Display panel and method for manufacturing the same
By setting up crisscrossing dams on the thin film transistors of the Mini/Micro LED display panel, and using the air column during laser cutting to blow away the glue charcoal, the problem of too shallow laser cutting depth and lobes is solved, and the yield of the display panel is improved .
Patent Information
- Application Number
- CN202210173397.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-02-24
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2042-02-24
AI Technical Summary
During the laser cutting process, the existing Mini/Micro LED display panels are carbonized by polymers, resulting in the residual by-products in the cutting heat-affected zone, preventing laser cutting, resulting in the glass cutting depth too shallow, and problems such as edge collapse and cracks during the lobe process. , affects product yield.
A crisscrossing dam is prepared on the thin film transistor, and an air column is formed between the encapsulation layer and the dam. During laser cutting, the air column expands and blows away the generated glue charcoal to form a smooth cutting surface.
By setting up an air column between the enclosure and the encapsulation layer, the glue carbonized substances can be effectively removed, the cutting depth of the glass substrate is ensured, and the defective phenomena such as lobe collapse is reduced, and the yield of the display panel is improved.
Smart Images

Figure CN114566462B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the display field, and in particular to a display panel and a method for preparing the same. Background Art
[0002] Mini / Micro LED display has the characteristics of self-luminescence, high efficiency, low power consumption, and high stability. It is an important choice for the next generation of mainstream display technology and has the potential to replace existing technologies in many fields.
[0003] Since a layer of encapsulation glue is required on the surface of the LED chip, the encapsulation glue is used to enhance the push-pull force and water and oxygen resistance between the LED chip and the substrate. The encapsulation glue is mostly silicone or epoxy resin. For glass-based mini / microled display panels, a knife wheel cannot be used for cutting. Laser cutting is the current mainstream cutting method. Due to the short laser pulse time and the extremely high peak energy of the laser pulse, for some high molecular polymers, cutting the heat-affected zone will cause carbonization of the polymer. The by-products remaining in the cutting channel will prevent the laser from cutting the underlying film layer, which will lead to too shallow a depth of cutting into the glass, and edge collapse and cracks will occur during the splitting process, affecting the product yield. Summary of the invention
[0004] The purpose of the present application is to provide a display panel and a method for preparing the same, which can solve the technical problems of the existing display panel cutting process, such as the glass cutting depth being too shallow, and the occurrence of edge collapse and cracks during the splitting process.
[0005] To achieve the above-mentioned purpose, the present application provides a method for preparing a display panel, comprising the following steps: providing a substrate, on which a thin film transistor is prepared; preparing criss-cross dams on the thin film transistors; soldering an LED chip on a pad of the substrate; applying encapsulation glue on the dams, and forming an encapsulation layer after baking, with an air column formed between the encapsulation layer and the dams; and cutting the substrate, wherein the carbonized glue produced during cutting is blown out of the cutting channel to form a smooth cutting surface.
[0006] Furthermore, the dam is made by a yellow light process; the material of the dam includes one of silicon nitride, silicon oxide, and high molecular polymer.
[0007] Furthermore, the step of soldering the LED chip on the pad of the substrate includes: brushing solder paste on the pad of the substrate; placing the LED chips one by one on the middle position of the pad using a die bonding machine; and performing reflow soldering on the LED chips.
[0008] Furthermore, the dam includes a plurality of crisscross strips and a hollow area formed between the plurality of crisscross strips; the air column is formed in the hollow area.
[0009] Furthermore, in the step of cutting the substrate and blowing the carbonized glue produced during cutting to the outside of the cutting channel to form a smooth cutting surface, a laser is used to perform laser cutting on the substrate. During the laser cutting process, the packaging layer will produce carbonized glue, and the carbonized glue is attached to the packaging layer and / or the dam. During the laser cutting process, the air column expands after being heated, and the packaging layer on the surface of the air column is removed while the carbonized glue is blown away to form a cutting channel.
[0010] Furthermore, in the step of preparing crisscross dams on the thin film transistor, the dams are arranged in a cutting area of the substrate; and the angle between the dams and the substrate is 0 to 180°.
[0011] Furthermore, a distance between a side of the dam close to the encapsulation layer and a side away from the encapsulation layer is 1 to 100 micrometers.
[0012] Furthermore, the wavelength of the ultraviolet light source of the laser is 343 nanometers to 10640 nanometers.
