Method for forming FinFET stacked gate memory

Through the formation method of FinFET stacked gate memory, including the processing of nitride layer, floating gate structure and oxide-nitride-oxide layer, the problems of difficulty in channel length scaling and poor reliability of stacked gate memory are solved, and high efficiency is achieved. The current is maintained and the density increases.

CN112786598BActive Publication Date: 2024-10-22INTEGRATED SILICON SOLUTION INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010776012.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-03-11
Filing Date
2020-08-05
Publication Date
2024-10-22
Estimated Expiration
2040-08-05

AI Technical Summary

Technical Problem

It is difficult to scale the channel length of stacked gate memory to less than 120 nanometers with existing technology, resulting in short channel effect and current loss, poor reliability, and limited maximum current, which affects the read limit.

Method used

By forming a nitride layer, removing part of the nitride layer, forming a floating gate structure, setting an oxide-nitride-oxide layer, and removing non-memory cell area layers, a FinFET stacked gate memory is formed to increase the effective channel width to improve reliability. .

Benefits of technology

It achieves improved reliability of FinFET stacked-gate memory that scales below 120 nanometers, avoids the problems of current loss and insufficient reliability, maintains appropriate memory cell current, and increases density.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112786598B_ABST
    Figure CN112786598B_ABST
Patent Text Reader

Abstract

A method for forming a FinFET stacked gate memory, the method comprising a nitride layer forming step, a removal step, a floating gate structure forming step, an oxide-nitride-oxide layer setting step, a removal step, and a control gate structure forming step. In the nitride layer step, the nitride layer is formed in a memory cell area. In the removal step, a portion of the nitride layer is removed. In the floating gate structure forming step, a first polysilicon is set to form a floating gate structure. In the oxide-nitride-oxide layer setting step, an oxide-nitride-oxide layer is set. In the removal step, a portion of the oxide-nitride-oxide layer is removed. In the control gate structure forming step, a second polysilicon is set to form a control gate structure. Therefore, it helps to improve the current stability of the FinFET stacked gate memory.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a stacked gate memory and a method for forming the same, and in particular to a FinFET stacked gate memory and a method for forming the same. Background Art

[0002] Figure 8 FIG. 2 shows a schematic diagram of a stacked memory 30 according to the prior art. Figure 8 It can be seen that in a high temperature furnace at 1000 degrees Celsius, a silicon oxide layer (SiO2) 31 is grown on a P-type silicon wafer 32, and a thickness of the silicon oxide layer 31 is about 200 angstroms. Then, a deep N-well, an N-well and a P-well are formed by mask and implant. A silicon nitride (Si3N4) layer 33 is deposited with a thickness of about 2000 angstroms, a photoprinting active area (AA) is applied to the transistor, and a silicon nitride / silicon oxide / silicon stacked structure is etched in sequence.

[0003] However, in the prior art, it is difficult to achieve the technology of scaling the channel length of the stacked gate memory 30 to less than 120 nanometers, because when the size is scaled, a short channel effect will be caused, which will increase the difficulty of size scaling, wherein the short channel effect includes a memory cell punch-through effect and a hot carrier injection, and therewith significant current loss and reliability issues. Further, because the effective channel width of the stacked gate memory 30 is less than 80 nanometers, the maximum current of the stacked gate memory 30 is limited. Furthermore, the limit value of the maximum current is less than 20 microamperes, and this causes difficulty in reading the limit. In other words, when the value of the read limit is small, it will lead to poor product reliability. Therefore, developing a FinFET stacked gate memory that can be scaled to less than 120 nanometers and has stable reliability has become an important and urgent problem to be solved in the industry. Summary of the invention

[0004] The present disclosure provides a method for forming a FinFET stacked gate memory, which improves the reliability of the FinFET stacked gate memory by increasing the effective channel width.

