A composite warp knitted fabric for nurse uniform and production method thereof

Through the design of three-layer warp knitted fabric and knitting dyeing and finishing process, combined with conductive composite yarn and antibacterial deodorant, the problem of insufficient functionality of existing nurse uniform fabrics is solved, achieving high density, non-see-through, multiple functionality and comfort performance High quality nurse uniform fabric, suitable for the daily wearing needs of medical staff.

CN113046906BActive Publication Date: 2024-10-25QUANZHOU HAITIAN MATERIAL TECH CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110381530.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-04-09
Publication Date
2024-10-25
Estimated Expiration
2041-04-09

AI Technical Summary

Technical Problem

Existing nurse uniform fabrics lack antibacterial, antistatic, waterproof, antifouling, oil-repellent and other functions, and are insufficient in comfort performance and cannot meet the needs of medical staff for being light, soft, and breathable.

Method used

Designed with a three-layer structure of warp knitted fabric, the front comb is woven from fine-denier, different-section low-elastic chemical fiber filaments, the middle comb is woven from low-elastic chemical fiber filaments and conductive composite yarns, and the back comb is woven from low-elastic chemical fiber filaments, combined with knitting In the weaving process, dyeing and finishing process, antibacterial deodorants and three-proof finishing agents are added, and the multiple functionalities and comfort properties of the fabric are achieved by optimizing the fabric structure and process parameters.

Benefits of technology

A high-density non-see-through fabric has been achieved, which has good moisture permeability, antibacterial, antistatic, waterproof, antifouling, and oil-repellent functions. It feels soft and has a simple preparation process, making it suitable for summer use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113046906B_ABST
    Figure CN113046906B_ABST
Patent Text Reader

Abstract

The present invention relates to a composite warp knitted fabric for nurse uniforms and a production method thereof, comprising a fabric body treated with antibacterial, waterproof, oil-repellent and anti-fouling treatments, wherein the fabric body comprises a front comb, a middle comb and a back comb, wherein the front comb is woven from fine denier low-elastic chemical fiber filaments with different cross sections, the middle comb is woven from low-elastic chemical fiber filaments and conductive composite yarns, and the back comb is woven from low-elastic chemical fiber filaments. The present invention has good wearing properties such as moisture permeability, soft hand feeling, dimensional stability, and anti-pilling, and the front comb yarn is preferably non-circular polyester filaments with different cross sections, and the front comb yarn is used to be on the surface of the fabric, so that the fabric forms a good moisture conduction ability, and the fabric has good moisture permeability, the middle comb weaves a chain-less padding organization, and the chain organization is used to make the coil stand upright, the fabric has good longitudinal structural stability, and the texture is clear, and the back comb selects a light network structure polyester filament to weave a warp velvet organization, and the back comb has a longer extension line in the middle of the fabric to improve the fabric density and soft hand feeling.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of knitted fabrics, and in particular to a composite warp knitted fabric for nurses' uniforms and a production method thereof. Background Art

[0002] The outbreak of the COVID-19 pandemic at the beginning of 2020 has made the whole society pay more attention to the safety and protection of medical staff. Isolation suits used by medical staff, clothing worn in daily work, surgical clothing, etc., have quickly become one of the research and development hotspots in the field of medical textiles. Existing nurses' clothing fabrics are generally made of polyester-cotton blended raw materials, and are prepared by woven weaving processing. The fabric is wide, does not shrink, and is opaque, which is convenient for cleaning and disinfection, but generally does not have the protective functions such as antibacterial and antibacterial, and the comfortable performance such as moisture conduction and moisture permeability in summer. According to the questionnaire survey results of the daily clothing worn by medical staff with doctors and nurses as the main research objects, medical staff have a certain demand for the style of daily clothing, and the demand for the comfortable performance such as light, soft, and breathable, as well as the functions of antibacterial, antistatic, waterproof, antifouling, and oil repelling is very strong. Based on this, the inventor has developed a nurse's warp knitted fabric with good wearing comfort performance and functions such as moisture permeability, antibacterial, antistatic, waterproof, antifouling, and oil repelling, and the preparation process is simple, suitable for the clothing fabrics used by medical staff such as nurses and doctors for daily wear. Summary of the invention

[0003] The purpose of the present invention is to address the above shortcomings and provide a composite warp-knitted fabric for nurse uniforms that has good wearing comfort properties and functions such as moisture permeability, antibacterial, antistatic, waterproof, antifouling and oil repellency.