[0013] Furthermore, the laser includes a nanosecond laser, a femtosecond laser, and a picosecond laser.
[0014] To achieve the above objectives, the present application also provides a display panel, which is prepared by the display panel preparation method as described above.
[0015] The technical effect of the present application is that a dam is set on the thin film transistor, and an air column is formed between the dam and the packaging layer. When the air column expands due to heat, it will blow away the generated carbonized glue and ensure the cutting depth of the glass substrate, so as to form a smooth cutting surface and improve the yield of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.
[0017] Figure 1 is a flow chart of a method for preparing a display panel provided in an embodiment of the present application;
[0018] Figure 2 is a schematic diagram of the structure after preparing the dam provided in the embodiment of the present application;
[0019] Figure 3is a schematic diagram of the structure after preparing the encapsulation layer provided in an embodiment of the present application;
[0020] Figure 4 is a schematic diagram of glue carbonization produced during laser cutting provided in an embodiment of the present application;
[0021] Figure 5 is a schematic diagram after laser cutting provided in an embodiment of the present application;
[0022] Figure 6 is a schematic diagram of a display panel provided in an embodiment of the present application.
[0023] Description of reference numerals:
[0024] 100, substrate; 200, thin film transistor; 300, dam; 400, encapsulation layer; 500, glue carbonization; 600, cutting channel;
[0025] 310. Strip; 320. Hollow area. DETAILED DESCRIPTION
[0026] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application. In addition, it should be understood that the specific implementation methods described herein are only used to illustrate and explain the present application, and are not used to limit the present application. In the present application, unless otherwise stated, the directional words such as "upper" and "lower" used generally refer to the upper and lower parts of the device in actual use or working state, specifically the drawing direction in the accompanying drawings; while "inside" and "outside" refer to the outline of the device.
[0027] The embodiments of the present application provide a display surface and a method for manufacturing the same. The following are detailed descriptions. It should be noted that the description order of the following embodiments is not intended to limit the preferred order of the embodiments.
[0028] like Figures 1 to 6 As shown, an embodiment of the present application provides a method for preparing a display panel, including steps S1 to S5.
[0029] S1 provides a substrate 100, on which a thin film transistor 200 is prepared. Specifically, the substrate 100 is a glass substrate, which plays a role of substrate and support. The thin film transistor 200 is arranged on the substrate 100, and the thin film transistor 200 is a circuit control switch of the display panel.
[0030] S2: a crisscross dam 300 is prepared on the thin film transistor 200 (see Figure 2 Specifically, an organic film (Polymer Film on Array, PFA) is formed on the thin film crystal 200, and a crisscross dam 300 is formed by a yellow light process.
[0031] The material of the dam 300 includes one of silicon nitride (SiNx), silicon oxide (SiOx), and high molecular polymer.
[0032] The dam 300 includes a plurality of crisscross strips 310 and a hollow area 320 formed between the plurality of crisscross strips. The strips 310 are long strips arranged horizontally or vertically, and crisscross to form a dam.
[0033] The included angle between the dam 300 and the substrate 100 is 0-180°.
[0034] The distance between the side of the dam 300 close to the thin film transistor 200 and the side away from the thin film transistor 200 is 1 to 100 microns, that is, the height of the dam 300 is 1 to 100 microns, and the size of the hollow area 320 is 1 to 100 microns, but this size is determined according to the surface tension of the packaging glue and is not fixed.
[0035] S3 solders the LED chip on the solder pad of the substrate 100, specifically, comprising the following steps:
[0036] The substrate 100 includes a plurality of pads, including a positive pad and a negative pad, and the positive pad and the negative pad are used to be connected to the positive electrode and the negative electrode on the LED chip correspondingly.
[0037] A steel mesh template matching the substrate 100 is used so that the holes on the steel mesh template can correspond to the pads on the substrate 100, and solder paste printing equipment is used to print solder paste on the substrate 100. When printing solder paste, the substrate 100 is first positioned on the support block, and the position of the steel mesh clamp on the threaded column is adjusted so that the steel mesh template can be rotated to fit the surface of the substrate 100, and then solder paste is poured on the steel mesh template, and then a scraper is used to scrape back and forth so that the solder paste passes through the upper hole of the steel mesh template and enters the pad.
