System and method for coating a substrate
By using a combination of layer thickness homogenization blades and linearly displaceable blade holders on a laser-irradiated transparent substrate, combined with force sensors and electromagnets, precise control and uniformity of thickness of highly viscous materials is achieved, solving existing technology problems The problem of difficulty in adjusting the medium thickness is that the thickness can be adjusted between 10 microns and 2000 microns.
Patent Information
- Application Number
- CN202080008421.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-01-06
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2040-01-06
AI Technical Summary
Existing coating systems have difficulty accurately controlling the coating of highly viscous materials on laser-irradiated transparent substrates, resulting in difficulty in precise adjustment of material thickness and poor uniformity.
A layer thickness homogenization blade mounted about a pivot axis is used in combination with a linearly displaceable blade holder, by positioning and locking the blade to ensure parallel contact with the straight surface portion of the laser-irradiated transparent substrate, and by gradually adjusting the blade to the substrate The separation distance between the blades is reduced to reduce the material thickness, and a force sensor and an electromagnet are used to precisely control and fix the blade position.
It achieves precise control of the thickness of highly viscous materials, and the thickness can be adjusted between 10 microns and 2000 microns, ensuring the uniformity and thickness accuracy of the material, and solving the problem of difficulty in thickness adjustment in the existing technology.
Smart Images

Figure CN113784800B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to systems and methods for accurately coating substrates with highly viscous materials. Background Art
[0002] Various types of systems and methods for coating substrates are known in the art. Summary of the invention
[0003] The present invention seeks to provide an improved system and method for coating a substrate with a highly viscous material.
[0004] Therefore, according to a preferred embodiment of the present invention, there is provided a method for coating a donor material onto a laser radiation transparent substrate having a straight surface portion, the method comprising: providing a layer thickness uniformizing blade pivotally mounted on a linearly displaceable blade holder about a pivot axis, the blade having a straight edge; initially positioning the linearly displaceable blade holder relative to the laser radiation transparent substrate so that the straight edge is placed coplanar with the straight surface portion of the laser radiation transparent substrate, wherein the straight surface portion is placed along a blade engagement axis perpendicular to the pivot axis; thereafter locking the layer thickness uniformizing blade to prevent it from being displaced relative to the linearly displaceable blade holder about the pivot axis; The shaft is pivotally movable; thereafter the linearly displaceable blade support and the layer thickness uniformizing blade are repositioned around a linear displacement axis perpendicular to the blade engagement axis and perpendicular to the pivot axis to a position where the straight edge is separated from the straight surface portion of the laser radiation transparent substrate by a certain separation distance, and the separation distance is uniform along the straight edge of the layer thickness uniformizing blade; the donor material is applied to the laser radiation transparent substrate; a mutual displacement between the layer thickness uniformizing blade and the laser radiation transparent substrate is provided along an axis parallel to the pivot axis, thereby reducing the thickness of the initial layer of the donor material; and the separation distance is maintained.
[0005] Preferably, the method further comprises sequentially repeating said repositioning and said providing mutual displacement steps at least once thereby to sequentially reduce said thickness of said donor material.
[0006] According to a preferred embodiment of the invention, said providing a mutual displacement comprises reducing said thickness of said donor material to a thickness between 10 micrometers and 2000 micrometers.
[0007] According to a preferred embodiment of the present invention, the initial positioning of the linearly displaceable blade support includes measuring the force exerted by the layer thickness uniformization blade on the laser radiation transparent substrate. Additionally or alternatively, the initial positioning includes initially positioning the layer thickness uniformization blade so that a portion of the straight edge of the blade contacts the laser radiation transparent substrate, while the blade is free to pivot about the pivot axis. Additionally, the initial positioning further includes thereafter lowering the layer thickness uniformization blade so that the straight edge is placed in parallel contact engagement with the laser radiation transparent substrate, while the blade is free to pivot about the pivot axis. Preferably, the initial positioning further includes thereafter further lowering the layer thickness uniformization blade until the measured force of the layer thickness uniformization blade on the laser radiation transparent substrate is about 150 grams, while the straight edge of the layer thickness uniformization blade is placed in parallel contact engagement with the laser radiation transparent substrate and the layer thickness uniformization blade remains free to pivot about the pivot axis.
