A method for manufacturing a shielded gate MOSFET device with an upper and lower structure
By using multiple etching and etching methods in shielded gate MOSFET devices, combined with the use of silicon nitride layers and field oxide layers, high-quality gate oxide layers and inter-gate oxide layers are formed, which solves the problem of high cost in the existing technology. Solve the problem of large capacitance and realize the production of low capacitance and high reliability devices.
Patent Information
- Application Number
- CN202111158564.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-30
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2041-09-30
AI Technical Summary
In the existing manufacturing method of upper and lower structure shielded gate MOSFET devices, the cost is high and it is difficult to form an inter-gate oxide layer of good quality and uniformity, resulting in a large capacitance of the device, and the lower end of the control gate is easy to form sharp corners, which reduces the reliability of the device. .
By forming deep trenches on the N epitaxial silicon substrate, depositing polysilicon and performing multiple etchings and etchings back, combined with the use of silicon nitride layers and field oxide layers, the gate oxide layer and the inter-gate oxide layer are formed using thermal oxidation methods. Reduce the overlapping area of the shielding grid and the control grid and reduce production costs.
It achieves a smaller overlapping area of the shield gate and the control gate, reduces the capacitance of the device, avoids the formation of sharp corners, and the process is simple, safe and reliable, and reduces production costs.
Smart Images

Figure CN114038751B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of design and manufacturing of shielded gate MOSFET (SGT-MOSFET) devices, and in particular to a manufacturing method of a shielded gate MOSFET device with a top-bottom structure. Background Art
[0002] Compared with traditional trench MOSFET, shielded gate MOSFET devices have the advantages of low on-resistance and low switching loss, so their application in the medium and low voltage power semiconductor market is gradually increasing. The gate of the shielded gate trench MOSFET structure includes both the shielding gate and the control gate. The existence of the shielding gate makes the longitudinal electric field similar to the rectangular distribution when the device breaks down. Compared with the traditional trench MOSFET, the application of a smaller resistivity epitaxial can obtain a higher breakdown voltage, so that the device has a smaller on-resistance. According to the relative position of the shielding gate and the control gate in the trench, shielded gate MOSFET devices are usually divided into two types: upper and lower structures and left and right structures. For shielded gate MOSFET devices with upper and lower structures, there are currently two mature manufacturing processes, mainly in the process methods and steps of making the inter-gate oxide layer (Inter Poly Oxide) after forming the shielding gate. One is to deposit the shielding gate polysilicon back into the trench to form a shielding gate, and then first fill the trench on the shielding gate with HDP and then etch back to a certain depth to form an inter-gate oxide layer, and then form a gate oxide layer on the sidewall of the trench by thermal oxidation. This method can control the thickness of the inter-gate oxide layer more accurately, but the manufacturing cost is relatively high. The other method is to deposit the shield gate polysilicon and etch it back into the groove to form a shield gate, and then wet etch the field oxide layer. Through thermal oxidation, a gate oxide layer and an inter-gate oxide layer are formed on the sidewalls of the trench and the top of the shield gate at the same time. The control gate is like a hat surrounding the upper part of the shield gate, so that the capacitance area between the shield gate and the control gate is larger, so the input capacitance of the device is relatively large. At the same time, there are sharp corners at the bottom of the control gate, which easily increases the leakage between the shield gate and the control gate, thereby reducing the reliability of the device. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a method for manufacturing a shielded gate MOSFET device with an upper and lower structure that can effectively reduce production costs, form an inter-gate oxide layer with good quality and uniformity, reduce the capacitance of the device, and has a simple, easy, safe and reliable preparation method in response to the above-mentioned defects of the prior art.
[0004] The object of the present invention is to achieve the following technical solution, a method for manufacturing a shielded gate MOSFET device with an upper and lower structure, the manufacturing method comprising the following steps:
[0005] 1) Depositing an oxide layer as a hard mask on the selected N epitaxial silicon substrate, using the first mask plate to perform photolithography and deep trench etching on the N epitaxial silicon substrate, and forming trenches in the primary cell region and the terminal region at the same time;
[0006] 2) Prepare a field oxide layer of corresponding thickness according to the breakdown voltage requirements of the product;
[0007] 3) Deposit polysilicon, and first etch back the polysilicon to form a shield gate close to the silicon surface. Then, chemical mechanical polishing is used to make the oxide layer thickness on the silicon surface less than 2000A, in order to reduce lateral etching during subsequent wet etching.