[0038] The substrate 100 printed with solder paste is taken out, and then the LED chips are placed one by one in the middle position of the pad using a die bonding machine. Finally, the substrate 100 is placed in a reflow soldering device, and the LED chips are reflow soldered to tightly solder the LED chips on the pad.
[0039] S4: coating the dam 300 with encapsulation glue, and baking to form an encapsulation layer 400 (see Figure 3 ), since the surface tension of the glue is large, the hollow area 320 in the middle of the dam 300 cannot be filled, so after baking, an air column will be formed between the encapsulation layer 400 and the dam 300, and the air column is formed in the hollow area 320. The encapsulation glue is glue such as silicone, epoxy resin, etc.
[0040] S5 cuts the substrate 100, and the carbonized glue produced during cutting is blown out of the cutting channel 600 to form a smooth cutting surface. Specifically, the substrate 100 is cut by a laser, and the wavelength of the ultraviolet light source of the laser is 343 nanometers to 10640 nanometers. The laser includes a nanosecond laser, a femtosecond laser, and a picosecond laser.
[0041] During the laser cutting process, the packaging layer 400 will produce glue carbonization 500, and the glue carbonization 500 is attached to the packaging layer 400 and / or the dam 300 (see Figure 4 ).
[0042] During the laser cutting process, the air column expands after being heated, and the impact force generated by the air explosion removes the encapsulation layer 400 on the surface of the air column and blows away the glue carbonization 500, forming a cutting channel 600 (see Figure 5 ), ensure the cutting depth of the glass substrate, so that the cutting position of the glass can be easily separated during the glass cracking process, reducing undesirable phenomena such as crack edge collapse.
[0043] like Figure 6 As shown, an embodiment of the present application further provides a display panel, which is prepared by the display panel preparation method as described above.
[0044] The technical effect of the display panel and the preparation method thereof described in the embodiment of the present application is that a dam is set on the thin film transistor, and an air column is formed between the dam and the encapsulation layer. After the air column expands due to heat, it will blow away the generated carbonized glue and ensure the cutting depth of the glass substrate, so as to form a smooth cutting surface and improve the yield of the display panel.
[0045] The above is a detailed introduction to a display panel and a preparation method thereof provided in an embodiment of the present application. Specific examples are used herein to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea. At the same time, for technical personnel in this field, according to the idea of the present application, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present application.
Claims
1. A method for preparing a display panel, characterized in that: The following steps are involved: Providing a substrate, on which a thin film transistor is prepared; preparing crisscross dams on the thin film transistor; Soldering an LED chip on the soldering pad of the substrate; Coating encapsulation glue on the dam, and forming an encapsulation layer after baking, and forming an air column between the encapsulation layer and the dam; as well as Cutting the substrate, wherein carbonized glue produced during cutting is blown out of the cutting channel to form a smooth cutting surface; The dam includes a plurality of crisscross strips and a hollow area formed between the plurality of crisscross strips; The air column is formed in the hollow area; The step of cutting the substrate and blowing the carbonized glue produced during cutting out of the cutting channel to form a smooth cutting surface comprises: The substrate is laser cut by using a laser. During the laser cutting process, the encapsulation layer will produce carbonized glue, and the carbonized glue is attached to the encapsulation layer and / or the dam. During the laser cutting process, the air column expands after being heated, and the encapsulation layer on the surface of the air column is removed while the carbonized glue is blown away to form a cutting channel.
2. The method for preparing a display panel according to claim 1, wherein: The dam is made by yellow light process; The material of the dam includes one of silicon nitride, silicon oxide and high molecular polymer.
3. The method for preparing a display panel according to claim 1, wherein: The step of soldering the LED chip on the solder pad of the substrate comprises: Apply solder paste on the pads of the substrate; Using a die bonding machine to place the LED chips one by one on the middle position of the pad; The LED chip is subjected to a reflow process.
4. The method for preparing a display panel according to claim 1, wherein: In the step of preparing crisscross dams on the thin film transistor, The dam is arranged in the cutting area of the substrate; The included angle between the dam and the substrate is 0-180°.
5. The method for preparing a display panel according to claim 1, wherein: The distance between the side of the dam close to the encapsulation layer and the side far from the encapsulation layer is 1-100 microns.
6. The method for preparing a display panel according to claim 1, wherein: The laser includes a nanosecond laser, a femtosecond laser, and a picosecond laser.