A composite bipolar plate for flow battery and a method for preparing the same

CN114497614BActive Publication Date: 2024-11-08SUQIAN TIMES ENERGY STORAGE TECH CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202111663586.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-31
Publication Date
2024-11-08
Estimated Expiration
2041-12-31

AI Technical Summary

Technical Problem

The existing flow battery bipolar plates are prone to leakage at the connection, resulting in liquid leakage, and are difficult to weld, limiting the battery life and packaging cost.

Method used

A composite bipolar plate consisting of conductive areas, insulating areas and transition areas is made of conductive materials and resin. The insulating areas are made of non-conductive polymer materials. The transition area is the conductive areas and insulating areas. The composite forms a low-resistance, high-sealing bipolar plate through a pressing process.

Benefits of technology

It realizes good conductivity, corrosion resistance and easy welding of the flow battery, avoids liquid leakage, improves the battery life and reduces the packaging cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114497614B_ABST
    Figure CN114497614B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for preparing a composite bipolar plate for a liquid flow battery. The bipolar plate has a conductive area, an insulating area and a transition area, so that the bipolar plate has good conductivity, corrosion resistance and easy welding, and solves the technical problem that the composite bipolar plate is difficult to be sealed and connected with materials such as diaphragms, electrode materials and frames. The occurrence of liquid leakage in the liquid flow battery can be effectively avoided, the battery service life is increased, the risk of leakage is reduced, and the battery packaging cost is reduced, which has great commercial value.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of preparation of bipolar plates for liquid flow batteries, and in particular relates to a highly sealed and easily welded composite bipolar plate for liquid flow batteries and a preparation method thereof. Background Art

[0002] The bipolar plates included in the liquid flow battery structure have the function of connecting the positive and negative electrodes of the single cell, and also play the role of separating the positive and negative liquids of the battery. At the same time, the electrode reactants can be evenly distributed to various parts of the electrode through the bipolar plates by setting flow channels and drainage fields. The bipolar plates must be good conductors with low resistance, because higher resistance tends to consume more electricity and generate heat at the same time. In order to effectively isolate the positive and negative electrode reaction liquids and place the positive and negative electrodes short-circuited, the bipolar plates must have sufficient barrier properties and airtightness, and no leakage to gaseous and liquid substances. Liquid flow batteries often have a long life, and the electrolyte of liquid flow batteries is often strongly acidic or alkaline, so the bipolar plates are required to have high mechanical strength, aging resistance and chemical corrosion resistance.

[0003] The bipolar plates currently used in the field of liquid flow batteries are mainly graphite-based bipolar plates and flexible graphite bipolar plates. Both have advantages such as good conductivity, low contact resistance, good stability, and corrosion resistance, but also have disadvantages such as poor mechanical properties, poor air tightness, and difficulty in welding. Therefore, leakage of liquid flow batteries often occurs at the connection between the bipolar plate and other materials, and leakage is a major obstacle to the development of liquid flow batteries. Summary of the invention

[0004] In order to solve the above problems, the present invention discloses a composite bipolar plate for a flow battery having good conductivity, corrosion resistance, easy weldability and high airtightness and a preparation method thereof.

[0005] To achieve the above object, the technical solution of the present invention is as follows:

[0006] One object of the present invention is to provide a composite bipolar plate for a liquid flow battery, wherein the middle of the composite bipolar plate is a conductive area, the edge of the composite bipolar plate is an insulating area, and a transition area is between the conductive area and the insulating area. The transition area connects the conductive area and the insulating area. The composite bipolar plate is formed by pressing the transition area on the outer ring of the pressed conductive area and pressing the insulating area on the outer ring of the transition area.

[0007] Furthermore, the thickness of the composite bipolar plate is 0.1-5 mm.

[0008] Furthermore, the material of the transition zone is a composite of the material of the conductive zone and the material of the insulating zone.