[0005] According to an embodiment of the present disclosure, a method for forming a FinFET stacked gate memory is provided, comprising a step of forming a nitride layer, a step of removing, a step of forming a floating gate structure, a step of setting an oxide-nitride-oxide layer, a step of removing, and a step of forming a control gate structure. In the step of forming a nitride layer, a nitride layer is formed in a memory cell region of a memory structure having a shallow trench isolation structure. In the step of removing, a portion of the nitride layer is removed, another portion of the nitride layer is the nitride layer that is not removed, another portion of the nitride layer is located below a surface of a substrate and a bottom of the shallow trench isolation structure, a shallow trench isolation oxide is disposed inside the shallow trench isolation structure, and a sidewall region is formed on a portion of the nitride layer by a plasma etching process. In the step of forming a floating gate structure, a tunnel oxide is disposed on a surface of the substrate and a surface of another portion of the nitride layer, and a first polysilicon is disposed on the tunnel oxide of the memory cell region and a surface of the substrate of a non-memory cell region of the memory structure to form a floating gate structure. In the step of setting the oxide-nitride-oxide layer, a portion of the shallow trench isolation oxide is removed, and an oxide-nitride-oxide layer is set on a surface of the floating gate structure, a surface of another portion of the nitride layer, and a surface of another portion of the shallow trench isolation oxide, wherein the other portion of the shallow trench isolation oxide is not removed when a portion of the shallow trench isolation oxide is removed in the memory cell area. In the step of removing, a portion of the oxide-nitride-oxide layer is removed in the non-memory cell area of ​​the memory structure. In the step of forming a control gate structure, a portion of the floating gate structure is removed in the non-memory cell area of ​​the memory structure, a second polysilicon is set on a surface of the oxide-nitride-oxide layer in the memory cell area and is set on the surface of the substrate and a surface of the shallow trench isolation oxide in the non-memory cell area of ​​the memory structure to form a control gate structure, and a FinFET stacked gate memory is formed. The tunneling oxide is set inside the sidewall region, the surface of the substrate, and the surface of another portion of the nitride layer.

[0006] According to the method for forming the FinFET stacked gate memory of the above-mentioned embodiment, the nitride layer can be made of silicon nitride.

[0007] According to the method for forming the FinFET stacked gate memory of the above-mentioned embodiment, the substrate can be made of silicon.

[0008] According to the method for forming a FinFET stacked gate memory of the embodiment described in the previous paragraph, in the removing step, a portion of the nitride layer is removed, and a thickness of the removed layer may be 300 angstroms to 1400 angstroms.

[0009] According to the method for forming a FinFET stacked gate memory of the embodiment described in the previous paragraph, in the step of providing an oxide-nitride-oxide layer, a portion of the shallow trench isolation oxide may be removed by a solution, and the solution may contain hydrofluoric acid.

[0010] According to the method for forming the FinFET stacked gate memory of the embodiment described in the previous paragraph, before the step of forming the control gate structure, a portion of the floating gate structure may be removed by an etching process.

[0011] According to the method for forming the FinFET stacked gate memory of the embodiment described in the previous paragraph, in the step of forming the nitride layer, the nitride layer in the non-memory cell region of the memory structure can be removed by an etching process.

[0012] According to the method for forming the FinFET stacked gate memory of the embodiment described in the previous paragraph, in the removal step, the shallow trench isolation oxide can be disposed in the shallow trench isolation structure by a chemical vapor deposition process.

[0013] According to the method for forming a FinFET stacked gate memory of the embodiment described in the previous paragraph, in the step of forming a floating gate structure, the floating gate structure may be subjected to a chemical mechanical polishing process to form a fin-shaped floating gate structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 A flowchart showing a method for forming a FinFET stacked gate memory according to an embodiment of the present invention is shown;

[0015] Figure 2 Show Figure 1 A schematic diagram of a step of forming a nitride layer in an embodiment;

[0016] Figure 3 Show Figure 1 A schematic diagram of a removal step in an embodiment;

[0017] Figure 4 Show Figure 1 A schematic diagram of a step of forming a floating gate structure in an embodiment;

[0018] Figure 5 Show Figure 1 A schematic diagram of a step of providing an oxide-nitride-oxide layer in an embodiment;

[0019] Figure 6 Show Figure 1 A schematic diagram of a removal step in an embodiment;

[0020] Figure 7 Show Figure 1 A schematic diagram of a step of forming a control gate structure in an embodiment; and

[0021] Figure 8 A schematic diagram of a stacked memory according to the prior art is shown.