[0008] According to a preferred embodiment of the present invention, locking the layer thickness uniformizing blade to prevent it from pivotally moving about the pivot axis relative to the linearly displaceable blade support is provided by an operation of an electromagnet mounted to the linearly displaceable blade support to attract a locking arm fixed to the layer thickness uniformizing blade.
[0009] Preferably, said repositioning takes place when said layer thickness equalization blade is not freely pivotable about said pivot axis.
[0010] According to another preferred embodiment of the present invention, a system for coating a donor material onto a laser radiation transparent substrate is also provided, the system comprising: a donor material applicator, which applies the donor material to the laser radiation transparent substrate; a multi-pass precise donor material thickness determiner, which is used to provide the donor material of a desired thickness on the laser radiation transparent substrate and comprises: a linearly displaceable blade support; a layer thickness uniformizing blade, which is lockably and pivotally mounted on the linearly displaceable blade support about a pivot axis, the blade having a straight edge; and a blade position maintainer, which is operable to maintain the straight edge at a desired separation distance from the laser radiation transparent substrate, the separation distance being uniform along the straight edge of the layer thickness uniformizing blade.
[0011] According to a preferred embodiment of the present invention, the desired thickness of the donor material on the laser radiation transparent substrate is between 10 microns and 2000 microns.
[0012] According to a preferred embodiment of the present invention, the linearly displaceable blade support is linearly displaceable perpendicularly to the pivot axis.
[0013] According to a preferred embodiment of the present invention, the linearly displaceable blade support also supports an electromagnet. In addition, when the straight edge of the layer thickness uniformizing blade is positioned at a desired separation distance from the laser radiation transparent substrate, the electromagnet can be selectively actuated to lock the layer thickness uniformizing blade relative to the linearly displaceable blade support to prevent the layer thickness uniformizing blade from rotating about the pivot axis.
[0014] Preferably, the blade position maintainer comprises a force sensor for sensing a force exerted by the layer thickness homogenizing blade on the laser radiation transparent substrate.
[0015] According to a preferred embodiment of the present invention, the multi-pass precise donor material thickness determiner also includes a linear shifter, which is used to linearly shift the linearly shiftable leaf support between sequential passes to sequentially reduce the thickness of the donor material until the desired thickness is reached. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] The present invention will be more fully understood and appreciated from the following detailed description taken in conjunction with the accompanying drawings, in which:
[0017] Figure 1 is a simplified pictorial illustration of a coating system constructed and operative in accordance with a preferred embodiment of the present invention together with a typical substrate to be coated;
[0018] Figure 2 yes Figure 1 A simplified schematic partially exploded view illustration of a coating system;
[0019] Figure 3A and 3B It is formed by intercepting in different directions Figure 1 and 2 A simplified diagrammatic illustration of a layer thickness homogenization blade positioning subsystem of a portion of a coating system;
[0020] Figure 4A and 4B are intercepted in different directions Figure 3A and 3B A simplified diagrammatic illustration of the layer thickness homogenization blade positioning subsystem;
[0021] 5A, 5B and 5C are Figures 3A to 4B Simplified corresponding front plan views and first and second cross-sectional illustrations of the layer thickness uniformization blade positioning subsystem, FIGS. 5B and 5C are taken along lines 5B-5B and 5C-5C in FIG. 5A ;
[0022] 6A, 6B and 6C are formed Figures 3A to 4BSimplified corresponding first and second diagrammatic and side view illustrations of a layer thickness equalization blade of a portion of a layer thickness equalization blade positioning subsystem;
[0023] Fig. 7A and 7B is formed Figures 3A to 5C Simplified first and second diagrammatic illustrations of a blade and electromagnet mounting bracket of a portion of a layer thickness uniformization blade positioning subsystem;
[0024] 8A, 8B and 8C are formed Figures 3A to 5C Simplified corresponding diagrammatic, front plan and cross-sectional view illustrations of a blade mounting shaft member of a portion of a layer thickness uniformization blade positioning subsystem, FIG8C being taken along line 8C-8C in FIG8B;
[0025] Fig. 9A and 9B is a simplified schematic illustration of a typical initial step in positioning a layer thickness uniformization blade relative to a substrate, Fig. 9A and 9B The intercepts are made in mutually perpendicular directions;
