Crossflow guides for preventing foaming in high convection plating tanks
By arranging a fluid containing unit and a cross-flow conduit in the electroplating device to control the flow of electrolyte, the problem of large electroplating feature size in the electrochemical deposition process is solved, and more uniform coating deposition and an efficient electroplating process are achieved.
Patent Information
- Application Number
- CN201980076026.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-11-19
- Filing Date
- 2019-11-15
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2039-11-15
AI Technical Summary
In modern integrated circuit manufacturing, the electrochemical deposition process faces complex packaging and large plating feature sizes in multi-chip interconnection technology, which leads to difficulty in fluid dynamics control and affects plating uniformity and plating efficiency.
Provide an electroplating device and method, by arranging a fluid containing unit, a substrate holder, a channeled ion resistive plate and a cross-flow conduit in an electroplating tank to control the flow of electrolyte and generate shear flow to achieve a more uniform plating layer deposition. The device includes a plating tank, a substrate holder, a channeled ion-resistive plate, a cross-flow conduit, and a flow restrictor to regulate the flow of electrolyte, ensure that the substrate is separated from the anode during plating, and to remove the electrolyte through the cross-flow conduit. Liquid is diverted to reduce splashing and foaming.
By controlling the fluid dynamics of the electrolyte, more uniform metal layer deposition is achieved, the quality of the coating and plating efficiency are improved, foam generation is reduced, and the stability and output of the plating device are enhanced.
Smart Images

Figure CN113056575B_ABST
Abstract
Description
[0001] Incorporated by Reference
[0002] The PCT application form is filed concurrently with this specification as a part of this application. Each application to which this application claims the benefit or priority as identified in the concurrently filed PCT application form is incorporated herein by reference in its entirety and for all purposes. Background Art
[0003] Electrochemical deposition processes are well established in modern integrated circuit manufacturing. The transition from aluminum to copper metal line interconnects in the early 21st century drove the need for increasingly complex electroplating processes and electroplating tools. Most of the complex processes evolved in response to the need for smaller current-carrying lines in device metallization layers. These copper lines are formed by electroplating metal into very narrow, high aspect ratio trenches and vias in a process commonly referred to as "damascene" (pre-passivation metallization).
[0004] Electrochemical deposition is now used for complex packaging and multi-chip interconnect technologies, which are commonly and colloquially referred to as wafer-level packaging (WLP) and through-silicon via (TSV) electrical connection technologies. Due in part to the typically larger feature sizes (compared to front-end-of-line (FEOL) interconnects) and high aspect ratios, these technologies present their own very significant challenges.
[0005] Compared to damascene applications, these techniques involve plating at significantly larger scales. Depending on the type and application of the package feature (e.g., die-to-die connection TSV, interconnect redistribution routing, or die-to-board or die-to-die soldering, such as flip-chip pillars), plated features in current technology are typically larger than about 2 microns and typically 5-300 microns (e.g., copper pillars can be about 50 microns). For some on-chip structures such as power buses, the features to be plated can be larger than 300 microns. The aspect ratio of WLP features is typically about 1:1 (height to width) or less, while TSV structures can have very high aspect ratios (e.g., in the vicinity of about 20:1). Summary of the invention
[0006] An apparatus for controlling electrolyte fluid dynamics during electroplating is provided. One aspect relates to an electroplating apparatus comprising: an electroplating tank configured to contain an electrolyte and an anode when electroplating a metal onto a substrate, the electroplating tank having a chamber wall of a fluid containing unit having a fluid level during electroplating; a substrate holder configured to hold the substrate so that a plating surface of the substrate is separated from the anode during electroplating; an ion-resistive plate with a channel, comprising a surface facing the substrate separated from the plating surface of the substrate by a cross-flow region; a cross-flow inlet of the cross-flow region for receiving the electrolyte flowing in the cross-flow region; and a cross-flow conduit comprising a channel for diverting the electrolyte from the cross-flow region to an outlet of the fluid containing unit leading to the electroplating tank, the outlet being below the fluid level and the cross-flow region being between the cross-flow inlet and the cross-flow conduit.
[0007] In various embodiments, the cross-flow region is defined at least in part by an upper surface of the channeled ion-resistive plate, a lower surface of the substrate in the substrate holder when in operation, and an insert.
[0008] In various embodiments, the cross-flow conduit is configured to receive electrolyte flowing out of the cross-flow region and direct the electrolyte to flow downwardly and away from the surface of the substrate.
[0009] In various embodiments, the device further comprises a flow restrictor for restricting the flow of the electrolyte in the cross-flow conduit. In some embodiments, the flow restrictor is a plate inserted below the channeled ion-resistive plate. In some embodiments, the flow restrictor is a motor-driven variable orifice plate that can vary the size of the opening of the cross-flow conduit. In some embodiments, the flow restrictor is a pressure relief valve that seals the electrolyte flow in response to whether a substrate is present in the electroplating tank based on the pressure of the electrolyte.
[0010] In various embodiments, the cross-flow conduit is an attachable diverting device that is attachable to the electroplating tank.
[0011] In various embodiments, the device further comprises a membrane frame beneath the channeled ion-resistive plate, wherein the cross-flow conduit further comprises a second channel in the membrane frame, the second channel being used to allow the electrolyte from the cross-flow region to flow to an outlet of the fluid containing unit leading to the electroplating tank.
[0012] In various embodiments, the device further comprises a weir wall. The device may also comprise an insert adjacent to the substrate holder, the insert comprising the weir wall for containing the electrolyte to a fluid level above the insert during electroplating to ensure complete wetting of the substrate as it enters. In certain embodiments, the weir wall comprises a base disposed above the insert.
[0013] In some embodiments, the weir wall is not part of the channeled ion-resistant plate.
[0014] In some embodiments, during operation, the cross-flow conduit prevents the electrolyte from flowing over a weir wall.
[0015] In various embodiments, the cross-flow conduit is disposed on a portion of the channeled ion-resistive plate adjacent to an outlet of the cross-flow region.
[0016] In various embodiments, wherein the device further comprises a membrane frame, the cross-flow conduit is additionally disposed on a portion of the membrane frame.
[0017] In various embodiments, the cross-flow conduit is additionally disposed on a portion of the chamber wall.
[0018] In various embodiments, the cross-flow conduit is disposed in a removable component.
[0019] In some embodiments, the device may also include a controller having executable instructions for electroplating material onto the substrate by: causing the electrolyte to flow from one side of the substrate across the surface of the substrate to the opposite side of the substrate by cross-flow; when the electrolyte flows to the opposite side of the substrate, causing the electrolyte flow to be diverted to below the fluid level to be collected in the fluid containing unit; and using the motor-driven variable orifice plate to widen and narrow the opening of the cross-flow conduit in response to the flow rate of the electrolyte.
[0020] On the other hand, it may involve a method for electroplating on a substrate, the method comprising: receiving a substrate in a substrate holder, wherein the substrate holder is configured to support the substrate so that a plating surface of the substrate is separated from an anode during electroplating; immersing the substrate in an electrolyte, wherein a cross-flow region is formed between the plating surface of the substrate and an upper surface of an ion-resistive plate with a channel; causing the electrolyte in contact with the substrate in the substrate holder to flow from under the ion-resistive plate with a channel, through the cross-flow region, across the ion-resistive plate with a channel, into the cross-flow region, and out of a cross-flow conduit; adjusting an opening of the cross-flow conduit using a flow restrictor; and electroplating material onto the plating surface of the substrate while causing the electrolyte to flow and adjusting the opening of the cross-flow conduit.
[0021] In various embodiments, the cross-flow region is defined at least in part by an upper surface of the channeled ion-resistive plate, a lower surface of the substrate in the substrate holder when in operation, and an insert.
[0022] In various embodiments, the cross-flow conduit is configured to receive the electrolyte flowing out of the cross-flow region and direct the electrolyte to flow downwardly and away from the surface of the substrate.
[0023] In various embodiments, the flow restrictor restricts the flow of the electrolyte in the cross-flow conduit. In some embodiments, the flow restrictor is a plate inserted below the channeled ion-resistive plate. In some embodiments, the flow restrictor is a motor-driven variable orifice plate that is capable of changing the opening size of the cross-flow conduit. In some embodiments, the flow restrictor is a pressure relief valve that seals the electrolyte flow in response to the presence of a substrate in the electroplating tank based on the pressure of the electrolyte.
[0024] In various embodiments, the cross-flow conduit is an attachable diverting device that is attachable to the electroplating tank.
[0025] In various embodiments, the method further comprises flowing the electrolyte from the cross-flow region to an outlet of the fluid containing unit leading to the electroplating cell using a second channel disposed in a membrane frame below the channeled ion-resistive plate.
[0026] In various embodiments, the substrate is completely wetted upon entry. The method is performed using an electroplating tank having a weir wall. The electroplating tank may also include an insert adjacent to the substrate holder, the insert including the weir wall, which is used to contain the electrolyte to a fluid level above the insert during electroplating to ensure complete wetting of the substrate upon entry. In some embodiments, the weir wall includes a base disposed above the insert. In some embodiments, the weir wall is not part of the channeled ion-resistant plate.
[0027] In some embodiments, during operation, the cross-flow conduit prevents the electrolyte from flowing over a weir wall.
[0028] In various embodiments, the cross-flow conduit is disposed on a portion of the channeled ion-resistive plate adjacent to an outlet of the cross-flow region.
[0029] In various embodiments, the cross-flow conduit is additionally disposed on a portion of the chamber wall.
[0030] In various embodiments, the cross-flow conduit is disposed in a removable component.
[0031] These and other aspects will be further described below with reference to the associated drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1A Depicted is a cross-sectional view of a portion of a substrate holding assembly including a cone and a cup.
[0033] Figure 1B Shown are top views of electroplating apparatus embodiments that may be used to facilitate lateral flow across a substrate surface and the fluid dynamics that may be achieved when certain embodiments are implemented.
[0034] Figure 1C A cross-section of an electroplating cell is shown with the flow at the outlet passing over a weir.
[0035] Figure 1D A close-up view of a cross-section of a cross-flow outlet of a channel-containing ion-resistive plate (CIRP) weir is shown, with fluid flowing over the upper portion of the CIRP weir.
[0036] Figure 1E A CIRP with a weir wall is shown.
[0037] Figure 2 An exploded view of the various portions of an electroplating apparatus typically found in a cathode chamber is shown according to certain embodiments disclosed herein.
[0038] Figure 3A close-up view of a cross-flow side inlet and surrounding hardware is shown according to certain embodiments disclosed herein.
[0039] Figure 4 Cross-sectional views of various portions of an electroplating apparatus are depicted according to certain embodiments disclosed herein.
[0040] Figure 5 Shown is a cross-flow jet manifold and jet head divided into 6 separate sections.
[0041] Figure 6 A top view of the CIRP and associated hardware with particular focus on the inlet side of the cross flow is shown.
[0042] Figure 7 A simplified top view of the CIRP and associated hardware is shown, showing the inlet and outlet sides of the cross-flow region.
[0043] Figures 8A-8B Exemplary designs of cross-flow inlet regions are shown according to certain embodiments.
[0044] Fig. 9 Close-up views of the cross-flow outlet, CIRP, membrane frame, cross-flow conduit, and surrounding hardware are shown according to various disclosed embodiments.
[0045] Fig.10 An exploded view of an embodiment having four modified components is shown according to certain disclosed embodiments: plating tank, membrane frame, CIRP, and front side insert for use with cross flow conduits.
[0046] Fig.11A A close-up view of a cross-section of a cross-flow conduit with a fixed flow restrictor plate is shown according to certain disclosed embodiments.
[0047] Fig. 11B Various designs of flow restrictor plates that may be used with certain disclosed embodiments are shown.
[0048] Fig.12 A close-up cross-sectional view of a cross-flow conduit with a motor-driven variable orifice flow restrictor plate is shown in accordance with certain disclosed embodiments.
[0049] Fig.13 A cross-sectional close-up view of a cross-flow conduit having a pressure relief valve flow restrictor is shown according to certain disclosed embodiments.
[0050] Fig.14 An illustration of an alternative embodiment using an attachable diverting device to divert fluid flow downward in a tool rather than using built-in cross-flow conduits is shown. DETAILED DESCRIPTION
[0051] The disclosed embodiments relate to methods and apparatus for controlling electrolyte fluid dynamics during electroplating. More specifically, the methods and apparatus described herein are particularly useful for plating metals on semiconductor wafer substrates, for example, through-resist plating (e.g., copper, nickel, tin, and tin alloy solders) and copper through-silicon via (TSV) features.
[0052] In this application, the terms "semiconductor wafer", "wafer", "substrate", "wafer substrate" and "partially manufactured integrated circuit" are used interchangeably. It should be understood by those of ordinary skill in the art that the term "partially manufactured integrated circuit" can refer to a silicon wafer during any of the many stages of integrated circuit fabrication thereon. The following detailed description assumes that the disclosed embodiments are implemented on a wafer. Typically, the diameter of the semiconductor wafer is 200 mm, 300 mm, or 450 mm. However, the disclosed embodiments are not so limited. The workpiece can have a variety of shapes, sizes, and materials. In addition to semiconductor wafers, other workpieces that can take advantage of the disclosed embodiments include various items such as printed circuit boards and the like.
[0053] In the following description, many specific details are set forth to provide a thorough understanding of the embodiments presented. The disclosed embodiments may be implemented without some or all of these specific details. In other cases, known processing operations are not described in detail to avoid unnecessarily obscuring the embodiments of the present invention. Although embodiments of the present invention will be described in conjunction with specific embodiments, it should be understood that it is not intended to limit the disclosed embodiments.
[0054] The methods and apparatus provided herein can be used for electroplating on various substrates, including electroplating on WLP, TSV and mosaic substrates. Various metals and metal alloys can be electroplated, including but not limited to electroplating copper, tin, silver, tin-silver alloys, nickel, gold, indium and cobalt. In a typical electroplating process, a wafer substrate containing an exposed conductive seed layer is cathode biased and contacted with a plating solution containing ions of the metal being plated. The ions are electrochemically reduced on the surface of the seed layer to form a metal layer. As an example, through-resist electroplating will be used to illustrate the various disclosed embodiments of the present invention, but the disclosed embodiments are not limited thereto.