[0004] The solution adopted by the present invention to solve the technical problem is: a composite warp-knitted fabric for nurse uniforms, comprising a fabric body treated with antibacterial, waterproof, oil-repellent and anti-fouling treatments, the fabric body comprising a front comb, a middle comb and a back comb, the front comb being woven from fine-denier low-elastic chemical fiber filaments with different cross-sections, the middle comb being woven from low-elastic chemical fiber filaments and conductive composite yarns, and the back comb being woven from low-elastic chemical fiber filaments.

[0005] Furthermore, in order to ensure that the fabric is not transparent, has a good hand feel, has good longitudinal structural stability, and has clear texture, a nurse skirt for summer can be made; the front comb is a warp plain structure, the middle comb is a braided chain-less pad structure, and the back comb is a warp velvet structure.

[0006] Furthermore, in order to blend the conductive composite yarn, make the fabric have anti-static function, and ensure the tightness of the fabric structure; the warp arrangement ratio of the low-elastic chemical fiber filament and the conductive composite yarn is 24:1.

[0007] Furthermore, the front comb is located on the surface of the fabric, in order to enable the fabric to form better moisture conductivity, ensure good moisture permeability, and improve the soft feel of the fabric; the front comb is woven with 75D / 72F low-elastic polyester filaments with non-circular cross-section and light network structure.

[0008] Furthermore, in order to ensure the tightness of the fabric structure and to ensure that the fabric has anti-static function, the middle comb is woven with low-elastic polyester filaments with a 75D / 36F circular cross-section and a light network structure and 70D conductive composite yarn.

[0009] Furthermore, in order to make the back comb have a longer extension line, thereby improving the fabric density and softness of the hand feel; the back comb is woven with low-elastic polyester filaments with a 75D / 36F circular cross-section and a light network structure.

[0010] In view of the above shortcomings, the present invention also provides a method for producing a composite warp-knitted fabric for nurse uniforms which has simple process and good wearing comfort properties and functions such as moisture permeability, antibacterial, antistatic, waterproof, antifouling and oil repellency.

[0011] Another solution adopted by the present invention to solve the technical problem is: a production method of a composite warp knitted fabric for nurse uniforms, including a knitting and weaving process and a dyeing and finishing process.

[0012] The knitting weaving process comprises: using fine-denier low-elastic chemical fiber filaments with different cross-sections to weave a warp plain structure as the front comb of the warp knitted fabric, using low-elastic chemical fiber filaments and conductive composite yarns in a warp-through arrangement ratio of 24:1 to weave a chain-lacked pad structure as the middle comb of the warp knitted fabric, and using low-elastic chemical fiber filaments to weave a warp pile structure as the back comb of the warp knitted fabric;

[0013] The dyeing and finishing process includes: cloth sorting process → edge binding process → scouring and degreasing process → hot washing and cold washing process → whitening and dyeing process → cleaning process → drainage process → dehydration process → slitting process → drying process → finished product padding and shaping process.

[0014] Furthermore, in order to ensure the moisture permeability, anti-static performance and tightness of the fabric; the front comb is woven with 75D / 72F low-elastic polyester filaments with a non-circular cross-section and a light network structure, the middle comb is woven with 75D / 36F low-elastic polyester filaments with a circular cross-section and a light network structure and 70D conductive composite yarn, and the back comb is woven with 75D / 36F low-elastic polyester filaments with a circular cross-section and a light network structure.

