A surface acoustic wave device electrode structure and manufacturing method thereof

By plating metal, semiconductor and metal electrode layers on the piezoelectric substrate of the surface acoustic wave filter, it hinders the migration of metal atoms, solving the problem of reduced power tolerance of the surface acoustic wave filter at high temperatures, and improving adhesion and Performance stability.

CN114553171BActive Publication Date: 2024-11-01BEIJING ZHONGKE FEIHONG SCI&TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210088875.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-25
Publication Date
2024-11-01
Estimated Expiration
2042-01-25

AI Technical Summary

Technical Problem

The power tolerance of surface acoustic wave filters decreases under high frequency, high power and high temperature conditions, resulting in problems of holes and weakening of adhesion in the metal electrode layer.

Method used

The first electrode layer made of metal material, the second electrode layer made of semiconductor material and the third electrode layer made of metal material are plating on a piezoelectric substrate, and the third electrode layer made of metal material is enhanced by placing semiconductor molecules. Focus on and improve power tolerance.

Benefits of technology

It effectively improves the power tolerance and adhesion of the surface acoustic wave filter, prevents metal atom agglomeration and hole formation, and ensures the stable performance of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114553171B_ABST
    Figure CN114553171B_ABST
Patent Text Reader

Abstract

The present application relates to an electrode structure of a surface acoustic wave device and a manufacturing method thereof, wherein the electrode structure includes a first electrode layer, a second electrode layer and a third electrode layer; the first electrode layer is plated on one side of the piezoelectric substrate; the second electrode layer is plated on one side of the first electrode layer away from the piezoelectric substrate; the third electrode layer is plated on one side of the second electrode layer away from the piezoelectric substrate; the first electrode layer and the third electrode layer are made of metal materials; the second electrode layer is made of semiconductor materials. When the second electrode layer is plated on the first electrode layer, as the surface acoustic wave filter is used for a long time, the high temperature generated by it makes the metal atoms have a tendency to move, but because the semiconductor molecules are relatively stable at this time, they can prevent the metal atoms from moving under the tendency to move, thereby improving the power tolerance of the surface acoustic wave filter to a certain extent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of surface acoustic wave devices, and in particular to a surface acoustic wave device electrode structure and a manufacturing method thereof. Background Art

[0002] Surface acoustic wave filters are widely used in mobile communication devices. With the development of science and technology, surface acoustic wave filters are developing in the direction of high frequency, high power tolerance, high temperature stability and small size.

[0003] It is understood that the operating frequency of the surface acoustic wave filter depends on the strip width of the interdigital electrode, that is, the higher the operating frequency of the surface acoustic wave filter, the thinner the electrode strip. Nowadays, the frequency requirements of the surface acoustic wave filter in the communication field are getting higher and higher, making the strip width of the interdigital electrode narrower and narrower. In this case, the power density of the surface acoustic wave filter also increases, which causes serious heat generation in its working state and generates more heat. The metal electrode layer plated on the piezoelectric substrate will be affected by high temperature and defects such as holes will appear, which will lead to a decrease in power tolerance. Summary of the invention

[0004] In order to improve the power tolerance of a surface acoustic wave filter, the present application provides a surface acoustic wave device electrode structure and a manufacturing method thereof.

[0005] In a first aspect, the present application provides a surface acoustic wave device electrode structure, which adopts the following technical solution:

[0006] A surface acoustic wave device electrode structure is plated on a piezoelectric substrate and includes a first electrode layer, a second electrode layer and a third electrode layer;

[0007] The first electrode layer is plated on one side of the piezoelectric substrate;

[0008] The second electrode layer is plated on a side of the first electrode layer away from the piezoelectric substrate;

[0009] The third electrode layer is plated on a side of the second electrode layer away from the piezoelectric substrate;

[0010] The first electrode layer and the third electrode layer are made of metal materials;

[0011] The second electrode layer is made of semiconductor material.

[0012] By adopting the above technical solution, since the second electrode layer is made of semiconductor material, it has the characteristic of being relatively stable at high temperatures. When the second electrode layer is plated on the first electrode layer, from a microscopic perspective, the semiconductor molecules and metal atoms are closely arranged. As the surface acoustic wave filter is used for a long time, the high temperature generated by it makes the metal atoms have a tendency to move, but since the semiconductor molecules are relatively stable at this time, they can prevent the metal atoms from moving under the tendency to move, thereby improving the power tolerance of the surface acoustic wave filter to a certain extent.