[0008] 4) Depositing a silicon nitride layer, the thickness of the silicon nitride layer is 1000A~3000A;
[0009] 5) Use the second mask to perform photolithography on the trench of the active area, and dry-etch to remove the exposed silicon nitride layer;
[0010] 6) Remove the field oxide layer on the sidewall of the trench in the active area by wet etching. The depth of the oxide layer etched in the trench is 0.5um~1.5um, which is determined by the breakdown voltage of the device design and the optimal channel length;
[0011] 7) Perform a second dry etching on the polysilicon in the trench of the original cell area to make the polysilicon layer 0.1~0.3 microns lower than the field oxide layer;
[0012] 8) Wet etching to remove the silicon nitride layer, and then wet etching to remove the oxide layer on the silicon surface, so that the height of the polysilicon shielding gate in the trench is controlled within 0.2 microns above or below the height of the field oxide layer;
[0013] 9) Forming a gate oxide layer on the sidewall of the trench by thermal oxidation, and forming an inter-gate oxide layer on the top of the polysilicon shielding gate;
[0014] 10) Deposit gate polysilicon and use chemical mechanical polishing or wet etching to etch the gate polysilicon to the silicon surface to form the control gate of the device;
[0015] 11) Perform subsequent process processing to complete the fabrication of the shielded gate MOSFET device.
[0016] Furthermore, the subsequent process in step 11) includes the following steps:
[0017] 12) Perform body region implantation and annealing to form a body region with a conductivity type opposite to that of the substrate and epitaxial layer;
[0018] 13) Use the third mask to perform source region photolithography and inject impurities of the same conductivity type as the substrate and epitaxy and anneal to form a heavily doped source region;
[0019] 14) Deposit a dielectric layer, then use the fourth mask to perform contact hole lithography, and etch to form source, gate and shield gate contact holes;
[0020] 15) Sputter the top metal, use the fifth mask to photolithography and etch to form the top metal;
[0021] 16) Deposit an oxide layer as a passivation layer, and use the sixth mask to etch the passivation layer to complete the top structure;
[0022] 17) Thin the back side of the silicon wafer to a specific thickness, and deposit metal on the back side by sputtering or evaporation to form the drain of the device.
[0023] Furthermore, in step 3), the polysilicon is deposited, and the first polysilicon back etching is performed close to the silicon surface, and then chemical mechanical polishing is performed to make the thickness of the oxide layer on the silicon surface less than 2000 Å, in order to reduce lateral etching during subsequent wet etching.
[0024] Furthermore, in step 7), silicon nitride is used as a hard mask in the second dry etching of the polysilicon, and after etching, the polysilicon layer is 0.1 um to 0.3 microns lower than the field oxide layer.
[0025] Furthermore, in step 8), the silicon nitride layer is removed by wet etching, and then the oxide layer on the silicon surface is removed by wet etching, so that the height difference between the polysilicon shielding gate in the trench and the field oxide layer is within 0.2 microns.
[0026] The beneficial technical effect of the present invention is that after the shield gate polysilicon is first etched back to the silicon surface, a silicon nitride layer is deposited as a hard mask, and then the field oxide layer is etched in the original cell area trench, and then the shield gate polysilicon is etched back for the second time, and then the field oxide layer is wet etched to form a structure in which the height difference between the shield gate polysilicon and the field oxide layer is within 0.2 microns in the original cell area trench, and then the gate oxide layer and the inter-gate oxide layer (IPO) are generated by thermal oxidation. The shield gate device formed by this manufacturing method has a smaller shield gate and control gate overlap area than the traditional manufacturing method, thereby reducing the capacitance of the device; in addition, compared with the traditional manufacturing method of forming an inter-gate oxide layer by filling etching through HDP, the cost is lower and the problem of forming a sharp corner at the lower end of the control gate is avoided. At the same time, the preparation method proposed by the present invention is compatible with the existing process steps, thereby effectively reducing the production cost, and the entire manufacturing process is safe and reliable. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a schematic diagram of deep trench etching;
[0028] Figure 2 It is a schematic diagram of the field oxide layer growth;