[0055] The disclosed embodiments relate to electroplating apparatus and electroplating methods. In particular, the disclosed embodiments relate to improving electrolyte fluid dynamics during electroplating of a metal layer onto a semiconductor substrate and the manner in which current and / or voltage is applied to the substrate during electroplating.
[0056] The disclosed embodiments include electroplating apparatus configured to control electrolyte fluid dynamics during electroplating to obtain a highly uniform coating and methods including controlling electrolyte fluid dynamics during electroplating to obtain a highly uniform coating. In a specific implementation, the disclosed embodiments employ methods and apparatus for generating shear flow (sometimes referred to as "cross flow" or flow having a velocity parallel to the workpiece surface).
[0057] The disclosed embodiments are suitable for filling a wide variety of features. In various embodiments, certain disclosed embodiments are suitable for filling features having a depth between about 2 μm and about 240 μm, or about 20 μm and about 240 μm. Features may have a width or diameter of about 10 μm to about 240 μm, or about 30 μm to about 200 μm. Features may have an aspect ratio of about 0.1:1 to about 4:1, or about 1:1.
[0058] Plating room
[0059] One embodiment is an electroplating apparatus comprising the following features: (a) an electroplating chamber configured to contain an electrolyte and an anode when electroplating metal onto a substrate, the substrate being substantially planar; (b) a substrate holder configured to hold the substrate so that a plating surface of the substrate is separated from the anode during electroplating; (c) a channeled ion-resistive plate (CIRP) comprising a substrate-facing surface substantially parallel to the plating surface of the substrate and separated from the plating surface of the substrate during electroplating, the CIRP comprising a plurality of non-connected channels, wherein the non-connected channels enable electrolyte to be transported through the element during electroplating; (d) a mechanism for generating and / or applying shear forces (cross flow) to the electrolyte flowing in a cross-flow region at the plating surface of the substrate; (e) an optional cross-flow region defined between the plating surface of the substrate and a surface of the channeled ion-resistive element facing the substrate, the cross-flow region having a height that can be dynamically controlled during the electroplating process; and (f) an optional mechanism for promoting shear flow near the periphery of the substrate, adjacent to the substrate / substrate holder interface. Although the wafer is substantially flat, it typically also has one or more microgrooves, and its surface may have one or more portions that are shielded from exposure to the electrolyte. In various embodiments, the apparatus further includes a mechanism for rotating the substrate and / or CIRP while causing the electrolyte in the plating tank to flow in the direction of the plating surface of the substrate. In certain embodiments, the apparatus may include a seal or flow ring configured to prevent the electrolyte from leaving the cross-flow region at a location other than a designated outlet located in the cross-flow region, the designated outlet being positioned azimuthally opposite to an inlet located in the cross-flow region.
[0060] In some such embodiments, when the substrate holder is in the lowest position, a seal or flow ring (e.g., a flow restriction element or insert, CIRP, etc.) can be provided between the bottom surface of the substrate holder and the upper surface of the element below the substrate holder. For example, the seal can prevent the electrolyte from leaking out of the device between the bottom of the substrate holder and the top of the flow restriction element. In a plurality of embodiments, the device can cycle between a sealed position (when the position of the substrate holder is at its lowest point and the height of the cross-flow region is at a minimum) and an unsealed position (when the substrate holder is raised and the height of the cross-flow region is relatively large). When the device is in the unsealed position, the substrate can be rotated. In these or other cases, when the substrate is in the sealed position, the substrate can also be rotated. The periodic sealing of the cross-flow can increase the volume and velocity of the electrolyte flowing laterally through the substrate surface, thereby providing improved plating uniformity.
[0061] In certain embodiments, the mechanism for applying the cross flow is an inlet having, for example, an appropriate flow directing and distributing device on or adjacent to the periphery of the CIRP. The inlet directs the cross-flow of the cathode electrolyte along the surface of the CIRP facing the substrate. The inlet is azimuthally asymmetric, partially following the periphery of the CIRP, and has one or more gaps, and defines a cross-flow jet manifold between the CIRP and the substantially flat substrate during electroplating. Other elements are optionally provided for working in coordination with the cross-flow jet manifold. These may include a cross-flow jet distribution nozzle and a cross-flow restriction ring or front side insert, which are further described below in conjunction with the accompanying drawings. The cross-flow restriction ring or front side insert can be semi-circular (180°), but in various embodiments can be fully circular (360°).
[0062] Embodiments herein can be implemented with multiple substrate sizes. In some cases, the diameter of the substrate is about 200mm, about 300mm or about 450mm. In addition, embodiments herein can be implemented with various overall flow rates. In some implementations, the total flow rate of electrolyte is between about 1-60L / min, greater than 20L / min, greater than 25L / min, between about 6-60L / min, between about 20-55L / min, between about 5-25L / min or between about 15-25L / min. The flow rate realized during electroplating can be limited by some hardware constraints (such as the size and capacity of the pump used). Those skilled in the art will appreciate that when disclosed technology is implemented with a larger pump, the flow rate quoted by the present invention will be higher.
[0063] In some embodiments, the electroplating device comprises separated anode and cathode chambers, wherein each chamber in the two chambers has different electrolyte compositions, electrolyte circulation, and / or fluid mechanics. Ion permeable membranes can be used to inhibit direct convection transport (mass movement through flow) of one or more components between these chambers and maintain the desired separation between these chambers. The membrane can block most of the electrolyte flow and prevent the transport of certain substances (such as organic additives) while allowing the transport of ions (such as cations). In some embodiments, the membrane comprises NAFION® of DuPont. TM Or related ion selective polymers. In other cases, the membrane does not include ion exchange materials, but rather includes microporous materials. Typically, the electrolyte in the cathode chamber is referred to as the "cathode electrolyte", and the electrolyte in the anode chamber is referred to as the "anolyte". Typically, the anolyte and the catholyte have different compositions, the anolyte contains little or no plating additives (e.g., promoters, inhibitors and / or equalizers), and the catholyte contains significant concentrations of such additives. The concentrations of metal ions and acids are also often different between the two chambers. Examples of electroplating devices containing separated anode chambers are described in U.S. Patent No. 6,527,920, filed on November 3, 2000; U.S. Patent No. 6,821,407, filed on August 27, 2002, and U.S. Patent No. 8,262,871, filed on December 17, 2009, each of which is incorporated herein by reference in its entirety.
[0064] In some embodiments, the anode membrane need not include ion exchange materials. In some embodiments, the membrane is made of a microporous material, such as polyethersulfone manufactured by Koch Membrane of Wilmington, Massachusetts. This membrane type is most notably suitable for inert anode applications, such as tin-silver electroplating and gold electroplating, and can therefore also be used for soluble anode applications, such as nickel electroplating.
[0065] In the following discussion, when referring to the "top" and "bottom" features (or similar terms, such as "upper" and "lower" features, etc.) or elements of the disclosed embodiments, the terms "top" and "bottom" are used simply for convenience, and the terms represent only a single framework of reference or implementation of the disclosed embodiments. Other configurations are possible, such as those in which the top and bottom components are reversed with respect to gravity and / or the top and bottom components become left and right components or right and left components.
[0066] Although some aspects of the invention described herein may be used in various types of electroplating apparatus, for simplicity and clarity, most of the examples will involve wafer-face-down, "fountain" electroplating apparatus. In such an apparatus, the workpiece to be plated (typically a semiconductor wafer in the embodiments described herein) generally has a generally horizontal orientation (perhaps in some cases varying some degrees from true horizontal for a portion of or during the entire electroplating process) and can be powered to rotate during electroplating, thereby producing a generally vertically upward electrolyte convection pattern. The integration of the impinging flow mass from the center to the edge of the wafer, and the inherently higher angular velocity of the rotating wafer at its edge relative to its center, produces radially increasing shear (wafer-parallel) flow rates. An example of components of a fountain-type electroplating tank / apparatus is manufactured by and available from Novellus Systems, Inc. of San Jose, California. Electroplating Systems. Additionally, fountain-type electroplating systems are described in, for example, U.S. Patent No. 6,800,187, filed August 10, 2001, and U.S. Patent No. 8,308,931, filed November 7, 2008, the entire contents of which are incorporated herein by reference.
[0067] The substrate to be plated is usually flat or substantially flat. As used herein, substrates with features such as grooves, through holes, photoresist patterns are considered to be substantially flat. Typically, these features are on a microscopic scale, but not necessarily always so. In many embodiments, one or more portions of the surface of the substrate can be shielded from exposure to the electrolyte.
[0068] Figure 1A The following description provides a general non-limiting background to aid in understanding the described apparatus and methods. A wafer holding and positioning apparatus for electrochemically processing semiconductor wafers may include a wafer engaging member (sometimes referred to herein as a "flip" member). The actual flip includes a cup 102 and a cone 103 (see Figure 1A ) so that pressure can be applied between the wafer and the seal, thereby securing the wafer in the cup.
[0069] The cup 102 is supported by a support rod 104, which is connected to a top plate 105. The assembly (102-105), collectively referred to as assembly 101, is driven by a motor (not shown) via a spindle 106. The motor (not shown) is connected to a mounting bracket (not shown). The spindle 106 transmits torque to the wafer 145 to allow it to rotate during electroplating. A cylinder (not shown) within the spindle 106 also provides a vertical force between the cup 102 and the cone 103 to create a seal between the wafer 145 contained in the cup 102 and the sealing component (lip seal) 143. For the purposes of discussion, the assembly including components 102-109 is collectively referred to as a wafer holder. However, it is noted that the concept of a "wafer holder" generally extends to various combinations and sub-combinations of components that engage a wafer and allow it to be moved and positioned.
[0070] The tilt assembly includes a first plate slidably connected to a second plate (both connected to a drive cylinder), which is connected to a mounting bracket. The drive cylinder provides a force for sliding the first plate (and therefore the wafer holder) over the second plate. The distal end of the wafer holder moves along an arcuate path (not shown) defining the contact area between the two plates, and as a result, the proximal end of the wafer holder (e.g., cup and cone assembly) tilts toward a virtual pivot. This allows the wafer to enter the plating bath at an angle.
[0071] The entire apparatus is raised vertically upward or lowered downward via another actuator (not shown) to immerse the proximal end of the wafer holder into the bath. This actuator (and the associated lifting motion) provides one possible mechanism to control the height of the cross-flow region between the substrate and the CIRP. Any similar mechanism capable of moving the wafer holder (or any part thereof that supports the actual wafer) toward / away from the CIRP may be used for this purpose. The apparatus provides a dual component positioning mechanism that allows for both vertical movement of the wafer along a trajectory perpendicular to the electrolyte and tilted movement away from the horizontal (parallel to the electrolyte surface) (angled wafer immersion capability). A more detailed description of the device's motion capabilities and associated hardware is described in U.S. patent application serial No. 16 / 101,291 filed on August 10, 2018, U.S. patent application publication No. 2017 / 0342590 filed on January 23, 2017, and U.S. Patent 6,551,487 filed on May 31, 2001 and issued on April 22, 2003, the entire contents of which are incorporated herein by reference.
[0072] Note that the device is typically used with a specific plating tank having a plating chamber containing an anode (e.g., a copper anode or a non-metallic inert anode) and an electrolyte. The plating tank may also include a pipe or pipe connection for circulating the electrolyte through the plating tank-and against the workpiece being plated. It may also include a membrane or other separator designed to keep different electrolyte chemicals in the anode compartment and the cathode compartment. In one embodiment, a membrane is used to define an anode compartment that contains an electrolyte that is substantially free of inhibitors, promoters, or other organic plating additives, or in another embodiment, wherein the inorganic plating compositions of the anolyte and the catholyte are substantially different. It may also be optionally provided that the anolyte is transported to the catholyte or to the device of the main plating bath by physical means (e.g., direct pumping, which includes valves (values), or overflow tanks).
[0073] The following description provides further details of the cup and cone assembly of the flip top. Figure 1A An assembly 101 is shown in cross-section and includes a cone 103 and a cup 102. Note that this figure is not meant to be an actual depiction of a cup and cone assembly, but rather a stylized depiction for purposes of discussion. The cup 102 is supported by a top plate 105 via support rods 104, which are connected via screws 108. Generally, the cup 102 provides a support upon which a wafer 145 rests. The cup 102 includes an opening through which electrolyte from a plating tank can contact the wafer. Note that the wafer 145 has a front side 142 on which electroplating is performed. The periphery of the wafer 145 rests on the cup 102. The cone 103 presses down on the back side of the wafer to hold the wafer in place during electroplating.
[0074] To load a wafer 145 into the assembly 101, the cone 103 is raised from its depicted position via the spindle 106 until the cone 103 contacts the top plate 105. From this position, a gap is created between the cup 102 and the cone 103, into which the wafer 145 can be inserted, thereby loading into the cup 102. The cone 103 is then lowered as depicted to engage the wafer 145 against the periphery of the cup 102 and to engage the set of electrical contacts (at the ends of the lip seal 143) that extend radially beyond the periphery of the wafer. Figure 1A not shown).
[0075] The spindle 106 transmits both the vertical force for engaging the cone 103 with the wafer 145 and the torque for rotating the assembly 101. These transmitted forces are Figure 1A As indicated by the arrow in FIG. 144 , it is noted that generally when the wafer 145 is rotated (as indicated by Figure 1A Wafer electroplating is performed when the wafer is electroplated (indicated by the dotted arrow at the top).
[0076] The cup 102 has a compressible lip seal 143 to form a fluid-tight seal when the cone 103 engages the wafer 145. The vertical force from the cone 132 and the wafer 145 compresses the lip seal 143 to form a fluid-tight seal. The lip seal 143 prevents the electrolyte from contacting the back side of the wafer 145 (where it can directly introduce contaminants such as copper or tin ions into the silicon) and prevents the electrolyte from contacting sensitive components of the device. There may also be a seal between the interface of the cup 102 and the wafer 145 that forms a fluid-tight seal to further protect the back side of the wafer 145.
[0077] Cone 103 also includes seal 149. As shown, seal 149 is located near the edge of cone 103 and the upper area of cup 102 when the edge of cone 103 and the upper area of cup 102 are engaged. This also protects the back side of wafer 145 from any electrolyte that may enter the flap from above cup 102. Seal 149 can be secured to cone 103 or cup 102 and can be a single seal or a multi-component seal.
