having large folds. As a result, one area or region of the stent structure will expand faster than another area. An example of this non-uniform expansion is shown in Figure 7B In both cases, the expanded or deployed diameter of the stent structure is the same (with or without uniform radial pressure applied by the balloon), but the stress distribution between the articulated regions of the stent structure is not uniform, which may result in a loss of radial strength. Figure 5 The application of non-uniform balloon pressure in the pattern shown can generate significant overstress both above and below the annulus of the expanded stent structure. The strain in the crown may exceed its yield strength, which may lead to significant loss of radial strength or even failure. Therefore, it is desirable to avoid non-uniform expansion of the stent structure (to avoid fracture or loss of strength of the stent structure annulus) for the sake of structural integrity.
[0028] If relatively low balloon pressure is used during crimping, then when the crimping leaves are removed to allow the polymer material to reset, there may not be a need to adjust the balloon pressure. However, if sufficiently high balloon pressure is used for crimping, then when the crimping leaves are retracted, the stent structure may expand outward (there is a net radially outward force on the stent structure when the radially inward force of the crimping leaves is eliminated). Therefore, it may be necessary to reduce the balloon pressure prior to removing the crimping leaves in order to maintain the stent structure diameter while the polymer material resets.
[0029] For embodiments in which a thin-walled stent structure is crimped, the balloon pressure is preferably maintained at a very high level (e.g., close to or exceeding the rated burst pressure of the balloon) as the blades compress the stent structure (high balloon pressure helps support the stent structure and prevent events such as strut flipping or twisting during diameter reduction). For these embodiments, when the blade pressure is removed, the balloon pressure is significantly reduced to avoid expansion of the stent structure. At the same time, a considerable balloon pressure must be maintained to ensure that small wrinkles are maintained. It has been found that if the pressure is reduced too much, large wrinkles will form when the polymer material is reset. As described above, the presence of large wrinkles can cause uneven expansion of the stent structure. The present invention provides pressure values used during the resetting of the polymer material that are relative to or independent of the balloon pressure used when the crimped blades press downward on the stent structure.
[0030] Although the present invention is primarily directed to crimping of stent structures, the scope of the present invention is not limited to stent structures. The present invention is also applicable to crimping of stents.
[0031] According to various aspects of the present invention, the present invention provides a medical device, a method for crimping, or a method for assembling a medical device, comprising the medical device having one or more of the following items (1) to (21), or any combination thereof:
[0032] (1) The medical device is a stent or stent structure crimped onto a balloon catheter.
[0033] (2) A crimping method using a crimping barrier or protective layer (e.g., a polymer material) that is disposed within the crimping aperture and between the crimper blades and the support structure.
[0034] (3) Reset the polymer material within the hole in the crimper head.
[0035] (4) Use of sliding wedge or iris-type crimpers, including but not limited to membrane head crimpers.
[0036] (5) The pre-crimping diameter of the stent structure is larger than the nominal diameter of the balloon used to crimp the stent structure onto the balloon catheter.
[0037] (6) During the curling process, the polymer material should be reset at least 2 times and 2 to 5 times.
[0038] (7) A stage in the curling process before the final dwell time, with a dwell time of 1 to 25 seconds.
[0039] (8) A method of crimping a thin-walled stent structure having a wall thickness of less than 125 microns, or less than 100 microns, or between 80 and 125 microns, onto a balloon.
[0040] (9) Has Figure 5 The support structure of the model shown.
[0041] (10) The pressure applied to the balloon during crimping may be higher than the nominal balloon pressure, and the balloon pressure is reduced (or released) after 50%-75% of the final crimp dwell time has been completed.
[0042] (11) A thin-walled stent structure supported within a crimping head by inflating a balloon to approximately the rated burst pressure of the balloon, or approximately 200-250 psi.
[0043] (12) The balloon pressure is released after the diameter is reduced by approximately 50% to 60% from the pre-crimping diameter.
[0044] (13) Second balloon pressure during reset or P2.
[0045] (14) First balloon pressure or P1 during diameter reduction and / or dwell period.
[0046] (15) applying a pressure P2 to the balloon material so that the balloon material maintains a shape that is complementary to the spaces between the struts of the stent structure almost everywhere on the circumference facing the luminal surface of the partially crimped stent structure (the balloon material is complementary when the stent structure is radially compressed by the balloon pressure P1 applied beforehand). The balloon material is complementary to these spaces when the length of the small folds is about the length between the struts of the stent structure, about equal to the distance separating the spaces between adjacent branch struts, or about the width of the struts.
[0047] (16) The polymer material is reset according to any combination of the following:
[0048] (a) performing a first resetting after a reduction of approximately 30% to 35% from the pre-crimp diameter, depending on the initial diameter size of the stent structure (smaller starting sizes mean a resetting is more likely to be needed within this range). The resetting may correspond to the time when the stent structure is removed from the crimper and alignment is checked (or the balloon of a balloon catheter is replaced with the balloon);
[0049] (b) Two or more resets may be performed, depending on the total travel from the initial diameter to the final crimped diameter; for example, two resets may be performed for a size reduction of 2:1 (ratio of initial diameter to final diameter); and three or more resets may be performed for a size reduction of 3:1 or more;
[0050] (c) For stent structures with closer struts, more resets were performed;
[0051] (d) resets are applied every time the diameter decreases by approximately 30-35% between process stages, but not exceeding 2, 3 or 4 resets in total during the entire crimping process; and / or
[0052] (e) is limited to a maximum of 5 or 2 to 5 resets. However, it is of course possible to perform more resets to achieve the desired result.
[0053] (17) A method comprising: using a scaffold structure made from a tube comprising a polymer, the polymer having a glass transition temperature, the scaffold structure having an outer diameter, and the outer diameter having a pre-crimping size; using a crimping device having a plurality of blades configured to form a hole, wherein the blades rotate relative to each other during crimping to increase or decrease the size of the hole; using a polymer material disposed within the hole; and crimping the scaffold structure to the balloon, the crimping comprising: disposing the scaffold structure and the balloon within the hole, wherein the polymer material is located between a surface of the scaffold structure and a surface of the blades, reducing the diameter of the scaffold structure from the pre-crimping size to a first size when the balloon has a first pressure, resetting the polymer material when the scaffold structure has approximately the first size and the balloon has a second pressure, reducing the diameter of the scaffold structure from approximately the first size to a second size when the balloon has the first pressure, and resetting the polymer material when the scaffold structure has approximately the second size and the balloon has the second pressure.
[0054] (18) The method of item (17), (19) or (20) in combination with one or more or any one of items (a) to (l):
[0055] (a) wherein the second pressure is between 3 and 4 atm or about 50% of the nominal balloon pressure.
