Asphalt mixture durability testing device
By designing the asphalt mixture durability test device and using the environmental simulator and rain simulator, the problem of low test accuracy in the existing technology has been solved, a more accurate simulation of the aging and fatigue of the asphalt mixture has been achieved, the test accuracy has been improved and Reduced costs.
Patent Information
- Application Number
- CN202110548591.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-05-19
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2041-05-19
AI Technical Summary
The existing pressure aging test cannot comprehensively simulate the actual long-term aging and mixture fatigue of asphalt pavement during use, resulting in low test accuracy.
An asphalt mixture durability test device is designed, including a test chamber, an environmental simulator and a host computer to simulate different working conditions. The air pressure, temperature and rain simulators are used to simulate actual usage conditions to improve test accuracy.
This device can more realistically simulate the aging and fatigue process of asphalt mixture under different working conditions, significantly improve the test accuracy and reduce the test cost.
Smart Images

Figure CN113218852B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of asphalt mixture durability testing, and in particular relates to an asphalt mixture durability testing device. Background Art
[0002] In recent years, in order to meet the needs of my country's rapid economic development, the construction of expressways has developed rapidly. Due to the advantages of comfortable driving, easy construction and maintenance, asphalt pavement is mostly used in newly built expressways. However, in the long-term use, asphalt pavement is often damaged prematurely due to aging and fatigue, and cannot meet the use requirements. At the same time, a pressure aging test for testing the durability of asphalt has emerged, and the pressure aging test has become a standard test method for asphalt aging testing. The asphalt sample is aged for 20 hours in a pressure tank with an inflation pressure of 2.1Mpa. The aging temperature is specified as 90℃~110℃ depending on the asphalt grade. The effect of this test on asphalt aging is equivalent to the aging of the surface asphalt of the road surface for 5 years during the service life.
[0003] The current pressure aging tests are only simulations of single use conditions and cannot comprehensively reflect the actual use of asphalt pavements. Therefore, it is necessary to provide a device that can conduct a comprehensive simulation test on the long-term aging of asphalt and the fatigue effect of the mixture during the use of asphalt pavements. Summary of the invention
[0004] The present invention provides an asphalt mixture durability testing device, aiming to solve the problem of low precision of pressure aging test in the prior art.
[0005] In order to solve the above technical problems, the technical solution adopted by the present disclosure is:
[0006] A durability test device for asphalt mixture comprises a test box, the test box comprises an inner cavity with an opening, the test box is provided with a sealing cover for closing the opening so that the inner cavity is in a sealed state, a durability tester is provided in the inner cavity, and an environmental simulator is also provided on the test box. The environmental simulator comprises an air source, the air source supplies gas to the inner cavity through an air pipe, an air pressure sensor and a temperature sensor are provided on the sealing cover, the air pressure sensor detects the air pressure parameter in the inner cavity, the temperature sensor detects the temperature parameter in the inner cavity, a heater is provided on the air pipe, the heater heats the gas flowing through the air pipe, the environmental simulator also comprises a water pump, the water pump supplies water to the inner cavity through a water pipe, a nozzle is provided in the inner cavity so that the water supplied by the water pump is uniformly sprayed into the inner cavity, and the asphalt mixture durability test device also comprises a host computer, and the temperature sensor, the air pressure sensor, the durability tester, the air source, the heater and the water pump all communicate with the host computer.
[0007] A further improved solution: the nozzle is fixed on the sealing cover, and a rain simulator is also provided on the sealing cover to make the water flow sprayed by the nozzle intermittent. The rain simulator can better simulate the actual working conditions and improve the test accuracy.
[0008] A further improved solution: the rain simulator includes a cover body arranged outside the nozzle, the cover body is rotatably connected to the sealing cover, the sealing cover is also provided with a motor for driving the cover body to rotate, the cover body is evenly provided with water retaining sheets along the rotation direction of the cover body, and a gap is provided between two adjacent water retaining sheets for water flow to pass through. The rain simulator has a simple structure and is easy to process, which reduces the use cost of the rain simulator.
[0009] Further improved solution: the cover is rotatably arranged on the sealing cover through a deep groove ball bearing, a fixing ring for mounting the deep groove ball bearing is integrally arranged on the sealing cover, the inner ring of the deep groove ball bearing is sleeved on the fixing ring, the cover is fixed on the outer ring of the deep groove ball bearing, a driving gear is arranged on the output shaft of the motor, and a driven gear meshing with the driving gear is arranged on the cover. The cover is easy to assemble and rotates flexibly, which optimizes the application performance of the rain simulator.