[0078] When electroplating begins, cone 103 is raised above cup 102 and wafer 145 is introduced into assembly 102. When wafer 145 is initially introduced into cup 102 - typically by a robotic arm - front face 142 of wafer 145 rests lightly against lip seal 143. To help achieve uniform electroplating, assembly 101 is rotated during electroplating. In subsequent figures, assembly 101 is depicted in a relatively simple manner and in association with components for controlling the fluid mechanics of the electrolyte on the plating side of the wafer during electroplating. Thus, what follows is an overview of mass transfer and fluid shear forces on the workpiece.
[0079] Figure 1B Certain techniques are related to those that can be used to stimulate cross flow across the surface of the substrate to be plated. Alternative schemes for stimulating cross flow are presented relative to the various techniques described in these figures. Therefore, certain elements described in the figures herein are optional and are not present in all embodiments.
[0080] In some embodiments, the electrolyte flow ports are configured to promote cross flow, either alone or in combination with flow shaping plates and flow diverters as described herein. Various embodiments are described below with respect to combinations of flow shaping plates and flow diverters, but the disclosed embodiments are not limited thereto. Note that in some embodiments, the magnitude of the electrolyte flow vector across the wafer surface is believed to be larger near the vent or gap and tapers across the wafer surface, being smallest in the interior of the pseudo chamber farthest from the vent or gap. Figure 1B As shown in , in some cases, in one example depicted at 204, using appropriately configured electrolyte flow ports 200, the size of these cross flow vectors 150 is made more uniform across the wafer surface.
[0081] Figure 1C A cross-sectional view of an electroplating tank having an edge flow element 151 installed therein is depicted. In this example, the edge flow element 151 is positioned radially outward of the raised platform portion of the CIRP 154. The shape of the edge flow element 151 causes electrolyte near the inlet to move upward at a certain angle to reach the cross-flow region 152, and similarly causes electrolyte near the outlet to move downward at a certain angle to leave the cross-flow region 152; however, the flow above the weir on the right side of the figure may cause splashing. The uppermost portion of the edge flow element 151 can extend above the plane of the raised platform portion of the CIRP 154. In other cases, the uppermost portion of the edge flow element 151 can be flush with the raised portion of the CIRP 154. In some cases, the position of the edge flow element 151 can be adjusted, as described elsewhere herein. The shape and position of the edge flow element 151 can promote a higher degree of cross-flow near the corner formed between the substrate and the substrate holder 156.
[0082] Figure 1D The effect of fluid 180 moving upward over CIRP weir wall 186 is shown, which causes entrained air and foam 182 to form in the fluid confinement unit of the holding tank fluid holding area 183. Some electroplating equipment delivers high cross flow between CIRP 184 and wafer 185, with the goal of providing fresh electrolyte deep into the features of the wafer. When the cross flow leaves the area between CIRP 184 and wafer 185, such as Figure 1D , it flows upward over the CIRP weir 186 on the CIRP 184, and then falls downward into the tank fluid holding area 183, which is an area for collecting the electroplating solution before it is drawn back into the larger electroplating bath reservoir. At low flow rates, the fluid waterfall falling above the CIRP weir 186 is not sufficiently turbulent to generate foam. However, at high flow rates, the solution not only flows downward in a more turbulent manner, but it also sprays outward above the CIRP weir 186, impacting the tank holding outer weir 181. This interaction entrains air and generates foam. In order to avoid the device from generating foam without using a diverting device as described herein, the electroplating dual fluid supply flow rate is limited to between 20L / min and about 55L / min, depending on the configuration of the hardware. In some cases, the hardware can limit the flow rate to about 70-90L / min. However, above about 20L / min to about 55L / min, significant foam will be generated, causing electroplating hardware failure or error. Limiting the flow rate to about 20 L / min to about 55 L / min can limit the metal ion supply depth through the photoresist features, thereby reducing plating throughput while also degrading performance across the wafer, such as silver content and uniformity.
[0083] Figure 1E A perspective view of a CIRP 171 with a CIRP weir wall 170 is shown, which causes fluid to move upward and over the CIRP weir wall 170, resulting in foam formation in the fluid containment cell, with arrows 172 depicting the cross-flow direction.
[0084] Components of electroplating equipment
[0085] Many drawings are provided to further illustrate and explain the embodiments disclosed herein. The drawings include, in particular, a plurality of drawings of structural elements and flow paths associated with the disclosed electroplating apparatus. These elements are given certain names / reference numerals, which are used consistently in describing certain figures herein.
[0086] The embodiments below assume that the electroplating apparatus mostly comprises a separate anode chamber. Figure 2 An exploded view of certain components of the electroplating apparatus is shown. The features described are housed in a cathode chamber that includes a membrane frame 274 and membrane that separates the anode chamber from the cathode chamber. Any possible number of anode and anode chamber configurations may be used. Figure 3 and 4 206 and 207. FIG. 208 is an example of a cross section of the device showing the catholyte flow into the device. In the embodiments below, the catholyte contained in the cathode chamber is mostly located in the processing area between the CIRP 206 and the wafer (not shown), or in the channel 258 used to deliver the catholyte to the manifold. Figure 3 Shown is a cross-sectional close-up of the cross-flow inlet side according to embodiments disclosed herein.
[0087] Much of the focus of the following description is on controlling the catholyte at the outlet to the fluid containment unit. The catholyte begins to enter the cross-flow region 226 via a channel comprising an opening in the CIRP 206 and the dispersed holes of the cross-flow initiation structure. The catholyte that reaches the cross-flow region 226 through the cross-flow initiation structure is directed substantially parallel to the surface of the workpiece.
[0088] As noted in the above discussion, in order to shape the electric field and control the flow characteristics of the electrolyte, a "channeled ion-resistive plate" 206 (or "CIRP") is positioned between the working electrode (wafer or substrate) and the counter electrode (anode) during electroplating. The various figures herein show the relative position of the CIRP 206 relative to other structural features of the disclosed device. An example of such a CIRP 206 is described in U.S. Patent No. 8,308,931, filed on November 7, 2008, the entire contents of which were previously incorporated herein by reference. The CIRP described therein is suitable for improving radial electroplating uniformity on wafer surfaces, such as those containing relatively low conductivity or those containing very thin resistive seed layers. Another example is described in U.S. Patent Publication Application No. 2017 / 0342590, filed on January 23, 2017, all of which are incorporated herein by reference. The aspects described herein are suitable for improving cross flow by controlling fluid flow near the edge of the wafer using edge flow elements. Additional aspects of certain embodiments of the channeled element are described below.
[0089] The "membrane frame" 274 (sometimes referred to as the anode membrane frame in other documents) is a structural element used in some embodiments to support the membrane 202 that separates the cathode chamber from the anode chamber. It may have other features related to certain embodiments disclosed herein. Specifically, with reference to the embodiments of the accompanying drawings, it may include a flow channel 258 for transporting cathode electrolyte toward the cross-flow region 226. The electroplating tank may also contain a tank weir wall 282, which is used to determine and adjust the level of the uppermost portion of the cathode electrolyte. The various figures herein depict the membrane frame 274 in the context of other structural features associated with the disclosed cross-flow device.
[0090] The membrane frame 274 is a rigid structure for holding the membrane 202, which is typically an ion exchange membrane responsible for separating the anode chamber from the cathode chamber. As explained, the anode chamber may contain an electrolyte of a first composition, while the cathode chamber contains an electrolyte of a second composition. The membrane frame 274 may also include a plurality of fluid control rods, which may be used to help control the fluid delivered to the CIRP 206. In certain embodiments, the control rods are optional. The membrane frame 274 defines the bottommost portion of the cathode chamber and the topmost portion of the anode chamber. The described components are all located on the workpiece side of the electrochemical plating tank above the anode chamber and the membrane 202. They can all be considered as a part of the cathode chamber. However, it should be understood that certain embodiments of the cross-flow injection device do not use a separated anode chamber, so the membrane frame 274 is not necessary.
[0091] Typically located between the workpiece and the membrane frame 274 is the CIRP 206 and a cross-flow ring gasket for certain embodiments, or a flow ring ( Figure 4 ) and a cross-flow confinement ring 210, each of which can be secured to the CIRP 206. More specifically, the cross-flow ring gasket can be positioned directly atop the CIRP 206, and the wafer cross-flow confinement ring 210 can be positioned above the cross-flow ring gasket and secured to the top surface of the CIRP 206, effectively sandwiching the gasket therebetween. The figures herein show the wafer cross-flow confinement ring 210 arranged relative to the CIRP 206. In some embodiments, the wafer cross-flow confinement ring 210 is referred to as a single-piece front-side insert assembly, which includes a front-side insert, a flow ring (a thin polymer piece), and a clamping ring that attaches the flow ring to the front-side insert.
[0092] like Figure 2 As shown, the uppermost relevant structural feature of the present disclosure is a workpiece or wafer holder. In some embodiments, as Figure 2 As shown, the workpiece holder may be a cup 254, which is commonly used in cone and cup flip-top designs, such as those of Novellus System and Lam Research mentioned above. The design included in the electroplating tool. For example, Figure 2 and 8A -8B shows the relative orientation of the cup 254 with respect to the other elements of the apparatus. In many embodiments herein, the distance between the cup 254 and the CIRP 206 can be dynamically controlled during the electroplating process, as discussed further below.
[0093] In various embodiments, edge flow elements ( Figure 2 (not shown). An edge flow element may be provided substantially above and / or within CIRP 206 and below cup 254. The edge flow element is further described below.
[0094] Flow paths through a device with cross-flow conduits
[0095] Figure 4 A cross-sectional view of an electroplating apparatus showing both an inlet side and an outlet side is shown according to some embodiments herein. Figure 4A cross section of an electroplating tank apparatus is shown according to certain disclosed embodiments. The electroplating tank apparatus comprises an electroplating tank 200, a membrane frame 274, a front side insert, a flow ring (with a flow ring weir 208a), a CIRP 206, a cross-flow conduit 280 as an outlet, a cup or a bus bar, and a wafer 245. The area between the electroplating tank 200 and the electroplating tank weir wall 282 is a fluid containing unit for collecting the cathode electrolyte overflowing during electroplating. The cross-flow conduit 280 comprises a channel formed in the electroplating tank 200, the membrane frame 274, and the CIRP 206, so that the fluid flow from the CIRP 206 and the wafer 245 flows under the front side insert (and flows over to ensure continuous wetting), flows downward through the cross-flow conduit 280, and then flows out through the outlet as indicated by the arrow and flows into the fluid containing unit. The cross-flow conduit 280 is azimuthally positioned and may be located (a) on opposite sides of the cross-flow inlet, or (b) within a range of angles (e.g., about 10 to 180 degrees) of the CIRP circumference occupied by the cross-flow conduit. The width or radial opening size of the cross-flow conduit 280 may be between about 0.1 cm and about 1 cm. Generally, the cross-flow conduit 280 is a "smile" shape. Figure 9-13 Other examples are described.
[0096] The black horizontal line in the fluid containment cell represents the fluid level in the containment cell during use. The arrows show the flow direction during electroplating, i.e., the fluid starts by flowing upward through the cross-flow inlet, upward in the cross-flow direction indicated by the large arrow through the CIRP 206 between the CIRP 206 and the wafer 245, then flows downward under the insert 210, through the cross-flow conduit 280, and then exits to the fluid containment cell.
[0097] During the electroplating process, the catholyte fills and occupies the area between the upper portion of the membrane 202 on the membrane frame 274 and the cross-flow region 226, where the fluid level in the fluid container is limited by the trough weir wall 282. This catholyte region can be broken down into three sub-regions: 1) the CIRP manifold region 208 below the CIRP 206 and (for designs employing anode compartment cationic membranes) above the separated anode compartment cationic membrane 202 (this element is sometimes also referred to as the lower manifold region 208), 2) the cross-flow region 226, which is between the wafer and the upper surface of the CIRP 206, and 3) the upper trough region or "electrolyte containment region", which is outside the flip cover / cup 254 and within the fluid containment cell within the trough weir wall 282, where the fluid level is above the insert. When the wafer is not immersed and the flip cover / cup 254 is not in the downward position, the second and third regions merge into one region.
[0098] The above-mentioned area (2) between the upper portion of CIRP 206 and the bottom of the workpiece placed in the workpiece holder 254 contains the catholyte and is called the "cross-flow area" 226. The gap formed in this area measured from the surface of the workpiece to the upper surface of CIRP 206 can be very small, such as between about 0.5 mm and about 15 mm, or about 2 mm in one example. The diameter of the cross-flow area 226 is generally defined by the diameter of the wafer, but the size can vary from about 150 mm (for smaller diameter wafers) to about 500 mm (for larger diameter wafers). Generally speaking, the shape of the cross-flow area 226 is flat and round.
[0099] The flow rate of the fluid flowing through the cross-flow region 226 can be changed according to different configurations. For a 300 mm wafer and a 2 mm high cross-flow region 226, the flow rate of a single slot can be at least about 20 L / min, or at least about 25 L / min, or between about 6 L / min and about 60 L / min, or between about 20 L / min and about 50 L / min.
[0100] In some embodiments, the catholyte enters the cathode chamber through a single inlet port. In other embodiments, the catholyte enters the cathode chamber through one or more ports located elsewhere in the electroplating tank. In some cases, there is a single inlet for the bath of the tank, which is at the periphery of the anode chamber and is segmented from the anode chamber tank wall. The inlet is connected to a central catholyte inlet manifold at the bottom of the tank and the anode chamber. In certain disclosed embodiments, the main catholyte manifold chamber feeds a plurality of catholyte chamber inlet holes (e.g., 12 catholyte chamber inlet holes). In various cases, these catholyte chamber inlet holes are divided into two groups: a first group that feeds the catholyte to the cross-flow injection manifold 222, and a second group that feeds the catholyte to the CIRP manifold 208. In various embodiments, the catholyte flows only through cross-flow and does not flow vertically upward through the membrane or through the CIRP manifold 208; however, in certain embodiments, the CIRP manifold 208 contains the catholyte but the electroplating is mainly performed by cross-flow in the cross-flow region 226.
