A diamond-sealed fiber grating sensor device and its manufacturing method
Through diamond sealing and vacuum hot pressing technology, the problem of insufficient sealing of fiber Bragg grating sensors in harsh environments is solved, the formation of a high-density layered structure is achieved, the acid and alkali resistance and high and low temperature resistance of the sensor are enhanced, and the service life is extended. and simplifies the production process.
Patent Information
- Application Number
- CN202111479168.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-06
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2041-12-06
AI Technical Summary
Existing fiber grating sensors are susceptible to physical collisions, acid, alkali and salt corrosion, and high and low temperature environments in severe weather and natural disasters, resulting in insufficient sealing and affecting the sensitivity and service life of the sensor.
Using a diamond-sealed fiber grating sensing device, the high-density and uniformly distributed metal-plated diamond particles are closely combined with the metal-plated fiber grating through vacuum hot pressing technology to form a high-density layered structure, which enhances sealing and utilizes the high hardness and hardness of diamond. Chemical stability against external erosion.
It achieves effective isolation from the external environment, improves the acid and alkali resistance, corrosion resistance and high and low temperature resistance of the sensor, extends the service life of the sensor, and simplifies the production process, making it suitable for mass production.
Smart Images

Figure CN114184216B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of optical fiber sensing, and specifically relates to an optical fiber grating sensing device and a manufacturing method thereof, in particular to an optical fiber grating sensing device sealed with diamond and a manufacturing method thereof. Background Art
[0002] Optical fiber is mainly made of quartz glass, and optical fiber sensors that use optical fiber as a transmission medium and manufacturing element have their unique advantages. Through different sealing materials and process designs, they can achieve the measurement of various physical quantities (such as temperature, strain, vibration, displacement, torque, etc.). Fiber grating sensors have the advantages of high precision, good long-term stability, anti-electromagnetic interference, and anti-mechanical fatigue, and are an ideal substitute for electrical sensors.
[0003] In recent years, with the development of intelligent transportation networks, fiber grating sensing technology has been widely used in the health monitoring system of roads, bridges and tunnels. However, ordinary fiber grating sealing technology is still very insufficient in resisting physical collisions, acid, alkali and salt erosion, and high and low temperature environments in special environments such as severe weather and natural disasters. In addition, the commonly used sealing method for grating sensors is structural assembly, and the gaps between structural parts are inevitably penetrated by corrosive substances (acids, alkalis, salts, etc.) in the air. Over time, it is very easy to damage the grating sealed inside, thereby affecting the sensitivity of the sensor and shortening the service life of the sensor.
[0004] In nature, diamonds are formed under high temperature (1800°C) and high pressure (70,000 atmospheres) conditions deep in the earth. The structure between carbon atoms is very strong and arranged regularly, so diamonds have the characteristics of high hardness, high melting point, high insulation, chemical stability, acid and alkali corrosion resistance, etc. Diamonds can now be artificially produced. If diamonds can be used to seal optical fiber Bragg gratings while maximizing the airtightness of the packaging process, then a series of problems in resisting the above-mentioned harsh conditions will be solved. Summary of the invention
[0005] In view of the above defects or improvement needs of the prior art, the present invention provides a fiber grating sensor device and a method for manufacturing the same, in particular, a fiber grating sensor device sealed with diamond and a method for manufacturing the same, the purpose of which is to utilize the fluidity of metal in a high-temperature molten state, through vacuum hot pressing, to tightly combine high-density and uniformly distributed metal-plated diamond particles with the metal-plated fiber grating, and to squeeze out excess metal liquid and air.
[0006] The final diamond-sealed fiber grating sensor device is integrally formed, and the diamonds inside it are distributed in high-density layers: on the one hand, it has good sealing properties, which can maximize the protection of the internal fiber grating from penetration and erosion by the external environment; at the same time, diamond itself has a high melting point, high hardness, strong chemical stability, and resistance to acid and alkali corrosion. Therefore, the sensor housing sealed with diamond can not only naturally resist external collisions, but also has excellent acid and alkali resistance, corrosion resistance, and high and low temperature resistance.
[0007] To achieve the above-mentioned purpose, according to one aspect of the present invention, there is provided a fiber grating sensing device using diamond sealing, comprising a fiber grating and a diamond, wherein the fiber grating is a fiber grating treated with high temperature annealing, and is a metal-plated grating made by a metal plating process; the diamond is a metal-plated diamond made by a salt bath method; the metal-plated grating is placed in a designed hot pressing mold, and metal foil and a metal mesh inlaid with metal-plated diamond particles are laid layer by layer in both the upper and lower directions of the metal-plated grating in the mold, and after vacuum hot pressing treatment, the diamonds are evenly distributed in high-density layers above and below the optical fiber.
