Removal of by-products (impurities)
By using adsorption filters and a dispersant-free approach in the electrolysis reactor, the problems of anode contamination and performance degradation during dye reduction are solved, achieving longer electrolytic cell life and purer dye products, reducing the presence of aniline risk.
Patent Information
- Application Number
- CN201980078092.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-11-29
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2039-11-29
AI Technical Summary
Existing electrolysis devices have problems with anode contamination and performance degradation during the dye reduction process. In particular, small molecule impurities migrate from the cathode chamber to the anode chamber, causing the anode to become inactive, affecting the purity of the dye and the life of the electrolytic cell.
An electrolysis reactor containing an adsorption filter is designed. Adsorption materials such as activated carbon and zeolite are used to remove molecular impurities in the anode electrolyte. The anode and cathode chambers are separated by semipermeable membrane partitions to control the osmotic pressure difference and prolong cleaning/ regeneration cycle and reduce the decomposition of stabilizers and improve dye purity through a dispersant-free approach.
It effectively reduces anode pollution, extends the service life of electrolytic cells, improves the purity and stability of dyes, especially reduces the presence of aniline in indigo dyes, and reduces health risks to workers.
Smart Images

Figure CN113166953B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of electrolysis with flow-through electrolytic cells suitable for the reduction of vat dyes such as indigo and sulphur dyes. Background Art
[0002] Reduction of vat dyes and sulfur dyes using electrolysis apparatus is known (see for example WO 2007 / 147283 A2). Although electrolysis is a clean method because it involves fewer chemicals than other reduction methods, it suffers from performance degradation after use due at least in part to electrode fouling.
[0003] DE102015202117A1 discloses an electrochemical method for converting carbon dioxide into carbon monoxide, methane or ethane. Undesirable byproducts are formates, which are deposited on the electrode surface. These byproducts are produced in the cathode chamber and are removed therefrom by a filter device located downstream of the gas separation.
[0004] US3,701,719A discloses electrochemical production of olefin oxides from olefins via halohydrin intermediates. An anode and cathode chamber are required to produce intermediates or final products, respectively. With regard to pollutant removal, the document teaches first separating the product, i.e., olefin oxide, from an aqueous medium, then introducing an inorganic oxidant into an aqueous medium containing pollutants, then passing the oxidant-treated aqueous medium through a pollutant removal zone, and recycling the decontaminated aqueous medium to an electrolytic cell.
[0005] None of these references deals with removing non-gaseous by-products or contaminants from a solution containing non-gaseous products. Summary of the invention
[0006] It is therefore a general object of the present invention to provide an electrolytic reactor suitable for dye reduction which has improved performance and lifetime, longer time intervals between regenerations and which preferably also produces purer dyes.
[0007] Now, in order to implement these and further objects of the invention (which will become clearer as the specification unfolds), the electrolysis reactor is characterized in that it comprises at least one electrolysis cell having an anode chamber and a cathode chamber, the chambers being separated by a partition, in particular a semipermeable membrane, the chambers each comprising an inlet and an outlet at opposite ends for the anode electrolyte and the cathode electrolyte, respectively, the inlet and the outlet of each chamber being connected to each other via an anode electrolyte circulation pipe or a cathode electrolyte circulation pipe, the anode electrolyte circulation pipe being equipped with an anode electrolyte container to form an anode electrolyte circuit, and the cathode electrolyte circulation pipe being equipped with a main container to form a cathode electrolyte circuit, wherein the anode electrolyte circulation pipe is further equipped with at least one adsorption filter, the adsorption filter comprising an adsorption material for adsorbing molecular impurities.
[0008] In the following description, some terms are used, and their meanings are further defined as follows:
[0009] In combinations, such as a diluted suspension, a suspension comprising a leuco dye, the term "suspension" also refers to the cathode electrolyte, provided that the suspension is disclosed as being fed to an electrolytic cell. The final reduced product is also referred to as leuco dye solution.
[0010] The term "alkaline electrolyte" does not necessarily mean that it has an alkaline pH, ie pH>7, but rather that it is a freshly supplied (ie dye-free) electrolyte solution. However, it is generally preferred that the alkaline electrolyte has an alkaline pH.
[0011] As used herein, the term "tube" encompasses all hollow cylindrical devices, ie, includes not only rigid tubes but also flexible tubes.
[0012] Within the scope of the present invention, it has been found that due to the osmotic pressure difference between the cathode compartment and the anode compartment, small molecules present in the substances used or produced by the electrolysis can migrate from one compartment through the partition, in particular the semipermeable membrane, to the other compartment and contaminate the electrodes. In particular in dye reduction processes, small molecules migrate from the cathode to the anode compartment, in particular the anode itself, thereby affecting the performance of the anode. In the case of indigo, such molecular impurities are specifically aniline. If such molecules are able to polymerize or otherwise react to insoluble substances due to the conditions in the anode compartment or the anode itself, the anode loses its activity and the electrolytic cell must be shut down for a potentially time-consuming anode cleaning.
[0013] The present invention is particularly suitable for dye reduction and is therefore described in more detail in such preferred embodiments.