[0101] As mentioned, the catholyte entering the cathode chamber flows into the cross-flow injection manifold 222, through the holes 246 in the spray head 242, and then into the cross-flow region 226. Flow entering directly from the cross-flow injection manifold region 222 can enter via the cross-flow restriction ring entry port (sometimes referred to as the cross-flow side inlet 250), parallel to the wafer and discharged from one side of the trough.
[0102] In some embodiments, the fluid entering the cathode chamber is directed to a plurality of channels distributed around the periphery of the cathode chamber portion of the electroplating tank chamber (usually the peripheral wall). In a specific embodiment, 12 such channels are included in the wall of the cathode chamber.
[0103] The channels in the cathode chamber wall can be connected to corresponding "cross-flow feed channels" in the membrane frame. Some of the feed channels deliver cathode electrolyte directly to the CIRP manifold 208. In some embodiments, the CIRP 206 may include multiple microchannels for allowing fluid to flow directly to the cross-flow region 226. Although not described, all embodiments herein can be implemented in the following manner: not only including cross-flow electrolyte, but also including upward flow of electrolyte through channels in the CIRP to impinge on the surface of the wafer. When microchannels are used, the cathode electrolyte provided to the manifold will then pass through the vertically oriented small channels of the CIRP 206 and then enter the cross-flow region 226 as a jet of cathode electrolyte.
[0104] As mentioned, in the embodiment depicted in the drawings, the catholyte is fed to the "CIRP manifold chamber" through 6 of the 12 catholyte feed lines / tubes. These 6 main tubes or lines feeding the CIRP manifold 208 are located below the exit cavity of the cross-flow confinement rings (where the fluid flows out of the cross-flow zone 226 below the wafer) and opposite all of the cross-flow zone components (cross-flow spray manifold 222, showerheads 242, and confinement ring inlet cavities).
[0105] As depicted in various figures, some of the cross-flow feed channels 258 in the membrane frame lead directly to the cross-flow injection manifold 222 (e.g., 6 of 12). These cross-flow feed channels 258 begin at the bottom of the anode compartment of the cell, then pass through matching channels of the membrane frame 274, and then connect with corresponding cross-flow feed channels 258 on the lower portion of the CIRP 206. For example, see Figure 3 .
[0106] In a specific embodiment, see Figure 3 , there are six separate feed channels 258 for delivering catholyte directly to the crossflow injection manifold 222 and then to the crossflow region 226. In order to create a crossflow in the crossflow region 226, these channels 258 exit into the crossflow region 226 in an azimuthally non-uniform manner. Specifically, they enter the crossflow region 226 at a specific side or azimuth region of the crossflow region 226. Figure 3In the particular embodiment shown, the fluid path for directly delivering catholyte to the cross-flow injection manifold 222 passes through four separate elements before reaching the cross-flow injection manifold 222: (1) a dedicated channel in the anode chamber wall within the tank, (2) a dedicated channel in the membrane frame 274, (3) a dedicated channel in the CIRP 206 (i.e., not a 1-D channel for delivering catholyte from the CIRP manifold 208 to the cross-flow region 226), and finally, (4) a flow path in the wafer cross-flow confinement ring 210.
[0107] As mentioned, in the membrane frame, the portion of the flow path that passes through the membrane frame 274 and feeds the cross-flow injection manifold 222 is referred to as the cross-flow feed channel 258. In various embodiments, microchannels are not present in the CIRP and are not used to deliver the catholyte to the cross-flow region 226. However, if microchannels are present in the CIRP, the "cross-flow feed channel" includes both the catholyte feed channel 258 that feeds the cross-flow injection manifold 222 and the catholyte feed channel that feeds the CIRP manifold 208. In the case where microchannels are not used, the cross-flow feed channel includes the catholyte feed channel 258 that feeds the cross-flow injection manifold 222.
[0108] refer to Figure 3 , the flow path of the catholyte moves in an upward vertical direction as the catholyte passes through the cross-flow feed channels 258 in the plate 206, and then it enters the cross-flow injection manifold 222 formed in the body of the CIRP 206. The cross-flow injection manifold 222 is an azimuthal cavity, which can be a channel dug into the CIRP 206 that is capable of distributing fluid from each individual feed channel 258 (e.g., from each of the individual 6 cross-flow feed channels) to the various multiple flow distribution holes of the cross-flow injector plate. Such a cross-flow injection manifold 222 is positioned along a corner portion of the perimeter or edge region of the CIRP 206. See, e.g. Figure 3 . In some embodiments, the cross-flow injection manifold 222 is formed in a C-shaped structure at an angle of about 90° to 180° in the peripheral area of the plate. In some embodiments, the angle range of the cross-flow injection manifold 222 is about 120° to about 170°, and in a more specific embodiment is between about 140° and 150°. In these or other embodiments, the angle range of the cross-flow injection manifold 222 is at least about 90°. In many implementations, the nozzle 242 spans approximately the same angular range as the cross-flow injection manifold 222. In addition, the overall inlet structure (which in many cases includes one or more of the cross-flow injection manifold 222, the nozzle 242, the nozzle hole 246, and the opening in the cross-flow restriction ring) can span these same angular ranges.
[0109] In some embodiments, the cross-flow in the injection manifold 222 forms a continuous fluid-coupled chamber within the CIRP 206. In this case, all of the cross-flow feed channels 258 feeding the cross-flow injection manifolds (e.g., all six) enter a continuous and connected cross-flow injection manifold chamber. In other embodiments, the cross-flow injection manifold 222 and / or the cross-flow injectors 242 are divided into two or more angularly different and fully or partially separated sections, such as Figure 5 (which shows 6 separated sections). In some embodiments, the number of angularly separated sections is between about 1-12, or between about 4-6. In a specific embodiment, each of these angularly different sections is fluidly connected to a separated cross-flow feed channel 258 disposed in the CIRP 206. Thus, for example, there may be six angularly different and separated sub-regions within the cross-flow injection manifold 222. In certain embodiments, each of these different sub-regions of the cross-flow injection manifold 222 has the same volume and / or the same angular range.
[0110] In many cases, the catholyte flows out of the cross-flow spray manifold 222 and through a cross-flow sprayhead plate having a plurality of angled, spaced-apart catholyte discharge ports (holes). See, e.g. Figure 3 and Figure 6 .
[0111] Flow path of a cross-flow conduit
[0112] Figure 6 A top view depicting the embedded cross-flow injection manifold 222 within the CIRP 206 is shown, along with the spray head 242 and the cross-flow region 226 of 139 outlet holes. Also shown are all six fluid adjustment rods 270 for the cross-flow injection manifold flow. In this drawing, the cross-flow restriction ring 210 is not installed, but the outline of the cross-flow restriction ring gasket 238 sealing between the cross-flow restriction ring 210 and the upper surface of the CIRP 206 is shown. Figure 6 Other elements shown in FIG. 2 include cross-flow restricting ring fasteners 218 , membrane frame 274 , and screw holes 278 on the anode side of CIRP 206 (eg, which may be used for cathode shield inserts).
[0113] In some embodiments, the geometry of the cross-flow restriction ring outlet can be adjusted to further optimize the cross-flow pattern. For example, the situation where the cross-flow pattern bifurcates to the edge of the restriction ring 210 can be corrected by reducing the opening area of the outer area of the cross-flow restriction ring outlet. In certain embodiments, the outlet manifold includes separated parts or ports, much like the cross-flow injection manifold 222. In some embodiments, the number of outlet parts is between about 1-12, or between about 4-6. The ports are separated along the azimuth and occupy different (usually adjacent) positions along the outlet manifold. In some cases, the relative flow rate through each port can be controlled separately. This control can be achieved, for example, by using a control rod similar to the control rod described relative to the inlet flow. In another embodiment, the flow through different parts of the outlet can be controlled by the geometry of the outlet manifold. For example, an outlet manifold with a smaller opening area near each side edge and a larger opening area near the center will result in a solution flow pattern in which more flows flow out near the center of the outlet and less flows flow out near the edge of the outlet. Other methods of controlling the relative flow rates through the ports in the outlet manifold may also be used (eg, pumps, etc.).
[0114] As mentioned, most of the electrolyte entering the cathode chamber is directed individually to the cross-flow injection manifold 222 and the CIRP manifold 208 through multiple channels 258 (e.g., 12 separate channels). In some embodiments, the flows through these separate channels 258 are controlled independently of each other by appropriate mechanisms. In some embodiments, the mechanism involves a separate pump for delivering fluid into the separate channels. In other embodiments, a single pump is used to supply the main cathode manifold, and various adjustable flow restriction elements can be set in one or more channels of the feed flow path, and the flow path is set to adjust the relative flow between each channel 258 and between the cross-flow injection manifold 222 and the CIRP manifold 208 area and / or along the angular periphery of the slot. In the various embodiments depicted in the figures, one or more fluid regulating rods 270 (sometimes also referred to as flow control elements) are arranged in the channels in which independent control is provided. In the depicted embodiment, the fluid regulating rod 270 provides an annular space in which the cathode electrolyte is constrained when it flows toward the cross-flow injection manifold 222 or the CIRP manifold 208. In the fully retracted state, the fluid regulating rod 270 provides substantially no resistance to flow. In the fully engaged state, the fluid regulating rod 270 provides maximum resistance to flow and, in some implementations, stops all flow through the passage. In an intermediate state or position, the rod 270 provides an intermediate level of restriction to flow as the fluid flows through the constrained annular space between the inner diameter of the passage and the outer diameter of the fluid regulating rod.
[0115] In some embodiments, adjustment of the fluid adjustment rod 270 enables an operator or controller of the electroplating cell to promote flow to the cross-flow jet manifold 222 or to the CIRP manifold 208. In certain embodiments, independent adjustment of the fluid adjustment rod 270 in the channel 258 that directly delivers electrolyte to the cross-flow jet manifold 222 enables an operator or controller to control the azimuthal component of the fluid flow flowing into the cross-flow region 226.
[0116] For example, in some embodiments, the cross-flow showerhead plate is integrated into the CIRP 206, such as Figure 6 246 . In some embodiments, the showerhead plate is bonded, bolted, or otherwise secured to the top of the cross-flow jet manifold 222 of the CIRP 206. In certain embodiments, the top surface of the cross-flow showerhead 242 is flush with or slightly above the plane or top surface of the CIRP 206. In this manner, the catholyte flowing through the cross-flow jet manifold 222 may initially travel vertically upward through the showerhead aperture 246, then travel laterally under the cross-flow confinement ring 210, and enter the cross-flow region 226, such that the catholyte enters the cross-flow region 226 in a direction substantially parallel to the top surface of the channeled ion-resistive plate. In other embodiments, the showerhead 242 may be oriented such that the catholyte flowing out of the showerhead aperture 246 is already traveling in a direction parallel to the wafer.
[0117] In one specific embodiment, the cross-flow showerhead 242 has 139 angled, spaced catholyte outlet holes. More generally, any number of holes that reasonably construct a uniform cross-flow within the cross-flow region 226 may also be employed. In some embodiments, there are between about 50 and about 300 such catholyte outlet holes in the cross-flow showerhead 242. In certain embodiments, there are between about 100 and 200 such holes. In some embodiments, there are between about 120 and 160 such holes. Typically, the size of the individual ports or holes may range in diameter from about 0.020" to 0.10", more specifically from about 0.03" to 0.06".
[0118] In some embodiments, the holes are arranged in a uniformly angular manner (e.g., the spacing between the holes is determined by the fixed angle between the center of the slot and two adjacent holes) along the entire angular range of the cross-flow nozzle 242. See, for example, Figure 3 and 7. In other embodiments, the holes are distributed along the angular range in an angularly non-uniform manner. However, in other embodiments, the angularly non-uniform hole distribution is still a linear ("x" direction) uniform distribution. In other words, in the latter case, the hole distribution is such that the holes are equally spaced if projected onto an axis perpendicular to the direction of the crossflow ("x" direction). Each hole is positioned at the same radial distance from the center of the slot and is spaced the same distance from adjacent holes in the "x" direction. The effective effect of having these angularly non-uniform holes is that the overall crossflow pattern is more uniform.
[0119] In some embodiments, the direction of catholyte flow out of cross-flow showerhead 242 is further controlled by wafer cross-flow restriction ring 210. In certain embodiments, the ring 210 extends around the entire circumference of CIRP 206. In some embodiments, the cross-flow restriction ring or front insert has an L-shape in cross section, such as Figure 3 and 4 As shown. In some embodiments, the wafer cross-flow restriction ring 210 includes a series of flow guiding elements, such as directional fins 266 that are fluidly connected to the outlet hole of the cross-flow nozzle 242. More specifically, the directional fins 266 are largely defined below the upper surface of the wafer cross-flow restriction ring 210 and in an isolated fluid channel between adjacent directional fins 266. In some cases, the purpose of the directional fins 266 is to redirect and restrict the flow leaving the cross-flow nozzle hole 246 from another radially inward direction to a "left to right" flow trajectory (the left is the inlet 250 side of the cross-flow, and the right is the outlet side 234). This helps to establish a substantially linear cross-flow pattern. The cathode electrolyte leaving the hole 246 of the cross-flow nozzle 242 is oriented by the directional fins 266 along the streamline of the flow generated by the orientation of the directional fins 266. In some embodiments, all the directional fins 266 of the wafer cross-flow restriction ring 210 are parallel to each other. This parallel configuration helps to establish a uniform cross-flow direction within the cross-flow region 226. In various embodiments, the directional fins 226 of the wafer cross flow restriction ring 210 are arranged along both the inlet 250 and outlet sides 234 of the cross flow region 226. For example, Figure 7 shown in top view.