[0015] Furthermore, in order to make the fabric have antibacterial, antibacterial and deodorizing functions; in the dyeing and finishing process, the whitening and dyeing process is:

[0016] Auxiliary solution is used in a dyeing machine to perform whitening and antibacterial finishing in one bath and one step, and the auxiliary solution formula is selected as follows: 0.09-0.11% of the fabric weight ratio of whitening agent SBV, 0.30-0.35% of the fabric weight ratio of whitening agent CPS-D, 0.8-1.2% of the fabric weight ratio of antibacterial deodorant, 1.98-2.02% of the fabric weight ratio of high temperature leveling agent TF212E, 1.0-1.5% of the fabric weight ratio of bath softener SF-66, 0.18-0.22% of the fabric weight ratio of acetic acid and 1.6-2.0% of the fabric weight ratio of detergent;

[0017] According to the bath ratio of 1:13-15, cold water is injected into the L-type high-temperature and high-pressure jet overflow dyeing machine, and the diluted auxiliary solution is gradually added into the dyeing machine from the additional cylinder of the dyeing machine. After running at room temperature for 5 minutes, the fabric is put in, and the evenly dispersed diluted brightener solution is added from the additional cylinder. After running for 3 minutes, the pH value of the dyeing solution is controlled to be 3.5-4.2, and the temperature is raised to 80°C at 2.5°C / min, kept warm for 5 minutes, and then raised to 110°C at 1.0°C / min, kept warm for 5 minutes, and then raised to 130°C at 1.0°C / min, kept warm for 30 minutes; then the temperature is lowered to 120°C at 2.0°C / min and kept warm for 5 minutes , cool down to 110℃ at 1.0℃ / min and keep warm for 5 minutes, then cool down to 80℃ at 1.5℃ / min, take samples for color matching, overflow wash to below 60℃ and drain, then add water according to the bath ratio of 1:10-12, heat to 60℃ at 3.5-4.0℃ / min, keep warm for 10 minutes and drain, cold wash and drain, then add water according to the bath ratio of 1:10-12, start the main pump to circulate the fabric in the dyeing machine, dilute and stir the detergent in the additional cylinder, then gradually add it into the dyeing machine, heat to 70℃ at 3.5-4.0℃ / min, keep warm for 20 minutes and drain out of the cylinder, dry the fabric to obtain a semi-finished product.

[0018] Furthermore, in order to make the fabric have good waterproof, antifouling and oil-repellent functions; in the dyeing and finishing process, the finished product padding and shaping process is:

[0019] A ten-box knitted fabric opening setting machine is used for padding setting, wherein the padding solution formula used is 50-60g / L of three-proofing additives, 13-15g / L of cross-linking agent and 4-5g / L of penetrant, and the pH value of the padding solution is adjusted to 4.0-5.0 with acetic acid.

[0020] Through the front padder of the ten-box knitted fabric opening and setting machine, a one-immersion-one-paving method is adopted, and the prepared padding solution is dipped and rolled at room temperature, and the liquid content of the cloth surface is 70-75%; the setting temperature of the ten-box knitted fabric opening and setting machine is controlled to be 180℃-190℃, the air volume is 1800-2000 revolutions / minute, and the machine speed is 10-15 meters / minute for padding and setting.

[0021] Compared with the prior art, the present invention has the following advantages:

[0022] (1) The fabric woven by the present invention is high-density and non-transparent, and adopts 75D low-elastic network structure polyester filament to weave three-comb full-thread warp knitted fabric on a warp knitting machine with a higher machine number, with the front comb warp flat, the middle comb weaving chain missing pad, and the back comb warp velvet. The appropriate warp let-off and fabric density are controlled to make the fabric weight per square meter 220g / m 2 The fabric has high density and is not transparent, so it can be used to make nurse skirts for summer;

[0023] (2) The present invention has good wearing properties such as moisture permeability, soft hand feeling, dimensional stability, and anti-pilling. The front combed yarn is preferably non-circular polyester filament with different cross-section. The front combed yarn is located on the surface of the fabric, so that the fabric has good moisture conductivity and good moisture permeability. Based on the fabric structure design, the front combed yarn is selected to fully wear the warp plain weave, and the characteristic of the front combed yarn being easily exposed on the surface of the fabric is used again to improve the soft hand feeling of the fabric by the fine denier fiber. The middle combed and back combed yarns are selected to use light network structure polyester filaments, and the middle combed yarn is woven with a chain-like lacking pad weave. The chain-like weave is used to make the coils stand upright, and the longitudinal structure of the fabric is stable and has a clear texture. The lacking pad weave is used to make the fabric structure more compact. The back combed yarn is selected to use light network structure polyester filaments to weave a warp pile weave, and the longer extension line of the back combed yarn in the middle of the fabric has the effect of increasing the fabric density and soft hand feeling; the shorter extension line of the front combed yarn covers the middle combed yarn and the back combed yarn, so that the fabric structure is stable, has a good refreshing feeling, and has excellent anti-pilling performance;

