One-piece large-wall vacuum cylinder extrusion die
By introducing designs such as protective molds, through holes, bullet-proof variable gaps, flow-blocking bosses, and trapezoidal pockets into the vacuum cylinder extrusion mold, the problems of poor weld quality and short mold life caused by large wall thicknesses were solved, and the problem was achieved Higher weld quality and longer mold life.
Patent Information
- Application Number
- CN202111490468.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-08
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-12-08
AI Technical Summary
Due to the large wall thickness of the existing integrated vacuum cylinder extrusion mold, it results in poor weld quality, short mold life, difficult processing, long cutting head and tail, and the large depth of the welding chamber results in high pressure and rough product surface.
An integrated large-walled vacuum cylinder extrusion mold including a protective mold, through holes, bulletproof variable gaps, flow-blocking bosses and trapezoidal pockets was designed. Through these designs, the risk of fracture of the upper mold is reduced and the welding quality is improved. Reduce head and tail cutting and enhance extrusion efficiency.
It extends the service life of the mold, improves the welding quality, reduces head and tail cuts, reduces the processing difficulty, improves the product yield, and significantly improves the product speed and welding quality in vacuum cylinder casting.
Smart Images

Figure CN114425571B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of extrusion dies, in particular to an integrated large-wall-thickness vacuum cylinder extrusion die. Background Art
[0002] The current one-piece vacuum cylinder has a thick wall (weld position ≥50mm) and a high specific gravity, resulting in a small extrusion ratio (ø580 extrusion cylinder extrusion ratio <10). When produced by a 110MN / ø580mm extruder, bubbles and holes often appear in the weld. In order to ensure the quality of the weld, the welding chamber must be made long and high enough, resulting in a long head and tail.
[0003] The current mold design requires that the upper mold be made very thick to ensure the strength of the mold and enhance the stability of the mold to prevent the diverter bridge from breaking during the extrusion process. In addition, in areas with thick walls, the lower mold needs to use a baffle to block the aluminum flow and at the same time extend the length of the working belt to achieve balanced aluminum flow.
[0004] The thickness of the upper mold of the existing mold is large, which makes processing and heat treatment more difficult and the cost of later mold repair is high. The large and deep welding chamber leads to high mold pressure, short mold life, and long product head and tail. In the location with thick wall, the lower mold is designed with a stopper and an extended working belt, which leads to high mold pressure and rough product surface.
[0005] In view of the above shortcomings, it is very necessary to study the improvement plan of mold design to extend the service life of the mold, reduce the difficulty of mold processing, improve the welding quality, avoid the appearance of pores, shorten the cutting head and tail, enhance the extrusion efficiency, and improve the product yield. Summary of the invention
[0006] The present invention provides an integrated large-wall-thickness vacuum cylinder extrusion die, which can extend the service life of the die, especially the upper die, improve the welding quality, avoid the occurrence of pores, shorten the cutting head and tail, reduce the processing difficulty of the die, and improve the product yield.
[0007] To achieve the above object, the technical solution of the present invention is:
[0008] An integrated large-walled vacuum cylinder extrusion die comprises an upper die and a lower die, and is further provided with a protective die, the protective die being attached to a side of the upper die away from the lower die and provided with a second diversion hole matching the position and shape of the first diversion hole of the upper die. The invention adds a protective die, and when subjected to an external extrusion force, the protective die protects the upper die, and the possibility of the diversion bridge of the upper die breaking is greatly reduced.
[0009] Furthermore, a through hole is provided at the core of the upper die. The addition of the through hole enables hot air to flow through the through hole during heat treatment of the upper die, resulting in more uniform heating, increased hardenability of the steel, and reduced possibility of mold cracking and scrapping.
[0010] Furthermore, an anti-bullet-change gap is provided between the protective mold and the upper mold. Furthermore, the anti-bullet-change gap is provided at the mold core of the protective mold, and the mold core of the protective mold facing the upper mold is recessed inward. Furthermore, the depth of the anti-bullet-change gap is 3.5-5 mm. By increasing the anti-bullet-change gap, the impact of the protective mold on the upper mold can be reduced, leaving a force-bearing space, and reducing the possibility of the upper mold breaking.
[0011] Furthermore, the first diverter holes at four diagonals are provided with flow blocking bosses at one end of the mold core, i.e., at the location of the maximum wall thickness. By providing the flow blocking bosses at the location of the thickest wall, the aluminum flow velocity can be reduced, the aluminum flow at the welding location can be increased, and the welding quality can be improved.
