Rotating electric machine with adhesive-reinforced rotor
By using non-magnetic reinforcement blocks and a polymer primer/adhesive layer in the rotor openings of the rotating electrical machine to bond the reinforcement blocks to the rotor laminations, the problem of stress concentration during high-speed operation is solved and the efficiency and performance of the motor are improved. .
Patent Information
- Application Number
- CN202110515861.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-10-29
- Filing Date
- 2021-05-12
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2041-05-12
AI Technical Summary
In rotating electrical machines, the concentration of mechanical stress in the rotor laminations during high-speed operation leads to deterioration. Existing methods strengthen the rotor by adding electrical steel, but this will reduce the operating efficiency and torque/speed performance of the motor.
Use non-magnetic, non-metallic, non-conductive reinforcement blocks (such as ceramic blocks or reinforced polymer materials) to fill the rotor openings and bond the reinforcement blocks to the rotor laminations through a polymer primer/adhesive layer to reduce flux leakage and provide mechanical support to improve the operating efficiency and performance of the motor.
It effectively reduces the stress concentration around the rotor laminations, improves the operating efficiency and performance of the motor, enhances mechanical support, and can operate at higher angular speeds while maintaining high tensile strength and elastic modulus.
Smart Images

Figure CN114513075B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a rotating electric machine having an adhesive reinforced rotor. Background Art
[0002] Rotating electric machines of the type used in electric drive systems operate in either a motoring or torque generating mode, in which output torque is transferred to a coupled load, such as one or more wheels of a motor vehicle, or a power generating mode, in which the machine is rotated for the purpose of generating electricity. In a typical configuration, the electric machine includes a cylindrical rotor formed from a stack of thin magnetic rotor lamination layers or "laminations." The magnetic material of the rotor laminations is typically an alloy of iron and silicon, commonly referred to in the art as electrical steel. In operation, the rotor and integrally connected rotor shaft rotate simultaneously when the excitation windings of the accompanying stator are sequentially energized by a high voltage power source, which typically includes a multi-cell high voltage traction battery pack and a power inverter.
[0003] As motor speeds increase, the power density of the motor also increases. However, higher speed rotation increases mechanical stresses on the crystal structure of the rotor laminations, with stress concentrations more prevalent near gaps, web areas, and other rotor openings in the rotor laminations. Therefore, to prevent stress-related degradation of the rotor laminations, manufacturers may attempt to strengthen or reinforce the rotor laminations with additional electrical steel. However, the added material can reduce the operating efficiency and overall torque / speed performance of the motor. Summary of the invention
[0004] Disclosed herein are rotary electric machines and adhesive-reinforced rotors for use therein, as well as related methods for manufacturing or assembling such rotors. Rotor stress concentrations around rotor openings defined by stacking of rotor lamination layers ("rotor laminations") are limiting factors in high-speed operating modes. It is recognized herein that certain types of adhesive reinforcement structures are capable of operating at higher angular speeds relative to electrical steel and other types of magnetic core materials used to construct individual rotor laminations. Therefore, the disclosed construction bonds reinforcement blocks to the rotor laminations around the inner periphery of at least some of the rotor openings to substantially fill the rotor openings. The construction has the desired effect of reducing the above-mentioned stress concentrations in the surrounding areas of the rotor laminations. In addition, the presence of the reinforcement blocks helps to reduce or eliminate thin magnetic bridges of the rotor laminations in the web region of the rotor laminations / rotor stack, thereby improving the operating efficiency and performance of the motor, for example, by reducing undesirable flux leakage / magnetic short circuits, while providing useful mechanical support.
[0005] More specifically, the present invention achieves structural and magnetic performance advantages by filling the defined voids of at least some rotor openings with non-magnetic, non-metallic, non-conductive reinforcement blocks (e.g., ceramic blocks or reinforced polymer material blocks). The reinforced polymer material can be formed and cured to construct the above-mentioned reinforcement blocks, and in different embodiments, such structures appear either inside the rotor laminations or separately from the rotor laminations. The present method also includes a thin layer of polymer material between the interface surface of the rotor laminations (i.e., the inner peripheral surface of the rotor opening) and the reinforcement blocks formed or provided therein, and / or between the interface surface of the rotor laminations and the permanent magnets disposed in the rotor openings.
[0006] In various embodiments described herein, the polymer material used to bond the reinforcement block to the rotor laminations is configured to function as both a primer material and an adhesive material to enhance the high speed operating performance of the rotor. Thus, the physical layer formed of such material is referred to herein as a polymer primer / adhesive layer. The polymer primer / adhesive layer primarily functions as an adhesive material when applied to smaller rotor openings or gaps in the rotor laminations, and primarily functions as a primer material when applied to larger rotor openings or gaps, with various use cases described in detail below.
[0007] In a particular embodiment, an adhesive-reinforced rotor for a rotating electric machine includes a stack of rotor lamination layers ("rotor laminations") constructed of a magnetic core material, each of the rotor laminations having an inner axial surface that collectively defines a set of rotor openings through the magnetic core material. One or more reinforcement blocks constructed of a non-magnetic, non-magnetic, and non-conductive material are disposed within a corresponding one of the rotor openings. A polymer primer / adhesive layer having a bond line thickness of less than 1 mm is disposed between the one or more reinforcement blocks and the inner axial surfaces of the rotor laminations. In this embodiment, the polymer primer / adhesive layer and the reinforcement blocks have a tensile strength of at least 50 MPa, and the elastic modulus of the reinforcement blocks is at least three times the elastic modulus of the primer / adhesive layer.
[0008] The elastic modulus of the reinforcement block may be at least 10 GPa, while the elastic modulus of the polymer primer / adhesive layer is less than 3 GPa. In some configurations where the reinforcement block is constructed of a reinforced polymer, at least 30% of the volume of the reinforcement block is composed of reinforcing fibers and / or particles, while less than 10% of the volume of the polymer primer / adhesive layer is composed of reinforcing fibers and / or particles.
[0009] In other embodiments, the reinforcement blocks may alternatively be constructed of ceramic materials.
[0010] In some embodiments, the polymer primer / adhesive layer has a bond line thickness between 0.05 mm and 0.2 mm, an elastic modulus of less than 1 GPa, and a coefficient of linear expansion of at least 40 ppm / °C.
[0011] The rotor may include permanent magnets, each respective one of the permanent magnets being disposed within a respective one of the rotor openings and bonded to the rotor laminations by a polymer primer / adhesive layer.