[0120] As noted, the catholyte flowing in the cross-flow region 226 generally flows from the inlet 250 region of the wafer cross-flow confinement ring 210 to the outlet side 234 of the ring 210, which will be referred to below as Figure 9-13Further illustrated is the cross-flow conduit. A certain amount of catholyte may also leak around the entire periphery of the substrate. This leakage may be minimal compared to the amount of catholyte that leaves the cross-flow region at the outlet side 234. In some embodiments, at the outlet side 234, there are multiple directional fins 266 that can be parallel to the directional fins 266 on the inlet side and can be aligned with the directional fins 266 on the inlet side. The cross-flow passes through the channels created by the directional fins 266 on the outlet side 234 and then ultimately and directly flows out of the cross-flow region 226. The flow then generally radially outwardly enters another area of the cathode chamber and passes over the chip holder 254 and the cross-flow confinement ring 210 and then through the cross-flow conduit 280 to a fluid containing unit confined by the plating tank weir wall 282 for collection and recycling. It should therefore be understood that the accompanying drawings (e.g., Figure 3 and 4 ) shows only a partial path of the entire path of the catholyte entering and leaving the cross-flow region. Figure 3 and 4 In the illustrated embodiment, for example, fluid flowing out of the cross-flow region 226 does not pass through small holes or flow back into a channel similar to the feed channel 258 on the inlet side when it accumulates in the above-mentioned accumulation region, but flows outward in a direction generally parallel to the chip.
[0121] Cross-flow injection module with flow path inlet
[0122] Figures 8A-8B 250 relative to the electroplating cup 254. The location of the cross-flow inlet 250 is at least partially defined by the location of the cross-flow restriction ring 210. Specifically, the inlet 250 can be considered to be the beginning where the cross-flow restriction ring 210 ends. Note that in the case of the initial design, as shown in FIG. Fig. 8A As shown, the confinement ring 210 ends (and the inlet 250 begins) below the edge of the wafer, whereas in a modified design, such as Figure 8B 226, the end / start point is below the plating cup and radially outward from the edge of the wafer compared to the initial design. In addition, the cross-flow injection manifold 222 in the early design has a step in the cross-flow annulus (where the generally left arrow begins to rise upward), which potentially creates some unwanted turbulence near the point where the fluid enters the cross-flow region 226. In some cases, edge flow elements (not shown) may be present near the periphery of the substrate and / or the periphery of the channeled ion-resistive plate. Near the inlet 250 and / or near the outlet (at Fig. 8A and 8BEdge flow elements may be present (not shown). Edge flow elements may be used to direct electrolyte into the corner formed between the plating surface of the substrate and the edge of the cup 254, thereby counteracting the relatively low cross flow that would otherwise be in this area.
[0123] Crossflow Duct Components
[0124] As above for Figure 4 As described, provided herein is an apparatus and method for diverting cross-flow in a plating tank to reduce foam generation and improve electrolyte flow during electroplating. Various embodiments disclosed herein relate to a flow diversion device, referred to as a cross-flow conduit (CFC), which diverts the cross-flow as it leaves the area below the wafer to minimize splashing, air entrainment, and subsequent foaming. Certain electroplating chemicals contain additives that tend to generate foam under high convection. Significant foam generation can cause errors in level sensors in the plating tank and plating bath reservoir, and can contaminate and corrode components as foam grows and migrates to other areas of the electroplating hardware.
[0125] Relative to the flow through the upper portion of the CIRP weir or any other weir (shown in Figure 1C and 1D The cross-flow solution is diverted into a cross-flow conduit containing a cutout in the CIRP, a cutout in the membrane frame, and a cutout in the plating tank, and then out into an external tank fluid containment unit that collects the solution and then drains it back into the bath. The point at which the flow leaves the CFC and meets the collected solution in the plating tank container is below the level of the solution. That is, the flow flows below the surface of the liquid rather than falling into a reservoir, more like an under-tow than a waterfall.
[0126] In various embodiments, the cross-flow conduit may also include various restrictor plates to maintain sufficient solution levels above the CIRP, which is necessary for proper wafer wetting as the wafer enters. The restrictor plates may be fixed, have a variable orifice design, or adjusted by a pressure relief valve. The cross-flow conduit may be built into the various hardware components (front side insert, CIRP, membrane frame, plating tank), or may be an attachable piece that mounts to and uses existing hardware. Figure 9-14 These various embodiments are described.
[0127] One embodiment involves a flow diverting device, referred to as a cross flow conduit (CFC), which diverts the cross flow as it exits the area beneath the wafer to minimize splashing, air entrainment, and subsequent foaming. Fig. 9 An example is provided in . Fig. 9A simplified diagram of a cross section of a portion of a plating tank apparatus according to certain disclosed embodiments where the cathode electrolyte exits is shown. The cross section includes a plating tank 900 having a tank weir wall 982, wherein the fluid containing unit 940 retains the fluid from the plating tank 900 when the fluid exits on the exit side of the cross flow. The plating tank 900 includes a CIRP 906 and a membrane frame 974. A channel is cut into the CIRP (at the edge closest to the cross flow exit). The same channel is also cut into the membrane frame 974 and the plating tank 900. These channels together create a cross flow conduit 980, wherein the front side insert 910 has the function of a roof / ceiling of the CFC, which diverts the cross flow solution to the bottom of the fluid container 940 (below the solution level) without mixing with air. Due to minimal interaction with the fluid and air and because the fluid no longer impacts on the tank wall 982 when leaving the cross flow, the generation of foam can be avoided. The plating tank 900 also includes an outlet for the fluid containing unit 940. The CIRP 906 and insert 910 are separated by a narrow channel 999 so that the insert 910 is used to hold the cup 902 in place to support the wafer 945. The insert 910 includes a weir wall 910w to contain the overflow area of the fluid above the upper portion of the insert 910 to ensure continuous flow of fluid above the wafer 945. The fluid flow from the cross-flow flows under the wafer 945, under the cup 902 in the narrow gap between the cup and the CIRP, through the narrow channel 999 between the insert 910 and the CIRP 906, down through the cross-flow conduit 980 to the fluid containment cell 940 where the fluid is then recirculated and drawn back to the inlet on the other side of the plating tank.
[0128] Fig.10 An exploded view of the different components of the electroplating tank is shown, including, from left to right, the electroplating tank 1010, the membrane frame 1012, the CIRP 1014, and the front insert 1016. The CIRP 1014, the membrane frame 1012, and the electroplating tank 1010 each include an opening 1020 on the annular outlet side so that when these openings are aligned, a cross-flow conduit is formed to allow fluid to flow downward through the CIRP opening, the membrane frame opening, and the electroplating tank opening (each of which is referred to as a component of the cross-flow conduit) to reach the outlet. The illustration of the tank shows that the upper portion of the opening is the cross-flow conduit inlet 1020a and the bottom of the opening is the cross-flow conduit outlet 1020b. The cross-flow conduit 1020 is also shown in both the membrane frame and the CIRP. As mentioned above Fig. 9As described above, the bottom of the front insert 1016 serves as the "roof" of the cross-flow conduit. The cross-flow conduit 1020 (also referred to as the channel formed by the opening of the plating tank, membrane frame, CIRP and limited by the bottom surface of the insert) is a channel in which the cross-flow is diverted from above the CIRP to below the fluid level into the containment area without mixing with the air turbulence. The cross-flow conduit can span four components of the entire plating tank device.
[0129] Regardless of the inherent foaming tendency of any chemical, certain disclosed embodiments are suitable for using ultra-high cross-flow for all electroplating chemicals. This will result in improved electroplating performance, including: higher Ag incorporation %, improved WiF uniformity, edge reduction, lower WiD for die types containing features with different critical dimensions, and other performance. WiF is the non-uniformity within the feature, which is a measure of the upper contour shape of an independent feature (bump / pillar). It is determined by taking the maximum height of each feature minus the minimum height and then taking the average of all features. In general, an average feature top with a small WiF is preferred, rather than a dome feature top with a higher WiF. WiD is the non-uniformity within the die, which is a measure of the height variation of all features within the die. It is usually calculated in the following way: take the half width of the bump height in each die, that is, the maximum value minus the minimum value and then divided by 2 ((max-min) / 2), take the average value over the entire wafer, and then divide it by the average bump height, and finally convert it to a percentage. Lower WiD values are preferred because they ensure that all bumps have proper solder contact when the final package is assembled. Improved convection can result in better ion transport to the bottom of the features, thereby increasing the plating rate and thus resulting in an overall higher wafer yield.
[0130] Flow Restrictor
[0131] Certain embodiments described herein also include an optional flow restrictor, which may be a flow restrictor plate or a valve. The flow restrictor plate can be used with a cross-flow conduit to modulate the flow of a fluid, by ensuring that sufficient fluid levels are maintained above the insert, so that the fluid can leave via an outlet but still maintain a continuous flow of the fluid on the wafer. Generally speaking, a flow restrictor can block about 15% to about 85% of the opening in the cross-flow conduit. In certain embodiments, the flow restrictor plate is a "smile" shaped plate in which various holes are cut, and various holes can change the flow restrictions at different regions of the cross-flow conduit. For example, there may be between about 25 holes and about 75 holes, or a continuous hole, or up to 500 small holes. Each hole may have the same size or may have different sizes, depending on the desired flow. The thickness of the flow restrictor plate may be between about 1mm and about 75mm and may span up to 100% of the cross-flow conduit length, which extends radially from one end of the cross-flow conduit to the other end. In various embodiments, the flow restrictor plate is positioned between the membrane frame and the slots but may also be positioned in other areas of the cross-flow conduit. In various embodiments, a flow restrictor valve is positioned in the cross-flow conduit.
[0132] Fig.11A An example of a flow restrictor plate 1170 between a membrane frame 1174 and a plating cell 1100 is shown having a cup 1102, a wafer 1145, an insert 1110 with a weir 1110w, a CIRP 1106, a membrane frame 1174, a plating cell weir wall 1182, and a fluid containment cell 1140. This example involves a fixed plate that modulates flow in a cross-flow conduit 1180 with a fixed orifice using a flow restrictor plate 1170. Care should be taken to reduce unnecessary pressure on the plating solution pump while ensuring proper wetting of the wafer as it enters by maintaining sufficient restriction to the upper portion of the insert 1110 to allow continuous wetting with sufficient fluid levels. In this embodiment, the weir has been moved from the CIRP to the flow insert 1110 as shown at the insert weir 1110w. Flow arrows 1199 show the direction of flow. A flow restrictor plate 1170 is attached to the CFC 1180 between the plating cell 1100 and the membrane frame 1174. An appropriate restrictor may be selected to maintain a sufficient fluid level above the CIRP / insert (necessary for proper wafer wetting as the wafer enters) while not overly restricting exit (adding unnecessary pressure head to the plating solution pump). The restrictor plate may be formed in a variety of outlet opening areas, with a variety of geometries, and made from a variety of materials (e.g., stainless steel, titanium, polyethylene terephthalate (PET), polycarbonate, polytetrafluoroethylene (PTFE)). Fig. 11BExamples of various geometric features are provided in 11-A, 11-B, and 11-C show various options for a single continuous hole in a flow restrictor plate, each hole being an opening of a different size, but ultimately spanning the entire plate. 11-D contains three separate cavities for certain openings (although the openings are shown as having similar sizes, it should be understood that cavities of various sizes and shapes can be used). In addition, 11-E, 11-F, 11-G, and 11-H show the option of using a circular hole, which has different types of holes that can be used depending on the desired flow. Each restrictor plate is a single, fixed size, and must be manually replaced if a different restrictor plate is desired.
[0133] Although Fig.11A Use a single size, fixed restrictor plate, but Fig.12 Another alternative embodiment of a restrictor plate 1270 using a motor driven variable orifice is provided. In this embodiment, the restrictor outlet size can be automatically adjusted by an externally controlled stepper motor 1270m or pneumatic line. Automatic control of the outlet size can adjust the fluid containment liquid level in real time to accommodate liquid surges during wafer / cup entry or large flow rate changes. The variable orifice can also adjust the back pressure induced on the plating pump by adjusting the outlet size so that it is small enough to maintain solution above the CIRP but not overly restrictive. As Fig.11A , Fig.12 The plating tank 1200 includes a plating tank weir wall 1282, a membrane frame 1274, a CIRP 1206, an insert 1210 with a weir 1210w, a cup 1202, and a wafer 1245. The opening of the CFC 1280 is regulated by a variable orifice flow restrictor plate 1270 to regulate the flow that ultimately leaves and reaches the fluid containment unit 1240.
[0134] Fig.13 Another embodiment involving a pressure relief valve is shown. Fig.11A and 12 , Fig.13 The embodiment includes a plating tank 1300 having a plating tank weir wall 1382, a membrane frame 1374, a CIRP 1306, an insert 1310 having a weir 1310w, a cup 1302, and a wafer 1345. The opening of the CFC 1380 is regulated by a pressure relief valve 1370 to regulate the flow of liquid that eventually leaves and reaches the fluid containing unit 1340. The pressure relief valve 1370 includes a spring 1370a and an O-ring 1370b. It should be understood that although in Fig.131302 is a spring embodiment, but various pressure relief valves may be used. In this embodiment, rather than restricting CFC 1380 to ensure that weir 1310w remains full, a pressure relief "valve" 1370 is used to seal the flow when cup 1302 is not in place. The embodiment includes a rod, spring 1370a, O-ring 1370b, and a series of holes in a membrane frame 1374. When cup 1302 is not in place, there is no dynamic pressure on valve 1370 and spring 1370a overcomes the static pressure, closing valve 1370. When cup 1302 is in place, the dynamic pressure of the fluid overcomes the spring force and opens valve 1370. The advantage of this embodiment is that it is low restriction when cup 1302 is in place, and high restriction when cup 1302 is not in place. Various pressure relief valves may be used in various embodiments. For example, a diaphragm may be used instead of a spring for some pressure relief valves.
[0135] In an alternative embodiment, an attachable steering device can be used as a retrofit kit for adjusting a device with CIRP, inserts, and a slot structure (the slot structure does not have a pre-cut channel for forming a cross-flow conduit). The device can be made of any chemically matched polymer (polycarbonate, PET, PPS, PE, PP, PVC, ABS). The opening size is about the same as that used in the integrated version described above and can have a similar restrictor plate as the integrated version. Fig.14 An example of an attachable steering device 1400 is included as shown in 14-A and 14-B, which can be attached (in a removable manner) to the rear end of the electroplating tank apparatus 1430 at the area where the cross-flow fluid exits. This device is an attachable component that can be installed into an existing electroplating process kit (requiring minimal hardware modifications for implementation). 14-B shows only the attachable steering device 1400. As shown in FIG. Fig.14 As shown in , the apparatus diverts the plating fluid downward, as indicated by arrow 1410 in 14-B and arrow 1420 in 14-D, eliminating the risk of splashing and forming foam on the upper portion of the weir.
