Uses temperature controlled airflow to create a smooth ceramic coating

By using temperature-controlled airflow to smooth the ceramic layer during ceramic thermal spraying, the problem of surface roughness after increasing thickness is solved, resulting in a smoother ceramic surface and reduced polishing requirements.

CN113174555BActive Publication Date: 2024-10-01GENERAL ELECTRIC TECH GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011399903.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-01-08
Filing Date
2020-12-04
Publication Date
2024-10-01
Estimated Expiration
2040-12-04

AI Technical Summary

Technical Problem

As the thickness of existing ceramic thermal barrier coatings (TBC) increases, the surface roughness problem is difficult to effectively solve, resulting in the need for expensive polishing processes to obtain a smooth surface.

Method used

Smooth solidification of the ceramic layer is achieved by using a temperature-controlled air flow during the thermal spraying process to smooth at least partially melted ceramic material on the surface, combined with movement of the thermal spray unit and gas nozzle to ensure synchronized transmission of the air flow and ceramic material flow.

Benefits of technology

The surface roughness is significantly reduced from the conventional 400Ra to about 200Ra, reducing the need for the polishing process and achieving a thicker ceramic layer and a smoother surface.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113174555B_ABST
    Figure CN113174555B_ABST
Patent Text Reader

Abstract

The present invention provides a method and coating system (100) for smoothing a surface (114, 166, 170) of a thermal barrier coating (TBC) (112) using a temperature controlled gas flow (142). A thermal spray unit (110) applies the TBC (112) to a surface (114, 166, 170). The thermal spray unit (110) generates a flow of TBC material (124) toward the surface (114, 166, 170). After thermally spraying the TBC (112) on the surface (114, 166, 170), the surface (114, 166, 170) of uncured TBC material (144) on the surface (114, 166, 170) is smoothed by transmitting a flow of temperature controlled gas (142) to the uncured TBC material (144) on the surface (114, 166, 170). The cured TBC (112) has a smoother surface (114, 166, 170) that requires much less polishing to achieve a desired surface roughness.
Need to check novelty before this filing date? Find Prior Art

Description

Background Art

[0001] The present disclosure relates generally to coating processes and, more particularly, to methods of thermally spraying metal parts with ceramics, such as thermal barrier coatings (TBCs), while delivering a temperature controlled gas flow across the surface to smooth the ceramic.

[0002] Ceramics are widely used for coating surfaces. For example, ceramics can be used as thermal barrier coatings (TBCs), which can be applied to various metal parts such as turbines to protect the underlying metal from high operating temperatures. TBCs can be applied to turbine blades, nozzles and shrouds in gas turbines, for example, to protect them from the heat of combustion gases in gas turbines. As the geometry of metal parts in turbines becomes more complex and the operating temperature of turbines increases, thicker TBCs are being adopted. This thicker TBC is challenging in maintaining a smooth TBC surface that does not affect performance. Typically, TBC surface roughness is a result of the spray angle relative to the surface being coated and the surface contaminants formed by the unmelted or partially melted powder particles that reside on the surface, which are subsequently coated. The thicker the TBC, the greater the surface roughness. At present, the surface roughness problem is solved by expensive surface polishing (e.g., using diamond-coated discs) to remove surface roughness and obtain the desired surface finish. Summary of the invention

[0003] A first aspect of the present disclosure provides a method comprising: thermally spraying a ceramic onto a surface, the thermal spraying producing a flow of ceramic material toward the surface; during the thermal spraying of the ceramic onto the surface, smoothing a layer of the at least partially molten ceramic material on the surface by transmitting a temperature-controlled gas flow to the at least partially molten ceramic material on the surface; and solidifying the ceramic.

[0004] A second aspect of the present disclosure provides a coating system, the coating system comprising: a thermal spray unit for applying a thermal barrier coating (TBC) onto a surface, the thermal spray unit generating a flow of TBC material; an actuator operatively coupled to the thermal spray unit to move the thermal spray unit across the surface; and a gas nozzle configured to deliver a temperature-controlled gas flow to at least partially melted TBC material on the surface when the thermal spray unit applies the TBC material onto the surface, the gas nozzle being movable with the thermal spray unit.

