Application of spinel single crystals as ferroelectrics, relaxor ferroelectrics, energy storage materials and rechargeable energy storage products
Through the preparation of spinel type single crystal AB2O4, the toxicity problem of lead-based materials is solved, lead-free ferroelectric and relaxor ferroelectrics are provided for energy storage materials and charging energy storage products, achieving green environmental protection and Excellent dielectric properties.
Patent Information
- Application Number
- CN202111664897.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-31
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-12-31
Smart Images

Figure CN114203443B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of electrochemical materials, and in particular to the application of spinel single crystals as ferroelectrics and relaxor ferroelectrics, energy storage materials and charging energy storage products. Background Art
[0002] With the rapid development of the world economy and the increasing demand for energy, the over-exploitation of non-renewable energy and environmental pollution are becoming increasingly serious. Since 2018, the National Energy Administration has issued and implemented a number of plans and policies on vigorously developing renewable energy, promoting green and low-carbon development, and accelerating the construction of ecological civilization. In particular, with the recent introduction of the concept of "carbon neutrality", a series of new energy sources such as photovoltaics and wind power are gradually becoming practical. Since these renewable energy sources generally have problems such as intermittency, randomness and volatility, in-depth research and development of advanced energy storage equipment and technologies are of great significance.
[0003] At present, commonly used energy storage capacitors can be divided into ferroelectrics, relaxor ferroelectrics, antiferroelectrics, linear dielectrics, etc. according to different dielectrics. Among many dielectrics, relaxor ferroelectrics exhibit both ferroelectricity and relaxority. Due to their many excellent properties, they are widely used in modern electronics, military weapons, medical equipment, aerospace and other fields. Compared with ordinary ferroelectrics, relaxor ferroelectrics have high dielectric constants, low residual polarization, large piezoelectric effects and nonlinear effects. In addition, they also have significant temperature dependence and frequency dependence.
[0004] To date, the research and application of ferroelectrics, including relaxor ferroelectric materials, have mainly focused on lead-based single crystals or ceramics with a perovskite structure. Since the toxicity of lead can cause great harm to the environment and human health, finding new lead-free ferroelectric materials has important practical significance.
[0005] In view of this, the present invention is proposed. Summary of the invention
[0006] The purpose of the present invention is to provide spinel single crystal as ferroelectric, application of relaxor ferroelectric, energy storage material and charging energy storage product.
[0007] The present invention is achieved in that:
[0008] In a first aspect, the present invention provides the application of spinel single crystal AB2O4 as a ferroelectric, wherein A in AB2O4 is Ca, Sr, Ba, Ti, V, Cr, Mn, Fe, Co, Ni, Cu or Zn, and B is a transition metal element or a rare earth element.
[0009] In an alternative embodiment, B is Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb or Lu.
[0010] In a second aspect, the present invention provides the application of spinel single crystal AB2O4 as a relaxor ferroelectric, wherein A is Sr and B is Tb.
[0011] In an optional embodiment, the method for preparing spinel single crystal AB2O4 comprises:
[0012] Synthesizing polycrystalline powder of AB2O4 according to the chemical composition of spinel single crystal AB2O4;
[0013] Pressing polycrystalline powder of AB2O4 into blanks;
[0014] The blank is calcined at 900-1400°C for 12-48h, and then a single crystal is grown using a laser floating zone method.
[0015] In an optional embodiment, the growth of the single crystal by the laser floating zone method is carried out in an inert gas atmosphere, and the oxygen content in the inert gas atmosphere is less than or equal to 20%.
[0016] In an alternative embodiment, the inert gas is argon.
[0017] In an optional embodiment, the pressure is controlled to be 0-10 MPa when growing single crystals by the laser floating zone method.
[0018] In an optional embodiment, the method of pressing the polycrystalline powder of AB2O4 into a blank is: isostatic pressing is used.
[0019] In an optional embodiment, the method of pressing the polycrystalline powder of AB2O4 into a blank is: the polycrystalline powder of AB2O4 is placed in a balloon and pressed into shape by isostatic pressing.