[0056] (b) wherein the stent structure is a thin-walled stent structure, and the first pressure is about the rated burst pressure of the balloon, or about 200-300 psi.
[0057] (c) Wherein, the curling device is a membrane head curler.
[0058] (d) wherein the polymer material is a polymer sheet.
[0059] (e) wherein the polymer material comprises a sheath.
[0060] (f) wherein the support structure has a curling temperature during the curling process.
[0061] (g) wherein the balloon has a nominal diameter, and wherein the pre-crimped dimension is greater than the nominal diameter.
[0062] (h) wherein the crimping step further comprises the following steps: after the diameter of the stent structure is reduced to the first diameter, removing the stent structure and the balloon from the crimping device, and then returning the stent structure to the crimping device.
[0063] (i) wherein said resetting of said polymeric material occurs while said scaffold structure has approximately said first dimension when said scaffold structure and balloon are removed from said crimping device.
[0064] (j) Wherein, the balloon is a first balloon, the method further comprising the steps of replacing the first balloon with a second balloon of a balloon catheter when the stent structure is removed from the crimping device, and crimping the stent structure onto the second balloon.
[0065] (k) wherein the scaffold structure diameter is reduced from the pre-crimping diameter to the first diameter using a first crimping device, and the scaffold structure diameter is reduced from the first size to the second size using a second crimping device.
[0066] (l) wherein the polymer material within the hole is reset more than twice during the curling process.
[0067] (m) wherein the pores are maintained constant before and after reducing the diameter of the scaffold structure from the first size to the second size while the balloon has approximately a nominal diameter.
[0068] (19) A method comprising: using a scaffold structure made of a tube comprising a polymer, the polymer having a glass transition temperature, the scaffold structure having an outer diameter, and the outer diameter having a pre-crimping size; using a balloon having a nominal diameter; using a polymer material disposed within the hole; and using a crimping device having a plurality of blades configured to form a hole, wherein the blades rotate relative to each other during crimping to increase or decrease the size of the hole; and crimping the scaffold structure to the balloon, the crimping comprising: configuring the scaffold structure and the balloon within the hole, reducing the diameter of the scaffold structure from the pre-crimping size to a first size when the balloon has a first pressure, the first size being 30% to 35% smaller than the pre-crimping size, and after reducing the diameter to the first size and while the balloon has a second pressure, increasing the hole size to eliminate the pressure of the blades from the surface of the scaffold structure, and then removing excess polymer material from the hole.
[0069] (20) A method comprising: using a stent structure made from a tube comprising a polymer, the polymer having a glass transition temperature, the stent structure having an outer diameter, and the outer diameter having a pre-crimping size; using a balloon having a nominal diameter; using a crimping device having a plurality of blades configured to form a hole; using a polymer material disposed within the hole; and crimping the stent structure onto the balloon, the crimping comprising: configuring the stent structure and the balloon within the hole so that the polymer material is located between a surface of the stent structure and a surface of the blades, reducing the diameter of the stent structure from the pre-crimping size to a second size, wherein the polymer material within the hole is reset 2 to 5 times while reducing the diameter of the stent structure from the pre-crimping size to the second size; and wherein the balloon has a first pressure when the stent structure diameter is reduced in size, and the balloon has a second pressure when the polymer material is reset.
[0070] (21) The method of item (17), (19) or (20) in combination with one or more or any one of items (a) to (c):
[0071] (a) wherein the polymer material comprises sheaths having different sizes.
[0072] (b) wherein the polymer material is a sheet material operated by a film head curler.
[0073] (c) wherein the scaffold structure comprises struts forming rings, wherein adjacent rings are connected to each other by at least two links, and the scaffold structure is curled to a theoretical minimum curling size (D-min).
[0074] Incorporated by reference
[0075] All publications and patent applications mentioned in this specification are incorporated herein by reference to the same extent as if each individual publication or patent application was specifically and individually indicated to be incorporated by reference. In the event of inconsistencies in the use of words and / or phrases between the incorporated publication or patent and this specification, these words and / or phrases will have a meaning consistent with the manner in which they are used in this specification.
[0076] BRIEF DESCRIPTION OF THE DRAWINGS
[0077] FIG. 1A is a perspective view of a prior art film head crimper.
[0078] 1B is a front view of the membrane crimper head shown in FIG. 1A when the crimper jaws are placed on a bracket.
[0079] Figure 2A-2Bis a scanning electron microscope (SEM) image of a cross section of a stent structure partially crimped to a catheter balloon within a crimper head. The polymer sheet of the crimping mechanism is wrapped around the stent structure and partially located between the struts of the stent structure.
[0080] Figure 3A and Figure 3B A first method (Method I) for crimping a scaffold structure according to the present invention is described.
[0081] Figure 4A and Figure 4B A second method (Method II) for crimping a scaffold structure according to the present invention is described.
[0082] Figure 5 The distal and proximal portions of a stent structure according to one of the embodiments are shown.
[0083] Figure 6 Shows Figure 5 A stent structure crimped to the balloon of a balloon catheter.
[0084] Fig. 7A is a cross-sectional view of a stent structure partially crimped to the balloon of a balloon catheter. This image shows the presence of large and small wrinkles in the balloon material when the pressure applied to the interior of the balloon is discontinued.
[0085] Figure 7B yes Fig. 7A Plan view of the stent structure after radial expansion from a crimped state using a balloon. The stent structure is crimped during resetting without applying pressure to the interior of the balloon. Therefore, during resetting, the balloon material has a similar Fig. 7A The shape shown. Figure 7B It can be seen that the rings of the stent structure are unevenly opened or expanded (compare Figure 7B This uneven unfolding from the curled state to the expanded state ( Figure 7B ) is caused by the uneven radial pressure applied by the balloon to the struts of the stent structure when the balloon is inflated. This uneven deployment is believed to be due to the presence of large wrinkles when the stent structure is fully crimped onto the balloon ( Fig. 7A ) caused by.
[0086] Fig. 8A is a cross-sectional view of a stent structure partially crimped to a balloon of a balloon catheter, wherein the balloon pressure is maintained when the crimp leaf pressure is removed to allow the polymer material to reset. This figure shows that when the pressure inside the balloon is significantly higher than Fig. 7A When the internal pressure of the balloon is medium, there are small wrinkles or no large wrinkles in the balloon material. Fig. 8AThe pressure inside the balloon is shown to be much higher than 1 atmosphere (1 atm). For example, the pressure inside the balloon is between about 3 atm and 4 atm.