[0005] The exemplary aspects of the present disclosure are designed to solve the problems described herein and / or other problems not discussed. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] These and other features of the present disclosure will be more readily understood from the following detailed description of various aspects of the present disclosure taken in conjunction with the accompanying drawings which depict various embodiments of the present disclosure, wherein:

[0007] Figure 1 is a schematic side view of a coating system according to an embodiment of the present disclosure; and

[0008] Figure 2 is a schematic side view of a polishing TBC according to an embodiment of the present disclosure.

[0009] Figure 3 is a block diagram of a method according to an embodiment of the present disclosure.

[0010] It should be noted that the drawings of the present disclosure are not necessarily drawn to scale. The drawings are intended to depict only typical aspects of the present disclosure and therefore should not be considered to limit the scope of the present disclosure. In the drawings, like numbers represent like elements between drawings. DETAILED DESCRIPTION

[0011] The terms used herein are only used for the purpose of describing specific embodiments and are not intended to limit the present disclosure. As used herein, the singular forms "one", "a kind of" and "the" are intended to also include plural forms, unless the context clearly states otherwise. It will be further understood that when used in the specification, the terms "include" and / or "comprising" specify the presence of stated features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or their groups. "Optional" or "optionally" means that the event or situation described subsequently may or may not occur, and the description includes instances where the event occurs and instances where the event does not occur.

[0012] Where an element or layer is referred to as being "on," "engaged to," "connected to," or "coupled to" another element or layer, it may be directly on, engaged to, connected to, or coupled to the other element or layer, or there may be intervening elements or layers. In contrast, when an element is referred to as being "directly on," "directly engaged to," "directly connected to," or "directly coupled to" another element or layer, there may be no intervening elements or layers. Other words used to describe the relationship between elements should be interpreted in a similar manner (e.g., "between" versus "directly between," "adjacent" versus "directly adjacent," etc.). As used herein, the term "and / or" includes any and all combinations of one or more of the associated listed items.

[0013] Embodiments of the present disclosure provide methods and coating systems for smoothing applied ceramic layers such as thermal barrier coatings (TBC) using temperature-controlled gas streams. A thermal spray unit coats ceramic on a surface. The thermal spray unit produces a flow of ceramic material toward the surface. After thermal spraying ceramic on the surface, the at least partially molten layer of ceramic material on the surface is smoothed by transmitting a temperature-controlled gas stream to the at least partially molten ceramic material on the surface. The solidified ceramic can be thicker and still have a smoother surface than when no gas stream is used. In a non-limiting example, the smoother surface can be about 200rA compared to conventional 400rA. Therefore, the ceramic can be thicker and require much less polishing to obtain the desired surface roughness.

[0014] See attached figure, Figure 1 A schematic side view of a coating system 100 according to an embodiment of the present disclosure is shown. As shown, the coating system 100 includes a thermal spray unit 110 to apply a ceramic such as a thermal barrier coating (TBC) 112 to a surface 114. Although the teachings of the present invention can be applied to any ceramic material, for the purpose of illustration, the present invention will relate to TBC 112. As used herein, a "surface" can be the surface of a base material or substrate of a component, the surface of an intermediate coating on a base material or substrate, or the surface of a front layer of a TBC. That is, the surface 114 can be the surface of a component 120 (e.g., a metal, a ceramic layer, a multi-material ceramic layer, etc.) or a layer on the component 120 (e.g., a bonding coating 122 on a metal component 120) or a front layer of a TBC. The metal component 120 can include any metal now known or later developed, such as a superalloy or ceramic for a turbine. As used herein, "superalloy" refers to an alloy having many superior physical properties compared to conventional alloys, such as, but not limited to: high mechanical strength, high thermal creep deformation resistance, such as Rene 108, CM247, Haynes alloy, Incalloy, MP98T, TMS alloy, CMSX single crystal alloy. In one embodiment, the teachings of the present invention may be particularly advantageous for superalloys having high γ' (γ') values. "γ'" (γ') is the primary strengthening phase of nickel-based alloys. Exemplary high γ' superalloys include, but are not limited to: Rene 108, N5, GTD 444, MarM 247, and IN 738.