[0024] (3) The present invention has multiple functions such as antibacterial, antistatic, waterproof, antifouling, and oil repellent. In the post-finishing process, by adding an antibacterial and deodorizing finishing agent during whitening and dyeing, and by optimizing the whitening auxiliary agent and the antibacterial finishing agent in the same bath process technology, the fabric has an antibacterial function. In the fabric structure design, by introducing conductive composite yarns, using the middle combing yarn guide needles to arrange the conductive composite yarns at intervals, and combining the selection of chain braiding and missing pad tissue structures, the fabric obtains an excellent antistatic effect. In the fabric padding and shaping stage, the three-proof finishing agent is introduced, and the fabric has good waterproof, antifouling and oil repellent functions through the optimized padding process and shaping combination. The antibacterial, waterproof, antifouling and oil repellent functions are all added in the post-finishing stage. The fabric is obtained by optimizing the process parameters, and it still has good composite functions after multiple washings;

[0025] (4) The preparation process of the present invention is simple. The fabric can be woven on a single-needle-bed three-comb warp knitting machine. The dyeing and finishing process is short, and the preparation process is simple. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The present invention will be further described below with reference to the accompanying drawings in conjunction with embodiments:

[0027] Figure 1 It is a structural schematic diagram of the present invention.

[0028] In the picture: 1- front comb; 2- middle comb; 3- back comb. DETAILED DESCRIPTION

[0029] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments:

[0030] Example 1: Figure 1 As shown, this embodiment provides an ultra-light and cool double-sided weft-knitted fabric, including a fabric body treated with antibacterial, waterproof, oil-repellent and anti-fouling treatments, the fabric body including a front comb 1, a middle comb 2 and a back comb 3, the front comb 1 is woven from fine-denier low-elastic chemical fiber filaments with different cross-sections, the middle comb 2 is woven from low-elastic chemical fiber filaments and conductive composite yarns, and the back comb 3 is woven from low-elastic chemical fiber filaments. The front comb 1 uses 75D / 72F "cross" shaped low-elastic polyester filaments with different cross-sections and light network structures to fully penetrate, the middle comb 2 uses 75D / 36F low-elastic polyester filaments with light network structures and 70D conductive composite yarns to fully penetrate in a 24:1 manner, and the back comb 3 uses 75D / 36F low-elastic polyester filaments with light network structures to fully penetrate. On a warp knitting machine with a machine gauge of 28 needles / 25.4mm, press Figure 1 The yarn padding motion diagram shown in the figure weaves warp flat, chain-stitched and warp pile structures. The warp let-offs of the front comb 1, middle comb 2 and back comb 3 are 1410, 365 and 1590 respectively. The horizontal density of the fabric is 24 longitudinal lines / cm, the width of the machine is 152cm, and the weight per square meter is 161g / m 2 .

[0031] In this embodiment, in order to ensure that the fabric is not transparent, has a good hand feel, has good longitudinal structural stability, and has clear texture, a nurse skirt for summer can be made; the front comb 1 is a warp plain structure, the middle comb 2 is a chain-cut pad structure, and the back comb 3 is a warp velvet structure.

[0032] In this embodiment, in order to blend the conductive composite yarn, make the fabric have antistatic function and ensure the tightness of the fabric structure, the threading arrangement ratio of the low-elastic chemical fiber filament and the conductive composite yarn is 24:1.

[0033] In this embodiment, the front comb 1 is on the surface of the fabric. In order to make the fabric have better moisture conductivity, ensure good moisture permeability, and improve the soft feel of the fabric, the front comb 1 is woven with 75D / 72F low-elastic polyester filaments with non-circular cross-section and light network structure.