[0026] Fig.10 is corresponding to Fig. 9A A simplified schematic illustration of further steps in positioning a layer thickness homogenization blade relative to a substrate;
[0027] Fig.11 is corresponding to Fig. 9A A simplified schematic illustration of yet a further step in positioning a layer thickness equalization blade relative to a substrate;
[0028] Fig.12 is corresponding to Fig. 9A A simplified schematic illustration of yet a further step in positioning a layer thickness equalization blade relative to a substrate;
[0029] Fig.13 is corresponding to Fig. 9A A simplified schematic illustration of additional steps in positioning a layer thickness uniformization blade relative to a substrate;
[0030] Fig.14 is corresponding to Fig. 9A a simplified schematic illustration of a further additional step in positioning a layer thickness uniformization blade relative to a substrate;
[0031] Fig.15 is using Figures 1 to 14 A simplified schematic illustration of typical initial steps in a system for coating a substrate with a highly viscous material;
[0032] Fig.16 is using Figures 1 to 14A simplified schematic illustration of further steps in a system for coating a substrate with a highly viscous material;
[0033] Fig.17 is using Figures 1 to 14 a simplified schematic illustration of yet a further step in a system for coating a substrate with a highly viscous material; and
[0034] Fig.18 is using Figures 1 to 14 A simplified schematic illustration of yet a further step in a system for coating a substrate with a highly viscous material. DETAILED DESCRIPTION
[0035] Reference now Figure 1 and 2 , which is a simplified pictorial illustration of a coating system 100 constructed and operative in accordance with a preferred embodiment of the present invention, along with a typical substrate to be coated.
[0036] like Figure 1 and 2 As seen in FIG. 1 , the coating system preferably includes a substrate assembly 110 that is generally stationary and may include a conventional vacuum chuck 112 for selectively holding a flat substrate 114 (preferably a laser radiation transparent substrate, preferably including a straight surface portion to be coated) securely thereon. The substrate assembly 110 is preferably formed from 6061T6 aluminum plate and machined to a high degree of parallelism between the substrate plane and the Y-stage mounting plate.
[0037] Preferably mounted on base assembly 110 is a Y-axis positioner 120, such as a Thorlabs NRT-100, which in turn supports a YZ adapter arm 130, typically formed from 6061T6 aluminum plate.
[0038] Preferably mounted to the YZ adapter arm 130 is a precision Z-axis positioner 140, such as a Thorlabs MTS25-Z8-25mm, which in turn supports a mounting bracket 150, typically formed of 6061T6 aluminum sheet. The mounting bracket 150 supports a layer thickness equalization blade positioning subsystem 160.
[0039] Now refer to Figures 3A to 5C , which illustrates the layer thickness uniformization blade positioning subsystem 160. Figures 3A to 5C As seen in FIG. 6A , the layer thickness equalization blade positioning subsystem 160 preferably includes a layer thickness equalization blade 170 preferably formed of 17-4HP steel, which will be described in more detail below with reference to FIGS. 6A to 6C .
[0040] The layer thickness equalization blade 170 is rotatably mounted to rotate about an axis 175 to a position hereinafter referred to as the layer thickness equalization blade 170 by means of an axis member 182 described in more detail hereinafter with reference to FIGS. 8A and 8B. Fig. 7A and 7B The blade and electromagnet described in more detail are mounted on a bracket 180, engaging a pair of rotating bearings 184, such as NSK angular contact 7900 bearings. A shaft 182 is fixed to the blade 170 along the axis 175 by means of screws 186.
[0041] The blade and electromagnet mounting bracket 180 also supports an electromagnet 190, such as a Magnetech R-0515-12, which can selectively lockably engage a locking arm 200 preferably formed of a ferromagnetic thin steel plate (e.g., 1020-1030). The locking arm 200 is selectively fixed to the layer thickness equalizing blade assembly 170 by fasteners not shown, so that the locking arm 200 fixes the angular orientation of the layer thickness equalizing blade 170 about the axis 175 by the locking of the electromagnet 190 magnetically engaged therewith.
[0042] The blade and electromagnet mounting bracket 180 is mounted to a force sensor 210 , such as a VISHAY LPS Loadcell, which is in turn supported by the mounting bracket 150 , by fasteners not shown.
[0043] Reference is now made to FIGS. 6A to 6C , which illustrate the layer thickness equalization blade 170. As seen in FIGS. 6A to 6C , the layer thickness equalization blade 170 preferably comprises a metal or plastic block having a generally flat back surface 300 from which extends a generally circular disc-shaped protrusion 302 formed with a threaded hole 303 for receiving the screw 186; a generally flat bottom surface 304 that is angled relative to the surface 300; and a generally flat blade front surface 306 that is angled relative to the bottom surface 304 and defines a blade engagement edge 308 together with the bottom surface 304.