[0136] application
[0137] Certain disclosed embodiments are suitable for use with a variety of applications. For example, certain embodiments may be suitable for use when flowing specific electrolyte chemicals. Exemplary surfactants that can be used in electrolyte chemicals suitable for use in disclosed embodiments with cross-flow conduits include: poly(ethylene glycol), poly(propylene glycol), pyridinium, or polyethyleneimine. In addition, the cross-flow conduit device is particularly suitable for flowing solutions with specific metal complexing agents or ligands such as silver complexing agents. Ethylenediaminetetraacetic acid (EDTA) is a complexing agent, but many chemical manufacturers use proprietary complexing agents for chemical baths containing silver. The disclosed embodiments are also suitable for use with grain refiners such as saccharin, bis-3-sulfopropyl disulfide, or 3-mercaptopropyl sulfonate.
[0138] The disclosed apparatus described herein is also suitable for use in electroplating apparatus for electroplating in through silicon via features, through resist plating applications commonly used in many WLP processes such as forming pillars, redistribution layers, micro-pillars, giant pillars, vias, and damascene processes (for filling nanoscale interconnects and trenches).
[0139] Device controller
[0140] In some embodiments, the device includes hardware for completing process operations and a system controller with instructions for controlling process operations according to the disclosed embodiments. The system controller will generally include one or more memory devices and one or more processors configured to execute instructions so that the device will execute the method according to the disclosed embodiments. A machine-readable medium containing instructions for controlling process operations according to the disclosed embodiments can be coupled to the system controller. Specifically, in some embodiments, the controller will specify the dwell time, the vertical moving distance of the substrate holder, the maximum vertical acceleration and deceleration of the substrate holder, the rotation speed of the substrate holder, the rotation step angle, the maximum acceleration and deceleration of the substrate holder, the current and / or voltage applied to the substrate (which may or may not be modulated or otherwise controlled in the manner described herein), the relative and absolute timing for moving the substrate holder, changing the current or voltage applied to the substrate, adjusting the flow restrictor plate that the orifice can be changed and / or adjusting the flow rate, and any combination thereof. In some embodiments, the user provides the desired dwell time and maximum rotation acceleration to the controller, and the controller is programmed to perform the entire method sequence based on these values and the values of other parameters stored in the memory. In some other embodiments, the user can additionally specify the desired level of the applied current and / or the applied voltage. In a specific embodiment, when the cross-flow region is in a sealed and unsealed state, the applied current or the applied voltage is modulated between a higher value and a lower value, respectively, and the controller can be programmed to ensure that only when the cross-flow region is in a sealed state, a higher current or a higher voltage is applied to the substrate. For example, after determining that the substrate holder has reached its lower position and thus seals the substrate holder, the controller can increase the applied current or the applied voltage from a lower value to a higher value. Similarly, before the substrate holder begins to move upward and unseal the cross-flow region, the controller can reduce the applied current or the applied voltage from a higher value to a lower value. This cautious timing can ensure that unless the cross-flow region is properly sealed, a higher current or a higher voltage will not be applied to the substrate, thereby ensuring that the limiting current will not be exceeded when the cross-flow region is in an unsealed state (when the limiting current is relatively low).
[0141] In some implementations, the controller is part of a system, which can be part of the above-described embodiments. Such a system can include a semiconductor processing device, which includes one or more processing tools, one or more chambers, one or more platforms for processing, and / or specific processing components (wafer pedestals, gas flow systems, etc.). These systems can be integrated with electronic devices to control the operation of these systems before, during, or after the processing of semiconductor wafers or substrates. Electronic devices can be referred to as "controllers", which can control various components or sub-parts of one or more systems. Depending on the processing requirements and / or the type of system, the controller can be programmed to control any of the processes disclosed herein, including controlling the delivery of electroplating fluids, power settings, wafer rotation, position and operation settings, wafer entry and exit tools and other transfer tools and / or the transmission of load locks connected to or interfaced with a specific system.
[0142] Broadly speaking, a controller can be defined as an electronic device with various integrated circuits, logic, memory, and / or software that receives instructions, issues instructions, controls operations, enables cleaning operations, enables endpoint measurements, etc. The integrated circuit may include a chip storing program instructions in the form of firmware, a digital signal processor (DSP), a chip defined as an application specific integrated circuit (ASIC), and / or one or more microprocessors or microcontrollers that execute program instructions (e.g., software). Program instructions may be instructions delivered to a controller or system in the form of various different settings (or program files), and different settings (or program files) define operating parameters for performing specific processing on or for a semiconductor wafer or to a system. In some embodiments, the operating parameters may be a part of a recipe for one or more processing steps in the manufacturing process of one or more (kinds) layers, materials, metals, oxides, silicon, silicon dioxide, surfaces, circuits, and / or bare chips defined by a process engineer to complete a wafer.
[0143] In some embodiments, the controller can be a part of or coupled to a computer that is integrated with the system, coupled, or connected to the system or a combination thereof through a network. For example, the controller can be in the "cloud" or all or part of a wafer factory (fab) host system, which can allow remote access to wafer processing. The computer can enable remote access to the system to monitor the current progress of the manufacturing operation, check the history of past manufacturing operations, check the trends or performance standards of multiple manufacturing operations, change the parameters of the current processing, set the processing steps to follow the current processing or start a new process. In some examples, a remote computer (e.g., a server) can provide a process recipe to the system through a network, which can include a local network or the Internet. The remote computer can include a user interface that allows input or programming of parameters and / or settings, which are then transmitted from the remote computer to the system. In some examples, the controller receives instructions in the form of data that specify the parameters of each processing step to be performed during one or more operations. It should be understood that these parameters can be for the type of process to be performed and the type of tool, and the controller is configured to connect or control the tool type. Thus, as described above, the controller may be distributed, for example, by including one or more discrete controllers that are networked together and work toward a common goal (e.g., the process and control described herein). Examples of distributed controllers for these purposes may be one or more integrated circuits within the chamber that communicate with one or more remote integrated circuits (e.g., at the platform level or as part of a remote computer) that combine to control the process within the chamber.
[0144] In various embodiments, system control software can be used to realize the control of relevant processing variables / conditions. Such software can control one or more of the relevant reactor operations. In a specific example, the software control program manipulates the position of the substrate holder (e.g., thereby controlling whether the cross-flow region is sealed), the current and / or voltage applied to the substrate (as described in the text, which can be modulated between a higher value and a lower value), and the relative timing of the substrate holder position and the current or voltage applied to the substrate. In some embodiments, one or more of these reactor operations can be realized by making one reactor operation depend on another reactor operation. Sometimes this is referred to as a reactor operation or component "subordinate" to another reactor operation or component. For example, (a) the firmware (sometimes referred to as the lifting firmware) and (b) the firmware controlling the power supply can be jointly controlled in this way. In an example, the firmware controlling the position of the substrate holder can depend on the firmware controlling the power supply, so that the substrate holder is only raised or lowered as indicated by the power supply firmware. For example, when the firmware controlling the power supply indicates that the power supply has reached a lower applied current or applied voltage, the substrate holder can be raised to unseal the cross-flow region. In another example, the firmware controlling the power supply may be dependent on the firmware controlling the position of the substrate holder, such that the power supply gradually increases / decreases the current as the substrate holder moves. For example, when the firmware controlling the position of the substrate holder indicates that the substrate holder has reached its lower position, thereby sealing the cross-flow region, the power supply may begin to increase the current or voltage applied to the substrate.
[0145] Exemplary systems may include, but are not limited to, plasma etching chambers or modules, deposition chambers or modules, spin rinse chambers or modules, metal plating chambers or modules, cleaning chambers or modules, chamfer edge etching chambers or modules, physical vapor deposition (PVD) chambers or modules, chemical vapor deposition (CVD) chambers or modules, atomic layer deposition (ALD) chambers or modules, atomic layer etching (ALE) chambers or modules, ion implantation chambers or modules, track chambers or modules, and any other semiconductor processing system that may be associated with or used in the preparation and / or manufacture of semiconductor wafers.
[0146] As described above, depending on one or more process steps to be performed by the tool, the controller can communicate with one or more other tool circuits or modules, other tool components, combination tools, other tool interfaces, adjacent tools, adjacent tools, tools located throughout the factory, a host computer, another controller, or tools used in material handling to move containers of wafers to and from tool locations and / or load ports in a semiconductor manufacturing facility.
[0147] The above-described apparatus / process can be used in conjunction with a photolithographic patterning tool or process, for example, for preparing or manufacturing semiconductor devices, displays, light emitting diodes, photovoltaic panels, etc. Typically, but not necessarily, such tools / processes will be used or performed with ordinary manufacturing facilities. The photolithographic patterning of films generally includes some or all of the following steps, each of which can be implemented using a number of possible tools: (1) applying a photoresist to a workpiece, i.e., a substrate, using a spin coating or spray coating tool; (2) curing the photoresist using a hot plate or heating furnace or a UV curing tool; (3) exposing the photoresist to visible light or ultraviolet light or X-ray light using a tool such as a wafer exposure machine; (4) developing the resist to selectively remove the resist and patterning the resist using a tool such as a wet bench; (5) transferring the resist pattern into an underlying film or workpiece by using a dry or plasma assisted etching tool; and (6) removing the resist using a tool such as an RF or microwave plasma resist stripper.
[0148] In some embodiments, the device also includes a flow restriction element that is positioned peripherally in the gap between the CIRP and the substrate holder and extends along the periphery of the CIRP. In these embodiments, the flow restriction element can form the wall of the cross-flow region. In some embodiments, the substrate-facing surface of the flow restriction element is circular, and the element is referred to as a flow restriction ring. When a flow restriction ring is used, a sealing member is configured to seal the outlet between the substrate holder and the substrate-facing surface of the flow restriction ring. Preferably, the sealing member seals at least 75% of the periphery of the ring. In an embodiment illustrated by the accompanying drawings and by experimental data, the sealing member seals 100% of the periphery of the ring. Note that when a flow restriction ring is used, the inlet and outlet for the electrolyte cross-flow region are positioned closer to the ion-resistive element than to the substrate-facing surface of the flow restriction ring. In some embodiments, the surface of the flow restriction ring facing the ion-resistive element is shaped to provide an outlet (outlet (e)) for cross-flow of the electrolyte. A suitable flow restriction ring is in Figure 7 An example of a cross-flow direction is shown in Figure 1E Shown in.
[0149] In other embodiments, the flow restriction element has a substrate-facing surface that extends only partially along the periphery of the ion-resistive element. Such a flow restriction element can have a wall that extends partially along the periphery of the ion-resistive element and a discharge region including one or more gaps, wherein the angle subtended by the discharge region is between about 20 degrees and 120 degrees. The gap in the discharge region can be used as an outlet for cross flow (outlet (e)). Such an element is also referred to as a diverter and is described herein. In these embodiments, a sealing member is positioned to seal the outlet between the substrate holder and the substrate-facing surface of the flow restriction element.
[0150] Modulate the applied current or voltage
[0151] During electroplating, electric current and / or voltage are supplied to the electroplating device in a certain way so that material is deposited on the substrate as cathode. When utilizing controlled current control electroplating process, relevant electric current is referred to as applied electric current. When utilizing controlled current control electroplating process, relevant potential is referred to as applied potential or applied voltage. In various embodiments herein, during electroplating, for example, when regulating cross flow region between sealed and unsealed state, applied electric current or applied potential can be modulated.
[0152] Sealed and unsealed cross-flow regions affect fluid dynamic conditions that affect the electroplating process. For example, when the cross-flow region is unsealed, a certain amount of electrolyte will leak out through the leakage gap between the substrate holder and the cross-flow confinement ring. Due to this leakage, the linear velocity of the electrolyte passing over the electroplating surface of the substrate is relatively low. In contrast, when the cross-flow region is sealed, no electrolyte (or less electrolyte in the case of incomplete sealing) leaves through the leakage gap, so the linear velocity of the electrolyte passing over the electroplating surface of the substrate is relatively high. Thus, the mass transfer of the electroplating surface of the substrate is relatively low when the cross-flow region is unsealed, and the mass transfer of the electroplating surface of the substrate is relatively high when the cross-flow region is sealed.
[0153] The mass transfer degree of the electroplating surface of the substrate has a strong influence on the current or voltage applied to the substrate. For example, it is usually desired to electroplate at the highest current or voltage that can be supported to deposit a film quickly, thereby maximizing the output. The highest current / voltage that can be supported is respectively referred to as limiting current or limiting voltage. These numerical values are affected by many factors, and these factors include, for example, the composition of the electrolyte and the fluid dynamic conditions in the deposition device. When electroplating occurs at the applied current or voltage that exceeds the limiting current or voltage, there is no sufficient metal support in the electrolyte to apply the current or voltage. Therefore, undesirable side reactions (such as hydrogen precipitation) and poor electroplating results can occur. For example, the film formed under the current that exceeds the limiting current is usually porous, includes dendritic growths and has poor electrical properties (such as low conductivity) and mechanical properties (such as shear strength).
[0154] Since the fluid dynamic conditions when the cross-flow region is sealed are different from the fluid dynamic conditions when the cross-flow region is unsealed, the limiting current and limiting voltage are also different for these two states. For example, when the cross-flow region is sealed and there is a relatively large mass transfer to the electroplated surface of the substrate, the limiting current and limiting voltage are relatively high. This is because there are relatively more metal ions at the electroplated surface of the substrate when the cross-flow region is sealed compared to when the cross-flow region is unsealed and the mass transfer to the electroplated surface of the substrate is relatively low.
[0155] The applied current or voltage is selected to ensure that the limiting current / limiting voltage is not exceeded during any part of the electroplating process. For example, in the case where the cross-flow region is adjusted between sealed and unsealed states and only a single current is applied during the entire electroplating period, the applied current should be selected so that the current applied when the cross-flow region is in the unsealed state does not exceed the limiting current. Since the limiting current is higher when the cross-flow region is in the sealed state, this also ensures that the applied current will never or rarely exceed the limiting current. A disadvantage of this scheme (e.g., using a single applied current) is that deposition occurs at a lower applied current than the current that can be supported when the cross-flow region is in the sealed state.