[0022] Description of reference numerals:

[0023] 100: Formation method of FinFET stacked gate memory

[0024] S101: Step of forming a nitride layer

[0025] S102: Removal Step

[0026] S103: Step of forming a floating gate structure

[0027] S104: Step of setting oxide-nitride-oxide layer

[0028] S105: Removal Step

[0029] S106: Forming a control gate structure Step 200: FinFET stacked gate memory

[0030] 210: Substrate

[0031] 211: Thin oxide layer

[0032] 220: Shallow Trench Isolation Structure

[0033] 221: Shallow Trench Isolation Oxide

[0034] 230: Storage unit area

[0035] 231: Nitride layer

[0036] 232: Tunneling oxide

[0037] 233: Floating gate structure

[0038] 234: Oxide-Nitride-Oxide Layer

[0039] 235: Control gate structure

[0040] 240: Non-storage unit area

[0041] 241: High Voltage N-Channel Logic Device

[0042] 242: Low Voltage N-Channel Logic Device

[0043] 243: High Voltage P-Channel Logic Device

[0044] 244: Low Voltage P-Channel Logic Device

[0045] 30: Stacked Gate Memory

[0046] 31: Silicon oxide layer

[0047] 32: P-type silicon wafer

[0048] 33: Silicon nitride layer DETAILED DESCRIPTION

[0049] Figure 1 FIG. 1 is a flow chart showing the steps of a method 100 for forming a FinFET stacked gate memory according to an embodiment of the present invention. Figure 1 It can be seen that the method 100 for forming a FinFET stacked gate memory includes a nitride layer forming step S101, a removal step S102, a floating gate structure forming step S103, an oxide-nitride-oxide layer setting step S104, a removal step S105 and a control gate structure forming step S106.

[0050] Figure 2 Show Figure 1 Schematic diagram of step S101 of forming a nitride layer in an embodiment. Figure 1 and Figure 2 It can be seen that a nitride layer 231 is formed in a memory cell area 230 of a memory structure (not shown) having a shallow trench isolation structure 220, and the nitride layer 231 can be a silicon nitride material, but is not limited thereto. Before the nitride layer forming step S101, the shallow trench isolation structure 220 can be formed by an etching process, and the depth of the shallow trench isolation structure 220 can be 2000 angstroms. In detail, the nitride layer 231 is formed on a thin oxide layer 211, and the thin oxide layer 211 is disposed on a substrate 210. The substrate 210 can be a silicon material. Before the removal step S102, the memory cell area 230 can be covered, and the nitride layer 231 in a non-memory cell area 240 can be removed by an etching process.

[0051] Figure 3 Show Figure 1 The schematic diagram of step S102 is removed in the embodiment. Figure 1 and Figure 3It can be seen that a portion of the nitride layer 231 is removed, another portion of the nitride layer 231 is the nitride layer 231 that is not removed, another portion of the nitride layer 231 is located below a surface of the substrate 210 and a bottom of the shallow trench isolation structure 220, and a shallow trench isolation oxide 221 is disposed inside the shallow trench isolation structure 220. Further, the thickness of the portion of the nitride layer 231 removed is 300 angstroms to 1400 angstroms, and a sidewall region is formed on a portion of the nitride layer 231 by a plasma etching process. It is worth mentioning that the depth of each sidewall region is similar. Specifically, the shallow trench isolation oxide 221 can be disposed inside the shallow trench isolation structure 220 by a chemical vapor deposition (CVD) process, and the shallow trench isolation oxide 221 is subjected to a chemical-mechanical polishing (CMP).

[0052] Figure 4 Show Figure 1 Schematic diagram of step S103 of forming a floating gate structure in an embodiment. Figure 1 and Figure 4 It can be seen that a tunnel oxide 232 is disposed on the surface of the substrate 210 and a surface of another portion of the nitride layer 231, and a first polysilicon is disposed on the tunnel oxide 232 of the memory cell area 230 and the surface of the substrate 210 of a non-memory cell area 240 of the memory structure to form a floating gate structure 233. In detail, at 300 degrees Celsius to 800 degrees Celsius, the first polysilicon is disposed on the tunnel oxide 232 by a plasma process or a chemical vapor deposition process, and the floating gate structure 233 is formed into a fin-shaped floating gate structure by chemical mechanical polishing. In the removal step S102, the tunnel oxide 232 is disposed inside the sidewall region. Therefore, it can help to increase an effective memory cell channel width.

[0053] Figure 5 Show Figure 1 Schematic diagram of step S104 of providing an oxide-nitride-oxide layer in an embodiment. Figure 1 and Figure 5It can be seen that a portion of the shallow trench isolation oxide 221 is removed, and an oxide-nitride-oxide layer 234 is disposed on a surface of the floating gate structure 233, a surface of another portion of the nitride layer 231, and a surface of another portion of the shallow trench isolation oxide 221, wherein the other portion of the shallow trench isolation oxide 221 is not removed when a portion of the shallow trench isolation oxide 221 is removed in the memory cell area 230. Specifically, a mask is used to remove a portion of the shallow trench isolation oxide 221 in the memory cell area 230, and a portion of the shallow trench isolation oxide 221 is removed by a solution, and the solution contains a hydrofluoric acid. After removing a portion of the shallow trench isolation oxide 221, a photoresist is removed, and the oxide-nitride-oxide layer 234 is deposited by a chemical vapor deposition process at 350 degrees Celsius to 800 degrees Celsius.