[0008] Preferably, the hot pressing mold is provided with a hot pressing base, an optical fiber and a fixing fixture thereof, an upper pressing cover matched with the hot pressing mold and an upper pressing head of the hot pressing equipment, and the pressing head of the hot pressing equipment is equipped with a pressure source.
[0009] At the same time, the invention provides a method for manufacturing a fiber grating sensor device sealed with diamond.
[0010] Preferably, the technical solution of the method for manufacturing the diamond-sealed fiber Bragg grating sensor device of the present application comprises the following steps:
[0011] S1, metal coating on the surface of fiber Bragg grating;
[0012] S2, coating metal on the surface of diamond particles;
[0013] S3, placing the metal-plated fiber Bragg grating in the designed hot pressing mold;
[0014] S4, laying metal foils and metal mesh inlaid with metal-coated diamond particles layer by layer on the grating in the hot pressing mold;
[0015] S5, putting into vacuum hot pressing furnace for hot pressing forming.
[0016] Preferably, in step S1, the optical fiber is a PI-coated fiber Bragg grating.
[0017] Preferably, in step S1, the fiber Bragg grating is a fiber Bragg grating that has been subjected to high temperature annealing treatment.
[0018] Preferably, in step S1, the fiber Bragg grating metallization process adopts a mixed process of magnetron sputtering and electroplating.
[0019] Preferably, in step S1, the length of the metal coating of the metal-coated grating is between 3 and 15 cm, and the thickness of the coating is between 300 and 900 μm.
[0020] Preferably, in any one of steps S1, S2, S3 and S4, the metal and the metal mesh are the same metal.
[0021] Preferably, in step S2, the diamond mesh size is between 100 and 200.
[0022] Preferably, in step S2, the diamond needs to be cleaned with hydrochloric acid, acetone or the like before metal plating.
[0023] Preferably, in step S2, the diamond metal plating process adopts a salt bath method.
[0024] Preferably, in step S2, the thickness of the metal coating on the surface of the metal-coated diamond is between 0.1 and 1 μm.
[0025] Preferably, in step S3, the hot pressing mold is made of a nickel-chromium alloy resistant to high temperature and high pressure.
[0026] Preferably, in step S3, optical fiber lead-out protection devices are provided on both sides of the hot pressing mold.
[0027] Preferably, in step S3, the hot pressing space and shape in the hot pressing mold are adjustable, and the optical fiber in the internal cavity can be laid to a length of not less than 3 cm.
[0028] Preferably, in step S4, the thickness of the metal foil is between 0.3 and 0.7 mm.
[0029] Preferably, in step S4, a metal mesh filled with metal-plated diamond particles is arranged between the metal foils to obtain a diamond-metal-based composite to be sintered; the metal mesh is made of the same material as the metal foil, that is, a metal matrix material, and its mesh specifications are consistent with the diamond powder specifications of the diamond powder layer.
[0030] Preferably, in step S5, the vacuum hot pressing sintering step is: evacuate the hot pressing furnace, heat it to 650-1100°C, keep the hot pressing furnace warm for 40-180 minutes, and then sinter the diamond-metal matrix composite material; after the sintered diamond-metal matrix composite material is naturally cooled, it can be taken out; the pressure of the hot pressing furnace in the hot pressing sintering step is 15-50MPa, and the vacuum degree is 20-100Pa.
[0031] In general, the above technical solutions conceived by the present invention can achieve the following beneficial effects compared with the prior art:
[0032] The diamond-sealed fiber grating sensing device provided by the present invention utilizes the fluidity of metal in a high-temperature molten state to tightly combine high-density and uniformly distributed metal-plated diamond particles with the metal-plated fiber grating and squeeze out excess metal liquid and air.