[0012] Furthermore, the top and tip of the diverter bridge on the discharge surface of the upper mold are transitioned into an inwardly concave rounded corner. This design can enhance the support strength of the diverter bridge, reduce the possibility of the diverter bridge breaking, and thus increase the stability and life of the mold.
[0013] Furthermore, the four corners of the working belt of the lower die are provided with trapezoidal pockets, and the edges of the trapezoidal pockets gradually transition from the side close to the matching stop to the side away from the matching stop along the discharge direction. This arrangement can increase the size of the corners for aluminum supply and prevent the local temperature of the four corners from being too high, greatly reducing the possibility of cracking on the surface of the vacuum cylinder body and further increasing the speed of extruding products.
[0014] Furthermore, a blocking angle is provided at the position where the welding chamber of the lower die transitions to the working zone, and the blocking angle is 3° to 6°. The blocking angle can reduce the flow velocity of the straight aluminum flow, so that the aluminum flow can be diverted to the welding position, thereby ensuring the welding quality, and at the same time reducing the depth of the welding chamber and reducing the head and tail cutting.
[0015] Furthermore, the four diagonal lengths of the working belt are shortened to 3-5 mm, and an oblique transition is adopted in the discharge direction. Shortening the working belt can reduce the extrusion pressure at the working belt position, thereby reducing the possibility of cracking of the working belt, while ensuring the surface quality of the vacuum cylinder body.
[0016] The above-mentioned integrated large-walled vacuum cylinder extrusion die can extend the service life of the die, especially the upper die, ensure the stability of the die, reduce the difficulty of die processing, reduce the pressure of the die extrusion process, improve the welding quality, shorten the cutting head and tail, enhance the extrusion efficiency, and improve the product yield.
[0017] The above mold is used in the casting of vacuum cylinder body, which has the following effects: (1) The product speed is increased from 0.6m / min to 1.0m / min, which is 54.5% higher. (2) The cutting head and tail are reduced from 5.5m to 2.5m, which is 33.3% shorter. (3) The welding quality is good, without holes, slag inclusions, etc. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a three-dimensional structural schematic diagram of the present invention.
[0019] Figure 2 It is a main structural schematic diagram of the present invention.
[0020] Figure 3 It is a schematic diagram of the three-dimensional structure of the protection mold.
[0021] Figure 4 It is a schematic diagram of the main structure of the upper mold.
[0022] Figure 5 It is a schematic diagram of the three-dimensional structure of the upper mold.
[0023] Figure 6 This is a schematic diagram of the three-dimensional structure of the upper mold from another angle.
[0024] Figure 7 It is a schematic diagram of the main structure of the lower mold.
[0025] Figure 8 It is a schematic diagram of the three-dimensional structure of the lower mold.
[0026] In the figure, the protective mold 1, the second diverter hole 101, the bulletproof variable gap 102, the upper mold 2, the first diverter hole 201, the diverter bridge 202, the through hole 203, the flow blocking boss 204, the diverter bridge top 205, the lower mold 3, the welding chamber 301, the trapezoidal pocket 302, and the position 303 where the welding chamber transitions to the working belt. DETAILED DESCRIPTION
[0027] The present invention is further described below in conjunction with specific embodiments and drawings, but the protection scope of the present invention is not limited to the following embodiments.
[0028] In the description of the present invention, it should be noted that the terms "upper" and "lower" etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, or are directions or positional relationships in which the product of the invention is usually placed when in use. These are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, they should not be understood as limitations on the present invention.
[0029] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0030] The foregoing description of specific exemplary embodiments of the present invention is for the purpose of illustration and demonstration. These descriptions are not intended to limit the present invention to the precise form disclosed, and it is clear that many changes and variations can be made based on the above teachings. The purpose of selecting and describing the exemplary embodiments is to explain the specific principles of the present invention and its practical application, so that those skilled in the art can realize and utilize various different exemplary embodiments of the present invention and various different selections and changes. The scope of the present invention is intended to be limited by the claims and their equivalents.