[0012] At least one of the reinforcement blocks may optionally define one or more coolant passages therethrough.
[0013] In some configurations, the polymeric primer / adhesive layer includes a void volume between 0.5% and 5% of the total volume of the primer / adhesive layer.
[0014] At least one of the reinforcement blocks may comprise a plurality of sections of polymer material bonded together using a polymer primer / adhesive layer.
[0015] Aspects of the present disclosure include a thin nucleation layer having a thickness of 20 nm or less deposited on or along the axially extending inner surface of the rotor laminations (ie, the peripheral surface of the rotor opening).
[0016] The outer surface of the reinforcement block may optionally define protrusions, each protrusion having a height between 95% and 99% of the thickness of the bond line.
[0017] A method of constructing the above-described adhesive-enhanced rotor for a rotating electric machine is also disclosed. In an exemplary embodiment, the method includes forming a stack of rotor laminations from a magnetic core material, the rotor laminations including axial inner surfaces that together define a set of rotor openings through the rotor laminations. The method includes coating the axial inner surfaces of the rotor laminations with a polymer primer / adhesive layer to a predetermined bond line thickness of less than 1 mm, and partially curing or b-staging the polymer primer / adhesive layer.
[0018] The method in this embodiment also includes inserting a reinforcement block constructed of a ceramic or reinforced polymer composite into one or more rotor openings after partially curing or b-staging the polymer primer / adhesive material. The elastic modulus of the reinforcement block is at least three times the elastic modulus of the polymer primer / adhesive material. The method includes bonding the reinforcement block to the rotor laminations around the axial inner surface using the polymer primer / adhesive material to reinforce the rotor.
[0019] In another aspect of the present disclosure, a rotating electric machine includes a rotor having a rotor lamination surrounded by a stator, the rotor lamination being formed of electrical steel and having an axial inner surface that collectively defines a set of rotor openings. The motor includes: one or more reinforcement blocks constructed of a ceramic material or a reinforced polymer composite and disposed within the rotor opening, wherein a corresponding outer surface of each of the reinforcement blocks defines a plurality of protrusions; and a nucleation layer bonded to the axial inner surface. In this particular embodiment, the nucleation layer is constructed of Al2O3 and has a thickness of less than 20 nm. A polymer primer / adhesive layer having a bond line thickness between 0.05 mm and 0.2 mm is disposed between each corresponding reinforcement block in the reinforcement block and the rotor lamination. The distance that the protrusion extends into the primer / adhesive layer is between 90% and 99% of the bond line thickness.
[0020] In this exemplary embodiment, the elastic modulus of the reinforced polymer material is at least 10 GPa, and the elastic modulus of the polymer primer / adhesive layer is less than 1 GPa. The polymer primer / adhesive layer and the reinforcement block have a tensile strength of at least 50 MPa and a linear expansion coefficient of about 10-20 ppm / °C or greater.
[0021] The present invention provides the following technical solutions:
[0022] 1. An adhesive-reinforced rotor for a rotating electrical machine, comprising:
[0023] a stack of rotor lamination layers constructed of a magnetic core material, each of the rotor lamination layers having an inner axial surface that collectively define a set of rotor openings through the magnetic core material;
[0024] one or more reinforcement blocks constructed of a non-magnetic, non-metallic, and non-conductive material, wherein the one or more reinforcement blocks are disposed within a corresponding one of the rotor openings; and
[0025] A polymer primer / adhesive layer having a bond line thickness of less than 1 mm, wherein the polymer primer / adhesive layer is disposed between the one or more reinforcement blocks and the inner axial surface of the rotor lamination layer, the polymer primer / adhesive layer and the reinforcement blocks having a tensile strength of at least 50 MPa, and the elastic modulus of the reinforcement blocks is at least three times the elastic modulus of the primer / adhesive layer.
[0026] 2. The adhesive-reinforced rotor of claim 1, wherein the elastic modulus of the reinforcement block is at least 10 GPa and the elastic modulus of the polymer primer / adhesive layer is less than 3 GPa.
[0027] 3. An adhesive-reinforced rotor according to claim 1, wherein at least 30% by volume of the reinforcement block consists of reinforcing fibers and / or particles, and wherein less than 10% by volume of the polymer primer / adhesive layer consists of the reinforcing fibers and / or particles.
[0028] 4. An adhesive-reinforced rotor according to Option 1, wherein the reinforcement block is constructed of a ceramic material.
[0029] 5. The adhesive-reinforced rotor of claim 1 wherein the polymer primer / adhesive layer has a bond line thickness between 0.05 mm and 0.2 mm, an elastic modulus of less than 1 GPa, and a coefficient of linear expansion of at least 40 ppm / °C.
[0030] 6. The adhesive-enhanced rotor of claim 1, further comprising a plurality of permanent magnets, each of the permanent magnets being disposed in a corresponding one of the rotor openings and bonded to the rotor lamination layers by the polymer primer / adhesive layer.
[0031] 7. The adhesive reinforced rotor of claim 1, wherein at least one of the reinforcement blocks defines one or more coolant passages therethrough.
[0032] 8. The adhesive-enhanced rotor of claim 1, wherein the primer / adhesive layer comprises a void volume between 0.5% and 5% of the total volume of the primer / adhesive layer.
[0033] 9. The adhesive reinforced rotor of claim 1, wherein at least one of the reinforcement blocks has a plurality of sections bonded together using the polymer primer / adhesive material.
[0034] 10. The adhesive-reinforced rotor of Option 1 further comprises a nucleation layer on or along the axially extending inner surface of the rotor lamination layer, wherein the nucleation layer has a thickness of 20 nm or less.
[0035] 11. The adhesive reinforced rotor of claim 1, wherein an outer surface of the reinforcement block defines a protrusion having a height between 95% and 99% of the thickness of the bond line.
[0036] 12. A method of constructing an adhesive reinforced rotor for a rotating electrical machine, the method comprising:
[0037] forming a stack of rotor lamination layers from a magnetic core material, the rotor laminations including axial inner surfaces that collectively define a set of rotor openings through the rotor lamination layers;
[0038] coating the axially inner surface of the rotor laminations with a polymer primer / adhesive layer to a predetermined bond line thickness of less than 1 mm;
[0039] partially curing or b-staging the polymer primer / adhesive layer;
[0040] inserting a reinforcement block constructed of a ceramic material or a reinforced polymer composite into one or more of the rotor openings of the rotor lamination layers after partially curing or b-staging the polymer primer / adhesive material, wherein the elastic modulus of the reinforcement block is at least three times the elastic modulus of the polymer primer / adhesive material; and
[0041] The rotor is reinforced by bonding the reinforcement blocks to the rotor lamination layers about an axial inner surface using the polymer primer / adhesive material.