[0020] In a third aspect, the present invention provides an energy storage material, which includes a spinel single crystal AB2O4, wherein A is Ca, Sr, Ba, Ti, V, Cr, Mn, Fe, Co, Ni, Cu or Zn, and B is a transition metal element or a rare earth element;
[0021] In an alternative embodiment, B is Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb or Lu.
[0022] In a fourth aspect, the present invention provides a charging energy storage product, comprising a spinel single crystal AB2O4, wherein A is Ca, Sr, Ba, Ti, V, Cr, Mn, Fe, Co, Ni, Cu or Zn, and B is a transition metal element or a rare earth element;
[0023] In an alternative embodiment, B is Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb or Lu.
[0024] The present invention has the following beneficial effects:
[0025] The spinel single crystals involved in this application have been found to have ferroelectricity at room temperature, and some of them also have relaxor properties, and can be used as relaxor ferroelectrics. These spinel single crystals do not contain lead, are non-toxic, harmless, green and environmentally friendly, and can be used in energy storage materials or rechargeable energy storage products. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0027] Figure 1 The dielectric constant ε and dielectric loss tanδ of the spinel single crystal provided in Example 1 at 0.1kHz, 0.2kHz, 0.5kHz and 1kHz are curves of variation with temperature;
[0028] Figure 2 The test results of the electric field hysteresis loop along the c-axis of the spinel single crystal provided in Example 1 at room temperature;
[0029] Figure 3 The test results of the electric field hysteresis loop along the a-axis of the spinel single crystal provided in Example 1 at different temperatures (1.8K, 260K, 280K, 300K);
[0030] Figure 4 The test results of the electric field hysteresis loop along the b-axis of the spinel single crystal provided in Example 1 at different temperatures (1.8K, 260K, 280K, 300K);
[0031] Figure 5 The dielectric constant ε and dielectric loss tanδ of the spinel single crystal provided in Example 2 at 1kHz, 10kHz and 100kHz vary with temperature;
[0032] Figure 6 The dielectric constant ε and dielectric loss tanδ of the spinel single crystal provided in Example 3 at 1 kHz, 10 kHz and 100 kHz vary with temperature. DETAILED DESCRIPTION
[0033] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the technical scheme in the embodiments of the present invention will be described clearly and completely below. If the specific conditions are not specified in the embodiments, they are carried out according to conventional conditions or conditions recommended by the manufacturer. If the manufacturer of the reagents or instruments used is not specified, they are all conventional products that can be purchased commercially.
[0034] The following is a detailed description of the application of the spinel single crystal provided in the embodiments of the present invention as a relaxor ferroelectric, energy storage material, and chargeable energy storage product.
[0035] The application of spinel single crystal AB2O4 as a relaxor ferroelectric, in which A is Ca, Sr, Ba, Ti, V, Cr, Mn, Fe, Co, Ni, Cu or Zn, and B is a transition metal element or a rare earth element.
[0036] The inventors have discovered that the above-mentioned spinel single crystal exhibits ferroelectricity at room temperature and is a new type of ferroelectric. This new type of ferroelectric does not contain lead, is greener, safer, and more environmentally friendly, and can be used as a new generation of excellent energy storage and fast charging materials.
[0037] The application of spinel single crystal AB2O4 as a relaxor ferroelectric, in which A is Sr and B is Tb.
[0038] The inventors found that the SrTb2O4 in the spinel single crystal has not only ferroelectricity but also relaxor properties. It is a new type of relaxor ferroelectric, which does not contain lead, is greener, safer and more environmentally friendly, and can be used as a new generation of excellent energy storage and fast charging materials, and has broad application prospects in the fields of micropositioners, actuators and sensitive structures.
[0039] Preferably, the B element is Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb or Lu.
[0040] The method for preparing the spinel single crystal comprises:
[0041] S1. Synthesize polycrystalline powder of AB2O4 according to the chemical composition of spinel single crystal AB2O4.