[0014] Using a suitable filter, molecular impurities can be removed to a high degree from the anolyte, resulting in less contamination of the anode, greater time intervals between cleaning / regeneration cycles, and maintaining an osmotic pressure difference. If the only impurities present are derived from impurities in the dye, the migration of impurities driven by osmotic pressure from the cathode chamber to the anode chamber consumes such impurities from the cathode electrolyte, producing a purer cathode electrolyte. If small molecules are produced during the reduction process, and if the migration of such molecules driven by osmotic pressure from the cathode chamber to the anode chamber is faster than the production of such molecules, a cleaner cathode electrolyte is also obtained.
[0015] Depending on the type of molecule to be removed, different adsorbent filter materials can be used, in particular adsorbent filter materials that can be easily regenerated. For example, the boiling point of aniline (one of the main impurities in indigo dyeing) is about 184°C, so the adsorbent material can be regenerated at a temperature of about 200°C, with additional application of vacuum at lower temperatures or for shorter periods of time.
[0016] Suitable adsorption filter materials are, for example, activated carbon and molecular sieves such as zeolites. For a good anolyte to flow through the adsorption filter, a particle size of about 1-3 mm, in particular about 2 mm, is preferred. Depending on the size of the adsorption filter, the desired flow rate, the concentration of impurities in the anolyte and the adsorption characteristics (kinetics and thermodynamics), the packing density of the adsorbent material can vary, and the shape of the adsorbent particles (i.e., spherical or irregular) can also vary. The optimal conditions for a specific process can be easily evaluated.
[0017] A preferred electrochemical cell of the present invention comprises a particle cathode, particularly a conductive carbon cathode such as a graphite cathode.
[0018] In another preferred embodiment, the catholyte comprises a vat dye or a sulfur dye, more preferably indigo.
[0019] Removing small molecules such as aniline, which is one of the impurities present in indigo, not only reduces deposits on the anode, but also produces a purer leuco dye and therefore also a purer colored fabric. This is a major advantage, especially in the case of aniline, which is known to be a strong blood poison.
[0020] Dye cathode electrolytes usually contain suspension stabilizers, in particular dispersants, also called dispersing agents. If such stabilizers are not stable enough under reducing conditions, in particular if they decompose into small molecules, they will also migrate to the anode compartment and be removed by the adsorption filter, so that the suspension is depleted of dispersants over time, which will affect the suspension stability at least in the early stages of the reduction process.
[0021] Therefore, the use of adsorption filters in the anolyte circuit is particularly suitable for reduction methods that do not involve stabilizers such as dispersants. A novel and creative method has also been developed that does not require a dispersant other than a dye compound, particularly a leuco dye. Such a method is further referred to as a dispersant-free method. Because the leuco dye is too large to pass through the separator, there is no risk that its stability effect is reduced due to exhaustion, because removing this molecule from the anolyte supports osmotic diffusion.
[0022] To initially produce a dispersant-reduced, or in particular dispersant-free, catholyte, i.e. if no corresponding leuco dye solution is available, the reduction or leuco dye production process, respectively, in an electrolysis reactor can be started as follows:
[0023] (i) preparing in a main container or in a first and main container a dilute suspension of the dye in an alkaline electrolyte by circulating and heating the suspension, optionally modifying the suspension by circulating it through one or more ultrasound devices,
[0024] (ii) electrochemically treating the diluted suspension of step (i) in at least one electrolytic cell to obtain a diluted leuco dye solution,
[0025] (iii) optionally sending the diluted leuco dye solution of step (ii) to a first or main vessel where it is supplied with additional dye by circulation and heating to obtain a suspension comprising leuco dye,
[0026] (iv) then circulating the suspension containing the leuco dye of step (iii) through at least one electrolytic cell to electrolytically convert the dye into a leuco dye, or to electrolytically convert the suspension containing the leuco dye into a solution containing the leuco dye, respectively, optionally
[0027] (v) Repeating steps (iii) and (iv) one or more times with the leuco dye solution of step (iv) and additional dye to form a leuco dye solution in an alkaline electrolyte.
[0028] Steps (iii) to (v) are optional, ie they are only carried out when the concentration of the leuco dye obtained in step (ii) is not concentrated enough to provide a suitable suspending effect.
[0029] For indigo as a preferred example, the preferred concentration of the dye suspension in step (i) is 100-200 g / L of an alkaline electrolyte, such as sodium hydroxide at a concentration of 2-10% w / v, preferably 4% w / v. The indigo and indigo white concentrations of the indigo suspension in the first step (iii) are 150-250 g / L, in the second step (iii) are 250-350 g / L, and in the third step (iii) are 300-380 g / L.
[0030] Concentrated leuco dye solution can be prepared by the alkaline electrolyte comprising leuco dye.This alkaline electrolyte comprising leuco dye is produced as shown above, or derives from the previous production of concentrated leuco dye.In the second case, when removing concentrated leuco dye solution batch, some leuco dye solutions stay in the reactor.Then dilute this concentrated leuco dye solution with alkaline electrolyte to form the alkaline electrolyte solution comprising leuco dye.