[0042] 13. A method according to claim 12, wherein coating the axial inner surface of the rotor lamination layer with the polymer primer / adhesive layer includes: flooding the rotor with a non-reinforced polymer material and thereafter removing excess thereof using gravity, capillary action, vacuum infiltration, forced air, mechanical rotation and / or mechanical vibration.
[0043] 14. The method of claim 12, further comprising coating the reinforcement block with the polymer primer / adhesive layer prior to inserting the reinforcement block into one or more of the rotor openings of the rotor lamination layers.
[0044] 15. The method according to embodiment 12 further includes inserting permanent magnets into at least some of the rotor openings, wherein inserting the reinforcement blocks includes pre-forming the reinforcement blocks to form pre-formed reinforcement blocks, and thereafter positioning the pre-formed reinforcement blocks adjacent to the permanent magnets within the rotor openings.
[0045] 16. The method of claim 12, further comprising introducing a blowing agent into the polymer primer / adhesive layer during the b-staging, thereby causing gaseous expansion of the polymer primer / adhesive layer to occur.
[0046] 17. The method according to claim 12, further comprising forming protrusions on an outer surface of the reinforcing block, each of the protrusions extending 90% to 99% of the predetermined bonding line thickness.
[0047] 18. The method of claim 12, further comprising applying a nucleation layer to the axial inner surface of the rotor lamination layer to a thickness of less than 20 nm.
[0048] 19. A rotating electrical machine comprising:
[0049] stator;
[0050] a rotor having a plurality of rotor lamination layers surrounded by the stator, the rotor lamination layers being formed of electrical steel and having axial inner surfaces that collectively define a set of rotor openings;
[0051] one or more reinforcement blocks constructed of a ceramic material or a reinforced polymer composite material and disposed within the rotor opening, wherein a respective outer surface of each of the reinforcement blocks defines a plurality of protrusions;
[0052] a nucleation layer bonded to the axial inner surface, constructed of Al2O3 and having a thickness of less than 20 nm; and
[0053] a polymer primer / adhesive layer having a bond line thickness of between 0.05 mm and 0.2 mm, the polymer primer / adhesive layer being constructed of a non-reinforced polymer material and disposed between each respective one of the one or more reinforcement blocks and the rotor lamination layer, wherein:
[0054] Each of the protrusions extends into the primer / adhesive layer a distance between 90% and 99% of the thickness of the bond line;
[0055] The reinforced polymer material has an elastic modulus of at least 10 GPa and the non-reinforced polymer material has an elastic modulus of less than 1 GPa; and
[0056] The non-reinforced polymer material and the reinforcement block each have a tensile strength of at least 50 MPa and a linear expansion coefficient of about 10-20 ppm / ° C. or greater.
[0057] 20. The rotating electric machine according to Option 19 further includes a group of permanent magnets, wherein each corresponding one of the permanent magnets is arranged in a corresponding one of the rotor openings, the outer surface of the permanent magnet is coated with the polymer primer / adhesive layer, and at least some of the reinforcement blocks define one or more coolant channels passing therethrough near at least some of the permanent magnets.
[0058] The above overview does not represent every embodiment or every aspect of the present disclosure. The above features and advantages of the present disclosure and other possible features and advantages will become clear from the following detailed description of the embodiments and best modes for carrying out the present disclosure when considered in conjunction with the accompanying drawings and the appended claims. In addition, the present disclosure explicitly includes combinations and sub-combinations of the elements and features presented above and below. BRIEF DESCRIPTION OF THE DRAWINGS
[0059] Figure 1 is a schematic diagram of an exemplary motor vehicle having an electric drive system including a rotating electric machine having an adhesive-reinforced rotor constructed as described herein.
[0060] Figure 2A , 2B and 2C can be used as Figure 1 Schematic plan view of a representative pole portion of an adhesive reinforced rotor of a portion of an electric machine shown in FIG.
[0061] Figure 3 and Figure 4 It is shown that the formation Figure 2A and Figure 2B Schematic flow chart of the method for a rotor shown in .
[0062] Figure 5A and Figure 5B Can be used as Figure 1 A schematic plan view of a pole portion of an alternative rotor of a portion of an electric machine, the alternative rotor defining a plurality of coolant channels therein.
[0063] Figure 6 is a schematic flow chart illustrating an example method of forming a rotor according to the present disclosure.
[0064] Figure 7 is a schematic illustration of alternative surface profiles that may be used as part of the various methods and rotor configurations described herein. DETAILED DESCRIPTION
[0065] The present disclosure can be implemented in many different forms. Representative examples of the present disclosure are shown in the drawings and described in detail herein as non-limiting examples of the disclosed principles. For this reason, elements and limitations described in the abstract, introduction, summary, and detailed description sections but not explicitly set forth in the claims should not be incorporated into the claims individually or collectively by implication, inference, or otherwise.
[0066] For the purpose of this specification, unless specifically denied, the use of the singular includes the plural, the use of the plural also includes the singular, the terms "and" and "or" shall be both conjunctive and disjunctive, "any" and "all" shall mean "any and all", and the words "include", "contain", "include", "have", etc. mean "including but not limited to". In addition, approximate words such as "about", "almost", "substantially", "substantially", "approximately", etc. may be used herein in the sense of "at, close to or nearly close to", or "within 0-5% of..." or "within an acceptable manufacturing tolerance" or their logical combinations.
[0067] Referring to the drawings, wherein like reference numerals refer to like parts, Figure 1 A motor vehicle 10 is schematically depicted having an electric drive system 11 comprising a rotating electrical machine (M E ) 12. As shown in the following reference Figure 2A-7 As described in detail, the electric machine 12 includes a rotor 12R that is enhanced and assembled according to the present disclosure. The described rotor 12R and the various methods 100, 200, and 300 used in its construction can benefit various types of wheeled and / or tracked land vehicles, propeller-driven watercraft and aircraft, mobile work platforms, etc. Non-vehicle systems can also benefit from the present teachings, including, for example, electrified powertrain architectures, power plants, mobile platforms, robots, lifting or conveying equipment, etc. Figure 1 The motor vehicle 10 shown in FIG. 1 is therefore merely illustrative of one possible advantageous application.