[0054] Figure 6 Show Figure 1 The schematic diagram of step S105 is removed in the embodiment. Figure 1 and Figure 6 It can be seen that a portion of the oxide-nitride-oxide layer 234 is removed in the non-memory cell region 240 of the memory structure.

[0055] Figure 7 Show Figure 1 Schematic diagram of step S106 of forming a control gate structure in an embodiment. Figure 1 and Figure 7 It can be seen that a portion of the floating gate structure 233 is removed in the non-memory cell area 240 of the memory structure, a second polysilicon is arranged on a surface of the oxide-nitride-oxide layer 234 in the memory cell area 230 and is arranged on a surface of the substrate 210 and a surface of the shallow trench isolation oxide 221 in the non-memory cell area 240 of the memory structure to form a control gate structure 235, and a FinFET stacked gate memory 200 is formed.

[0056] Depend on Figure 6 and Figure 7 It can be seen that the mask is used to cover the memory cell region 230, and the oxide-nitride-oxide layer 234 and the floating gate structure 233 disposed in the non-memory cell region 240 are removed by an etching process to reserve space for multiple peripheral devices. Further, it is beneficial to form source / drain junctions for the memory cell region 230 and the peripheral devices, and to form contacts / metal connection points to achieve appropriate electrical connection strength.

[0057] By using the method for forming the FinFET stacked gate memory of the present invention, the channel width can be maintained at a size scaled to less than 120 nanometers, and the effective channel width can be increased. Furthermore, the problem of excessive current loss and insufficient reliability can be avoided, and the current of the appropriate memory cell can be maintained. Furthermore, the size limit of the FinFET stacked gate memory can be reduced, so the density of the FinFET stacked gate memory can be increased.

[0058] Depend on Figure 7 It can be known that the FinFET stacked gate memory 200 of the present invention includes a substrate 210 , a shallow trench isolation structure 220 , a memory cell region 230 and a non-memory cell region 240 .

[0059] Specifically, the STI structure 220 is disposed on the substrate 210 and includes a STI oxide 221. The STI oxide 221 is disposed on the STI structure 220 and can be made of silicon oxide and have a thickness of 600 angstroms to 2400 angstroms.

[0060] The memory cell region 230 includes a nitride layer 231, a tunnel oxide 232, a floating gate structure 233, an oxide-nitride-oxide layer 234 and a control gate structure 235. The nitride layer 231 is disposed below a surface of the shallow trench isolation structure 220 and the surface of the substrate 210. The tunnel oxide 232 is disposed on the substrate 210, and the tunnel oxide 232 can be made of silicon oxide, and the thickness of the tunnel oxide 232 can be 70 angstroms to 105 angstroms. It is worth mentioning that the optimal thickness of the tunnel oxide 232 is 95 angstroms, but it is not limited thereto. The floating gate structure 233 is disposed on the tunnel oxide 232. The oxide-nitride-oxide layer 234 is disposed between the floating gate structure 233 and the shallow trench isolation oxide 221, and the shallow trench isolation oxide 221 is disposed between the oxide-nitride-oxide layer 234 and the nitride layer 231. The control gate structure 235 is disposed in the oxide-nitride-oxide layer 234, and the oxide-nitride-oxide layer 234 is located between the floating gate structure 233 and the control gate structure 235. Specifically, the thickness of the floating gate structure 233 is 1000 angstroms, the thickness of the oxide-nitride-oxide layer 234 is 65 angstroms / 80 angstroms / 65 angstroms, and the thickness of the control gate structure 235 is 2000 angstroms, but the present invention is not limited thereto.

[0061] In detail, the oxide-nitride-oxide layer 234 may be made of silicon oxide / silicon nitride / silicon oxide. Furthermore, silicon nitride may be replaced by a high-k insulating material such as aluminum oxide, zirconium oxide, hafnium oxide, titanium dioxide, or strontium titanate. Therefore, the oxide-nitride-oxide layer 234 may also be made of silicon oxide / aluminum oxide / silicon oxide, silicon oxide / zirconium oxide / silicon oxide, silicon oxide / hafnium oxide / silicon oxide, silicon oxide / titanium dioxide / silicon oxide, or silicon oxide / strontium titanate / silicon oxide, but is not limited thereto.