[0033] Because the final diamond-sealed fiber Bragg grating sensor device is integrally formed, the diamonds inside it are distributed in high-density layers: on the one hand, it has good sealing properties, which can maximize the protection of the internal fiber Bragg grating from penetration and erosion by the external environment; at the same time, diamond itself has a high melting point, high hardness, strong chemical stability, and resistance to acid and alkali corrosion. Therefore, the sensor housing sealed with diamonds can not only naturally resist external collisions, but also has excellent acid and alkali resistance, corrosion resistance, and high and low temperature resistance; and the production process is simple, the equipment is simple, and the repeatability is good, which is suitable for mass production. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0035] Figure 1 is a schematic diagram of the structure of the annealed fiber Bragg grating after metal plating provided by an embodiment of the present invention;
[0036] Figure 2 It is a schematic diagram of the arrangement and structure of the metal-plated grating, metal-plated diamond, metal foil, and metal mesh inside the hot pressing mold provided by an embodiment of the present invention;
[0037] Figure 3 is a schematic diagram of the appearance of a hot pressing mold provided by an embodiment of the present invention;
[0038] Figure 4 is a schematic diagram of the internal environment of a vacuum hot pressing furnace during the hot pressing process of the device provided in an embodiment of the present invention;
[0039] Figure 5 It is a schematic diagram of the steps of a method for manufacturing a diamond-sealed fiber Bragg grating sensing device provided in an embodiment of the present invention.
[0040] In all the drawings, the same figure marks are used to represent the same elements or structures, among which: 1 is PI coated optical fiber, 2 is grating area, 3 is metal layer of metal-plated optical fiber, 4 is metal-plated diamond, 5 is metal mesh, 6 is metal foil; 7 is hot pressing mold, 8 is hot pressing base, 9 is optical fiber and its fixing clamp, 10 is the upper pressure cover matching the hot pressing mold, and 11 is the pressure head (pressure source) on the hot pressing equipment. DETAILED DESCRIPTION
[0041] In order to make the purpose, technical scheme and advantages of the present invention clearer, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0042] In order to overcome the defects of the prior art or to meet the need for improvement, an embodiment of the present invention provides a diamond-sealed fiber grating sensor device and a method for manufacturing the same, which utilizes the fluidity of metal in a high-temperature molten state and, through vacuum hot pressing, allows high-density, uniformly distributed metal-plated diamond particles to be tightly combined with the metal-plated fiber grating, and squeezes out excess metal liquid and air.
[0043] The diamond-sealed fiber Bragg grating sensing device and the manufacturing method thereof provided in the embodiment of the present invention mainly include the following steps:
[0044] S1, metal coating on the surface of fiber Bragg grating;
[0045] S2, coating metal on the surface of diamond particles;
[0046] S3, placing the metal-plated fiber Bragg grating in the designed hot pressing mold;
[0047] S4, laying metal foils and metal mesh inlaid with metal-coated diamond particles layer by layer on the grating in the hot pressing mold;
[0048] S5, putting into vacuum hot pressing furnace for hot pressing forming.
[0049] It should be noted that in step S1, the optical fiber is a PI-coated fiber Bragg grating. The PI coating has better high temperature resistance under harsh conditions and also provides effective protection for the optical fiber in subsequent heat treatment steps such as metal plating.
[0050] It should be noted that in step S1, the fiber Bragg grating adopts the PI coated fiber Bragg grating which has been subjected to high temperature annealing treatment, so as to further improve the high temperature resistance of the fiber Bragg grating after the annealing process.
[0051] It should be noted that in step S1, the fiber grating metal plating process adopts a mixed process of magnetron sputtering and electroplating: first, an ultra-high vacuum magnetron sputtering coating machine is used to coat a layer of metal film on the surface of the optical fiber. The purpose of this coating is to make the fiber grating conductive to facilitate the next step of electroplating. The thickness of this coating is 100 to 300 nm, and silver plating, copper plating, etc. can be selected; then electroplating thickening is performed, and the electrolyte solution metal plating scheme adopted in this article is used.
[0052] It should be noted that, in step S1, the length of the metal coating of the metal-coated grating is between 3 and 15 cm, the thickness of the coating is between 300 and 900 μm, and the grating should be wrapped in the middle of the metal coating.
[0053] It should be noted that in steps S1, S2, S3 and S4, the metal and the metal mesh are the same metal.
[0054] It should be noted that, in step S2, the diamond mesh size is between 100 and 200.
[0055] It should be noted that, in step S2, the diamond needs to be cleaned with hydrochloric acid, acetone, etc. before metal plating to improve the surface activity of the diamond.
[0056] It should be noted that in step S2, the diamond metal plating process adopts a salt bath method, that is, firstly, the metal powder and the diamond are placed in a crucible and mixed thoroughly, and then covered with a chloride-based salt, and the crucible is placed in a high-temperature resistance furnace after being heated to 650-1300°C, and kept warm for 60-180 minutes, and then taken out after cooling to room temperature as the furnace temperature, and the salt residue is removed, so that the diamond coated with a metal film can be obtained.