[0068] The electric drive system 11 includes a rotary electric machine 12, the operation of which is controlled by a control signal (arrow CC) from an onboard controller (C) 50. O ) real-time adjustment and control. Those skilled in the art will understand that Figure 1 The schematic diagram of the controller 35 is a motor controller that generates and sends control signals (arrow CC O ) to one or more related subsystems within the electric drive system 11 in response to an input signal (arrow CC I ), such as driver pedal request, temperature and angular velocity of the motor 12, etc.
[0069] Instructions for controlling the motor 12 may be recorded in a memory (M) and may be activated in response to an input signal (arrow CC). I) is executed in real time by one or more processors (P). Although omitted for simplicity, the controller 35 may include one or more electronic control modules, units, processors and their associated hardware components, and will be equipped with sufficient tangible and non-tangible memory (M) variants, application specific integrated circuits (ASICs), systems on chips (SoCs), input / output circuits, high-speed clocks or oscillators, and other hardware and software required to provide the required functions.
[0070] Figure 1 The motor 12 also includes a stator 12S. As is understood in the art, the stator 12S may include slots wound or filled with conductive stator windings (not shown) such that when energized, interaction between the stator 12S and the rotor 12R causes rotation of the rotor 12R. The rotor 12R is coupled to one or more wheels 14 disposed on a drive axle 22 via an output member 19. In the illustrated optional hybrid embodiment of the motor vehicle 10, an internal combustion engine (E) 17 having a plurality of combustion cylinders 17C is coupled to the motor 10 via an input clutch C I The engine torque (arrow T E ) is transmitted to an input member 21 of a transmission (T) 20 (eg, a multi-speed gearbox). In other embodiments, such as when the motor vehicle 10 is configured as a battery electric vehicle, the engine 17 is omitted.
[0071] In the hybrid embodiment shown, the motor torque (arrow T) from the electric machine 12 is M ) alone or together with the engine torque provided by the engine 17 (arrow T E ) are transmitted to the input member 21. In other embodiments, the motor 12 alone provides power to the transmission 20, that is, the motor torque (arrow T M ) provides the input torque (arrow T I ), or the motor 12 may be directly coupled to one or more wheels 14 to act as a wheel motor (not shown). In the exemplary embodiment shown, the output torque (arrow T O ) is guided by the output member 121 of the transmission 20 to the wheels 14 via the drive axle 22 to propel the motor vehicle 10.
[0072] exist Figure 1 1 is schematically shown in FIG. 1 , with a stator 12S coaxially arranged relative to a rotor 12R in a typical radial flux configuration, although the present teachings may also be extended to an axial flux configuration. In some embodiments, the electric machine 12 may be configured as a multi-phase / alternating current (AC) traction or propulsion motor. When so configured, the electric drive system 11 may include a high voltage traction battery pack (B HV) 15, for example, a multi-cell rechargeable lithium-ion configuration or another suitable high voltage / high power battery chemistry. Although the term "high voltage" is relative to typical 12-15V auxiliary voltage levels, and thus may require voltage levels anywhere in excess of the aforementioned auxiliary voltage levels, exemplary battery electric propulsion applications of the type contemplated herein may require the battery pack 15 to have a voltage capacity of 300-500 V or more.
[0073] Still refer to Figure 1 , the battery pack 15 can be electrically connected to a power inverter module (PIM) 16 via a high-voltage DC voltage bus (VDC), and the PIM 16 is in turn electrically connected to the stator 12S via a high-voltage AC voltage bus (VAC). Although omitted for simplicity of illustration, the PIM 16 is internally configured and externally controlled via on / off state control of multiple dies of semiconductor switches, such switches are typically implemented as IGBTs or MOSFETs. Therefore, the DC input voltage of the PIM 16 is inverted and controlled by high-speed pulse width modulation or other suitable switching operations of the PIM 16 to ultimately deliver an AC output voltage and corresponding phase currents (Ia, Ib, Ic). During regenerative events such as braking, the PIM 16 can operate in the opposite manner, that is, by converting the AC input voltage to a DC output voltage suitable for recharging the constituent battery cells of the battery pack 15.
[0074] Other components can be connected to Figure 1 The electric drive system 11 shown in FIG. 1 may include, but is not limited to, the DC-DC converter / auxiliary power module (APM) 25 shown and a power module 25 at a lower auxiliary voltage (V AUX ) is operated by a lead-acid or other type of auxiliary battery (B AUX ) 26. As mentioned above, the auxiliary voltage level is typically 12 V to 15 V, and therefore the APM 25 can operate through internal switching operations and signal filtering, as is well known in the art, to receive a relatively high DC voltage from the DC voltage bus (VDC) and convert the auxiliary voltage (V AUX ) is output to the auxiliary battery 26. Thus, the electric machine 12 is only one of multiple devices that require a reliable and continuous supply of electrical energy from the battery pack 15 during ongoing propulsion operation of the motor vehicle 10.
[0075] Reference now Figure 2A and 2B , provides Figure 1 1 is a schematic plan view of a representative magnetic pole portion 12R-MAG of a rotor 12R shown in FIG. 1 , the magnetic pole portion 12R-MAG comprising a stack of rotor laminations 120, one of the rotor laminations being Figure 2A and 2B12R-MAG. The rotor laminations 120 define one or more rotor openings 120-O. As is understood in the art, such magnetic pole segments 12R-MAG are repeated around the entire circumference of the annular rotor laminations 120, and in a given configuration of the rotor 12R, the number of such magnetic pole segments 12R-MAG is therefore equal to the number of magnetic poles of the rotor 12R. The exemplary magnetic pole segments 12R-MAG are depicted with non-limiting representative dimensions and internal configurations, in this case, as Figure 1 One of the six magnetic pole portions 12R-MAG in the six-pole configuration of the rotor 12R, defining four rotor openings 120-O for each magnetic pole portion 12R-MAG. In other words, in various embodiments, the rotor 12R may have fewer or more magnetic pole portions 12R-MAG, with or without the depicted number, shape, and orientation of the rotor openings 120-O.
[0076] As is understood in the art, each fully formed rotor lamination 120 defines a closed ring or loop having an outer diameter surface 23-O and an inner diameter surface 23-I, and thus a given magnetic pole portion 12R-MAG extends radially between the corresponding outer diameter surface 23-O and inner diameter surface 23-I. When fully assembled, the rotor 12R and its constituent axially extending stacked rotor laminations 120 form a cylindrical hub. A rotor shaft (not shown) may be splined or otherwise connected to the inner diameter surface 23-I of the stacked rotor laminations 120 and coupled to a load 24, such as an output member 19, a transmission 20, and / or an axle 22, as shown. Figure 1 as shown in .