[0029] Figure 3 This is a schematic diagram of the shield gate polysilicon filling and etching back;
[0030] Figure 4 It is a schematic diagram of silicon nitride deposition;
[0031] Figure 5 It is a schematic diagram of silicon nitride photolithography etching;
[0032] Figure 6 This is a schematic diagram of etching the field oxide layer;
[0033] Figure 7 It is a schematic diagram of shield gate polysilicon etching;
[0034] Figure 8 It is a schematic diagram of silicon nitride removal and oxide layer removal;
[0035] Fig. 9 It is a schematic diagram of the growth of gate oxide layer and inter-gate oxide layer;
[0036] Fig.10 Schematic diagram of control gate polysilicon filling and etching back. DETAILED DESCRIPTION
[0037] In order to enable those skilled in the art to more clearly understand the objectives, technical solutions and advantages of the present invention, the present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0038] like Figure 1-10 As shown, the present invention proposes a method for manufacturing a shielded gate MOSFET device with an upper and lower structure, especially a relatively unique manufacturing method from the deposition of the shielding gate to the formation of the control gate. The present invention is to deposit a layer of silicon nitride as a hard mask after the shielding gate is filled and etched back to the silicon surface for the first time, and then etch the silicon nitride layer and the field oxide layer on the top of the original cell area trench, and then perform a second shielding gate polysilicon etching, and then use a thermal oxidation process to grow an oxide layer on the sidewall of the trench and the top of the shielding gate to form the gate oxide layer and the inter-gate oxide layer (IPO) of the device. The preparation method proposed by the present invention avoids the traditional method of forming an inter-gate oxide layer by HDP filling, and its specific manufacturing method includes the following steps:
[0039] 1) depositing an oxide layer with a thickness of 0.5-1 μm on a selected N epitaxial silicon substrate 2 as a hard mask, using the first mask of the present invention to perform photolithography and deep trench etching on the N epitaxial silicon substrate 2, and simultaneously forming trenches 3 in the primary cell region and the terminal region; Figure 1 shown.
[0040] 2) A field oxide layer 4 of corresponding thickness is prepared according to the breakdown voltage requirement of the product. The field oxide layer 4 can be formed by thermal oxidation or by thermal oxidation plus deposition of an oxide layer; Figure 2 shown.
[0041] 3) Deposit polysilicon, and then perform the first back etching of the polysilicon close to the silicon surface to form a shield gate 5, and then use chemical mechanical polishing to make the oxide layer thickness on the silicon surface less than 2000A, in order to reduce the lateral etching during the subsequent wet etching; Figure 3 shown.
[0042] 4) depositing a silicon nitride layer 6 as a hard mask, the thickness of the silicon nitride layer 6 being about 1000A~3000A; Figure 4 shown.
[0043] 5) Using the second mask of the present invention, photolithography is performed on the grooves in the active area, and the exposed silicon nitride layer 6 is removed by dry etching; Figure 5 shown.
[0044] 6) Remove the field oxide layer 4 on the sidewall of the trench in the active area by wet etching. The depth of the oxide layer 4 etched in the trench is 0.5um~1.5um, which is determined by the breakdown voltage of the device design and the channel length to achieve the optimal value; Figure 6 shown.
[0045] 7) Perform a second dry etching on the polysilicon in the trench of the original cell area. Silicon nitride is used as a hard mask in the dry etching, so that the polysilicon layer is lower than the field oxide layer 4, and the height difference between the polysilicon layer and the field oxide layer 4 is about 0.1um~0.3um; Figure 7 shown.
[0046] 8) Wet etching to remove the silicon nitride layer, and then wet etching to remove the oxide layer on the silicon surface, so that the height difference between the polysilicon shielding gate in the trench and the field oxide layer 4 is controlled within 0.2 microns; Figure 8 shown.
[0047] 9) forming a gate oxide layer 8 on the sidewall of the trench by thermal oxidation, and forming an inter-gate oxide layer 7 on the top of the polysilicon shielding gate; Fig. 9 shown.
[0048] 10) depositing gate polysilicon, and etching the gate polysilicon to the silicon surface by chemical mechanical polishing or wet etching to form the control gate 9 of the device; Fig.10 The top of the shielding gate and the bottom of the control gate of the shielding gate MOSFET device formed by this manufacturing method are almost parallel, so that the inter-gate capacitance area is small and the capacitance is correspondingly low.