[0031] A concentrated leuco dye solution can be produced in an electrochemical reactor using an alkaline electrolyte solution containing the leuco dye as follows:
[0032] (i) adding a first portion of the dye to be reacted to form the leuco dye to an alkaline electrolyte solution containing the leuco dye in a first or main container and circulating, optionally passing through one or more ultrasound devices and preferably heating to form a first cathode electrolyte,
[0033] (ii) feeding the first cathode electrolyte of step (i), preferably via a filter for removing oversized particles and optionally a heating device, to at least one electrolytic cell, and
[0034] (iii) starting at least one electrolytic cell by gradually increasing the voltage to a conversion voltage and a maximum conversion power,
[0035] (iv) adding a further portion of the dye to be reacted, thereby increasing the power, preferably to maximum power and continuous conversion,
[0036] (v) optionally repeating step (iv) until the desired concentration of the leuco dye is obtained,
[0037] (vi) converting the dye into a leuco dye until the power drops to a threshold switching power due to the dye conversion,
[0038] (vii) Removal of the leuco dye solution.
[0039] The additional dye may be added by adding a solid dye to the main container, or by feeding a portion of a solution or suspension containing the leuco dye from the main container or the cathode electrolyte circulation loop into a first container where it is diluted with an alkaline electrolyte and the solid dye and circulated to form a suitably uniform suspension which is then supplied to the main container.
[0040] Typically, particularly for indigo, it has been found that leuco dye solutions in alkaline electrolytes (leuco dye concentration being only 5% w / v) can stably suspend up to 20% w / v of the dye, e.g. 5-10% w / v leuco dye for 10-20% w / v dye.
[0041] To produce such a concentrated indigo solution, the following procedure has proven to be good:
[0042] For example, a good final indigo solution is obtained with 300 kg of indigo in 1000-1500 L of electrolyte.
[0043] Initially, a portion of the indigo solution is left in the main container or pumped into the first container, replenished with alkaline electrolyte (e.g. made from concentrated electrolyte and water) and indigo. It has proven to be suitable to keep about 200 L of indigo solution in the container, which is then replenished with 300-600 L of alkaline electrolyte. Due to the additional indigo solution in the tubes and electrolytic cells, etc., the indigo concentration is increased once it mixes with the contents of the tubes, cells, etc. Therefore, although a 5% indigo concentration is sufficient to stabilize a suspension with up to 20% indigo, higher indigo concentrations are usually used. The volume information given below refers to the volume in the first container and the main container.
[0044] The first portion of indigo to be reacted to indigo white, for example 150 kg, is added to 500 L of an alkaline electrolyte solution containing indigo white (preferably 15%-20% indigo white concentration, 2%-10% NaOH concentration, in particular about 4%) in the first container or, if the first container is not present, the main container, and circulated, optionally passed through one or more ultrasound devices, and heated to form a first indigo suspension. If the first container is present, the suspension is circulated through the first container and the ultrasound device for about 30 min. Once pumped into the main container, it is circulated again for about 20 min through a second ultrasound and at least when ready to be supplied to the cathode through a particle filter and a heat exchanger.
[0045] Once the suspension is homogeneous (indigo particle size below 50 μm) and has the desired temperature of about 50° C.-65° C., preferably 60° C., the first indigo suspension is fed into the electrolytic cells (all electrolytic cells of all working stacks in parallel) and then the electrolytic cells, e.g. all electrolytic cells of the stack, are started by increasing the voltage stepwise to the switching voltage and maximum switching power, e.g. from 7 volts to 11 volts at 0.5 volts / about every 2 minutes. All electrolytic cells of one stack and preferably all stacks are fed and started simultaneously. The preparation of step (i) takes about 1-2 hours and the start-up of the electrochemical process takes about 15 minutes.
[0046] At a maximum conversion voltage of 11 volts, the conversion power is about 170 A for an indigo suspension containing 150 kg indigo in 500-800 L indigo catholyte. Once the maximum current is reached, additional indigo, for example 50 kg, is prepared in the indigo solution in the first vessel and supplied to the main vessel, which again generates an enhanced current and continues the reduction. The indigo solution used to suspend the indigo is typically diluted with electrolyte to an indigo concentration of 5-20% weight / volume (w / v), more preferably 10-20%.
[0047] Once all the indigo has been added, for example three times 50 kg indigo in about 150-400 L to a total of 300 kg indigo in 1000-1500 L electrolyte, the power decreases with decreasing indigo concentration. Since no further indigo should be supplied, the voltage also decreases slowly, depending on the measured power or on the indigo concentration, respectively.
[0048] It has also been found that cleaning / regeneration of not only the anode compartment or cathode compartment, respectively, but also the cathode compartment, can be easily performed by cleaning with a strong acid, especially if the process is performed with the above-mentioned improvements. The acidic solution can be circulated through the anode and / or cathode for a specific time, or until the cleaning solution has reached a predetermined or constant impurity level. The anode is then washed with water directly, or with water after washing with a base such as caustic soda, usually also by circulating the base through the anode compartment.
[0049] In the case of, for example, indigo reduction, the acid wash is carried out for a suitable time, for example 10-60 min, followed by washing the bed with a base such as caustic soda (to remove acid and electrode contaminants), followed by washing with water, or less preferably directly with water. Although the washing can be carried out simultaneously for both electrodes (i.e. cathode and anode), in the case of several stacks of electrolytic cells, it is preferred to carry out the cleaning / regeneration of cathodes and anodes in a sequential manner, i.e. first the cathodes of all stacks, in a preferred embodiment one stack at a time, and subsequently cleaning all the anodes of one stack during the suspension preparation.