[0077] Each of the rotor laminations 120 may be independently stamped from a thin blank of electrical steel or another magnetic or ferromagnetic core material suitable for the application. Figure 2A ) or permanent magnet assisted embodiment ( Figure 2B ), the rotor laminations 120 may independently and / or collectively define one or more of the above-mentioned rotor openings 120-O, albeit at the expense of additional components, but Figure 2B The example embodiments of FIG. 4 may provide certain magnetic performance advantages via the inclusion of permanent magnets 40 .
[0078] In the presently disclosed construction, at least some of the rotor openings 120-O are substantially occupied or filled by solid or semi-solid reinforcement blocks 30 constructed of various possible non-metallic, non-conductive, non-magnetic materials described herein, and in certain configurations may be constructed of permanent magnets 40. The composition of such permanent magnets 40 may vary depending on the intended application, and suitable exemplary non-limiting compositions include ferrites, neodymium (NdFeB), samarium-cobalt (SmCo), iron nitride or manganese-based magnets, etc.
[0079] Likewise, the shape, size, profile, and number of permanent magnets 40 occupying a given one of the rotor openings 120-O may vary in different embodiments. For example, for ease of manufacture and to simplify assembly and / or increase cost savings, it may be desirable for the permanent magnet 40 or a portion thereof to have a generally rectangular polyhedral shape. Alternatively, within the scope of the present disclosure, the permanent magnet 40 may be a polyhedral block magnet, a V-shaped or U-shaped magnet, a ring / ring magnet, a bread loaf magnet, a curved tile magnet, etc. Therefore, the depicted arrangements of the various permanent magnets 40 are examples of the present teachings and are therefore non-limiting.
[0080] Also within the scope of the present disclosure, Figure 1 The rotor 12R may include a polymer primer / adhesive layer 50 disposed between the reinforcement block 30 and the electrical steel or other magnetic core material of the surrounding rotor laminations 120, and / or Figure 2B The polymer primer / adhesive layer 50 is constructed of epoxy resin or other polymer material suitable for the application, various examples of which are described below. In terms of its thickness, the polymer primer / adhesive layer 50 may have a bond line thickness (T BL )(See Figure 2C An exemplary lower limit of about 0.01 mm is contemplated, and in representative embodiments a thickness range of about 0.05 mm to about 0.2 mm is possible.
[0081] As contemplated herein, within the exemplary range, when polymer primer / adhesive layer 50 is used as a primer, a relatively thick application of polymer primer / adhesive layer 50 may be used, i.e., to improve the bond strength between reinforcement block 30 and the surface of rotor lamination 120 defining rotor opening 120-O in which reinforcement block 30 is disposed. When used in other locations, such as between one of permanent magnets 40 and the core material of rotor lamination 120, as Figure 2B As shown in , the material of polymer primer / adhesive layer 50 acts as the primary adhesive.
[0082] Brief reference Figure 2C , the bond line thickness of the polymer primer / adhesive layer 50 (T BL ) is defined between the interfacing axial surfaces 130 and 220 of the respective reinforcement block 30 and rotor lamination 120. The actual bond line thickness (T BL ) may be determined based on the materials of construction of rotor laminations 120, polymer primer / adhesive layer 50, and reinforcement blocks 30, as well as the intended end use of rotor 12R. In general, the bond line thickness (T BL) can be between about 0.1 mm and about 1 mm for optimal performance. The material thickness is determined by the size of the small gap 34 between the interface surfaces 130 and 220, within which the material of the polymer primer / adhesive layer 50 is applied, pulled through, or otherwise provided, as described below.
[0083] Material Properties: In various disclosed embodiments, and as described above, the reinforcement block 30 can be constructed as a solid block of a non-magnetic, non-conductive, non-metallic material (such as ceramic), or as a reinforced polymer material. The reinforcement block 30 can have a relatively high elastic modulus, for example, in excess of about 10 Gpa, and have a high tensile strength in excess of about 50 MPa. Suitable materials will also have a linear thermal expansion coefficient that is similar to that of electrical steel, for example, about 10-20 ppm / °C or higher. In certain embodiments, the reinforcement block 30 is formed of a polymer molding compound, for example, an epoxy resin or other polymer resin containing a predetermined volume of reinforcing particles and / or fibers (such as glass fibers or carbon fibers) of the type commonly used in injection molding, compression molding, and transfer molding processes. Other constructions may include phenolic molding compounds or continuous fiber composites, typically with the composition of the reinforcement material accounting for about 30-40% of the volume of the reinforcement block 30 formed.
[0084] With respect to the polymer primer / adhesive layer 50, the material used for construction is used to transfer mechanical stresses from the rotor laminations 120 to the reinforcement blocks 30 and, if used, to the permanent magnets 40 contained within the rotor laminations 120. Suitable examples of polymer materials that may be used for this purpose include, but are not limited to, mixtures of epoxies, acrylates, polyurethanes, polyimides, and / or bismaleimides, or possibly other materials that provide sufficiently high bonding strength to adjacent sub-stages.
[0085] Relative to the polymer materials used to construct some embodiments of the reinforcement block 30 as described above, the construction material of the polymer primer / adhesive layer 50 can have a relatively low elastic modulus, for example, less than 3 GPa, or less than about 1 GPa in different embodiments, with a similarly high tensile strength of about 50 MPa or more. Within the disclosed ranges, the lower elastic modulus of the polymer primer / adhesive layer 50 can help relieve stresses between different construction materials, for example due to different thermal expansion and other factors or effects.
[0086] By way of example and not limitation, the elastic modulus of reinforcement block 30 may be at least three times the corresponding elastic modulus of polymer primer / adhesive layer 50. Thus, polymer primer / adhesive layer 50 is made more compliant than the material of reinforcement block 30 and also has a relatively high elongation at break. As will be appreciated by one of ordinary skill in the art, elongation at break is a measure of the ductility of a material, i.e., the amount of strain a given material can withstand before failing under a tensile test load.