[0015] The thermal spray unit 110 generates a flow of TBC material 124, such as a spray plume of ceramic material. The thermal spray unit 110 may employ any now known or later developed thermal process to spray the TBC material 124 or any other desired ceramic onto the surface 114. In one embodiment, the thermal spray unit 110 may include a plasma spray unit. In other embodiments, the thermal spray unit 110 may include an arc spray unit, a combustion spray unit, or a high velocity oxygen fuel (HVOF) coating unit. The thermal spray unit 110 may also include any of a variety of low pressure coating systems.

[0016] The bond coating 122, if used, may include any now known or later developed bond coating material, such as, but not limited to, nickel or platinum aluminum compounds, nickel chromium aluminum yttrium (NiCrAlY), or nickel cobalt chromium aluminum yttrium (NiCoCrAlY). The bond coating 122 may have a thickness of, for example, <500 microns. If necessary, the bond coating 122 and the TBC 112 may be used together. The TBC 112 may include any now known or later developed ceramic TBC material, such as, but not limited to, yttria stabilized zirconia (YSZ), mullite, and alumina. The TBC 112 may also include additional layers (not shown), such as thermally grown oxides. The TBC 112 may have a variety of porosities and / or densities. The TBC 112 may be dense vertical cracking. As described above, the geometry of the composite metal component 120 may require a thicker TBC 112. To this end, the thickness of TBC 112 may range, for example, from about 0.127 millimeters (mm) (0.005 inches) to about 2.54 mm (0.1 inches), depending on the type of material being applied. TBC 112 and bond coating 122 may be over the entire surface 114 of metal component 120 or over only a portion of surface 114.

[0017] The coating system 100 may also include an actuator 130 operatively coupled to the thermal spray unit 110 to move the thermal spray unit 110 across the surface 114, i.e., as it coats the surface 114. The actuator 130 may include any now known or later developed actuator system capable of controlling the motion of the thermal spray unit 110, such as a linear actuator, a motor, a robotic system 132 (shown in phantom), etc. Although shown at an angle generally perpendicular to the surface 114, the actuator 130 may also include an angle adjustment actuator (see arrow A) configured to control the angle of attack of the thermal spray unit 110 relative to the surface, i.e., the angle of the stream of the TBC material 124 relative to the surface 114. The angle of attack may allow for the creation of different TBC properties, such as density, porosity, thickness, etc.

[0018] The coating system 100 may also include a gas nozzle 140 configured to deliver a temperature-controlled gas flow 142 to the at least partially melted TBC material 144 (or other ceramic) on the surface 114 while or after the thermal spray unit 110 applies the TBC material 124 to the surface 114. "At least partially melted" means that at least some of the TBC material 144 is not solidified, for example, it is semi-molten. When the temperature-controlled gas flow 142 impacts the at least partially melted TBC material 144, it smoothes the surface of the material. More specifically, the gas flow 142 smoothes portions of the peaks of the at least partially melted TBC material 144, making the peaks smaller. It may also remove unmelted or partially melted powder particles residing on the surface 114. The temperature-controlled gas flow 142 may be provided by any now known or later developed source, such as a pump (shown), a pressurized supply source, etc. The temperature-controlled gas flow 142 may include air or an inert gas such as argon or nitrogen. A thermal controller 150 may be provided to control the temperature of the temperature-controlled gas. The thermal controller 150 may include any form of heat exchanger suitable for the gas used, such as an air conditioner, a heater, etc. The temperature may be in the range of, for example, about 204.4 degrees Celsius (°C) (400°F) to about 1093.3°C (2000°F). The temperature may be selected based on a variety of factors, such as, but not limited to: the ability to produce the desired smoothness without otherwise affecting the curing of the TBC material, the ability to reduce surface roughness, the type of gas, the type of TBC material, the machine room environment in which the gas is applied, etc. As schematically indicated by, for example, a coupling element 160, the gas nozzle 140 may be directly coupled to move with the thermal spray unit 110, or otherwise configured to move with the thermal spray unit 110. In this way, as the thermal spray unit 110 advances, the gas nozzle 140 also advances. The distance between the gas nozzle 140 and the thermal spray unit 110 may be predetermined, or may be changed during use according to, for example, the geometry of the metal part 120.