[0050] The advantage of cleaning the electrodes during the preparation of the suspension is that the entire stack remains in the production of the leuco dye, and since the preparation of a fresh suspension in a batch procedure takes at least 1 hour, while a longer cycle through an ultrasound device, i.e. up to 2 hours, improves the suspension quality, careful cleaning / regeneration of the electrodes and preparation of the suspension require almost the same amount of time. Therefore, carrying out both steps simultaneously does not extend the required time in any way or only minimally.
[0051] The concentration of a suitable acidic solution is 10-100 g / L, more preferably 40-60 g / L, most preferably about 50 g / L, or 0.25-30 M, preferably 1-2 M, more preferably 1.3-1.4 M (referring to protons) in deionized water. If an alkaline solution such as caustic soda is used after the acid solution cleaning, the concentration is typically 10-100 g / L, more preferably 20-60 g / L, most preferably 40 g / L, or 0.1-2.5 M, preferably 0.5-1.5 M (referring to hydroxide) in deionized water.
[0052] For the washing step, the strong acid is preferably selected from HCl, H2SO4, HNO3, and mixtures thereof.
[0053] The cleaning solution may be circulated through a filter to retain small particles of metal sources or worn electrode material, and through a carbon or other adsorbent filter to adsorb dissolved contaminants. BRIEF DESCRIPTION OF THE DRAWINGS
[0054] The present invention will be better understood when considering the following detailed description, and objects other than those mentioned above will become apparent. This specification refers to the accompanying drawings, in which:
[0055] Figure 1 The removal of by-products in a process where a leuco dye is used as dispersant and preferably as the sole dispersant is shown.
[0056] Figure 2a Six stacks are shown schematically, with associated supply and withdrawal lines, and
[0057] Figure 2b A stack is shown in more detail, having five electrolytic cells.
[0058] Figure 3 The major components of the overall electrochemical reactor suitable for by-product removal are shown, and the electrolytic cell is shown in an enlarged view.
[0059] Figure 4 Components of an electrolytic reactor are shown in more detail for preparing a cathode electrolyte in the presence of a first container.
[0060] Figure 5 The preparation of a dye suspension is shown in the presence of a first container and using an in-house produced leuco dye as a dispersant.
[0061] Figure 6 A reactor and method for regenerating electrodes by means of electrode cleaning are shown. For the sake of clarity, the cathode electrolyte and anolyte circulation loops are omitted. There is no circulation of the anolyte and cathode electrolyte in the electrolytic cell during the cleaning process. DETAILED DESCRIPTION
[0062] The process will now be further described with respect to a dye reduction process, in particular an indigo reduction process.
[0063] Figure 1 The basic arrangement of an anolyte circuit is shown, having an electrolytic cell 4 comprising a cathode chamber 41 and an anode chamber 42 separated from each other by a partition 43, in particular a semipermeable membrane. An electrolyte, in particular caustic soda, is supplied to the anolyte container 3 via an anolyte supply pipe 31. The anolyte is supplied from the anolyte container 3 to the anode chamber 42 via an anolyte outlet 32, entering the anolyte circulation loop or the anolyte circulation pipe 33 (which is respectively equipped with an anolyte circulation pump P02). The anolyte enters the anode chamber via an anolyte inlet 421, passes through the anode chamber 42, and returns from the anode chamber 42 to the anolyte container 3 via an anolyte outlet 422a and an anolyte return pipe 422b. An adsorption filter 332 is also provided in the anolyte circulation loop, which can be placed anywhere in the loop, for example as Figure 1 As shown, between the anode electrolyte outlet 422a and the anode electrolyte container 3, or as Figure 3 As shown, between the anolyte outlet 32 of the anolyte container 3 and the anolyte inlet 421 entering the anode chamber 42. Figure 1As shown, the cathode electrolyte enters the cathode chamber 41 from the main container 1 via the cathode electrolyte outlet 12 and the cathode electrolyte supply pipe 151 equipped with a cathode electrolyte supply pump P01, via the cathode electrolyte inlet 411, passes through the cathode chamber 41 and returns to the main container 1 via the reduced cathode electrolyte outlet 412a, the reduced cathode electrolyte return pipe 412b and the reduced cathode electrolyte inlet 13.
[0064] Also like Figure 1 As shown, the cathode electrolyte suspension can be prepared in the first container 2, and in a preferred embodiment, an electrolyte containing a leuco dye is used as the suspension medium, i.e., a medium without a dispersant other than the leuco dye. In a first step, the dye is suspended in the electrolyte and preferably in the first container 2 via an ultrasonic device (e.g. Figure 4 ) is circulated, then sent to the main container 1 and then reduced by circulating it through the cathode chamber 41. Once the reduction is completed, at least a portion of the electrolyte solution containing the leuco dye is returned from the main container 1 to the first container 2 (as shown by the semicircular arrow) by means of a pump P04, where it is supplemented with additional dye and processed as described above.