[0087] Figure 8B yes Fig. 8A 1. A plan view of a stent structure after radial expansion from a crimped state by inflating a balloon. When a resetting period occurs while providing pressure to the balloon, such as providing a pressure between about 3 atm and 4 atm during resetting, the stent structure shown in this figure is crimped. DETAILED DESCRIPTION OF THE INVENTION
[0089] In the description, reference numerals appearing in the drawings and the description indicate corresponding or similar elements throughout the different views.
[0090] For the purposes of this invention, the following terms and definitions apply:
[0091] The terms "about", "approximately", "roughly", or "substantially" mean 30%, 20%, 15%, 10%, 5%, 4%, 3%, 2%, 1.5%, 1%, between 1% and 2%, between 1% and 3%, between 1% and 5%, or between 0.5% and 5% less than or greater than a specified value, the range or each endpoint of a specified range, or a 1-σ, 2-σ, 3-σ variance (Gaussian distribution) from the stated mean or expected value. For example, d1 is about d2 means that d1 is 30%, 20%, 15%, 10%, 5%, 4%, 3%, 2%, 1.5%, 1%, 0%, between 1% and 2%, between 1% and 3%, between 1% and 5%, or between 0.5% and 5% different from d2. If d1 is an average value, then d2 is about d1 means that d2 is within the 1-σ, 2-σ, or 3-σ variance or standard deviation of d1.
[0092] It should be understood that any numerical value, range, or any range endpoint prefixed by the words "about", "approximately", "roughly", or "substantially" described in the present invention (including, for example, "almost nothing", "approximately", "approximately all", etc.) also describes or discloses the same numerical value, range, or any range endpoint not prefixed by the words "about", "approximately", "roughly", or "substantially".
[0093] "Glass transition temperature" TG is the temperature at which the amorphous domains of a polymer transition from a brittle glassy state to a solid deformable or ductile state at atmospheric pressure. This application defines TG and a method of finding polymer TG or low TG (lower end of TG range) in the same manner as in US20160081824.
[0094] "Stent" refers to a permanent, durable or non-degradable structure generally composed of a non-degradable metal or metal alloy structure, but in general, a "scaffold" refers to a temporary structure comprising a bioresorbable or biodegradable polymer, metal, alloy, or combination thereof and capable of radially supporting a blood vessel for a limited period of time of 3, 6, or 12 months after implantation. However, it should be understood that the art sometimes uses the term "stent" when referring to any of the above types of structures, and vice versa.
[0095] "Inflated diameter" or "expanded diameter" refers to the inner or outer diameter of a stent structure when its supporting balloon is inflated to expand the stent structure from its crimped configuration for implantation into a blood vessel. The inflated diameter may refer to the diameter of the expanded balloon that exceeds the nominal diameter (e.g., a 6.5 mm balloon has a nominal diameter of 6.5 mm, or when inflated to its nominal inflated diameter, has a diameter of 6.5 mm). The diameter of a stent structure, after being pressurized by balloons to reach its inflated or expanded diameter, may be reduced to some extent by recoil effects primarily, partially, or entirely related to the manner in which the stent structure is manufactured and processed, the materials of the stent structure, and the design of the stent structure. When referring to the fully inflated diameter of a balloon, it refers to the balloon pressurization corresponding to or greater than the nominal inflated diameter. Balloon pressure may be expressed in pressure units (e.g., psi or N / m 2 ) or relative to standard atmospheric pressure (abbreviated "atm"). One atmosphere is equivalent to about 14.7 psi or 101325 Pascals or N / m 2 The balloon inflation pressure gauge of a typical balloon catheter has a nominal or fully inflated pressure of between about 6 - 8 atm and has a rated burst pressure of about 16 atm.
[0096] When referring to a diameter, this shall mean either the inner diameter or the outer diameter unless otherwise stated or implied in the context of the specification.
[0097] The "post-expanded diameter" (PDD) of a stent structure refers to the inner diameter of the stent structure after increasing to its expanded diameter and removing the balloon from the patient's vasculature. The PDD causes a recoil effect. For example, an acute PDD refers to the diameter of the stent structure that causes acute recoil in the stent structure.
[0098] "Pre-crimp diameter" refers to the outer diameter (OD) of a tube used to make a stent structure (e.g., cut from dipping, injection molding, extruding, radially expanding, die-drawing, and / or annealing the tube), or the outer diameter (OD) of a stent structure before it is crimped onto a balloon. Similarly, "crimp diameter" refers to the OD of the stent structure when crimped onto a balloon. The "pre-crimp diameter" may be approximately 2 to 2.5, 2 to 2.3, 2.3, 2, 2.5, or 3.0 times larger than the crimp diameter, and approximately 0.9, 1.0, 1.1, 1.3, and approximately 1 to 1.5 times larger than the expanded diameter, the nominal balloon diameter, or the expanded diameter. For purposes of the present invention, crimping refers to a reduction in diameter of a stent structure characterized by significant plastic deformation, i.e., due to plastic deformation, such as in the case of a stent or stent structure having an undulating annular pattern, at the crowns, such as Figure 5 As shown, the diameter is reduced by more than 10% or more than 50%. When the stent structure is deployed or expanded by the balloon, the inflated balloon causes the stent structure to plastically deform from its crimped diameter. The method for manufacturing a crimped stent structure according to the disclosed content is described in US Patent Application US20130255853.
[0099] The "crimping stage" or "stage" of a crimping process refers to the period of time during which the jaws of the crimping device remain fixed or the orifice of the crimping head remains at a constant diameter. The duration of the stage may be referred to as the dwell time or dwell period. In the initial stage before the final dwell, the dwell time may range from 1 second to 25 seconds. After reaching the final crimping diameter, the dwell time may be between 50 seconds and 300 seconds. As the crimping device moves from the first stage to the second stage, respectively, the orifice of the crimping device is reduced from a first diameter to a second diameter. For the purposes of the present invention, a reduction in orifice size (e.g., from a first diameter or orifice size to a second diameter or orifice size) is understood to be the same as the actual outer diameter of the stent structure within the orifice when the stent structure is crimped by the crimper and reduced in size. However, it should be understood that the programmed orifice size may not be exactly the same as the outer diameter of the crimped stent structure size, particularly when the stent structure is crimped to a very small diameter.
[0100] Materials "comprising" or "including" poly(L-lactide) or PLLA include, but are not limited to, PLLA polymers, blends or mixtures comprising PLLA and another polymer, and copolymers of PLLA and another polymer. Thus, a strut comprising PLLA means that the strut can be made of a material comprising any of a PLLA polymer, a blend or mixture comprising PLLA and another polymer, and a copolymer of PLLA and another polymer.