[0013] Optionally, the first electrode layer includes an adhesion layer and an electrode layer;

[0014] The adhesion layer is made of metal chromium or metal titanium;

[0015] The electrode layer is made of metal aluminum, metal copper or aluminum-copper alloy;

[0016] The second electrode layer is made of indium tin oxide or indium zinc oxide;

[0017] The third electrode layer is made of metal aluminum, metal copper or aluminum-copper alloy.

[0018] By adopting the above technical solution, the adhesion of the adhesion layer and the third electrode layer can be increased.

[0019] Optionally, the thickness of the adhesion layer is in the range of 1 to 5 nm, the thickness of the electrode layer is in the range of 10 to 100 nm, and the thickness of the second electrode layer is in the range of 1 to 100 nm.

[0020] By adopting the above technical solution, the adhesion can be improved while ensuring the performance of the surface acoustic wave filter.

[0021] Optionally, the thickness of the third electrode layer is in the range of 2 to 10 um.

[0022] By adopting the above technical solution, the thickness of the third electrode layer is greater than the thickness of the first electrode layer and the second electrode layer, so as to increase the adhesion.

[0023] Optionally, a wiring position is reserved on the side of the piezoelectric substrate where the first electrode layer is located, the wiring position is located at a non-edge of the piezoelectric substrate, and the first electrode layer, the second electrode layer and the third electrode layer are plated at positions outside the wiring position;

[0024] The side of the first electrode layer is plated with a fourth electrode layer, and the fourth electrode layer is made of indium tin oxide or indium zinc oxide.

[0025] By adopting the above technical solution, the first electrode layer can be better fixed to prevent the metal atoms from moving after being heated.

[0026] In a second aspect, the present application provides a method for manufacturing an electrode structure of a surface acoustic wave device, using the following technical solution:

[0027] A method for manufacturing an electrode structure of a surface acoustic wave device, comprising plating a first electrode layer on one surface of a piezoelectric substrate, plating a second electrode layer on the first electrode layer, and plating a third electrode layer on the second electrode layer;

[0028] The first electrode layer and the third electrode layer are made of metal materials;

[0029] The second electrode layer is made of semiconductor material.

[0030] Optionally, the first electrode layer includes an adhesion layer and an electrode layer;

[0031] The adhesion layer is made of metal chromium or metal titanium;

[0032] The electrode layer is made of metal aluminum, metal copper or aluminum-copper alloy;

[0033] The second electrode layer is made of indium tin oxide or indium zinc oxide;

[0034] The third electrode layer is made of metal aluminum, metal copper or aluminum-copper alloy.

[0035] Optionally, the thickness of the adhesion layer is in the range of 1 to 5 nm, the thickness of the electrode layer is in the range of 10 to 100 nm, the thickness of the second electrode layer is in the range of 1 to 100 nm, and the thickness of the third electrode layer is in the range of 2 to 10 um.

[0036] Optionally, the first electrode layer and the third electrode layer are made by evaporation technology or sputtering coating technology, and the second electrode layer is made by sputtering coating technology.

[0037] Optionally, during the coating process, the evaporation rate is 1-10Å / s and the sputtering rate is 1-10Å / s.

[0038] By adopting the above technical solution, the quality of the first electrode layer, the second electrode layer and the third electrode layer is improved.

[0039] In summary, the present application includes at least one of the following beneficial technical effects:

[0040] 1. When the second electrode layer is plated on the first electrode layer, as the surface acoustic wave filter is used for a long time, the high temperature generated makes the metal atoms tend to move. However, since the semiconductor molecules are relatively stable at this time, they can prevent the metal atoms from moving under the tendency to move, thereby improving the power tolerance of the surface acoustic wave filter to a certain extent;

[0041] 2. The adhesion layer and the third electrode layer can enhance adhesion;

[0042] 3. Evaporation or sputtering is performed at a speed of 1-10Å / s to ensure that the first electrode layer, the second electrode layer and the third electrode layer have good quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 It is a structural schematic diagram of the electrode structure of the surface acoustic wave device of Example 1 of the present application.

[0044] Figure 2 It is a structural schematic diagram of the electrode structure of the surface acoustic wave device of the second embodiment of the present application.