[0065] If necessary, a further circulation loop can be provided in the main container 1 for improving the suspension before it is supplied to the cathode chamber 41, for example also equipped with ultrasound equipment and optionally also with heating means (see Figure 3 ).
[0066] Although Figure 1 Only one electrolytic cell is shown (and in other figures), but for industrial purposes it is preferred to have at least 4 electrolytic cells in at least two stacks of two electrolytic cells each.
[0067] FIG. 2 shows an arrangement of several stacks 5 of electrolytic cells 4 , each stack comprising several electrolytic cells 4 , and all stacks 5 and all electrolytic cells 4 of one stack 5 being connected in parallel, so that one stack can be isolated for cleaning / regeneration.
[0068] The preferred number of stacking body is at least 4, more preferably 6.In the situation of 6 stacking bodies, usually all in work, but in the situation of maintaining more than 2 hours, preferably 5 in work, and 1 is closed.In the situation of 6 stacking bodies 5, usually separate 1 at each time and be used for cathode cleaning / regeneration in the leuco dye suspension preparation process, thereby the negative electrode of whole stacking bodies is cleaned in 6 days, and all anodes of a stacking body are cleaned together on the 7th day.Because anode needs regeneration less than negative electrode, it has been proved that advantageously after cleaning all negative electrodes, one by one stacking body cleans anode, promptly cleans the negative electrode of each stacking body once a week, and all anodes of one stacking body are cleaned once in 7 weeks.
[0069] The advantage of cleaning the electrodes during the preparation of the suspension is that the entire stack remains in the production of leuco dye, and since the preparation of a new suspension in a batch procedure takes at least 1 hour, while a longer cycle through an ultrasound device, i.e. up to 2 hours, improves the suspension quality, careful cleaning / regeneration of the electrodes and preparation of the suspension require almost the same amount of time. Therefore, carrying out both steps simultaneously does not extend the required time in any way or only minimally.
[0070] Cleaning the cathodes of at least only one stack at a time has several advantages, namely
[0071] - the water required for the preparation of the suspension can be supplied via the cathode of the stack to be regenerated, thereby avoiding the loss of leuco dye,
[0072] - the water required for the suspension preparation is sufficient to remove all the leuco dye from one stack, but may be less effective in the case of several stacks,
[0073] - Less cleaning solution is required because the cleaning solution is recirculated.
[0074] Each stack preferably contains 1 to 10 electrolytic cells, preferably 4 to 6 electrolytic cells, in particular 5 electrolytic cells. For an electrochemical reactor suitable for producing 1000 kg of leuco dye, in particular for example a 30% strength indigo white solution within 24 h, an electrochemical reactor having 6 stacks of 5 electrolytic cells each (usually all 6 stacks, but at least 5 stacks are in operation) has proven suitable, in particular an electrolytic cell with a cathode chamber having a carbon cathode with the following dimensions and particles:
[0075] -0.3m 2 Separator area / cell;
[0076] - The dimensions of the cathode chamber containing granular graphite carbon are 0.4 m high, 0.7 m wide and 0.04 m thick;
[0077] -Carbon particle size is 1mm-0.3mm;
[0078] - The dimensions of the stainless steel cathode current collector and anode are 0.6m high and 0.9m large.
[0079] More information about suitable electrodes can be found in WO 2007 / 147283 A2, the disclosure of which is incorporated herein by reference in its entirety. Such information relates to the determination of, for example, the sphericity and flow properties of the microparticles.
[0080] Figure 3 An electrolysis reactor is shown in more detail, but without the first container 2 .
[0081] like Figure 1As already shown, the anolyte is supplied to the anolyte container 3 via the anolyte supply pipe 31 or once reduction has begun via the anolyte inlet 35, and is supplied to the anode chamber 42 via the anolyte outlet 32, the anolyte pump P02, the anolyte heating device 331 and the anolyte inlet 421. After leaving the anode chamber 42 via the anolyte outlet 422a, the anolyte is recycled to the anolyte container 3 via the anolyte return pipe 422b and the anolyte inlet 35.
[0082] In the anolyte circuit there is an adsorption filter 332. As already indicated, this adsorption filter 332 can be placed anywhere, but if a heating device is present, it is preferably placed just before the anolyte heating device 331, since here the temperature is lowest and thus the adsorption is best.
[0083] On the cathode side of the reactor, the main vessel 1 has a main suspension circulation loop 14, which comprises a main suspension circulation pump P03 and preferably an ultrasound device 141 (see Figure 4 ), used to circulate the suspension, thereby improving its homogeneity.
[0084] After the suspension has circulated for a period of time (depending on the quality of the dye, i.e. its particle size and particle distribution), the main suspension circulation loop 14 is closed and the valve to the cathode electrolyte outlet 12 is opened. The cathode electrolyte is then circulated through the cathode electrolyte circulation loop 15 by pumping it with the cathode electrolyte pump P01, through another optional ultrasound device 154, a particle filter 152 (for removing oversized particles if still present) and a cathode electrolyte heating device (heat exchanger) 153 via the cathode electrolyte supply pipe 151, and enters the cathode chamber 41 of the electrolytic cell 4 separated from the anode chamber 42 by a partition 43 (preferably a semipermeable membrane) via the cathode electrolyte inlet 411. After passing the cathode, the cathode electrolyte returns to the main container 1 via the reduced cathode electrolyte outlet 412a, the reduced cathode electrolyte return pipe 412b and the reduced cathode electrolyte inlet 13.