[0031] An integrated large-wall vacuum cylinder extrusion die, such as Figure 1 and 2As shown, it includes an upper mold 2 and a lower mold 3, and is also provided with a protective mold 1. The protective mold 1 is attached to the side of the upper mold 2 away from the lower mold 3, and is provided with a second diversion hole 101 that matches the position and shape of the first diversion hole 201 of the upper mold 2. The shape and size of the protective mold 1 are basically similar to those of the traditional upper mold, but the thickness is generally set to 140~160mm. The protective mold 1 is combined with the upper mold 2 in the form adopted in this embodiment: the protective mold 1 is the same as the traditional upper mold 2, and a protective mold concave part that is concave inward is provided on the side attached to the upper mold 2, and a protruding part of the upper mold that is protruding outward is provided on the side attached to the protective mold. The protective mold concave part can be matched and sleeved on the periphery of the protruding part of the upper mold so that they are combined together when used. The protective mold concave part is generally cylindrical or truncated cone-shaped. If it is truncated cone-shaped, the small end faces outward and the large end faces inward. Of course, the protective mold 1, the upper mold 2 and the lower mold 3 are also better fixed together by bolts. The traditional extrusion die only includes an upper die and a lower die. During extrusion, the shunt bridge of the upper die is prone to breakage due to the influence of the extrusion external force. In order to ensure the strength of the die, the upper die needs to be made very thick to ensure the stability of the die and prevent the shunt bridge from breaking during the extrusion process. However, this method increases the difficulty of processing and heat treatment due to the large thickness of the upper die, and the cost of later die repair or replacement is high. The present invention adds a protective die 1. When subjected to the extrusion external force, the protective die 1 protects the upper die 2, and the possibility of the shunt bridge 202 of the upper die 2 breaking is greatly reduced. If the shunt bridge of the protective die 1 breaks, the protective die 1 can be replaced. The thickness of the protective die is small, and the replacement cost is low. In addition, since the upper die 2 is not damaged, it will not affect the quality of the finished product during the extrusion process.
[0032] Furthermore, a through hole 203 is provided at the core of the upper mold 2. The addition of the through hole 203 allows hot air to flow through the through hole 203 when the upper mold 2 is heat treated before the extrusion process, so that the heating is more uniform, the hardenability of the steel is increased, and the possibility of cracking and scrapping of the mold is reduced.
[0033] Furthermore, an anti-bullet-change gap 102 is provided between the protective mold 1 and the upper mold 2. By increasing the anti-bullet-change gap, the impact of the protective mold 1 on the upper mold 2 can be reduced, leaving a force-bearing space, and reducing the possibility of the upper mold 2 breaking. Furthermore, this embodiment provides a preferred setting method of the anti-bullet-change gap 102. The anti-bullet-change gap 102 is provided at the core of the protective mold 1. The core of the protective mold 1 facing the upper mold 2 is recessed inward. Here, inward refers to the direction away from the upper mold 2. Since the impact force at the core is greater, it is more appropriate to set it at the core. Furthermore, the maximum depth of the anti-bullet-change gap is 3.5~5mm. It is at the center of the protective mold 1 and then transitions to the surrounding in a sloped manner. This depth can ensure the support strength for the upper mold 2 and prevent excessive impact force on the upper mold 2.
[0034] Further, combined with Figures 3-5 As shown, the upper mold 2 is generally provided with 8 first diverter holes 201, which surround the mold core and are respectively located at the top, bottom, left, right and four diagonal corners of the mold core. The first diverter holes 201 located at the four diagonal corners are provided with a flow blocking boss at one end facing the mold core. The first diverter holes located at the four diagonal corners have a thicker wall at one end facing the mold core. The aluminum flow velocity here is large, which can easily cause uneven distribution of aluminum liquid. A flow blocking boss 204 is specially provided to reduce the aluminum flow velocity, increase the aluminum flow at the welding position, and improve the welding quality. The flow blocking boss 204 generally adopts a slope structure, and the slope of the inlet is gentle, and the slope of the outlet is steep. The slope of the inlet is gentle, so that the aluminum flow slowly climbs when entering, which can better slow down the flow velocity of the aluminum flow.
[0035] Furthermore, the top 205 of the diverter bridge on the discharge surface of the upper mold 2 and the bridge tip are inwardly concave with a rounded transition, and the depth of the concave is generally 8~25mm. The inward concave here refers to the concave toward the side away from the lower mold 3. Among them, the bridge tip refers to the end of the diverter bridge 202 connected to the mold core. Increasing the transition radius of the top 205 and the bridge tip, the fillet R ≥ 45mm, and forming an arc transition with the bottom fillet of the bridge can enhance the support strength of the diverter bridge 202, reduce the possibility of the diverter bridge 202 breaking, and ensure that the product is well welded, thereby increasing the stability and life of the mold. The top and bridge tip positions of the diverter bridge of the traditional upper mold 2 are usually linear connection structures. If the thickness of the diverter bridge 202 is directly increased to enhance the support strength of the diverter bridge 202, it will cause pores to easily appear at the welding position, affecting the quality of the vacuum cylinder body. By setting a rounded transition method to increase the support strength of the diverter bridge 202, there will be no pore problem, which effectively ensures the quality of the vacuum cylinder body.