[0010] A further improved solution: the heater comprises a heat preservation shell and a heating element arranged in the heat preservation shell, an air flow channel is arranged in the heat preservation shell, a joint is arranged on the heat preservation shell, the air pipe is connected to the air flow channel through the joint, and a heat insulation pad is arranged between the heat preservation shell and the heat preservation shell. The heat preservation shell is easy to assemble with the air pipe. In addition, the provision of the heat insulation pad can reduce heat loss and reduce the use cost.
[0011] A further improved solution: the airflow channel is arranged in the heating element in a serpentine shape. The airflow channel has a longer length, which can effectively heat the gas flowing through the airflow channel and reduce the volume of the heater.
[0012] A further improved solution is that a sealing ring is provided between the sealing cover and the test box, and the sealing ring is bonded to the sealing cover. The provision of the sealing ring improves the sealing performance of the inner cavity.
[0013] A further improved solution: the sealing cover is further provided with a through hole, a part of the air pipe and a part of the water pipe are both provided in the through hole, and the through hole is filled with packaging glue. The provision of the packaging glue improves the sealing performance of the inner cavity.
[0014] The beneficial effects of the present disclosure are:
[0015] An asphalt mixture durability test device disclosed in the present invention comprises a test box, the test box comprises an inner cavity with an opening, the test box is provided with a sealing cover for closing the opening so that the inner cavity is in a sealed state, a durability tester is provided in the inner cavity, and an environmental simulator is also provided on the test box. The environmental simulator comprises an air source, the air source supplies gas to the inner cavity through an air pipe, an air pressure sensor and a temperature sensor are provided on the sealing cover, the air pressure sensor detects the air pressure parameter in the inner cavity, the temperature sensor detects the temperature parameter in the inner cavity, a heater is provided on the air pipe, the heater heats the gas flowing through the air pipe, the environmental simulator further comprises a water pump, the water pump supplies water to the inner cavity through a water pipe, and a nozzle is provided in the inner cavity so that the water supplied by the water pump is uniformly sprayed into the inner cavity. The asphalt mixture durability test device further comprises a host computer, and the temperature sensor, the air pressure sensor, the durability tester, the air source, the heater and the water pump all communicate with the host computer. In actual application, this solution can simulate different working conditions. It can also simulate rainy environment under the premise that the air pressure and temperature meet the requirements. Compared with the existing technology, this solution greatly improves the test accuracy of the asphalt mixture durability test device. In addition, this solution has a simple structure and is easy to process, which reduces the test cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the technical solutions of the embodiments of the present disclosure, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present disclosure and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without paying creative work.
[0017] Figure 1 It is a schematic diagram of the asphalt mixture durability test device in the present disclosure.
[0018] Figure 2 It is a schematic diagram of the first direction after the cover body and the nozzle are assembled in the present disclosure.
[0019] Figure 3 It is a schematic diagram of the second direction after the cover body and the nozzle are assembled in the present disclosure.
[0020] Figure 4 It is a schematic diagram of the heater.
[0021] Description of the numbers in the figure:
[0022] 1-test box; 11-inner cavity; 2-sealing cover; 21-sealing ring; 22-packaging glue; 3-durability tester; 41-air source; 42-air pipe; 5-air pressure sensor; 6-temperature sensor; 7-heater; 71-insulation shell; 72-heating element; 73-air flow channel; 74-connector; 81-water pump; 82-water pipe; 83-nozzle; 84-hood; 85-motor; 86-water retaining plate; 87-gap; 9-host computer. DETAILED DESCRIPTION
[0023] The following will be combined with the drawings in the embodiments of the present disclosure to clearly and completely describe the technical solutions in the embodiments of the present disclosure. It should be understood that the specific embodiments described herein are only used to explain the present disclosure and are not used to limit the present disclosure. Based on the embodiments of the present disclosure, all other embodiments obtained by those skilled in the art without creative work belong to the protection scope of the present disclosure.
[0024] See also Figures 1 to 4 A durability test device for asphalt mixture, comprising a test box 1, the test box 1 comprising an inner cavity 11 with an opening, the test box 1 being provided with a sealing cover 2 for closing the opening so that the inner cavity 11 is in a sealed state, a durability tester 3 being provided in the inner cavity 11, the test box 1 being further provided with an environmental simulator, the environmental simulator comprising an air source 41, the air source 41 supplying gas to the inner cavity 11 through an air pipe 42, an air pressure sensor 5 and a temperature sensor 6 being provided on the sealing cover 2, the air pressure sensor 5 detecting air pressure parameters in the inner cavity 11, the temperature sensor 6 detecting the The temperature parameters in the inner cavity 11, the air pipe 42 is provided with a heater 7, the heater 7 heats the gas flowing through the air pipe 42, the environmental simulator also includes a water pump 81, the water pump 81 supplies water to the inner cavity 11 through the water pipe 82, the inner cavity 11 is provided with a nozzle 83 for uniformly spraying the water supplied by the water pump 81 into the inner cavity 11, the asphalt mixture durability test device also includes a host computer 9, the temperature sensor 6, the air pressure sensor 5, the durability tester 3, the air source 41, the heater 7 and the water pump 81 all communicate with the host computer 9.