[0034] In this embodiment, in order to ensure the tightness of the fabric structure and to ensure that the fabric has an anti-static function, the middle comb 2 is woven from low-elastic polyester filaments with a 75D / 36F circular cross-section and a light network structure and 70D conductive composite yarn.

[0035] In this embodiment, in order to make the back comb 3 have a longer extension line, thereby improving the fabric density and softness of the hand feel; the back comb 3 is woven with low-elastic polyester filaments with a 75D / 36F circular cross-section and a light network structure.

[0036] Embodiment 2: A method for producing a composite warp knitted fabric for nurse uniforms, comprising a knitting and weaving process and a dyeing and finishing process.

[0037] The knitting weaving process comprises: using fine denier low-elastic chemical fiber filaments with different cross-sections to weave into a warp plain structure as a front comb 1 of the warp knitted fabric, using low-elastic chemical fiber filaments and conductive composite yarns to weave into a chain-lacked pad structure as a middle comb 2 of the warp knitted fabric according to a warp insertion ratio of 24:1, using low-elastic chemical fiber filaments to weave into a warp pile structure as a back comb 3 of the warp knitted fabric, the front comb 1 uses 75D / 72F "cross" shaped low-elastic polyester filaments with different cross-sections and light network structure to fully penetrate, the middle comb 2 uses 75D / 36F low-elastic polyester filaments with light network structure and 70D conductive composite yarns to fully penetrate in a 24:1 manner, and the back comb 3 uses 75D / 36F low-elastic polyester filaments with light network structure to fully penetrate, on a warp knitting machine with a machine number of 28 needles / 25.4mm, according to Figure 1 The yarn padding motion diagram shown in the figure weaves plain warp, chain-knitted missing pad, and warp pile. The warp let-offs of front comb 1, middle comb 2, and back comb 3 are 1410, 365, and 1590 respectively. The horizontal density of the fabric is 24 longitudinal lines / cm, the width of the machine is 152cm, and the weight per square meter is 161g / m 2 ;

[0038] The dyeing and finishing process includes: cloth sorting process → edge binding process → scouring and degreasing process → hot washing and cold washing process → whitening and dyeing process → cleaning process → drainage process → dehydration process → slitting process → drying process → finished product padding and shaping process.

[0039] In this embodiment, in order to ensure the moisture permeability, anti-static performance and tightness of the fabric; the front comb 1 is woven from 75D / 72F low-elastic polyester filaments with a non-circular cross-section and a light network structure, the middle comb 2 is woven from 75D / 36F low-elastic polyester filaments with a circular cross-section and a light network structure and 70D conductive composite yarn, and the back comb 3 is woven from 75D / 36F low-elastic polyester filaments with a circular cross-section and a light network structure.

[0040] In this embodiment, in order to make the fabric have antibacterial, antibacterial and deodorizing functions; in the dyeing and finishing process, the whitening and dyeing process is:

[0041] Auxiliary solution is used in a dyeing machine for one-bath one-step dyeing and finishing of whitening and antibacterial finishing, and the auxiliary solution formula is selected as follows: 0.105% of the fabric weight ratio of whitening agent SBV, 0.32% of the fabric weight ratio of whitening agent CPS-D, 1% of the fabric weight ratio of antibacterial deodorant, 2% of the fabric weight ratio of high temperature leveling agent TF212E, 1.5% of the fabric weight ratio of bath softener SF-66, 0.2% of the fabric weight ratio of acetic acid, and 1.8% of the fabric weight ratio of detergent;