[0085] As shown in the accompanying drawings 413a and 413b, in a preferred embodiment, the cathode electrolyte direction can be reversed. This helps to avoid blockages caused by the use of particle electrodes in combination with suspensions. Therefore, it is preferred to reverse the flow direction regularly, for example, reverse all the way every 3 minutes. Because the electrolysis should not be affected by the reversal of the flow direction, it is important that the particle bed of the electrode is filled the same in both directions. This is achieved by ensuring that the flow and the particle bed are such that the bed is always pressed tightly against the upper or lower grid, which keeps the particles in the electrode chamber.
[0086] Depending on the type of electrode, the direction of the electrolyte can be reversed in one or both compartments.
[0087] All vessels 1 , 2 , 3 additionally have supplies for nitrogen, caustic soda and optionally further supplies as well as a degasser and a solution removal line for removing leuco dye or, in the case of anode cleaning, anolyte.
[0088] Figure 4 and 5 The preparation of the cathode electrolyte via the first container 2 for suspension preparation is shown. The solid dye from the solid dye container 21a is supplied to the alkaline electrolyte such as a solution of caustic soda or an alkaline electrolyte containing the desired concentration of leuco dye in the first container 2 via the solid dye inlet 21b. The first container may have a first suspension circulation loop 22, optionally equipped with an ultrasound device 221. Once the dye suspension has reached the desired homogeneity, it is supplied to the main container 1 via the suspension outlet 23 and the dye suspension inlet 11b, driven by a pump P05. Once the suspension is in the main container 1, the procedure is as follows Figure 1 and 3 described.
[0089] As also already indicated above, in order to start the dye reduction, in a first preparation step, a diluted suspension is prepared and electrolytic reduction is carried out in the electrolytic cell 4. Once the dye has been reduced to a leuco dye, it can be replenished with additional dye in the main container 1, or more preferably, some of the produced leuco dye can be transferred from the main container 1 to the first container 2 via the leuco dye outlet 16, the leuco dye return pipe 24 equipped with a leuco dye return pump P04 and a leuco dye inlet 241, to be replenished with additional dye. The suspension containing the leuco dye can then first be processed in the first suspension circulation loop 22 to improve its homogeneity, and then supplied to the main container 1 and finally to the electrolytic cell, as described above.
[0090] Similarly, once leuco dye production has begun, a portion of the concentrated leuco dye is removed and a portion of the leuco dye solution remains in the reactor. This remaining leuco dye solution can then remain in the main container 1, or preferably as Figure 4 and 5 As shown, the leuco dye solution is supplied to the first container 2 via the leuco dye return pipe 24. In the main container 1 or preferably the first container 2, the leuco dye solution is diluted with additional electrolyte, such as caustic soda, and replenished with dye. In order to produce a highly concentrated dispersant-free leuco dye solution, it has proven to be advantageous to add the alkaline electrolyte and the leuco dye in several portions, and for each addition, the leuco dye solution is returned from the main container 1 to the main container 2, as shown in the accompanying drawings, for example Figure 1 In the case of indigo white, a concentration of 5-20% has been found to be suitable for stabilizing suspensions containing indigo in an amount of up to 20%.
[0091] Once the dye has been reduced to the desired concentration of leuco dye, the majority of the leuco dye is removed from the reactor via concentrated leuco dye outlet 44, with a small portion remaining for the next reduction cycle.
[0092] Whether or not the adsorption filter is present, the anode must be regenerated from time to time. The same is true for the cathode, especially the particle carbon cathode. In order to keep the reactor working, it has been proven to be advantageous to clean / regenerate all the cathodes of a stack at the same time during the suspension preparation process, while the cathode electrolyte circulates through the other stacks. In a more preferred cathode regeneration step, the water used to prepare the suspension is supplied to the main container 1 or the first container 2 via the cathode chamber 41. In a continuous production reactor, such as a reactor that produces one batch per day, it is usually sufficient to regenerate the cathode once a week, while the anode requires a lower regeneration frequency, such as once every seven weeks. For a reactor with 6 stacks, this means that the cathodes of all stacks are cleaned after six days, the anodes of one stack are cleaned on the seventh day, the anodes of the second stack are cleaned on the seventh day of the second week, and so on. In the case of more than one stack, the reactor shutdown can also be kept to a minimum. Even if maintenance takes more time, it is usually sufficient to separate one stack while the other stacks remain operational.
[0093] It has now been found that anode cleaning, particularly if polymeric deposits on the anode are kept to a minimum, can be readily performed by circulating an acidic cleaning solution through the anode compartment. The same procedure can also be applied to cathodes, particularly particulate carbon cathodes.