[0087] Additionally, the coefficient of linear thermal expansion or CLTE of the polymer primer / adhesive layer 50 can be close to that of the electrical steel or other magnetic core material used to construct the rotor laminations 120, for example, about 10-20 ppm / °C as described above, or greater than about 40 ppm / °C in other embodiments. With respect to the relative terms "reinforced" and "non-reinforced" as used herein, the material of the reinforcement block 30 and the material of the polymer primer / adhesive layer 50 can include an amount of reinforcement material, wherein the amount of reinforcement material of the reinforcement block 30 is significantly higher than the amount of reinforcement material that may be present in the polymer primer / adhesive layer 50.
[0088] In a possible embodiment, at least 30% by volume of the optional polymer material used to construct the reinforcement block 30 may be composed of fibers and / or suspended particles of the above-described type. Alternatively, as described above, some or all of the reinforcement block 30 may be constructed of a solid, monolithic block of a non-polymeric material suitable for the application (e.g., ceramic). In contrast, less than about 10% by volume of the polymer primer / adhesive layer 50 may be composed of such reinforcing fibers and / or suspended particles, and thus, to that extent, the polymer primer / adhesive 50 is non-reinforcing relative to the reinforcement block 30.
[0089] The following will now be described with reference to the remaining drawings Figure 1 The above rotor 12R is manufactured. First, turn to Figure 3 ,form Figure 1 The method 100 of the adhesive enhanced rotor 12R described above begins at process block B102, where a sufficient number of rotor laminations 120 for an application are manufactured. Figure 3 A portion of one such rotor lamination 120 is depicted in FIG. As is understood in the art, block B102 may entail stamping or die-stamping individual or stacked blanks of electrical steel or another magnetic core material. The rotor laminations 120, formed in thin layers rather than a single homogenous stack to help reduce eddy current losses, are then stacked one on top of the other to form a cylindrical rotor stack with the aid of a fixture (not shown) according to recognized manufacturing processes. The rotor laminations 120 may be loosely stacked, or the rotor laminations 120 may be bonded and / or welded together into a final stack depending on the application.
[0090] After manufacturing or otherwise providing the rotor laminations 120 or their stacks in frame B102, the method 100 proceeds to optional frame B104. Frame B104 may require inserting the permanent magnets 40 into at least some / one or more of the defined rotor openings 120-O. As shown, there is a small circumferential gap 34 between the reinforcement block 30, the permanent magnet 40 and the axial surface 220 defining the rotor opening 120-O. Such gaps 34 facilitate the insertion of the reinforcement block 30 and the optional permanent magnet 40, and also provide space for applying the disclosed polymer primer / adhesive layer 50. Once the optional permanent magnet 40 has been inserted into the rotor opening 120-O, the method 100 proceeds to frame B106.
[0091] Block B106 of the method 100 may include coating the axial surface 220 of the rotor lamination 120 with the non-reinforced polymer material described above to a predetermined bond line thickness (T BL ), bond line thickness (T BL )exist Figure 2C In a possible method, block B106 may be performed by flooding the rotor 12R with the polymer material of the polymer primer / adhesive layer 50 and then removing the excess material via gravity, capillary action, vacuum infiltration, forced air, mechanical rotation, and / or vibration. The polymer material used to construct the polymer primer / adhesive layer 50 should have a sufficiently low viscosity to allow Figure 2C The various gaps 34 in the are filled. However, in the case of a higher viscosity material, block B106 may include applying positive pressure to gently push the material into the gaps 34.
[0092] Alternatively, block B106 may be performed using a fluidized bed coating process. As is understood in the art, when the material is in particulate form, such a process subjects the rotor stack of formed rotor laminations 120 to a radiant and / or conductive heat source, with or without the inclusion of permanent magnets 40, prior to immersing the heated rotor laminations 120 in a vibrating bed of non-reinforced polymer material. Air may be forced into the bed, and the air pressure and mechanical vibrations together cause the particles to adhere to the exposed axial surfaces 220 of the rotor laminations 120. The resulting coating thickness using such a fluidized bed coating process is generally proportional to the elapsed time of the rotor stack into the fluidized bed and the number of immersions.
[0093] Within the scope of method 100, polymer primer / adhesive layer 50 may be partially cured in a process referred to as "b-staging" prior to proceeding to block B108. The increased viscosity and cross-linking provided by b-staging may help prevent non-reinforced materials of polymer primer / adhesive layer 50 from washing away. Suitable curing processes include ultraviolet curing, optical curing using, for example, a xenon lamp, and / or infrared curing. Such exemplary methods may be used as a non-thermal method to partially cure the material of primer / adhesive layer 50, such as by inserting a heat / light rod (not shown) into rotor opening 120-O.
[0094] With or without first coating the reinforcement block 30 with a polymer primer / adhesive layer 50, the reinforcement block 30 may then be inserted into and thereby disposed in one or more rotor openings 120-O of the rotor lamination 120 as part of box B108, wherein some of the polymer primer / adhesive layer 50 contacts and coats the surface of the reinforcement block 30. In some embodiments, the reinforcement block 30 may be preformed in a separate process and then inserted into the rotor opening 120-O around the installed permanent magnet 40. Such a process, which may require additional steps associated with directly molding the reinforcement block 30 into the rotor opening 120-O, has the advantage of separating the adhesive requirements from the overall structural requirements, thereby allowing improved optimization. Alternatively, the reinforcement block 30 may be overmolded into the rotor opening 120-O around the installed permanent magnet 40.
[0095] refer to Figure 4 ,form Figure 1 The alternative method 200 of adhesive-reinforced rotor 12R begins at block B202 by molding or pre-forming reinforcement blocks 30 outside the footprint of rotor laminations 120. Molding a polymer into a semi-solid or solid block of material may include using an injection molding process, wherein the material is applied to a sacrificial or reusable mold having a shape required for insertion into rotor opening 120-O, or other processes that result in the formation of such reinforcement blocks 30. Other suitable reinforcement blocks 30 of solid ceramic construction or solid construction may also be pre-formed outside of rotor laminations 120.
[0096] At block B204, the formed reinforcement block 30 and permanent magnet 40 (if used) are coated with the polymer material of the polymer primer / adhesive layer 50. A variety of techniques may be used to coat the exposed surfaces of the reinforcement block 30 and permanent magnet 40, such as, but not limited to, brushing, rolling, and / or spraying the polymer material onto the exposed surfaces.
[0097] Thereafter, at Block B206, the now coated and preformed reinforcement block 30 and possibly the optional permanent magnet 40 are carefully inserted into the designated rotor opening 120-O previously formed at Block B102 (see Figure 3 ). Thus, b-staging may be used as part of method 200 to help enhance the insertion of mass 30 and permanent magnet 40 .