[0045] Figure 3 It is a schematic flow chart of a method for manufacturing an electrode structure of a surface acoustic wave device according to an embodiment of the present application.

[0046] Explanation of the accompanying drawings: 1. piezoelectric substrate; 2. first electrode layer; 21. adhesion layer; 22. electrode layer; 3. second electrode layer; 4. third electrode layer; 5. fourth electrode layer; 6. wire. DETAILED DESCRIPTION

[0047] The following is combined with Figure 1-3 This application is described in further detail.

[0048] The embodiment of the present application discloses a surface acoustic wave device electrode structure.

[0049] Embodiment 1:

[0050] Reference Figure 1 The surface acoustic wave device electrode structure includes a first electrode layer 2, a second electrode layer 3 and a third electrode layer 4. The first electrode layer 2, the second electrode layer 3 and the third electrode layer 4 are plated on the piezoelectric substrate 1 of the surface acoustic wave filter, so that the surface acoustic wave filter has good power tolerance.

[0051] The piezoelectric substrate 1 is a piezoelectric material with piezoelectric effect, mainly made of lithium tantalate, lithium niobate, quartz or a piezoelectric material with a multilayer film structure, preferably a 42° YX lithium tantalate substrate.

[0052] The first electrode layer 2 is plated on one side of the piezoelectric substrate 1. The first electrode layer 2 includes an adhesion layer 21 and an electrode layer 22 made of metal materials. Specifically, the adhesion layer 21 is made of metal titanium or metal chromium, so that the adhesion layer 21 has good adhesion to the piezoelectric substrate 1. It is worth noting that when the metal titanium film or the metal chromium film is plated on the piezoelectric substrate 1, its thickness is preferably 1 to 10 nm. When the thickness of the metal titanium film or the metal chromium film exceeds 10 nm, it may affect the performance of the final surface acoustic wave filter.

[0053] The electrode layer 22 is usually made of metal aluminum, metal copper or aluminum-copper alloy. It is understood that the selection of the material for the electrode layer 22 mainly depends on the actual requirements of the surface acoustic wave filter. For example, according to different actual requirements of the surface acoustic wave filter, different proportions of aluminum-copper alloy or aluminum-magnesium alloy can be selected for production, and other metals such as gold, silver, platinum, etc. can also be selected.

[0054] When the metal aluminum film, metal copper film or aluminum-copper alloy film is plated, its thickness is preferably 10-100 nm, so that the manufactured surface acoustic wave filter has good performance.

[0055] It should be noted that when the first electrode layer 2 is plated on the piezoelectric substrate 1 , preferably, the adhesion layer 21 is plated first and then the electrode layer 22 is plated, so that the subsequently plated metal has better orientation and adhesion and is not easy to fall off.

[0056] Further, the second electrode layer 3 is plated on the side of the first electrode layer 2 away from the piezoelectric substrate 1. The second electrode layer 3 is made of a semiconductor material. In the present application, the second electrode layer 3 is preferably made of an indium tin oxide material or an indium zinc oxide material. It can be understood that indium tin oxide or indium zinc oxide has good stability in a high temperature environment. That is, from a microscopic point of view, the arrangement structure of indium tin oxide molecules and indium zinc oxide molecules is relatively stable, and no molecular movement will occur in a high temperature environment. Therefore, after the second electrode layer 3 is plated on the first electrode layer 2, when the manufactured product is used for a long time, the heat generated by the piezoelectric substrate 1 causes the metal aluminum atoms, metal copper atoms or aluminum-copper alloy atoms to have a tendency to agglomerate. At this time, since the indium tin oxide molecules or indium zinc oxide molecules are relatively stably arranged on the metal atoms, the indium tin oxide molecules or indium zinc oxide molecules can hinder the migration of metal atoms in the direction of the movement of the metal atoms, and then can hinder the agglomeration of metal atoms, so that the manufactured surface acoustic wave filter has a higher power tolerance.

[0057] Preferably, the thickness of the indium tin oxide film or the indium zinc oxide film is 1-100 nm, so that the manufactured surface acoustic wave filter can have better performance.

[0058] The third electrode layer 4 is plated on the side of the second electrode layer 3 away from the first electrode layer 2. Specifically, the third electrode layer 4 is also made of a metal material, preferably aluminum, copper or an aluminum-copper alloy in the present application. Further, the selection of the metal material should also be based on the requirements for the surface acoustic wave filter.