[0019] The coating system 100 may also include an angle adjustment actuator 160 (schematically shown by arrow 162) operatively coupled to the gas nozzle 140 to control the angle of attack of the temperature controlled gas flow 142 relative to the flow of the TBC material 124. In one embodiment, the angle adjustment actuator 160 controls the angle of attack α of the temperature controlled gas flow 142 relative to the flow of the TBC material 124 between 5° and 85°. The angle of attack α may be predetermined or may vary during use depending on, for example, the thickness of the TBC 112 and / or the geometry of the metal part 120.

[0020] Figure 3 300 according to an embodiment of the present disclosure. In operation, as Figure 3As shown, at process 310, the coating system 100 thermally sprays the TBC 112 (or other ceramic), such as yttria-stabilized zirconia (YSZ), mullite, and alumina, onto the surface 114. That is, the thermal spray unit 110 generates a stream of the TBC material 124 toward the surface 114, such as by using a plasma spray of the TBC material 124. Depending on the material, the thickness of the TBC material 124 on the surface 114 can be, for example, between about 0.127 millimeters (mm) (0.005 inches) and 2.54 mm (0.1 inches). When this occurs, the TBC material 124 is deposited on the surface 114. Figure 3 In process 312, after thermally spraying the TBC onto the surface, the layer of at least partially melted TBC material 144 on the surface 114 is smoothed by delivering a flow of a temperature-controlled gas stream 142 onto the at least partially melted TBC material 144 on the surface 114. Processes P10 and P12 may occur simultaneously. As the thermal spray unit 110 moves over the surface 114, a gas nozzle 140 for delivering the temperature-controlled gas stream to the surface 114 may move with the thermal spray unit 110 for plasma spraying the TBC 112, i.e., because the gas nozzle 140 is coupled to the thermal spray unit 110 or otherwise configured to move with it. As described above, the temperature-controlled gas stream 142 may include air or an inert gas (such as argon or nitrogen) and may have a temperature in the range of, for example, about 204.4 degrees Celsius (°C) (400°F) to about 1093.3°C (2000°F). The delivery of the flow of the temperature controlled gas stream 142 may include controlling the angle of attack of the gas stream relative to the flow of the TBC material 124 to optimize smoothing. The angle of attack α of the flow of the temperature controlled gas stream 142 relative to the flow of the TBC material 124 is between 5° and 85°. The pressure of the temperature controlled gas stream 142 may also be controlled, for example, between about 0.034 megapascals (MPa) (5 pounds per square inch (psi)) and about 0.82 MPa (120 psi). Other parameters of the temperature controlled gas stream 142, such as the flow rate, may also be controlled.

[0021] Once completed, Figure 3In the process 314 of , TBC112 (or other ceramics) can be cured. The curing may include any curing treatment known now or developed later, such as not performing any operation (atmospheric progressive), cooling, heating, drying, exposure to certain types of light, etc. Any necessary curing process can be performed after curing. Conventionally, TBC112 will have a surface roughness of about 400Ra after curing. The roughness can be quantified by the change of the surface direction relative to its ideal level. If the change is large, the surface is rough, and if the change is small, the surface is smooth. As described in the American Society of Mechanical Engineering (AMERICAN Society of Mechanical Engineering, ASME) B46.1, Ra is the arithmetic mean of the absolute value of the profile height deviation relative to the mean line, recorded in the evaluation length. That is, Ra is the average value of a group of individual measurements of the minimum and maximum heights of the surface. Forming TBC 112 according to an embodiment of the present invention can produce a roughness of about 200Ra, which requires significantly less polishing to obtain the desired surface roughness, such as 40Ra. Figure 2 A polishing surface 170 of the TBC 112 is shown to further smooth the surface of the TBC. Polishing may be performed using any now known or later developed polishing system 172 (eg, with a diamond coated disk).

[0022] Embodiments of the method according to the present invention clean the surface of the metal part 120, but also smooth the peaks by creating cross-jet plumes of temperature controlled gas flow 142 to smooth the peaks of the layer of at least partially melted TBC material 144. The result is a much smoother final TBC surface.