[0036] Furthermore, trapezoidal pockets 302 are provided at the four corners of the working belt of the lower mold 3. The trapezoidal pockets 302 are concave downward, and the edges of the trapezoidal pockets 302 gradually transition at an angle from the side close to the matching stop to the side away from the matching stop along the discharge direction. The matching stop mentioned here refers to the protruding part of the lower mold, which can match the position where the upper mold 2 and the lower mold 3 are combined together by inserting the recessed part of the upper mold. The traditional square diagonal shape will cause the aluminum liquid to flow poorly, which will cause the local temperature to be too high, making the surface of the vacuum cylinder body easy to crack. The setting of the trapezoidal pocket 302 is large at the outer end and small at the inner end close to the center, and it is transitioned at an angle, which can better guide the aluminum liquid to flow out, so that the temperature of the four corners of the welding chamber 301 is similar to that of other parts, greatly reducing the possibility of cracking of the vacuum cylinder body, while ensuring the size of the corners.
[0037] Further, combined with Figure 7 and 8As shown, the position 303 where the welding chamber of the lower die 3 transitions to the working belt is provided with an obstruction angle, which is 3° to 6°, and is the angle between the lower die 3 and the vertical plane when the lower die 3 is placed horizontally (i.e., when the working belt is vertical). The obstruction angle 303 can reduce the flow velocity of the aluminum flow in the straight punching part, further divert it to the welding position, ensure the welding quality, and reduce the depth of the welding chamber and the cutting head and tail at the same time.
[0038] Furthermore, the lengths of the four diagonal working belts are shortened, and the discharging direction is transitioned at an angle, and the shortened area is shortened to 3-5 mm at most. The general length of the working belt is 30-40% of 35 mm, and the design of this embodiment shortens the four diagonal working belts. Figure 8 As shown, the oblique angle transition refers to a gradual slowdown rather than a right-angle transition, which is similar to a parabolic transition method, reducing the extrusion pressure at the working belt position, thereby reducing the possibility of cracking of the working belt, while ensuring the surface quality and size of the vacuum cylinder body.
Claims
1. An integrated large-wall vacuum cylinder extrusion die, comprising an upper die and a lower die, characterized in that: A protection mold is also provided, which is attached to a side of the upper mold away from the lower mold and is provided with a second diversion hole that matches the position and shape of the first diversion hole of the upper mold; A through hole is provided at the mold core of the upper mold; An anti-bullet gap is provided between the protection die and the upper die; The first diverter holes at four diagonal positions are provided with flow blocking bosses at one end facing the mold core; The four corners of the working belt of the lower die are provided with trapezoidal pockets, and the edges of the trapezoidal pockets gradually transition at an oblique angle from the side close to the matching stop to the side away from the matching stop along the discharge direction.
2. The one-piece large-wall-thickness vacuum cylinder extrusion die according to claim 1 is characterized in that: The anti-bullet variable gap is arranged on the mold core of the protection mold, and the mold core of the protection mold facing the upper mold is concave inwards.
3. The one-piece large-walled vacuum cylinder extrusion die according to claim 1 is characterized in that: The top and tip of the diverter bridge on one side of the discharge surface of the upper die are in an inwardly concave rounded transition.
4. The one-piece large-walled vacuum cylinder extrusion die according to claim 1 is characterized in that: A blocking angle is provided at the position where the welding chamber of the lower die transitions to the working zone, and the blocking angle is 3° to 6°.
5. The one-piece large-walled vacuum cylinder extrusion die according to claim 1 is characterized in that: The four diagonal lengths of the working belt are shortened to 3-5 mm, and an oblique angle transition is adopted in the discharge direction.
6. The one-piece large-walled vacuum cylinder extrusion die according to claim 1 or 2, characterized in that: The depth of the bulletproof variable gap is 3.5-5 mm.
Citation Information
Patent Citations
Huge thin-wall cylindrical aluminum profile extrusion mould and profile processing method
CN107755450A
Aluminum alloy large round tube die
CN107838217A
Die for producing section bar with large width and thick wall thickness
CN210614681U