[0044] The blade front surface 306 terminates upwardly at a lateral projection 310, above which a locking arm mounting surface (including an attachment surface 312, including a threaded locking mounting arm fastener attachment aperture 314 and a recessed locking arm engagement surface 316) is located. Surfaces 312 and 316 terminate at a blade top surface 320, which is preferably perpendicular to surfaces 312 and 316 and to surface 300.
[0045] Reference now Fig. 7A and 7B , which illustrates the blade and electromagnet mounting bracket 180. Fig. 7A and 7BAs seen in FIG. 1 , the blade and electromagnet mounting bracket 180 comprises a generally rectangular aluminum block defining a generally flat top surface 350 extending from a first end surface 352 to a slightly raised mounting surface 354 that is generally parallel to the top surface 350 and has a threaded aperture 356 for mounting the blade and electromagnet mounting bracket 180 to the force sensor 210 via fasteners (not shown). The mounting surface 354 terminates in a channel 358 that is at the height of the top surface 350 and separates the mounting surface from a raised edge surface 360 that is slightly higher than the height of the mounting surface 354.
[0046] The raised edge surface 360 terminates in a second end surface 362 that extends generally perpendicular to the top surface 350 to an inclined surface 364 that terminates in an intermediate bottom surface 366 that is generally parallel to the top surface 350. The bottom surface 366 terminates in a third end surface 367 that in turn terminates in an inclined surface 368. The inclined surface 368 terminates in a bottom surface 390 that is parallel to the top surface 350. The bottom surface 390 terminates in an inclined surface 392 that terminates in the first end surface 352. The blade and electromagnet mounting bracket 180 is formed with Figure 7B a generally planar front surface 394 best seen in FIG. 1 , and Fig. 7A The generally flat rear surface 396 is best seen in FIG.
[0047] The blade and electromagnet mounting bracket 180 is formed with a through bearing receiving hole 400 having an inwardly directed edge 402 at the front surface 394 and is configured to receive and retain the bearing 184 therein. The blade and electromagnet mounting bracket 180 is also formed with a through electromagnet receiving hole 410 and is configured to receive the electromagnet 190.
[0048] The slot 420 extends between the hole 410 and the top surface 350. The slot 420 enables the electromagnet 190 to be clamped within the hole by tightening the hole 410 via a tightening screw, not shown, which engages a threaded aperture 422 on an opposite side of the slot 420.
[0049] Recess 430 extends between holes 400 and 410 and is formed with a threaded aperture 432. Recess 440 is located beside hole 410 and is formed with an aperture 442. Recesses 430 and 440 and corresponding apertures 432 and 442 are provided to receive a not shown bearing retaining screw that holds bearing 184 in place in hole 400 of blade and electromagnet mounting bracket 180.
[0050] Reference is now made to FIGS. 8A to 8C , which illustrate shaft 182. As seen in FIGS. 8A to 8C , shaft 182 is a generally cylindrical hollow object of circular symmetry, preferably formed of aluminum, and having a circular cylindrical body 500 and an annular flange 502 at a first end thereof. A through central hole 504 extends through flange 502 and body 500 and has a tapered opening 506 at flange 502. Screw 186 ( Figure 4B ) extends through the hole 504 and the threaded aperture 303 of the blade 170 is uniformly formed with the threaded engagement layer.
[0051] Reference now Fig. 9A and 9B , which is a simplified schematic illustration of a typical initial step in positioning a layer thickness homogenization blade relative to a substrate, Fig. 9A and 9B are intercepted in mutually perpendicular directions. Fig. 9A and 9B As seen in FIG. 1 , the blade 170 is located above and not in contact with the substrate 114 and is free to pivot on the bearing 184 about the axis 175 due to the fact that the electromagnet 190 is not operable to lock the position of the locking arm 200 fixed to the blade 170 .
[0052] Fig.10 The blade 170 is illustrated lowered until the blade engagement edge 308 contacts the substrate 114, typically at the corner of the blade 170. Due to the fact that the electromagnet 190 is not operable to lock the position of the locking arm 200 secured to the blade 170, the blade 170 remains free to pivot about the axis 175 on the bearing 184.