[0057] It should be noted that, in step S2, the thickness of the metal coating on the surface of the metal-plated diamond is between 0.1 and 1 μm.
[0058] It should be noted that in step S3, the hot pressing mold is made of high temperature and high pressure resistant nickel-chromium alloy.
[0059] It should be noted that, in step S3, optical fiber lead-out protection devices are provided on both sides of the hot pressing mold.
[0060] It should be noted that, in step S3, the hot pressing space and shape in the hot pressing mold can be adjusted according to the situation, but the laying length of the optical fiber in the internal cavity must not be less than 3 cm.
[0061] It should be noted that, in step S4, the thickness of the metal foil is between 0.3 mm and 0.7 mm.
[0062] It should be noted that in step S4, a metal mesh filled with metal-plated diamond particles is arranged between the metal foils to obtain a diamond-metal-based composite to be sintered; the material of the metal mesh is the same as that of the metal foil, which is a metal matrix material, and its mesh specifications are consistent with the diamond powder specifications of the diamond powder layer.
[0063] It should be noted that in step S5, the vacuum hot pressing sintering step is: evacuate the hot pressing furnace, heat it to 650-1100°C, keep the hot pressing furnace warm for 40-180 minutes, and then sinter the diamond-metal matrix composite material. After the sintering, the diamond-metal matrix composite material is naturally cooled and then taken out; the pressure of the hot pressing furnace in the hot pressing sintering step is 15-50MPa, and the vacuum degree is 20-1Pa.
[0064] In the specific implementation:
[0065] A fiber grating sensor device sealed with diamond is used to resist physical collision, acid, alkali and salt corrosion, high and low temperature changes and other harsh conditions in the application environment, and has extremely high airtightness. Figure 1 As shown, its structure includes:
[0066] The PI coated fiber Bragg grating 1 is annealed to further improve the high temperature resistance of the fiber Bragg grating 2 on the basis of the high temperature resistance of the PI coating. The specific process parameters are annealing at 950-1200°C and an annealing time of 60-120 minutes. The fiber Bragg grating after annealing can withstand a temperature of up to 1200°C.
[0067] A mixed process of magnetron sputtering and electroplating is used to plate metal for PI fiber Bragg gratings: first, an ultra-high vacuum magnetron sputtering coating machine is used to plate a layer of metallic silver on the surface of the optical fiber. The purpose is to make the fiber Bragg grating conductive and to facilitate the next step of electroplating. The thickness of the silver plating is about 100nm; then the electroplating is thickened. This article adopts the copper sulfate solution to electroplate copper on the fiber Bragg grating. The final metal coating 3: the length is 12cm~13cm, and the coating thickness is 670μm.
[0068] Before metal plating, the diamond is cleaned with hydrochloric acid and acetone to improve the surface activity of the diamond. The salt bath method is used to make copper-plated diamond. The specific method is: first, copper powder and 100-mesh diamond particles are placed in a crucible and mixed thoroughly, and then covered with calcium chloride salt. After the high-temperature resistance furnace is heated to 1100°C, the crucible is placed in it, kept warm for 150 minutes, and then taken out after cooling to room temperature with the furnace temperature, and the salt residue is removed with hot water. After vacuum drying, copper-plated diamond can be obtained, and the coating thickness is 0.3~0.6μm.
[0069] Hot pressing mold 7 Figure 3As shown, it is provided with a hot pressing base 8, an optical fiber and its fixing fixture 9, an upper pressing cover 10 matched with a hot pressing mold, and a pressing head 11 on the hot pressing equipment, and a pressure source is installed on the pressing head on the hot pressing equipment.
[0070] A layer of graphite paper is placed in the hot pressing mold 7 in advance to facilitate demoulding after sintering; the copper-plated grating is placed in the designed hot pressing mold, such as Figure 2 As shown, copper foil 6 and copper mesh 5 inlaid with copper-plated diamond particles 4 are laid layer by layer in the upper and lower directions of the copper-plated grating in the mold. Then, the mold is placed in a vacuum hot press furnace for sintering. Figure 4 As shown, the specific hot pressing parameters are set as follows:
[0071] The diamond-copper-based matrix composite obtained in the above steps is placed in a vacuum hot pressing furnace together with the optical fiber mold, evacuated to below 10-1Pa, heated to 1100°C, kept warm for 50 minutes, hot pressed and sintered at a pressure of 40MPa, and cooled while maintaining pressure; then reheated to 1020°C, kept warm for 70 minutes and hot pressed and sintered at a pressure of 40MPa; when the hot pressing furnace is cooled to 200°C, the pressure is released until the sintering is completed; after the equipment is cooled to room temperature, the hot pressing mold and the sample sintered material are taken out, and finally the sample is taken out using a demolding machine.