[0094] For such cleaning or regeneration steps, e.g. Figure 6As shown, the electrochemical reactor also has a stack or a device for supplying a cleaning solution to an electrolytic cell. These devices include at least one cleaning medium supply pipe 61, for supplying a cleaning / regeneration solution to a cathode or anode, and at least one cleaning medium on the side of the electrolytic cell opposite to the inlet removes a pipe 62, for removing an acidic cleaning solution and water and preferably an alkaline solution. These cleaning medium supply pipes 61 can be the bypass (i.e., using the same inlet and outlet) of a cathode electrolyte supply pipe 151 and an anode electrolyte supply pipe 31, or an independent pipe with its own inlet and outlet adjacent to the inlet and outlet of a cathode electrolyte circulation loop or an anode electrolyte circulation loop. Typically, one or more cleaning medium supply pipes 61 are connected to an acid container 63a to supply acid, and are optionally connected to an alkali container 63b to supply alkali, and are connected to a water line for supplying deionized water. One or more cleaning media remove pipes 62 and are directly supplied to a wastewater treatment plant (WWTP), or are supplied to a wastewater container for storing wastewater. In a preferred embodiment, the cleaning solution circulates for a certain period of time, i.e., until their pollution reaches an undesirable level. In the case of circulation, the cleaning medium removal pipe 62 is connected to the containers 63a, 63b via the cleaning medium circulation device 64. In this case, it is preferred to have one or more particle filters and / or adsorption filters for retaining small particles of metal source and ground electrode material during the cleaning cycle, preferably in the cleaning medium circulation pipe 64 just downstream of the electrolytic cell, or for adsorbing dissolved contaminants located somewhere.
[0095] Cleaning or regenerating the anode or both electrodes in the electrochemical reactor of the present invention, respectively, comprises cleaning the anode chamber and / or cathode chamber 41, 42, respectively, with a strong acid (pK<1) by circulating the acidic solution through the chambers 41, 42, in particular the electrode beds, and then cleaning the chambers 41, 42 with water, which is optionally and preferably carried out after cleaning the acid-treated chambers 41, 42 with an alkaline solution, preferably caustic soda, to more effectively remove acid and electrode contaminants.
[0096] This regeneration step removes, for example, deposits from the anode and metals such as iron and / or nickel from the particle surface of the particulate carbon-based cathode. Since such metals are believed to have a catalytic effect on H2 production that competes with the desired reduction, such a cleaning step, in addition to removing other deposits, also significantly benefits the overall performance of the electrolysis reactor.
[0097] In the case of indigo reduction, the acid wash is carried out for a suitable time, e.g. 10-60 min, followed by a bed wash with a base such as caustic soda (to remove acid and electrode contaminants), followed by a water wash, or less preferably directly with water. Although the wash can be carried out simultaneously for both electrodes (i.e. cathode and anode), the above procedure is preferred.
[0098] The concentration of a suitable acidic solution is 10-100 g / L, more preferably 40-60 g / L, most preferably about 50 g / L, or 0.25-30 M, preferably 1-2 M, more preferably 1.3-1.4 M (referring to protons) in deionized water. If an alkaline solution such as caustic soda is used after the acid solution cleaning, the concentration is typically 10-100 g / L, more preferably 20-60 g / L, most preferably 40 g / L, or 0.1-2.5 M, preferably 0.5-1.5 M (referring to hydroxide) in deionized water.
[0099] For the regeneration step, the strong acid is preferably selected from HCl, H2SO4, HNO3, and mixtures thereof.
[0100] While there have been shown and described presently preferred embodiments of the invention, it is to be distinctly understood that the invention is not limited thereto but may be otherwise variously embodied and practiced within the scope of the appended claims.
[0101] List of reference numerals:
[0102] 1 main container
[0103] 11a Solid dye inlet
[0104] 11b Dye suspension inlet
[0105] 12 Catholyte outlet
[0106] 13 Reduced cathode electrolyte inlet
[0107] 14 Main suspension circulation loop
[0108] P03 Main suspension circulation pump
[0109] 141 Ultrasonic equipment in the main suspension circulation loop
[0110] 15 Catholyte circulation pipe or cathode electrolyte circulation loop
[0111] 151 Catholyte supply pipe
[0112] P01 Catholyte supply pump
[0113] 152 Particle filter in cathode electrolyte supply pipe
[0114] 153 Cathode electrolyte heating device (heat exchanger)
[0115] 154 Ultrasonic device in the cathode electrolyte supply pipe
[0116] 16 Leuco dye export
[0117] 2 First container
[0118] 21a Solid dye container
[0119] 21b Solid dye inlet
[0120] 22 First suspension circulation loop
[0121] 221 Ultrasonic device in the first suspension circulation loop
[0122] 23 First suspension outlet
[0123] 231 First suspension supply pipe
[0124] P05 First suspension supply pump
[0125] 24 Leuco dye return pipe
[0126] 241 Leuco Dye Inlet
[0127] 25. First suspension mixer
[0128] P04 Leuco dye return pump
[0129] 3 Anolyte container
[0130] 31 Anode electrolyte supply pipe
[0131] 32 Anolyte outlet
[0132] 33 Anode electrolyte circulation pipe or anode electrolyte circulation loop
[0133] 331 Anode electrolyte heating device such as heat exchanger
[0134] 332 Adsorption filter
[0135] P02 Anolyte Pump
[0136] 35 Anode electrolyte inlet
[0137] 4 Electrolytic Cell
[0138] 41 Catholyte compartment or cathode compartment
[0139] 411 Catholyte inlet