[0059] In order to ensure better adhesion between the first electrode layer 2 and the piezoelectric substrate 1, when plating the third electrode layer 4, the thickness of the metal aluminum, metal copper or aluminum-copper alloy is preferably 10nm~2um, while ensuring that its thickness will not affect the performance of the manufactured surface acoustic wave filter.

[0060] Embodiment 2:

[0061] The only difference between this embodiment and the first embodiment is that:

[0062] Reference Figure 2 Although the second electrode layer 3 plated on the first electrode layer 2 can suppress the migration of metal atoms in the first electrode layer 2 to a certain extent, the metal atoms at the edge of the first electrode layer 2 are subject to less resistance than the metal atoms at non-edges, and are therefore more likely to migrate. For this reason, a fourth electrode layer 5 is also plated on the side of the first electrode layer 2.

[0063] Likewise, the fourth electrode layer 5 is also made of a semiconductor material, specifically indium tin oxide or indium zinc oxide.

[0064] Considering that after the fourth electrode layer 5 is plated on the side of the first electrode layer 2, the fourth electrode layer 5 and the second electrode layer 3 made of semiconductor material will have some influence on the conductivity between the third electrode layer 4 and the first electrode layer 2, therefore, the embodiment of the present application improves the structure of the first electrode layer 2, the second electrode layer 3 and the third electrode layer 4.

[0065] Specifically, a wiring position is reserved on the side of the piezoelectric substrate 1 where the first electrode layer 2 needs to be plated. The first electrode layer 2, the second electrode layer 3 and the third electrode layer 4 are all plated at positions outside the wiring position. The wiring position is used to set a wire 6 to connect the third electrode layer 4 and the first electrode layer 2, which can increase their conductivity.

[0066] It should be noted that the wiring position is preferably set at the non-edge of the piezoelectric substrate 1, so that the fourth electrode can completely cover the side of the first electrode layer 2, thereby better hindering the migration of metal atoms in the first electrode layer 2 when the manufactured surface acoustic wave filter is working, so as to improve power tolerance.

[0067] The implementation principle of the electrode structure of a surface acoustic wave device in an embodiment of the present application is: by plating a first electrode layer 2 made of a metal material, a second electrode layer 3 made of a semiconductor material and a third electrode layer 4 made of a metal material on a piezoelectric substrate 1, the heat-stable semiconductor molecules of the manufactured surface acoustic wave filter can hinder the migration of metal atoms that tend to agglomerate when heated during use, so as to prevent the metal atoms from agglomerating to form holes, thereby improving the power tolerance of the surface acoustic wave filter.

[0068] Reference Figure 3 The present application also discloses a method for manufacturing an electrode structure of a surface acoustic wave device. The manufacturing method specifically comprises the following steps:

[0069] Step S1: Select the 42° The substrate is used as a piezoelectric substrate, and a photoresist with a certain thickness is spin-coated on the piezoelectric substrate.

[0070] Step S2: After exposure and development, the required interdigital image is obtained.

[0071] Step S3: Plasma primer.

[0072] Step S4: placing the piezoelectric substrate into an electron beam coating machine and a magnetron sputtering device to coat the first electrode layer, the second electrode layer and the third electrode layer in sequence.

[0073] Step S5: peeling off the obtained piezoelectric substrate in an acetone solution to obtain the desired surface acoustic wave filter.

[0074] Among them, step 4 in the embodiment of the present application is specifically as follows: after placing the piezoelectric substrate into the electron beam coating machine, evacuate to below 1×10-5Pa, evaporate 1nm of metal chromium, and then evaporate 40nm of metal aluminum, with a deposition rate of 0.5Å / s. Of course, in addition to plating 1nm of metal chromium, 1nm of metal titanium can also be plated as an adhesion layer of the first electrode layer to improve the adhesion to the piezoelectric substrate. Not only that, the thickness of the adhesion layer formed by evaporating metal chromium or metal titanium is preferably 1~5nm. In addition, the electrode layer of the first electrode layer formed by evaporating metal aluminum can also be made of evaporated metal copper or aluminum-copper alloy, with a thickness of 10~100nm, which can be made into a surface acoustic wave filter with better performance.

[0075] In the process of coating the first electrode layer, electron evaporation technology or sputtering coating technology can be used, and the deposition rate is preferably 1-10Å / s.