[0101] When referring to a direction perpendicular to or parallel to the axis AA (e.g. Figure 5), it will mean a direction perpendicular to or parallel to the axial direction of the support structure or tube. Similarly, when referring to a direction perpendicular to or parallel to the axis BB (e.g., as shown in Figure 5 BB and perpendicular to the axis BB. Thus, the sinusoidal rings of the support structure (periodically) extend parallel to the circumferential direction or parallel to the axis BB and perpendicular to the axis AA, while in one embodiment, the connecting rods extend parallel to the axial direction or axis AA of the support structure or tube and perpendicular to the axis BB.
[0102] Where the same element number is used for multiple figures, it should be understood that the same description first used for the element in the first figure applies to the embodiment described in the subsequent figures, unless otherwise specified.
[0103] A thickness dimension (e.g., the thickness of a wall, strut, ring, or link) refers to a dimension measured perpendicular to axes AA and BB. A width dimension is measured in a plane defined by axes AA and BB; more specifically, the width is the cross-sectional width from one side of the adjacent structure to the other; thus, the link 334 can have a constant link width. Furthermore, it should be understood that the so-called plane of axes AA and BB is not technically a plane, as it describes the surface of a tubular structure having a central lumen axis parallel to axis AA. Thus, if a cylindrical coordinate system is used to describe the position of a stent structure, one may choose to treat the BB axis as an angular component (i.e., axis AA is the Z axis, and the position of the luminal / abluminal surfaces of the crowns, links, rings, etc. is determined by angular coordinates and radial coordinate constants).
[0104] "Thin wall thickness", "thin wall stent structure", "thin wall" refers to struts, rings, links or bar arms made of a polymer with a wall thickness of less than 125 microns. The polymer may comprise poly(L-lactide).
[0105] The "curling temperature" of the present invention refers to a temperature that is higher than ambient temperature and slightly lower than or approximately equal to the glass transition temperature (TG) of the polymer (e.g., poly(L-lactide)) of the scaffold structure. In a preferred embodiment, the curling temperature is between TG and 15 degrees less than TG, or between TG and 10 degrees or 5 degrees less than TG. In other embodiments, the curling temperature is achieved by heating the scaffold structure to a temperature at least 20 degrees lower than TG and preferably to a temperature at least 15 degrees lower than TG.
[0106] like Figure 3B and 4BAs shown in the crimping step in, "resetting the polymer material within the pore" or "resetting the polymer material within the pore" refers to one or both of removing excess polymer material from the pore of a crimping head formed by interconnected blades or wedges of a mechanical crimping device (e.g., an iris or sliding wedge crimper) or enlarging / opening the pore to substantially eliminate blade pressure on the stent structure (in the case of a membrane head crimper). The blades or wedges converge on the stent structure to reduce the diameter of the stent structure (and crimp the stent structure onto the balloon). An example of a membrane head crimper is the MSI TM SC775S / 875S, which is available from Machine Solutions. To this end, the polymer material is reset in the hole by fully opening the crimping hole so that the polymer sheet material automatically returns to its starting position and becomes fully taut and a new sheet of polymer material is crimped. After this step, the hole is then returned to the support structure to continue the crimping process. The resetting of the polymer material may include, for example, removing the support structure and balloon from the crimping head when the first sheath is replaced by the second sheath. Alternatively, the resetting of the polymer material may be performed without removing the support structure and balloon from the crimping head. For example, taking a membrane head crimper as an example, when the hole is opened, the support structure and balloon do not move and remain in the crimping head, the polymer material is reset, and then the hole is closed again on the support structure and balloon.
[0107] The term "first pressure" or "P1" shall refer to the pressure applied to the balloon when using the crimping head to reduce the diameter size of the support structure, and / or during the dwell period or when the hole size maintains a constant diameter and limits the support structure from rebounding outward. P1 can range between about 3 or 4 atmospheres, up to the rated burst pressure of the balloon. Preferably, P1 is between about 200 psi and 250 psi, or between about 13 atm and 17 atm. In other embodiments, P1 is higher than P2, or is at least twice the pressure of P2. In a preferred embodiment, the support structure is a thin-walled support structure, and P1 is between about 200 psi and 250 psi, between about 13 atm and 17 atm, or about the rated burst pressure of the balloon to provide additional support for the support structure struts when the rings of the support structure are deformed by the crimper blades. In other embodiments, P1 can range between about 4 atm and 13 atm.
[0108] The term "second pressure" or "P2" shall refer to the pressure applied to the balloon during the resetting of the polymer material, and / or when the crimping leaf pressure is removed or the outward rebound of the stent structure is not restricted. P2 may be above 1 atm, from above 1 atm to 3 atm, up to about 3 or 4 atm, greater than 4 atm and less than P1, or about 50% of the nominal inflation pressure of the balloon. DETAILED DESCRIPTION
[0109] An effective stent crimping process must meet at least the following objectives:
[0110] • Structural integrity: Avoid compromising the structural integrity of the stent structure when it is crimped to or expanded by the balloon.
[0111] • Safe delivery to the implantation site: Avoid detachment or separation of the stent structure from the balloon during delivery to the implantation site.
[0112] • Expansion uniformity: Avoid uneven expansion of the stent structure rings, which can lead to structural failure and / or shorten fatigue life.
[0113] As previously reported in US20140096357, stent structures are not as resilient as stents made of metal with high ductility. Therefore, meeting all of the above requirements is more challenging for polymer stent structures, especially for thin-walled stent structures, because the thin-walled stent structures can be more easily broken during crimping or balloon expansion, and are more prone to twisting, flipping or overlapping during crimping.
[0114] According to the curling method provided by the present invention, the curling method comprises the following steps: wherein, the polymer material is reset or replaced in the curling head so that any interference between the downward compression of the support structure struts by the curler blades and the polymer material is minimized. The polymer material is used to protect the surface or the support structure or a coating arranged on the support structure (or support). However, as the support structure is further curled downward and its diameter is reduced, when the support structure has a larger diameter, the polymer material around the support structure becomes excessive, resulting in wrinkles, rolling, relaxation or tension loss. Although the curling mechanism may include a tensioning portion, the tensioning portion applies a tensioning force (as a means of absorbing excess relaxation in the polymer material) when the hole is reduced due to the presence of blades that are closely adjacent to the surface of the support structure struts or in contact with the surface of the support structure struts, the tensioning force cannot remove material from the vicinity of the support structure. In order to solve this problem, the curling hole is opened and the sheet material is reset (or replaced in the case of using a sheath).