[0042] According to the bath ratio of 1:13-15, cold water is injected into the L-type high-temperature and high-pressure jet overflow dyeing machine, and the diluted auxiliary solution is gradually added into the dyeing machine from the additional cylinder of the dyeing machine (the auxiliary solution is diluted at 1:10-50, the larger the amount, the smaller the proportion, and the smaller the amount, the larger the proportion). After running at room temperature for 5 minutes, put the fabric in, and add the evenly dispersed diluted brightener solution from the additional cylinder (the brightener SBV or brightener CPS-D or a mixture of the two brighteners is used as the brightener solution, and the brightener solution is diluted at 1:15-100, the larger the amount, the smaller the proportion, and the smaller the amount, the larger the proportion). After running for 3 minutes, the pH value of the dye solution is controlled to be 3.5-4.2, and the temperature is raised to 80°C at 2.5°C / min, kept warm for 5 minutes, and then raised to 110°C at 1.0°C / min, kept warm for 5 minutes, and then raised to 13 0℃, keep warm for 30 minutes; then cool down to 120℃ at 2.0℃ / min and keep warm for 5 minutes, cool down to 110℃ at 1.0℃ / min and keep warm for 5 minutes, cool down to 80℃ at 1.5℃ / min, take samples for color matching, overflow wash to below 60℃ and drain, then add water according to the bath ratio of 1:10-12, heat to 60℃ at 3.5-4.0℃ / min, keep warm for 10 minutes and drain, cold wash and drain, then add water according to the bath ratio of 1:10-12, start the main pump to circulate the fabric in the dyeing machine, dilute and stir the detergent in the additional cylinder, and then gradually add it into the dyeing machine (the detergent is diluted at 1:10-50, the larger the amount, the smaller the proportion), heat to 70℃ at 3.5-4.0℃ / min, keep warm for 20 minutes and drain out of the cylinder, and dry the fabric to obtain a semi-finished product.

[0043] In this embodiment, in order to make the fabric have good waterproof, anti-fouling and oil-repellent functions; in the dyeing and finishing process, the finished product padding and shaping process is:

[0044] A ten-box knitted fabric opening setting machine is used for padding setting, wherein the padding solution formula used is 50-60g / L of three-proofing additives, 13-15g / L of cross-linking agent and 4-5g / L of penetrant, and the pH value of the padding solution is adjusted to 4.0-5.0 with acetic acid.

[0045] Through the front padder of the ten-box knitted fabric opening and setting machine, a one-immersion-one-paving method is adopted, and the prepared padding solution is dipped and rolled at room temperature, and the liquid content of the cloth surface is 70-75%; the setting temperature of the ten-box knitted fabric opening and setting machine is controlled to be 180℃-190℃, the air volume is 1800-2000 revolutions / minute, and the machine speed is 10-15 meters / minute for padding and setting.

[0046] The multifunctional composite nurse uniform warp knitted fabric produced by the above method was left to stand for 48 hours under standard conditions, and then the moisture permeability, antibacterial rate, charge surface density, waterproof performance, oil repellency, stain resistance of the fabric after 100 washes were tested with reference to the standard. The pH value, washing size change rate, distortion change rate, anti-pilling, and snagging properties of the fabric were also tested. The corresponding reference standards and test results are shown in Table 1.

[0047] Table 1 Fabric performance test results

[0048]

[0049]

[0050] The preferred embodiments listed above further illustrate the objectives, technical solutions and advantages of the present invention in detail. It should be understood that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A composite warp knitted fabric for nurse uniforms, characterized in that: The invention comprises a fabric body woven by a single needle bed three-comb warp knitting machine and treated with antibacterial, waterproof, oil-repellent and anti-fouling treatments. The fabric body comprises a front comb, a middle comb and a back comb. The front comb is a warp plain structure, and the front comb is woven by 75D / 72F non-circular cross-section, light network structure, low-elastic polyester filaments, and full-threading. The middle comb is a chain-knitted pad structure, and the middle comb is woven by 75D / 36F circular cross-section, light network structure, low-elastic polyester filaments and 70D conductive composite yarns. The warp arrangement ratio of the low-elastic chemical fiber filaments and the conductive composite yarns is 24:

1. The back comb is a warp pile structure, and the back comb is woven by 75D / 36F circular cross-section, light network structure, low-elastic polyester filaments, and full-threading. The horizontal density of the lower woven fabric is 24 longitudinal rows / cm.