[0009] Furthermore, the material of the conductive area is mainly prepared by a composite of a conductive material and a resin; the conductive material is one or more of artificial graphite, graphene, carbon fiber, carbon nanotubes, and conductive plastic particles; the resin is one or more of PE, PP, PVDF, PTFE, PA, PS, ABS, ASA, PC, PMMA, POM, PES, PEEK, and PBT.

[0010] Furthermore, the material of the insulating area is mainly made of non-conductive polymer material, and the non-conductive polymer material is one or more of PE, PP, PVDF, PTFE, PA, PS, ABS, ASA, PC, PMMA, POM, PES, PEEK, and PBT.

[0011] Another object of the present invention is to provide a method for preparing a composite bipolar plate for a flow battery, comprising the following steps:

[0012] (1) Add the resin and the conductive material to the diluent, stir and mix them evenly, remove the diluent, apply pressure and press repeatedly, and cut the outer frame to obtain the conductive area;

[0013] (2) Mixing resin, conductive material and non-conductive polymer material uniformly to obtain a mixture, and evenly spreading the mixture on the outer circle of the conductive area, first at room temperature and then at elevated temperature, applying pressure and repeatedly pressing until forming, and cutting the outer frame to obtain a semi-finished bipolar plate containing a conductive area and a transition area;

[0014] (3) The non-conductive polymer material is evenly dispersed on the outer ring of the semi-finished bipolar plate, pressure is applied and pressed repeatedly, and the burrs are trimmed to obtain a composite bipolar plate.

[0015] Before applying pressure and pressing in step (1), the step also includes spraying graphene, which can effectively improve the conductivity of the product and enhance the surface smoothness of the product.

[0016] When applying pressure to press, cold pressing or hot pressing can be performed, and those skilled in the art can adjust it according to the physical properties of the resin, the conductive material and the non-conductive polymer material.

[0017] Furthermore, in step (1), the weight ratio of the total weight of the resin and the conductive material to the diluent is 1:2-1:100; and the applied pressure is 0.5-50 MPa.

[0018] Furthermore, the diluent is one or more of water, ethanol, methanol, ethylene glycol, ethyl ether, butylene glycol, isopropanol, n-butanol, acetonitrile, ethyl acetate, benzene, and toluene.

[0019] Furthermore, in step (2), the mass ratio of the resin to the conductive material to the non-conductive polymer material is 1:1:1-1:10:20, and the applied pressure is 0.5-50 MPa.

[0020] Furthermore, in step (3), the applied pressure is 0.5-50 MPa.

[0021] The beneficial effects of the present invention are:

[0022] The present invention discloses a composite bipolar plate for a liquid flow battery. The bipolar plate has a conductive area, an insulating area and a transition area. The conductive area is used for conducting, isolating and draining. The insulating area is used for welding with other polymer materials to ensure the airtightness of the battery. The material of the transition area is composited by the conductive area material and the insulating area resin. The material of this area takes into account the characteristics of the conductive area and the insulating area materials. After processing, it can be connected with the conductive area material and the insulating area material. The transition area plays the role of bridging the conductive area and the insulating area. The existence of the three areas makes the bipolar plate have good conductivity, corrosion resistance and easy welding, solves the technical problem that the composite bipolar plate is difficult to seal and connect with the diaphragm, electrode material, frame and other materials, can effectively avoid the occurrence of liquid flow battery leakage, improve the battery life, reduce the risk of leakage, reduce the battery packaging cost, and has great commercial value.

[0023] The bipolar plate of the present invention has a low-resistance, non-penetrable high-conductivity area, which can effectively ensure the conductivity of the battery pack; the bipolar plate has a pure resin area, which is convenient for welding with modules such as membranes, electrode materials, and frames, and can effectively avoid the occurrence of gas leakage and liquid leakage in fuel cells, liquid flow batteries, etc., thereby increasing the battery life and reducing the battery packaging cost.

[0024] The invention discloses a method for preparing a composite bipolar plate for a liquid flow battery, which has a simple process flow, low cost and is suitable for large-scale production. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a schematic diagram of the structure of the composite bipolar plate of the present invention;

[0026] List of Figure Symbols:

[0027] 1. Conductive zone; 2. Transition zone; 3. Insulation zone. DETAILED DESCRIPTION

[0028] The present invention will be further explained below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the following specific embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention.