[0115] FIG. 2A to FIG. 2B1 shows what happens when the polymer sheet material becomes slack without removing the diameter and blades to reset the sheet, or if the sheet is not relatively taut near the surface of the stent structure. The interior of the crimping head of the membrane head crimper is shown. Although the membrane head crimper includes the tensioning mechanism described above, the sheet material can still be trapped between the struts of the stent structure because the proximity of the blades to the surface of the stent structure limits the effectiveness of the tensioning mechanism. Basically, during the crimping stage or the diameter reduction between stages, the blades are pressed down on the surface of the stent structure, or the blades are very close to the surface of the stent structure, thereby limiting the movement of the polymer material disposed between the blades and the surface of the stent structure when tension is applied to the portion of the sheet material outside the hole. Since the polymer material is sandwiched between the blades and the stent structure, the tension applied to the outside of the blades is reacted by the compressive force on the polymer material. As shown, the stent structure 300 (partially crimped to the balloon 15) has struts 330. The portion 128 of the sheet 124a / 125a is sandwiched between the folded struts 330. As the struts attempt to fold around the crown, thereby reducing the size of the ring and the diameter of the stent structure, the loose polymer material 128 is pulled or pushed into the open spaces between the struts by the converging leaves. Figure 2A-2B Especially for thin-walled stent structure struts, excessive interaction between the extruded sheet and the folded struts often leads to undesirable curled units.
[0116] It has been found that resetting or removing excess polymer material after diameter reduction (by retracting the leaves or increasing the hole size so that the external tensioning force pulls the polymer material away from the surface of the stent structure) can make a significant difference in crimp quality and production output. Through testing and experimentation, it has been found that resetting or removing excess polymer sheet material (or in an alternative embodiment, replacing the first sheath with a smaller second sheath) at a critical time after diameter reduction (as described below) prevents the polymer material from significantly interfering with the desired folding of the ring struts around the crown during the subsequent diameter reduction step.
[0117] As previously discussed with reference to FIG. 1B , for the film head crimper, when the support structure (or support 100) is located within the aperture of the crimping assembly 20, the first sheet 125a and the second sheet 124a are both positioned relative to the wedge or blade 22 of the crimping device. The two sheets pass between the two blades 22 on opposite sides of the support 100, and tensions T1 and T2 are applied to collect excess sheet material as the iris of the crimping assembly is reduced in size by the converging blades 22. Although the tensioning mechanism is intended to keep the sheets relatively taut, the sheet material still accumulates in an unacceptable manner, as described above.
[0118] Fig. 7Ais a cross-sectional view of the balloon 12 of the stent structure 10 partially crimped to the balloon catheter 2 when a pressure less than P2 is applied to the balloon 12. This view shows the presence of large and small wrinkles in the balloon material 12a. Figure 7B Shown in use Fig. 7A 1. The condition after the stent structure 10 is expanded by the balloon 12 having large folds in the fully curled stent structure. The large folds (when present below the fully curled stent structure) cause the area of the balloon to expand at a different rate than the area of the balloon having small folds. Due to this irregular expansion, uneven radial outward pressure is applied to the balloon, thereby forming a pattern of the expanded stent structure. Section II of the stent structure is subjected to a smaller radial outward pressure than expected, while Section I of the stent structure is subjected to a larger radial outward pressure than expected. Alternatively, optionally, Section II elements of the stent structure network, such as the crown, do not reach the strain level that the crown is designed to withstand, while Section I elements exceed this design strain. The end result is that the desired expanded diameter is achieved, but at the expense of over-strained elements in Region I. Therefore, when the stent structure is implanted in a blood vessel and subjected to cyclic radial loads, the crown of the ring in Region I may be prone to loss of strength or failure.
[0119] Fig. 8A 1 is a cross-sectional view of a stent structure 10 partially crimped to a balloon 12 of a balloon catheter 2, wherein a balloon pressure P2 is applied to the balloon 12. This view shows the presence of small wrinkles or the absence of large wrinkles. The balloon material 12a has a shape that is complementary to the spaces between the struts 10a, 10b of the stent structure and partially enters these spaces during the crimping process. The length of the small wrinkles is approximately equal to the length of the struts (different from the length of the small wrinkles). Fig. 7A The pleat length shown is the distance between adjacent pleats in the material 12a. Fig. 7A Compared with the situation Fig. 8A The variation of the fold length of the balloon material 12a in the embodiment is much smaller or the range of the fold length is narrower. It is found that without applying P2, the folding of the balloon material 12a will be uneven, such as Fig. 7A shown.
[0120] In some embodiments, when the length of the small folds is approximately the space between the struts of the stent structure, the balloon material is complementary to the space between the struts, for example, the balloon fold length is approximately equal to the distance from the first strut to the third strut, and there is a second strut between the first strut and the third strut, or between the first strut and the third strut. Fig. 8A In the example of , the corrugation is approximately equal to the width of the strut 10a, or the distance from the first space to the adjacent space separating the struts. If the pressure is not less than P2, there is no such complementary balloon material, and if the pressure is too high, the balloon pressure will expand the stent structure.
[0121] Figure 8B yes Fig. 8A The stent structure 10 is shown in plan view after radial expansion from a crimped state using a balloon 12. The stent structure is crimped due to the pressure P2 applied during resetting. Figure 7B In contrast, the expansion is uniform and there is no area on the stent structure that exceeds or falls below the design strain.
[0122] Figure 3A , 3B (Method I) and Figure 4A , 4B (Method II) is a flow chart showing two embodiments of a crimping method that can achieve the aforementioned objectives of a stent structure (including a thin-walled stent structure). In each of these embodiments, a stent structure that is crimped to a balloon is laser cut from a radially expanded tube. However, the crimping method is not limited to stent structures made from laser cut tubes. Other stent structure types, such as stent structures that are not radially expanded or stent structures made from polymer sheets (rather than tubes) are included within the scope of the present invention. In addition, the starting outer diameter size of the stent structure (e.g., a coronary stent structure) can be between 3.0 mm and 4.25 mm or between 2.0 mm and 6 mm. For peripheral stent structures, the starting outer diameter size can be between 6 mm and 10 mm.
[0123] Both crimping methods I and II may use 1 or 2 balloons. The two balloons referred to in the figures and in the following discussion are referred to as "Balloon A" and "Balloon B", respectively. Balloon A refers to the balloon of the finished balloon catheter. Balloon B refers to a temporary or sacrificial balloon or balloon catheter used during the initial stages and then replaced by Balloon A during the final alignment or alignment check, as described below. It is desirable to use Balloon B (later replaced by Balloon A) to implement Method I or Method II when the starting inner diameter size of the scaffold structure is greater than or equal to the diameter size of Balloon A (when Balloon A is inflated to its nominal inflated diameter, or when Balloon A is inflated beyond this size).