[0156] In order to overcome this limitation, thereby maximizing yield, the applied current or voltage can be modulated with the cross-flow region. In this way, the electroplating device can be operated under conditions close to the limiting current or voltage during the entire deposition process, thereby maximizing yield and achieving high-quality film deposition at the same time. In various examples, a relatively low current is applied to the substrate when the cross-flow region is not sealed and a relatively high current is applied to the substrate when the cross-flow region is sealed. Similarly, in some examples, a relatively low voltage is applied to the substrate when the cross-flow region is not sealed and a relatively high voltage is applied to the substrate when the cross-flow region is sealed.
[0157] In certain embodiments, the material is plated at both higher and lower levels of applied current or applied voltage. When the cross-flow region is not sealed and a lower current or voltage is applied to the substrate, a small amount of material or in some cases no more than a negligible amount of material is plated onto the substrate in these or other cases. In some embodiments, this means that when the cross-flow region is sealed, at least about 70% by weight (in some cases at least about 99% by weight) of the electrodeposited material can be deposited onto the substrate.
[0158] Characteristics of ion-resistive elements
[0159] Electrical functions
[0160] In some embodiments, CIRP 206 approximates a nearly constant and uniform current source in the vicinity of the substrate (cathode), and, therefore, in some cases, may be referred to as a high resistance virtual anode (HRVA). As described above, when provided in plate form, the element may also be referred to as a channeled ion-resistive plate (CIRP). Typically, CIRP 206 is placed in close proximity to the wafer. In comparison, an anode that is also in close proximity to the substrate will be significantly less prone to providing a nearly constant current to the wafer, but will simply support a constant potential surface on the anode metal surface, allowing the current to be maximum where the net resistance from the anode surface to the endpoint (e.g., a peripheral contact point on the wafer) is small. Therefore, although CIRP 206 has been referred to as a high resistance virtual anode (HRVA), this does not mean that the two are electrochemically interchangeable. Under optimal operating conditions, CIRP 206 will more closely approximate and perhaps be better described as a virtual uniform current source, where a nearly constant current is supplied from the upper plane of the entire CIRP 206. While the CIRP can certainly be considered a "virtual current source," i.e., it is the plane from which current emanates, and since it can be considered the place or source from which the anodic current emanates, it can be considered a "virtual anode," the relatively high ionic resistivity of the CIRP 206 (relative to the electrolyte) results in nearly uniform current flow across its entire face, and results in a further advantageous overall superior wafer uniformity compared to having a metal anode in the same physical location. The plate's resistance to the flow of ionic current increases with increasing specific resistivity of the electrolyte contained within the channels of the plate 206 (often, but not always, having a resistivity that is the same or nearly similar to that of the catholyte), increasing plate thickness, decreasing porosity (less partial cross-sectional area for current flow, e.g., fewer pores of the same diameter, or the same number of pores of a smaller diameter, etc.).
[0161] structure
[0162] In many but not all embodiments, the CIRP 206 contains micro-sized (typically less than 0.04") through-holes that are spatially and ionically isolated from each other and do not form interconnecting channels within the bulk of the CIRP. These through-holes are often referred to as non-connected through-holes. They typically extend in one dimension, usually but not necessarily perpendicular to the plated surface of the wafer (in some embodiments, the non-connected holes are angled relative to the wafer, which is generally parallel to the front surface of the CIRP). Generally, the through-holes are parallel to each other. Typically, these holes are arranged in a square array. In other cases, the layout is an offset spiral pattern. These through-holes are different from three-dimensional porous networks, in which the through-holes are formed by the wafer. The through holes regulate both the flow of ionic current and the flow of fluid parallel to the surface therein, and straighten the paths of both the flow of current and the flow of fluid toward the wafer surface, so that the channels extend in three dimensions and form an interconnected pore structure. However, in certain embodiments, such a porous plate with an interconnected network of holes can be used instead of a one-dimensional channeled element (CIRP). When the distance from the top surface of the plate to the wafer is small (e.g., a gap of about 1 / 10 the size of the wafer radius, e.g., less than about 5 mm), the flow of current and the divergence of the flow of fluid are both locally confined, transmitted, and aligned with the CIRP channels.
[0163] An exemplary CIRP 206 is a disk made of a solid, non-porous dielectric material that is ionically resistive and electrically resistive. The material is chemically stable in the plating solution used. In some cases, the CIRP 206 is made of a ceramic material (e.g., aluminum oxide, tin oxide, titanium oxide, or a mixture of metal oxides) or a plastic material (e.g., polyethylene, polypropylene, polyvinylidene fluoride (PVDF), polytetrafluoroethylene, polysulfone, polyvinyl chloride (PVC), polycarbonate, etc.) and has between about 6,000 and 12,000 non-interconnecting through holes. In many embodiments, the CIRP disk 206 is substantially coextensive with the wafer (e.g., when a 300 mm wafer is used, the diameter of the CIRP disk 206 is about 300 mm) and is placed in close proximity to the wafer, such as directly below the wafer in a wafer-face-down electroplating apparatus. Preferably, the electroplated surface of the wafer is within about 10 mm, more preferably within about 5 mm, of the closest CIRP surface. To this end, the top surface of the CIRP 206 can be flat or substantially flat. Typically, both the top and bottom surfaces of CIRP 206 are flat or substantially flat.
[0164] Another characteristic of CIRP 206 is the diameter or major dimension of the through-holes and its relationship to the distance between CIRP 206 and the substrate. In some embodiments, the diameter of each through-hole (or the diameter of a majority of the through-holes, or the average diameter of the through-holes) is no greater than the distance from the plated wafer surface to the nearest surface of CIRP 206. Thus, in these embodiments, when CIRP 206 is placed within about 5 mm of the plated wafer surface, the diameter or major dimension of the through-holes should not exceed about 5 mm.
[0165] As described above, the overall ionic resistance and flow resistance of the plate 206 depends on the thickness of the plate as well as both the overall porosity (the fraction of the area available for flow through the plate) and the size / diameter of the holes. A plate with low porosity will have a higher impact flow rate and ionic resistance. Comparing plates of the same porosity, a plate with smaller diameter 1-dimensional holes (and therefore a larger number of 1-dimensional holes) will have a more microscopically uniform distribution of current across the wafer because there are more individual current sources, which behave more as point sources that can be distributed over the same gap, and have a higher overall pressure drop (high viscous flow resistance).
[0166] However, as described above, in some cases, the ion-resistive plate 206 is porous. The holes in the plate 206 may not form independent one-dimensional channels, but may form a through-hole grid that may or may not be interconnected. It should be understood that as used herein, the terms channeled ion-resistive plate and channeled ion-resistive element (CIRP) are intended to include this embodiment unless otherwise specified.
[0167] In some embodiments, the CIRP 206 can be modified to include (or accommodate) an edge flow element. The edge flow element can be an integral part of the CIRP 206 (e.g., the CIRP and the edge flow element together form an integral structure), or it can be a replaceable component mounted on or near the CIRP 206. The edge flow element promotes a higher degree of cross flow, and therefore promotes shear forces on the substrate surface, near the edge of the substrate (e.g., near the interface between the substrate and the substrate holder). In the absence of an edge flow element, an area of relatively low cross flow can be generated near the interface of the substrate and the substrate holder, for example due to the geometry of the substrate and the substrate holder and the flow direction of the electrolyte. The edge flow element can serve to enhance the cross flow in this area, thereby promoting more uniform electroplating results across the substrate. Further details regarding the edge flow element are described below.
[0168] Distance between wafer and CIRP
[0169] In some embodiments, the wafer holder 254 and associated positioning mechanism hold the rotating wafer in close proximity to the parallel upper surface of the CIRP 206. During electroplating, the substrate is typically positioned so that it is parallel or approximately parallel to the ion-resistive element (e.g., within about 10°). Although the substrate may have certain features on it, only the generally flat shape of the substrate is considered when determining whether the substrate and the ion-resistive plate are substantially parallel.
[0170] In typical cases, the separation distance is about 0.5-15 mm, or about 0.5-10 mm, or about 2-8 mm. In some cases, the separation distance is about 2 mm or less, such as about 1 mm or less. The separation distance between the wafer and the CIRP 206 corresponds to the height of the cross-flow region. As described above, this distance / height can be adjusted during the electroplating process to promote a higher degree of mass transfer on the substrate surface.
[0171] This small plate-to-wafer distance can produce a plating pattern on the wafer associated with a close "imaging" of individual holes of the pattern, especially near the center of wafer rotation. In this case, a pattern of plating rings (thickness or plating texture) can be produced near the center of the wafer. To avoid this phenomenon, in some embodiments, the individual holes in the CIRP 206 (especially at the center of the wafer and near the center of the wafer) can be constructed to have particularly small sizes, such as less than about 1 / 5 of the plate-to-wafer gap. When coupled with wafer rotation, the small aperture allows the flow rate of the impinging fluid flowing upward as a jet from the plate 206 to be time-averaged and reduce or avoid small-scale non-uniformities (e.g., those on the order of microns). Despite the above precautions, and depending on the properties of the plating bath used (e.g., the specific metal deposited, the conductivity, and the bath additives used), in some cases, due to the time-averaged exposure and close imaging of the pattern of different thicknesses (e.g., in a "bull's eye" shape around the center of the wafer) and corresponding to the individual hole pattern used, deposition may be prone to proceed with a microscopic non-uniform pattern (e.g., a shaped center ring). This can occur and affect deposition if the finite hole pattern produces an inhomogeneous impingement flow pattern. In such cases, it has been found that introducing a lateral flow across the center of the wafer, and / or modifying the regular pattern of holes exactly at and / or near the center, both largely eliminates the evidence of microscopic inhomogeneities otherwise found there.
[0172] Porosity of CIRP
[0173] In various embodiments, CIRP 206 has a porosity and pore size small enough to provide a viscous flow resistance back pressure and a high vertical impingement flow rate at normal operating volume flow rates. In some cases, about 1-25% of CIRP 206 is open area to allow fluid to reach the wafer surface. In a specific embodiment, about 2-5% of plate 206 is open area. In another embodiment, about 5-25%, or about 10-25%, or about 15-25%, or about 15-20% of plate 206 is open area. In a specific embodiment, the open area of plate 206 is about 3.2%, and the effective total open cross-sectional area is about 23cm 2 .
[0174] In general, the CIRP can be more porous in the case where the cross-flow regions are intermittently sealed than in the more conventional case where such sealing does not occur. In conventional cases, the CIRP porosity is sometimes limited to about 5% or less. In various embodiments herein where the cross-flow regions are intermittently (or continuously) sealed, the CIRP porosity can be greater, such as a maximum porosity of about 10%, or about 15%, or about 20%, or about 25%. In some such embodiments, the CIRP can have a minimum porosity of about 3%, or about 5%, or about 10%, or about 15%.
[0175] Hole size for plates with channels
[0176] The porosity of CIRP 206 can be implemented in many different ways. In various embodiments, it is achieved with many vertical holes of small diameter. In some cases, plate 206 is not composed of a single "drilled" hole, but is made of a sintered plate of continuous porous material. An example of such a sintered plate is described in U.S. Patent No. 6,964,792, the entire contents of which are incorporated herein by reference. In some embodiments, the drilled non-connected holes have a diameter of about 0.01 to 0.05 inches. In some cases, the diameter of the holes is about 0.02 to 0.03 inches. As described above, in various embodiments, the diameter of the holes is at most about 0.2 times the gap distance between CIRP 206 and the wafer. The cross-section of the holes is usually, but not necessarily, circular. In addition, in order to simplify the structure, all holes in plate 206 may have the same diameter. However, this is not necessarily the case, and both the individual size and the local density of the holes over the entire plate surface may vary due to specific needs.
[0177] As an example, a solid plate made of a suitable ceramic or plastic material (generally a dielectrically insulating and mechanically strong material) has a large number of small holes disposed therein, for example, at least about 1000 or at least about 3000 or at least about 5000 or at least about 6000 (9465 holes of 0.026 inches in diameter have been found to be useful). As mentioned, some designs have about 9000 holes. The porosity of the plate 206 is sometimes less than about 25%, or less than about 20%, or less than about 5% so that the total flow rate required to produce a high impact velocity is not too large. The use of smaller holes helps to produce a large pressure drop across the plate compared to larger holes, thereby helping to produce a more uniform upward velocity through the plate.
[0178] Generally, the distribution of holes throughout the CIRP 206 has a uniform density and is non-random. However, in some cases, the density of holes may vary, particularly in the radial direction. In a specific embodiment, as described more fully below, there is a greater density and / or diameter of holes in the region of the plate that directs flow toward the center of the rotating substrate. Additionally, in some embodiments, holes that direct electrolyte at or near the center of a rotating wafer may direct flow at non-perpendicular angles relative to the wafer surface. Additionally, the hole pattern in this region may have a random or partially random distribution of non-uniform plating "rings" to account for possible interactions between a limited number of holes and a rotating wafer. In some embodiments, the hole density adjacent to the open portion of a diverter or confinement ring 210 is lower than the hole density in regions of the CIRP 206 that are farther from the open portion of the connected diverter or confinement ring 210.
[0179] Protrusion
[0180] In certain embodiments, the top surface of the CIRP may be modified to increase the maximum deposition rate and improve plating uniformity across the surface of the wafer and within individual plated features. The modification of the CIRP top surface may take the form of a collection of protrusions.
[0181] A protrusion is defined as a structure placed / attached on the substrate-facing side of the CIRP in the cross-flow region extending between the CIRP plane and the wafer. The CIRP plane (also called the ion-resistive element plane) is defined as the top surface of the CIRP, excluding any protrusions. The CIRP plane is where the protrusions connect to the CIRP and where fluid flows from the CIRP into the cross-flow region.
[0182] The protrusions can be oriented in a variety of ways, but in many embodiments, the protrusions are in the form of long, thin ribs located between the columns of holes in the CIRP and are oriented so that the length of the protrusion (i.e., its major / longest dimension) is perpendicular to the cross-flow through the cross-flow region. In some cases, the width of the protrusion can be less than about 1 mm. In some cases, the aspect ratio of the protrusion is at least about 3:1, or at least about 4:1, or at least about 5:1.