[0025] The durability tester 3 is a common tester in the prior art, and the host computer 9 is also a common computer in the prior art. The host computer 9 is mainly used to perform relevant control and obtain the detection parameters of the durability tester 3. The main improvement of this solution is not the durability tester 3 and the host computer 9 themselves, so the configuration method and working principle of the durability tester 3 and the host computer 9 refer to the prior art.
[0026] The inner cavity 11 should maintain its sealing characteristics during the test, so the structure that the inner cavity 11 communicates with the outside world should be minimized. In this solution, the heater 7 is arranged on the air pipe 42, and the air pipe 42 increases the temperature in the inner cavity 11 while supplying air to the inner cavity 11, thereby reducing the characteristics of the inner cavity 11 communicating with the outside world and improving the sealing characteristics of the inner cavity 11.
[0027] In addition, the environmental simulator further includes a water pump 81, which is mainly used to spray water onto the test sample in the inner cavity 11 to obtain an environment closer to the actual working condition. This solution can simulate the actual working condition more realistically and improve the test accuracy.
[0028] Since the environmental simulator sprays water into the inner cavity 11 , the electronic components disposed in the inner cavity 11 should have a certain waterproof capability. For example, the relevant electronic components may be packaged to obtain waterproof capability.
[0029] On the basis of the above scheme: the nozzle 83 is fixed on the sealing cover 2, and a rain simulator is also provided on the sealing cover 2 to make the water flow sprayed by the nozzle 83 intermittent. Since the water flow sprayed by the nozzle 83 is continuous, while the rain in the actual working condition is not continuous, the real working condition can be better simulated by providing a rain simulator.
[0030] The rain simulator includes a cover body 84 that is covered outside the nozzle 83, the cover body 84 is rotatably connected to the sealing cover 2, and the sealing cover 2 is also provided with a motor 85 that drives the cover body 84 to rotate, and the cover body 84 is evenly distributed with water retaining sheets 86 along the rotation direction of the cover body 84, and a gap 87 for water flow to pass is provided between two adjacent water retaining sheets 86. The rain simulator has a simple structure and is easy to process, which reduces the use cost of the rain simulator.
[0031] The cover 84 mainly serves to interrupt the water flow. The water flow sprayed by the nozzle 83 points to a certain direction, such as the direction of the sample, and the cover 84 can guide part of the water flow to other directions while interrupting the water flow to achieve the function of simulating rain. The cover 84 can guide the water flow to the surrounding of the sample, etc. The cover 84 can be made of plastic material.
[0032] The cover body 84 is rotatably arranged on the sealing cover 2 through a deep groove ball bearing, a fixing ring for mounting the deep groove ball bearing is integrally arranged on the sealing cover 2, the inner ring of the deep groove ball bearing is sleeved on the fixing ring, the cover body 84 is fixed on the outer ring of the deep groove ball bearing, a driving gear is arranged on the output shaft of the motor 85, and a driven gear meshing with the driving gear is arranged on the cover body 84. The deep groove ball bearing can withstand a certain axial force, and the deep groove ball bearing is not easy to fail during use, which prolongs the service life of the deep groove ball shaft.
[0033] The fixing ring can be an integral structure with the sealing cover 2. The inner ring of the deep groove ball bearing and the cover body 84 can be connected by interference fit.
[0034] On the basis of any of the above schemes: the heater 7 includes an insulation shell 71 and a heating element 72 arranged in the insulation shell 71, an air flow channel 73 is arranged in the heating element 72, a joint 74 is arranged on the insulation shell 71, the air pipe 42 is connected to the air flow channel 73 through the joint 74, and an insulation pad is arranged between the heating element 72 and the insulation shell 71.
[0035] The air flow channel 73 is arranged in a serpentine shape in the heating element 72. The heating element 72 can be an electric heating element, etc. The heating element 72 can be controlled by a host computer. The host computer 9 controls the working state of the heating element 72 according to the parameters detected by the temperature sensor 6.