[0053] Fig.11 The blade 170 is further lowered until the blade engagement edge 308 is placed in parallel contacting engagement with the substrate 114. Due to the fact that the electromagnet 190 is not operable to lock the position of the locking arm 200 fixed to the blade 170, the blade 170 remains free to pivot about the axis 175 on the bearing 184.
[0054] Fig.12 The blade 170 is further lowered until the measured force of the blade 170 on the substrate 114 as measured by the force sensor 150 is preferably about 150 grams, and the lower edge 308 is placed in parallel contact engagement with the substrate 114 and the blade 170 and because the electromagnet 190 is inoperable to lock the position of the locking arm 200 fixed to the blade 170, the blade 170 remains free to pivot about the axis 175 on the bearing 184.
[0055] Fig.13 When the blade 170 is in the above reference Fig.12In the described operational orientation, the position of the locking arm 200 fixed to the blade 170 is locked by operation of the electromagnet 190, thereby locking the blade to prevent it from pivoting about the axis 175 and maintaining the blade in an orientation about the axis 175, wherein the lower edge 308 is placed in parallel contact engagement with the substrate 114.
[0056] Fig.14 The blade 170 and pivot axis 175 are shown raised along the Z axis to define a predetermined desired separation distance 505, typically 2 mm, between the blade engagement edge 308 and the substrate 114. Due to the fact that the electromagnet 190 is operable to lock the position of the locking arm 200 fixed to the blade 170, the blade 170 is not free to pivot about the axis 175 on the bearing 184.
[0057] Reference now Fig.15 , which is using Figures 1 to 14 A simplified schematic illustration of typical steps in a system for coating a substrate (preferably a laser radiation transparent substrate) with a donor material (preferably a highly viscous material). Fig.15 As seen in FIG. 5 , donor material 510 , preferably a highly viscous material such as Henkel 8143 having a viscosity of 20,000 centipoise, is deposited onto substrate 114 downstream of blade 170 , the direction of movement of blade 170 along the Y-axis being indicated by arrow 520 .
[0058] like Fig.16 , 17 18, multiple passes of the blade 170 occur and between each pass, the separation distance between the blade engaging edge 308 and the substrate 114 is reduced by lowering the blade and pivot shaft 175 along the Z axis so that the desired final thickness of the material 510 is generally between 10 and 150 mm. Fig.16 In the embodiment, a separation distance 530 of typically 1 mm is defined between the blade engaging edge 308 and the substrate 114, and typically Fig.17 In the embodiment, a separation distance 540 of typically 0.3 mm is defined between the blade engaging edge 308 and the substrate 114, and typically Fig.18 In FIG. 5 , a separation distance 550 of typically 0.05 mm (but may be as low as 10 μm for lower viscosity materials 510 ) is defined between the blade engaging edge 308 and the substrate 114 .
[0059] It should be appreciated that the separation distance between the blade-joining edge 308 and the substrate 114 described above, which reduces the thickness of the donor material on the substrate 114 to a desired final thickness, is uniform along the entire blade-joining edge 308. As described above, the separation distance varies as the blade 170 is lowered relative to the substrate 114. By reducing the separation distance, the thickness of the donor material 510 is preferably reduced to a final thickness defined by the final separation distance, preferably between 10 microns and 2000 microns.
[0060] It will be apparent to persons skilled in the art that the present invention is not limited to what is specifically described and shown herein, but also encompasses combinations and sub-combinations of features described herein that are not in the prior art, and modifications thereof.
Claims
1. A method for applying a donor material to a laser radiation transparent substrate having a straight surface portion, the method comprising: providing a layer thickness equalizing blade pivotably mounted about a pivot axis to a linearly displaceable blade support, the blade having a straight edge, wherein the layer thickness equalizing blade is pivotably mounted to the shaft member; initially positioning the linearly displaceable blade support relative to the laser radiation transparent substrate such that the straight edge is disposed coplanarly with the straight surface portion of the laser radiation transparent substrate, wherein the straight surface portion is disposed along a blade engagement axis that is perpendicular to the pivot axis; thereafter locking the layer thickness equalizing blade to prevent pivotable movement thereof relative to the linearly displaceable blade support about the pivot axis; thereafter repositioning the linearly displaceable blade support and the layer thickness uniformizing blade about a linear displacement axis perpendicular to the blade engagement axis and perpendicular to the pivot axis to a position where the straight edge is separated from the straight surface portion of the laser radiation transparent substrate by a separation distance that is uniform along the straight edge of the layer thickness uniformizing blade; applying the donor material to the laser radiation transparent substrate; providing a mutual displacement between the layer thickness homogenizing blade and the laser radiation transparent substrate along an axis parallel to the pivot axis, thereby to reduce the thickness of the initial layer of the donor material; and The separation distance is maintained.