[0072] It will be easily understood by those skilled in the art that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A diamond-sealed fiber Bragg grating sensing device, comprising a fiber Bragg grating and diamond, It is characterized in that The fiber grating is a fiber grating treated with high temperature annealing, and the metal-plated grating is made by metal plating process; the diamond is a metal-plated diamond made by salt bath method; the metal-plated grating is placed in a designed hot pressing mold, and metal foil and metal mesh inlaid with metal-plated diamond particles are laid layer by layer in the upper and lower directions of the metal-plated grating in the hot pressing mold, and after vacuum hot pressing treatment, the diamonds are evenly distributed in high density in layers above and below the optical fiber.
2. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 1, It is characterized in that The following steps are involved: S1, metal coating on the surface of fiber Bragg grating; S2, coating metal on the surface of diamond particles; S3, placing the metal-plated fiber Bragg grating in the designed hot pressing mold; S4, laying metal foils and metal mesh inlaid with metal-coated diamond particles layer by layer on the grating in the hot pressing mold; S5, putting into vacuum hot pressing furnace for hot pressing forming.
3. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 2, It is characterized in that In step S1, the optical fiber is a PI-coated fiber Bragg grating.
4. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 3, It is characterized in that In step S1, the fiber Bragg grating is a fiber Bragg grating that has been subjected to high temperature annealing treatment.
5. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 4, It is characterized in that In step S1, the fiber Bragg grating metallization process adopts a mixed process of magnetron sputtering and electroplating.
6. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 5, It is characterized in that In step S1, the length of the metal coating of the metal-coated grating is between 3 and 15 cm, and the thickness of the coating is between 300 and 900 μm.
7. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 2, It is characterized in that In steps S1, S2, S3 and S4, the metal and the metal mesh are the same metal.
8. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S2, the diamond mesh size is between 100 and 200.
9. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S2, the diamond needs to be cleaned with hydrochloric acid and acetone before metal plating.
10. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S2, the diamond metallization process adopts a salt bath method.
11. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S2, the thickness of the metal coating on the surface of the metal-coated diamond is between 0.1 and 1 μm.
12. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S3, the hot pressing mold is made of a nickel-chromium alloy resistant to high temperature and high pressure.
13. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S3, optical fiber lead-out protection devices are provided on both sides of the hot pressing mold.
14. The method for manufacturing a diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S3, the hot pressing space and shape in the hot pressing mold are adjustable, and the optical fiber in the internal cavity can be laid to a length of not less than 3 cm.
15. The method for manufacturing the diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S4, the thickness of the metal foil is 0.3-0.7 mm.
16. The method for manufacturing a diamond-sealed fiber Bragg grating sensor device according to claim 7, It is characterized in that In step S4, a metal mesh filled with metal-plated diamond particles is arranged between the metal foils to obtain a diamond-metal-based composite to be sintered; the metal mesh is made of the same metal matrix material as the metal foil, and its mesh specifications are consistent with the diamond powder specifications of the diamond powder layer.
17. The method for manufacturing a diamond-sealed fiber Bragg grating sensor device according to claim 2, It is characterized in that In step S5, the vacuum hot pressing sintering step is: evacuate the hot pressing furnace, heat it to 650~1100°C, keep the hot pressing furnace warm for 40~180min, and then sinter the diamond-metal matrix composite material. After the sintering, the diamond-metal matrix composite material is naturally cooled and then taken out. The pressure of the hot pressing furnace in the hot pressing sintering step is 15~50MPa, and the vacuum degree is 20~100Pa.
Citation Information
Patent Citations
Method for manufacturing Al-Sn alloy-based nickel-plated high-temperature-resistant fiber grating sensor
CN102601344A
Thin fiber and manufacture method thereof
CN103135163A
Optical fiber temperature sensor packaged by diamond casing and resistant to seawater erosion
CN105222921A
Optical and optoelectronic articles
CN1555497A
Method for forming a protective coating on an optical fiber
US20030202763A1