[0183] In many implementations, the protrusions are oriented so that their lengths are perpendicular or substantially perpendicular to the cross-flow direction across the wafer surface (sometimes referred to herein as the "z" direction). In some cases, the protrusions are oriented at different angles or groups of angles.
[0184] A wide variety of protrusion shapes, sizes, and layouts may be used. In some embodiments, the protrusions have faces that are substantially perpendicular to the surface of the CIRP, while in other embodiments, the protrusions have faces that are positioned at an angle relative to the face of the CIRP. In other embodiments, the protrusions may be shaped so that they do not have any flat faces. Some embodiments may employ a variety of protrusion shapes and / or sizes and / or orientations.
[0185] Alternative embodiments of ion-resistive elements
[0186] In various embodiments, the ion-resistive element may have characteristics that are different from those described above. For example, although many of the foregoing descriptions refer to the CIRP as a plate, the ion-resistive element may also be configured as a membrane, filter, or other porous structure. Examples of porous structures that can be used as ion-resistive elements include, but are not limited to, ion-resistive membranes and filters, nanoporous cationic membranes, and other porous plates and membranes with appropriate ionic resistivities. Broadly speaking, such ion-resistive elements can be shaped, sized, positioned, and have the same or similar characteristics as those described above for the ion-resistive plate with channels. Therefore, any description provided herein with respect to the CIRP (e.g., regarding size, porosity, ionic resistivity, materials, etc.) may also be applied to different ion-resistive elements used in place of the CIRP.
[0187] Such structures may also have certain characteristics that differ from those described herein with respect to CIRP. For example, the ion-resistive membrane used in place of CIRP may be thinner than a typical CIRP. In certain embodiments, the porous structure used in place of CIRP may be disposed on a support or other structure for structural stability. In some embodiments, the ion-resistive element may have through holes that are interconnected, while in other cases, the through holes may be non-interconnected.
[0188] In cases where the cross-flow region is defined between the substrate and a supported membrane or sintered element structure (e.g., a supported filter medium, sintered glass, or porous ceramic element), the pore size of each hole can be less than about 0.01 inches. For this type of undrilled continuous porous material, the open area can be larger than the open area of a channeled plate made by drilling individual holes in a solid sheet of material (e.g., greater than about 30% open area, with a maximum open area of about 50% or 40% in some embodiments). Ion-resistant structures made from non-drilled continuous porous materials can utilize smaller pore sizes (e.g., compared to drilled CIRPs) to impart viscous flow resistance to avoid short-circuiting electrolyte through the membrane / element surface. There is a balance between pore size, open area, and net flow resistance to avoid flow short-circuiting. Higher porosity materials / structures typically utilize smaller pores and / or greater element thicknesses to achieve this balance.
[0189] An example of a suitable material of this type is a mechanically strong filter media sheet, stretched across and supported from below by an open framework network, having an average pore size of less than about 5 μm, a porosity of about 35% or less, and a thickness of 0.001 inch or more. Several specific examples of suitable sheet membranes include SelRO nanofiltration MPF-34 membranes, HKF-328 polysulfone ultrafiltration membranes, and MFK-618 0.1 μm pore size polysulfone membranes provided by Koch Membrane Systems, Inc. (Willington, MA). Cationic and anionic membranes (e.g., Nafion TM ) because they offer high resistance to flow and the ability to conduct ionic electricity across the membrane. In the case where the ion-resistive element is a sintered (fused) porous glass or ceramic element, the thickness of the element as well as the average and maximum pore sizes determine the resistance to flow through the ion-resistive element. Typically, the resistance to flow through the ion-resistive element (whether implemented as a membrane, filter, sintered / fused glass element, porous ceramic element, CIRP, etc.) should allow for a static water pressure of less than about 100 milliliters per minute (ml / min) per inch per square centimeter of surface area, more typically less than about 20 ml / min / cm 2 / in of water, for example less than about 5ml / min / cm 2 / in of water.
[0190] Edge Flow Element
[0191] In many implementations, the electroplating results can be improved by using edge flow elements and / or flow inserts. Generally speaking, edge flow elements affect the flow distribution near the periphery of the substrate, near the interface between the substrate and the substrate holder. In some embodiments, the edge flow element can be integrated with the CIRP. In some embodiments, the edge flow element can be integrated with the substrate holder. In other embodiments, the edge flow element can be a separate component that can be mounted on the CIRP or the substrate holder. The edge flow element can be used to adjust the flow distribution near the edge of the substrate as required by a specific application. Advantageously, the flow element promotes a high degree of cross flow near the periphery of the substrate, thereby promoting more uniform (from the center to the edge of the substrate), high-quality electroplating results. The edge flow element is typically located at least partially radially inside the inner edge of the substrate holder / the periphery of the substrate. In some cases, the edge flow element can be at least partially located at other locations, such as below the substrate holder and / or radially outside the substrate holder, as further described below. In some figures of this article, the edge flow element is referred to as a "flow element".
[0192] The edge flow element can be made of a variety of materials. In some cases, the edge flow element can be made of the same material as the CIRP and / or substrate holder. Generally speaking, the material of the edge flow element is electrically insulating.
[0193] Another method of improving the cross flow near the periphery of the substrate is to use fast substrate rotation. However, fast substrate rotation presents its own set of disadvantages, and can be avoided in various embodiments. For example, if the substrate is rotated too fast, it can prevent the formation of enough cross flow across the substrate surface. Therefore, in some embodiments, the substrate can be rotated at a speed between about 50-300RPM, for example, at a speed between about 100-200RPM. Similarly, the cross flow near the periphery of the substrate can be promoted by using a relatively small gap between CIRP and the substrate. However, the smaller CIRP-substrate gap leads to a more sensitive and more stringent tolerance range of the process variables. The electroplating process.
[0194] Edge flow elements may be installed to help overcome low convection and low plating rates near the edge of the wafer. This may also help overcome differences due to different photoresist / feature heights.
[0195] In certain embodiments, the edge flow element may be shaped so that the cross flow in the cross flow region is more favorably directed into the corner formed by the substrate and substrate holder.A variety of shapes may be used to achieve this goal.
[0196] It should be understood that the configuration and / or method described herein are exemplary in nature, and these specific embodiments or examples are not considered in a limiting sense, because many variations are feasible. The specific routine or method described in the present invention can represent one or more of the processing strategies of any number. Therefore, the various operations shown can be performed in the sequence shown, performed in other sequences, performed in parallel or omitted in some cases. Equally, the order of the above method can be changed.
[0197] The subject matter of the present disclosure includes all novel and nonobvious combinations and subcombinations of the various methods, systems and configurations disclosed herein, and other features, functions, operations, and / or properties, as well as any and all equivalents thereof.
[0198] Additional Embodiments
[0199] Some observations showing that improved cross flow through cross flow region 226 is desirable are presented in this section. In this section, two basic plating tank designs were tested. Both designs include a confinement ring 210, sometimes referred to as a diverter, defining a cross flow region 226 on top of the CIRP 206. Neither design includes an edge flow element, but such an element can be added to either setup as needed. The first design, sometimes referred to as a control design and / or TC1 design, does not include a side inlet to the cross flow region 226. In contrast, in the control design, all flows entering the cross flow region 226 originate below the CIRP 206 and travel upward through the holes in the CIRP 206, then impact on the wafer and flow across the face of the substrate. A second design, sometimes referred to as the second design and / or the TC2 design, includes a cross-flow injection manifold 222 and all associated hardware for injecting fluid directly into the cross-flow region 226 without passing through channels or holes in the CIRP 206 (note, however, that in some cases, the flow delivered to the cross-flow injection manifold passes through dedicated channels near the periphery of the CIRP 206 that are different and / or separate from the channels used to direct fluid from the CIRP manifold 208 to the cross-flow region 226).
[0200] Other Implementations
[0201] Although some details of the foregoing embodiments have been described for the purpose of clarity of understanding, it will be apparent that certain changes and modifications may be made within the scope of the appended claims. It should be noted that the processes, systems, and devices of the embodiments of the present invention may be implemented in many alternative ways. Therefore, the embodiments of the present invention should be regarded as illustrative rather than restrictive, and the embodiments are not limited to the specific details provided herein.
Claims
1. An electroplating device, comprising: an electroplating cell configured to contain an electrolyte and an anode when electroplating a metal onto a substrate, the electroplating cell having a chamber wall of a fluid containing cell having a fluid level during electroplating; a substrate holder configured to hold the substrate so that a plating surface of the substrate is separated from the anode during electroplating; a channeled ion-resistive plate comprising a substrate-facing surface separated from said electroplating surface of said substrate by a cross-flow region; a cross-flow inlet of the cross-flow region, which is used to provide electrolyte to the cross-flow region; as well as A cross-flow conduit comprising a channel for diverting the electrolyte from the cross-flow region to an outlet feeding the fluid containing unit of the electroplating tank, wherein the outlet is below the fluid level and the cross-flow region is between the cross-flow inlet and the cross-flow conduit, wherein the electroplating device further comprises a membrane frame below the ion-resistive plate with the channel, wherein the cross-flow conduit further comprises a second channel in the membrane frame, wherein the second channel is for diverting the electrolyte from the cross-flow region to the inlet of the fluid containing unit leading to the electroplating tank.
2. An electroplating apparatus according to claim 1, wherein the cross-flow region is at least partially defined by: an upper surface of the channeled ion-resistive plate, a lower surface of the substrate in the substrate holder when in operation, and an insert.
3. The electroplating apparatus according to claim 1, wherein the cross-flow conduit is configured to receive the electrolyte flowing out of the cross-flow region and guide the electrolyte to flow downward and away from the surface of the substrate.
4. The electroplating device according to claim 1 further comprises a flow restrictor for limiting the flow of the electrolyte in the cross-flow conduit.
5. The electroplating apparatus according to claim 4, wherein the flow restrictor is at least one of: a plate inserted below the ion-resistive plate having channels; a motor-driven variable orifice plate capable of varying the size of the opening of the cross-flow conduit; or A pressure relief valve controls the flow of electrolyte through the cross-flow conduit based on the pressure of the electrolyte in response to the presence of a substrate in the electroplating cell.
6. The electroplating apparatus according to claim 5, further comprising a controller having executable instructions, wherein the executable instructions are used to electroplate a material onto the substrate by: Passing an electrolyte across a surface of the substrate from one side of the substrate to an opposite side of the substrate by cross flow; When the electrolyte flows to the opposite side of the substrate, diverting the flow of the electrolyte to below the level of the fluid for collection in the fluid containing unit; as well as The motor-driven variable orifice plate is used to widen and narrow the opening of the cross-flow conduit in response to the flow rate of the electrolyte.
7. The electroplating apparatus of claim 1, wherein the cross-flow conduit is an attachable diverting device that can be attached to the electroplating tank.
8. The electroplating apparatus according to any one of claims 1 to 7, further comprising a weir wall.
9. A method for electroplating on a substrate in a plating bath, comprising: receiving a substrate in a substrate holder, wherein the substrate holder is configured to support the substrate such that a plating side of the substrate is separated from an anode during electroplating; immersing the substrate in an electrolyte, wherein a cross-flow region is formed between the electroplating surface of the substrate and an upper surface of an ion-resistive plate having channels; causing the electrolyte in contact with the substrate in the substrate holder to flow from beneath the channeled ion-resistive plate, through the cross-flow region, across the channeled ion-resistive plate, and out of the cross-flow conduit; regulating the opening of the cross-flow conduit using a flow restrictor; as well as electroplating material onto the plating surface of the substrate while flowing the electrolyte and adjusting the opening of the cross-flow conduit; wherein the electroplating cell comprises a membrane frame having an opening, wherein the cross-flow conduit is at least partially defined by the opening in the membrane frame, and wherein causing the electrolyte to flow out of the cross-flow conduit comprises causing the electrolyte to flow through the opening in the membrane frame.
10. The method according to claim 9, wherein: The electroplating tank includes a fluid containing unit for holding the electrolyte after the electrolyte has passed through the cross-flow region, wherein the fluid containing unit has a fluid level during electroplating, wherein the cross-flow conduit includes a channel for diverting electrolyte from the cross-flow region to an outlet feeding the fluid containing unit, and wherein the outlet is below the fluid level in the fluid containing unit.
11. The method of claim 9, wherein the cross-flow conduit is configured to receive electrolyte flowing out of the cross-flow region and direct the electrolyte to flow downwardly away from the surface of the substrate.
12. The method according to claim 9, wherein: The flow restrictor includes a motor-driven variable orifice plate capable of varying a size of an opening to the cross-flow conduit, and wherein adjusting the opening of the cross-flow conduit includes engaging the motor-driven variable orifice plate.
13. The method according to claim 9, wherein: The flow restrictor includes a pressure relief valve that seals electrolyte flow based on a pressure of the electrolyte in response to whether a substrate is present in the electroplating tank, and wherein adjusting the opening of the cross-flow conduit includes adjusting the pressure relief valve.
14. The method according to claim 9, wherein: The cross-flow conduit includes an attachable diverting device that can be attached to the electroplating tank.
15. The method according to any one of claims 9 to 13, wherein: During electroplating, the cross-flow conduit prevents electrolyte from flowing over the weir walls of the electroplating tank.
16. A method for electroplating on a substrate in a plating bath, the method comprising: receiving a substrate in a substrate holder, wherein the substrate holder is configured to hold the substrate such that a plating side of the substrate is separated from an anode during electroplating; immersing the substrate in an electrolyte, wherein a cross-flow region is formed between the electroplating surface of the substrate and an upper surface of an ion-resistive plate having channels; as well as flowing the electrolyte in contact with the substrate in the substrate holder from beneath the channeled ion-resistive plate, through the cross-flow region, across the channeled ion-resistive plate, through the cross-flow conduit, and through an outlet feeding a fluid containment cell; wherein the fluid containing unit has a fluid level during electroplating, wherein said outlet feeding said fluid containing cell is below said fluid level in said fluid containing cell; and Wherein, the cross-flow conduit includes an attachable steering device capable of being attached to the electroplating tank.
17. The method according to claim 16, wherein: The channeled ion-resistive plate includes an opening, and wherein the cross-flow conduit is at least partially defined by the opening in the channeled ion-resistive plate.