[0098] In order to ensure that the gap 34 between the reinforcement block 30 and the permanent magnet 40 and / or the rotor lamination 120 is fully filled with the polymer material of the polymer primer / adhesive layer 50, in some embodiments, the polymer material can be configured to increase the volume during the curing process. This effect can be achieved by introducing a predetermined volume of a foaming agent into the non-reinforced polymer material. For example, the foaming agent can be configured to release a controlled amount of carbon dioxide, nitrogen, or another inert gas during the curing process. Doing so will cause the gas expansion of the unreinforced polymer material, thereby effectively creating small voids or bubbles in the polymer primer / adhesive layer 50. If the total void volume provided by such voids is carefully controlled and adjusted to less than 5% of the volume of the non-reinforced polymer material, for example between 0.5% and 5%, the resulting bond strength will not be significantly affected.
[0099] Corresponding Figure 3 and Figure 4 The methods 100 and 200 may optionally include the use of nanoscale surface treatments to further optimize the adhesion and retention of the various structural layers (i.e., the polymer primer / adhesive layer 50, the reinforcement block 30, the rotor laminations 120, and the optional permanent magnets 40). For example, the axially extending inner surface 120-O of the rotor laminations 120 may be coated with a thin nucleation layer such as aluminum oxide (Al2O3), and a phosphate-based coating or a silane-based coating may be used in different embodiments. The term "thin" as used herein is nanoscale, such as less than about 20 nm, such as 5 nm to 20 nm, with the smaller end of the scale providing the optimal benefits. For the polymer materials used in the composition of the polymer primer / adhesive layer 50 and in some embodiments of the reinforcement block 30, processes such as fluorination, silane-based polymers, or under-curing may be used.
[0100] Brief reference Figure 5A and 5B In the various embodiments described above, the reinforcement block 30 may optionally define one or more coolant passages 60. It should be understood that an electrical coolant (not shown) suitable for the application may be circulated through the provided coolant passages 60 via a coolant system (not shown) to help regulate the Figure 1 The temperature of the rotor 12R. Figure 5A In the embodiment of the present invention, for example, the coolant passage 60 may be present at one or more locations in at least some of the rotor openings 120-O, and / or in a non-limiting manner. Figure 5B In the embodiment of FIG. 4 , the permanent magnet 40 is adjacent to the permanent magnet 40 .
[0101] Figure 5A and Figure 5B The coolant passages 60 may be formed in a variety of ways, including by molding the shape of the coolant passages 60 into the reinforcement block 30 during its formation. This process may be aided by sacrificial material that is then removed after solidification. For larger rotor openings 120-O, correspondingly larger reinforcement blocks 30 may be formed in multiple sections (see Figure 5A ), each having a simpler geometry, and then bonding the segments together, for example, using the same non-reinforced polymer material as polymer primer / adhesive layer 50 or another suitable material.
[0102] Figure 6 Another method 300 is depicted that can facilitate Figure 2A-5B The method 300 may include forming the rotor laminations 120 shown in the figure. Due to the cantilever nature of the magnetic flux path inside the rotor laminations 120, a step-by-step stamping process may be required to manufacture the rotor laminations 120 of the shown configuration with minimal sheet warpage. Starting at block B302, the method 300 may include stamping or punching the rotor laminations 120 without forming the rotor openings 120-O. Therefore, the rotor laminations 120 are initially configured as a solid, continuous annular band.
[0103] Once a sufficient number of such rotor laminations 120 for an application have been formed in this manner, the method 300 proceeds to box B304. At box B304, the method 300 includes stamping or punching a first set of rotor openings 120-O1 through each of the rotor laminations 120 constructed in box B302. Similarly, at box B306, a second set of rotor openings 120-O2 can be formed symmetrically relative to the first set of rotor openings 120-O1 formed in box B304, such that the radially extending magnetic rib portions 120-R of each of the rotor laminations 120 symmetrically separate the respective first and second sets of rotor openings 120-O1 and 120-O2. Subsequently, at box B308, such rib portions 12O-R are cut away and removed to form a final formed rotor lamination 120 as described above, for example, as Figure 3 As shown in box B102.
[0104] refer to Figure 7 , the various methods 100, 200, and 300 described above may include forming or providing a plurality of protrusions 70, such as raised bumps, bosses, and / or other regular or irregular surface protrusions or asperities. Such protrusions 70, shown in more detail in inset area AA, may be formed on or molded into an outer surface 130 of the reinforcement block 30, which in this case is a particular outer surface of the reinforcement block 30 that faces a surface 220 of the surrounding rotor laminations 120 when the reinforcement block 30 has been inserted into the rotor opening 120-O.
[0105] The height of the protrusion 70 may not exceed the thickness of the bonding line (T BL ), and ideally slightly shorter, where “slightly” in the exemplary embodiment refers to the bond line thickness (T BL ) is about 95-99%. Therefore, in order to facilitate the sliding engagement of the reinforcement block 30 into the rotor opening 120-O, when molding the reinforcement block 30 so that it is thicker than the bonding line thickness (T BL ) is shorter, this in turn will provide a gap in the fit and a protrusion 70 can be formed.
[0106] Therefore, the above disclosure realizes that the rotor laminations 120 are stacked in Figure 1 The adhesive-reinforced construction of the rotor 12R shown in the non-limiting application of the present invention, wherein the rotor 12R is reinforced via a reinforcement block 30 and a polymer primer / adhesive layer 50 configured as described herein. Within the structure of the reinforcement block 30, an optional configuration of the rotor 12R may include Figure 2B-4 and 5B permanent magnet 40, and / or Figure 5A and Figure 5B As shown in FIG. 60 , the reinforcement block 30 may include Figure 7 The use of structural polymers, ceramics and / or other high stiffness and low conductivity materials may be used for added reinforcement, and a nanoscale nucleation layer may be applied to the rotor laminations 120 to further enhance the bonding of the polymer primer / adhesive layer 50 to the surface 220 of the rotor laminations 120.
[0107] The detailed description and the accompanying drawings or illustrations are support and description of the present teaching, but the scope of the present teaching is limited only by the claims. Although some optimal modes and other embodiments for carrying out the present teaching have been described in detail, there are various alternative designs and embodiments for practicing the present teaching defined in the appended claims. Moreover, the present disclosure explicitly includes combinations and sub-combinations of the elements and features presented above and below.