2. A method for producing a composite warp knitted fabric for nurse uniforms, characterized in that: Including knitting and weaving technology and dyeing and finishing technology, The knitting weaving process comprises: knitting on a single needle bed three-comb warp knitting machine, using 75D / 72F non-circular cross-section, light network structure low-elastic polyester filaments to fully weave into a warp plain structure as the front comb of the warp knitted fabric, using 75D / 36F circular cross-section, light network structure low-elastic polyester filaments and 70D conductive composite yarns to fully weave into a braided chain missing pad structure at a warp arrangement ratio of 24:1 as the middle comb of the warp knitted fabric, using 75D / 36F circular cross-section, light network structure low-elastic polyester filaments to fully weave into a warp pile structure as the back comb of the warp knitted fabric, and the horizontal density of the lower woven fabric is 24 longitudinal rows / cm; The dyeing and finishing process includes: cloth arrangement process Edge Binding Process Refining and degreasing process Hot and cold wash cycles Whitening and dyeing process Cleaning process Drainage process Dehydration process Slitting process Drying process Finished product padding and shaping process.

3. The method for producing the warp knitted fabric for composite nurse uniforms according to claim 2, characterized in that: In the dyeing and finishing process, the whitening and dyeing process is: Auxiliary solution is used in a dyeing machine for one-bath one-step dyeing and finishing of whitening and antibacterial finishing, and the auxiliary solution formula is selected as follows: 0.09-0.11% of the fabric weight ratio of whitening agent SBV, 0.30-0.35% of the fabric weight ratio of whitening agent CPS-D, 0.8-1.2% of the fabric weight ratio of antibacterial deodorant, 1.98-2.02% of the fabric weight ratio of high temperature leveling agent TF212E, 1.0-1.5% of the fabric weight ratio of bath softener SF-66, 0.18-0.22% of the fabric weight ratio of acetic acid, and 1.6-2.0% of the fabric weight ratio of detergent; According to the bath ratio of 1:13-15, cold water was injected into the L-type high-temperature and high-pressure jet overflow dyeing machine, and the diluted auxiliary solution was gradually added into the dyeing machine from the additional cylinder of the dyeing machine. After running for 5 minutes at room temperature, the fabric was put in, and the evenly dispersed diluted brightener solution was added from the additional cylinder. After running for 3 minutes, the pH value of the dyeing solution was controlled to be 3.5-4.2, and the temperature was raised to 80°C at 2.5°C / min, kept warm for 5 minutes, and then raised to 110°C at 1.0°C / min, kept warm for 5 minutes, and then raised to 130°C at 1.0°C / min, kept warm for 30 minutes; then cooled to 120°C at 2.0°C / min. ℃ keep warm for 5 minutes, cool down to 110℃ at 1.0℃ / min and keep warm for 5 minutes, then cool down to 80℃ at 1.5℃ / min, take samples for color matching, overflow wash to below 60℃ and drain, then add water according to the bath ratio of 1:10-12, heat to 60℃ at 3.5-4.0℃ / min, keep warm for 10 minutes and drain, cold wash and drain, then add water according to the bath ratio of 1:10-12, start the main pump to circulate the fabric in the dyeing machine, dilute and stir the detergent in the additional cylinder, then gradually add it into the dyeing machine, heat to 70℃ at 3.5-4.0℃ / min, keep warm for 20 minutes and drain out of the cylinder.

4. The method for producing the composite warp knitted fabric for nurse uniforms according to claim 2, characterized in that: In the dyeing and finishing process, the finished product padding and shaping process is as follows: A ten-box knitted fabric opening setting machine is used for padding setting, wherein the padding solution formula used is 50-60g / L of three-proofing additives, 13-15g / L of cross-linking agent and 4-5g / L of penetrant, and the pH value of the padding solution is adjusted to 4.0-5.0 with acetic acid. Through the front roller of the ten-box knitted fabric opening and setting machine, the prepared padding solution is dipped and rolled at room temperature in a one-dipping and one-rolling manner, and the liquid content on the fabric surface is 70-75%; the setting temperature of the ten-box knitted fabric opening and setting machine is controlled to be 180℃-190℃, the air volume is 1800-2000 rpm, and the machine speed is 10-15 m / min for padding and setting.