[0124] In a preferred embodiment of the crimping method, a membrane head crimper is used to crimp the stent structure to the balloon catheter. For the membrane head crimper, a polymer material in the form of a polymer sheet dispensed by a pair of rollers (FIGS. 1A-1B) is used to protect the stent structure from the crimper blades. Thus, for this type of crimper, the "resetting polymer material in the hole" step refers to the process of opening the hole to automatically remove excess polymer sheet material from the hole and re-tensioning the polymer sheet. However, it should be understood that the present invention is not limited to the use of a membrane head crimper and can be implemented by alternative arrangements for configuring and removing or resetting polymer material in the crimping hole (e.g., using multiple sheaths).
[0125] Reference Figure 3A-3B (Method I), two crimper setups or devices are used. The first crimper setup is used for the crimping stage before the final alignment check ( Figure 3A ), and a second crimper is set up for the final alignment check stage after that ( Figure 3B ).
[0126] Pre-curling procedure : The stent structure is disposed on balloon A (or balloon B if two balloons are to be used). The balloon is inflated to its nominal diameter or to a post-expanded diameter (larger than the nominal diameter size), or more generally, the balloon is fully inflated so that its size is at least equal to or exceeds the inner diameter of the stent structure so as to support the stent structure during the initial crimping step. The stent structure is aligned with the proximal and distal markings on the balloon (not required if balloon B is used). The crimper head, stent structure and / or balloon may also be deionized to eliminate static charges that may cause the stent structure to deviate from alignment with the balloon markings during the crimping process. It has been found that static charge accumulation can not only cause misalignment between the stent structure and the balloon, but also cause irregular crimping of the stent structure (metal stents generally do not produce static charge accumulation because the balloon is in sliding contact with the metal rather than a polymer surface). The stent structure is then inserted into the crimper head while the balloon is kept fully inflated.
[0127] Phase I : The stent structure supported on a fully inflated balloon is located within the crimping head. The temperature for crimping or crimping temperature is set during this stage, as well as the starting iris or orifice size corresponding to the input outer diameter of the stent structure (e.g., 3.5 mm). In a preferred embodiment, the blades of the iris or sliding wedge crimping device are heated to achieve the desired crimping temperature (or a heated liquid or gas may be used). After the stent structure reaches the crimping temperature, the iris of the crimper closes to reduce the inner diameter (ID) of the stent structure to less than the outer diameter (OD) of the fully inflated balloon, while the balloon pressure is P1.
[0128] Phase II : The crimper jaws maintain a fixed diameter during the dwell period while the balloon pressure is P1. At the end of this dwell period, the stent structure and balloon are removed from the crimping device. When removed from the crimping device, the balloon may have a pressure of P2.
[0129] Verify alignment / change balloon : If the final alignment of the balloon markers does not need to be checked or verified, or if balloon A is used for both phases I and II, the removal after phase II can be skipped. In the illustrated embodiment, the scaffold structure supported on the balloon is removed from the crimping device to verify that the scaffold structure is located between the balloon markers (when balloon A is used for phases I and II), or balloon A is used to replace balloon B and the scaffold structure is aligned with the balloon markers.
[0130] Now refer to Figure 3B , continue with Method I. Figure 3B The curling steps shown use the same Figure 3A The curl settings in different curl settings.
[0131] Phase III : After the stent structure and inflated balloon A are returned to the crimper, the iris diameter is set to a diameter slightly higher than the stent structure diameter at the end of Phase II (to account for recoil forces). The size of the iris or hole remains constant for a period of time sufficient to allow the stent structure temperature to return to the crimping temperature.
[0132] After reaching the crimping temperature, the scaffold structure diameter is reduced while the balloon has a pressure P1. The balloon has a pressure P1 for reducing the diameter after stage III.
[0133] Stage IV : After the scaffold structure diameter is reduced from the diameter of stage III and the balloon has a pressure of P1, the crimping hole remains constant during the dwell period. After stage IV, when the scaffold structure diameter is reduced from the diameter of stage III to the diameter of stage IV, or when the diameter is reduced from the initial diameter to the diameter of stage IV, after stage IV, the polymer sheet of the membrane head crimper is reset to remove excess sheet material from the hole. When the polymer material is reset, the balloon has a pressure of P2.
[0134] Applying pressure to the balloon during the crimping process helps ensure or improve the retention of the stent structure on the balloon in addition to helping promote uniform expansion of the balloon. The balloon pressure can be released after 50%-75% of the final crimping dwell time is completed. When reducing the diameter of the stent structure (or stent diameter) and during the dwell period, a pressure of 75-250 psi is generally applied, or more preferably, between about 200-250 psi, between about 200-280 psi, and between about 200-300 psi is applied when crimping thin-walled stent structures. The pressure is selected to obtain the lowest possible cross profile, ensure adequate retention, and provide radial support for the stent structure struts when the rings are folded by the crimper blades.
[0135] Phase V – VIII : These stages follow a similar approach to stages III-IV: a dwell is performed at each stage and the diameter is reduced between stages while the balloon has a pressure P1. At the end of the dwell period, while the balloon has a pressure P2, the orifice is fully opened and excess polymer sheet material is removed from the orifice. Figure 3A-3B In the example of FIG. 5 , a total of three resets of polymer materials are shown. The resets are all performed after the final alignment check.
[0136] Optional Stage / Final Curl: After resetting (immediately after stage VIII), there may be a number of other optional stages. At the end of these stages, the balloon is finally pressurized at the final crimp diameter and balloon pressure P1. The pressurization may be a leak check. After this final step, the stent structure is fully crimped to the balloon catheter, removed from the crimping head, and deployed in the constraining sheath.
[0137] Figure 4A-4B (Method II) describes an alternative crimping method. In addition to the following, the instructions are attached Figure 3A-3B The same approach can be applied to Figure 4A-4B Method I uses a different crimper assembly or setup after the final alignment check. Steps III through VIII in Method I are performed on the other crimper assembly or setup. Therefore, the resetting of the polymer material can be done automatically during the final alignment check in Method I (after Stage II and before Stage III). This is exactly what is needed to re-set the polymer material in the hole. Figure 3A In method II, a single crimping device or setup (configuration) is used for the crimping. In stage II of method II ( Figure 4A ) is completed, the polymer material is reset. The resetting may be performed before or after the alignment check and / or replacement of the balloon (when balloon B is used in Phase I and Phase II), assuming that the final alignment check has also been completed (this step is optional in some embodiments). Methods I and II have a total of 4 steps shown, in which the polymer material within the hole is reset. For Method I, when a second crimping device / setting is used after the alignment check, an additional substantially completed resetting step may be performed (thus, a total of 4 resets are performed for Method I). Based on an inspection of the stent structure crimped to the balloon, the number of resets for a specific stent structure size, balloon size and associated D-min (defined below) is optimally selected. The criteria used to judge the effectiveness of the selected number of resets are the three crimping goals listed above (structural integrity, stent structure retention and uniform expansion). It should be understood that the interference of the polymer material with the strut folding, especially in Figure 2A-2B The kind shown in , can adversely affect any or all three curling objectives. Balanced against the need to reset the polymer material is the time required for the reset and the throughput benefits.