2. The method of claim 1, further comprising sequentially repeating the repositioning and providing mutual displacement steps at least once thereby to sequentially reduce the thickness of the donor material.
3. The method of claim 1 and wherein said providing a mutual displacement comprises reducing the thickness of the donor material to a thickness of between 10 microns and 2000 microns.
4. The method of claim 1, and wherein said initially positioning said linearly displaceable blade support comprises measuring a force exerted by said layer thickness homogenizing blade on said laser radiation transparent substrate.
5. The method according to claim 1, and wherein the initially positioning comprises initially positioning the layer thickness uniformizing blade such that a portion of the straight edge of the layer thickness uniformizing blade contacts the laser radiation transparent substrate while the layer thickness uniformizing blade is free to pivot about the pivot axis.
6. The method of claim 5, wherein said initially positioning further comprises thereafter lowering said layer thickness homogenizing blade such that said straight edge is placed in parallel contacting engagement with said laser radiation transparent substrate while said layer thickness homogenizing blade is free to pivot about said pivot axis.
7. The method of claim 6, wherein the initial positioning further comprises thereafter further lowering the layer thickness uniformizing blade until the measured force of the layer thickness uniformizing blade on the laser radiation transparent substrate is approximately 150 grams, while the straight edge of the layer thickness uniformizing blade is placed in parallel contacting engagement with the laser radiation transparent substrate and the layer thickness uniformizing blade remains free to pivot about the pivot axis.
8. The method according to claim 1, wherein locking the layer thickness uniformizing blade to prevent it from pivotally moving about the pivot axis relative to the linearly displaceable blade support is provided by an operation of an electromagnet mounted to the linearly displaceable blade support to attract a locking arm fixed to the layer thickness uniformizing blade.
9. The method of claim 1, wherein the repositioning occurs when the layer thickness equalization blade is not freely pivotable about the pivot axis.
10. A system for applying a donor material to a laser radiation transparent substrate, the system comprising: a donor material applicator for applying a donor material to the laser radiation transparent substrate; A multi-pass precision donor material thickness determiner for providing a desired thickness of the donor material onto the laser radiation transparent substrate and comprising: Linear displaceable blade bracket; a layer thickness equalizing blade lockably pivotably mounted to the linearly displaceable blade support about a pivot axis, the layer thickness equalizing blade having a straight edge, wherein the layer thickness equalizing blade is pivotably mounted to a shaft member; a blade position maintainer operable to maintain the straight edge at a desired separation distance from the laser radiation transparent substrate, the separation distance being uniform along the straight edge of the layer thickness uniformizing blade; as well as A locking arm is selectively fixed to the layer thickness equalizing blade such that the locking arm fixes the angular orientation of the layer thickness equalizing blade about the pivot axis by magnetically locking the locking arm by an electromagnet.
11. The system of claim 10, wherein the multi-pass precise donor material thickness determiner is configured to produce the desired thickness of the donor material on the laser radiation transparent substrate between 10 microns and 2000 microns.
12. The system of claim 10, wherein the linearly displaceable blade support is linearly displaceable perpendicular to the pivot axis.
13. The system of claim 10, wherein the linearly displaceable blade support further supports an electromagnet.
14. The system of claim 13, wherein when the straight edge of the layer thickness uniformizing blade is positioned at a desired separation distance from the laser radiation transparent substrate, the electromagnet is selectively actuatable to lock the layer thickness uniformizing blade relative to the linearly displaceable blade support to prevent the layer thickness uniformizing blade from rotating about the pivot axis.
15. The system of claim 10, wherein the blade position maintainer comprises a force sensor for sensing a force exerted by the layer thickness uniformization blade on the laser radiation transparent substrate.
16. The system of claim 10, wherein the linearly displaceable leaf support is configured to linearly displace between sequential passes to sequentially reduce the thickness of the donor material until the desired thickness is reached.
Citation Information
Patent Citations
Method and device for nano-micro transformation of metal material surface
CN101555543A
Device and method for producing sheet for abrasive coating and the sheet
CN1691988A
Donor substrate assembly applicable to circuit repairing
CN201976350U
Squeegee device