[0023] As used throughout the specification and claims, approximate language can be used to modify any quantitative representation that can be allowed to vary without causing a change in the basic function associated with it. Therefore, the values ​​modified by one or more terms (such as "about", "approximately" and "substantially") are not limited to the specified precise values. In at least some cases, approximate language can correspond to the precision of the instrument used to measure the value. Here and throughout the specification and claims, range limitations can be combined and / or interchangeable. Unless the context or language indicates otherwise, these ranges are identified and include all subranges contained therein. "Approximately" applied to a specific value of a range applies to both end values, unless otherwise dependent on the precision of the instrument for measuring the value, otherwise + / -10% of one or more of the values ​​can be indicated.

[0024] The corresponding structures, materials, actions and equivalents of all means or steps plus function elements in the following claims are intended to include any structure, material or action for performing functions in conjunction with other claimed elements specifically claimed. A description of the present disclosure has been given for the purpose of illustration and description, but it is not intended to be exhaustive or to limit the present disclosure to the disclosed form. Many modifications and variations will be apparent to those of ordinary skill in the art without departing from the scope and essence of the present disclosure. Embodiments have been selected and described in order to best explain the principles and practical applications of the present disclosure, and to enable other persons of ordinary skill in the art to understand the various embodiments of the present disclosure with various modifications suitable for the intended specific use.

Claims

1. A coating method comprising: thermally spraying a ceramic (112) onto a surface (114, 166, 170), the thermal spraying producing a flow of ceramic material (124) toward the surface (114, 166, 170); During thermal spraying of the ceramic (112) onto the surface (114, 166, 170), smoothing the layer of the at least partially melted ceramic material (144) on the surface (114, 166, 170) by delivering a flow of a temperature controlled gas (142) having a temperature in the range of 204.4°C to 1093.3°C onto the at least partially melted ceramic material (144) on the surface (114, 166, 170) and controlling the angle of attack of the flow of the temperature controlled gas (142) relative to the flow of the ceramic material (124); and The ceramic (112) is cured.

2. The method of claim 1, wherein the temperature controlled gas (142) comprises at least one of air, argon, and nitrogen.

3. The method of claim 1, wherein the angle of attack of the flow of the temperature controlled gas (142) relative to the flow of the ceramic material (124) is between 5° and 85°.

4. The method of claim 1, further comprising polishing the surface (114, 166, 170) to further smooth the surface (114, 166, 170) of the ceramic (112).

5. The method of claim 1, further comprising moving a gas nozzle (140) with a thermal spray unit (110), the gas nozzle (140) being used to deliver a flow of the temperature controlled gas (142) across the surface (114, 166, 170), the thermal spray unit (110) being used to thermally spray the ceramic (112) as the thermal spray unit (110) moves over the surface (114, 166, 170).

6. The method of claim 1, wherein the surface (114, 166, 170) has a surface roughness of 200 Ra after the curing.

7. The method of claim 1, wherein the thermal spraying comprises plasma spraying the ceramic material (124).

8. The method of claim 1, wherein the ceramic material (124) comprises yttria stabilized zirconia (YSZ), mullite, and alumina.

9. The method of claim 1, wherein the ceramic material (144) on the surface (114, 166, 170) has a thickness greater than 2.54 millimeters.

10. A coating system (100), comprising: A thermal spray unit (110) for applying a thermal barrier coating (TBC) (112) on a surface (114, 166, 170), the thermal spray unit (110) generating a flow of TBC material (124); an actuator (130) operatively coupled to the thermal spray unit (110) to move the thermal spray unit (110) over the surface (114, 166, 170); a gas nozzle (140) configured to deliver a temperature-controlled gas (142) to uncured TBC material (144) on the surface (114, 166, 170) after the thermal spray unit (110) applies the TBC material (124) to the surface (114, 166, 170), the gas nozzle (140) being operatively coupled for movement with the thermal spray unit (110); a thermal controller (150) for controlling the temperature of the temperature-controlled gas (142), wherein the temperature is within a range of 204.4°C to 1093.3°C; and An angle adjustment actuator (162) is operatively coupled to the gas nozzle (140) to control an angle of attack of the temperature controlled gas (142) relative to a flow of the TBC material (124).

11. The coating system (100) of claim 10, wherein the temperature controlled gas (142) comprises at least one of air, argon, and nitrogen.