[0042] S2. Press the polycrystalline powder of AB2O4 into a blank.
[0043] Specifically, the polycrystalline powder of AB2O4 is loaded into a balloon and is pressed into a blank of a fixed solid shape by isostatic pressing.
[0044] S3, calcining the blank at 900-1400°C for 12-48h, and then growing single crystals by laser floating zone method in an inert atmosphere with the pressure controlled at 0-10MPa. The laser floating zone method is suitable for growing large single crystals with high melting point and high quality.
[0045] Preferably, the inert gas is argon. The inert atmosphere may contain oxygen, and the oxygen content is less than or equal to 20%.
[0046] The embodiments of the present application provide the application of spinel single crystal AB2O4 as a relaxor ferroelectric in energy storage materials.
[0047] The energy storage material provided in the embodiment of the present application includes spinel single crystal AB2O4, wherein A is Ca, Sr or Ba, and B is a transition metal element or a rare earth element.
[0048] The fast charging product provided in the embodiment of the present application includes spinel single crystal AB2O4, wherein A is Ca, Sr or Ba, and B is a transition metal element or a rare earth element.
[0049] The features and performance of the present invention are further described in detail below in conjunction with the embodiments.
[0050] Example 1
[0051] The polycrystalline powder of SrTb2O4 was synthesized according to the chemical composition of spinel single crystal SrTb2O4.
[0052] The polycrystalline powder of SrTb2O4 is loaded into a balloon and is pressed into a blank with a fixed solid shape by isostatic pressing.
[0053] The blank was calcined at 900°C for 48 hours, and then a single crystal was grown by a laser floating zone method in a mixed atmosphere of argon and oxygen with the pressure controlled within 0-10 MPa.
[0054] Example 2
[0055] The polycrystalline powder of SrHo2O4 was synthesized according to the chemical composition of spinel single crystal SrHo2O4.
[0056] The polycrystalline powder of SrHo2O4 is loaded into a balloon and is pressed into a blank with a fixed solid shape by isostatic pressing.
[0057] The blank was calcined at 1400°C for 12 hours, and then a single crystal was grown by a laser floating zone method in a mixed atmosphere of argon and oxygen with the pressure controlled within 0-10 MPa.
[0058] Example 3
[0059] The polycrystalline powder of SrGd2O4 was synthesized according to the chemical composition of spinel single crystal SrGd2O4.
[0060] The polycrystalline powder of SrGd2O4 is placed in a balloon and is pressed into a blank with a fixed solid shape by isostatic pressing.
[0061] The blank was calcined at 1200°C for 36 hours, and then a single crystal was grown by a laser floating zone method in a mixed atmosphere of argon and oxygen with the pressure controlled within 0-10MPa.
[0062] Experimental Example 1
[0063] Test Example 1 The dielectric constant ε and dielectric loss tanδ of the spinel single crystal at different frequencies vary with temperature, and the variation curve is shown in the following figure: Figure 1 shown.
[0064] pass Figure 1 It can be seen that the dielectric constant has a wide range of extreme values and corresponds to a relatively wide temperature position, and has a frequency dependence, which is different from traditional ferroelectrics that show a sharp Curie temperature point. The dielectric temperature spectrum and loss change with frequency and have obvious dispersion characteristics. In a wider temperature range, it exhibits dielectric relaxation characteristics. In addition, the dielectric test of the single crystal also shows obvious anisotropy. When the temperature reaches 400K, the dielectric constant continues to rise with temperature changes, that is, it exhibits relaxor ferroelectricity when the temperature is below 400K. The huge dielectric constant is also one of the characteristics of relaxor ferroelectrics.
[0065] Test Example 1 Spinel single crystal hysteresis loop at different temperatures, the test results are as follows Figure 2-4 shown.
[0066] pass Figure 2-4 It can be seen that the polarization intensity increases significantly with the increase of temperature, showing excellent pyroelectric performance, which makes it also have certain research and potential application in the field of infrared detection. In addition, the hysteresis loop has strong anisotropy and becomes "thin" at high temperature.