[0029] Example 1

[0030] Dilute 300g of phenolic resin with 10kg of ethanol, add 700g of expanded graphite, stir and mix thoroughly, and place the resulting slurry mixture evenly in the pressing tank. Under a vacuum of 120Pa, remove the ethanol diluent, and press repeatedly at room temperature under a pressure of 0.5Mpa. After heating to 155℃, press again repeatedly under a pressure of 0.5Mpa. The conductive plate is initially formed and the outer frame is cut. 30g of phenolic resin, 70g of expanded graphite, and 100g of polyethylene powder are fully mixed and evenly sprinkled on the outer ring of the conductive plate, placed in a press, and repeatedly pressed at 155℃ and 2Mpa pressure to form, trim the outer frame, and obtain a semi-finished bipolar plate. 100g of polyethylene powder is evenly dispersed on the outer edge of the semi-finished bipolar plate, and repeatedly pressed at 165℃ and 10Mpa pressure, and the burrs are trimmed to obtain a finished plate. After testing, the thickness of the bipolar plate is 0.5mm, the conductive area of ​​the bipolar plate is black, and the resistance is 0.02Ω / cm 2 The outer frame of the bipolar plate is white, insulated and non-conductive.

[0031] Example 2

[0032] Mix 100g PVDF with 400g expanded graphite, add 1100g ethanol and continue to stir and mix evenly to obtain a slightly wet paste solid, evenly distribute it in the pressure tank, spray 20g graphene evenly on its surface, gradually heat it to 200℃ and dry it for 20min. Repeatedly press the conductive plate at 200℃ and 50Mpa pressure to make the conductive plate initially formed, and cut the outer frame. Mix 20g PVDF resin, 80g expanded graphite, and 100g PP powder evenly, sprinkle them evenly on the outer circle of the conductive plate, put them into the press and repeatedly press them at 180℃ and 50Mpa pressure, trim the outer frame, and get the semi-finished bipolar plate. Disperse 100g PP powder evenly on the outer edge of the semi-finished bipolar plate, press it repeatedly at 180℃ and high pressure 50Mpa, trim the burrs, and get the finished plate. After testing, the thickness of the bipolar plate is 0.38mm, the conductive area of ​​the bipolar plate is black, and the resistance is 0.008Ω / cm 2 The outer frame of the bipolar plate is milky white and insulated and non-conductive.

[0033] Example 3

[0034] Spread the carbon fiber cloth evenly, mix 150g PE powder and 400g graphite powder thoroughly, evenly disperse them on both sides of the carbon fiber cloth, flatten it gently, spray 600g benzene on the surface of the sample to soak the liquid, flatten it again, let it stand for 1 hour, gradually heat it to 90℃, and capture the gas with a slight negative pressure. Press the conductive plate repeatedly at 90℃ and 50Mpa pressure, and capture the gas with a slight negative pressure during the process. Cut the outer frame of the rough conductive plate. Mix 120g PE resin and 80g graphite powder thoroughly, sprinkle them evenly on the outer circle of the conductive plate, put them into the press and press them repeatedly at 80℃ and 50Mpa pressure to form them. During the process, the gas is captured with a slight negative pressure, and the outer frame is trimmed to obtain a semi-finished bipolar plate. Disperse 100g PE powder evenly on the outer edge of the semi-finished bipolar plate, press it repeatedly at 80℃ and high pressure 50Mpa, trim the burrs, and obtain the finished plate. After testing, the thickness of the bipolar plate is 0.4mm, the conductive area of ​​the bipolar plate is black, and the resistance is 0.022Ω / cm 2 The outer frame of the bipolar plate is milky white and insulated and non-conductive.