[0140] 412a Reduced cathode electrolyte outlet
[0141] 412b Reduced cathode electrolyte return pipe
[0142] 413a Bypass for changing the direction of cathode electrolyte
[0143] 413b Bypass for changing the direction of cathode electrolyte
[0144] 42 Anolyte chamber or anode chamber
[0145] 421 Anode electrolyte inlet
[0146] 422a Anode electrolyte outlet
[0147] 422b Anode electrolyte return pipe
[0148] 43. separator, semipermeable membrane
[0149] 44 Concentrated leuco dye export (in batches)
[0150] 5. Stack of electrolytic cells
[0151] 61 Cleaning medium supply pipe
[0152] 62 Cleaning medium removal tube
[0153] 63a Acid container
[0154] 63b Alkali container
[0155] 64 Cleaning medium circulation device
Claims
1. An electrolytic reactor suitable for reducing vat dyes or sulfur dyes, the reactor comprising at least one electrolytic cell (4) having an anode chamber (42) and a cathode chamber (41), the chambers (41, 42) being separated by a partition (43), the chambers (41, 42) each comprising an inlet (411, 421) and an outlet (412a, 422a) for an anode electrolyte and a cathode electrolyte, respectively, at opposite ends, the inlet (411, 421) and the outlet (412a, 422a) of each chamber being connected to each other via an anode electrolyte circulation pipe (33) or a cathode electrolyte circulation pipe (15), the anode electrolyte circulation pipe (33) being equipped with an anode electrolyte container (3) to form an anode electrolyte circuit, and the cathode electrolyte circulation pipe (15) being equipped with a main container (1) to form a cathode electrolyte circuit, wherein the anode electrolyte circulation pipe (33) is further equipped with at least one adsorption filter (332), the adsorption filter (332) comprising an adsorption material for adsorbing molecular impurities.
2. The electrolytic reactor according to claim 1, wherein the separator (43) is a semipermeable membrane.
3. The electrolytic reactor according to claim 1, wherein the adsorption material in the adsorption filter (332) comprises activated carbon or molecular sieve.
4. The electrolytic reactor according to claim 1, wherein the adsorption material in the adsorption filter (332) contains activated carbon or consists of activated carbon.
5. An electrolysis reactor according to any one of claims 1 to 4, wherein the cathode chamber (41) comprises a particle cathode.
6. The electrolytic reactor of claim 1, wherein the cathode electrolyte comprises indigo.
7. The electrolytic reactor according to claim 1, wherein the main container (1) has a main suspension circulation loop (14) for circulating the dye suspension.
8. The electrolytic reactor according to claim 7, wherein the main suspension circulation loop (14) is equipped with a first ultrasonic device (141).
9. An electrolytic reactor according to claim 7 or 8, wherein the main container (1) is combined with a first container (2) for preparing a suspension so that the suspension from the first container (2) can be fed into the main container (1), and the colorless dye solution can be fed from the main container (1) back to the first container (2), and wherein the first container (2) has a first suspension circulation loop (22) for circulating the first suspension before it is transported back to the main container (1).
10. The electrolytic reactor according to claim 9, wherein the first suspension circulation loop (22) is equipped with a second ultrasonic device (221).
11. The electrolytic reactor according to claim 1, comprising at least 4 electrolytic cells (4) in the form of a stack (5) of at least two electrolytic cells, wherein the electrolytic cells (4) of one stack (5) and all stacks (5) are connected in parallel.
12. The electrolytic reactor according to claim 1, wherein at least one of the anode chamber (42) and the cathode chamber (41) has a cleaning device independently of each other, the cleaning device being selected from a first cleaning device (61) for providing one or more cleaning solutions and water, a second cleaning device (62) for removing one or more cleaning solutions and water, and a third cleaning device (64) for circulating one or more cleaning solutions and water.
13. A method for improving anode performance in the reduction of vat dyes or sulfur dyes, the method comprising utilizing an electrolytic reactor according to any one of claims 1 to 12, and continuously cleaning the anode electrolyte in an adsorption filter (332) respectively integrated in an anode electrolyte circulation pipe (33) by continuously flowing the anode electrolyte through the adsorption filter (332).
14. The method of claim 13, wherein the dye is indigo.
15. Use of an adsorption filter (332) in an electrolytic reactor according to any one of claims 1 to 12, for removing undesirable molecular products and / or by-products and / or impurities from the anode electrolyte during the electrochemical urn dye or sulfur dye reduction process, wherein at least a portion of the undesirable molecular products and / or by-products and / or impurities are reaction products present in or formed in the cathode electrolyte, and wherein part or all of the molecular products and / or by-products and / or impurities enter the anode electrolyte through the partition (43), where they are adsorbed onto the adsorption filter (332), thereby achieving purification of the cathode electrolyte, i.e., the dye liquid.
16. The use according to claim 15, wherein the dye is indigo.
Citation Information
Patent Citations
Process and electrolysis system for carbon dioxide utilization
DE102015202117A1
Continuous electrochemical process for reaction of compounds containing aliphatic unsaturation
US3701719A
Electrochemical reactor
WO2007147283A2
Electrochemical reactor and its cleaning or regeneration
CN113166954A
Leucodye (such as leucoindigo) as dispersing aid
CN113195791A