[0138] According to one embodiment, whenever the space between struts is large enough to accommodate the sheet material (close to the final crimp diameter, the space between struts may be too small for the sheet material) and the percentage of diameter reduction is sufficient to cause material accumulation between the blades and the surface of the stent structure, the polymer material should be reset. This period of diameter reduction and the resulting crimp size will be referred to as the critical crimp time.
[0139] Resetting should not be too frequent as this would make the crimping process very time consuming. Therefore, whenever the diameter of the stent construct is reduced, it is not considered feasible or cost effective to perform a reset. A balance is required. The reset point within the critical crimping time period should be chosen so that the yield is good but the crimping time does not become overly onerous.
[0140] Based on extensive testing of different scaffold structure types, the critical crimp time period may be reset ("reset") one or more times to the polymer material within the pores according to one or more of the following rules:
[0141] • The first reset is performed after a reduction of approximately 30-35% from the initial diameter, depending on the initial diameter size of the stent construct (a smaller starting size means a reset is more likely to be needed within this range). The reset may correspond to the time when the stent construct is removed from the crimper and alignment is checked (or switched to balloon A);
[0142] • 2 or more resets may be selected depending on the total travel from the initial diameter to the final crimped diameter; for example, for a diameter reduction of 2:1 (ratio of initial diameter to final diameter), 2 resets should be performed; for a diameter reduction of 3:1 or more, 3 or more resets should be performed;
[0143] • For stent designs where struts are closer together, more resetting should be performed;
[0144] • Resets should be performed every time the diameter decreases by approximately 30-35% between stages, but the total number of resets should not exceed 2, 3 or 4 during the entire crimping process; and / or
[0145] • Limited to a maximum of 5 or 2 to 5 resets. However, it is of course possible to perform more resets in order to achieve the desired result.
[0146] Figure 6 A side view of a stent structure 300 crimped to a balloon catheter is shown, the stent structure having a shaft 2 , a balloon 15 with distal and proximal ends 17a , 17b (wherein a balloon marker is found). The catheter is supported on a mandrel 8 .
[0147] Figure 5 Shown in a state before expansion or curling Figure 6 300. This figure shows an example of a network of struts and links for the stent structure 300. The left or distal portion 302 (i.e., Figure 5The left side of the apparatus (shown in FIG. 1 ) includes sinusoidal rings 312a, 312b, and 312c, with ring 312a being the outermost ring. Rings 312a and 312b are adjacent to each other by two links 334 and a marker link 20. Rings 312d and 312e are adjacent to each other by three links 334 extending parallel to axis AA. Links 334 extend parallel to axis AA and have a constant cross-sectional moment of inertia over their length, meaning that links 334 have a constant width and thickness, and the location of the center of mass or geometric center (or longitudinal axis) of the links is parallel to axis AA. The right or proximal portion 304 (i.e., Figure 5 The right side of the support structure 300 includes sinusoidal rings 312d, 312e and 312f, wherein ring 312f is the outermost ring. Ring 312d and ring 312e are adjacent to each other through three connecting rods 334. Ring 312e and ring 312f are adjacent to the marking link 20 through two connecting rods 334. Therefore, the support structure 300 has a marking link 20, which extends between the outermost link and the adjacent inner ring and is adjacent to the outermost link and the adjacent inner ring. The support structure 300 may have 15-20 rings 312, for example 15, 18 or 20 rings 312, which are interconnected to each other through the connecting rod 334.
[0148] The ring 312, such as the ring 312b, may be sinusoidal, meaning that the curvature of the ring along the axis BB is best described by a sine wave, wherein the wavelength of the sine wave is equal to the distance between adjacent peaks 311a of the ring. The ring may have a constant width at the two crowns 307, 309 and 310 and at the struts 330, which connect one crown to the adjacent crown.
[0149] There are three types of crowns in each inner ring 312b to 312e: U-shaped crown, Y-shaped crown and W-shaped crown. The outermost ring has only Y-shaped crown or W-shaped crown, and U-shaped crown. The peak or peak 311a (or the trough or valley 311b) can correspond to the U-shaped crown, Y-shaped crown or W-shaped crown. For the outermost ring 312a, there are only U-shaped crown and W-shaped crown. For the outermost ring 312f, there are only U-shaped crown and Y-shaped crown. The marking link 20 is adjacent to the ring by forming a W-shaped crown with the first ring (e.g., ring 312e) and a Y-shaped crown with the second ring (e.g., ring 312f).
[0150] The connecting rod 334 is connected to the ring 312f at the Y-shaped crown 310. A "Y-shaped crown" refers to a crown where the angle extending between the struts 330 of the ring 312 and the connecting rod 334 is an obtuse angle (greater than 90 degrees). The connecting rod 334 is connected to the ring 312a at the W-shaped crown 309. A "W-shaped crown" refers to a crown where the angle extending between the struts 330 and the connecting rod 334 is an acute angle (less than 90 degrees). The U-shaped crown 307 is a crown that does not have a connecting rod connected to it. The marking connecting rod 20 is connected to the ring at the W-shaped crown 314 and the Y-shaped crown 316.
[0151] For the support structure 300, each ring 312 has 6 peaks or crests 311a and 6 troughs or valleys 311b. The peaks 311a are always followed by valleys 311b. Ring 312b has 12 crowns: 3 W-shaped crowns 309, 3 Y-shaped crowns 310, and 6 U-shaped crowns 307.
[0152] The crimp diameter applied to the stent structure 300 (using, for example, Method I or Method II) can be expressed as a theoretical minimum crimp diameter, where the struts converging on the same crown contact each other when the stent structure is fully crimped, i.e., when the stent structure is removed from the crimping device, or when it is deployed in a constraining sheath shortly after crimping. Under these conditions, the equation for the theoretical minimum crimp diameter (D-min) is as follows:
[0153] D-min = (1 / π) x [(n×strut_width) + (m×connecting_rod_width)] + 2*t
[0154] in
[0155] "n" is the number of struts in the ring (12 struts for stent structure 300),
[0156] "Strut_width" is the width of the struts (170 microns for scaffold structure 300),
[0157] "m" is the number of links connecting adjacent rings (3 for stent structure 300),
[0158] "Link_Width" is the width of the link (127 microns for scaffold structure 300), and
[0159] "t" is the wall thickness (93 microns for stent structure 300).