[0035] Performance Testing

[0036] Cut a white PP plate frame with a thickness of mm, and weld it tightly with the outer frame of the bipolar plate obtained in Example 2 using a carbon dioxide laser (40W) at a welding speed of 0.8m / min. After repeated tapping, the bipolar plate and the PP plate frame are tightly connected. A tensile test was carried out on a universal tensile testing machine, and the maximum tensile force of the weld was measured to be 343N.

[0037] It should be noted that the above content only illustrates the technical idea of ​​the present invention and cannot be used to limit the protection scope of the present invention. For ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications all fall within the protection scope of the claims of the present invention.

Claims

1. A composite bipolar plate for a flow battery, characterized in that: The middle of the composite bipolar plate is a conductive area, the edge of the composite bipolar plate is an insulating area, and the conductive area and the insulating area are connected by a transition area. The composite bipolar plate is formed by pressing the transition area on the outer ring of the pressed conductive area, and pressing the insulating area on the outer ring of the transition area. The material of the transition zone is a composite of the material of the conductive zone and the material of the insulating zone; the material of the insulating zone is mainly made of a non-conductive polymer material; the material of the conductive zone is mainly made of a composite of a conductive material and a resin; The preparation steps of the conductive area are: adding resin and conductive material into a diluent, stirring and mixing evenly, removing the diluent, applying pressure and repeatedly pressing, and cutting the outer frame to obtain the conductive area; In the transition zone, the mass ratio of the resin to the conductive material to the non-conductive polymer material is 1:1:1-1:10:20; In the conductive area, the weight ratio of the total weight of the resin and the conductive material to the diluent is 1:2-1:

100.

2. A composite bipolar plate for a flow battery according to claim 1, characterized in that: The thickness of the composite bipolar plate is 0.1-5 mm.

3. A composite bipolar plate for a flow battery according to claim 1, characterized in that: The conductive material is one or more of artificial graphite, graphene, carbon fiber, carbon nanotubes, and conductive plastic particles; the resin is one or more of PE, PP, PVDF, PTFE, PA, PS, ABS, ASA, PC, PMMA, POM, PES, PEEK, and PBT.

4. A composite bipolar plate for a flow battery according to claim 1, characterized in that: The non-conductive polymer material is one or more of PE, PP, PVDF, PTFE, PA, PS, ABS, ASA, PC, PMMA, POM, PES, PEEK, and PBT.

5. A method for preparing a composite bipolar plate for a flow battery according to any one of claims 1 to 4, characterized in that: The following steps are involved: (1) Adding resin and conductive material to a diluent, stirring and mixing them evenly, removing the diluent, applying pressure and repeatedly pressing, and cutting the outer frame to obtain a conductive area; (2) Mixing resin, conductive material and non-conductive polymer material evenly to obtain a mixture, evenly spreading the mixture on the outer ring of the conductive area, applying pressure and repeatedly pressing until it is formed, and cutting the outer frame to obtain a bipolar plate semi-finished product containing a conductive area and a transition area; (3) Evenly dispersing the non-conductive polymer material on the outer ring of the bipolar plate semi-finished product, applying pressure and repeatedly pressing, and trimming the burrs to obtain a composite bipolar plate; In step (1), the weight ratio of the total weight of the resin and the conductive material to the diluent is 1:2-1:100; In step (2), the mass ratio of the resin to the conductive material to the non-conductive polymer material is 1:1:1-1:10:

20.

6. The method for preparing a composite bipolar plate for a flow battery according to claim 5, characterized in that: The diluent is one or more of water, ethanol, methanol, ethylene glycol, ethyl ether, butylene glycol, isopropanol, n-butanol, acetonitrile, ethyl acetate, benzene and toluene.

Citation Information

Patent Citations

  • Flexibility enhanced bipolar plate for liquid energy-storing battery and manufacture thereof

    CN101308924A

  • Low electrical resistance bipolar plate-diffusion media assembly

    CN101335357A

  • A method for prepare a metal graphite composite bipolar plate of a proton exchange membrane fuel cell

    CN108963294A

  • Flow battery unit forming process

    CN112264708A

  • Composite graphite material for bipolar plate of fuel cell and preparation method of composite graphite material

    CN113555578A