[0049] 11) Perform subsequent process treatment to complete the fabrication of shielded gate MOSFET devices, including body region implantation and annealing; photolithography of source region and implantation of source region; deposition of dielectric layer, photolithography of contact holes, etching of dielectric layer; sputtering of top metal, photolithography of top metal; deposition of passivation layer, photolithography of passivation layer, completion of fabrication of top structure; then wafer thinning and back metal deposition, etc., which specifically includes the following steps:
[0050] 12) Perform body region implantation and annealing to form a body region with a conductivity type opposite to that of the substrate and epitaxial layer;
[0051] 13) Use the third mask to perform source region photolithography and inject impurities of the same conductivity type as the substrate and epitaxy and anneal to form a heavily doped source region;
[0052] 14) Deposit a dielectric layer, then use the fourth mask to perform contact hole photolithography, and etch to form source, gate and shield gate contact holes;
[0053] 15) Sputter the top metal, use the fifth mask to photolithography and etch to form the top metal;
[0054] 16) Deposit an oxide layer as a passivation layer, and use the sixth mask to etch the passivation layer to complete the top structure;
[0055] 17) The back side of the silicon wafer is thinned to a specific thickness, and a back side metal is deposited by sputtering or evaporation to form the drain 1 of the device.
[0056] After the polysilicon is filled in the trench, the present invention performs the first polysilicon back etching, deposits the silicon nitride layer as a hard mask, then performs the field oxide layer etching first, then performs the second shield gate polysilicon etching, performs the oxide layer wet etching again, and then performs thermal oxidation to generate the gate oxide layer and the inter-gate oxide layer (IPO), forming an inter-gate oxide layer with good quality and uniformity, while reducing the overlapping area of the shield gate and the control gate in the traditional manufacturing method, and correspondingly reducing the capacitance of the device; in addition, compared with the traditional manufacturing method of forming the inter-gate oxide layer by filling etching through HDP, the cost is lower and the problem of forming a sharp corner at the lower end of the control gate is avoided. At the same time, the preparation method proposed by the present invention is compatible with the existing process steps, thereby effectively reducing the production cost, and the entire manufacturing process is safe and reliable.
[0057] The specific embodiments described herein are merely illustrative of the principles and effects of the present invention and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A method for manufacturing a shielded gate MOSFET device with an upper and lower structure, characterized in that: The production method comprises the following steps: 1) depositing an oxide layer as a hard mask on the selected N epitaxial silicon substrate, using the first mask plate to perform photolithography and etching on the N epitaxial silicon substrate to simultaneously form deep trenches in the primary cell region and the terminal region; 2) Prepare a field oxide layer of corresponding thickness according to the breakdown voltage requirements of the product; the field oxide layer covers the surface of the N epitaxial silicon substrate and the surface of the deep trench; 3) Deposit polysilicon, perform the first polysilicon back etching close to the silicon surface to form a shield gate, and then use chemical mechanical polishing to make the oxide layer thickness on the silicon surface less than 2000 angstroms, in order to reduce lateral etching during subsequent wet etching; the top surface of the shield gate is flush with the top surface of the field oxide layer; 4) Depositing a silicon nitride layer, the thickness of the silicon nitride layer is 1000 angstroms to 3000 angstroms; 5) Use the second mask to perform photolithography on the trench of the active area, and dry-etch to remove the exposed silicon nitride layer; 6) Remove the field oxide layer on the sidewall of the trench in the active area by wet etching. The depth of the field oxide layer etched in the trench is 0.5um~1.5um, which is determined by the breakdown voltage of the device design and the optimal channel length; 7) Using the silicon nitride layer as a mask, perform a second dry etching on the polysilicon in the trench of the original cell area, so that the polysilicon layer in the trench of the original cell area is 0.1~0.3 microns lower than the field oxide layer; 8) Wet etching to remove the silicon nitride layer, and then wet etching to remove the field oxide layer on the silicon surface, so that the height difference between the polysilicon shield gate and the field oxide layer in the trench is within 0.2 microns; 9) Forming a gate oxide layer on the sidewall of the trench by thermal oxidation, and forming an inter-gate oxide layer on the top of the polysilicon shielding gate; 10) Deposit gate polysilicon and use chemical mechanical polishing or wet etching to etch the gate polysilicon to the silicon surface to form the control gate of the device; 11) Perform body region implantation and annealing to form a body region with a conductivity type opposite to that of the substrate and epitaxial layer; 12) Use the third mask to perform source region photolithography and inject impurities of the same conductivity type as the substrate and epitaxy and anneal to form a heavily doped source region; 13) Deposit a dielectric layer, then use the fourth mask to perform contact hole lithography, and etch to form source, gate and shield gate contact holes; 14) Sputter the top metal, use the fifth mask to photolithography and etch to form the top metal; 15) Deposit an oxide layer as a passivation layer, and use the sixth mask to etch the passivation layer to complete the top structure; 16) Thin the back side of the silicon wafer to a specific thickness and deposit metal on the back side by sputtering or evaporation to form the drain of the device.