[0036] On the basis of any of the above solutions: a sealing ring 21 is provided between the sealing cover 2 and the test box 1 , and the sealing ring 21 is bonded to the sealing cover 2 .
[0037] The sealing cover 2 is also provided with a through hole, a part of the air pipe 42 and a part of the water pipe 82 are both provided in the through hole, and the through hole is filled with a packaging glue 22. The provision of the packaging glue 22 improves the sealing performance of the inner cavity 11. The sealing cover 2 can be fixed to the test box 1 by screws.
[0038] The asphalt mixture durability test device disclosed in the present invention is further introduced below in combination with the application mode:
[0039] First, position the sample on the durability tester 3, then close the sealing cover 2 to make the inner cavity 11 in a sealed state. Then, the host computer controls the operation of the environmental simulator to supply air into the inner cavity 11, increase the temperature of the inner cavity 11, and spray water into the inner cavity 11 to simulate actual working conditions. The temperature sensor 6 and the air pressure sensor 5 feed back the detected parameters to the upper box meter, and the upper computer 9 controls the working state of the heater 7 and the air source 41 according to the parameters detected by the temperature sensor 6 and the air pressure sensor 5. The environmental simulator simulates the environment in the inner cavity 11, and then the durability tester 3 performs relevant tests, and finally the host computer stores or displays the test parameters.
[0040] The present disclosure is not limited to the above optional implementation modes. Under the premise of not conflicting with each other, the various schemes can be combined arbitrarily. Anyone can derive other forms of products under the inspiration of the present disclosure. However, no matter what changes are made in their shapes or structures, all technical schemes that fall within the scope of the claims of the present disclosure shall fall within the protection scope of the present disclosure.
Claims
1. An asphalt mixture durability test device, Features: The test box comprises a test box, the test box comprises an inner cavity with an opening, the test box is provided with a sealing cover for closing the opening so that the inner cavity is in a sealed state, a durability tester is provided in the inner cavity, the test box is also provided with an environmental simulator, the environmental simulator comprises an air source, the air source supplies gas to the inner cavity through an air pipe, an air pressure sensor and a temperature sensor are provided on the sealing cover, the air pressure sensor detects the air pressure parameter in the inner cavity, the temperature sensor detects the temperature parameter in the inner cavity, a heater is provided on the air pipe, the heater heats the gas flowing through the air pipe, the environmental simulator also comprises a water pump, the water pump supplies water to the inner cavity through a water pipe, a nozzle is provided in the inner cavity so that the water supplied by the water pump is uniformly sprayed into the inner cavity, the asphalt mixture durability test device also comprises a host computer, the temperature sensor, the air pressure sensor, the durability tester, the air source, the heater and the water pump all communicate with the host computer; The nozzle is fixed on the sealing cover, and the sealing cover is also provided with a rain simulator which makes the water flow sprayed from the nozzle intermittent; The rain simulator comprises a cover body which is arranged outside the nozzle, the cover body is rotatably connected to the sealing cover, the sealing cover is also provided with a motor for driving the cover body to rotate, the cover body is evenly provided with water retaining sheets along the rotation direction of the cover body, and a gap is provided between two adjacent water retaining sheets for water flow to pass through; The cover body is rotatably arranged on the sealing cover through a deep groove ball bearing, a fixing ring for mounting the deep groove ball bearing is integrally arranged on the sealing cover, an inner ring of the deep groove ball bearing is sleeved on the fixing ring, the cover body is fixed on the outer ring of the deep groove ball bearing, a driving gear is arranged on the output shaft of the motor, and a driven gear meshing with the driving gear is arranged on the cover body; The heater comprises a heat preservation shell and a heating element arranged in the heat preservation shell, an air flow channel is arranged in the heat preservation shell, a joint is arranged on the heat preservation shell, the air pipe is communicated with the air flow channel through the joint, and a heat insulation pad is arranged between the heating element and the heat preservation shell; The air flow channel is arranged in the heating body in a serpentine shape.
2. An asphalt mixture durability testing device according to claim 1, Features: A sealing ring is arranged between the sealing cover and the test box, and the sealing ring is bonded to the sealing cover.
3. An asphalt mixture durability testing device according to claim 2, Features: The sealing cover is also provided with a through hole, a part of the air pipe and a part of the water pipe are both arranged in the through hole, and the through hole is filled with packaging glue.
Citation Information
Patent Citations
Asphalt mixture durability testing device
CN215066048U
Wheel tracking test method for pavement by means of random travel wheel load and wheel tracking tester for pavement by means of random travel wheel load
JP2006170680A
Method for predicting bitumen properties
WO2019234762A1