[0160] Therefore, for Figure 5 For the support structure 300, D-min = (1 / π) x [(12 x 170) + (3 x 127)] + 2 x (93) = 957 microns.
[0161] The above description of exemplary embodiments of the present invention, including the contents described in the Abstract, is not intended to be exhaustive or to limit the invention to the precise forms disclosed. Although specific embodiments and examples of the present invention are described in the present invention for illustrative purposes, those skilled in the relevant art will recognize that various modifications may be made within the scope of the invention.
[0162] These modifications can be made to the invention in light of the above detailed description.The terms used in the claims should not be construed to limit the invention to the specific embodiments disclosed in the specification.
Claims
1. A method for crimping a stent structure, comprising: using a scaffold made from a tube comprising a polymer, the polymer having a glass transition temperature, the scaffold having an outer diameter, and the outer diameter having a pre-crimp dimension; using a crimping device having a plurality of blades configured to form an aperture, wherein the blades rotate relative to each other during crimping to increase or decrease the size of the aperture; using a polymer material disposed within the pores; and The stent structure is crimped onto a balloon, wherein the crimping comprises: disposing the scaffold structure and the balloon within the aperture, wherein the polymer material is located between a surface of the scaffold structure and a surface of the blade, reducing the outer diameter of the stent structure from the pre-crimping size to a first size when the balloon has a first pressure, resetting the polymer material when the stent structure has the first size and the balloon has a second pressure, reducing the outer diameter of the stent structure from the first size to a second size when the balloon has the first pressure, and The polymer material is reset when the stent structure has the second size and the balloon has the second pressure.
2. The method according to claim 1, wherein: The second pressure is between 1 atmosphere (1 atm) and 4 atmospheres (4 atm) or 50% of the nominal balloon pressure.
3. The method according to claim 1, wherein: The stent structure is a thin wall stent structure, and the first pressure is the rated burst pressure of the balloon, or 200-300 psi.
4. The method according to claim 1, wherein: The crimping device is a film-headed crimper.
5. The method according to claim 1, wherein: The polymer material is a polymer sheet.
6. The method according to claim 1, wherein: The polymer material comprises a sheath.
7. The method according to claim 1, wherein: The stent structure has a crimping temperature during the crimping process.
8. The method according to claim 1, wherein: The balloon has a nominal diameter, and wherein the pre-crimped dimension is greater than the nominal diameter.
9. The method according to claim 1, wherein the curling step further comprises the following steps: After the scaffold structure is reduced in diameter to the first size, the scaffold structure and balloon are removed from the crimping device and then the scaffold structure is returned to the crimping device.
10. The method according to claim 9, wherein: When the scaffold structure and balloon are removed from the crimping device, the resetting of the polymer material occurs while the scaffold structure has the first dimension.
11. The method according to claim 9, wherein: The balloon is a first balloon, and the method further comprises the steps of replacing the first balloon with a second balloon of a balloon catheter and crimping the stent structure to the second balloon when the stent structure is removed from the crimping device.
12. The method according to claim 9, wherein: The scaffold structure diameter is reduced from the pre-crimping diameter to the first size using a first crimping device, and the scaffold structure diameter is reduced from the first size to the second size using a second crimping device.
13. The method according to claim 1, wherein: The polymer material within the hole is reset more than two times during the curling process.
14. The method according to claim 1, wherein: The apertures are held constant for a dwell time between 1 second and 25 seconds before and after reducing the scaffold structure diameter from the first size to the second size.
15. A method for crimping a stent structure, comprising: using a stent structure made from a tube comprising a polymer, the polymer having a glass transition temperature, the stent structure having an outer diameter, and the outer diameter having a pre-crimp dimension; Use a balloon with a nominal diameter; Using a polymer material disposed within the aperture of a crimping device; and using the crimping device having a plurality of blades configured to form the aperture, wherein the blades rotate relative to each other during the crimping process to increase or decrease the size of the aperture; and The stent structure is crimped onto the balloon, wherein the crimping comprises: disposing the stent structure and the balloon in the hole, When the balloon has a first pressure, the outer diameter of the support structure is reduced from the pre-crimping size to a first size, the first size being 30% to 35% smaller than the pre-crimping size, and after the outer diameter is reduced to the first size and the balloon has a second pressure, the pore size is increased to eliminate the pressure of the leaves from the surface of the support structure, and then excess polymer material is removed from the pores.
16. A method for crimping a stent structure, comprising: using a stent structure made from a tube comprising a polymer, the polymer having a glass transition temperature, the stent structure having an outer diameter, and the outer diameter having a pre-crimp dimension; Use a balloon with a nominal diameter; using a crimping device having a plurality of blades configured to form an aperture; using a polymer material disposed within the pores; and The stent structure is crimped onto the balloon, wherein the crimping comprises: disposing the support structure and the balloon within the aperture so that the polymer material is located between the support structure surface and the blade surface, reducing the outer diameter of the stent structure from the pre-crimping size to a second size, wherein the polymer material within the pores is repositioned 2 to 5 times while reducing the stent structure diameter from the pre-crimping size to the second size; and Wherein, when the diameter of the stent structure is reduced, the balloon has a first pressure, and when the polymer material is reset, the balloon has a second pressure.
17. The method according to claim 16, wherein: The polymer material comprises sheaths having different sizes.
18. The method according to claim 16, wherein: The polymer material is a sheet material that is handled by a film head crimper.
19. The method according to claim 16, wherein: The scaffold structure comprises struts forming rings, wherein adjacent rings are connected to each other by at least two links, and the scaffold structure is crimped to a theoretical minimum crimp size (D-min): D-min = (1 / π)× [(n×support_width) + (m×connecting_width)] + 2*t in "n" is the number of rods in the ring, "Strut_Width" is the width of the strut, "m" is the number of links connecting adjacent rings, "connecting_rod_width" is the width of the connecting rod, and "t" is the wall thickness.
Citation Information
Patent Citations
Polymeric Stent
US20100004735A1
Uniform Crimping and Deployment Methods for Polymer Scaffold
US20130255853A1
Method of Uniform Crimping and Expansion of Medical Devices
US20140096357A1
Crimping polymer scaffolds
US20160081824A1
Crimping methods for thin-walled scaffolds
CN110290914A