Claims
1. An adhesive-reinforced rotor for a rotating electrical machine, comprising: a stack of rotor lamination layers constructed of a magnetic core material, each of the rotor lamination layers having an inner axial surface that collectively define a set of rotor openings through the magnetic core material; one or more reinforcement blocks constructed of a non-magnetic, non-metallic, and non-conductive material, wherein the one or more reinforcement blocks are disposed within a corresponding one of the rotor openings; and A polymer primer / adhesive layer having a bond line thickness of less than 1 mm, wherein the polymer primer / adhesive layer is disposed between the one or more reinforcement blocks and the inner axial surface of the rotor lamination layer, the polymer primer / adhesive layer and the reinforcement blocks having a tensile strength of at least 50 MPa, and the elastic modulus of the reinforcement blocks is at least three times the elastic modulus of the primer / adhesive layer.
2. The adhesive-reinforced rotor of claim 1, wherein: The elastic modulus of the reinforcement block is at least 10 GPa, and the elastic modulus of the polymer primer / adhesive layer is less than 3 GPa.
3. The adhesive-reinforced rotor of claim 1, wherein: At least 30% by volume of the reinforcement block consists of reinforcement fibers and / or particles, and wherein less than 10% by volume of the polymer primer / adhesive layer consists of the reinforcement fibers and / or particles.
4. The adhesive-reinforced rotor of claim 1, wherein: The reinforcement block is constructed of a ceramic material.
5. The adhesive-reinforced rotor of claim 1, wherein: The polymer primer / adhesive layer has a bond line thickness between 0.05 mm and 0.2 mm, an elastic modulus of less than 1 GPa, and a linear expansion coefficient of at least 40 ppm / °C.
6. The adhesive enhanced rotor of claim 1 further comprising a plurality of permanent magnets, each respective one of said permanent magnets being disposed in a corresponding one of said rotor openings and bonded to said rotor lamination layers by said polymer primer / adhesive layer.
7. The adhesive-reinforced rotor of claim 1, wherein: At least one of the reinforcement blocks defines one or more coolant passages therethrough.
8. The adhesive-reinforced rotor of claim 1, wherein: The primer / adhesive layer includes a void volume between 0.5% and 5% of the total volume of the primer / adhesive layer.
9. The adhesive-reinforced rotor of claim 1, wherein: At least one of the reinforcement blocks has a plurality of sections bonded together using the polymer primer / adhesive material.
10. The adhesive-enhanced rotor of claim 1, further comprising a nucleation layer on or along the axially extending inner surface of the rotor lamination layer, wherein: The nucleation layer has a thickness of 20 nm or less.
11. The adhesive-reinforced rotor of claim 1 , wherein: An outer surface of the reinforcement block defines a protrusion having a height between 95% and 99% of a thickness of the bond line.
12. A method of constructing an adhesive-reinforced rotor for a rotating electrical machine, the method comprising: forming a stack of rotor lamination layers from a magnetic core material, the rotor laminations including axial inner surfaces that collectively define a set of rotor openings through the rotor lamination layers; coating the axially inner surface of the rotor laminations with a polymer primer / adhesive layer to a predetermined bond line thickness of less than 1 mm; partially curing or b-staging the polymer primer / adhesive layer; inserting a reinforcement block constructed of a ceramic material or a reinforced polymer composite into one or more of the rotor openings of the rotor lamination layers after partially curing or b-staging the polymer primer / adhesive material, wherein the elastic modulus of the reinforcement block is at least three times the elastic modulus of the polymer primer / adhesive material; as well as The rotor is reinforced by bonding the reinforcement blocks to the rotor lamination layers about an axial inner surface using the polymer primer / adhesive material.
13. The method according to claim 12, wherein: Coating the axially inner surface of the rotor lamination layers with the polymer primer / adhesive layer includes flooding the rotor with a non-reinforced polymer material and thereafter removing excess thereof using gravity, capillary action, vacuum penetration, forced air, mechanical rotation and / or mechanical vibration.
14. The method of claim 12, further comprising coating the reinforcement block with the polymer primer / adhesive layer prior to inserting the reinforcement block into one or more of the rotor openings of the rotor lamination layers.
15. The method of claim 12, further comprising inserting permanent magnets into at least some of the rotor openings, wherein: Inserting the reinforcement block includes pre-forming the reinforcement block to form a pre-formed reinforcement block, and thereafter positioning the pre-formed reinforcement block adjacent to the permanent magnet within the rotor opening.
16. The method of claim 12, further comprising introducing a blowing agent into the polymer primer / adhesive layer during the b-staging, thereby causing gaseous expansion of the polymer primer / adhesive layer to occur.
17. The method of claim 12, further comprising forming protrusions on an outer surface of the reinforcement block, each of the protrusions extending 90% to 99% of the predetermined bonding line thickness.
18. The method of claim 12, further comprising applying a nucleation layer to the axially inner surface of the rotor lamination layers to a thickness of less than 20 nm.
19. A rotating electrical machine comprising: stator; a rotor having a plurality of rotor lamination layers surrounded by the stator, the rotor lamination layers being formed of electrical steel and having axial inner surfaces that collectively define a set of rotor openings; one or more reinforcement blocks constructed of a ceramic material or a reinforced polymer composite material and disposed within the rotor opening, wherein a respective outer surface of each of the reinforcement blocks defines a plurality of protrusions; a nucleation layer bonded to the axial inner surface, constructed of Al2O3 and having a thickness of less than 20 nm; and a polymer primer / adhesive layer having a bond line thickness of between 0.05 mm and 0.2 mm, the polymer primer / adhesive layer being constructed of a non-reinforced polymer material and disposed between each respective one of the one or more reinforcement blocks and the rotor lamination layer, wherein: Each of the protrusions extends into the primer / adhesive layer a distance between 90% and 99% of the thickness of the bond line; The reinforced polymer material has an elastic modulus of at least 10 GPa and the non-reinforced polymer material has an elastic modulus of less than 1 GPa; and The non-reinforced polymer material and the reinforcement block each have a tensile strength of at least 50 MPa and a linear expansion coefficient of 10-20 ppm / ° C. or more.
20. The rotating electric machine of claim 19, further comprising a set of permanent magnets, wherein Each respective one of the permanent magnets is disposed in a respective one of the rotor openings, an outer surface of the permanent magnet being coated with the polymer primer / adhesive layer, and at least some of the reinforcement blocks defining one or more coolant passages therethrough adjacent at least some of the permanent magnets.