[0067] Based on the above two experiments, it can be seen that the spinel single crystal provided in the embodiment of the present application has ferroelectricity and relaxor properties, and is a new type of lead-free relaxor ferroelectric, which can be used in energy storage materials or fast charging products.
[0068] Example 2
[0069] Test Example 2 The dielectric constant ε and dielectric loss tanδ of the spinel single crystal at different frequencies vary with temperature, and the variation curve is shown in the figure below: Figure 5 shown.
[0070] pass Figure 5It can be seen that the dielectric constant changes with temperature and shows an obvious ferroelectric transition peak at room temperature, indicating that the spinel single crystal provided in the embodiment of the present application has ferroelectricity and is a new type of lead-free ferroelectric, which can be used in energy storage materials or fast charging products.
[0071] Example 3
[0072] Test Example 3 The dielectric constant ε and dielectric loss tanδ of the spinel single crystal at different frequencies vary with temperature, and the variation curve is shown in the figure below: Figure 6 shown.
[0073] pass Figure 6 It can be seen that the dielectric constant changes with temperature and shows an obvious ferroelectric transition peak at room temperature, indicating that the spinel single crystal provided in the embodiment of the present application has ferroelectricity and is a new type of lead-free ferroelectric, which can be used in energy storage materials or fast charging products.
[0074] In summary, the spinel single crystals involved in this application have ferroelectricity at room temperature, and some have relaxor properties, and can be used as relaxor ferroelectrics. Such ferroelectrics do not contain lead, are non-toxic, harmless, and green. The above spinel single crystals can be used as ferroelectrics, including relaxor ferroelectrics, in energy storage materials or rechargeable energy storage products.
[0075] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. Application of spinel single crystal AB2O4 as ferroelectric, wherein A in AB2O4 is Ca, Sr, Ba, Ti, V, Cr, Mn, Fe, Co, Ni, Cu or Zn, and B is a transition metal element or a rare earth element; B is Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb or Lu.
2. Application of spinel single crystal AB2O4 as relaxor ferroelectric, in which A is Sr and B is Tb.
3. The use according to claim 1 or 2, characterized in that: The method for preparing the spinel single crystal AB2O4 comprises: Synthesizing polycrystalline powder of AB2O4 according to the chemical composition of spinel single crystal AB2O4; Pressing the polycrystalline powder of AB2O4 into a blank; The blank is calcined at 900-1400° C. for 12-48 hours, and then a single crystal is grown by a laser floating zone method.
4. The use according to claim 3, characterized in that: The single crystal is grown by a laser floating zone method in an inert gas atmosphere, wherein the oxygen content in the inert gas atmosphere is less than or equal to 20%.
5. The use according to claim 4, characterized in that: The inert gas is argon.
6. The use according to claim 3, characterized in that: When growing single crystals using the laser floating zone method, the pressure is controlled to be 0 to 10 MPa.
7. The use according to claim 3, characterized in that: The method of pressing the polycrystalline powder of AB2O4 into a blank is: isostatic pressing.
8. The use according to claim 7, characterized in that: The method of pressing the polycrystalline powder of AB2O4 into a blank is as follows: the polycrystalline powder of AB2O4 is placed in a balloon and is pressed into shape by isostatic pressing.
9. An energy storage material, characterized in that: Including spinel type single crystal AB2O4, wherein A is Ca, Sr, Ba, Ti, V, Cr, Mn, Fe, Co, Ni, Cu or Zn, and B is a transition metal element or a rare earth element; B is Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb or Lu.
10. A charging energy storage product, characterized in that: Including spinel type single crystal AB2O4, wherein A is Ca, Sr, Ba, Ti, V, Cr, Mn, Fe, Co, Ni, Cu or Zn, and B is a transition metal element or a rare earth element; B is Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb or Lu.
Citation Information
Patent Citations
Ferroelectric thin film
US20110079883A1