[0076] When coating the second electrode layer, the piezoelectric substrate is placed in a magnetron sputtering device, the argon gas flow rate is set to 20 ml / min, the gas pressure is stabilized at 0.5 Pa, and a 5 nm indium tin oxide film is sputtered by sputtering coating technology. Of course, indium zinc oxide can also be used, with a thickness of 1 to 100 nm, and its deposition rate is preferably 1-10 Å / s.

[0077] The method for coating the third electrode layer is the same as the method for coating the first electrode layer. Metal aluminum, metal copper or aluminum-copper alloy can be coated by electron evaporation technology or sputtering coating technology. The thickness is preferably 10nm~2um, and the deposition rate is preferably 1-10Å / s.

[0078] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.

Claims

1. A surface acoustic wave device electrode structure, plated on a piezoelectric substrate, characterized in that: It comprises a first electrode layer (2), a second electrode layer (3) and a third electrode layer (4); The first electrode layer (2) is plated on one side of the piezoelectric substrate (1); The second electrode layer (3) is plated on a side of the first electrode layer (2) away from the piezoelectric substrate (1); The third electrode layer (4) is plated on a side of the second electrode layer (3) away from the piezoelectric substrate (1); The first electrode layer (2) and the third electrode layer (4) are made of metal materials; The second electrode layer (3) is made of semiconductor material; The first electrode layer (2) comprises an adhesion layer (21) and an electrode layer (22); The adhesion layer (21) is made of metal chromium or metal titanium; The electrode layer (22) is made of metal aluminum, metal copper or aluminum-copper alloy; The second electrode layer (3) is made of indium tin oxide or indium zinc oxide; The third electrode layer (4) is made of metal aluminum, metal copper or an aluminum-copper alloy.

2. The surface acoustic wave device electrode structure according to claim 1, wherein: The thickness of the adhesion layer (21) ranges from 1 to 5 nm, the thickness of the electrode layer (22) ranges from 10 to 100 nm, and the thickness of the second electrode layer (3) ranges from 1 to 100 nm.

3. The surface acoustic wave device electrode structure according to claim 2, wherein: The thickness of the third electrode layer (4) ranges from 10 nm to 2 um.

4. The surface acoustic wave device electrode structure according to claim 3, wherein: A wiring position is reserved on the side of the piezoelectric substrate (1) where the first electrode layer (2) is located, the wiring position is located at a non-edge portion of the piezoelectric substrate (1), and the first electrode layer (2), the second electrode layer (3) and the third electrode layer (4) are plated at positions outside the wiring position; The side of the first electrode layer (2) is plated with a fourth electrode layer (5), and the fourth electrode layer (5) is made of indium tin oxide or indium zinc oxide.

5. A method for manufacturing an electrode structure of a surface acoustic wave device, characterized in that: The method comprises plating a first electrode layer (2) on one surface of a piezoelectric substrate (1), plating a second electrode layer (3) on the first electrode layer (2), and plating a third electrode layer (4) on the second electrode layer (3); The first electrode layer (2) and the third electrode layer (4) are made of metal materials; The second electrode layer (3) is made of semiconductor material; The first electrode layer (2) comprises an adhesion layer (21) and an electrode layer (22); The adhesion layer (21) is made of metal chromium or metal titanium; The electrode layer (22) is made of metal aluminum, metal copper or aluminum-copper alloy; The second electrode layer (3) is made of indium tin oxide or indium zinc oxide; The third electrode layer (4) is made of metal aluminum, metal copper or an aluminum-copper alloy.

6. The method for manufacturing a surface acoustic wave device electrode structure according to claim 5, characterized in that: The thickness of the adhesion layer (21) ranges from 1 to 5 nm, the thickness of the electrode layer (22) ranges from 10 to 100 nm, the thickness of the second electrode layer (3) ranges from 1 to 100 nm, and the thickness of the third electrode layer (4) ranges from 10 nm to 2 μm.

7. The method for manufacturing a surface acoustic wave device electrode structure according to claim 6, wherein: The first electrode layer (2) and the third electrode layer (4) are made by evaporation technology or sputtering coating technology, and the second electrode layer (3) is made by sputtering coating technology.

8. The method for manufacturing a surface acoustic wave device electrode structure according to claim 5, wherein: During the coating process, the evaporation rate is 1-10Å / s and the sputtering rate is 1-10Å / s.