[0062] The non-memory cell region 240 is connected to the memory cell region 230 and includes a plurality of peripheral devices. In further detail, the memory cell region 230 is electrically isolated from the non-memory cell region 240, so that no short circuit occurs between the memory cell region 230 and the non-memory cell region 240. In detail, the peripheral devices include a high voltage N-type channel (HVN) logic device 241, a low voltage N-type channel (LVN) logic device 242, a high voltage P-type channel (HVP) logic device 243, and a low voltage P-type channel (LVP) logic device 244.

[0063] Furthermore, a triple P-well (not shown) is located in a deep N-well (not shown) of the substrate 210 in the memory cell region 230, and a P-well (P-well) (not shown) is located next to an N-well (N-well) (not shown) of the substrate 210 in the non-memory cell region 240.

[0064] By using the FinFET stacked gate memory of the present invention, the effective memory cell channel width can be increased, the size of the memory structure can be further reduced, and the current of the FinFET stacked gate memory can be maintained unchanged.

[0065] Although the present invention has been disclosed as above by way of embodiments, it is not intended to limit the present invention. Any person skilled in the art may make slight changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be determined by the claims.

Claims

1. A method for forming a FinFET stacked gate memory, characterized in that: Include: a step of forming a nitride layer, wherein a nitride layer is formed in a memory cell region of a memory structure having a shallow trench isolation structure; a removal step, wherein a portion of the nitride layer is removed, another portion of the nitride layer is the nitride layer that is not removed, the other portion of the nitride layer is located below a surface of a substrate and a bottom of the shallow trench isolation structure, a shallow trench isolation oxide is disposed inside the shallow trench isolation structure, and a sidewall region is formed on the portion of the nitride layer by a plasma etching process; a step of forming a floating gate structure, wherein a tunnel oxide is disposed on a surface of the substrate and a surface of the other portion of the nitride layer, and a first polysilicon is disposed on the tunnel oxide in the memory cell region and the surface of the substrate in a non-memory cell region of the memory structure to form a floating gate structure; a step of disposing an oxide-nitride-oxide layer, wherein a portion of the shallow trench isolation oxide is removed, and an oxide-nitride-oxide layer is disposed on a surface of the floating gate structure, a surface of another portion of the nitride layer, and a surface of another portion of the shallow trench isolation oxide, wherein the other portion of the shallow trench isolation oxide is not removed when the portion of the shallow trench isolation oxide is removed in the memory cell region; a removing step, wherein a portion of the oxide-nitride-oxide layer is removed in the non-memory cell region of the memory structure; as well as a step of forming a control gate structure, wherein a portion of the floating gate structure is removed in the non-memory cell region of the memory structure, a second polysilicon is disposed on a surface of the oxide-nitride-oxide layer in the memory cell region and is disposed on the surface of the substrate and a surface of the shallow trench isolation oxide in the non-memory cell region of the memory structure to form a control gate structure, and a FinFET stacked gate memory is formed; The tunnel oxide is arranged inside the sidewall region, on the surface of the substrate and on the surface of the other part of the nitride layer.

2. The method for forming a FinFET stacked gate memory according to claim 1, wherein: The nitride layer is made of silicon nitride.

3. The method for forming a FinFET stacked gate memory according to claim 1, wherein: The substrate is made of silicon.

4. The method for forming a FinFET stacked gate memory according to claim 1, wherein: In the removing step, the portion of the nitride layer is removed, and a thickness of the removed portion is 300 angstroms to 1400 angstroms.

5. The method for forming a FinFET stacked gate memory according to claim 1, wherein: In the step of providing the oxide-nitride-oxide layer, the portion of the shallow trench isolation oxide is removed by a solution, and the solution contains hydrofluoric acid.

6. The method for forming a FinFET stacked gate memory according to claim 1, wherein: Before the step of forming the control gate structure, the portion of the floating gate structure is removed by an etching process.

7. The method for forming a FinFET stacked gate memory according to claim 1, wherein: In the step of forming the nitride layer, the nitride layer in the non-memory cell region of the memory structure is removed by an etching process.

8. The method for forming a FinFET stacked gate memory according to claim 1, wherein: In the removing step, the shallow trench isolation oxide is disposed in the shallow trench isolation structure by a chemical vapor deposition process.

9. The method for forming a FinFET stacked gate memory according to claim 1, wherein: In the step of forming the floating gate structure, the floating gate structure is subjected to a chemical mechanical polishing process to form a fin-shaped floating gate structure.